Titanium nano coating decorative plate base material grain drawing process
By using a double-station wire drawing mechanism and a wire drawing speed warning mechanism in the wire drawing process of titanium nano-coated decorative panel substrate, the problem of inefficient processing efficiency caused by equipment damage is solved, and a more efficient and continuous wire drawing processing process is achieved.
Patent Information
- Application Number
- CN202411322379.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-23
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the wire drawing process, the processing efficiency of the titanium nano-coated decorative board substrate is often caused by damage to the wire drawing equipment, and the equipment needs to be shut down for maintenance, which affects the processing continuity.
The double-station wire drawing mechanism and the wire drawing speed warning mechanism are used to ensure that the other mechanism can be replaced immediately when one mechanism is damaged, avoid shutdown and repair, and improve cleaning and wire drawing efficiency through steps such as mechanical soaking and wiping cleaning and step-by-step wire drawing.
The continuous and efficiency of the wire drawing process of titanium nano-coated decorative panel substrate is achieved, avoiding stagnation caused by equipment damage, and ensuring smoother processing and higher quality.
Smart Images

Figure CN118990140A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of titanium nano-coating decorative plate substrate processing, in particular to a titanium nano-coating decorative plate substrate grain drawing process. Background Art
[0002] Titanium nano-coated decorative plate substrate is a plate made by improving the performance and appearance of the metal surface through a nano-particle coating of titanium or titanium compounds. Before use, in order to ensure the aesthetics of the titanium nano-coated decorative plate substrate, the titanium nano-coated decorative plate substrate needs to be subjected to wire drawing.
[0003] At present, the general process of wire drawing processing of surface texture of titanium nano-coated decorative plate substrate is: cleaning of substrate, selection of wire drawing tools, preheating before wire drawing, wire drawing of substrate surface and annealing treatment. Although the wire drawing processing of surface texture of titanium nano-coated decorative plate substrate can be achieved under the above wire drawing process, the wire drawing is mainly carried out by single-station wire drawing equipment under the above wire drawing process, and the wire drawing mechanism of the wire drawing equipment of titanium nano-coated decorative plate substrate is often damaged during the wire drawing process. In this case, the equipment can only be shut down for maintenance before the wire drawing processing of titanium nano-coated decorative plate substrate can continue, resulting in the entire wire drawing processing process of the surface texture of titanium nano-coated decorative plate substrate not being smooth enough and the wire drawing processing efficiency is relatively low. Summary of the invention
[0004] The purpose of the present invention is to provide a titanium nano-coated decorative plate substrate wire drawing process in order to solve the above problems.
[0005] The present invention achieves the above-mentioned purpose through the following technical solutions:
[0006] A titanium nano-coated decorative plate substrate wire drawing process, comprising the following steps:
[0007] Step 1: Pretreatment of the substrate: cleaning the surface of the titanium nano-coated decorative plate substrate to be drawn to remove oil and oxides on the surface, and determining the drawing direction and depth of the titanium nano-coated decorative plate substrate according to the drawing requirements;
[0008] Step 2: Configuration of wire drawing tools: a double-station wire drawing mechanism is arranged on the wire drawing platform of the titanium nano-coated decorative plate substrate to ensure that the double-station wire drawing mechanisms can be interchanged with each other, and a wire drawing speed warning mechanism is arranged on the wire drawing platform;
[0009] Step 3: preheating the substrate, preheating the titanium nano-coated decorative plate substrate to be drawn to a specified temperature;
[0010] Step 4: Substrate drawing: Place the preheated titanium nano-coated decorative panel substrate on the drawing platform, and use the drawing mechanism to perform the drawing operation at a suitable drawing speed and pressure;
[0011] Step 5: annealing of the substrate, placing the titanium nano-coated decorative plate substrate after wire drawing in an annealing furnace for annealing to eliminate the residual stress inside the titanium nano-coated decorative plate substrate after wire drawing, and ensure the stability of the shape and size of the titanium nano-coated decorative plate substrate after wire drawing;
[0012] Step 6: Cleaning and protection: remove the debris remaining on the surface of the titanium nano-coated decorative board substrate after annealing, and apply a transparent protective layer on the titanium nano-coated decorative board substrate to complete the wire drawing process of the titanium nano-coated decorative board substrate.
[0013] Furthermore, in step 1, when cleaning the oil stains and oxides on the surface of the substrate, it is mainly achieved by mechanical immersion and wiping cleaning. Under such a cleaning method, not only can the cleaning efficiency of the substrate surface be higher, but also the manual labor intensity of cleaning the oil stains and oxides on the surface of the substrate can be reduced.
[0014] Furthermore, in step 1, in addition to determining the wire drawing direction and depth, the wire drawing passes and speed must also be determined to ensure the quality of the titanium nano-coated decorative plate substrate after wire drawing.
[0015] Furthermore, the two wire drawing mechanisms on the wire drawing platform in the step 2 have the same structure, and the two wire drawing mechanisms are replaced with the help of an electric slide rail when in use. Such a design can ensure the urgent use of the other wire drawing mechanism when one wire drawing machine is damaged, thereby avoiding long-term shutdown and maintenance of the wire drawing equipment, making the wire drawing process of the titanium nano-coated decorative panel substrate more continuous and the wire drawing efficiency higher.
[0016] Furthermore, the wire drawing speed warning mechanism in step 2 is composed of a speed detection instrument and an alarm, so that when the wire drawing speed of the titanium nano-coated decorative plate substrate is too fast, an alarm can be issued in time to remind the staff to make timely adjustments. This design can avoid excessive damage and scrapping of the titanium nano-coated decorative plate substrate during wire drawing due to the wire drawing speed.
[0017] Furthermore, the preheating temperature in step 3 is 900°C-100°C, and in step 4, the titanium nano-coated decorative plate substrate is firstly rough-drawn during wire drawing, and then fine-drawn. The step-by-step wire drawing method can make the wire drawing texture on the surface of the titanium nano-coated decorative plate substrate more refined.
[0018] Furthermore, the purpose of controlling the drawing speed and pressure in step 4 is that too fast a drawing speed and too high a pressure may cause surface distortion and cracking.
[0019] The beneficial effects of the present invention are:
[0020] The present invention adopts a replaceable double-station wire drawing mechanism in the wire drawing process. When one wire drawing mechanism is damaged during the wire drawing process of the surface texture of the titanium nano-coated decorative plate substrate, the other wire drawing mechanism can be replaced and put into use to ensure the continuation of the wire drawing process of the surface texture of the titanium nano-coated decorative plate substrate, avoiding the disadvantage of long-term stagnation of the wire drawing process of the surface texture of the titanium nano-coated decorative plate substrate due to damage to the wire drawing equipment, making the entire wire drawing process of the surface texture of the titanium nano-coated decorative plate substrate smoother and improving the wire drawing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The present invention provides a flow chart of a titanium nano-coated decorative plate substrate wire drawing process. DETAILED DESCRIPTION
[0022] A titanium nano-coated decorative plate substrate wire drawing process, comprising the following steps:
[0023] Step 1: Pretreatment of the substrate: cleaning the surface of the titanium nano-coated decorative plate substrate to be drawn to remove oil and oxides on the surface, and determining the drawing direction and depth of the titanium nano-coated decorative plate substrate according to the drawing requirements;
[0024] Step 2: Configuration of wire drawing tools: a double-station wire drawing mechanism is arranged on the wire drawing platform of the titanium nano-coated decorative plate substrate to ensure that the double-station wire drawing mechanisms can be interchanged with each other, and a wire drawing speed warning mechanism is arranged on the wire drawing platform;
[0025] Step 3: preheating the substrate, preheating the titanium nano-coated decorative plate substrate to be drawn to a specified temperature;
[0026] Step 4: Substrate drawing: Place the preheated titanium nano-coated decorative panel substrate on the drawing platform, and use the drawing mechanism to perform the drawing operation at a suitable drawing speed and pressure;
[0027] Step 5: annealing of the substrate, placing the titanium nano-coated decorative plate substrate after wire drawing in an annealing furnace for annealing to eliminate the residual stress inside the titanium nano-coated decorative plate substrate after wire drawing, and ensure the stability of the shape and size of the titanium nano-coated decorative plate substrate after wire drawing;
[0028] Step 6: Cleaning and protection: remove the debris remaining on the surface of the titanium nano-coated decorative board substrate after annealing, and apply a transparent protective layer on the titanium nano-coated decorative board substrate to complete the wire drawing process of the titanium nano-coated decorative board substrate.
[0029] In this embodiment, in step 1, cleaning of oil stains and oxides on the surface of the substrate is mainly achieved by mechanical immersion and wiping cleaning. Under such a cleaning method, not only the cleaning efficiency of the substrate surface can be improved, but also the manual labor intensity of cleaning the oil stains and oxides on the surface of the substrate can be reduced.
[0030] In this embodiment, in step 1, in addition to determining the wire drawing direction and depth, the wire drawing passes and speed also need to be determined to ensure the quality of the titanium nano-coated decorative plate substrate after wire drawing.
[0031] In this embodiment, the two wire drawing mechanisms on the wire drawing platform in step 2 have the same structure, and the two wire drawing mechanisms are replaced with the help of an electric slide rail when in use. This design can ensure the urgent use of the other wire drawing mechanism when one wire drawing machine is damaged, avoiding long-term shutdown and maintenance of the wire drawing equipment, making the wire drawing process of the titanium nano-coated decorative panel substrate more continuous and the wire drawing efficiency higher.
[0032] In this embodiment, the wire drawing speed warning mechanism in step 2 is composed of a speed detection instrument and an alarm, so that when the wire drawing speed of the titanium nano-coated decorative plate substrate is too fast, an alarm is promptly issued to remind the staff to make timely adjustments. This design can avoid excessive damage and scrapping of the titanium nano-coated decorative plate substrate due to the wire drawing speed.
[0033] In this embodiment, the preheating temperature in step 3 is 900°C-100°C, and in step 4, the titanium nano-coated decorative plate substrate is firstly rough-drawn during wire drawing, and then fine-drawn. The step-by-step wire drawing method can make the wire drawing texture on the surface of the titanium nano-coated decorative plate substrate finer.
[0034] In this embodiment, the purpose of controlling the wire drawing speed and pressure in step 4 is that too fast wire drawing speed and too high pressure may cause surface distortion and cracking.
[0035] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A titanium nano-coated decorative plate substrate wire drawing process, characterized in that: It includes the following steps: Step 1: Pretreatment of the substrate: cleaning the surface of the titanium nano-coated decorative plate substrate to be drawn to remove oil and oxides on the surface, and determining the drawing direction and depth of the titanium nano-coated decorative plate substrate according to the drawing requirements; Step 2: Configuration of wire drawing tools: a double-station wire drawing mechanism is arranged on the wire drawing platform of the titanium nano-coated decorative plate substrate to ensure that the double-station wire drawing mechanisms can be interchanged with each other, and a wire drawing speed warning mechanism is arranged on the wire drawing platform; Step 3: preheating the substrate, preheating the titanium nano-coated decorative plate substrate to be drawn to a specified temperature; Step 4: Substrate drawing: Place the preheated titanium nano-coated decorative panel substrate on the drawing platform, and use the drawing mechanism to perform the drawing operation at a suitable drawing speed and pressure; Step 5: annealing of the substrate, placing the titanium nano-coated decorative plate substrate after wire drawing in an annealing furnace for annealing to eliminate the residual stress inside the titanium nano-coated decorative plate substrate after wire drawing, and ensure the stability of the shape and size of the titanium nano-coated decorative plate substrate after wire drawing; Step 6: Cleaning and protection: remove the debris remaining on the surface of the titanium nano-coated decorative board substrate after annealing, and apply a transparent protective layer on the titanium nano-coated decorative board substrate to complete the wire drawing process of the titanium nano-coated decorative board substrate.
2. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: In the step 1, when cleaning the oil stains and oxides on the surface of the substrate, it is mainly achieved by mechanical immersion wiping cleaning.
3. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: In step 1, the drawing direction and depth must be determined while also determining the drawing passes and speed.
4. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: The two wire drawing mechanisms on the wire drawing platform in step 2 have the same structure, and the two wire drawing mechanisms are transposed by means of an electric slide rail when in use.
5. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: The wire drawing speed warning mechanism in step 2 is composed of a speed detection instrument and an alarm, so as to promptly issue an alarm when the wire drawing speed of the titanium nano-coated decorative plate substrate is too fast, and remind the staff to make timely adjustments.
6. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: The preheating temperature in step 3 is 900° C.-100° C., and in step 4, the titanium nano-coated decorative plate substrate is firstly subjected to rough wire drawing during wire drawing, and then fine wire drawing is performed on the titanium nano-coated decorative plate substrate.
7. The titanium nano-coated decorative plate substrate wire drawing process according to claim 1, characterized in that: The purpose of controlling the drawing speed and pressure in step 4 is that too fast a drawing speed and too high a pressure may cause surface distortion and cracking.
Citation Information
Patent Citations
Surface wiredrawing treatment method for stainless steel decorative plate
CN114800181A
Cladding wiredrawing aluminum plate and surface wiredrawing treatment method thereof
CN115972709A
Production process of fingerprint-free wiredrawing stainless steel plate
CN117000805A
Preparation method of TA4 titanium alloy foil for OLED flexible screen metal mask plate
CN117019915A
Cold stamping device of rotation type multi -press head auto parts
CN208772276U