Prediction method for predicting sublance insertion depth by adopting sublance and furnace lining thickness gauge
By calculating the formulas for the sub-lance and the furnace lining thickness gauge, the insertion depth of the sub-lance can be predicted, thus solving the problem of sub-lance damage caused by irregular thickening or thinning of the converter bottom, and realizing safe and accurate measurement of the sub-lance.
Patent Information
- Application Number
- CN202310581208.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-22
- Publication Date
- 2024-11-22
AI Technical Summary
In existing technologies, irregular thickening or thinning of the converter bottom causes the sub-lance probe to make rigid contact with the bottom, resulting in damage to the sub-lance or insufficient insertion depth for measurement, and making it impossible to accurately predict the insertion depth of the sub-lance.
By using the calculation formulas of the auxiliary lance and furnace lining thickness gauge, the distance from the auxiliary lance probe to the furnace bottom from the molten steel surface is predicted. Combined with the converter molten pool level and furnace bottom thickness, the insertion depth of the auxiliary lance is adjusted to avoid damage and ensure measurement accuracy.
It effectively prevents damage to the secondary gun probe, ensures measurement accuracy, avoids measurement failures caused by irregular thickening or thinning, and improves the measurement success rate.
Smart Images

Figure CN118996043A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a prediction method, in particular to a prediction method for predicting the insertion depth of an auxiliary gun by using an auxiliary gun and a furnace lining thickness gauge, and belongs to the technical field of online measurement of auxiliary guns in steel enterprises. Background Art
[0002] Meishan Steel Plant currently has 5 converters. During the existing converter production process, due to various reasons, the bottom of the converter thickens irregularly during the entire furnace smelting process. If the thickened part of the converter bottom is on the measuring side of the auxiliary gun, and the thickened part of the converter bottom is too much, when the auxiliary gun is measured online, the gun head of the auxiliary gun will make rigid contact with the bottom of the converter, resulting in damage to the auxiliary gun probe, making it impossible for the auxiliary gun to complete the measurement. At the same time, due to various reasons, the bottom of the converter is irregularly thinned during the entire furnace smelting process. If the bottom of the converter is thinned too much at the auxiliary gun measurement point, the auxiliary gun insertion depth is too shallow and the auxiliary gun cannot be measured. In the measurement process of the converter auxiliary gun, a new solution is urgently needed to predict the thickness of the converter bottom to solve the above technical problems. Summary of the invention
[0003] The present invention is aimed at the problems existing in the prior art and provides a method for predicting the insertion depth of the auxiliary gun by using an auxiliary gun and a furnace lining thickness gauge. The technical solution specifically relates to a method for preventing the thickness of the converter bottom from being predicted due to the irregularity of the thickening of the converter bottom during the production process, which causes the auxiliary gun probe to be in rigid contact with the converter bottom during online measurement of the converter auxiliary gun, thereby damaging the auxiliary gun probe and making it impossible for the auxiliary gun to complete the measurement. The problem of the converter bottom increasing irregularly during the production process of the existing converter, which causes the auxiliary gun tip to be in rigid contact with the converter bottom during the measurement process, thereby damaging the auxiliary gun tip and making it impossible for the auxiliary gun to complete the measurement, is solved. Ensuring that the auxiliary gun tip is at a certain safety distance from the converter bottom during the measurement process is the main factor in ensuring that the auxiliary gun tip is not damaged and that the auxiliary gun completes the measurement. Its main control principle is to predict the distance between the auxiliary gun probe and the converter bottom through the relevant calculation formula according to the molten pool level measured by the auxiliary gun online, the lining thickness of the converter bottom measured by the lining thickness gauge and the base height of the converter. Through the implementation of this technology, it can be ensured that when the converter is in the whole service of smelting, the auxiliary gun head will not be damaged due to the increase of the converter bottom, and it can also be ensured that when the converter is in the whole service of smelting, the lining will be thinned due to the erosion of the converter bottom, making the auxiliary gun insertion depth too shallow and unable to be measured.
[0004] In order to achieve the above object, the technical solution of the present invention is as follows: a method for predicting the insertion depth of a secondary gun using a secondary gun and a furnace lining thickness gauge, characterized in that the method comprises the following steps:
[0005] Step 1: Calculation formula for the distance between the auxiliary gun probe and the furnace bottom from the molten steel surface;
[0006] Step 2: Determine the thickening of the converter bottom;
[0007] The third step is to determine the thinning of the converter bottom.
[0008] As an improvement of the present invention, the first step is to calculate the distance between the auxiliary gun probe and the furnace bottom from the molten steel surface, as follows:
[0009] H = h1-h2,
[0010] H: The distance between the auxiliary gun probe and the bottom of the furnace from the molten steel surface,
[0011] h1: molten pool level measured by the auxiliary gun,
[0012] h2: The thickness gauge measures the thickness of the converter bottom.
[0013] D = d1-d2,
[0014] D: Change in converter bottom,
[0015] d1: The thickness of the converter bottom measured by the thickness gauge,
[0016] d2: masonry thickness of converter bottom,
[0017] C: Insertion depth of the auxiliary gun.
[0018] As an improvement of the present invention, in the second step, the converter bottom is thickened.
[0019] During the whole smelting process of the converter, due to the production process, raw materials and maintenance of the converter bottom refractory materials, the thickness of the converter bottom refractory materials may increase compared with the original converter bottom refractory materials over a certain period of time.
[0020] The details are as follows: When the sublance measures in the molten steel, in order to ensure accurate measurement and obtain qualified steel samples, there are certain range requirements for the depth of the sublance probe inserted into the molten steel surface. The insertion depth (C) of the sublance is usually between 30 - 70 cm. If the insertion depth of the sublance is too shallow, the sublance cannot obtain qualified steel samples and the temperature measurement error is relatively large. When the insertion depth of the sublance is too deep, the sublance probe is affected by high temperature in the molten steel, which will damage the connectors and holders of the sublance. Therefore, it is necessary to dynamically adjust the insertion depth of the sublance according to the amount of molten iron charged in the converter and the molten bath level of the converter. When the change amount (D) of the converter bottom > 0, it indicates that the converter bottom is in a thickening state. Due to the irregular thickening of the converter bottom, during the on-line measurement of the converter sublance, since the thickness of the converter bottom cannot be predicted, the sublance probe makes rigid contact with the converter bottom, resulting in damage to the sublance probe and the sublance being unable to complete the measurement. Therefore, through the on-line measurement of the molten bath level of the converter by the sublance and the thickness of the converter bottom measured by the converter lining thickness gauge, the distance H from the molten steel surface to the converter bottom by the sublance probe is calculated through the corresponding calculation formula, and the distance between the converter bottom and the insertion depth during the on-line measurement of the sublance is compared, so as to predict whether the sublance can measure normally or the possible measurement consequences. The measurement points of the sublance are usually at a certain distance from the center of the converter. And for the converter bottom, during the whole campaign process, the thickening of each point at the bottom of the furnace is non-linear. The thickness of the converter bottom is measured by the converter lining thickness gauge (h2). In this example, the average value of the bottom thickness of each point within a circle with a radius of 30 cm centered on the measurement point of the sublance is used as the bottom thickness of the sublance measurement point. When comparing the distance (H) from the molten steel surface to the bottom of the furnace by the sublance probe with the insertion depth of the sublance, when the distance (H) from the molten steel surface to the bottom of the furnace by the sublance probe < 30 cm, the sublance probe may make rigid contact with the converter bottom, resulting in damage to the sublance probe or a shallow insertion depth of the sublance, making the sublance unable to complete the correct measurement, and it is necessary to perform process treatment on the converter bottom. When 30 cm ≤ C ≤ 45 cm for the distance (H) from the molten steel surface to the bottom of the furnace by the sublance probe, the sublance can measure, but a warning is given. When 45 cm < C < 70 cm for the distance (H) from the molten steel surface to the bottom of the furnace by the sublance probe, the insertion depth of the sublance is appropriate and the sublance can measure.
[0021] As an improvement of the present invention, in the third step, in the case of the converter bottom thinning, during the whole campaign smelting process of the converter, due to reasons such as production process, raw materials, and maintenance of the converter bottom refractories, the refractories at the bottom of the converter may be thinned compared with the thickness of the original converter bottom refractories within a certain period of time.
[0022] The details are as follows: When the sublance measures in the molten steel, in order to ensure accurate measurement and obtain qualified steel samples, there are certain range requirements for the depth of the sublance probe inserted into the molten steel surface. The insertion depth (C) of the sublance is usually between 30 - 70 cm. If the insertion depth of the sublance is too shallow, the sublance cannot obtain qualified steel samples and the temperature measurement error is large. When the insertion depth of the sublance is too deep, the sublance probe is affected by high temperature in the molten steel, which will damage the connectors and holders of the sublance. Therefore, it is necessary to dynamically adjust the insertion depth of the sublance according to the molten steel charge and the bath level of the converter. When the change amount (D) of the converter bottom < 0, it indicates that the converter bottom is in a thinning state. Due to the irregularity of the converter bottom thinning, during the on-line measurement of the converter sublance, since the thickness of the converter bottom cannot be predicted, the insertion depth of the sublance is too shallow, causing the sublance to be unable to complete the measurement. Therefore, through the on-line measurement of the converter bath level by the sublance and the thickness of the converter bottom measured by the converter lining thickness gauge, the distance (H) from the sublance tip to the converter bottom from the molten steel surface is calculated through the corresponding calculation formula, and the distance between the converter bottom and the insertion depth during the on-line measurement of the sublance is compared, so as to predict whether the sublance can measure normally or the possible measurement consequences. The measurement point of the sublance is usually at a certain distance from the converter center. And for the converter bottom, during the whole campaign, the thinning of each point at the bottom is irregular. The thickness of the converter bottom is measured by the converter lining thickness gauge (h2). In this example, the average value of the bottom thickness of each point within a circle with a radius of 30 cm centered on the measurement point of the sublance in the converter is used as the bottom thickness (h2) of the sublance measurement point. By comparing the distance (H) from the sublance probe to the bottom from the molten steel surface with the insertion depth of the sublance, when 45 cm < C < 70 cm for the distance (H) from the sublance probe to the bottom from the molten steel surface, the insertion depth of the sublance is appropriate and the sublance can measure. When 70 cm < C < 80 cm for the distance (H) from the sublance probe to the bottom from the molten steel surface, the insertion depth of the sublance is too deep and the sublance cannot measure. It is necessary to adjust the mechanical lower limit of the sublance body to the lower limit for the sublance to complete the measurement. When the distance (H) from the sublance probe to the bottom from the molten steel surface > 80 cm, the insertion depth of the sublance is inappropriate and the sublance cannot measure. Even if the mechanical lower limit of the sublance body is adjusted to the lower limit, the sublance cannot complete the measurement. In this case, it is necessary to stop the converter production, and through the corresponding converter bottom process gunning technology, make the refractory material of the converter bottom reach a certain thickness before production can resume and the sublance can complete the measurement.
[0023] Compared with the prior art, the present invention has the following advantages. The prior art cannot predict whether the insertion depth of the auxiliary gun is appropriate through the auxiliary gun and the furnace lining thickness gauge before the auxiliary gun is measured. The present invention can predict whether the insertion depth of the auxiliary gun is appropriate by calculating through the auxiliary gun and the furnace lining thickness gauge through relevant formulas. Since the converter is thickened during the production process of the whole furnace operation, it is prevented that the thickness of the converter bottom cannot be predicted during the online measurement of the converter auxiliary gun, causing the auxiliary gun probe to rigidly contact the converter bottom, causing damage to the auxiliary gun probe, and making it impossible for the auxiliary gun to complete the measurement. The present invention can predict whether the insertion depth of the auxiliary gun is appropriate before the auxiliary gun is measured, so that the insertion depth of the auxiliary gun can be adjusted before measurement. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 : It is a schematic diagram showing the cross-section of the auxiliary gun from the center line of the converter during the measurement process;
[0025] Figure 2 : It is a top-down schematic diagram showing the distance between the auxiliary gun and the converter centerline during the measurement process. DETAILED DESCRIPTION
[0026] In order to deepen the understanding of the present invention, the present embodiment is described in detail below with reference to the accompanying drawings.
[0027] Example 1: See Figure 1 A method for predicting the insertion depth of a secondary gun using a secondary gun and a furnace lining thickness gauge, the method comprising the following steps:
[0028] Step 1: Calculation formula for the distance between the auxiliary gun probe and the molten steel surface and the furnace bottom
[0029] The details are as follows:
[0030] H=h1-h2
[0031] H: The distance between the auxiliary gun probe and the molten steel surface and the furnace bottom
[0032] h1: molten pool level measured by the auxiliary gun
[0033] h2: Thickness gauge measures the thickness of the converter bottom
[0034] D=d1-d2
[0035] D: Change in converter bottom
[0036] d1: The thickness of the converter bottom measured by the thickness gauge
[0037] d2: masonry thickness of converter bottom
[0038] C: Insertion depth of auxiliary gun
[0039] Step 2. Condition of the increased thickness of the converter bottom
[0040] During the smelting process of the entire converter campaign, due to reasons such as production processes, raw materials, and the maintenance of the refractory material at the converter bottom, the refractory material at the converter bottom may increase in thickness compared to the original refractory material at the converter bottom within a certain period.
[0041] Specifically as follows: When the sublance measures in the molten steel, to ensure accurate measurement and obtain a qualified steel sample, there are certain range requirements for the depth of the sublance probe inserted into the molten steel surface. The insertion depth (C) of the sublance is usually between 30 - 70 cm. If the insertion depth of the sublance is too shallow, the sublance cannot obtain a qualified steel sample and the temperature measurement error is relatively large. When the insertion depth of the sublance is too deep, the sublance probe is affected by high temperature in the molten steel, which will damage the connectors and holders of the sublance. Therefore, it is necessary to dynamically adjust the insertion depth of the sublance according to the amount of molten iron charged into the converter and the molten bath level of the converter. When the change amount (D) of the converter bottom > 0, it indicates that the converter bottom is in a state of increased thickness. Due to the irregularity of the increase in the converter bottom thickness, during the on-line measurement of the converter sublance, since the thickness of the converter bottom cannot be predicted, the sublance probe makes rigid contact with the converter bottom, resulting in damage to the sublance probe and making the sublance unable to complete the measurement. Therefore, by measuring the molten bath level of the converter with the on-line sublance and the thickness of the converter bottom measured by the converter lining thickness gauge, the distance H from the molten steel surface to the converter bottom of the sublance probe is calculated through the corresponding calculation formula, and the distance of the converter bottom is compared with the insertion depth during the on-line measurement of the sublance, so as to predict whether the sublance can measure normally or the possible measurement consequences. The measurement points of the sublance are usually at a certain distance from the center of the converter. During the entire converter campaign, the thickness increase of each point at the converter bottom is non-linear. The thickness of the converter bottom is measured by the converter lining thickness gauge (h2). In this example, the average value of the bottom thickness of each point within a circle with a radius of 30 cm centered on the measurement point of the sublance is used as the bottom thickness of the sublance measurement point. When comparing the distance (H) from the molten steel surface to the bottom of the sublance probe with the insertion depth of the sublance, when the distance (H) from the molten steel surface to the bottom of the sublance probe < 30 cm, the sublance probe may make rigid contact with the converter bottom, resulting in damage to the sublance probe or a shallow insertion depth of the sublance, making the sublance unable to complete the correct measurement, and it is necessary to perform process treatment on the converter bottom. When 30 cm ≤ C ≤ 45 cm for the distance (H) from the molten steel surface to the bottom of the sublance probe, the sublance can measure, but a warning is given. When 45 cm < C < 70 cm for the distance (H) from the molten steel surface to the bottom of the sublance probe, the insertion depth of the sublance is appropriate and the sublance can measure.
[0042] Step 3. Condition of the decreased thickness of the converter bottom
[0043] During the smelting process of the entire converter campaign, due to reasons such as production processes, raw materials, and the maintenance of the refractory materials at the bottom of the converter, the refractory materials at the bottom of the converter may be thinned compared to the original thickness of the refractory materials at the bottom of the converter over a certain period of time.
[0044] Specifically as follows: When the sublance measures in the molten steel, to ensure accurate measurement and obtain a qualified steel sample, there are certain range requirements for the depth of the sublance probe inserted into the molten steel surface. The insertion depth (C) of the sublance is usually between 30 - 70 cm. If the insertion depth of the sublance is too shallow, the sublance cannot obtain a qualified steel sample and the temperature measurement error is large. When the insertion depth of the sublance is too deep, the sublance probe is affected by high temperature in the molten steel, which will damage the connectors and holders of the sublance. Therefore, it is necessary to dynamically adjust the insertion depth of the sublance according to the molten steel charge and the molten bath level of the converter. When the change amount (D) of the converter bottom < 0, it indicates that the converter bottom is in a thinning state. Due to the irregularity of the thinning of the converter bottom, when the sublance measures online in the converter, since the thickness of the converter bottom cannot be predicted, the insertion depth of the sublance is too shallow, resulting in the sublance being unable to complete the measurement. Therefore, by measuring the molten bath level of the converter with the sublance online and the thickness of the converter bottom measured by the converter lining thickness gauge, the distance (H) from the molten steel surface to the converter bottom of the sublance tip is calculated through the corresponding calculation formula, and the distance of the converter bottom is compared with the insertion depth during the online measurement of the sublance, so as to predict whether the sublance can measure normally or the possible measurement consequences. The measurement points of the sublance are usually at a certain distance from the center of the converter. During the entire converter campaign, the thinning of each point at the bottom of the converter is irregular. The thickness of the converter bottom is measured by the converter lining thickness gauge (h2). In this case, the average value of the bottom thickness of each point within a circle with a radius of 30 cm centered on the measurement point of the sublance in the converter is used as the bottom thickness (h2) of the sublance measurement point. When comparing the distance (H) from the sublance probe to the bottom from the molten steel surface with the insertion depth of the sublance, when 45 cm < C < 70 cm for the distance (H) from the sublance probe to the bottom from the molten steel surface, the insertion depth of the sublance is appropriate and the sublance can measure. When 70 cm < C < 80 cm for the distance (H) from the sublance probe to the bottom from the molten steel surface, the insertion depth of the sublance is too deep and the sublance cannot measure. The mechanical lower limit of the sublance body must be adjusted to the lower limit for the sublance to complete the measurement. When the distance (H) from the sublance probe to the bottom from the molten steel surface > 80 cm, the insertion depth of the sublance is inappropriate and the sublance cannot measure. Even if the mechanical lower limit of the sublance body is adjusted to the lower limit, the sublance cannot complete the measurement. In this case, it is necessary to stop the production of the converter. Through the corresponding converter bottom process gunning technology, the refractory materials at the bottom of the converter reach a certain thickness before production can resume and the sublance can complete the measurement.
[0045] It should be noted that the above embodiments are not intended to limit the protection scope of the present invention, and equivalent changes or substitutions made on the basis of the above technical solutions all fall within the protection scope of the claims of the present invention.
Claims
1. A prediction method for the insertion depth of the auxiliary gun using an auxiliary gun and a furnace lining thickness gauge, It is characterized in that The method comprises the following steps: Step 1: Calculation formula for the distance between the auxiliary gun probe and the furnace bottom from the molten steel surface; Step 2: Determine the thickening of the converter bottom; The third step is to determine the thinning of the converter bottom.
2. The method for predicting the insertion depth of the auxiliary gun using the auxiliary gun and the furnace lining thickness gauge according to claim 1 is characterized in that the first step is to calculate the distance between the auxiliary gun probe and the furnace bottom from the molten steel surface according to the formula, The details are as follows: H = h1-h2, H: The distance between the auxiliary gun probe and the bottom of the furnace from the molten steel surface, h1: molten pool level measured by the auxiliary gun, h2: The thickness gauge measures the thickness of the converter bottom. D = d1-d2, D: Change in converter bottom, d1: The thickness of the converter bottom measured by the thickness gauge, d2: masonry thickness of converter bottom, C: Insertion depth of the auxiliary gun.
3. The method for predicting the insertion depth of the auxiliary gun using the auxiliary gun and the furnace lining thickness gauge according to claim 2, It is characterized in that The second step is the thickening of the converter bottom, as follows: when the auxiliary gun is measuring in the molten steel, the insertion depth (C) of the auxiliary gun is usually between 30-70cm. When the change in the converter bottom (D)>0, it indicates that the converter bottom is in a thickening state. Due to the irregularity of the thickening of the converter bottom, the thickness of the converter bottom cannot be predicted during the online measurement of the converter auxiliary gun, causing the auxiliary gun probe to rigidly contact the converter bottom, causing damage to the auxiliary gun probe and making it impossible for the auxiliary gun to complete the measurement. Therefore, the auxiliary gun is used to measure the converter's molten pool level online and the thickness of the converter bottom measured by the lining thickness gauge. The distance H between the auxiliary gun probe and the converter bottom is calculated from the molten steel surface through the corresponding calculation formula, and the distance between the converter bottom and the auxiliary gun is compared with the insertion depth of the auxiliary gun during online measurement, so as to predict whether the auxiliary gun can measure normally or the possible measurement consequences.
4. The method for predicting the insertion depth of the auxiliary gun using the auxiliary gun and the furnace lining thickness gauge according to claim 3, It is characterized in that The third step is the thinning of the converter bottom, as follows: when the auxiliary gun is measuring in the molten steel, in order to ensure accurate measurement and obtain qualified steel samples, there is a certain range requirement for the depth of the auxiliary gun probe inserted into the molten steel surface. The insertion depth (C) of the auxiliary gun is usually between 30-70cm. If the insertion depth of the auxiliary gun is too shallow, the auxiliary gun cannot obtain qualified steel samples and the temperature measurement error is large. When the insertion depth of the auxiliary gun is too deep, the auxiliary gun probe is affected by the high temperature in the molten steel, which will damage the connector and holder of the auxiliary gun. Therefore, the auxiliary gun insertion depth is adjusted dynamically according to the amount of molten steel charged and the molten pool level of the converter. When the change in the converter bottom (D) is <0, it indicates that the converter The bottom of the converter is in a thinning state. Due to the irregularity of the thinning of the converter bottom, when the converter auxiliary gun is measured online, the thickness of the converter bottom cannot be predicted, resulting in the insertion depth of the auxiliary gun being too shallow, making it impossible for the auxiliary gun to complete the measurement. Therefore, the auxiliary gun is used to measure the converter's molten pool level online and the thickness of the converter bottom measured by the lining thickness gauge. The distance (H) between the auxiliary gun head and the molten steel surface and the converter bottom is calculated by the corresponding calculation formula, and the distance of the converter bottom is compared with the insertion depth of the auxiliary gun during online measurement, so as to predict whether the auxiliary gun can be measured normally or the possible measurement consequences. The thickness of the converter bottom is measured by the converter lining thickness gauge (h2).