Method and system for extracting lithium from lithium ore with zero emission of CO2
The CO2 concentration in flue gas is increased through CO2 concentration preheating and predecomposition system and energy-saving preheating system, which solves the problem of low CO2 concentration in limestone sintering method, and achieves zero CO2 emissions and energy consumption in lithium ore extraction process. reduce.
Patent Information
- Application Number
- CN202411057193.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-22
AI Technical Summary
During the lithium extraction process of lithium ore, the CO2 concentration in the flue gas is low, which cannot meet the carbonization demand of leaching liquid, resulting in increased production costs, large carbon emissions, and high system energy consumption.
A method for lithium extraction of lithium with zero CO2 emissions was designed. Through CO2 concentration preheating and predecomposition system and energy-saving preheating system, the CO2 concentration in flue gas is increased, the carbonization process needs are met, and waste heat recovery and utilization are reduced. Energy consumption.
It achieves zero CO2 emissions, reduces production costs and energy consumption, improves the preparation efficiency and recovery rate of lithium carbonate, and simplifies the process flow.
Smart Images

Figure CN118996152A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium extraction from lithium ore, and in particular to a method and system for extracting lithium from lithium ore with zero CO2 emission. Background Art
[0002] Lithium is an indispensable mineral raw material for the development of new energy industry. It is widely used in lithium batteries, glass and ceramics, lithium-based grease, metallurgical casting, medicine and atomic energy industry. In recent years, with the vigorous development of power battery industry, the demand for lithium has shown explosive growth, which has also promoted the continuous advancement of lithium extraction technology.
[0003] Lithium resources are divided into brine type and ore type. Rock lithium minerals mainly include spodumene, lepidolite, phosphate lithium aluminum stone and petalite. At present, the lithium resources mined commercially are mainly brine lithium ore and spodumene ore. Although the total amount of brine lithium resources is dominant and the cost of lithium extraction from brine is lower than that from ore, the output of lithium extraction from ore has exceeded that of lithium extraction from brine since 2018. The reason is that the production cycle of lithium extraction from brine is long and it is easily affected by weather, resulting in slow expansion of lithium extraction from brine. In 2018, the output of lithium extraction from ore accounted for 51%, and in 2019, about 60% of lithium salt products came from lithium extraction from ore. Analysis of future new and expanded projects for lithium salt production in the world shows that the proportion of lithium extraction from ore will further increase in the future.
[0004] The technology of lithium extraction from ores is mature, mainly including sulfuric acid method, limestone sintering method, chlorination roasting method, and soda pressure cooking method. Among them, the sulfuric acid method is the main industrial production method for lithium extraction from ores at home and abroad. The sulfate method can process almost all lithium-containing ores, but the temperature of the roasting process must be strictly controlled, and the high price of potassium sulfate makes its production cost high. There are problems such as high impurity content in the leachate and large consumption of sulfuric acid; the practicality of the limestone sintering method is also very common and suitable for decomposing almost all lithium minerals, but it has the disadvantages of high energy consumption, low recovery rate and high quality requirements for lime; the chlorination roasting method has the advantages of simple process flow and lithium recovery rate of up to 90%, but it has the disadvantages of difficult collection of gaseous product LiCl produced by high-temperature chlorination; the soda pressure cooking method has more stringent requirements on production process conditions and production raw materials. The future trend of lithium extraction technology from ores is to reduce costs, reduce energy consumption, and increase lithium yield.
[0005] The limestone sintering method is to mix lithium ore with limestone and sinter them to convert lithium into lithium hydroxide, grind and soak in water to obtain lithium hydroxide leachate, remove impurities and evaporate and crystallize to obtain lithium hydroxide product, and then introduce carbon dioxide to carbonate to obtain lithium carbonate.
[0006] Taking spodumene as an example, the main reaction equation involved in the conventional production process of limestone sintering is:
[0007] Li2O·Al2O3·4SiO2+8CaCO3→Li2Al2O4+4Ca2SiO4+8CO2 (1)
[0008] 2Li(OH)+CO2→Li2CO3+H2O (2)
[0009] A major drawback of the limestone sintering method for lithium extraction is that the carbonation process of the lithium hydroxide leachate requires flue gas containing medium or high concentrations of CO2 or pure CO2 gas, and the CO2 concentration needs to be ≥40%. The higher the CO2 concentration, the higher the carbonation efficiency of the leachate. The conventional limestone sintering method uses air combustion, which results in a large amount of flue gas and a low CO2 concentration (CO2 concentration is about 10-20%), which cannot meet the needs of the leachate carbonation process. Therefore, a large amount of pure CO2 gas needs to be purchased, resulting in a significant increase in production costs; at the same time, a large amount of flue gas containing CO2 is discharged, resulting in a significant increase in carbon emission reduction pressure.
[0010] Based on the above background, without purchasing additional pure CO2 gas, the research optimizes and improves the existing limestone sintering process so that the sintering system can produce lithium-based compounds normally while preparing the flue gas containing medium and high concentrations of CO2 required for the carbonation process, and further reduce the system's CO2 emissions, thereby preparing lithium carbonate with higher efficiency and lower cost. This will become the key to the large-scale preparation of lithium carbonate by limestone sintering.
[0011] Therefore, based on market demand and the key scientific and technological challenges faced, a method and system for extracting lithium from lithium ore with zero CO2 emissions is provided, which fully considers the demand for medium and high concentrations of CO2 for carbonation of the leaching solution in the lithium carbonate preparation process, and at the same time solves the problems of high energy consumption, low leaching rate and large carbon emissions in the lithium ore extraction system, so that the entire production system has low energy consumption and low cost, and realizes zero CO2 emissions, carbon utilization and waste heat utilization functions, which has important practical significance. Summary of the invention
[0012] In order to solve the problems existing in the prior art, the present invention provides a method and system for extracting lithium from lithium ore with zero CO2 emissions. The present invention solves the technical problems that the CO2 concentration in the flue gas of the existing limestone sintering method is relatively low, resulting in the inability to utilize carbon in the subsequent carbonation process of the leaching solution, which leads to a significant increase in production costs, and the high energy consumption of the entire system, which leads to a significant increase in the pressure of carbon emission reduction, and achieves zero CO2 emissions.
[0013] The present invention is achieved by: a method for extracting lithium from lithium ore with zero CO2 emission, comprising the following steps:
[0014] Raw material preparation:
[0015] Lithium ore and limestone are mixed in a certain proportion, and the mixed raw materials are ground to prepare raw material powder with particle size meeting the requirements;
[0016] Clinker preparation and high CO2 concentration flue gas preparation:
[0017] The raw meal powder is fed into the CO2 concentration preheating and predecomposition system and the energy-saving preheating system of different equipment specifications at a predetermined feeding ratio, and then all enters the decomposition furnace of the CO2 concentration preheating and predecomposition system for calcination and decomposition through the corresponding multi-stage cyclone preheater of the two systems; the hot raw meal after decomposition all enters the rotary kiln through the kiln tail smoke chamber for calcination, and high-temperature kiln gas and high-temperature lithium-based compound clinker are generated in the rotary kiln, and the high-temperature lithium-based compound clinker is cooled by a cooler to obtain a lithium-based clinker product;
[0018] High-purity O2 and high-temperature kiln gas enter the decomposition furnace of the CO2 concentration, preheating and predecomposition system. The flue gas generated in the decomposition furnace enters the multi-stage cyclone preheater of the CO2 concentration, preheating and predecomposition system to exchange heat with the raw material to become low-temperature and high-CO2 concentration flue gas. This low-temperature and high-CO2 concentration flue gas is discharged through the air outlet of the cyclone separator at the top of the multi-stage cyclone preheater of the CO2 concentration, preheating and predecomposition system. The temperature range of the low-temperature and high-CO2 concentration flue gas is 200-350°C, and the wet-base CO2 concentration of the low-temperature and high-CO2 concentration flue gas is 40-60%, the O2 concentration is 2-4%, the N2 concentration is 18-40%, and the H2O concentration is 8-20%;
[0019] The high-temperature tertiary air enters the multi-stage cyclone preheater of the energy-saving preheating system, exchanges heat with the raw material to become low-temperature flue gas, which is discharged through the air outlet of the cyclone separator at the top of the multi-stage cyclone preheater of the energy-saving preheating system. The temperature range of this low-temperature flue gas is 240-450℃, and the CO2 concentration in this low-temperature flue gas is zero;
[0020] Clinker Carbonation:
[0021] The lithium-based clinker product is ground and then immersed in water and filtered to obtain lithium hydroxide leachate and waste residue. The lithium hydroxide leachate is evaporated and concentrated and then carbonated. During the carbonation, the lithium hydroxide leachate fully reacts with the high CO2 concentration gas produced by the CO2 concentration, preheating and predecomposition system, and then evaporated, separated and crystallized to obtain a lithium carbonate product.
[0022] In the above technical solution, preferably, the raw meal powder feeding ratio of the CO2 concentration preheating and predecomposition system to the energy-saving preheating system is 1:1 to 1:8.
[0023] In the above technical solution, preferably, the O2 concentration in the high-purity O2 is 50-99%.
[0024] In the above technical solution, preferably, the low-temperature flue gas discharged from the outlet of the energy-saving preheating system recovers part of the heat through the waste heat recovery system and then enters the flue gas treatment system, and after the flue gas treatment, enters the chimney and is discharged into the atmosphere.
[0025] A lithium ore extraction system with zero CO2 emission, comprising a CO2 concentration preheating and predecomposition system, an energy-saving preheating system, a kiln tail smoke chamber, a rotary kiln, a cooler, a tertiary air duct and a leachate carbonation system;
[0026] The CO2 concentration, preheating and predecomposition system comprises a decomposition furnace and a first row of cyclone preheaters; a burner is arranged on the decomposition furnace, the bottom of the decomposition furnace is connected to a high-purity oxygen inlet, the bottom of the decomposition furnace is communicated with the kiln tail smoke chamber, and a raw material inlet is provided on the decomposition furnace; the air inlet of the cyclone separator at the bottom end of the first row of cyclone preheaters is connected to the air outlet pipe of the decomposition furnace, and the air outlet of the cyclone separator at the top end of the first row of cyclone preheaters discharges low-temperature and high CO2 concentration flue gas; the feed inlet of the cyclone separator at the top end of the first row of cyclone preheaters is used for feeding raw material powder, the discharge port of the second-to-last cyclone separator of the first row of cyclone preheaters is connected to the decomposition furnace, and the discharge port of the cyclone separator at the bottom end of the first row of cyclone preheaters is communicated with the kiln tail smoke chamber;
[0027] The energy-saving preheating system comprises a second row of cyclone preheaters, the tertiary air duct is connected to the cooler and the air inlet of the cyclone separator at the bottom end of the second row of cyclone preheaters, the air outlet of the cyclone separator at the top end of the second row of cyclone preheaters discharges low-temperature flue gas, and the CO2 concentration in the low-temperature flue gas is zero; the feed inlet of the cyclone separator at the top end of the second row of cyclone preheaters is used for raw material feeding, and the discharge port of the cyclone separator at the bottom end of the second row of cyclone preheaters is connected to the decomposition furnace;
[0028] The kiln tail smoke chamber, rotary kiln and cooler are connected in sequence; the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the leaching liquid carbonation system, and the clinker outlet of the cooler is connected to the feed inlet of the leaching liquid carbonation system.
[0029] In the above technical scheme, preferably, the leachate carbonation system includes a water immersion and filtration device, an evaporation and concentration device and a carbonation device, the lithium-based clinker outlet of the cooler is connected to the feed inlet of the water immersion and filtration device, the leachate outlet of the water immersion and filtration device is connected to the liquid inlet of the evaporation and concentration device, the liquid outlet of the evaporation and concentration device is connected to the liquid inlet of the carbonation device, and the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the carbonation device.
[0030] In the above technical scheme, it is further preferred that the leachate carbonation system also includes a grinding system, which is located between the cooler and the water immersion and filtering device, the lithium-based clinker outlet of the cooler is connected to the material inlet of the grinding system, and the material outlet of the grinding system is connected to the feed inlet of the water immersion and filtering device.
[0031] In the above technical solution, preferably, the raw material inlet is provided in plurality.
[0032] In the above technical solution, preferably, the number of stages of the first row of cyclone preheaters is 5 to 7; the number of stages of the second row of cyclone preheaters is 5 to 7.
[0033] The principle of the present invention is:
[0034] The main disadvantage of the conventional limestone sintering method is that the carbonation process of the leachate requires the provision of flue gas or pure CO2 gas containing medium or high concentrations of CO2 (CO2 concentration ≥ 40%, and the higher the CO2 concentration, the higher the carbonation efficiency of the leachate), while the conventional limestone sintering method uses conventional air as the combustion medium, resulting in a large amount of flue gas at the outlet of the preheating and predecomposition system and a low CO2 concentration (CO2 wet basis concentration is about 10-20%), which cannot meet the carbonation requirements of the leachate, and thus requires the provision of flue gas containing medium or high concentrations of CO2 or the purchase of pure CO2 gas, resulting in a significant increase in production costs; at the same time, a large amount of flue gas containing CO2 is discharged from the preheating and predecomposition system, resulting in a significant increase in the pressure to reduce carbon emissions.
[0035] According to the main reaction equations involved in the limestone sintering production process, it can be seen that, in theory, 1 mol of spodumene needs to react with 8 mol of limestone to generate 8 mol of CO2, while 2 mol of lithium hydroxide only requires 1 mol of CO2 to prepare lithium carbonate products. Considering that the lithium component in lithium hydroxide all comes from spodumene, that is, in the limestone roasting process, theoretically, 1 mol of spodumene can produce 8 mol of CO2, but only 1 mol of CO2 is needed to prepare lithium carbonate products.
[0036] Based on the above analysis, the present invention is designed as two preheating systems with different specifications. Among them, the high-temperature tertiary air from the cooler enters the energy-saving preheating system to preheat the raw material. The energy-saving preheating system does not produce CO2 gas, and the outlet of the preheater in this column achieves zero CO2 emission. The raw materials from the energy-saving preheating system and the CO2 concentration preheating system are calcined and decomposed in the decomposition furnace of the CO2 concentration system after sufficient gas-solid heat exchange. The decomposition furnace of the CO2 concentration system uses high-purity O2 and high-temperature flue gas from the kiln tail smoke chamber to mix and assist combustion. Since all fuels and calcium carbonate decompose to produce CO2, the CO2 concentration in the low-temperature flue gas discharged from the outlet of the top cyclone separator of the CO2 concentration system is significantly increased, and at the same time, the flue gas required by the leaching solution carbonation system is generated (the CO2 concentration and the total amount of CO2 in the flue gas meet the needs of the carbonation link), and the CO2 concentration preheating and predecomposition system can be designed with the most economical oxygen production capacity to reduce the oxygen production cost.
[0037] The present invention rationally designs the CO2 concentration, preheating and predecomposition system to ensure that the CO2 content in the flue gas entering the leaching liquid carbonation system at the outlet of the CO2 concentration, preheating and predecomposition system just meets the leaching liquid carbonation demand, and realizes the carbon utilization of the CO2 concentration system on the basis of ensuring the carbonation efficiency of the leaching liquid carbonation system and the lithium carbonate output of the system.
[0038] The advantages and positive effects of the present invention are:
[0039] 1. The present invention fully considers the technical characteristics that the CO2 concentration of the flue gas at the outlet of the preheater in the conventional rotary kiln production process is low, which leads to low CO2 concentration in the flue gas and inability to utilize carbon in subsequent carbonation. The CO2 concentration of the flue gas at the outlet of the CO2 concentration preheating and predecomposition system is significantly increased from 10-20% (wet basis) to more than 40% (wet basis), so that the CO2 flue gas generated by the system itself can be used in the subsequent carbonation link, thereby achieving the purpose of carbon utilization and reducing production costs.
[0040] 2. Based on the reaction equation of spodumene and limestone and the amount of carbon dioxide required for carbonation, the present invention is designed as two systems with different specifications. Among them, the raw material of the energy-saving preheating system is preheated with high-temperature tertiary air from the cooler. The energy-saving preheating system does not produce CO2 gas and has zero CO2 emissions.
[0041] 3. The present invention feeds the raw materials from the energy-saving preheating system and the CO2 concentration, preheating and predecomposition system into the decomposition furnace of the CO2 concentration, preheating and predecomposition system for calcination and decomposition after sufficient gas-solid heat exchange. The decomposition furnace of the CO2 concentration, preheating and predecomposition system adopts high-purity O2 and high-temperature flue gas from the kiln tail smoke chamber to assist combustion. Since all fuels and calcium carbonate decompose to produce CO2, the CO2 concentration in the low-temperature flue gas discharged from the outlet of the top cyclone separator of the CO2 concentration, preheating and predecomposition system is significantly increased, and at the same time, the flue gas required by the carbonation system of the leaching solution is generated (the CO2 concentration and the total amount of CO2 in the flue gas both meet the needs of the carbonation link), and the CO2 concentration, preheating and predecomposition system can be designed with the most economical oxygen production capacity to reduce the oxygen production cost.
[0042] 4. The cyclone preheater outlet temperature of the entire system of the present invention is low, the air volume is small, the system energy consumption is low, and the flue gas at the outlet of the energy-saving preheating system can be used as waste heat to reduce the energy loss of the entire production line.
[0043] 5. The limestone sintering system provided by the present invention does not require redesign of key sintering equipment such as rotary kiln, cooler and kiln head burner, which greatly simplifies the process flow and reduces the transformation cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0045] Figure 1 This is a process flow chart of extracting lithium from lithium ore with zero CO2 emission according to an embodiment of the present invention;
[0046] Figure 2 This is a flow chart of a sintering system for extracting lithium from lithium ore with zero CO2 emissions according to an embodiment of the present invention.
[0047] In the figure: 1. CO2 concentration, preheating and predecomposition system; 2. Energy-saving preheating system; 3. Kiln tail smoke chamber; 4. Rotary kiln; 5. Cooler; 6. Tertiary air duct. DETAILED DESCRIPTION
[0048] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solution of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0049] Example
[0050] like Figure 1 As shown, the purpose of the present invention is achieved through the following process flow, which mainly includes the following process flow:
[0051] Lithium ore and limestone are mixed in a certain proportion. The mixed raw materials are fed into the raw material grinding system for grinding to prepare raw material powder with particle size meeting the requirements.
[0052] The raw meal powder is fed into the CO2 concentration preheating and predecomposition system 1 and the energy-saving preheating system 2 of different equipment specifications at a predetermined feeding ratio, and is respectively fed into the CO2 concentration preheating and predecomposition system 1 and the energy-saving preheating system 2 for gas-solid heat exchange corresponding to the two systems, and then all enter the decomposition furnace of the CO2 concentration preheating and predecomposition system 1 for calcination and decomposition; the hot raw meal after decomposition all enters the rotary kiln 4 through the kiln tail smoke chamber 3 for calcination, and high-temperature kiln gas and high-temperature lithium-based compound clinker are generated in the rotary kiln 4, and the high-temperature lithium-based compound clinker is cooled by the cooler 5 to obtain the lithium-based clinker product;
[0053] The high-purity O2 prepared by the oxygen production equipment and the high-temperature kiln gas enter the decomposition furnace of the CO2 concentration preheating and predecomposition system 1, and the mixed flue gas contains 30-45% O2 and 55-70% N2. The high-concentration O2 causes the fuel in the decomposition furnace of the CO2 concentration preheating and predecomposition system 1 to burn and decompose the limestone to produce high-concentration CO2; the flue gas discharged from the top outlet of the CO2 concentration preheating and predecomposition system 1 is low-temperature and high-CO2 concentration flue gas, and the temperature range of the low-temperature and high-CO2 concentration flue gas is 200-350°C (depending on the number of stages of the first row of cyclone preheaters), and the wet-base CO2 concentration of the low-temperature and high-CO2 concentration flue gas is 40-60%, the O2 concentration is 2-4%, the N2 concentration is 18-40%, and the H2O concentration is 8-20%;
[0054] The high-temperature tertiary air enters the multi-stage cyclone preheater of the energy-saving preheating system 2, exchanges heat with the raw material to become low-temperature flue gas, and the low-temperature flue gas is discharged through the air outlet of the cyclone separator at the top of the multi-stage cyclone preheater of the energy-saving preheating system 2. The temperature range of this low-temperature flue gas is 240-450°C, the CO2 concentration in this low-temperature flue gas is zero, and there is no carbon dioxide emission; this low-temperature flue gas enters the flue gas treatment system after part of the heat is recovered by the waste heat recovery system, and after the flue gas treatment, it enters the chimney and is discharged into the atmosphere.
[0055] After the lithium-based clinker product is ground by the grinding system, it enters the water immersion and filtration device for water immersion and filtration to obtain lithium hydroxide leachate and waste residue. The lithium hydroxide leachate is evaporated and concentrated and then enters the carbonation device for carbonation. During carbonation, the lithium hydroxide leachate fully reacts with the high CO2 concentration gas generated by the CO2 concentration, preheating and predecomposition system 1, and then undergoes multiple processes such as evaporation, separation, and crystallization to obtain a lithium carbonate product.
[0056] In the embodiment, taking spodumene ore as an example, the specifications of two different CO2 concentration preheating and predecomposition systems 1 and energy-saving preheating systems 2 of the present invention are described, which are determined by the following steps:
[0057] Based on the reaction equations (1) and (2) involved in the limestone roasting production process, the molar ratio of lithium-based compounds Li2Al2O4 to CO2 is 1:8, the molar ratio of lithium-based compounds Li2Al2O4 to Li2CO3 is 1:1, and the molar ratio of Li2CO3 to CO2 is 1:1. The production of 1 mole of Li2CO3 produces 8 moles of CO2, and carbonation requires 1 mole of CO2. Based on the qualitative and quantitative logical relationship of these reactions, two columns of CO2 concentration, preheating and predecomposition systems 1 and energy-saving preheating systems 2 with different specifications are considered. The raw material powder feeding ratio of the CO2 concentration, preheating and predecomposition system 1 and the energy-saving preheating system 2 is 1:1 to 1:8, and the specifications can be flexibly adjusted according to specific production needs.
[0058] Based on the carbon dioxide flow rate and concentration per unit time required for carbonation, a CO2 concentration preheating and predecomposition system 1 is designed, which is mainly responsible for the preparation of flue gas with high CO2 concentration. The high CO2 concentration flue gas comes from the CO2 produced by the decomposition of all calcium carbonate in the decomposition furnace, the rotary kiln 4 and the CO2 produced by the combustion of fuel in the decomposition furnace. The CO2 concentration in the flue gas is ≥40%. The raw material feed amount, fuel amount and required high-purity oxygen amount of this CO2 concentration preheating and predecomposition system 1 are inferred according to the CO2 concentration and flue gas volume. According to the flue gas volume in different parts, the equipment specifications of the decomposition furnace, cyclone separator, air duct and other equipment of this CO2 concentration preheating and predecomposition system 1 are designed.
[0059] According to market demand, the design scale of lithium carbonate production line is determined. Based on the annual operation time of the production line, the lithium carbonate output per unit time is designed, the total raw material feed amount and fuel amount are determined, and a rotary kiln 4 calcination system is designed, which is mainly responsible for the preparation of lithium-based compounds. The total raw material powder feed amount minus the raw material powder feed amount of CO2 concentration preheating and predecomposition system 1 is the raw material powder feed amount of energy-saving preheating system 2, and then the equipment specifications of cyclone separator and air duct of this energy-saving preheating system 2 are designed.
[0060] like Figure 2 As shown, the CO2 zero-emission lithium ore lithium extraction system provided by an embodiment of the present invention includes a CO2 concentration preheating and predecomposition system 1, an energy-saving preheating system 2, a kiln tail smoke chamber 3, a rotary kiln 4, a cooler 5, a tertiary air duct 6 and a leachate carbonation system.
[0061] The CO2 concentration, preheating and predecomposition system 1 comprises a decomposition furnace and a first row of cyclone preheaters; a burner is arranged on the decomposition furnace, a high-purity oxygen inlet is connected to the bottom of the decomposition furnace, the bottom of the decomposition furnace is connected to the kiln tail smoke chamber 3, and a raw material inlet is provided on the decomposition furnace; in order to regulate the temperature field distribution in the decomposition furnace, multiple raw material inlets can be provided, and those skilled in the art can set them according to actual needs. Figure 2 The raw material inlet shown in the figure includes a first raw material inlet and a second raw material inlet. The air inlet of the cyclone separator at the bottom end of the first row of cyclone preheaters is connected to the air outlet pipe of the decomposition furnace, and the air outlet of the cyclone separator at the top end of the first row of cyclone preheaters discharges low-temperature and high-CO2 concentration flue gas, the temperature range of the low-temperature and high-CO2 concentration flue gas is 200-350°C (depending on the number of stages of the first row of cyclone preheaters), and the wet-based CO2 concentration in the low-temperature and high-CO2 concentration flue gas is ≥40%; the feed inlet of the cyclone separator at the top end of the first row of cyclone preheaters is used for feeding raw material powder, the discharge port of the second-to-last cyclone separator of the first row of cyclone preheaters is connected to the decomposition furnace, and the discharge port of the cyclone separator at the bottom end of the first row of cyclone preheaters is connected to the kiln tail smoke chamber 3.
[0062] The energy-saving preheating system 2 includes a second row of cyclone preheaters, the tertiary air duct 6 connects the cooler 5 and the air inlet of the cyclone separator at the bottom end of the second row of cyclone preheaters, and the air outlet of the cyclone separator at the top end of the second row of cyclone preheaters discharges low-temperature flue gas, the temperature range of this low-temperature flue gas is 240-450°C (depending on the stage number of the second row of cyclone preheaters), and the CO2 concentration in this low-temperature flue gas is zero; the feed port of the cyclone separator at the top end of the second row of cyclone preheaters is used for raw material feeding, and the discharge port of the cyclone separator at the bottom end of the second row of cyclone preheaters is connected to the decomposition furnace.
[0063] The kiln tail smoke chamber 3, rotary kiln 4, and cooler 5 are connected in sequence; the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the leachate carbonation system, and the clinker outlet of the cooler 5 is connected to the feed inlet of the leachate carbonation system.
[0064] The number of stages of the first row of cyclone preheaters is preferably 5 to 7; the number of stages of the second row of cyclone preheaters is preferably 5 to 7.
[0065] It should be noted that the number of CO2 concentration preheating and predecomposition systems 1 and energy-saving preheating systems 2 is only for illustration, and those skilled in the art can set them according to actual needs. The cooler 5 can be a grate cooler 5, a single-cylinder cooler 5 or a multi-cylinder cooler 5, and the fan can adopt a combination of existing multiple fans.
[0066] The leachate carbonation system comprises a water immersion and filtering device, an evaporation and concentration device and a carbonation device. The lithium-based clinker outlet of the cooler 5 is connected to the feed inlet of the water immersion and filtering device, the leachate outlet of the water immersion and filtering device is connected to the liquid inlet of the evaporation and concentration device, the liquid outlet of the evaporation and concentration device is connected to the liquid inlet of the carbonation device, and the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the carbonation device.
[0067] The leachate carbonation system also includes a grinding system, which is located between the cooler 5 and the water immersion and filtering device. The lithium-based clinker outlet of the cooler 5 is connected to the material inlet of the grinding system, and the material outlet of the grinding system is connected to the feed inlet of the water immersion and filtering device.
[0068] The method for extracting lithium from lithium ore with zero CO2 emission based on the above system comprises the following steps:
[0069] Lithium ore and limestone are mixed in a certain proportion, and the mixed raw materials are ground to prepare raw material powder with particle size meeting the requirements.
[0070] The raw meal powder is fed into the first row cyclone preheater and the second row cyclone preheater at a predetermined feeding ratio, and the raw meal powder is heat exchanged and gas-solid separated with the corresponding flue gas in each cyclone preheater;
[0071] The raw meal preheated by the first row of cyclone preheaters enters the calciner, and the raw meal preheated by the second row of cyclone preheaters enters the calciner;
[0072] High-purity oxygen with a concentration of 80-99% and high-temperature kiln gas enter the decomposition furnace. High-purity O2 can improve fuel combustion efficiency and flue gas CO2 concentration. The large amount of heat released by fuel combustion is used for the raw material in the decomposition furnace to absorb heat and decompose, obtain hot raw material, and produce a large amount of flue gas. The flue gas generated in the decomposition furnace enters the first row of cyclone preheaters and exchanges heat with the raw material to become low-temperature high-CO2 concentration flue gas. The low-temperature high-CO2 concentration flue gas is discharged through the air outlet of the cyclone separator at the top of the first row of cyclone preheaters, and enters the leaching liquid carbonation system to carbonize the leaching liquid. The temperature range of this low-temperature high-CO2 concentration flue gas is 200-350℃, and the wet-base CO2 concentration in the low-temperature high-CO2 concentration flue gas is 40-60%, the O2 concentration is 2-4%, the N2 concentration is 18-40%, and the H2O concentration is 8-20%;
[0073] The high-temperature tertiary air enters the second row of cyclone preheaters and exchanges heat with the raw material to become low-temperature flue gas. The low-temperature flue gas is discharged through the outlet of the cyclone separator at the top of the second row of cyclone preheaters and the waste heat is utilized. The temperature range of this low-temperature flue gas is 240-450℃, the CO2 concentration in the low-temperature flue gas is zero, and there is no carbon dioxide emission. This low-temperature flue gas recovers part of the heat through the waste heat recovery and utilization system and enters the flue gas treatment system. After the flue gas is treated, it enters the chimney and is discharged into the atmosphere.
[0074] The hot raw material generated in the decomposition furnace enters the rotary kiln 4 through the kiln tail smoke chamber 3, and is calcined in the rotary kiln 4 to form lithium-based compound clinker. The fuel in the rotary kiln 4 is burned to generate high-temperature kiln gas. The lithium-based compound clinker enters the cooler 5 from the outlet of the rotary kiln 4 and exchanges heat with the air to obtain cooled lithium-based clinker.
[0075] The lithium-based clinker is ground and then immersed in water and filtered to obtain lithium hydroxide leachate and waste residue. The lithium hydroxide leachate is evaporated and concentrated and then carbonated. During the carbonation, the lithium hydroxide leachate fully reacts with the high CO2 concentration gas generated by the CO2 concentration, preheating and predecomposition system 1, and then evaporated, separated and crystallized to obtain a lithium carbonate product.
[0076] The above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit the same. Although the present invention has been described in detail with reference to the above embodiments, a person skilled in the art can still modify or make equivalent substitutions to the specific implementations of the present invention. Any modifications or equivalent substitutions that do not depart from the spirit and scope of the present invention are within the scope of protection of the claims of the present invention to be approved.
Claims
1. A method for extracting lithium from lithium ore with zero CO2 emission, characterized in that: The steps include: Raw material preparation: Lithium ore and limestone are mixed in a certain proportion, and the mixed raw materials are ground to prepare raw material powder with particle size meeting the requirements; Clinker preparation and high CO2 concentration flue gas preparation: The raw meal powder is fed into the CO2 concentration preheating and predecomposition system and the energy-saving preheating system of different equipment specifications at a predetermined feeding ratio, and then all enters the decomposition furnace of the CO2 concentration preheating and predecomposition system for calcination and decomposition through the corresponding multi-stage cyclone preheater of the two systems; the hot raw meal after decomposition all enters the rotary kiln through the kiln tail smoke chamber for calcination, and high-temperature kiln gas and high-temperature lithium-based compound clinker are generated in the rotary kiln, and the high-temperature lithium-based compound clinker is cooled by a cooler to obtain a lithium-based clinker product; High-purity O2 and high-temperature kiln gas enter the decomposition furnace of the CO2 concentration, preheating and predecomposition system. The flue gas generated in the decomposition furnace enters the multi-stage cyclone preheater of the CO2 concentration, preheating and predecomposition system to exchange heat with the raw material to become low-temperature and high-CO2 concentration flue gas. This low-temperature and high-CO2 concentration flue gas is discharged through the air outlet of the cyclone separator at the top of the multi-stage cyclone preheater of the CO2 concentration, preheating and predecomposition system. The temperature range of the low-temperature and high-CO2 concentration flue gas is 200-350°C, and the wet-base CO2 concentration of the low-temperature and high-CO2 concentration flue gas is 40-60%, the O2 concentration is 2-4%, the N2 concentration is 18-40%, and the H2O concentration is 8-20%; The high-temperature tertiary air enters the multi-stage cyclone preheater of the energy-saving preheating system, exchanges heat with the raw material to become low-temperature flue gas, which is discharged through the air outlet of the cyclone separator at the top of the multi-stage cyclone preheater of the energy-saving preheating system. The temperature range of this low-temperature flue gas is 240-450℃, and the CO2 concentration in this low-temperature flue gas is zero; Clinker Carbonation: The lithium-based clinker product is ground and then immersed in water and filtered to obtain lithium hydroxide leachate and waste residue. The lithium hydroxide leachate is evaporated and concentrated and then carbonated. During the carbonation, the lithium hydroxide leachate fully reacts with the high CO2 concentration gas produced by the CO2 concentration, preheating and predecomposition system, and then evaporated, separated and crystallized to obtain a lithium carbonate product.
2. The method for extracting lithium from lithium ore with zero CO2 emission according to claim 1, characterized in that: The raw meal powder feeding ratio of the CO2 concentration preheating and predecomposition system and the energy-saving preheating system is 1:1 to 1:
8.
3. The method for extracting lithium from lithium ore with zero CO2 emission according to claim 1, characterized in that: The O2 concentration in the high-purity O2 is 50-99%.
4. The method for extracting lithium from lithium ore with zero CO2 emission according to claim 1, characterized in that: The low-temperature flue gas discharged from the outlet of the energy-saving preheating system recovers part of the heat through the waste heat recovery system and then enters the flue gas treatment system. After the flue gas treatment, it enters the chimney and is discharged into the atmosphere.
5. A lithium ore extraction system with zero CO2 emission, characterized in that: It includes CO2 concentration preheating and predecomposition system, energy-saving preheating system, kiln tail smoke chamber, rotary kiln, cooler, tertiary air duct and leachate carbonation system; The CO2 concentration, preheating and predecomposition system comprises a decomposition furnace and a first row of cyclone preheaters; a burner is arranged on the decomposition furnace, the bottom of the decomposition furnace is connected to a high-purity oxygen inlet, the bottom of the decomposition furnace is communicated with the kiln tail smoke chamber, and a raw material inlet is provided on the decomposition furnace; the air inlet of the cyclone separator at the bottom end of the first row of cyclone preheaters is connected to the air outlet pipe of the decomposition furnace, and the air outlet of the cyclone separator at the top end of the first row of cyclone preheaters discharges low-temperature and high CO2 concentration flue gas; the feed inlet of the cyclone separator at the top end of the first row of cyclone preheaters is used for feeding raw material powder, the discharge port of the second-to-last cyclone separator of the first row of cyclone preheaters is connected to the decomposition furnace, and the discharge port of the cyclone separator at the bottom end of the first row of cyclone preheaters is communicated with the kiln tail smoke chamber; The energy-saving preheating system comprises a second row of cyclone preheaters, the tertiary air duct is connected to the cooler and the air inlet of the cyclone separator at the bottom end of the second row of cyclone preheaters, the air outlet of the cyclone separator at the top end of the second row of cyclone preheaters discharges low-temperature flue gas, and the CO2 concentration in the low-temperature flue gas is zero; the feed inlet of the cyclone separator at the top end of the second row of cyclone preheaters is used for raw material feeding, and the discharge port of the cyclone separator at the bottom end of the second row of cyclone preheaters is connected to the decomposition furnace; The kiln tail smoke chamber, rotary kiln and cooler are connected in sequence; the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the leaching liquid carbonation system, and the clinker outlet of the cooler is connected to the feed inlet of the leaching liquid carbonation system.
6. The CO2-free lithium ore extraction system according to claim 5, characterized in that: The leachate carbonation system comprises a water immersion and filtering device, an evaporation and concentration device and a carbonation device. The lithium-based clinker outlet of the cooler is connected to the feed inlet of the water immersion and filtering device, the leachate outlet of the water immersion and filtering device is connected to the liquid inlet of the evaporation and concentration device, the liquid outlet of the evaporation and concentration device is connected to the liquid inlet of the carbonation device, and the air outlet of the top cyclone separator of the first row of cyclone preheaters is connected to the air inlet of the carbonation device.
7. The CO2-free lithium ore extraction system according to claim 6, characterized in that: The leachate carbonation system also includes a grinding system, which is located between a cooler and a water immersion and filtering device, wherein a lithium-based clinker outlet of the cooler is connected to a material inlet of the grinding system, and a material outlet of the grinding system is connected to a feed inlet of the water immersion and filtering device.
8. The CO2-free lithium ore extraction system according to claim 5, characterized in that: The raw material inlet is arranged in plurality.
9. The CO2-free lithium ore extraction system according to claim 5, characterized in that: The number of stages of the first row of cyclone preheaters is 5 to 7; the number of stages of the second row of cyclone preheaters is 5 to 7.