Laser-induced breakdown spectroscopy quantitative analysis method for elements on inner wall surface of magnetic confinement fusion device

By optimizing the experimental parameters of laser-induced breakdown spectroscopy and establishing a pre-classification model for the components of deposited impurities in the traditional method, the problem of low quantitative analysis accuracy of the surface deposition impurities layer on the wall material in traditional methods is solved, and high-precision multi-element quantitative analysis is achieved, suitable for magnetic Research on wall materials for constrained fusion devices.

CN119000648AActive Publication Date: 2024-11-22DALIAN UNIV OF TECH

Patent Information

Application Number
CN202411244039.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-11-22
Estimated Expiration
2044-09-05

AI Technical Summary

Technical Problem

Traditional laser-induced breakdown spectroscopy method cannot achieve high-precision quantitative analysis of impurity layer components on the surface of wall materials in magnetically constrained fusion devices, especially under the conditions of complex interaction between plasma and wall materials and variable elements, resulting in The quantitative analysis accuracy is poor and cannot meet the needs of high-parameter operation.

Method used

By optimizing the experimental parameters of laser-induced breakdown spectral, a pre-classification model of the components of deposited impurities and a characteristic spectrum line spectral correction factor database is established to realize local thermodynamic equilibrium and chemical dose ablation of laser ablation plasma, using three-dimensional spatial scanning and multivariate statistics The learning method is used to classify matrix attributes and modify spectral spectral to improve the accuracy of quantitative analysis.

Benefits of technology

The composition of impurity film deposited on the surface of wall materials is achieved remotely and online quantitatively measured in high vacuum and strong magnetic field environments, improving the quantitative accuracy of LIBS technology under extreme conditions, and can synchronously analyze the content of multiple elements, which has important scientific research and technology. Promotional value.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119000648A_ABST
    Figure CN119000648A_ABST
Patent Text Reader

Abstract

The invention discloses a laser-induced breakdown spectroscopy quantitative analysis method for elements on the inner wall surface of a magnetic confinement fusion device, and belongs to the technical field of laser spectrum analysis. According to the method, based on laser-induced breakdown spectroscopy data of an impurity layer on the surface of a wall material, according to a relation of spectral line intensity of each element in characteristic spectrum data, a matrix attribute of a to-be-detected impurity layer is pre-judged through a deposited impurity film component pre-classification model; selecting a spectrum standard sample similar to a to-be-detected sample matrix according to matrix attributes, performing single-standard-sample correction spectrum calculation, correcting a characteristic spectral line error, and then performing quantitative analysis; the device can carry out large-range and high-resolution quantitative measurement on the contents of corrosion redeposition impurities, a wall treatment coating layer, retention fuel, other impurity elements and the like of the wall material of the magnetic confinement device. According to the method, rich information of the component structure of the impurity layer deposited on the wall surface is provided, and an important basis can be provided for operation fuel injection, wall treatment maintenance, high-parameter plasma control and the like of the magnetic confinement fusion device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of laser spectrum analysis, and in particular relates to a method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectrum. Background Art

[0002] Magnetic confinement nuclear fusion is currently the most likely way to achieve controlled thermonuclear fusion. Research is being conducted at home and abroad on the long pulse and high parameter operation of magnetic confinement fusion devices. During the high parameter operation of magnetic confinement fusion devices, the interaction between plasma and wall materials will affect the service life of key materials such as divertor target plates and first walls. At the same time, the high-quality ordinal metal impurities (such as tungsten) produced will contaminate the core plasma, cause plasma rupture, and affect the stable operation of the device. The development of quantitative online analysis technology for wall surface components is crucial for a deep understanding of the interaction mechanism between plasma and wall materials and the development of effective control methods. Laser-induced breakdown spectroscopy (LIBS) has the advantages of in-situ, online, real-time, and all-element synchronous analysis. It is a very potential in-situ diagnostic technology for wall materials of magnetic confinement fusion devices. It mainly generates laser-induced plasma by ablating the sample surface with high-energy laser pulses, and calculates the content information of each element based on the plasma emission spectrum. The traditional external standard method is limited by the difficulty of online measurement of batch standard samples and cannot achieve accurate quantitative analysis. The traditional calibration-free laser induced breakdown spectroscopy (CF-LIBS) method collects the spectrum of laser ablation plasma in a local thermal equilibrium state, establishes a Boltzmann slope diagram based on the intensity of the characteristic line of the laser ablation plasma and the plasma parameters (plasma electron density and temperature), calculates the relative proportion of each element according to the intercept of the distribution fitting line of the characteristic spectrum data points of each species, and finds the content of each element. However, it is found in practice that the traditional CF-LIBS method has poor quantitative analysis accuracy due to the differences in the response efficiency of the plasma emission spectrum optical collection system in different bands, the errors caused by spectral parameters and self-absorption, and cannot meet the needs of accurate quantitative analysis of the elements of the wall surface deposition layer under vacuum and far field conditions. The one-point calibration LIBS (OPC-LIBS) method is based on the CF-LIBS method, and corrects the calculation error of CF-LIBS by using a single block of spectral standards with known components that are consistent or similar to the matrix of the sample to be tested. The principle is to compare the actual value of each element content of the reference spectral standard with the predicted value of each content by CF-LIBS, and calculate the correction coefficient of each element characteristic spectrum through the difference between the predicted value and the actual value. Under the premise of consistent matrix, this correction coefficient can comprehensively correct the errors caused by the optical collection system, spectral parameters, and self-absorption. However, in the actual application of OPC-LIBS, it is not necessarily true that the matrix of the selected spectral standard is the same or similar to that of the sample to be tested.For example, when the content of the elements in the sample to be tested varies widely, it is impossible to find a spectral standard that is suitable for all samples. The experimental results show that the quantitative accuracy of OPC-LIBS varies with the content of each element. The greater the difference with the spectral standard, the greater the error of its quantitative analysis. According to the wall material, structure and operating parameters of the magnetic confinement fusion device, the components of the impurity layer deposited on the wall surface during its operation mainly come from the wall treatment coating elements (boron, lithium, etc.), wall material deposited impurity elements (tungsten, molybdenum, carbon, iron, etc.) and retained fuel (deuterium, tritium) and reaction products (helium). During the LIBS quantitative analysis process, the difference in the impurity composition of the wall material deposition layer makes the external standard method, CF-LIBS and OPC-LIBS unable to meet the needs of accurate quantitative analysis of multiple elements in a large range. CF-LIBS has poor accuracy. The premise for the application of both the external standard method and the OPC-LIBS model is to meet the consistency of the analysis of the impurity layer matrix (physical and chemical properties of the material). However, during the operation of magnetic confinement fusion, the interaction between plasma and wall materials is extremely complex. The components of the deposited migration impurities are complex and changeable under different discharge types, parameters and spatial positions, but the types of elements they contain are relatively fixed. For example, in the full superconducting tokamak nuclear fusion experimental device (EAST), there are huge differences in the deposited impurities at different positions in the divertor area. The tungsten divertor target plate at the impact point is severely ablated, and the tungsten content of the nearby sedimentary layer is relatively large. The transport impurity deposition in the dome area is relatively serious, and the content of wall treatment elements such as boron and lithium is relatively large. In the process of using the same nanosecond laser pulse to ablate the impurity layer, there are significant differences in the ablation quality, plasma size, plasma temperature, density and other parameters of the deposition layer with tungsten as the main component and boron as the main component. The influence of this matrix effect will cause a large impact on the quantitative analysis of the emission light of the laser-induced plasma. The traditional external standard method, CF-LIBS and OPC-LIBS cannot meet the needs of high-precision quantitative measurement under the condition of a wide range of element content changes. Therefore, it is urgent to further develop high-precision LIBS quantitative analysis methods. Summary of the invention

[0003] The purpose of the present invention is to propose an in-situ, online, rapid and high-precision quantitative analysis method for the component content of the impurity layer deposited on the surface of the wall material during the operation of the reactor inner wall material of the magnetic confinement fusion device and the future magnetic confinement nuclear fusion power station.

[0004] The technical solution adopted by the present invention to achieve the above-mentioned purpose is:

[0005] A method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy, comprising:

[0006] Step 1: Optimize the experimental parameters of laser-induced breakdown spectroscopy in vacuum and strong magnetic field environment

[0007] In view of the high vacuum and strong magnetic field environment inside the vacuum chamber of the magnetic confinement focusing device, the optimization parameter adjustment of the LIBS experiment is carried out, including: adjusting the energy density of the incident laser so that the laser ablates the impurity film and the generated plasma belongs to chemical dose ablation. All elements in the impurity film are effectively excited, and the luminescent elements in the laser ablation plasma are consistent with the elements in the impurity film; adjusting the gate delay and gate width time of the spectrometer so that the laser ablation plasma is in a local thermodynamic equilibrium state.

[0008] Based on the optimization of the laser energy density and the spectrometer acquisition time, the type of characteristic spectrum of the laser ablation plasma radiation is consistent with the type of elements in the impurity film, the intensity of the characteristic spectral line is related to the element content of the film, and the intensity of a series of characteristic spectra generated by the transition process between different energy levels of each element satisfies the Boltzmann distribution law.

[0009] Step 2: Establish a pre-classification model for deposited impurity film composition

[0010] During the operation of the magnetic confinement fusion device, the impurity film deposited on the surface of the wall material mainly comes from the erosion, transport and redeposition of the wall material (tungsten, molybdenum, carbon, iron, etc.), as well as the coating elements (boron, lithium, etc.) used in the wall treatment process and their erosion, transport and redeposition. For different positions of the magnetic confinement device and different fusion plasma operating conditions, the deposited impurity film on the surface of the wall material will be complex and changeable, but it is mainly a combination of these two types of elements. Collect real impurity deposited film samples or prepare simulated samples in the laboratory. Due to the difference in the matrix, the impurity films composed of different contents of multiple elements have huge differences in the absorption of laser, heat conduction, plasma generation, and the interaction process between plasma and laser during the interaction between the pulsed laser and the impurity film, which affects the subsequent quantitative division of characteristic spectra. Therefore, by classifying the components of the impurity film, the difference in this matrix effect is quantified. After classification, the difference in matrix effect within each category subset can be ignored, and it is considered to be approximately the same matrix.

[0011] The deposited impurity film composition pre-classification model classifies the matrix properties of the sample based on the LIBS characteristic spectrum analysis of the impurity film, and each classification is used as a subset of the same matrix of the co-deposited film.

[0012] Step 3: Establish a database of spectral correction factors for characteristic spectral lines of each element

[0013] In each co-deposited thin film homologous substrate subset, standard thin film samples are selected and LIBS characteristic spectra of each standard thin film sample are collected; based on the LIBS characteristic spectra, a characteristic spectral line spectrum correction factor database is obtained through a single standard sample correction model.

[0014] Step 4: LIBS online measurement of magnetic confinement fusion device

[0015] Based on the optimized parameter conditions, the LIBS characteristic spectrum of the impurity deposition layer is collected by the LIBS online measurement system; the matrix property of the co-deposited film is judged by the deposited impurity film component pre-classification model; the corresponding characteristic spectrum correction coefficient in the characteristic spectrum correction factor database is read according to the matrix property; the characteristic spectrum line in the online LIBS spectrum is multiplied by the correction coefficient and then CF-LIBS calculation is performed to obtain the LIBS quantitative analysis result.

[0016] Step 5: Quantitative analysis of the three-dimensional distribution of the impurity layer components deposited on the wall material surface

[0017] The LIBS online measurement system is used to scan in three-dimensional space to collect LIBS characteristic spectra at different points of the wall material; the matrix properties are judged according to the deposited impurity film component pre-classification model and the corresponding characteristic spectrum correction coefficients are selected from the characteristic spectrum correction factor database based on the matrix properties; and the CF-LIBS calculation is then performed to obtain the content value of the elements contained at each point, and the spatial distribution relationship of each element is reconstructed.

[0018] Furthermore, in step 1, a nanosecond laser pulse with a wavelength of 1064 nm is used, and the energy density when irradiating the surface of the impurity film is higher than 5 J / cm 2 .

[0019] Furthermore, in step 1, the gate delay time and gate width time of the spectrometer are 100-200ns and 100-200ns, respectively.

[0020] Furthermore, in step 2, the pre-classification model of the deposited impurity film composition is established as follows:

[0021] Step 2.1: Collect or prepare several impurity film samples;

[0022] Step 2.2: Measure the content of each element in all impurity film samples by SIMS, ICP-MS and other detection methods;

[0023] Step 2.3: Based on the measured content of each element in the impurity film sample, the impurity film layer samples are classified as follows: 1) Samples with only one element content greater than 60% are classified as "unit-based" samples, and are subdivided into tungsten-based, molybdenum-based, boron-based, lithium-based and other sample categories according to the main elements; 2) Samples with two elements with a content greater than 40% at the same time are classified as "binary-based" samples, and are subdivided into tungsten-molybdenum-based, tungsten-boron-based, molybdenum-lithium-based and other sample categories according to the types of the two main elements; 3) Samples with three elements with a content greater than 30% at the same time are classified as "ternary-based" samples, and are subdivided into tungsten-molybdenum-boron-based, tungsten-iron-lithium-based and other sample categories according to the types of the three main elements; each type of impurity film layer sample is respectively regarded as a subset of the same matrix of the co-deposited film;

[0024] Step 2.4: Collect LIBS spectra of all impurity film samples;

[0025] Step 2.5: According to the intensity of the characteristic spectral lines of each element in the LIBS spectrum, establish the relationship between the content ratio of the elements and the intensity ratio of the characteristic spectral lines of the corresponding elements in the LIBS spectrum; specifically, the intensity of the characteristic spectral lines of the main elements in the impurity film sample composed of n elements is ratioed with the intensity of the characteristic spectral lines of the remaining elements, and the ratio should be within an interval M n Inside, M n It is an n-dimensional array, and the array is used as a dividing boundary to indicate whether each value is an upper limit or a lower limit. In the future analysis of unknown thin film samples, based on the characteristic spectrum data, the characteristic spectral line ratio relationship between these deposited impurity elements is solved respectively, the attribution of the main elements is analyzed, and the classification of the impurity film is confirmed.

[0026] Furthermore, in step 2, the method for establishing a pre-classification model of the deposited impurity film composition also includes multivariate statistical methods and artificial intelligence algorithms; wherein the multivariate statistical method can perform classification modeling according to models such as PCA and PLS, and by inputting spectral data and establishing a mapping relationship between classification features based on the intensity information of the characteristic spectrum, a judgment value of the matrix properties of the impurity film is given.

[0027] Furthermore, in step 3, the specific process of establishing the database of spectral correction factors of characteristic spectral lines of each element is as follows:

[0028] Step 3.1: Select a standard film sample from each co-deposited film substrate subset, and set the parameters of the laser and spectrometer of the LIBS online measurement system to be consistent with the optimized parameters set in step 1 under the 1:1 simulated fusion device operating vacuum, strong magnetic field, and optical path conditions, so that the LIBS analysis process meets the chemical dose ablation and local thermal equilibrium conditions, and then measure the LIBS characteristic spectrum of each standard film sample.

[0029] Step 3.2: The Thomson scattering method is used to measure the plasma temperature generated by laser ablation of a standard thin film sample under LIBS optimized experimental conditions. The inverse of the plasma temperature is used as a reference value for the slope fitting of the subsequent Boltzmann distribution diagram to correct the deviation of the plasma temperature calculated by the traditional Boltzmann and Saha-Boltzmann methods and improve the accuracy of the composition calculation.

[0030] Step 3.3: Perform CF-LIBS quantitative analysis and calculation on the characteristic spectra of each standard film sample collected, and compare the calculated results with the content values ​​of each element of the corresponding standard film sample to find the deviation between the calculated value and the theoretical value; calculate the intercept of the linear distribution of the characteristic spectrum data points of each element in the Boltzmann slope diagram by the true content, and perform regression correction with reference to the calculated value of the true content in the Boltzmann slope diagram to obtain the correction coefficients of the characteristic spectra of all elements for the same matrix subset of the co-deposited film. The correction coefficients of the characteristic spectra of all elements for the same matrix subset of each co-deposited film together constitute the characteristic spectrum correction factor database. The correction coefficient is the corresponding spectral correction coefficient of the LIBS analysis of the same matrix subset of each deposited film, which has comprehensively corrected the optical instrument parameters, spectroscopy parameters and the self-absorption coefficient of the characteristic spectrum in each matrix.

[0031] Furthermore, in step 3, the selection criteria for the standard film samples are samples whose content values ​​of each component in the corresponding co-deposited film and matrix subset are in the middle of the corresponding range.

[0032] Beneficial effects of the present invention: The method described in the present invention can achieve remote online quantitative measurement of the composition of co-deposited impurity films (thickness of tens of nanometers and above) under extreme measurement conditions such as high vacuum and strong magnetic field, and synchronously quantitatively analyze the content of elements such as tungsten, molybdenum, iron, carbon, boron, lithium, deuterium, tritium, helium, etc. in the impurity films; it can perform large-scale spatial and high-resolution quantitative measurement of impurity films deposited on the surface of wall materials, which is of great significance to the research on magnetic confinement fusion, and also has important reference significance for online measurement work in other fields. The present invention proposes the idea and method of impurity film matrix classification for the first time. By pre-classifying the samples to be tested and establishing correction factors for factors such as optical system, spectral parameters and self-absorption under the same matrix conditions, the quantitative accuracy of LIBS under extreme conditions can be significantly improved, which is of great value and significance to the promotion of LIBS technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 It is a flow chart of the screening type single standard sample corrected laser induced breakdown spectroscopy quantitative analysis method according to an embodiment of the present invention.

[0034] Figure 2 1 is a relationship diagram between the spectral line ratio and the element content ratio of the embodiment of the present invention.

[0035] Figure 3 1 and 2 are Boltzmann slope diagrams of the spectral standard thin film samples according to the embodiments of the present invention; wherein (a) is CF-LIBS and (b) is OPC-LIBS.

[0036] Figure 4The quantitative analysis results of the embodiments of the present invention using traditional CF-LIBS, OPC-LIBS and COPC-LIBS (method of the present invention) are compared. DETAILED DESCRIPTION

[0037] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the specific implementation modes of the present invention will be described in detail below with reference to the accompanying drawings.

[0038] like Figure 1 As shown, an embodiment of the present invention provides a method for quantitatively analyzing the elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy, comprising the following steps:

[0039] Step 1) Setting the instrument parameters of the LIBS measurement system, where the laser output energy is higher than 5 J / cm 2 The gate delay time and gate width time of the spectrometer are 100ns and 200ns, respectively, which ensure that the pulse laser ablation of the impurity film is stoichiometric ablation. At the time of spectrum acquisition, the laser ablation plasma is in a local thermal equilibrium state of high temperature and high density.

[0040] Step 2) At the time of spectrum acquisition, the temperature and density of the plasma generated by the ablation of the impurity film are synchronously measured by a Thomson scattering spectrometer.

[0041] Step 3) Collect or prepare impurity film samples composed of multiple elements such as tungsten, molybdenum, boron, lithium, and iron, and quantitatively analyze the content of each element in the impurity film samples by inductively coupled plasma mass spectrometry or spectroscopy technology; perform LIBS measurement of the impurity film samples under vacuum and magnetic field conditions, and store spectral data.

[0042] Step 4) By using the ratio of the characteristic spectral line intensities, an interval array is established to divide the different substrates of the co-deposited thin film. Figure 2 As shown in the figure, the co-deposited impurity deposited film with molybdenum and tungsten as the main elements, the ratio of the characteristic spectral lines of molybdenum and tungsten elements is compared, and the characteristic spectral line intensity ratio is divided into three sections: <0.6, >0.6 and <1.75, and >1.75, corresponding to tungsten-based samples, tungsten-molybdenum-based samples, and molybdenum-based samples, respectively. The molybdenum-tungsten characteristic peak ratio of the unknown sample can be measured to distinguish the category of the sample. In actual operation, the LIBS characteristic spectral line intensity ratio between each element should be considered according to the type and number of elements included, and the sample types should be divided in the form of an array.

[0043] Step 5) Select samples with tungsten and molybdenum contents in the middle of the distribution range in the three sub-intervals as spectral standard film samples for the single standard correction model, and determine the true content of each element by inductively coupled plasma mass spectrometry or spectroscopy. Figure 3 As shown, this figure is only for the convenience of display, and the molybdenum-tungsten ratio relationship is selected. Figure 3 (a) is the Boltzmann slope diagram of the CF-LIBS quantitative analysis of the standard thin film sample. Each element has a corresponding spectral data distribution scatter diagram. The relative content of each element is obtained based on the intercept of the fitting straight line. Figure 3 (b) is the Boltzmann slope diagram of the OPC-LIBS quantitative analysis of the spectral standard film sample. Its slope can be given as a reference by referring to the plasma temperature measured by Thomson spectroscopy technology, and the intercept can be calculated based on the actual content of each element. In this figure, the characteristic spectral data points of each element are in an ideal linear distribution state. Figure 3 The data point in (a) moves to Figure 3 The spectral intensity correction factor can be calculated by using the coordinate position of (b). This correction factor can comprehensively correct the errors caused by the optical collection system, spectral parameters, and self-absorption, greatly improving the quantitative accuracy.

[0044] Step 6) Reference Figure 2 Three subsets of the spectral standard film samples are selected respectively to establish three sets of characteristic spectral coefficients.

[0045] Step 7) In the online LIBS experiment of the magnetic confinement fusion device, the laser and spectrometer are operated under the optimal experimental conditions (laser energy density 5J / cm 2 The spectrometer gate delay is 100ns, the gate width is 200ns, and the collected LIBS spectra are used to determine the ratio of the characteristic spectral intensities of each element and to clarify the ratio relationship between the molybdenum and tungsten contents. Based on the classification criteria, the matrix properties are classified.

[0046] Based on the matrix property classification, the corresponding characteristic spectrum correction coefficient is read, the spectral data to be analyzed is corrected for spectral line intensity, and then CF-LIBS calculation is performed to obtain high-precision quantitative analysis results. Figure 4 The online LIBS quantitative analysis accuracy under the condition of large-scale variation of tungsten (10% to 92%) and molybdenum (2% to 71%) elements is given. The absolute error of the quantitative analysis of tungsten content measured by different methods is 13.07% for the traditional CF-LIBS quantitative analysis and 9.66% for OPC-LIBS. The absolute error of the spectrum calculation method proposed by the present invention, which selects spectral standards similar to the matrix of the sample to be tested according to attribute classification and corrects the spectrum by a single standard sample, is only 4.34%, which greatly improves the quantitative accuracy of online LIBS measurement of magnetic confinement fusion device.

[0047] Finally, it should be noted that the above embodiments are intended to illustrate the technical solutions of the present invention and do not constitute any form of limitation on the present invention. Those skilled in the art should fully understand that it is completely feasible to modify the technical solutions described in the above embodiments or to perform equivalent replacements on any part or all of the technical features therein. These modifications or replacements, as long as they do not deviate from the scope of protection determined by the claims of the present invention, should be regarded as reasonable extensions of the present invention.

Claims

1. A method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy, characterized in that: The following steps are involved: Optimize the experimental parameters of laser-induced breakdown spectroscopy in vacuum and strong magnetic field environment, including: adjust the energy density of the incident laser so that the laser ablates the impurity film, the plasma generated belongs to chemical dose ablation, and the luminescent elements in the laser ablation plasma are consistent with the elements in the impurity film; adjust the gate delay and gate width time of the spectrometer so that the laser ablation plasma is in a local thermodynamic equilibrium state; Establishing a pre-classification model for the composition of deposited impurity films, wherein the pre-classification model for the composition of deposited impurity films classifies the matrix properties of the samples according to the LIBS characteristic spectral line analysis of the impurity films, and each classification is regarded as a subset of the same matrix of the co-deposited films; Select standard thin film samples in each co-deposited thin film homogeneous matrix subset and collect LIBS characteristic spectra of each standard thin film sample, and obtain a characteristic spectral line spectrum correction factor database based on the LIBS characteristic spectra through a single standard sample correction model; Based on the optimized parameter conditions, the LIBS characteristic spectrum of the impurity deposition layer is collected by the LIBS online measurement system; the matrix property of the co-deposited film is judged by the deposited impurity film component pre-classification model; the corresponding characteristic spectrum correction coefficient in the characteristic spectrum correction factor database is read according to the matrix property; the characteristic spectrum line in the online LIBS spectrum is multiplied by the correction coefficient and then CF-LIBS calculation is performed to obtain the LIBS quantitative analysis result.

2. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 1, characterized in that: The deposited impurity film composition pre-classification model is established as follows: Collect or prepare several impurity film samples; Measure the content of each element in all impurity film samples; Based on the measured content of each element in the impurity film samples, the impurity film samples are classified as follows: 1) Samples with only one element content greater than 60% are classified as "unit-based" samples, and the sample categories are subdivided according to the main elements; 2) Samples with two elements with contents greater than 40% at the same time are classified as "binary-based" samples, and the sample categories are subdivided according to the types of the two main elements; 3) Samples with three elements with contents greater than 30% at the same time are classified as "ternary-based" samples, and the sample categories are subdivided according to the types of the three main elements; each type of impurity film sample is regarded as a subset of the same matrix of the co-deposited film; Collect LIBS spectra of all impurity film samples; According to the intensity of the characteristic spectral lines of each element in the LIBS spectrum, the relationship between the content ratio of the elements and the intensity ratio of the characteristic spectral lines of the corresponding elements in the LIBS spectrum is established; specifically, the characteristic spectral line intensity of the main element in the impurity film sample composed of n elements is respectively ratioed with the characteristic spectral line intensity of the remaining elements, and the ratio should be within an interval M n Inside, M n Is an n-dimensional array, and the array is used as a dividing boundary to indicate whether each value is an upper limit or a lower limit.

3. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 1, characterized in that: The process of establishing the characteristic line spectrum correction factor database is as follows: A standard film sample is selected from each co-deposited film homologous substrate subset, and the parameters of the laser and spectrometer of the LIBS online measurement system are set to be consistent with the set optimization parameters under the 1:1 simulated fusion device operating vacuum, strong magnetic field, and optical path conditions, and the LIBS characteristic spectrum of each standard film sample is measured; The Thomson scattering method is used to measure the plasma temperature generated by laser ablation of a standard thin film sample under the experimental conditions of LIBS optimized parameters. The inverse of the plasma temperature is used as a reference value for the slope fitting of the subsequent Boltzmann distribution diagram. The characteristic spectra of each standard thin film sample collected were subjected to CF-LIBS quantitative analysis and calculation, and the calculation results were compared with the content values ​​of each element of the corresponding standard thin film samples to find the deviation between the calculated value and the theoretical value; the intercept of the linear distribution of the characteristic spectral line data points of each element in the Boltzmann slope diagram was calculated according to the true content, and regression correction was performed in the Boltzmann slope diagram with reference to the calculated value of the true content to obtain the correction coefficients of the characteristic spectra of all elements for the same matrix subset of the co-deposited film.

4. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 3, characterized in that: The selection criteria of the standard film sample are samples whose content values ​​of each component in the co-deposited film and the matrix subset are in the middle of the corresponding range.

5. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 1, characterized in that: The energy density of the nanosecond laser pulse with a wavelength of 1064nm is higher than 5J / cm 2 .

6. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 1, characterized in that: The gate delay time and gate width time used by the spectrometer are 100-200ns and 100-200ns, respectively.

7. The method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to claim 1, characterized in that: The method for establishing the pre-classification model of the deposited impurity film composition also includes a multivariate statistical method and an artificial intelligence algorithm; wherein the multivariate statistical method can perform classification modeling according to the PCA and PLS models, establish a mapping relationship between classification features based on the intensity information of the characteristic spectrum by inputting spectral data, and give a judgment value of the matrix property of the impurity film.

8. A method for quantitative analysis of elements on the inner wall surface of a magnetic confinement fusion device by laser induced breakdown spectroscopy according to any one of claims 1 to 7, characterized in that: The LIBS online measurement system is used to scan in three-dimensional space and collect LIBS characteristic spectra at different points of the wall material; The matrix properties are judged according to the deposited impurity film component pre-classification model and the corresponding characteristic spectrum correction coefficients are selected from the characteristic spectrum correction factor database based on the matrix properties; then CF-LIBS calculation is performed to obtain the content value of the elements contained in each point, and the spatial distribution relationship of each element is reconstructed.

Citation Information

Patent Citations

  • Method for quantitative analysis of elements in unknown sample by spectrum combined with mass spectrometry

    CN107271429A

  • Method for in-situ real-time quantitative diagnosis of fusion device surface wall part corrosion deposition

    CN111929127A

  • Data processing method for improving classification accuracy of laser-induced breakdown spectroscopy

    CN112782151A

  • Single standard sample correction laser-induced breakdown spectroscopy quantitative method and system

    CN115201180A

  • System and method for analyzing impurity elements on surface of divertor of EAST Tokamak device

    CN115753715A

Cited By

  • Method and system for detecting impurities in glucosamine production process

    CN119619020A

  • Method for representing thickness of thin film of superconducting cavity of accelerator

    CN120467201A

  • Pulse energy control method and system for femtosecond laser processing of carbon nanotube film

    CN121535322A

  • Method for detecting amount of regenerated lithium in positive electrode material of lithium iron phosphate battery

    CN121577610A