Aggregate water content detection method, system and equipment for concrete mixing plant
By combining image acquisition components and moisture meters in a concrete mixing plant, the moisture content of aggregates can be detected in real time, solving the problems of low detection efficiency and poor stability, and ensuring concrete quality.
Patent Information
- Application Number
- CN202411166950.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-22
AI Technical Summary
The existing concrete mixing plant has low efficiency and instability in detecting aggregate moisture content, which affects the quality of concrete.
Image acquisition components are used to acquire images of the material being fed, and moisture content is measured using a moisture meter. The measured moisture content is determined by matching and verifying the predicted moisture content with the measured moisture content.
It enables real-time and accurate detection of aggregate moisture content in concrete mixing plants, thereby improving the quality of concrete processing.
Smart Images

Figure CN119000677A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of concrete production, and in particular to a method, system and equipment for detecting moisture content of aggregates used in concrete mixing plants. Background Art
[0002] The concrete production system should not only undertake all the concrete production of the project and meet the needs of concrete pouring construction progress and monthly and hourly pouring strength, but also adjust the mix ratio according to the building characteristics, construction environment, and various special needs of construction plans of different projects. It should be able to produce multiple grades, multiple levels and multiple varieties of concrete, and be able to adapt to the changes and needs of concrete pouring and transportation plans. The moisture content of the raw materials, sand and gravel, plays a vital role.
[0003] At present, the moisture content of aggregates in concrete mixing plants is tested through laboratory sampling and manual judgment by experienced inspectors. However, laboratory sampling is inefficient and lacks timeliness, which will affect the accuracy of concrete water distribution and thus the quality of concrete. Manual judgment depends on the state of the inspector, and the concrete processing site has the characteristics of poor environment and high labor intensity, which will affect the state of the inspector, resulting in unstable judgment results, and thus affecting the quality of concrete processing. Summary of the invention
[0004] In order to help improve the effect of aggregate moisture content detection, the present application provides an aggregate moisture content detection method, system and equipment for a concrete mixing plant.
[0005] In the first aspect, the present application provides a method for detecting moisture content of aggregates in a concrete mixing plant, which adopts the following technical solution: A method for detecting moisture content of aggregates in a concrete mixing plant, the method comprising: Acquire a feeding image, and predict the moisture content of the aggregate based on the feeding image to obtain a predicted moisture content; the feeding image includes an image of an aggregate feeding area of the concrete mixing station; Obtaining a measured moisture content collected by a moisture meter, wherein the moisture meter is used to measure the moisture content of aggregates in the aggregate feeding area; determining whether the predicted moisture content matches the measured moisture content; In the case where the predicted moisture content matches the measured moisture content, a measured moisture content of the aggregate in the aggregate loading area is determined based on the predicted moisture content and the measured moisture content.
[0006] By adopting the above technical scheme, the predicted moisture content of the aggregate can be obtained based on the aggregate image of the aggregate feeding area, and the measured moisture content of the aggregate in the aggregate feeding area can be determined in combination with the measured moisture content of the aggregate in the aggregate feeding area collected by the moisture meter. In this way, the moisture content of the aggregate entering the mixing station can be detected in real time and accurately during the operation of the mixing station, which can help improve the quality of concrete processing.
[0007] Optionally, after determining whether the predicted moisture content matches the measured moisture content, the method further includes: In the case where the predicted moisture content does not match the measured moisture content, obtaining a reference index value and an actual index value of the collection influencing index corresponding to the predicted moisture content, wherein the reference index value refers to the index value used in the process of determining the predicted moisture content, and the actual index value is obtained by real-time collection of the aggregate feeding area; Determining whether the reference index value matches the actual index value; In the case that the reference index value does not match the actual index value, the predicted moisture content is re-determined using the actual index value as the reference index value, and the step of determining whether the predicted moisture content matches the measured moisture content is returned to be executed.
[0008] By adopting the above technical scheme, when the reference index value does not match the actual index value, the actual index value can be used as the reference index value to redetermine the predicted moisture content. This can help correct the impact of the index value error on the predicted moisture content, ensure the accuracy of the predicted moisture content, and further help to accurately determine the measured moisture content.
[0009] Optionally, after determining whether the reference indicator value matches the actual indicator value, the step further includes: In the case where the reference index value matches the actual index value, determining a change in the predicted moisture content and a change in the measured moisture content; Determining whether the change in the measured moisture content matches the change in the predicted moisture content; When the change in the measured moisture content does not match the change in the predicted moisture content, the measured moisture content is determined to be abnormal, and the measured moisture content is determined based on the predicted moisture content and a predetermined prediction error, wherein the prediction error is used to indicate the corresponding relationship between the predicted moisture content and the measured moisture content.
[0010] By adopting the above technical scheme, when it is determined that the measured moisture content is abnormal, the measured moisture content can be determined directly based on the predicted moisture content. This can help avoid the influence of the abnormal measured moisture content on the accuracy of the measured moisture content, thereby helping to ensure the accuracy of the measured moisture content.
[0011] Optionally, after determining whether the change in the measured moisture content matches the change in the predicted moisture content, the method further includes: When the change of the measured moisture content matches the change of the predicted moisture content, recording a measurement abnormality; Determining whether the number of measurement anomalies is less than or equal to a preset number threshold; When the number of measurement anomalies is less than or equal to the preset number threshold, adjusting the measured moisture content to obtain an adjusted measured moisture content; The measured moisture cut is determined based on the predicted moisture cut and the adjusted measured moisture cut.
[0012] By adopting the above technical solution, the measured moisture content can be adjusted first when a measurement abnormality is determined, and then the measured moisture content is determined by combining the predicted moisture content and the adjusted measured moisture content, which can help improve the accuracy of the determined measured moisture content.
[0013] Optionally, the determining whether the number of measurement anomalies is less than a measurement number threshold further includes: When the number of measurement anomalies is greater than the preset number threshold, the measured moisture content is determined to be abnormal, and the measured moisture content is determined based on the predicted moisture content and a predetermined prediction error.
[0014] Optionally, determining whether the predicted moisture content matches the measured moisture content includes: Determine whether the difference between the predicted moisture content and the measured moisture content is greater than a preset difference threshold; In the case where the gap is greater than the gap threshold, determining whether a ratio of the gap value to the measured moisture content is less than a preset ratio threshold; When the ratio is less than the ratio threshold, it is determined that the measured water content matches the predicted water content.
[0015] By adopting the above technical solution, when the difference between the preset moisture content and the measured moisture content is large, the ratio of the difference value to the measured moisture content can be further combined to determine whether the measured moisture content matches the preset moisture content, which can help improve the accuracy of the matching result. Optionally, the feeding image includes a thermal imaging image, and the moisture content of the aggregate in the aggregate feeding area is predicted based on the feeding image to obtain the predicted moisture content, including: determining an aggregate image corresponding to the aggregate from the thermal imaging image; determining temperature distribution data of the aggregate surface based on the aggregate image; Inputting the temperature distribution data into a moisture content prediction model to obtain a predicted moisture content; The moisture content prediction model is obtained based on training data, and the training data includes at least one group of sample data, and each group of sample data includes temperature distribution data of sample sand and gravel and actual moisture content of the sample sand and gravel.
[0016] By adopting the above technical scheme, the temperature distribution data of the aggregate surface can be determined based on the thermal imaging image in the loading image, and the moisture content corresponding to the temperature distribution can be predicted based on the moisture content prediction model to obtain the predicted moisture content, thereby realizing real-time prediction of the aggregate moisture content.
[0017] Optionally, the temperature distribution data includes a reference temperature value and a temperature difference value, and determining the temperature distribution data of the aggregate surface based on the aggregate image includes: Dividing the aggregate image into at least two image blocks; For each of the image blocks, determining a temperature corresponding to the image block based on image information corresponding to the image block; Determine an average value of the temperatures corresponding to the image blocks as the reference temperature; The maximum difference value of the temperatures corresponding to the image blocks is determined as the temperature difference value.
[0018] By adopting the above technical solution, the temperature distribution data can not only reflect the temperature value corresponding to the aggregate, but also reflect the temperature difference of aggregates at different positions, which can help improve the reference value of the temperature distribution data, and further help improve the accuracy of the final predicted moisture content.
[0019] In a second aspect, the present application provides an aggregate moisture content measurement system for a concrete mixing plant, which adopts the following technical solution: A system for measuring moisture content of aggregates in a concrete mixing plant, the system comprising a controller, an image acquisition component and a moisture meter, wherein the controller is connected to the image acquisition component and the moisture meter respectively; The image acquisition component is used to acquire images of the aggregate loading area of the concrete mixing station; The moisture meter is used to measure the moisture content of the aggregate in the aggregate feeding area; The controller is used to execute any one of the aggregate moisture content detection methods for a concrete mixing plant provided in the first aspect.
[0020] In a third aspect, the present application provides an electronic device, which adopts the following technical solution: An electronic device, comprising: at least one processor; Memory; At least one application, wherein the at least one application is stored in a memory and configured to be executed by at least one processor, and the at least one application is configured to: execute any one of the aggregate moisture content detection methods for a concrete mixing plant provided in the first aspect.
[0021] In summary, the present application includes at least one of the following beneficial technical effects: 1. The predicted moisture content of the aggregate can be obtained based on the loading image of the aggregate loading area, and the measured moisture content of the aggregate in the aggregate loading area can be determined in combination with the measured moisture content of the aggregate in the aggregate loading area collected by the moisture meter. In this way, the moisture content of the aggregate entering the mixing station can be detected in real time and accurately during the operation of the mixing station, which can help improve the quality of concrete processing.
[0022] 2. Before combining the predicted moisture content with the measured moisture content to determine the measured moisture content, it is possible to first determine whether the predicted moisture content matches the measured moisture content. This allows for mutual verification between the predicted moisture content and the measured moisture content, which can help ensure the validity of the predicted moisture content and the measured moisture content involved in the measured moisture content calculation, and thus can help improve the accuracy of the measured moisture content. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a flow chart of a first method for detecting moisture content of aggregates in a concrete mixing plant provided in an embodiment of the present application; Figure 2 It is a flow chart of a second method for detecting moisture content of aggregates in a concrete mixing plant provided in an embodiment of the present application; Figure 3 It is a flow chart of a third method for detecting moisture content of aggregates in a concrete mixing plant provided in an embodiment of the present application; Figure 4 It is a flow chart of a fourth method for detecting moisture content of aggregates in a concrete mixing plant provided in an embodiment of the present application; Figure 5 It is a flow chart of a method for determining a predicted moisture content provided in an embodiment of the present application; Figure 6 is a flow chart of another method for determining predicted moisture content provided in an embodiment of the present application; Figure 7 It is a structural schematic diagram of an aggregate moisture content detection system for a concrete mixing plant provided in an embodiment of the present application; Figure 8 It is a structural schematic diagram of an electronic device provided in an embodiment of the present application. DETAILED DESCRIPTION
[0024] In order to make the purpose, technical solutions and advantages of this application more clear, the following Figure 1-8 It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0025] The present application embodiment discloses a method for detecting the moisture content of aggregates in a concrete mixing plant. Figure 1 , the aggregate moisture content detection method includes the following steps: Step 101, obtaining a material loading image, and predicting the moisture content of the aggregate based on the material loading image to obtain a predicted moisture content.
[0026] The loading image includes an image of the aggregate loading area of the concrete mixing station. Specifically, the loading image is collected by an image acquisition component set in the aggregate loading area of the concrete mixing station. In actual implementation, the image acquisition direction of the image acquisition component can be directly facing the aggregate loading area, or it can also be collected by collecting the mirror image of the aggregate loading area displayed in the optical reflector set in the aggregate loading area. This embodiment does not limit the collection method of the loading image.
[0027] Optionally, the moisture content of the aggregate is predicted based on the loading image to obtain the predicted moisture content, including: parsing the image corresponding to the aggregate in the loading image to obtain image feature information; and determining the predicted moisture content based on the image feature information.
[0028] The corresponding relationship between the image feature information and the moisture content is preset, and the image feature information is set based on the type of the feeding image. For example, when the feeding image includes a thermal imaging image, the image feature information includes temperature information. For another example, when the feeding image information includes an ultrasonic image, the image feature information includes an ultrasonic echo signal.
[0029] In actual implementation, the feeding image information may include an image of the entire aggregate feeding area, or may also include an image of a preset area in the aggregate feeding area, such as an image within a preset distance range from the feeding port.
[0030] Step 102, obtaining the measured moisture content collected by the moisture meter.
[0031] Among them, the moisture meter is used to measure the moisture content of aggregates in the aggregate feeding area.
[0032] In one example, the moisture meter is a non-contact moisture meter, such as a microwave moisture meter. In actual implementation, the moisture meter may also be a contact moisture meter, such as a capacitive moisture meter, as long as the moisture content can be measured.
[0033] Since the measurement range of the moisture meter is limited, that is, it can only detect the moisture content of aggregates in a small range, and in the actual production process, the aggregate feeding area usually includes a large amount of aggregates, so the moisture meter can only detect the moisture content of a small part of the aggregates in the feeding area. In actual implementation, the moisture meter can be fixed or mobile, for example: held by a staff member. Furthermore, after the moisture meter collects the measured moisture content, it will automatically upload the measured moisture content.
[0034] In actual implementation, the range of aggregates corresponding to the loading image is larger than the range of aggregates that can be collected by the moisture meter. In this embodiment, the moisture content of the aggregates is determined separately by combining the loading image and the moisture meter. This can help to increase the range of moisture content used for reference, and further help to improve the accuracy of the moisture content finally determined.
[0035] Step 103, determining whether the predicted moisture content matches the measured moisture content.
[0036] Generally speaking, the moisture content of aggregates at different positions in the aggregate feeding area is similar, that is, the predicted moisture content and the measured moisture content should be similar. However, in actual application, the prediction and measurement process may be affected by environmental factors, collection errors, calculation errors, equipment failures and other factors, which will lead to inaccurate predicted moisture content or measured moisture content. Therefore, it is necessary to determine whether the predicted moisture content and the measured moisture content are similar by determining whether the predicted moisture content matches the measured moisture content before calculating the moisture content.
[0037] In this embodiment, the matching method between the predicted moisture content and the measured moisture content is pre-set, for example: whether the predicted moisture content matches the measured moisture content can be judged based on at least one factor such as the gap between the predicted moisture content and the measured moisture content, the ratio between the predicted moisture content and the measured moisture content, etc.
[0038] In one example, determining whether the predicted moisture content matches the measured moisture content includes: determining whether the difference between the predicted moisture content and the measured moisture content is greater than a preset difference threshold; when the difference is less than or equal to the difference threshold, determining that the measured moisture content matches the preset moisture content; when the difference is greater than the difference threshold, determining whether the ratio of the difference value to the measured moisture content is less than a preset ratio threshold; when the ratio is less than the ratio threshold, determining that the measured moisture content matches the predicted moisture content; when the ratio is greater than or equal to the ratio threshold, determining that the measured moisture content does not match the preset moisture content. In the above technical solution, when the difference between the preset moisture content and the measured moisture content is large, further combining the size of the ratio of the difference value to the measured moisture content to determine whether the measured moisture content matches the preset moisture content, which can help improve the accuracy of the matching result. In addition, since the difference between the predicted moisture content and the measured moisture content is less than or equal to the difference value threshold, the measured moisture content is directly determined to match the predicted moisture content without calculating and judging the ratio of the difference value to the measured moisture content. This can help reduce the amount of calculation in the matching process, and thus help improve the efficiency of moisture content detection.
[0039] Step 104 , when the predicted moisture content matches the measured moisture content, determine the measured moisture content of the aggregate in the aggregate loading area based on the predicted moisture content and the measured moisture content.
[0040] Specifically, when the predicted moisture content matches the measured moisture content, it means that the predicted moisture content is close to the measured moisture content, which further indicates that the error between the predicted moisture content and the measured moisture content is small. At this time, the predicted moisture content and the measured moisture content can be combined to determine the final measured moisture content.
[0041] Optionally, determining the measured moisture content of aggregate in the aggregate loading area based on the predicted moisture content and the measured moisture content includes: determining a weighted average of the predicted moisture content and the measured moisture content as the measured moisture content.
[0042] The weight distribution between the predicted moisture content and the measured moisture content can be preset, for example, the weights of the predicted moisture content and the measured moisture content are the same, or the weight distribution can be dynamically adjusted in combination with the actual situation. In actual implementation, the weight distribution can be dynamically adjusted in combination with the ambient temperature of the aggregate feeding area. For example, when the ambient temperature is greater than the upper limit of the optimal temperature, the ambient temperature has a greater impact on the accuracy of the predicted moisture content. At this time, the weight of the predicted moisture content can be appropriately reduced to improve the accuracy of the measured moisture content.
[0043] The implementation principle of a method for detecting the moisture content of aggregates in a concrete mixing station provided in an embodiment of the present application is as follows: obtaining a feeding image, and predicting the moisture content of the aggregates based on the feeding image to obtain the predicted moisture content; the feeding image includes an image of the aggregate feeding area of the concrete mixing station; obtaining the measured moisture content collected by a moisture meter, and the moisture meter is used to measure the moisture content of the aggregates in the aggregate feeding area; determining whether the predicted moisture content matches the measured moisture content; when the predicted moisture content matches the measured moisture content, determining the measured moisture content of the aggregates in the aggregate feeding area based on the predicted moisture content and the measured moisture content. By adopting the above technical solution, the predicted moisture content of the aggregates can be obtained based on the feeding image information of the aggregate feeding area, and the measured moisture content of the aggregates in the aggregate feeding area can be determined in combination with the measured moisture content of the aggregates in the aggregate feeding area collected by the moisture meter. In this way, the moisture content of the aggregates entering the mixing station can be detected in real time and accurately during the operation of the mixing station, which can help improve the quality of concrete processing.
[0044] In addition, since it is first determined whether the predicted moisture content matches the measured moisture content before combining the predicted moisture content and the measured moisture content to determine the measured moisture content, mutual verification between the predicted moisture content and the measured moisture content can be achieved, which can help ensure the validity of the predicted moisture content and the measured moisture content involved in the measured moisture content calculation, and further help improve the accuracy of the measured moisture content.
[0045] In some embodiments, reference Figure 2 , step 103, after determining whether the predicted moisture content matches the measured moisture content, the following steps are also included: Step 201 : when the predicted water content does not match the measured water content, obtain a reference index value and an actual index value of a collection influencing index corresponding to the predicted water content.
[0046] The reference index value refers to the index value used in the process of predicting the moisture content, and the actual index value is obtained by real-time collection of the aggregate feeding area. Specifically, since the index value of the collection influencing index such as environmental factors and the working parameters of the collection equipment will affect the collection of the feeding image, the index value of the collection influencing index needs to be considered in the process of predicting the moisture content based on the feeding image, which can help improve the accuracy of the prediction results.
[0047] Since the collected index value is relatively fixed within a period of time, in this embodiment, the reference index value can be predetermined, for example, the most recently acquired actual index value is determined as the reference index value, or the reference index value is determined based on multiple actual index values collected historically. In this way, it is not necessary to obtain the actual index value in each water content prediction process, which can help reduce the frequency of collecting the actual index value.
[0048] In actual implementation, the number of the collection influencing indicators may be one or more than two. When there are more than two collection influencing indicators, it is necessary to obtain the indicator value corresponding to each collection influencing indicator respectively.
[0049] Step 202: Determine whether the reference index value matches the actual index value.
[0050] Specifically, when the predicted moisture content does not match the measured moisture content, it means that the predicted moisture content may be abnormal, and the abnormality of the predicted moisture content may be caused by inaccurate reference index value used in the prediction process. Therefore, this embodiment will check whether the reference index value matches the actual index value.
[0051] Optionally, determining whether the reference indicator value matches the actual indicator value includes: determining whether the difference between the reference indicator value and the actual indicator value is less than the difference threshold corresponding to the collection influencing indicator; if so, determining that the reference indicator value matches the actual indicator value; if not, determining that the reference indicator value does not match the actual indicator value.
[0052] Furthermore, in the case where there are more than two acquisition influencing index values, it is necessary to match the reference index value and the actual index value corresponding to each acquisition influencing index respectively.
[0053] Step 203, when the reference index value does not match the actual index value, the actual index value is used as the reference index value to redetermine the predicted moisture content, and the process returns to the step of determining whether the predicted moisture content matches the measured moisture content, that is, returns to step 103.
[0054] Specifically, when the reference index value does not match the actual index value, it means that there may be an error in the process of determining the predicted moisture content. At this time, using the actual index value as the reference index value to re-determine the predicted moisture content can correct the impact of the index value error on the accuracy of the predicted moisture content, thereby improving the accuracy of the predicted moisture content.
[0055] It should be noted that since the re-determined predicted moisture content can correct the impact of the index value error on the predicted moisture content and ensure the accuracy of the predicted moisture content, therefore, determining whether the predicted moisture content matches the measured moisture content after the predicted moisture content is re-determined can help determine whether there is a large error in the measured moisture content, and further help determine the final method for determining the measured moisture content.
[0056] Furthermore, in the case where the reference indicator value does not match the actual indicator value, the reference indicator value may be updated based on the actual indicator value, thereby achieving dynamic updating of the reference indicator value, which in turn may help improve the accuracy of the reference indicator value.
[0057] Optionally, when the reference index value matches the actual index value, it can be directly determined that the measured moisture content is abnormal, or other methods can be combined to further determine whether the measured index value is abnormal.
[0058] In the above implementation, since the predicted moisture content does not match the measured moisture content, it will be further determined whether the reference index value used in the process of determining the predicted moisture content matches the real-time index value of the aggregate feeding area. If there is a mismatch, the actual index value is used as a reference to the reference index value to redetermine the predicted moisture content. This can help correct the impact of the index value error on the predicted moisture content, ensure the accuracy of the predicted moisture content, and further help to accurately determine the measured moisture content.
[0059] For further reference, Figure 3 , step 202, after determining whether the reference index value matches the actual index value, the following steps are also included: Step 301, when the reference index value matches the actual index value, determining the change of the predicted water content and the change of the measured water content.
[0060] Specifically, when the reference index value matches the actual index value, the accuracy of the predicted moisture content is high. At this time, the change in the predicted moisture content and the change in the measured moisture content can be further combined to determine whether there is an abnormality in the measured moisture content.
[0061] In one example, the change condition includes a change direction, that is, an increase or decrease, such as a change direction relative to the data determined last time or several times.
[0062] In another example, the change condition includes a change range, such as a change range relative to the data determined last time or several times.
[0063] Step 302: Determine whether the change in the measured moisture content matches the change in the predicted moisture content.
[0064] In one example, the change includes a direction of change. At this time, determining whether the change of the measured moisture content matches the change of the predicted moisture content includes: determining whether the change direction of the measured moisture content is the same as the change direction of the predicted moisture content; if not, determining that the change of the measured moisture content does not match the change of the predicted moisture content; if so, it can be directly determined that the change of the measured moisture content matches the change of the predicted moisture content, or it can be combined with other factors to further determine whether the change of the measured moisture content matches the change of the predicted moisture content.
[0065] In another example, the change includes the amplitude of the change. At this time, determining whether the change of the measured moisture content matches the change of the predicted moisture content includes: determining whether the difference between the amplitude of the change of the measured moisture content and the amplitude of the change of the predicted moisture content is less than a preset amplitude difference threshold; if not, determining that the change of the measured moisture content does not match the change of the predicted moisture content.
[0066] Step 303: When the change in the measured moisture content does not match the change in the predicted moisture content, determine that the measured moisture content is abnormal, and determine the measured moisture content based on the predicted moisture content and a predetermined prediction error.
[0067] The prediction error is used to indicate the corresponding relationship between the predicted moisture content and the measured moisture content. Specifically, the prediction error can be fixed or dynamically determined in combination with historical data. In actual implementation, the prediction error can be determined based on the relationship between the predicted moisture content in the historical data and the corresponding measured moisture content.
[0068] In one example, the prediction error is determined by taking the average value of the ratio of the measured moisture content to the corresponding predicted moisture content within a historical reference time period as the prediction error. Accordingly, the measured moisture content is determined based on the predicted moisture content and the predetermined prediction error, including: determining the product of the predicted moisture content and the prediction error as the measured moisture content.
[0069] Optionally, when the change in the measured moisture content does not match the change in the predicted moisture content, a measurement abnormality prompt message may be generated and output to prompt the staff to inspect the moisture meter.
[0070] Optionally, when the change in the measured moisture content matches the change in the predicted moisture content, the measured moisture content may be determined directly based on the measured moisture content and the predicted moisture content, or the calculation method of the moisture content may be further determined in other ways.
[0071] In the above implementation, since the reference index value does not match the actual index value, whether the measured moisture content is abnormal is further determined by combining the matching relationship between the change in the actual moisture content and the change in the predicted moisture content. In the case where the measured moisture content is abnormal, the measured moisture content is directly determined based on the predicted moisture content. This can help avoid the influence of the abnormal measured moisture content on the accuracy of the measured moisture content, thereby helping to ensure the accuracy of the measured moisture content.
[0072] Further, refer to Figure 4 , step 302, after determining whether the measured moisture content change matches the predicted moisture content change, the following steps are also included: Step 401, when the change of the measured moisture content matches the change of the predicted moisture content, a measurement abnormality is recorded.
[0073] Among them, the measurement anomalies are calculated cumulatively within a reference time period, and the reference time period is set according to actual needs, for example: the reference time period is a production cycle.
[0074] Step 402: Determine whether the number of measurement anomalies is less than or equal to a preset number threshold.
[0075] Step 403: When the number of measurement anomalies is less than or equal to a preset number threshold, the measured moisture content is adjusted to obtain an adjusted measured moisture content.
[0076] Specifically, when the number of measurement anomalies is less than or equal to the preset number threshold, that is, the difference between the measured moisture content and the predicted moisture content may be caused by normal fluctuations in the measured moisture content. At this time, the error in the measured moisture content can be reduced by adjusting the measured moisture content.
[0077] In one example, the measured moisture content is adjusted to obtain the adjusted measured moisture content, including: when the measured moisture content is less than the predicted moisture content, the measured moisture content is increased by a preset adjustment amplitude to obtain the adjusted measured moisture content; when the measured moisture content is greater than the predicted moisture content, the measured moisture content is increased by a preset adjustment amplitude to obtain the adjusted measured moisture content.
[0078] Furthermore, the preset adjustment range is determined in combination with the matching standard between the predicted moisture content and the measured moisture content and the matching standard between the change in the measured moisture content and the change in the predicted moisture content. This can help ensure that the adjusted measured moisture content matches the predicted moisture content as much as possible, thereby helping to improve the accuracy of the measured moisture content adjustment and further improve the accuracy of the measured moisture content.
[0079] Specifically, when the number of abnormal measurements is large, it means that the accuracy of the measured moisture content is generally poor, that is, the measured moisture content is abnormal. At this time, the measured moisture content is directly determined based on the predicted moisture content. This can help avoid the impact of abnormal measured moisture content on the accuracy of the measured moisture content, thereby helping to ensure the accuracy of the measured moisture content.
[0080] Step 404 , determining a measured moisture content based on the predicted moisture content and the adjusted measured moisture content.
[0081] Specifically, the method for determining the measured moisture content based on the predicted moisture content and the adjusted measured moisture content is described in the above step 104, which will not be described in detail in this embodiment.
[0082] Optionally, after step 402, determining whether the number of measurement anomalies is less than or equal to a preset number threshold, further includes: when the number of measurement anomalies is greater than the preset number threshold, determining that the measured moisture content is abnormal, and predicting the moisture content based on the predicted moisture content and a predetermined prediction error.
[0083] In the above technical scheme, since the measurement anomaly can be recorded when the change in the measured moisture content matches the change in the predicted moisture content, and the measured moisture content can be adjusted when the number of measurement anomalies is less than or equal to the preset number threshold, and the measured moisture content can be determined based on the predicted moisture content and the adjusted measured moisture content, the measured moisture content can be adjusted first when the measurement anomaly is determined, and then the measured moisture content can be determined in combination with the predicted moisture content and the adjusted measured moisture content, which can help improve the accuracy of the determined measured moisture content.
[0084] In some embodiments, the loading image includes a thermal imaging image, referring to Figure 5 In step 101, the moisture content of the aggregate is predicted based on the loading image to obtain the predicted moisture content, including the following steps: Step 501, determining an aggregate image corresponding to the aggregate from a thermal imaging image.
[0085] The aggregate image refers to the image of the location where the aggregate exists. Specifically, the amount and location distribution of aggregate in the aggregate feeding area may change dynamically, which means that the thermal imaging image may include images of locations where the aggregate does not exist in the aggregate feeding area. Therefore, in the actual analysis process, the locations of the non-existent aggregates need to be removed from the thermal imaging image to obtain the aggregate image.
[0086] In one example, determining an aggregate image corresponding to an aggregate from a thermal imaging image includes: obtaining a background temperature of an aggregate loading area; and determining an area corresponding to an image position in the thermal imaging image where a temperature difference corresponding to the background temperature is greater than a preset temperature difference threshold as an aggregate image.
[0087] The background temperature refers to the temperature when there is no aggregate in the aggregate feeding area. The background temperature may be a preset value, or may be collected in real time by a preset temperature sensor.
[0088] The preset temperature difference threshold is set based on the acquisition accuracy of the thermal imaging image.
[0089] In another example, determining an aggregate image corresponding to the aggregate from the thermal imaging image includes: determining an aggregate region where the aggregate exists in the aggregate loading region; and determining an image corresponding to the aggregate region in the thermal imaging image as the aggregate image.
[0090] The aggregate area can be obtained by performing image recognition on an image of the aggregate feeding area. For example, the feeding image also includes a color image, and the location of the aggregate in the aggregate feeding area can be accurately identified by the color image.
[0091] Step 502: determining temperature distribution data of the aggregate surface based on the aggregate image.
[0092] Specifically, since the aggregate image is captured from the thermal imaging image, and the thermal imaging image can reflect the temperature of the surface of the object, the temperature distribution data of the aggregate surface can be determined based on the aggregate image alone.
[0093] Optionally, the temperature distribution data may include at least one of the data reflecting the temperature distribution, such as the average value, maximum value, maximum value, temperature difference, etc., which may be set according to actual needs.
[0094] Step 503: input the temperature distribution data into a moisture content prediction model to obtain a predicted moisture content.
[0095] The moisture content prediction model is obtained based on training data, and the training data includes at least one set of sample data, each set of sample data includes temperature distribution data of sample sand and gravel and actual moisture content of the sample sand and gravel. Specifically, the temperature distribution data of the sample sand and gravel can also be determined by placing the sample sand and gravel in the aggregate feeding area and by the methods in the above steps 501 and 502, which can help improve the reference value of the temperature distribution data. In addition, the actual moisture content of the sand and gravel sample can be obtained by experimentally measuring the sample sand and gravel in the laboratory, such as: measured by the drying method, which can help improve the accuracy of the actual moisture content.
[0096] In the above technical scheme, since the temperature distribution data of the aggregate surface can be determined based on the thermal imaging image in the loading image, and the moisture content corresponding to the temperature distribution can be predicted based on the moisture content prediction model to obtain the predicted moisture content, the moisture content of the aggregate can be predicted based on the temperature distribution of the aggregate, thereby realizing real-time prediction of the moisture content of the aggregate.
[0097] Furthermore, the temperature distribution data includes a reference temperature value and a temperature difference value. Figure 6 The above step 502, determining the temperature distribution data of the aggregate surface based on the aggregate image, includes the following steps: Step 601: divide the aggregate image into at least two image blocks.
[0098] Specifically, since the distribution range of aggregates in the aggregate loading area may be large, the temperature of aggregates at different positions may be different. In order to improve the accuracy of the distribution data, in this embodiment, the aggregate image is first divided into at least two image blocks, and the conditions of different image blocks are compared to obtain temperature distribution data.
[0099] Optionally, dividing the aggregate image into at least two image blocks includes: analyzing the temperature change in the aggregate image to obtain aggregate piles; when there are more than two aggregate piles, dividing the image blocks based on the positions of the aggregate piles so that each image block includes at least one aggregate pile; when there is only one aggregate pile, dividing the aggregate pile into at least two image blocks along an axis passing through the top of the pile so that each image block includes at least a portion of the aggregate pile.
[0100] In one example, the aggregate image may belong to a pre-trained pile recognition model to obtain the position of the aggregate pile in the aggregate image, wherein the pile recognition model is trained based on training data, the training data includes at least one set of sample data, each set of sample data includes a sample image and the position of the aggregate pile in the sample image.
[0101] In actual implementation, the aggregate image may also be divided in other ways, for example, the aggregate image may be divided into a number of image blocks of similar size according to size.
[0102] Step 602: for each image block, determine the temperature corresponding to the image block based on image information corresponding to the image block.
[0103] Optionally, the average value of the temperatures at various positions in the image block indicated by the image information is determined as the temperature corresponding to the image block.
[0104] Step 603: determine the average value of the temperatures corresponding to the respective image blocks as the reference temperature.
[0105] Step 604: determine the maximum difference between the temperatures corresponding to the image blocks as the temperature difference.
[0106] Correspondingly, the above step 503, inputting the temperature distribution data into the moisture content prediction model to obtain the predicted moisture content, includes: inputting the reference temperature and the temperature difference into the moisture content prediction model to obtain the predicted moisture content.
[0107] In the above technical solution, since the thermal imaging image can be divided into at least two image blocks, and the reference temperature and temperature difference of the thermal imaging image can be determined based on the temperature corresponding to each image block, the temperature distribution data can not only reflect the temperature value corresponding to the aggregate, but also reflect the temperature difference of aggregates at different positions, which can help to improve the reference value of the temperature distribution data, and further help to improve the accuracy of the predicted moisture content finally determined.
[0108] The present application also provides an aggregate moisture content measurement system for a concrete mixing plant. Figure 7 , the system includes a controller 710, an image acquisition component 720 and a moisture meter 730, and the controller 710 is connected to the image acquisition component 720 and the moisture meter 730 respectively; The image acquisition component 720 is used to acquire images of the aggregate loading area of the concrete mixing station, that is, the loading image in the above method embodiment. In one example, the image acquisition component 720 includes a thermal imager for acquiring thermal imaging images.
[0109] The moisture meter 730 is used to measure the moisture content of the aggregate in the aggregate feeding area. The moisture meter 720 can be a microwave moisture meter or a capacitive moisture meter.
[0110] The controller 710 is used to execute the aggregate moisture content measurement method for a concrete mixing plant provided by the above method embodiment.
[0111] The present application also provides an electronic device, such as Figure 8 As shown, Figure 8 The electronic device 800 shown includes: a processor 801 and a memory 803. The processor 801 and the memory 803 are connected, such as through a bus 802. Optionally, the electronic device 800 may also include a transceiver 804. It should be noted that in actual applications, the transceiver 804 is not limited to one, and the structure of the electronic device 800 does not constitute a limitation on the embodiments of the present application.
[0112] The processor 801 may be a CPU (Central Processing Unit), a general-purpose processor, a DSP (Digital Signal Processor), an ASIC (Application Specific Integrated Circuit), an FPGA (Field Programmable Gate Array), or other programmable logic devices, transistor logic devices, hardware components, or any combination thereof. It may implement or execute various exemplary logic blocks, modules, and circuits described in conjunction with the disclosure of this application. The processor 801 may also be a combination that implements computing functions, such as a combination of one or more microprocessors, a combination of a DSP and a microprocessor, and the like.
[0113] The bus 802 may include a path to transmit information between the above components. The bus 802 may be a PCI (Peripheral Component Interconnect) bus or an EISA (Extended Industry Standard Architecture) bus. The bus 802 may be divided into an address bus, a data bus, a control bus, etc. Figure 8 Only one thick line is used in the diagram, but this does not mean that there is only one bus or only one type of bus.
[0114] The memory 803 may be a ROM (Read Only Memory) or other types of static storage devices that can store static information and instructions, a RAM (Random Access Memory) or other types of dynamic storage devices that can store information and instructions, or an EEPROM (Electrically Erasable Programmable Read Only Memory), a CD-ROM (Compact Disc Read Only Memory) or other optical disk storage, optical disk storage (including compressed optical disk, laser disk, optical disk, digital versatile disk, Blu-ray disk, etc.), a magnetic disk storage medium or other magnetic storage device, or any other medium that can be used to carry or store the desired program code in the form of instructions or data structures and can be accessed by a computer, but is not limited thereto.
[0115] The memory 803 is used to store the application code for executing the solution of the present application, and the execution is controlled by the processor 801. The processor 801 is used to execute the application code stored in the memory 803 to implement the content shown in the above method embodiment.
[0116] The electronic devices include, but are not limited to, mobile terminals such as mobile phones, laptop computers, digital broadcast receivers, PDAs (personal digital assistants), PADs (tablet computers), PMPs (portable multimedia players), vehicle-mounted terminals (such as vehicle-mounted navigation terminals), and fixed terminals such as digital TVs, desktop computers, etc. It can also be a server, etc. Figure 8 The electronic device shown is merely an example and should not bring any limitation to the functions and scope of use of the embodiments of the present application.
[0117] The embodiment of the present application also provides a computer-readable storage medium, on which a computer program is stored. When the computer program is executed in a computer, the computer is caused to execute the aggregate moisture content detection method for a concrete mixing plant provided in the above embodiment.
[0118] It should be understood that although the steps in the flowchart of the accompanying drawings are shown in sequence according to the instructions of the arrows, these steps are not necessarily performed in the order indicated by the arrows. Unless otherwise clearly stated in this document, the execution of these steps is not strictly limited in order and can be performed in other orders.
[0119] The above are only some implementation methods of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present application. These improvements and modifications should also be regarded as the scope of protection of the present application.
Claims
1. A method for detecting moisture content of aggregates in a concrete mixing plant. It is characterized in that The method comprises: Acquire a feeding image, and predict the moisture content of the aggregate based on the feeding image to obtain a predicted moisture content; the feeding image includes an image of an aggregate feeding area of the concrete mixing station; Obtaining a measured moisture content collected by a moisture meter, wherein the moisture meter is used to measure the moisture content of aggregates in the aggregate feeding area; determining whether the predicted moisture content matches the measured moisture content; In the case where the predicted moisture content matches the measured moisture content, a measured moisture content of the aggregate in the aggregate loading area is determined based on the predicted moisture content and the measured moisture content.
2. The method according to claim 1, It is characterized in that After determining whether the predicted moisture content matches the measured moisture content, the method further includes: In the case where the predicted moisture content does not match the measured moisture content, obtaining a reference index value and an actual index value of the collection influencing index corresponding to the predicted moisture content, wherein the reference index value refers to the index value used in the process of determining the predicted moisture content, and the actual index value is obtained by real-time collection of the aggregate feeding area; Determining whether the reference index value matches the actual index value; In the case that the reference index value does not match the actual index value, the predicted moisture content is re-determined using the actual index value as the reference index value, and the step of determining whether the predicted moisture content matches the measured moisture content is returned to be executed.
3. The method according to claim 2, It is characterized in that After determining whether the reference index value matches the actual index value, the method further includes: In the case where the reference index value matches the actual index value, determining a change in the predicted moisture content and a change in the measured moisture content; Determining whether the change in the measured moisture content matches the change in the predicted moisture content; When the change in the measured moisture content does not match the change in the predicted moisture content, the measured moisture content is determined to be abnormal, and the measured moisture content is determined based on the predicted moisture content and a predetermined prediction error, wherein the prediction error is used to indicate the corresponding relationship between the predicted moisture content and the measured moisture content.
4. The method according to claim 3, It is characterized in that After determining whether the change in the measured moisture content matches the change in the predicted moisture content, the method further includes: When the change of the measured moisture content matches the change of the predicted moisture content, recording a measurement abnormality; Determining whether the number of measurement anomalies is less than or equal to a preset number threshold; When the number of measurement anomalies is less than or equal to the preset number threshold, adjusting the measured moisture content to obtain an adjusted measured moisture content; The measured moisture cut is determined based on the predicted moisture cut and the adjusted measured moisture cut.
5. The method according to claim 4, It is characterized in that The determining whether the number of measurement anomalies is less than a measurement number threshold further includes: When the number of measurement anomalies is greater than the preset number threshold, the measured moisture content is determined to be abnormal, and the measured moisture content is determined based on the predicted moisture content and a predetermined prediction error.
6. The method according to claim 1, It is characterized in that The determining whether the predicted moisture content matches the measured moisture content includes: Determine whether the difference between the predicted moisture content and the measured moisture content is greater than a preset difference threshold; In the case where the gap is greater than the gap threshold, determining whether a ratio of the gap value to the measured moisture content is less than a preset ratio threshold; When the ratio is less than the ratio threshold, it is determined that the measured water content matches the predicted water content.
7. The method according to claim 1, It is characterized in that The feeding image includes a thermal imaging image, and the moisture content of the aggregate in the aggregate feeding area is predicted based on the feeding image to obtain the predicted moisture content, including: determining an aggregate image corresponding to the aggregate from the thermal imaging image; determining temperature distribution data of the aggregate surface based on the aggregate image; Inputting the temperature distribution data into a moisture content prediction model to obtain a predicted moisture content; The moisture content prediction model is obtained based on training data, and the training data includes at least one group of sample data, each group of sample data includes temperature distribution data of sample sand and gravel and actual moisture content of the sample sand and gravel.
8. The method according to claim 7, It is characterized in that The temperature distribution data includes a reference temperature value and a temperature difference value, and the determining the temperature distribution data of the aggregate surface based on the aggregate image includes: Dividing the aggregate image into at least two image blocks; For each of the image blocks, determining a temperature corresponding to the image block based on image information corresponding to the image block; Determine an average value of the temperatures corresponding to the image blocks as the reference temperature; The maximum difference value of the temperatures corresponding to the image blocks is determined as the temperature difference value.
9. An aggregate moisture content measurement system for a concrete mixing plant, It is characterized in that The system comprises a controller, an image acquisition component and a moisture meter, wherein the controller is connected to the image acquisition component and the moisture meter respectively; The image acquisition component is used to acquire images of the aggregate loading area of the concrete mixing station; The moisture meter is used to measure the moisture content of the aggregate in the aggregate feeding area; The controller is used to execute the aggregate moisture content detection method for a concrete mixing plant according to any one of claims 1 to 8.
10. An electronic device, It is characterized in that The electronic device comprises: at least one processor; Memory; At least one application, wherein the at least one application is stored in a memory and configured to be executed by at least one processor, and the at least one application is configured to: execute the aggregate moisture content detection method for a concrete mixing plant according to any one of claims 1-8.