Thin film capacitor and preparation method thereof, tumor treatment electrode patch and tumor treatment system
By adopting a multi-layer conductive layer structure and liquid metal filling design in the film capacitor, the tip discharge problem when the film capacitor is bent is solved, ensuring electrical connectivity and therapeutic effect.
Patent Information
- Application Number
- CN202310579360.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-22
- Publication Date
- 2024-11-22
AI Technical Summary
When existing membrane capacitors in tumor electric field treatment are bent, small gaps appear between the metal electrode layers, resulting in tip discharge, affecting the normal use of capacitor electrodes.
A multi-layer conductive layer structure is adopted, including an overlapping first conductive layer, a second conductive layer and a first flexible conductive layer. The first flexible conductive layer is filled between the first conductive layer and the second conductive layer, and the thickness of the flexible conductive layer is The conductive layer spacing can be changed to ensure electrical connectivity, and the flexible frame can be filled with liquid metal to maintain the conductive layer contact and avoid interlayer gaps.
It effectively avoids crack transmission and tip discharge of the metal electrode layer, ensuring the electrical connectivity and therapeutic effect of the film capacitor when bending.
Smart Images

Figure CN119008241A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of tumor treatment, and specifically to a film capacitor for tumor treatment and a preparation method thereof, a tumor treatment electrode patch, and a tumor treatment system. Background Art
[0002] Currently, there are many methods for treating tumors. Common treatments include surgical operation, radiotherapy, chemotherapy, molecular targeted therapy, etc. However, common treatments all have corresponding disadvantages. For example, radiotherapy or chemotherapy will kill normal cells. For another example, although surgical operation can cure early tumors, some patients may be easily injured due to surgical contraindications.
[0003] The use of alternating electric fields to treat tumors is one of the most cutting-edge tumor treatment methods currently under development. Tumor electric field therapy applies an alternating electric field to the treatment site of the human body, thereby affecting the aggregation of tumor microtubule proteins and preventing spindle formation, thereby achieving the purpose of inhibiting the mitotic process of cancer cells and inducing apoptosis of cancer cells. Specifically, the existing tumor electric field therapy mainly attaches electrode patches to the opposite sides of the patient's treatment site, such as the two sides of the patient's waist, and uses the thin film capacitors in the electrode patches to block the current from flowing directly to the patient. At the same time, the electrode plates of the thin film capacitors on the opposite sides apply an alternating electric field to the patient's treatment site, thereby achieving the purpose of tumor treatment.
[0004] In the prior art, since the treatment area of the patient is usually a curved surface rather than a flat surface, the film capacitor is required to have a certain degree of flexibility to adapt to the curved treatment area of the patient. Specifically, to ensure that the film capacitor has a certain degree of flexibility, the metal electrode layer of the film capacitor needs to be thinner and thus have a certain degree of flexibility. Summary of the invention
[0005] It should be noted that the following contents are phenomena discovered by the inventors after in-depth research and should not be considered as prior art known to those skilled in the art.
[0006] After in-depth research, the inventors found that setting the metal electrode layer as a multi-layer structure can slow down the transmission of metal cracks between different metal layers, thereby avoiding the generation of penetrating cracks in the metal electrode layer to a certain extent. However, when the film capacitor is bent, small gaps will appear between different metal layers, which will cause tip discharge and affect the normal use of the capacitor electrode.
[0007] The present application provides a thin film capacitor for tumor treatment and a preparation method thereof, a tumor treatment electrode patch, and a tumor treatment system, aiming to solve the technical problem of tip discharge caused by tiny gaps between different metal layers of a thin film capacitor.
[0008] In a first aspect, the present application provides a film capacitor for tumor treatment, characterized in that it includes:
[0009] a first electrode layer and a second electrode layer;
[0010] A dielectric layer, the dielectric layer is located between the first electrode layer and the second electrode layer;
[0011] The first electrode layer includes a first conductive layer, a second conductive layer and a first flexible conductive layer that overlap each other, and the first flexible conductive layer is filled between the first conductive layer and the second conductive layer;
[0012] The thickness of the first flexible conductive layer may vary with the distance between the first conductive layer and the second conductive layer at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer and the second conductive layer.
[0013] In some embodiments, the first conductive layer is laminated to the dielectric layer;
[0014] The tensile index of the second conductive layer is greater than the tensile index of the first flexible conductive layer, and the tensile index of the first flexible conductive layer is greater than the tensile index of the first conductive layer.
[0015] In some embodiments, the overall elastic modulus of the first electrode layer, the dielectric layer, and the first conductive layer, and the elastic modulus of the second conductive layer are greater than the elastic modulus of the first flexible conductive layer.
[0016] In some embodiments, when the thin film capacitor is curved in an arch shape, a bending radius of the first conductive layer is greater than a bending radius of the second conductive layer.
[0017] In some embodiments, the first flexible conductive layer includes conductive paper and a conductive elastomer; preferably, the conductive elastomer is conductive silicone or conductive rubber.
[0018] In some embodiments, the first flexible conductive layer includes a flexible frame and liquid metal;
[0019] The side of the flexible frame facing the first conductive layer is bonded to the edge region of the first conductive layer, and the side facing the second conductive layer is bonded to the edge region of the second conductive layer. Liquid metal is filled in the flexible frame.
[0020] In some embodiments, when the film capacitor is curved in an arch shape;
[0021] When the film capacitor is bent in an arch shape, the liquid metal is kept in close contact with the first conductive layer, and the liquid metal is kept in close contact with the second conductive layer.
[0022] In some embodiments, the second electrode layer includes a third conductive layer, a fourth conductive layer and a second flexible conductive layer, and the second flexible conductive layer is filled between the third conductive layer and the fourth conductive layer;
[0023] The thickness of the second flexible conductive layer can be changed with the distance between the third conductive layer and the fourth conductive layer at corresponding positions to ensure the electrical connectivity between the third conductive layer and the fourth conductive layer.
[0024] In some embodiments, the first flexible conductive layer has a thickness of 0.001 mm to 1 mm.
[0025] In some embodiments, the first flexible conductive layer has a thickness of 0.01 mm to 0.8 mm.
[0026] In some embodiments, the thickness of the first flexible conductive layer is 0.1 mm to 0.6 mm.
[0027] In some embodiments, the first conductive layer has a thickness of 10 nm to 1000 nm.
[0028] In some embodiments, the first conductive layer has a thickness of 10 nm to 800 nm.
[0029] In a second aspect, the present application provides a method for preparing a thin film capacitor for tumor treatment, comprising:
[0030] providing a second electrode layer;
[0031] forming a dielectric layer on the second electrode layer;
[0032] forming a first electrode layer on the dielectric layer, wherein the first electrode layer comprises an overlapping first conductive layer, a second conductive layer and a first flexible conductive layer, and the first flexible conductive layer is filled between the first conductive layer and the second conductive layer;
[0033] The thickness of the first flexible conductive layer may vary with the distance between the first conductive layer and the second conductive layer at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer and the second conductive layer.
[0034] In some embodiments, the first conductive layer is laminated to the dielectric layer;
[0035] The tensile index of the second conductive layer is greater than the tensile index of the first flexible conductive layer, and the tensile index of the first flexible conductive layer is greater than the tensile index of the first conductive layer.
[0036] In a third aspect, the present application provides a tumor treatment electrode patch, comprising the thin film capacitor as described in the first aspect.
[0037] In a fourth aspect, the present application provides a tumor treatment system, comprising the tumor treatment electrode patch as described in the third aspect.
[0038] The present application sets the electrode layer as a mutually independent multi-layer conductive layer structure. When cracks occur in a single conductive layer, the phenomenon of mutual transmission of such cracks can be avoided, thereby avoiding the occurrence of penetrating cracks in the electrode layer as much as possible. In addition, a flexible conductive layer is filled between each stack of the electrode layer. Since the thickness of the flexible conductive layer can change with the spacing between corresponding parts of adjacent conductive layers, the electrical connectivity between the conductive layers can be guaranteed, thereby avoiding the tip discharge phenomenon caused by the appearance of interlayer gaps between the conductive layers. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0040] Figure 1 is a structural schematic diagram of a thin film capacitor provided in an embodiment of the present application;
[0041] Figure 2 This is a schematic diagram of the structure of a film capacitor in use state provided in an embodiment of the present application;
[0042] Figure 3 is a schematic diagram of another use state structure of the film capacitor provided in the embodiment of the present application;
[0043] Figure 4 is another structural schematic diagram of a film capacitor provided in an embodiment of the present application;
[0044] Figure 5 is a schematic diagram of another use state structure of the film capacitor provided in the embodiment of the present application;
[0045] Figure 6 is another structural schematic diagram of a film capacitor provided in an embodiment of the present application;
[0046] Figure 7 is another structural schematic diagram of a film capacitor provided in an embodiment of the present application;
[0047] Figure 8 is another structural schematic diagram of a film capacitor provided in an embodiment of the present application;
[0048] Fig. 9 is another structural schematic diagram of a film capacitor provided in an embodiment of the present application;
[0049] Fig.10 It is a schematic diagram of a process of preparing a thin film capacitor provided in an embodiment of the present application;
[0050] Fig.11 It is a flow chart of a method for preparing a thin film capacitor provided in an embodiment of the present application.
[0051] Among them, 10 is a first electrode layer, 11 is a first conductive layer, 12 is a second conductive layer, 13 is a first flexible conductive layer, 131 is a flexible frame, 132 is liquid metal, 20 is a second electrode layer, 21 is a third conductive layer, 22 is a fourth conductive layer, 23 is a second flexible conductive layer, 30 is a dielectric layer, 40 is a flexible substrate, and 50 is a conductive attachment layer. DETAILED DESCRIPTION
[0052] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0053] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0054] In this application, the word "exemplary" is used to mean "serving as an example, illustration, or illustration." Any embodiment described in this application as "exemplary" is not necessarily to be construed as being preferred or advantageous over other embodiments. The following description is given to enable any person skilled in the art to implement and use the invention. In the following description, details are listed for the purpose of explanation. It should be understood that a person of ordinary skill in the art can recognize that the invention can be implemented without using these specific details. In other instances, well-known structures and processes are not elaborated in detail to avoid obscuring the description of the invention with unnecessary details. Therefore, the present invention is not intended to be limited to the embodiments shown, but is consistent with the widest scope consistent with the principles and features disclosed in this application.
[0055] The embodiments of the present application provide a thin film capacitor for tumor treatment and a preparation method thereof, a tumor treatment electrode patch, and a tumor treatment system, which are described in detail below.
[0056] First, see Figure 1 , Figure 1 A schematic diagram of the structure of a thin film capacitor in an embodiment of the present application is shown, wherein the thin film capacitor comprises:
[0057] A first electrode layer 10 and a second electrode layer 20;
[0058] A dielectric layer 30, the dielectric layer 30 is located between the first electrode layer 10 and the second electrode layer 20;
[0059] The first electrode layer 10 includes a first conductive layer 11, a second conductive layer 12 and a first flexible conductive layer 13 that overlap each other. The first flexible conductive layer 13 is filled between the first conductive layer 11 and the second conductive layer 12.
[0060] The thickness of the first flexible conductive layer 13 may vary with the distance between the first conductive layer 11 and the second conductive layer 12 at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer 11 and the second conductive layer 12 .
[0061] Specifically, the first electrode layer 10 and the second electrode layer 20 constitute the two poles of the film capacitor connected to the AC power supply, so as to facilitate the input of AC voltage signals into the film capacitor through the first electrode layer 10 and the second electrode layer 20. Generally, the film capacitor has a side close to the skin and a side away from the skin, the first electrode layer 10 is located on the side of the film capacitor close to the skin, and the second electrode layer 20 is located on the side of the film capacitor away from the skin. The second electrode layer 20 can be directly connected to the AC power supply, while the first electrode layer 10 can be coupled to the AC power supply through the human body and the film capacitor at a relative position attached to the other side of the human body.
[0062] In some embodiments of the present application, the second electrode layer 20 can be a thin and flexible metal layer, such as a metal copper foil, so that the second electrode layer 20 has better flexibility and is easy to bend, thereby making the film capacitor bend as a whole and better fit the skin surface of the human body. It can be understood that the second electrode layer 20 can also be made of other metal materials or non-metallic conductive materials, such as metal silver foil or conductive graphite.
[0063] In some embodiments of the present application, the thickness of the second electrode layer 20 is 0.005 mm-1 mm. Preferably, the thickness of the first electrode layer 10 is 0.01-0.1 mm. More preferably, the thickness of the second electrode layer 20 is 0.01-0.05 mm. The thickness of the second electrode layer 20 satisfies the above range, which can ensure the flexibility of the second electrode layer 20 on the one hand, and prevent the second electrode layer 20 from being too thin and easy to crack on the other hand.
[0064] In some embodiments of the present application, the second electrode layer 20 may refer to a corresponding metal layer on a circuit board, for example, a portion of a copper foil area is exposed on the circuit board, and a dielectric layer 30 is formed in the copper foil area, and the power interface of the circuit board can conveniently connect the two poles of the power supply. Preferably, the circuit board may be a flexible circuit board, such as a flexible printed circuit board made of polyimide or polyester film as a substrate, so as to simplify the electrical connection structure of the film capacitor while making the film capacitor flexible and bendable.
[0065] The dielectric layer 30 is made of an insulating material and can prevent current from flowing through, so as to prevent the current connected to the second electrode layer 20 of the thin film capacitor from directly acting on the human body. In some embodiments of the present application, the dielectric layer 30 can be made of an organic material or an inorganic material, such as ceramic, glass, mica, polypropylene, polystyrene or polyethylene terephthalate.
[0066] Preferably, the material of the dielectric layer 30 may include one or more of poly(VDF-TrFE-CTFE)(poly(vinylidene fluoride-trifluoroethylene-chlorotrifluoroethylene)), poly(VDF-TrFE-CFE)(poly(vinylidene fluoride-trifluoroethylene-1-chlorofluoroethylene)), poly(VDF-TrFECFE-CTFE)(poly(vinylidene fluoride-trifluoroethylene-chlorotrifluoroethylene-chlorofluoroethylene)), and poly(VDF-DB)(poly(vinylidene fluoride-diethylene glycol butyl ether)). Since the above materials have a higher dielectric constant, they help to increase the capacitance of the thin film capacitor when the thickness and area of the dielectric layer 30 are certain, thereby better applying the tumor treatment alternating electric field to the patient's treatment site.
[0067] In some embodiments of the present application, the thickness of the dielectric layer 30 is 1um to 100um. In some embodiments of the present application, the thickness of the dielectric layer 30 is 1um to 10um. Preferably, the thickness of the dielectric layer 30 is 2um to 8um. The thickness of the dielectric layer 30 meets the above-mentioned size requirements, so that the film capacitor has a higher capacitance, and at the same time, it can also avoid the phenomenon of breakdown of the film capacitor due to the excessive thickness of the dielectric layer 30.
[0068] In some embodiments of the present application, the dielectric layer 30 can be formed on the second electrode layer 20 by spin coating, scraping, atomization, casting or screen printing. In some other embodiments of the present application, the dielectric layer 30 is directly attached to the second electrode layer 20 in the form of a finished film.
[0069] In some embodiments of the present application, the material of the first conductive layer 11 can be one or a combination of Al, Ti, Au, Ag, Zn, Cu, Pt, Cr, Fe, Sn or Ni. For example, the first conductive layer 11 includes a magnetron sputtered Al material layer, a Zn material layer and an Ag material layer in sequence. For another example, the first conductive layer 11 includes a magnetron sputtered Al material layer or an Au material layer. In some embodiments of the present application, the first conductive layer 11 can be formed by spin coating or spray coating of non-metallic conductive materials such as graphite and conductive silicon.
[0070] In some embodiments of the present application, the thickness of the first conductive layer 11 is 1 nm to 1000 nm. Preferably, the thickness of the first conductive layer 11 is 10 nm to 800 nm. More preferably, the thickness of the first conductive layer 11 is 50 nm to 300 nm. The first conductive layer 11 having the above-mentioned size range can have good flexibility, and can also prevent the first conductive layer 11 from being too thick and prone to cracking due to bending, or from being too thin and unable to completely cover the dielectric layer 30.
[0071] It can be understood that the above-mentioned crack phenomenon of the first conductive layer 11 due to bending refers to only considering the change in the thickness of the first conductive layer 11. In fact, the crack phenomenon of the first conductive layer 11 is also related to the preparation process (such as sputtering, pressing or casting, etc.) or the structure of the metal layer itself.
[0072] The second conductive layer 12 is a thin and flexible metal layer, such as a metal copper foil with a thickness of 0.1 mm to 1 mm, so that the second conductive layer 12 has good flexibility and is easy to bend, thereby making the film capacitor bend as a whole and completely close to the skin surface of the human body. It can be understood that the second conductive layer 12 can also be made of other metal materials, such as metal silver foil.
[0073] In some embodiments of the present application, the second conductive layer 12 is preferably a stainless steel metal layer or a titanium metal layer. When the tumor treatment electrode patch is attached to the surface of human skin, the sweat exuded from the human skin or the water vapor generated by the hydrogel may penetrate into the interior of the film capacitor. The second conductive layer 12 is preferably set to a stainless steel metal layer or a titanium metal layer. On the one hand, it can prevent the second conductive layer 12 from corrosion, and on the other hand, it can also prevent the water vapor generated by the sweat or hydrogel from penetrating into the dielectric layer 30 inside the film capacitor, thereby avoiding the phenomenon of dielectric layer 30 of the film capacitor being broken down and damaged due to moisture.
[0074] In some embodiments of the present application, the thickness of the second conductive layer 12 is 0.005 mm-1 mm. Preferably, the thickness of the second conductive layer 12 is 0.01-0.1 mm. More preferably, the thickness of the second conductive layer 12 is 0.01-0.05 mm. The thickness of the second conductive layer 12 satisfies the above range, which can ensure the flexibility of the second conductive layer 12 on the one hand, and prevent the second conductive layer 12 from being too thin and easy to crack on the other hand.
[0075] The first flexible conductive layer 13 has conductivity and a small elastic modulus, so that the first flexible conductive layer 13 electrically connects the second conductive layer 12 with the first conductive layer 11, ensuring the electrical connectivity between the second conductive layer 12 and the first conductive layer 11. Meanwhile, the small elastic modulus of the first flexible conductive layer 13 can avoid the phenomenon of tiny gaps between the second conductive layer 12 and the first conductive layer 11, and prevent the phenomenon of tip discharge between the second conductive layer 12 and the first conductive layer 11.
[0076] In some embodiments of the present application, the thickness of the first flexible conductive layer 13 is 0.001 mm to 1 mm. Preferably, the thickness of the first flexible conductive layer 13 is 0.01 mm to 0.8 mm. More preferably, the thickness of the first flexible conductive layer 13 is 0.1 mm to 0.6 mm. Specifically, the thickness of the first flexible conductive layer 13 meets the above dimensions, which can avoid the phenomenon that the first flexible conductive layer 13 is too thick and its flexibility is reduced, and can also prevent the first flexible conductive layer 13 from being too thin and causing it to crack.
[0077] Preferably, the first flexible conductive layer 13 may include conductive paper, so that the first flexible conductive layer 13 further has higher tensile and tearing strength, and avoids the first flexible conductive layer 13 from being torn when the film capacitor is bent in contact with the surface of the human body. In some embodiments of the present application, the first flexible conductive layer 13 may also include a conductive elastomer, such as conductive rubber or conductive silicone.
[0078] It can be understood that the first flexible conductive layer 13 can also be formed by stacking at least two of conductive paper, conductive rubber and conductive silicone. For example, conductive paper and conductive rubber are stacked to form the first flexible conductive layer. The conductive paper ensures the tensile performance of the first flexible conductive layer 13, while the conductive rubber ensures the elasticity of the first flexible conductive layer 13.
[0079] In the embodiment of the present application, the present application sets the first electrode layer 10 as a multi-layer conductive layer structure, and when a crack occurs in a certain conductive layer, the phenomenon of such cracks being transmitted to each other can be avoided, thereby avoiding the first electrode layer 10 from having a penetrating crack as much as possible. At the same time, the first flexible conductive layer 13 is filled between the first conductive layer 11 and the second conductive layer 12. Since the thickness of the first flexible conductive layer 13 can change with the spacing between the corresponding parts of the first conductive layer 11 and the second conductive layer 12, the electrical connectivity between the first conductive layer 11 and the second conductive layer 12 can be guaranteed, and the tip discharge phenomenon caused by the interlayer gap between the first conductive layer 11 and the second conductive layer 12 can be avoided.
[0080] It should be noted that the thickness of the first flexible conductive layer 13 may refer to the minimum thickness, maximum thickness or average thickness of the first flexible conductive layer 13, and the spacing at the corresponding positions of the first conductive layer 11 and the second conductive layer 12 may refer to the minimum spacing, maximum spacing or average spacing between the first conductive layer 11 and the second conductive layer 12. When the thin film capacitor is bent, at least one of the minimum spacing, maximum spacing or average spacing between the first conductive layer 11 and the second conductive layer 12 will change, and the thickness (minimum thickness, maximum thickness or average thickness) of the first flexible conductive layer 13 will change accordingly, so that the two sides of the first flexible conductive layer 13 are respectively in close contact with the first conductive layer 11 and the second conductive layer 12, thereby ensuring the electrical connectivity between the first conductive layer 11 and the second conductive layer 12.
[0081] In some embodiments of the present application, the first conductive layer 11 is bonded to the dielectric layer 30; the tensile index of the second conductive layer 12 is greater than the tensile index of the first flexible conductive layer 13, and the tensile index of the first flexible conductive layer 13 is greater than the tensile index of the first conductive layer 11. In other words, the tensile indexes of the second conductive layer 12, the first flexible conductive layer 13, and the first conductive layer 11 decrease in sequence, so that the tensile index of the second conductive layer 12 far from the dielectric layer 30 is the largest, and the tensile index of the first conductive layer 11 close to the dielectric layer 30 is the smallest. When the film capacitor is bent, the second conductive layer 12 can protect the first conductive layer 11 and the first flexible conductive layer 13 from cracking, and the first flexible conductive layer 13 can protect the first conductive layer 11 from cracking, so that the first conductive layer 11 has double protection and is prevented from cracking as much as possible.
[0082] It should be noted that the tensile index refers to the tensile strength of the sample (the first conductive layer 11, the second conductive layer 12 or the first flexible conductive layer 13), which shows the maximum tensile strength that the sample can withstand before breaking. In some embodiments of the present application, the tensile index of the first flexible conductive layer 13 may be the maximum tensile strength that it can withstand before breaking. In some embodiments of the present application, the tensile index of the first conductive layer 11 may be the maximum tensile strength that it can withstand before breaking, and the tensile index of the second conductive layer 12 may be the maximum tensile strength that it can withstand before breaking.
[0083] In some embodiments of the present application, the overall elastic modulus of the first electrode layer 10, the dielectric layer 30 and the first conductive layer 11 and the elastic modulus of the second conductive layer 12 are greater than the elastic modulus of the first flexible conductive layer 13. That is to say, in the entire thin film capacitor, the elastic modulus of the first flexible conductive layer 13 is the smallest, so the elastic deformation of the first flexible conductive layer 13 is the largest, so that the first flexible conductive layer 13 can fully fill the space between the first conductive layer 11 and the second conductive layer 12, so that the electrical connectivity between the first conductive layer 11 and the second conductive layer 12 is ensured by the first flexible conductive layer 13; when used specifically, the first flexible conductive layer 13 is generally in an elastic compression state, and the first flexible conductive layer 13 will generate elastic force to act on the second conductive layer 12, so that the second conductive layer 12 close to the human skin is kept as close to the skin as possible, and finally ensure that the thin film capacitor can better couple the alternating electric field to the human body and perform treatment.
[0084] In some embodiments of the present application, when the thin film capacitor is curved in an arch shape, the bending radius of the first conductive layer 11 is greater than the bending radius of the second conductive layer 12. Figure 2 For example, Figure 2 A schematic diagram of a use state of the thin film capacitor in an embodiment of the present application is shown. When the thin film capacitor is arched in the direction from the first electrode layer 10 to the second electrode layer 20, the bending radius of the first conductive layer 11 is greater than the bending radius of the second conductive layer 12.
[0085] It should be noted that when the thin film capacitor is arched in the direction from the first electrode layer 10 to the second electrode layer 20, the arched part of the first flexible conductive layer 13 is subjected to greater pressure. Since the first flexible conductive layer 13 has a relatively small elastic modulus, its upper surface part (for example, the center) will be concave downward, and the first flexible conductive layer 13 absorbs part of the extrusion force generated by the deformation of the second conductive layer 12, and finally reduces the transmission of this extrusion force so that the bending radius of the second conductive layer 12 is smaller than the bending radius of the first conductive layer 11. That is to say, the second conductive layer 12 with a smaller bending radius has a greater bending degree, and the first conductive layer 11 with a larger bending radius has a smaller bending degree, which is beneficial to further improve the anti-cracking performance of the first conductive layer 11.
[0086] by Figure 3 For example, Figure 3 A schematic diagram of a usage state of a thin film capacitor in an embodiment of the present application is shown, wherein when the thin film capacitor is arched in the direction from the second electrode layer 20 to the first electrode layer 10, the bending radius of the first conductive layer 11 is greater than the bending radius of the second conductive layer 12.
[0087] Similarly, when the thin film capacitor is arched in the direction from the second electrode layer 20 to the first electrode layer 10, without considering other influencing factors, when the overall thickness formed by the second electrode layer 20, the dielectric layer 30 and the first conductive layer 11 is greater than the second conductive layer, its deformation resistance is stronger. At the same time, the elastic first flexible conductive layer 13 is filled between the first conductive layer 11 and the second conductive layer 12. Under the same external force, the bending degree of the second conductive layer 12 will be more serious, while the bending degree of the first conductive layer 11 will be lighter, thereby preventing the first conductive layer 11 from cracking.
[0088] It should be pointed out that the arch refers to the part of the corresponding film layer that is most severely bent. Figure 2 or Figure 3 For example, the film capacitor is arched at the center, and the arched part of the first flexible conductive layer 13 refers to the center of the first flexible conductive layer 13. It can be understood that the arched part of the first flexible conductive layer 13 can also refer to a region at a certain distance (e.g., 1 cm) between the first flexible conductive layer 13 and the center; or, the first flexible conductive layer 13 can also be set as a multi-layer structure, such as a first flexible conductive layer 13 composed of multiple layers of conductive paper, to further improve the anti-cracking performance of the first electrode layer 10.
[0089] In some embodiments of the present application, see Figure 4 , Figure 4 Another structural schematic diagram of the thin film capacitor in the embodiment of the present application is shown, wherein the first flexible conductive layer 13 includes a flexible frame 131 and liquid metal 132; the flexible frame 131 is bonded to the edge area of the first conductive layer 11 on one side facing the first conductive layer 11, and is bonded to the edge area of the second conductive layer 12 on one side facing the second conductive layer 12, and the liquid metal 132 is filled in the flexible frame 131.
[0090] It should be noted that since the two sides of the flexible frame 131 are respectively adhered to the first conductive layer 11 and the second conductive layer 12, the flexible frame 131, the first conductive layer 11 and the second conductive layer 12 enclose a closed space, and by filling the closed space with liquid metal 132, when the thin film capacitor bends and deforms so that the shape of the closed space changes, the fluidity of the liquid metal 132 will enable it to maintain contact with the first conductive layer 11 and the second conductive layer 12, thereby achieving the purpose of ensuring the electrical connectivity between the first conductive layer 11 and the second conductive layer 12.
[0091] Exemplarily, the flexible frame 131 may be a double-sided tape with adhesiveness, or a rubber frame bonded between the first conductive layer 11 and the second conductive layer 12 by glue; the liquid metal 132 may include one or more of gallium (Ga), gallium-indium alloy, gallium-indium-tin alloy, rubidium (Rb), cesium (Cs), and mercury (Hg).
[0092] Further, in some embodiments of the present application, continue to refer to Figure 5 , Figure 5 A schematic diagram of another usage state of the film capacitor in the embodiment of the present application is shown, wherein when the film capacitor is bent in an arch shape, the liquid metal 132 maintains close contact with the first conductive layer 11, and the liquid metal 132 maintains close contact with the second conductive layer 12.
[0093] It should be noted that the surfaces of the first conductive layer 11 and the second conductive layer 12 are uneven, have microscopic pits or microscopic protrusions, and directly contacting the first conductive layer 11 and the second conductive layer 12 will cause a tiny gap between the two, which is easy to cause a tip discharge phenomenon. In the above embodiment, taking the film capacitor as an example of an arched bend in the direction from the first electrode layer 10 to the second electrode layer 20, when the film capacitor is arched, due to the fluidity of the liquid metal 132, the liquid metal 132 will enter the microscopic pits on the surfaces of the first conductive layer 11 and the second conductive layer 12, so that the liquid metal 132 is in close contact with the first conductive layer 11, and the liquid metal 132 is in close contact with the second conductive layer 12, avoiding the tip discharge phenomenon caused by the tiny gap between the first flexible conductive layer 13 and the first conductive layer 11 or the first flexible conductive layer 13 and the second conductive layer 12.
[0094] It can be understood that a conductive liquid (such as an electrolyte solution) can also be filled in the enclosed space formed by the flexible frame 131, the first conductive layer 11 and the second conductive layer 12 to ensure electrical connectivity between the first conductive layer 11 and the second conductive layer 12 and avoid the generation of an interlayer gap between the first conductive layer 11 and the second conductive layer 12.
[0095] In some embodiments of the present application, for example, for embodiments in which the dielectric layer 30 is a finished film, see Figure 6 , Figure 6 Another structural schematic diagram of the thin film capacitor in the embodiment of the present application is shown, wherein the second electrode layer 20 includes a third conductive layer 21, a fourth conductive layer 22 and a second flexible conductive layer 23, and the second flexible conductive layer 23 is filled between the third conductive layer 21 and the fourth conductive layer 22; the thickness of the second flexible conductive layer 23 can change with the spacing between the corresponding parts of the third conductive layer 21 and the fourth conductive layer 22 to ensure the electrical connectivity between the third conductive layer 21 and the fourth conductive layer 22.
[0096] Similarly, since the second electrode layer 20 includes multiple conductive layers, when a crack occurs in a conductive layer of the second electrode layer, the phenomenon of such cracks being transmitted to each other can be avoided, thereby avoiding the occurrence of penetrating cracks in the second electrode layer 20 as much as possible. At the same time, the second flexible conductive layer 23 is filled between the third conductive layer 21 and the fourth conductive layer 22. Since the thickness of the second flexible conductive layer 23 can change with the spacing between the corresponding parts of the third conductive layer 21 and the fourth conductive layer 22, the electrical connectivity between the third conductive layer 21 and the fourth conductive layer 22 can be guaranteed, and the tip discharge phenomenon caused by the interlayer gap between the third conductive layer 21 and the fourth conductive layer 22 can be avoided.
[0097] In some embodiments of the present application, the material of the third conductive layer 21 can be one or a combination of Al, Ti, Au, Ag, Zn, Cu or Ni. In some embodiments of the present application, the third conductive layer 21 can be formed by spin coating or spray coating of non-metallic materials such as graphite and conductive silicon.
[0098] In some embodiments of the present application, in some embodiments of the present application, the thickness of the third conductive layer 21 is 1nm to 1000nm. Preferably, the thickness of the third conductive layer 21 is 10nm to 800nm. More preferably, the thickness of the third conductive layer 21 is 50nm to 300nm. Among them, the third conductive layer 21 meets the above size range and can have good flexibility, and can also prevent the third conductive layer 21 from being too thick and prone to cracks due to bending or being too thin and unable to completely cover the dielectric layer 30.
[0099] In some embodiments of the present application, the third conductive layer 21 can be formed on the side of the dielectric layer 30 away from the first electrode layer 10 by magnetron sputtering. During the magnetron sputtering process, the target material (such as aluminum or titanium) is sputtered by ion bombardment to produce target atoms or molecules with small diameters that can be deposited and enter the tiny pits on the surface of the dielectric layer 30, thereby compensating for the surface defects of the dielectric layer 30. In some embodiments of the present application, the third conductive layer 21 can also be formed on the side of the dielectric layer 30 away from the first electrode layer 10 by electron beam evaporation. During the electron beam evaporation process, accelerated electrons are used to bombard the coating material (such as zinc or gold), and the kinetic energy of the electrons is converted into heat energy to heat and evaporate the coating material, and finally the third conductive layer 21 is formed on the surface of the dielectric layer 30.
[0100] The fourth conductive layer 22 is a thin and flexible metal layer, such as a metal copper foil with a thickness of 0.1 mm to 1 mm, so that the fourth conductive layer 22 is flexible and easy to bend, thereby making the film capacitor bend as a whole and completely close to the skin surface of the human body. It can be understood that the fourth conductive layer 22 can also be made of other metal materials, such as metal silver foil.
[0101] In some embodiments of the present application, the fourth conductive layer 22 is preferably a stainless steel metal layer or a titanium metal layer, which can prevent the fourth conductive layer 22 from corrosion on the one hand, and block external water vapor from penetrating into the dielectric layer 30 inside the thin film capacitor on the other hand, thereby avoiding the dielectric layer 30 of the thin film capacitor from being broken down and damaged.
[0102] In some embodiments of the present application, the thickness of the fourth conductive layer 22 is 0.005 mm-1 mm. Preferably, the thickness of the fourth conductive layer 22 is 0.01-0.1 mm. More preferably, the thickness of the fourth conductive layer 22 is 0.01-0.05 mm. The thickness of the fourth conductive layer 22 meets the above range, which can ensure the flexibility of the fourth conductive layer 22 on the one hand, and prevent the fourth conductive layer 22 from being too thin and easy to crack on the other hand.
[0103] The second flexible conductive layer 23 has conductivity and a small elastic modulus, so that the second flexible conductive layer 23 electrically connects the fourth conductive layer 22 with the third conductive layer 21, ensuring the electrical connectivity between the fourth conductive layer 22 and the third conductive layer 21. Meanwhile, the small elastic modulus of the second flexible conductive layer 23 can avoid the phenomenon of tiny gaps between the fourth conductive layer 22 and the third conductive layer 21, thereby preventing the occurrence of tip discharge between the fourth conductive layer 22 and the third conductive layer 21.
[0104] Preferably, the second flexible conductive layer 23 may be conductive paper, so that the second flexible conductive layer 23 has higher tensile and tearing strength, and avoids the second flexible conductive layer 23 from being torn when the film capacitor is bent in contact with the human body surface. In some embodiments of the present application, the second flexible conductive layer 23 may also be a conductive elastomer, such as conductive rubber or conductive silicone.
[0105] In some embodiments of the present application, the third conductive layer 21 is bonded to the dielectric layer 30, the tensile index of the fourth conductive layer 22 is greater than the tensile index of the second flexible conductive layer 23, and the tensile index of the second flexible conductive layer 23 is greater than the tensile index of the third conductive layer 21, so that the third conductive layer 21 is protected by the second flexible conductive layer 23 and the fourth conductive layer 22 with a larger tensile index, which is beneficial to prevent the third conductive layer 21 from cracking.
[0106] In some embodiments of the present application, see Figure 7 , Figure 7 Another structural schematic diagram of the thin film capacitor in an embodiment of the present application is shown, wherein the second flexible conductive layer 23 includes a flexible frame 131 and liquid metal 132; the flexible frame 131 is bonded to the edge area of the third conductive layer 21 on one side facing the third conductive layer 21, and is bonded to the edge area of the fourth conductive layer 22 on one side facing the fourth conductive layer 22, and the liquid metal 132 is filled in the flexible frame 131.
[0107] It should be noted that since the two sides of the flexible frame 131 are respectively adhered to the third conductive layer 21 and the fourth conductive layer 22, the flexible frame 131, the third conductive layer 21 and the fourth conductive layer 22 enclose a closed space, and by filling the closed space with liquid metal 132, when the thin film capacitor bends and deforms so that the shape of the closed space changes, the fluidity of the liquid metal 132 will enable it to maintain contact with the third conductive layer 21 and the fourth conductive layer 22, thereby achieving the purpose of ensuring the electrical connectivity between the third conductive layer 21 and the fourth conductive layer 22.
[0108] At the same time, due to the fluidity of the liquid metal 132, the liquid metal 132 will enter the microscopic pits on the surfaces of the third conductive layer 21 and the fourth conductive layer 22, so that the liquid metal 132 maintains close contact with the third conductive layer 21, and the liquid metal 132 maintains close contact with the fourth conductive layer 22, thereby avoiding the tip discharge phenomenon caused by the appearance of tiny gaps between the second flexible conductive layer 23 and the third conductive layer 21 or the second flexible conductive layer 23 and the fourth conductive layer 22.
[0109] In some embodiments of the present application, the first conductive layer 11 can repair surface defects of the dielectric layer 30 facing away from the second electrode layer 20 to avoid the generation of tiny gaps between the dielectric layer 30 and the first conductive layer 11 and the resulting air gap ionization phenomenon.
[0110] It should be noted that no matter whether the dielectric layer 30 is formed on the second electrode layer 20 by solution preparation or finished film bonding, the surface of the dielectric layer 30 has surface defects, which refers to the uneven surface of the dielectric layer 30 (or the finished film of the dielectric layer 30) after it is formed.
[0111] In some embodiments of the present application, the first conductive layer 11 can be formed on the side of the dielectric layer 30 away from the second electrode layer 20 by magnetron sputtering. In the magnetron sputtering process, the target material (such as aluminum or titanium) is sputtered by ion bombardment to produce target atoms or molecules with small diameters that can be deposited and enter the tiny pits on the surface of the dielectric layer 30, thereby compensating for the surface defects of the dielectric layer 30. In some embodiments of the present application, the first conductive layer 11 can also be formed on the side of the dielectric layer 30 away from the second electrode layer 20 by electron beam evaporation. In the electron beam evaporation process, accelerated electrons are used to bombard the coating material (such as zinc or gold), and the kinetic energy of the electrons is converted into heat energy to heat and evaporate the coating material, and finally the first conductive layer 11 is formed on the surface of the dielectric layer 30.
[0112] In some embodiments of the present application, the first conductive layer 11 includes overlapping aluminum metal layers and zinc metal layers, and the aluminum metal layer is located between the zinc metal layer and the dielectric layer 30, that is, the aluminum metal layer first covers the dielectric layer 30, and then the zinc metal layer covers the aluminum metal layer. Since the aluminum metal layer has good ductility and conductive layer, the phenomenon of cracks in the aluminum metal layer when the thin film capacitor is bent can be avoided as much as possible; at the same time, the zinc metal layer has good calendering properties and stable chemical properties, which can protect the aluminum metal layer from oxidation and avoid cracks in the zinc metal layer as much as possible.
[0113] In some embodiments of the present application, for example, for an embodiment in which the first conductive layer 11 includes overlapping aluminum metal layers and zinc metal layers, when preparing the first conductive layer 11, an aluminum metal layer can be first formed on the surface of the dielectric layer 30 by magnetron sputtering, and then a zinc metal layer can be formed on the aluminum metal layer by magnetron sputtering.
[0114] In some embodiments of the present application, the first conductive layer 11 includes overlapping aluminum metal layers and gold (Au) metal layers, and the aluminum metal layer is located between the gold (Au) metal layer and the dielectric layer 30, so that the gold (Au) metal layer with more stable chemical properties protects the aluminum metal layer.
[0115] In some embodiments of the present application, the first conductive layer 11 includes an overlapping aluminum metal layer and a titanium metal layer, and the aluminum metal layer is protected by the titanium metal layer having stable chemical properties and high structural strength.
[0116] In some embodiments of the present application, the first conductive layer 11 includes overlapping titanium metal layers and gold (Au) metal layers, and the titanium metal layers with stable chemical properties and high structural strength are used to protect the gold (Au) metal layers.
[0117] In some embodiments of the present application, for example, the first conductive layer 11 includes an overlapping aluminum metal layer and a zinc metal layer, the thickness of the aluminum metal layer is 1 nm to 1000 nm, and the thickness of the zinc metal layer is 1 nm to 1000 nm.
[0118] It can be understood that the first conductive layer 11 can also be formed on the surface of the dielectric layer 30 by other physical vapor deposition methods, such as arc plasma plating, ion plating and molecular beam epitaxy, so as to compensate for the surface defects of the dielectric layer 30; or, the first conductive layer 11 can also include multiple metal layers of different materials (such as aluminum, silver, zinc, titanium and gold) or metal layers of the same material (such as aluminum).
[0119] In some embodiments of the present application, see Figure 8 , Figure 8 Another structural schematic diagram of a thin film capacitor in an embodiment of the present application is shown, wherein the thin film capacitor further includes a flexible substrate 40, and the second electrode layer 20 is attached to the flexible substrate 40. Preferably, the flexible substrate 40 is an insulating polyimide film so that the thin film capacitor is flexible and can be bent. In some embodiments of the present application, the flexible substrate 40 and the second electrode layer 20 form a flexible circuit board.
[0120] In some embodiments of the present application, see Fig. 9 , Fig. 9 Another structural schematic diagram of the film capacitor in the embodiment of the present application is shown, wherein the film capacitor further includes a conductive attachment layer 50 attached to the second conductive layer 12, and the conductive attachment layer 50 is flexible and sticky, so as to adhere to the surface of human skin through the conductive attachment layer 50, and minimize contact damage caused by mismatch between the film capacitor and soft tissue. Exemplarily, the conductive attachment layer 50 can be a conductive hydrogel or a conductive silicone gel.
[0121] Furthermore, in order to better implement the thin film capacitor in the embodiment of the present application, on the basis of the thin film capacitor, the present application also provides a method for preparing the thin film capacitor, see Fig.10 , Fig.10A schematic flow chart of a method for preparing a thin film capacitor in an embodiment of the present application is shown, wherein the method for preparing a thin film capacitor includes:
[0122] Step S901, providing a second electrode layer 20;
[0123] In some embodiments of the present application, the second electrode layer 20 may refer to a corresponding metal layer on a circuit board, for example, a portion of a copper foil area is exposed on the circuit board, and a dielectric layer 30 is formed in the copper foil area, and the power interface of the circuit board can conveniently connect the two poles of the power supply. Preferably, the circuit board may be a flexible circuit board, such as a flexible printed circuit board made of polyimide or polyester film as a substrate, so as to simplify the electrical connection structure of the film capacitor while making the film capacitor flexible and bendable.
[0124] Step S902, forming a dielectric layer 30 on the second electrode layer 20;
[0125] In some embodiments of the present application, the dielectric layer 30 may be a finished film. In some other embodiments of the present application, the dielectric layer 30 may be formed on a metal copper foil area of a circuit board by atomization.
[0126] Preferably, the material of the dielectric layer 30 may include one or more of poly(vinylidene fluoride-trifluoroethylene-chlorotrifluoroethylene), poly(vinylidene fluoride-trifluoroethylene-1-chlorofluoroethylene), poly(VDF-DB) (poly(vinylidene fluoride-diethylene glycol butyl ether)) or poly(vinylidene fluoride-trifluoroethylene-chlorotrifluoroethylene-chlorofluoroethylene).
[0127] Step S903, forming a first electrode layer 10 on the dielectric layer 30, wherein the first electrode layer 10 includes an overlapping first conductive layer 11, a second conductive layer 12 and a first flexible conductive layer 13, and the first flexible conductive layer 13 is filled between the first conductive layer 11 and the second conductive layer 12;
[0128] The thickness of the first flexible conductive layer 13 may vary with the distance between the first conductive layer 11 and the second conductive layer 12 at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer 11 and the second conductive layer 12 .
[0129] The first flexible conductive layer 13 has conductivity and a small elastic modulus, so that the first flexible conductive layer 13 electrically connects the second conductive layer 12 with the first conductive layer 11, ensuring the electrical connectivity between the second conductive layer 12 and the first conductive layer 11. Meanwhile, the small elastic modulus of the first flexible conductive layer 13 can avoid the phenomenon of tiny gaps between the second conductive layer 12 and the first conductive layer 11, and prevent the phenomenon of tip discharge between the second conductive layer 12 and the first conductive layer 11.
[0130] Preferably, the first flexible conductive layer 13 may be conductive paper, so that the first flexible conductive layer 13 has higher tensile and tearing strength, and avoids the first flexible conductive layer 13 from being torn when the film capacitor is bent in contact with the human body surface. In some embodiments of the present application, the first flexible conductive layer 13 may also be conductive rubber or conductive silicone.
[0131] In the embodiment of the present application, the present application sets the first electrode layer 10 as a multi-layer conductive layer. When a crack occurs in a certain conductive layer, the phenomenon of mutual transmission of such cracks can be avoided, thereby avoiding the occurrence of penetrating cracks in the first electrode layer 10 as much as possible. At the same time, the first flexible conductive layer 13 is filled between the first conductive layer 11 and the second conductive layer 12. Since the thickness of the first flexible conductive layer 13 can change with the spacing between the corresponding parts of the first conductive layer 11 and the second conductive layer 12, the electrical connectivity between the first conductive layer 11 and the second conductive layer 12 can be guaranteed, and the tip discharge phenomenon caused by the interlayer gap between the first conductive layer 11 and the second conductive layer 12 can be avoided.
[0132] Further, see Fig.11 , Fig.11 Another schematic diagram of a process for preparing a thin film capacitor in an embodiment of the present application is shown, wherein the process for preparing a thin film capacitor includes:
[0133] Step S1001, providing a second electrode layer 20;
[0134] Step S1002, forming a dielectric layer 30 on the second electrode layer 20;
[0135] Step S1003, forming a first conductive layer 11 on the dielectric layer 30;
[0136] Step S1004, forming a first flexible conductive layer 13 on the first conductive layer 11;
[0137] Step S1005 , forming a second conductive layer 12 on the first flexible conductive layer 13 .
[0138] In some embodiments of the present application, the first conductive layer 11 can be formed on the side of the dielectric layer 30 away from the second electrode layer 20 by magnetron sputtering. In some embodiments of the present application, the first conductive layer 11 can also be formed on the side of the dielectric layer 30 away from the second electrode layer 20 by electron beam evaporation. In some embodiments of the present application, for example, for an embodiment in which the first conductive layer 11 includes overlapping aluminum metal layers and zinc metal layers, when preparing the first conductive layer 11, an aluminum metal layer can be first formed on the surface of the dielectric layer 30 by magnetron sputtering, and then a zinc metal layer can be formed on the aluminum metal layer by magnetron sputtering.
[0139] In some embodiments of the present application, the first flexible conductive layer 13 can be directly formed on the first conductive layer 11 in a manner of being bonded to the first conductive layer 11. In some embodiments of the present application, the first flexible conductive layer 13 can be attached to the first conductive layer 11 by glue bonding. In some embodiments of the present application, the first conductive layer 11 is bonded to the dielectric layer 30, and the tensile index of the first flexible conductive layer 13 is greater than the tensile index of the first conductive layer 11.
[0140] In some embodiments of the present application, the second conductive layer 12 may be directly formed on the first flexible conductive layer 13 in a manner of being bonded to the first flexible conductive layer 13. In some embodiments of the present application, the second conductive layer 12 may be bonded to the first flexible conductive layer 13 by glue.
[0141] It can be understood that the above-mentioned method for preparing thin film capacitors is intended to clearly illustrate the implementation verification process of the present application. The method for preparing thin film capacitors can also be implemented in other alternative ways. For example, after the entire first electrode layer is formed, the first electrode layer is bonded to the dielectric layer to complete the process of forming the first electrode layer on the dielectric layer; for another example, the copper foil of the circuit board can be used as the second electrode layer; for another example, the first electrode layer can be formed first, and then the dielectric layer can be formed on the first electrode layer.
[0142] Furthermore, in order to better implement the film capacitor in the embodiment of the present application, on the basis of the film capacitor, the present application also provides a tumor treatment electrode patch, and the tumor treatment electrode patch includes a film capacitor as in any of the above embodiments. Since the tumor treatment electrode patch in the embodiment of the present application is provided with the film capacitor of the above embodiment, it has all the beneficial effects of the above film capacitor, which will not be described in detail here.
[0143] Furthermore, in order to better implement the tumor treatment electrode patch in the embodiment of the present application, on the basis of the tumor treatment electrode patch, the present application also provides a tumor treatment system, and the tumor treatment system includes the tumor treatment electrode patch as in any of the above embodiments. Since the tumor treatment system in the embodiment of the present application is provided with the film capacitor of the above embodiment, it has all the beneficial effects of the above film capacitor, which will not be described in detail here.
[0144] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, please refer to the detailed description of other embodiments above, and will not be repeated here.
[0145] The basic concepts have been described above. Obviously, for those skilled in the art, the above detailed disclosure is only for example and does not constitute a limitation of the present application. Although not explicitly stated herein, those skilled in the art may make various modifications, improvements and amendments to the present application. Such modifications, improvements and amendments are suggested in the present application, so such modifications, improvements and amendments still belong to the spirit and scope of the exemplary embodiments of the present application.
[0146] At the same time, the present application uses specific words to describe the embodiments of the present application. For example, "one embodiment", "an embodiment", and / or "some embodiments" refer to a certain feature, structure or characteristic related to at least one embodiment of the present application. Therefore, it should be emphasized and noted that "one embodiment" or "an embodiment" or "an alternative embodiment" mentioned twice or more in different positions in this specification does not necessarily refer to the same embodiment. In addition, some features, structures or characteristics in one or more embodiments of the present application can be appropriately combined.
[0147] Similarly, it should be noted that in order to simplify the description of the disclosure of this application and thus help understand one or more embodiments of the invention, in the above description of the embodiments of this application, multiple features are sometimes combined into one embodiment, figure or description thereof. However, this disclosure method does not mean that the features required by the object of this application are more than the features mentioned in the claims. In fact, the features of the embodiments are less than all the features of the single embodiment disclosed above.
[0148] In some embodiments, numbers describing the number of components and attributes are used. It should be understood that such numbers used in the description of the embodiments are modified by the modifiers "about", "approximately" or "substantially" in some examples. Unless otherwise specified, "about", "approximately" or "substantially" indicate that the numbers are allowed to vary by ±20%. Accordingly, in some embodiments, the numerical parameters used in the specification and claims are approximate values, which may change according to the required features of individual embodiments. In some embodiments, the numerical parameters should take into account the specified significant digits and adopt the general method of retaining digits. Although the numerical domains and parameters used to confirm the breadth of their range in some embodiments of the present application are approximate values, in specific embodiments, the setting of such numerical values is as accurate as possible within the feasible range.
[0149] Each patent, patent application, patent application publication, and other materials, such as articles, books, specifications, publications, documents, etc., cited in this application is hereby incorporated by reference in its entirety, except for application history documents that are inconsistent with or conflicting with the content of this application, and documents that limit the broadest scope of the claims of this application (currently or later attached to this application). It should be noted that if the descriptions, definitions, and / or use of terms in the accompanying materials of this application are inconsistent or conflicting with the content described in this application, the descriptions, definitions, and / or use of terms in this application shall prevail.
[0150] The above is a detailed introduction to a thin film capacitor for tumor treatment and its preparation method, a tumor treatment electrode patch, and a tumor treatment system provided in the embodiments of the present application. Specific examples are used in this article to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea; at the same time, for technical personnel in this field, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A film capacitor, characterized in that: include: a first electrode layer and a second electrode layer; a dielectric layer, the dielectric layer being located between the first electrode layer and the second electrode layer; The first electrode layer includes a first conductive layer, a second conductive layer and a first flexible conductive layer that overlap each other, and the first flexible conductive layer is filled between the first conductive layer and the second conductive layer; The thickness of the first flexible conductive layer may vary with the distance between the first conductive layer and the second conductive layer at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer and the second conductive layer.
2. The film capacitor according to claim 1, wherein: The first conductive layer is bonded to the dielectric layer; The tensile index of the second conductive layer is greater than that of the first flexible conductive layer, and the tensile index of the first flexible conductive layer is greater than that of the first conductive layer.
3. The film capacitor according to claim 2, characterized in that: The overall elastic modulus of the first electrode layer, the dielectric layer, and the first conductive layer, and the elastic modulus of the second conductive layer are greater than the elastic modulus of the first flexible conductive layer.
4. The film capacitor according to claim 3, characterized in that: When the thin film capacitor is curved in an arch shape, a bending radius of the first conductive layer is greater than a bending radius of the second conductive layer.
5. The film capacitor according to claim 1, wherein: The first flexible conductive layer includes conductive paper or conductive elastomer; preferably, the conductive elastomer is conductive silicone or conductive rubber.
6. The film capacitor according to claim 1, wherein: The first flexible conductive layer includes a flexible frame and liquid metal; The side of the flexible frame facing the first conductive layer is bonded to the edge region of the first conductive layer, and the side facing the second conductive layer is bonded to the edge region of the second conductive layer. The liquid metal is filled in the flexible frame.
7. The film capacitor according to claim 6, wherein: When the film capacitor is bent in an arch shape, the liquid metal is kept in close contact with the first conductive layer, and the liquid metal is kept in close contact with the second conductive layer.
8. The film capacitor according to claim 1, wherein: The second electrode layer includes a third conductive layer, a fourth conductive layer and a second flexible conductive layer, and the second flexible conductive layer is filled between the third conductive layer and the fourth conductive layer; The thickness of the second flexible conductive layer may be changed with the distance between the third conductive layer and the fourth conductive layer at corresponding positions to ensure electrical connectivity between the third conductive layer and the fourth conductive layer.
9. The film capacitor according to claim 1, wherein: The thickness of the first flexible conductive layer is 0.001 mm to 1 mm.
10. The film capacitor according to claim 1, wherein: The thickness of the first flexible conductive layer is 0.01 mm to 0.8 mm; preferably, the thickness of the first flexible conductive layer is 0.1 mm to 0.6 mm.
11. A method for preparing a thin film capacitor, characterized in that: include: providing a second electrode layer; forming a dielectric layer on the second electrode layer; forming a first electrode layer on the dielectric layer, wherein the first electrode layer comprises a first conductive layer, a second conductive layer and a first flexible conductive layer which are overlapped, and the first flexible conductive layer is filled between the first conductive layer and the second conductive layer; The thickness of the first flexible conductive layer may vary with the distance between the first conductive layer and the second conductive layer at corresponding positions, so as to ensure the electrical connectivity between the first conductive layer and the second conductive layer.
12. The preparation method according to claim 11, characterized in that: The first conductive layer is attached to the dielectric layer, the tensile index of the second conductive layer is greater than the tensile index of the first flexible conductive layer, and the tensile index of the first flexible conductive layer is greater than the tensile index of the first conductive layer.
13. A tumor treatment electrode patch, characterized in that: Comprising the film capacitor according to any one of claims 1 to 10.
14. A tumor treatment system, characterized in that: Comprising the tumor treatment electrode patch as described in claim 13.