Epitaxial wafer and edge defect detection method and device and processing method thereof

By acquiring area and brightness characteristics at the edge sampling position of the epitaxial wafer, and automatically judging defects, the problem of subjectivity and low efficiency of manual detection in the prior art is solved, and efficient and accurate edge defect detection is achieved.

CN119008446APending Publication Date: 2024-11-22XIAN ESWIN MATERIAL TECHNOLOGY CO LTD +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411209401.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, epitaxial wafer edge defect detection relies on manual judgment, and there are problems such as strong subjectivity, low accuracy and slow detection efficiency.

Method used

By acquiring the area and brightness characteristics of abnormal defects at multiple sampling positions on the edge of the epitaxial wafer, comparing and setting judgment conditions, automatically determining whether there is a target edge defect, and using a computing device to perform a detection method to improve detection accuracy and efficiency.

Benefits of technology

It provides an objective, accurate and efficient epitaxial wafer edge defect detection solution, which reduces manual participation, improves detection accuracy and efficiency, and avoids subjective judgment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008446A_ABST
    Figure CN119008446A_ABST
Patent Text Reader

Abstract

The invention provides an epitaxial wafer, an epitaxial wafer edge defect detection method, an epitaxial wafer edge defect detection device and an epitaxial wafer edge defect processing method. The detection method comprises the following steps: acquiring the area of an abnormal defect and the brightness characteristic of the abnormal defect at each sampling position in a plurality of sampling positions at the edge of an epitaxial wafer; comparing the area of the abnormal defect at each sampling position, the brightness characteristic of the abnormal defect and each sampling position with a set judgment condition; and when the sampling position meeting the judgment condition exists, determining that the epitaxial wafer has the target edge defect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor manufacturing technology, and in particular to a method and device for detecting defects of an epitaxial wafer and its edge, and a processing method thereof. Background Art

[0002] With the development of semiconductor technology, semiconductor devices tend to be increasingly miniaturized. The defects on the wafer have an increasingly greater impact on the semiconductor process. As the feature size continues to shrink, the device is closer to the edge of the wafer. The impact of wafer edge defects on the yield and performance of semiconductor devices is becoming more and more important.

[0003] At present, the detection methods of epitaxial wafer edge defects mostly rely on manual judgment by visual inspectors. However, manual judgment by visual inspectors is usually subjective; in addition, manual judgment by visual inspectors is slow and inefficient. Therefore, it is necessary to establish an objective, accurate and efficient epitaxial wafer edge defect detection solution. Summary of the invention

[0004] The present invention provides a method, device and processing method for detecting epitaxial wafers and edge defects thereof; provides an objective detection scheme for edge defects of epitaxial wafers, and also improves the detection accuracy and detection efficiency of edge defects of epitaxial wafers.

[0005] The technical solution of the present disclosure is achieved as follows: In a first aspect, the present disclosure provides a method for detecting edge defects of an epitaxial wafer, the method comprising: At a plurality of sampling positions at the edge of the epitaxial wafer, the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position are obtained; Comparing the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position with the set judgment conditions; When there is a sampling position that meets the determination condition, it is determined that the epitaxial wafer has a target edge defect.

[0006] In a second aspect, the present disclosure provides a device for detecting edge defects of an epitaxial wafer, the device comprising: an acquisition unit, a comparison unit and a determination unit; wherein: The acquisition unit is configured to acquire the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position among multiple sampling positions at the edge of the epitaxial wafer; The comparison unit is configured to compare the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position with the set determination condition; The determination unit is configured to determine that a target edge defect exists in the epitaxial wafer when there is a sampling position that meets the determination condition.

[0007] In a third aspect, the present disclosure provides a computing device, comprising: a processor and a memory; the processor is used to execute instructions stored in the memory to implement the method for detecting edge defects of epitaxial wafers as described in the first aspect.

[0008] In a fourth aspect, the present disclosure provides a computer storage medium, wherein the storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the method for detecting edge defects of epitaxial wafers as described in the first aspect.

[0009] In a fifth aspect, the present disclosure provides a method for processing an epitaxial wafer, the method comprising: Inspecting the epitaxial wafer using the method for detecting edge defects of the epitaxial wafer described in the first aspect; When the detection result indicates that the epitaxial wafer does not have the target edge defect, the epitaxial wafer is subsequently processed according to a set process flow.

[0010] In a sixth aspect, the present disclosure provides an epitaxial wafer, which is obtained by the processing method described in the fifth aspect, and the epitaxial wafer is determined to have no target edge defects through the edge defect detection method of the epitaxial wafer described in the first aspect.

[0011] The present invention provides a method, device and processing method for detecting epitaxial wafers and their edge defects; by utilizing the abnormal defect area, image features and position at each sampling position on the edge of the epitaxial wafer to detect whether a target edge defect exists, it not only provides an objective detection scheme for the edge defects of the epitaxial wafer, but also improves the detection accuracy and efficiency of the edge defects of the epitaxial wafer. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Schematic top view of an epitaxial growth apparatus provided for the present disclosure.

[0013] Figure 2 A schematic diagram of the structure of a processing chamber for performing an epitaxial deposition process provided by the present disclosure.

[0014] Figure 3 A schematic flow chart of a method for detecting edge defects of an epitaxial wafer provided in the present invention.

[0015] Figure 4 A surface schematic diagram of an epitaxial wafer provided in the present disclosure.

[0016] Figure 5A cross-sectional view of an edge portion of an epitaxial wafer provided by the present disclosure in a height direction.

[0017] Figure 6 A schematic diagram of the relative position of an edge of a wafer and a support of a Loadlock chamber provided in the present invention.

[0018] Figure 7 A schematic diagram of the relative position of another edge of a wafer and a support of a Loadlock chamber provided in the present invention.

[0019] Figure 8 A detailed schematic diagram of a method for detecting edge defects of an epitaxial wafer provided in the present invention.

[0020] Fig. 9 A schematic diagram of the structure of an edge detection device provided by the present invention.

[0021] Fig.10 An image at a sampling location provided by the present disclosure.

[0022] Fig.11 An image at another sampling location provided by the present disclosure.

[0023] Fig.12 A schematic diagram of the composition of an epitaxial wafer edge defect detection device provided in the present invention.

[0024] Fig.13 A schematic diagram of another device for detecting edge defects of epitaxial wafers provided in the present invention.

[0025] Fig.14 A schematic diagram of the structure of a computing device provided by the present disclosure. DETAILED DESCRIPTION

[0026] The technical solutions in the present disclosure will be described clearly and completely below in conjunction with the accompanying drawings in the present disclosure.

[0027] See also Figure 1 , which shows a schematic top view of an epitaxial growth device 100 applicable to the technical solution of the embodiment of the present disclosure. The epitaxial growth device 100 generally includes: a factory interface (Factory Interface) 102, load lock (Loadlock) chambers 104, 106, a transfer chamber (Transfer chamber) 108, and a process chamber (Process chamber) 120, 122. Figure 1As shown, wafers in the epitaxial growth apparatus 100 (shown as gray circles in the figure) can be processed in various chambers and transferred between various chambers (shown as solid arrows and dashed arrows in the figure) without being exposed to the surrounding environment outside the epitaxial growth apparatus 100. For example, wafers can be processed in various chambers under low pressure (e.g., less than or equal to about 300 Torr) or vacuum environments or transferred between these various chambers without destroying the low pressure or vacuum environment between various processes performed on these wafers in the epitaxial growth apparatus 100. Figure 1 As shown, the epitaxial growth device 100 has more than one processing chamber, and can perform the epitaxial deposition process of multiple wafers in one batch, thereby improving the production efficiency of epitaxial wafers.

[0028] exist Figure 1 In the example shown, the factory interface 102 includes a docking station 140. The epitaxial growth apparatus 100 also includes a plurality of front opening unit (FOUP) 144 adapted to the docking station 140. In some examples, the epitaxial growth apparatus 100 can be operated by a robot ( Figure 1 ), the wafer can be transferred from the front-opening standard cabin 144 to the docking station 140, and then transferred from the docking station 140 to the load lock chambers 104, 106.

[0029] The load lock chambers 104, 106 have respective ports coupled to the factory interface 102 and respective ports coupled to the transfer chamber 108. The transfer chamber 108 further has respective ports coupled to the process chambers 120, 122. In some examples, the ports may be slit openings with slit valves that can be connected to the process chambers 120, 122 by a robot ( Figure 1 The ports are used to allow wafers to pass through the ports and to provide sealing between the corresponding chambers to prevent gas from passing between the corresponding chambers. Generally speaking, in order to transfer a wafer through any port, the port is open; otherwise, the port is closed.

[0030] The load lock chambers 104, 106, the transfer chamber 108, and the processing chambers 120, 122 may be fluidly coupled to a gas and pressure control system ( Figure 1106). The gas and pressure control system may include one or more gas pumps (e.g., a turbo pump, a cryopump, a roughing pump, etc.), a gas source, various valves, and conduits fluidly coupled to various chambers. In operation, a robot of the factory interface 102 transfers a wafer from the FOUP 144 through a port to the load lock chamber 104 or 106. The gas and pressure control system then pumps down the load lock chamber 104 or 106. The gas and pressure control system further maintains the transfer chamber 108 at an internal low pressure or vacuum environment (which may include an inert gas). Thus, the pumping down of the load lock chamber 104 or 106 facilitates the passage of substrates between, for example, the atmospheric environment of the factory interface 102 and the low pressure or vacuum environment of the transfer chamber 108.

[0031] When the wafer is in the already evacuated load lock chamber 104 or 106, the robot transfers the wafer from the load lock chamber 104 or 106 through the port into the transfer chamber 108. The robot can then transfer the wafer to the processing chamber 120, 122 for processing.

[0032] The processing chamber 120 can be any suitable chamber for processing wafers. In some examples, the processing chamber 120 can be used to perform a cleaning process, or to perform an etching process, or to perform a respective epitaxial growth process. In some examples, see Figure 2 , a processing chamber 120 for performing an epitaxial deposition process includes: a susceptor 10 and a susceptor support frame 20A. The susceptor 10 is capable of horizontally supporting a wafer W. The susceptor support frame 20A is capable of driving the susceptor 10 to rotate around a central axis X at a certain speed during vapor deposition. During the rotation of the susceptor 10, the wafer W rotates around the central axis X together with the susceptor 10. Specifically, the wafer W remains stationary relative to the susceptor 10, and a small gap G is provided between the radial edge of the susceptor 10 and an adjacent component 10A (e.g., a preheating ring).

[0033] The chamber RC is enclosed by an upper bell jar 30A and a lower bell jar 30B, and the chamber RC accommodates a base 10 and a base support frame 20A. The upper bell jar 30A and the lower bell jar 30B can be made of transparent quartz, for example. The base 10 divides the chamber RC into an upper reaction chamber RC1 and a lower reaction chamber RC2. The wafer W is accommodated in the upper reaction chamber RC1. The gas pressure in the upper reaction chamber RC1 is slightly greater than the gas pressure in the lower reaction chamber RC2 so that the gas in the upper reaction chamber RC1 enters the lower reaction chamber RC2 through the gap G.

[0034] An air inlet 40 and an exhaust port 50 are formed on the left and right sides of the chamber RC, respectively. Specifically, the air inlet 40 is used to transport reaction gases, such as silicon source gas, carrier gas and dopant gas, into the upper reaction chamber RC1. Silicon atoms are generated by the reaction of the silicon source gas and the carrier gas and deposited on the wafer W to form an epitaxial layer on the surface of the wafer W by vapor deposition. The epitaxial layer of the wafer W is doped with a dopant gas to obtain a desired resistivity. For example, chlorosilane-based gases such as trichlorosilane SiHCl3 or dichlorosilane SiH2Cl2 are used as silicon source gases. Hydrogen H2 is used as a carrier gas. Gases with doping elements such as diborane B2H6 or phosphine PH3 are used as dopant gases. The exhaust port 50 is used to discharge the reaction exhaust gas out of the chamber RC.

[0035] In order to grow an epitaxial layer on the wafer W, the reaction gas (silicon source gas and carrier gas) is driven to flow along the upper surface of the wafer W, and the wafer W supported by the susceptor 10 is heated to about 1000° C. to 1200° C. To this end, heat sources providing a high temperature reaction environment are respectively arranged above and below the chamber RC. Figure 1 As shown, the heat source may use a plurality of heating bulbs 60, such as infrared lamps or far infrared lamps. The plurality of heating bulbs 60 are disposed on the periphery of the upper bell jar 30A and the lower bell jar 30B to heat the susceptor 10 and the wafer W by radiant heat from above and below the chamber 2 through the upper bell jar 30A and the lower bell jar 30B.

[0036] exist Figure 2 In the processing chamber 120 shown, a wafer support rod 80A and a wafer support rod carrier 90 arranged directly below the wafer support rod 80A are also provided. Before vapor deposition, the upper bell jar 30A is opened. The wafer W is transferred from the transfer chamber 108 to the wafer support rod 80A by a robot manipulator (not shown in the figure). Then, the wafer support rod 80A is driven down by the descent of the wafer support rod carrier 90, so that the wafer W is loaded into the base 10. Finally, the upper bell jar 30A is closed to complete the process of moving the wafer to the inside of the chamber RC. After completing the process of moving the wafer to the inside of the chamber RC, vapor deposition is performed. After the vapor deposition is completed, the upper bell jar 30A is opened. The wafer support rod 80A is driven up by the rise of the wafer support rod carrier 90 to lift the epitaxial wafer from the base 10. Finally, the epitaxial wafer is moved from the inside of the chamber RC to the transfer chamber 108 by the robot manipulator. In addition, in Figure 2 The illustrated processing chamber 120 further includes a mounting member 70 for assembling various components of the processing chamber 120 .

[0037] In conjunction with the above-mentioned examples of the epitaxial growth device 100 and the processing chamber 120, when performing an epitaxial process, such as a vapor deposition process, and during the transmission process of each chamber of the epitaxial growth device 100, surface defects such as mechanical damage, particle defects, haze defects, scratch defects, etc. are usually formed on the surface of the epitaxial wafer. In addition, during the vapor deposition process, epitaxial stacking faults (ESF, Epitaxy Stacking Fault) and the like are also formed. Among the exemplary defects of the wafer described above, the types of defects that epitaxial wafers usually face include ESF defects, Particle defects, Scratch defects, etc.

[0038] During the epitaxial process and the transmission process, the above defects may also appear on the edge of the epitaxial wafer. As the impact of wafer edge defects on the yield and performance of semiconductor devices becomes increasingly greater, the edge defect detection of epitaxial wafers is also worthy of more attention. At present, the use of manual visual inspection to detect edge defects will have problems such as strong subjectivity, low accuracy and detection efficiency, and slow detection speed. In order to solve the above problems and improve the detection accuracy and detection efficiency of edge defects of epitaxial wafers, the present disclosure provides a method for detecting edge defects of epitaxial wafers, see Figure 3 , the detection method may include steps S310 to S330.

[0039] In step S310 , at a plurality of sampling positions at the edge of the epitaxial wafer, the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position are obtained.

[0040] For example, see Figure 4 The schematic diagram of the surface of the epitaxial wafer shown in FIG. 1 shows a region of 3-5 mm from the periphery of the wafer 1 toward the center O of the wafer. Figure 4 The circular area between the dotted circle and the solid circle is defined as the edge portion 7 of the wafer 1. In some examples, the present disclosure can select the plurality of sampling positions (Lo) at equal intervals according to the set sampling angle at the edge portion 7 of the epitaxial wafer 1. For example, Figure 4 As shown, the line connecting the notch of the wafer and the center O is used as a reference, and counterclockwise rotation is performed successively according to the set sampling angle θ, so as to obtain multiple uniformly distributed sampling positions. In some examples, the set angle θ can be 5 degrees, 10 degrees, 15 degrees, 20 degrees, etc.

[0041] For any exemplary sampling position in the edge portion 7, its cross-sectional view in the wafer height direction is as follows: Figure 5 As shown, in Figure 5In the figure, in addition to the upper surface 2 and the lower surface 3 which are consistent with the radial direction of the wafer 1, the wafer 1 also includes an edge portion 7 which is composed of a chamfered surface 4 on the upper surface side, a chamfered surface 5 on the lower surface side, and an edge surface 6. At this exemplary sampling position, for the edge portion 7, the chamfered surface 4 on the upper surface side and the chamfered surface 5 on the lower surface side are inclined relative to the upper surface 2 and the lower surface 3, and the edge surface 6 is the portion of the edge portion 7 other than the chamfered surface 4 on the upper surface side and the chamfered surface 5 on the lower surface side, and is perpendicular to the upper surface 2 and the lower surface 3. The edge surface 6 may also be a slightly curved surface. The boundaries between the chamfered surface 4 on the upper surface side and the chamfered surface 5 on the lower surface side and the edge surface 6 are as shown in FIG. Figure 5 As shown, it is usually smoothly formed.

[0042] For step S310, specifically, at each sampling position of the edge part, an image at each sampling position is collected by the edge detection device of the wafer, and the image is an image including the chamfered surface 4 on the upper surface side, the chamfered surface 5 on the lower surface side, and the edge surface 6. By analyzing the image, it is known whether there is an abnormal defect at each sampling position, and when an abnormal defect exists, the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect are obtained.

[0043] In step S320, the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position are compared with the set determination conditions.

[0044] It should be noted that at any sampling position, the area of ​​the abnormal defect is used to characterize the size of the range covered by the abnormal defect at the sampling position. The brightness characteristics of the abnormal defect are used to characterize the severity of the abnormal defect at the sampling position. This is because the brightness characteristics of a normal defect-free wafer surface are usually close to bright white, while defects on the wafer surface will reduce the brightness, and the degree of brightness reduction is positively correlated with the severity of the defect. The sampling position can determine whether the position is in contact with a component or part in the epitaxial growth device 100 during the epitaxial process.

[0045] In the present disclosure, corresponding determination conditions are set for the above three parameter values, and it is possible to confirm whether the abnormal defect at the sampling position is a target edge defect by setting the determination conditions. In some examples, when a target edge defect exists, the epitaxial wafer can be identified as NG, and the epitaxial wafer identified as NG is scrapped.

[0046] In some examples, the determination conditions corresponding to the above three parameter values ​​may be: The area of ​​the abnormal defect at each sampling position is greater than the set area threshold. The brightness characteristic of the abnormal defect at each sampling position is less than the set brightness threshold. Each sampling position is a set target position. In the present disclosure, the target position is a position of the epitaxial wafer corresponding to a support of a loadlock chamber 104 during an epitaxial process.

[0047] For the above example, specifically, by setting the area threshold, it can be confirmed whether the size of the range covered by the abnormal defect is too large, by setting the brightness threshold, it can be confirmed whether the abnormal defect is too serious, and by setting the target position, it can be determined whether the abnormal defect is caused by contact with components or parts in the epitaxial growth equipment 100.

[0048] It should be noted that during the epitaxial process, the wafer Figure 1 The epitaxial growth device 100 shown in the figure is transferred, transported and processed in each chamber. The defects caused by the edge of the epitaxial wafer are related to whether there is interference with the four support pins A, B, C, and D in the loadlock chamber 104. In detail, when the wafer 1 is in a normal position in the loadlock chamber 104, the center of the wafer 1 coincides with the center of the carrier 1044 of the loadlock chamber 104. At this time, the relative position of the edge of the wafer 1 and the support pins is as shown in FIG. Figure 6 As shown, in this case, the edge of the wafer 1 does not interfere with any of the four supports, so there will be no defects on the edge of the wafer 1. If the wafer 1 deviates in the loadlock chamber 104, it will interfere with the supports, such as Figure 7 As shown, taking the case where the wafer 1 is offset toward the direction of the supports C and D as an example, scratches or particles will be generated on the edge of the wafer 1 at the positions corresponding to the supports C and D. In detail, if the interference phenomenon is relatively mild, particles will be generated at the corresponding positions of the edge, and the particles will form stacking fault (ESF) defects after the epitaxial deposition process. If the interference phenomenon is more serious, a scratch defect will be generated at the corresponding position of the edge, and the scratch defect will still remain after the epitaxial deposition process. Based on this, in the present disclosure, the target position is set to the corresponding position of the support in the loadlock chamber 104, so whether the abnormal defect on the edge is caused by the above-mentioned interference phenomenon can be judged based on whether the sampling position is the target position.

[0049] In step S330 , when there is a sampling position that meets the determination condition, it is determined that the epitaxial wafer has a target edge defect.

[0050] In the present disclosure, when the above three parameter values ​​at any sampling position of the epitaxial wafer meet the set judgment conditions, it means that the abnormal defect of the epitaxial wafer at the sampling position is a target edge defect. Based on the target edge defect, the technical solution of the present disclosure identifies the epitaxial wafer as NG, and the epitaxial wafer identified as NG is scrapped.

[0051] In addition, as the epitaxial production continues, the above-mentioned determination conditions also need to be continuously updated. Based on this, in some examples, the method for detecting edge defects of epitaxial wafers provided in the present disclosure may also include: When the epitaxial wafer has a target edge defect, the type of the target edge defect is detected by a scanning electron microscope, and the determination condition is updated according to the detection result.

[0052] For the above example, specifically, for epitaxial wafers identified as NG, a scanning electron microscope (SEM) can be used to further perform morphological defect analysis, and the type of the target edge defect can be determined through analysis. In addition, the judgment conditions can be updated using the data in the analysis process, thereby further improving the accuracy of subsequent edge defect detection. It can be understood that the process of morphological defect analysis by SEM in this example can be performed manually, but compared to the related schemes that use manual visual inspection to perform a complete edge defect detection process, the scheme provided by the present disclosure still reduces manual participation, avoids subjective judgment, and improves the detection accuracy and efficiency of edge defects of epitaxial wafers.

[0053] Through the above technical scheme, the abnormal defect area, image features and position at each sampling position on the edge of the epitaxial wafer are used to detect whether there is a target edge defect, which not only provides an objective detection scheme for the edge defects of the epitaxial wafer, but also improves the detection accuracy and efficiency of the edge defects of the epitaxial wafer.

[0054] Based on the above technical solution, see Figure 8 , which shows a detailed process of a method for detecting edge defects of an epitaxial wafer provided by the present disclosure, and the detailed process can be used as the aforementioned Figure 3 A specific implementation example of the solution shown, the detailed process may include: S801: Acquire multiple sampling positions at an angle interval of 5 degrees on the edge of the epitaxial wafer to be measured.

[0055] In the present disclosure, Figure 4 As shown, the line connecting the notch of the wafer and the center O can be used as a reference, and 5 degrees can be used as a sampling angle θ to rotate counterclockwise successively, so as to obtain multiple uniformly distributed sampling positions.

[0056] S802: Collect an image at each sampling position using a wafer edge detection device.

[0057] Exemplarily, the structure of the edge detection device is shown as follows: Fig. 9 As shown, in Fig. 9 In the embodiment, the epitaxial wafer W to be tested is placed flat on a supporting platform 10 that can rotate around a central axis C, and the rotation of the epitaxial wafer W to be tested is controlled so that the laser emitter 20 emits a laser beam Laser to each sampling position. The scanning camera 30 collects the reflected light or refracted light of the laser beam at each sampling position (as shown by the dotted arrows) to collect the image at each sampling position and transmit it to the computing device 40. In the present disclosure, the computing device 40 can execute the technical solution of the present disclosure according to the collected image at each sampling position, so as to detect the edge defects of the epitaxial wafer.

[0058] S803: For each image at the sampling position, obtain the minimum enclosing area containing the abnormal defect.

[0059] For example, the images collected by the above step S802 are respectively as follows: Fig.10 and Fig.11 As shown, in Fig.10 and Fig.11 In FIG. 1 , the defects of the upper surface chamfered surface 4, the edge surface 6, and the lower surface chamfered surface 5 are combined from top to bottom. Fig.10 and Fig.11 In , for each abnormal defect at the sampling position, the minimum enclosing area of ​​the abnormal defect is obtained, such as Fig.10 The rectangular frame 1 shown in FIG. Fig.11 In the middle are the rectangular boxes 1 and 2. Fig.10 and Fig.11 It can be seen that these rectangular frames can enclose the abnormal defects and have the smallest size. Therefore, the area covered by these rectangular frames is the minimum enclosing area containing the abnormal defects described in this step.

[0060] S804: Determine the area of ​​the minimum enclosing region as the area of ​​the abnormal defect.

[0061] For example, the morphology of an abnormal defect is usually irregular, and the area of ​​the abnormal defect cannot be directly calculated. In the present disclosure, since the minimum enclosing area can completely enclose the abnormal defect and has the smallest size, there is a positive correlation between the area of ​​the minimum enclosing area and the area of ​​the abnormal defect. Based on this, the present disclosure regards the area of ​​the area as the area of ​​the abnormal defect it encloses, thereby facilitating the calculation of the area of ​​the abnormal defect.

[0062] S805: Determine the grayscale average value of all pixels in the minimum enclosing area as the brightness feature of the abnormal defect.

[0063] Exemplarily, in the present disclosure, the brightness feature is characterized by grayscale value, and the larger the grayscale value of a pixel, the brighter the brightness of the pixel. In the present disclosure, the brightness feature of the abnormal defect is characterized by the mean of the grayscale values ​​in the area covered by the abnormal defect. For the same reason as the example described in the aforementioned step S804, the size of the area covered by the abnormal defect is positively correlated with the size covered by the minimum enclosing area of ​​the abnormal defect. Based on this, the present disclosure regards the grayscale average value of all pixels in the minimum enclosing area as the brightness feature of the abnormal defect.

[0064] It should be noted that, through the above steps, after obtaining each sampling position and the area and brightness characteristics of the abnormal defects at each sampling position, it is possible to make a judgment based on the judgment conditions described in the aforementioned technical solution to determine whether the epitaxial wafer to be tested is judged to be NG. It can be understood that there are a total of 3 judgment conditions, and the judgment order in the specific implementation process can be selected according to the actual situation. In this detailed process, subsequent steps S806 to S808 are judged for these three judgment conditions respectively, and the execution order can also be selected according to the actual situation. This disclosure does not make specific limitations on this.

[0065] S806: Determine whether the area of ​​the abnormal defect at each sampling position is greater than a set area threshold.

[0066] In the specific implementation process, a three-digit binary value is set for each sampling position, and these three digits correspond to the judgment results of S806, S807 and S808 respectively. For example, the binary value corresponding to the sampling position Lo is X1X2X3, X1 represents the judgment result of step S806, X2 represents the judgment result of S807, and X3 represents the judgment result of step S808. When the area of ​​the abnormal defect at the sampling position Lo is greater than the area threshold, X1 takes the value of 1, otherwise, X1 takes the value of 0. In detail, combined with the aforementioned step S804, that is, when the area of ​​the minimum enclosing area of ​​the abnormal defect at the sampling position Lo is greater than the area threshold, X1 takes the value of 1, otherwise, X1 takes the value of 0.

[0067] S807: Determine whether the brightness feature of the abnormal defect at each sampling position is less than a set brightness threshold.

[0068] In the specific implementation process, combined with the aforementioned exemplary sampling position Lo, when the brightness feature of the abnormal defect at the sampling position Lo is less than the area brightness threshold, X2 takes a value of 1, otherwise, X2 takes a value of 0. In detail, combined with the aforementioned step S805, that is, when the grayscale average value of all pixels in the minimum enclosing area of ​​the abnormal defect at the sampling position Lo is less than the grayscale threshold, X2 takes a value of 1, otherwise, X2 takes a value of 0.

[0069] S808: Determine whether each sampling position is a set target position.

[0070] In the present disclosure, in combination with the aforementioned technical solution, the target position is the position of the epitaxial wafer to be tested corresponding to the support of the load lock chamber during the epitaxial process.

[0071] In a specific implementation, in combination with the above exemplary sampling position Lo, when the sampling position Lo is a position corresponding to the support member of the load lock chamber, X3 takes a value of 1, otherwise, X3 takes a value of 0. Figure 6 and Figure 7 For example, the angles of the support pins A, B, C, and D corresponding to the wafer 1 are 75°, 105°, 255°, and 285°, respectively. That is, based on the line connecting the notch of the wafer and the center O, when the sampling position Lo is at the above angle on the wafer surface, it can be considered that the sampling position is at a position corresponding to the support pin of the load lock chamber.

[0072] It should be noted that in Figure 8 In the technical solution shown, steps S806 to S808 can be used as Figure 3 A specific implementation method of step S320 in the illustrated scheme.

[0073] S809: Determine whether there is a sampling position where all the judgment conditions are yes; if there is a sampling position where all the judgment conditions are yes, execute step S810: determine whether the epitaxial wafer to be tested has a target edge defect, and rate the epitaxial wafer to be tested as NG. Continue to execute step S811. Otherwise, execute step S812.

[0074] Combined with the specific implementation process in the aforementioned steps S806 to S808, taking the sampling position Lo as an example, when the corresponding binary value X1X2X3 is 111, the sampling position Lo is determined to be a sampling position where all the judgment conditions are yes, thereby determining that the epitaxial wafer to be tested has a target edge defect, and based on the target edge defect, the epitaxial wafer to be tested is rated as NG, and the epitaxial wafer to be tested is scrapped. . The comparison result corresponding to the judgment condition may include: the area of ​​the abnormal defect at the sampling position is greater than the set area threshold; the brightness feature of the abnormal defect at the sampling position is less than the set brightness threshold; the sampling position is at the target position.

[0075] In the present disclosure, when no corresponding binary value is 111 in all sampling positions, S812 is executed.

[0076] S811: Detect the type of target edge defects in the epitaxial wafer to be tested by a scanning electron microscope, and update the determination conditions according to the detection results.

[0077] In a specific implementation process, the area threshold and the brightness threshold can be updated according to the detection results, so as to improve the accuracy of subsequent edge defect detection.

[0078] S812: When there is no sampling position where all the determination conditions are yes, the epitaxial wafer to be tested is subsequently processed according to the set process flow.

[0079] In the present disclosure, in a specific implementation process, when the epitaxial wafer to be tested has a sampling position where all the judgment conditions are yes, the epitaxial wafer to be tested is judged as NG and scrapped. When the epitaxial wafer to be tested does not have a sampling position where all the judgment conditions are yes, it means that the epitaxial wafer to be tested meets the specification requirements and can be processed in the subsequent process according to the process flow.

[0080] See also Fig.12 , which shows a device 120 for detecting edge defects of an epitaxial wafer provided by the present disclosure, the device 120 comprises: an acquisition unit 1201, a comparison unit 1202 and a determination unit 1203; wherein, The acquisition unit 1201 is configured to acquire the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position among multiple sampling positions at the edge of the epitaxial wafer; The comparison unit 1202 is configured to compare the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position with the set determination condition; The determination unit 1203 is configured to determine that the epitaxial wafer has a target edge defect when there is a sampling position that meets the determination condition.

[0081] In some examples, the acquisition unit 1201 is configured to: Acquire an image at each sampling position; The area of ​​the abnormal defect and the brightness characteristics of the abnormal defect are obtained in the image.

[0082] In some examples, the acquisition unit 1201 is configured to: In the image, obtaining a minimum enclosing area containing an abnormal defect; Determining the area of ​​the minimum enclosing region as the area of ​​the abnormal defect; The grayscale average value of all pixels in the minimum enclosing area is determined as the brightness feature of the abnormal defect.

[0083] In some examples, the comparison unit 1202 is configured to: Determining whether the area of ​​the abnormal defect at each sampling position is greater than a set area threshold; Determining whether the brightness characteristic of the abnormal defect at each sampling position is less than a set brightness threshold; Determine whether each sampling position is a set target position; wherein the target position is a position of the epitaxial wafer corresponding to a support of a load lock chamber during an epitaxial process.

[0084] In some examples, the determining unit 1203 is configured to: When there is a sampling position among all the sampling positions that simultaneously satisfies the set comparison result, it is determined that the epitaxial wafer has a target edge defect; wherein the comparison result includes: the area of ​​the abnormal defect at the sampling position is greater than the set area threshold; the brightness feature of the abnormal defect at the sampling position is less than the set brightness threshold; the sampling position is at the target position.

[0085] For some examples, see Fig.13 The device 120 further includes a detection unit 1204 configured to: When the epitaxial wafer has a target edge defect, the type of the target edge defect is detected by a scanning electron microscope, and the determination condition is updated according to the detection result.

[0086] In some examples, the acquisition unit 1201 is further configured to: The plurality of sampling positions are selected at equal intervals on the edge of the epitaxial wafer according to a set sampling angle.

[0087] Please refer to Fig.14 , which shows a structural block diagram of a computing device provided by an exemplary embodiment of the present disclosure. In some examples, the computing device 1400 can be at least one of a smart phone, a smart watch, a desktop computer, a laptop, a virtual reality terminal, an augmented reality terminal, a wireless terminal, and a laptop portable computer. The computing device 1400 has a communication function and can access a wired network or a wireless network. The computing device 1400 can generally refer to one of a plurality of terminals, and those skilled in the art can know that the number of the above terminals can be more or less. In some examples, the computing device 1400 can receive data based on the wired network or wireless network to which it is connected. It can be understood that the computing device 1400 undertakes the calculation and processing work of the technical solution of the present disclosure, and the present disclosure does not limit this.

[0088] like Fig.14 As shown, the computing device in the present disclosure may include one or more of the following components: a processor 1410 and a memory 1420 .

[0089] Optionally, the processor 1410 uses various interfaces and lines to connect various parts within the entire computing device, and executes various functions of the computing device and processes data by running or executing instructions, programs, code sets or instruction sets stored in the memory 1420, and calling data stored in the memory 1420. Optionally, the processor 1410 can be implemented in at least one hardware form of digital signal processing (DSP), field-programmable gate array (FPGA), and programmable logic array (PLA). The processor 1410 can integrate one or a combination of a central processing unit (CPU), a graphics processing unit (GPU), a neural network processor (NPU), and a baseband chip. Among them, the CPU mainly processes the operating system, user interface, and application programs; the GPU is responsible for rendering and drawing the content that needs to be displayed on the touch display; the NPU is used to implement artificial intelligence (AI) functions; and the baseband chip is used to process wireless communications. It is understandable that the above-mentioned baseband chip may not be integrated into the processor 1410, but may be implemented by a separate chip.

[0090] The memory 1420 may include a random access memory (RAM) or a read-only memory (ROM). Optionally, the memory 1420 includes a non-transitory computer-readable storage medium. The memory 1420 may be used to store instructions, programs, codes, code sets, or instruction sets. The memory 1420 may include a program storage area and a data storage area, wherein the program storage area may store instructions for implementing an operating system, instructions for at least one function (such as a touch function, a sound playback function, an image playback function, etc.), instructions for implementing the above various method embodiments, etc.; the data storage area may store data created according to the use of the computing device, etc.

[0091] In addition, those skilled in the art can understand that the structure of the computing device shown in the above drawings does not constitute a limitation on the computing device, and the computing device may include more or fewer components than shown in the figure, or combine certain components, or arrange the components differently. For example, the computing device also includes a display screen, a camera assembly, a microphone, a speaker, a radio frequency circuit, an input unit, a sensor (such as an acceleration sensor, an angular velocity sensor, a light sensor, etc.), an audio circuit, a WiFi module, a power supply, a Bluetooth module and other components, which will not be described in detail here.

[0092] The present disclosure also provides a computer-readable storage medium storing at least one instruction, wherein the at least one instruction is used to be executed by a processor to implement the method for detecting edge defects of epitaxial wafers as described in the above embodiments.

[0093] The present disclosure also provides a computer program product, which includes computer instructions stored in a computer-readable storage medium; a processor of a computing device reads the computer instructions from the computer-readable storage medium, and the processor executes the computer instructions, so that the computing device executes to implement the method for detecting edge defects of epitaxial wafers described in the above-mentioned embodiments.

[0094] In addition, the present disclosure also provides a method for processing an epitaxial wafer, the method comprising: Inspecting the epitaxial wafer using the epitaxial wafer edge defect detection method described in each of the above embodiments; When the detection result indicates that the epitaxial wafer does not have the target edge defect, the epitaxial wafer is subsequently processed according to a set process flow.

[0095] In addition, the present disclosure also provides an epitaxial wafer, which is obtained by the aforementioned epitaxial wafer processing method, and the epitaxial wafer is determined to have no target edge defects through the epitaxial wafer edge defect detection method described in the above-mentioned embodiments.

[0096] Those skilled in the art should be aware that in one or more of the above examples, the functions described in the present disclosure can be implemented using hardware, software, firmware, or any combination thereof. When implemented using software, these functions can be stored in a computer-readable medium or transmitted as one or more instructions or codes on a computer-readable medium. Computer-readable media include computer storage media and communication media, wherein communication media include any media that facilitates the transmission of computer programs from one place to another. Storage media can be any available media that can be accessed by a general or special-purpose computer.

[0097] It should be noted that the technical solutions described in the present disclosure can be combined arbitrarily without conflict.

[0098] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A method for detecting edge defects of an epitaxial wafer, characterized in that: The method comprises: At a plurality of sampling positions at the edge of the epitaxial wafer, the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position are obtained; Comparing the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position with the set judgment conditions; When there is a sampling position that meets the determination condition, it is determined that the epitaxial wafer has a target edge defect.

2. The method according to claim 1, characterized in that The step of obtaining the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position includes: Acquire an image at each sampling position; The area of ​​the abnormal defect and the brightness characteristics of the abnormal defect are obtained in the image.

3. The method according to claim 2, characterized in that The obtaining of the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect in the image includes: In the image, obtaining a minimum enclosing area containing an abnormal defect; Determining the area of ​​the minimum enclosing region as the area of ​​the abnormal defect; The grayscale average value of all pixels in the minimum enclosing area is determined as the brightness feature of the abnormal defect.

4. The method according to claim 1, characterized in that: The comparing the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect and each sampling position with the set judgment condition includes: Determining whether the area of ​​the abnormal defect at each sampling position is greater than a set area threshold; Determining whether the brightness characteristic of the abnormal defect at each sampling position is less than a set brightness threshold; Determine whether each sampling position is a set target position; wherein the target position is a position of the epitaxial wafer corresponding to a support of a load lock chamber during an epitaxial process.

5. The method according to claim 4, characterized in that When there is a sampling position that meets the determination condition, determining that the epitaxial wafer has a target edge defect includes: When there is a sampling position among all the sampling positions that simultaneously satisfies the set comparison result, it is determined that the epitaxial wafer has a target edge defect; wherein the comparison result includes: the area of ​​the abnormal defect at the sampling position is greater than the set area threshold; the brightness feature of the abnormal defect at the sampling position is less than the set brightness threshold; the sampling position is at the target position.

6. The method according to claim 5, characterized in that The method further comprises: When the epitaxial wafer has a target edge defect, the type of the target edge defect is detected by a scanning electron microscope, and the determination condition is updated according to the detection result.

7. The method according to claim 1, characterized in that The method further comprises: The plurality of sampling positions are selected at equal intervals on the edge of the epitaxial wafer according to a set sampling angle.

8. A device for detecting edge defects of epitaxial wafers, characterized in that: The device comprises: an acquisition unit, a comparison unit and a determination unit; wherein, The acquisition unit is configured to acquire the area of ​​the abnormal defect and the brightness characteristics of the abnormal defect at each sampling position among multiple sampling positions at the edge of the epitaxial wafer; The comparison unit is configured to compare the area of ​​the abnormal defect at each sampling position, the brightness characteristics of the abnormal defect, and each sampling position with the set determination condition; The determination unit is configured to determine that a target edge defect exists in the epitaxial wafer when there is a sampling position that meets the determination condition.

9. A method for processing an epitaxial wafer, characterized in that: The method comprises: Inspecting the epitaxial wafer by the method for detecting edge defects of the epitaxial wafer according to any one of claims 1 to 7; When the detection result indicates that the epitaxial wafer does not have the target edge defect, the epitaxial wafer is subsequently processed according to a set process flow.

10. An epitaxial wafer, characterized in that: The epitaxial wafer is obtained by the processing method of claim 9, and the epitaxial wafer is determined to have no target edge defects by the edge defect detection method of the epitaxial wafer of any one of claims 1 to 7.

Citation Information

Cited By

  • Method and system for detecting chemical contamination on back surface of wafer

    CN120404766A