Method for preparing rice bran protein-epigallotein gallate binary nanoparticles under assistance of supergravity rotating packed bed
Through supergravity rotary filling bed technology, rice bran protein and epigalactine gallate were covalently combined with epigalactine gallate to prepare rice bran protein-epagate gallate binary nanoparticles with higher emulsification and stability, which solved the problem of The problems of complex process and long time in the prior art have expanded the application potential of rice bran in the food field.
Patent Information
- Application Number
- CN202411123863.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-26
AI Technical Summary
The process of preparing protein-polyphenol binary nanoparticles in the prior art is complex and time-consuming, which limits the application of rice bran protein in the food field, especially its low antioxidant and emulsification characteristics.
Using supergravity rotary filling bed technology, rice bran protein and epigallocate gallate are covalently combined, and binary nanoparticles are prepared through efficient rotary flow and mixing process to improve their emulsification and stability.
It effectively improves the emulsification characteristics of rice bran protein and the bioavailability of epigallocate gallate, simplifies the process flow, enhances the functional properties of nanoparticles, and does not add chemical emulsifiers, achieving a green and safe preparation process.
Smart Images

Figure CN119014553A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of food, and relates to a method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles with the assistance of a high-gravity rotating packed bed. Technical Background
[0002] Rice bran protein (RBP) is a high-quality plant protein with a wide range of sources. It is a high-quality protein resource among plant proteins. Rice bran protein also has good self-assembly properties and can be used as a wall material for transporting bioactive substances. However, the antioxidant and emulsifying properties of a single RBP are relatively low, which has certain drawbacks in application and limits the application of rice bran protein.
[0003] Epigallocatechin gallate is the most effective active ingredient in tea polyphenols. It has antioxidant properties and can protect the body from various diseases by scavenging free radicals. At the same time, EGCG has antibacterial, antiviral, antioxidant, anti-atherosclerotic, anti-thrombotic, anti-angiogenic, anti-inflammatory and anti-tumor effects. EGCG is rich in hydroxyl groups, which enables it to form hydrogen bonds with proteins. Therefore, rice bran protein and EGCG are effectively combined through interaction. By covalently binding EGCG, the antioxidant and emulsifying properties of RBP can be effectively improved, and the application of rice bran in the food field can be expanded. The existing patent "A method for preparing sugarcane leaf polyphenol-zein covalent composite nanoparticles and its application" CN202311636493.3 obtains sugarcane leaf polyphenol-zein covalent composite nanoparticles by covalent bonding, which improves the antioxidant capacity of the protein and broadens its scope of use.
[0004] According to investigations, the current process for preparing protein-polyphenol binary nanoparticles is complex and takes a long time to prepare. The high-gravity rotating packed bed is a new technology that uses a high-gravity environment with a much greater acceleration than the earth's gravity to enhance mass transfer and micro-mixing processes. When the rotating bed rotates at high speed, the reactants enter its interior through laminar flow or bubble flow, rotate and flow in the gaps between the packings, and form a liquid film on the surface of the packing, which can achieve rapid mixing and mass transfer, thereby increasing the reaction rate. It can efficiently prepare nanoparticles, simplify the process flow, and provide new ideas for the preparation of rice bran protein-epigallocatechin gallate binary nanoparticles.
[0005] Therefore, the present invention first hydrates rice bran protein and epigallocatechin gallate overnight to prepare a stock solution, and then intervenes in a high-gravity rotating packed bed to efficiently and quickly prepare rice bran protein-epigallocatechin gallate binary nanoparticles, giving the nanoparticles better emulsification properties, thereby providing a theoretical basis for developing the application of nanoparticles in the food field. Summary of the invention
[0006] The purpose of the present invention is to provide a method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high-gravity rotating packed bed. The method effectively utilizes the existing abundant and cheap rice bran resources, ensures the biological activity of epigallocatechin gallate in the nanoparticles, and also improves the stability of the nanoparticles.
[0007] The objective of the present invention is achieved through the following technical solutions:
[0008] The defatted rice bran and deionized water were mixed in a ratio of 1:9, homogenized for 5min-10min, and then magnetically stirred at room temperature for 1h-2h, the pH was adjusted to 9.5, and the mixture was stirred on a magnetic stirrer. After filtering to remove the rice bran residue, the mixture was centrifuged at 8000r / min-10000r / min at room temperature for 30min to obtain the supernatant, the pH of the supernatant was adjusted, the supernatant was removed by centrifugation at room temperature for 30min, the precipitate was diluted and the pH was adjusted to neutral, and the rice bran protein was obtained by freeze-drying; EGCG and RBP stock solutions were prepared respectively; the EGCG stock solution and the RPB stock solution were placed in a high-gravity rotating packed bed at room temperature, EGCG was added according to the mass of RPB, the total solid concentration was controlled, the pH of the mixed system was adjusted to 9.0 with a NaOH solution, and the motor reaction was started; the obtained mixed solution was dialyzed at 4°C for 48h in a dialysis bag of 8000-14000kDa, the water was changed regularly to remove free EGCG, and RE binary nanoparticles were obtained after freeze-drying.
[0009] Furthermore, during the extraction of rice bran protein, the mixed solution should be adjusted to a pH of 9.5, magnetically stirred at 50°C to 55°C for 3 hours, the supernatant pH should be adjusted to 4.4, allowed to stand for 40 minutes, centrifuged at 10,000 r / min at room temperature for 30 minutes to remove the supernatant, the precipitate should be diluted and the pH value should be adjusted to neutral, and freeze-dried to obtain rice bran protein;
[0010] Furthermore, the prepared EGCG stock solution and RBP stock solution should have a concentration of 10 mg / mL to 20 mg / mL and be hydrated overnight in a 4°C refrigerator;
[0011] Furthermore, the specific steps of introducing the mixed solution into the high gravity rotating reaction bed are as follows: the rotor speed of the rotating bed is 300r / min to 1100r / min, preferably 600r / min to 800r / min; the time of introducing into the high gravity rotating reaction bed is 40min to 60min, preferably 45min to 55min; the feed flow rate is 200 to 300mL / min;
[0012] Furthermore, the mixed solution is introduced into the high gravity reaction bed, the addition amount of epigallocatechin gallate (EGCG) should be controlled to be 1.5% to 3.5% of the mass of rice bran protein (RBP), the total solid concentration of the mixed solution is 10 mg / L to 25 mg / L, and the pH of the mixed system is 9.0;
[0013] The beneficial effects of the present invention are:
[0014] (1) Due to its structural characteristics, rice bran protein has poor solubility in water, which limits its application. The preparation of binary nanoparticles effectively improves the emulsification properties of rice bran protein, laying the foundation for subsequent applications;
[0015] (2) Epigallocatechin gallate has certain antioxidant properties and can protect the body from various diseases by scavenging free radicals, but it is unstable. Through the preparation of binary nanoparticles, the activity loss of epigallocatechin gallate caused by environmental factors is reduced, and its bioavailability is improved;
[0016] (3) The binary nanoparticles were prepared using a high-gravity rotating packed bed reactor, which effectively increased the reaction rate of rice bran protein and epigallocatechin gallate and enhanced the functional properties of the protein nanoparticles. In addition, no chemical emulsifiers were added during the preparation process, which is green and safe, further expanding the application potential of the prepared nanoparticles.
[0017] (4) Utilizing rice bran, a by-product of rice processing, saves agricultural resources and improves the comprehensive utilization level of rice bran.
[0018] (5) The binary nanoparticles prepared by the present invention have a grafting amount of 13.73-23.17, a grafting rate of 66.48%-95.61%, a particle size of 92.58nm-121.86nm, a turbidity of 0.034-0.050, a PDI of 0.328-0.450, a potential of -17.2-21.9mV, an emulsification property of 73.7-85.9, and an emulsification stability of 84.3%-95.4%. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 This is a graph showing the test results of the grafting amount and grafting rate of rice bran protein-epigallocatechin gallate binary nanoparticles.
[0020] Figure 2 This is a graph showing the particle size and turbidity test results of rice bran protein-epigallocatechin gallate binary nanoparticles.
[0021] Figure 3 This is a graph showing the PDI and potential test results of rice bran protein-epigallocatechin gallate binary nanoparticles.
[0022] Figure 4 This is a graph showing the emulsification and emulsification stability test results of rice bran protein-epigallocatechin gallate binary nanoparticles.
[0023] Figure 5 Flow chart of the method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by high gravity rotating packed bed. DETAILED DESCRIPTION
[0024] Example 1
[0025] A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed, the specific steps are as follows:
[0026] (1) Extract rice bran protein by alkali dissolution and acid precipitation method: defatted rice bran and deionized water were mixed in a ratio of 1:9, homogenized for 5 minutes, and magnetically stirred at room temperature for 1 hour. The pH was adjusted to 9.5 using 1M NaOH solution, and magnetically stirred at 55°C for 3 hours. After filtering to remove the rice bran residue, the supernatant was centrifuged at 10,000 r / min at room temperature for 30 minutes to obtain the supernatant. The pH of the supernatant was adjusted to 4.4 using 1M HCl solution, and the mixture was allowed to stand for 40 minutes. The supernatant was removed by centrifugation at 10,000 r / min at room temperature for 30 minutes, the precipitate was diluted and the pH value was adjusted to neutral, and the mixture was pre-frozen at -20°C for 24 hours and placed in a freeze dryer. The mixture was freeze-dried for 48 hours to obtain rice bran protein RBP.
[0027] (2) Preparation of rice bran protein RBP and epigallocatechin gallate EGCG: RBP and EGCG were dissolved in deionized water at a concentration of 10 mg / mL, respectively, and stirred on a magnetic stirrer at room temperature for 3 h. The RBP and EGCG solutions were then hydrated overnight at 4°C to obtain RBP and EGCG stock solutions.
[0028] (3) Preparation of rice bran protein-epigallocatechin gallate binary nanoparticles: 10 mL of RPB stock solution and 0.15 mL of EGCG stock solution (the amount of EGCG added was controlled to be 1.5% of the mass of rice bran protein RBP) were placed in a high gravity rotating packed bed at room temperature, 10139.85 mL of deionized water was added, the total solid concentration was controlled to be 10 mg / L, the pH of the mixed system was adjusted to 9.0 with NaOH solution, the feed flow rate was 200 mL / min, the speed was 600 r / min, and the motor reaction was started. The mixed solution was dialyzed at 4°C for 48 h in a 8000-14000 kDa dialysis bag, the water was changed every 6-8 h to remove free EGCG, and the RE binary nanoparticles were obtained after freeze drying.
[0029] (4) The prepared rice bran protein-epigallocatechin gallate binary nanoparticles have a grafting amount of 13.73, a grafting rate of 95.61%, a particle size of 105.84 nm, a turbidity of 0.038, a PDI of 0.41, a potential of -18.45 mV, an emulsification property of 73.7, and an emulsion stability of 84.3%.
[0030] Example 2
[0031] A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed, which is different from Example 1 in that:
[0032] In step (3), 10 mL of RPB stock solution and 0.2 mL of EGCG stock solution (the amount of EGCG added is controlled to be 2% of the mass of rice bran protein RBP) are placed in a high gravity rotating packed bed at room temperature, 10189.8 mL of deionized water is added, the total solid concentration is controlled to be 10 mg / L, the pH of the mixed system is adjusted to 9.0 with a NaOH solution, the feed flow rate is 200 mL / min, the speed is 600 r / min, and the motor reaction is started. The mixed solution is dialyzed at 4° C. for 48 hours in a dialysis bag of 8000 to 14000 kDa, the water is changed every 6 to 8 hours to remove free EGCG, and RE binary nanoparticles are obtained after freeze drying.
[0033] The prepared rice bran protein-epigallocatechin gallate binary nanoparticles have a grafting amount of 19.32, a grafting rate of 87.55%, a particle size of 115.7 nm, a turbidity of 0.035, a PDI of 0.44, a potential of -18.9 mV, an emulsification property of 77.1, and an emulsification stability of 89.6%.
[0034] Example 3
[0035] A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed, which is different from Example 1 in that:
[0036] In step (3), 10 mL of RPB stock solution and 0.25 mL of EGCG stock solution (the amount of EGCG added is controlled to be 2.5% of the mass of rice bran protein RBP) are placed in a high gravity rotating packed bed at room temperature, 15367.75 mL of deionized water is added, the total solid concentration is controlled to be 10 mg / L, the pH of the mixed system is adjusted to 9.0 with a NaOH solution, the feed flow rate is 200 mL / min, the speed is 600 r / min, and the motor reaction is started. The mixed solution is dialyzed in a 8000-14000 kDa dialysis bag at 4° C. for 48 hours, the water is changed every 6 hours to 8 hours to remove free EGCG, and RE binary nanoparticles are obtained after freeze drying.
[0037] The prepared rice bran protein-epigallocatechin gallate binary nanoparticles have a grafting amount of 20.88, a grafting rate of 83.51%, a particle size of 121.9 nm, a turbidity of 0.047, a PDI of 0.44, a potential of -20.1 mV, an emulsification property of 79.4, and an emulsification stability of 91.6%.
[0038] Example 4
[0039] A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed, which is different from Example 1 in that:
[0040] In step (3), 10 mL of RPB stock solution and 0.3 mL of EGCG stock solution (the amount of EGCG added is controlled to be 3% of the mass of rice bran protein RBP) are placed in a high gravity rotating packed bed at room temperature, 15439.7 mL of deionized water is added, the total solid concentration is controlled to be 10 mg / L, the pH of the mixed system is adjusted to 9.0 with a NaOH solution, the feed flow rate is 200 mL / min, the speed is 600 r / min, and the motor reaction is started. The mixed solution is dialyzed in a 8000-14000 kDa dialysis bag at 4° C. for 48 hours, the water is changed every 6 hours to 8 hours to remove free EGCG, and RE binary nanoparticles are obtained after freeze drying.
[0041] The prepared rice bran protein-epigallocatechin gallate binary nanoparticles have a grafting amount of 22.44, a grafting rate of 74.78%, a particle size of 92.58 nm, a turbidity of 0.034, a PDI of 0.33, a potential of -21.9 mV, an emulsification property of 85.9, and an emulsification stability of 95.4%.
[0042] Example 5
[0043] A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles, which is different from Example 1 in that:
[0044] In step (3), 20 mL of RPB stock solution and 0.7 mL of EGCG stock solution (the amount of EGCG added is controlled to be 3.5% of the mass of rice bran protein RBP) are placed in a high gravity rotating packed bed at room temperature, 20679.3 mL of deionized water is added, the total solid concentration is controlled to be 20 mg / L, the pH of the mixed system is adjusted to 9.0 with a NaOH solution, the feed flow rate is 200 mL / min, the speed is 600 r / min, and the motor reaction is started. The mixed solution is dialyzed in a 8000-14000 kDa dialysis bag at 4° C. for 48 hours, the water is changed every 6 hours to 8 hours to remove free EGCG, and RE binary nanoparticles are obtained after freeze drying.
[0045] The prepared rice bran protein-epigallocatechin gallate binary nanoparticles have a grafting amount of 23.14, a grafting rate of 66.48%, a particle size of 121.86 nm, a turbidity of 0.050, a PDI of 0.450, a potential of -17.2 mV, an emulsification property of 81.2, and an emulsification stability of 94.2%.
[0046] Figure 1-Figure 4 The grafting amount, grafting rate, particle size, turbidity, particle size distribution (PDI), Zeta potential, emulsification and emulsification stability were used as research indicators to explore the effects of different EGCG addition amounts in Examples 1-5 on the formation process of rice bran protein-epigallocatechin gallate (RE) binary nanoparticles.
[0047] like Figure 1 As shown, the amount of EGCG added in the RE binary nanoparticles prepared in Examples 1-5 was between 1.5% and 3.5% of the mass of rice bran protein RBP, the grafting amount was between 13.73% and 23.14%, and the grafting rate was between 66.48% and 95.61%. An appropriate amount of EGCG promoted the increase of grafting sites, while too high a concentration reduced the grafting efficiency. In Example 4, the grafting amount reached the highest when the EGCG addition was 3%.
[0048] like Figure 2 , 3 As shown, the particle size of the rice bran protein-epigallocatechin gallate (RE) binary nanoparticles prepared in Examples 1-5 is between 92.58-121.9 nm, the turbidity is between 0.034-0.050, the PDI is between 0.328-0.450, and the potential value is between -17.2--21.9 mV, indicating that the nanoparticles prepared in all examples have uniform particle size distribution, good dispersibility and transparency, and good stability. The particles prepared in Example 4 have the best PDI, and the particles are more uniform and stable.
[0049] like Figure 4 As shown, the emulsification of rice bran protein-epigallocatechin gallate (RE) binary nanoparticles prepared in Examples 1-5 was between 73.7% and 85.9%, and the emulsification stability was between 84.3% and 95.4%, which further proved that the particles of Example 4 performed best in both emulsification and emulsification stability, and a higher amount of EGCG added enhanced the interfacial activity and stability of the nanoparticles, thereby improving their emulsification properties.
[0050] In summary, by adjusting the amount of EGCG added, the various performance indicators of rice bran protein-epigallocatechin gallate binary nanoparticles can be optimized. Among them, Example 4 showed the best PDI value, higher grafting amount, good particle size distribution, low turbidity, and excellent emulsification and emulsification stability when the EGCG addition amount was 3%. Under this condition, the interaction between EGCG and rice bran protein reached the best state, and the efficient mixing and dispersion of the ultra-gravity rotating packed bed technology promoted the uniform formation and stable existence of nanoparticles.
Claims
1. A method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed, characterized in that: 1) defatted rice bran is mixed with deionized water, stirred at room temperature, the pH of the solution is adjusted to alkaline, stirred, filtered to remove rice bran residue, centrifuged to obtain supernatant, the pH of the supernatant is adjusted to 4.4, allowed to stand, centrifuged to remove the supernatant, diluted the precipitate and adjusted the pH to neutral, inverted plate freezing for 24 hours, and freeze-dried to obtain rice bran protein RBP; 2) Epigallocatechin gallate EGCG was dissolved in deionized water and stirred on a magnetic stirrer at room temperature, and then the EGCG solution was hydrated at 4°C overnight to obtain an EGCG stock solution; 3) dissolving the rice bran protein RBP prepared in step 1) in deionized water, stirring on a magnetic stirrer at room temperature for 3 h to 4 h, and then hydrating the rice bran protein RPB solution at 4° C. overnight; Obtain rice bran protein RBP stock solution; 4) placing the EGCG stock solution and the RPB stock solution in step 2) and step 3) in a high gravity rotating packed bed at room temperature, controlling the total solid concentration, adjusting the pH of the mixed system to alkaline with a 1M NaOH solution, and starting the motor reaction; 5) dialyzing the mixed solution in step 4) in a 8000-14000 kDa dialysis bag, changing the water every 6-8 hours to remove free EGCG; 6) freeze-drying the nanoparticle solution prepared in step 5) to obtain rice bran protein-epigallocatechin gallate RE binary nanoparticles.
2. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: Step 1) is specifically as follows: defatted rice bran and deionized water are mixed in a ratio of 1:9, homogenized for 5 minutes, magnetically stirred at room temperature for 1 hour to 1.5 hours, adjusted to pH 9.5 with a 1M NaOH solution, magnetically stirred at 50°C to 55°C for 3 hours, filtered to remove rice bran residue, centrifuged at room temperature for 30 minutes at 10000 r / min to obtain a supernatant, adjusted to pH 4.4 with a 1M HCl solution, allowed to stand for 40 minutes to 60 minutes, centrifuged at room temperature for 30 minutes at 10000 r / min to remove the supernatant, diluted the precipitate and adjusted the pH value to neutral, inverted plate frozen for 24 hours, and freeze-dried for 48 hours to obtain rice bran protein.
3. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: In the step 2), the concentration of the epigallocatechin gallate EGCG stock solution is 10 mg / mL to 20 mg / mL.
4. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: In the step 3), the concentration of the rice bran protein RBP stock solution is 10 mg / mL~20mg / mL.
5. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: In the step 4), the amount of epigallocatechin gallate EGCG added is 1.5% to 3.5% of the mass of rice bran protein RBP, the total solid concentration is 10 mg / L to 25 mg / L, and the pH of the mixed system is 9.
0.
6. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: In the step 4), the mixed solution is introduced into a high gravity rotating packed bed; the rotor speed of the rotating bed is 300 r / min to 1200 r / min, preferably 600 r / min to 800 r / min; and the feed flow rate is 200 mL / min to 300 mL / min.
7. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 6, characterized in that: In the step 4), the mixed solution is introduced into a high gravity rotating packed bed; the rotor speed of the rotating bed is 600 r / min to 800 r / min.
8. The method for preparing rice bran protein-epigallocatechin gallate binary nanoparticles assisted by a high gravity rotating packed bed according to claim 1, characterized in that: In the step 5), the dialysis is performed at 4° C. for 48 hours.
Citation Information
Patent Citations
Preparation method and application of sugarcane leaf polyphenol-zein covalent composite nanoparticles
CN117659450A
Cited By
Temperature-responsive drug-loaded Pickering emulsion, preparation method and application
CN121401199A