MEMS sensor and preparation method thereof
By setting spaced movable mass blocks and preset gaps in the device layer of the MEMS sensor, using the DRIE process to form differential output, the problems of high epitaxial growth cost and limited design in the prior art are solved, and the more High performance, sensitivity and complexity.
Patent Information
- Application Number
- CN202310628808.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-24
- Filing Date
- 2023-05-30
- Publication Date
- 2024-11-26
AI Technical Summary
The existing MEMS sensor design is limited by the single-piece device layer in terms of performance, robustness and complexity, and the multi-epitaxial growth process is costly and prone to warping and other problems, making it difficult to achieve a double-layer or multi-layer device structure.
Design a MEMS sensor, by setting several spaced movable mass blocks in the device layer, supporting and forming preset gaps using anchor points, etching into differential output electrical signals through DRIE process, allowing greater design flexibility and Higher sensitivity while achieving mold size reduction and complex design.
It improves the performance, reliability and accuracy of the sensor, achieves higher sensitivity and driving force, enhances signal-to-noise ratio and anti-interference ability, and reduces the mold size, making the design more complex and accurate.
Smart Images

Figure CN119018839A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of micro-electromechanical systems, in particular to a MEMS sensor and a preparation method thereof. Background Art
[0002] Many current designs of MEMS sensors, such as microphones, pressure sensors, and inertial sensors, use a single device layer and one or more sacrificial layers. Releasing the sacrificial layer allows the device layer to move. Without increasing the die size, single-piece device layer designs are approaching limitations in terms of performance, robustness, and sensibility. Therefore, the demand for dual-layer or multi-layer device structures continues to increase.
[0003] In the prior art, one possible process includes multi-epitaxial growth of the device layer, while other processes such as chemical vapor deposition (CVD) and silicon dioxide etching are used to achieve the dual device layer, but multi-epitaxial growth of the device layer requires a very high budget and may cause unexpected effects such as warping. Summary of the invention
[0004] The object of the present invention is to provide a MEMS sensor and a method for preparing the same to solve the technical problems in the prior art, which can allow the design of multi-layer devices and further improve performance, reliability, complexity and mold size.
[0005] The present invention provides a MEMS sensor, comprising:
[0006] A bottom electrode layer and a top electrode layer are arranged at intervals, and a cavity is formed between the bottom electrode layer and the top electrode layer;
[0007] The device layer is accommodated in the cavity, and the device layer includes a plurality of movable mass blocks arranged at intervals. The movable mass blocks are supported on the bottom electrode layer through anchor points. A preset gap is formed between the movable mass blocks and the top electrode layer. There are differences in the preset gaps formed by different movable mass blocks.
[0008] A MEMS sensor as described above, wherein preferably, the plurality of movable mass blocks include a first movable mass block, a second movable mass block and a third movable mass block, the second movable mass block is located between the first movable mass block and the third movable mass block, a first preset gap is formed between the first movable mass block and the top electrode layer, a second preset gap is formed between the second movable mass block and the top electrode layer, a third preset gap is formed between the third movable mass block and the top electrode layer, and there are differences in height values of the first preset gap, the second preset gap and the third preset gap.
[0009] In the MEMS sensor as described above, preferably, the height value of the first preset gap, the height value of the third preset gap, and the height value of the second preset gap increase in sequence.
[0010] In the MEMS sensor as described above, preferably, the height value of the first preset gap is the same as the height value of the third preset gap, and the height value of the second preset gap is greater than the height values of the first preset gap and the third preset gap.
[0011] In the MEMS sensor as described above, preferably, the bottom of the first movable mass block and the third movable mass block are connected to one anchor point, and the bottom of the second movable mass block is connected to two anchor points.
[0012] In the MEMS sensor as described above, preferably, a plurality of openings are formed on the top electrode layer, and the plurality of openings are distributed at intervals along the radial direction of the top electrode layer.
[0013] In a second aspect, the present invention further provides a method for preparing a MEMS sensor, which is used to prepare the aforementioned MEMS sensor, comprising the following steps:
[0014] Step S1: forming a bottom electrode layer, a sacrificial layer, a device layer and a top electrode layer in sequence from bottom to top;
[0015] Step S2: etching the device layer to form a plurality of movable mass blocks arranged at intervals;
[0016] Step S3: releasing the sacrificial layer in the device layer.
[0017] In the method for preparing a MEMS sensor as described above, preferably, step S1 includes:
[0018] Step 101: forming a bottom electrode layer;
[0019] Step 102: forming a sacrificial layer on the bottom electrode layer, and etching a top surface of the sacrificial layer to form a stepped interface and a plurality of grooves;
[0020] Step 103: forming a device layer on the sacrificial layer, wherein the movable mass block of the device layer is stacked on the step interface, and the anchor point of the device layer is formed in the groove;
[0021] Step 104: Form the top electrode layer, and form a plurality of openings on the top electrode layer.
[0022] In the method for preparing a MEMS sensor as described above, preferably, in the step S2, the device layer is etched by a DRIE process to form a plurality of movable mass blocks arranged at intervals.
[0023] In the method for preparing a MEMS sensor as described above, preferably, the material of the device layer is lead zirconium titanate, aluminum nitride, barium titanate or a mixture of the above materials.
[0024] Compared with the prior art, the present invention forms a differential output electrical signal by setting the device layer to a number of movable mass blocks arranged at intervals. The preset gaps formed by different movable mass blocks are different. This allows greater design flexibility and provides the sensor with higher sensitivity and greater driving force. It can also achieve a reduction in mold size while realizing a more complex design with higher precision and miniaturization. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 is a cross-sectional schematic diagram of a MEMS sensor according to Embodiment 1 of the present invention;
[0026] Figure 2a-2c is a flow chart of the preparation of the MEMS sensor of the first embodiment provided by the present invention;
[0027] Figure 3 is a cross-sectional schematic diagram of a MEMS sensor according to Embodiment 2 of the present invention;
[0028] Figure 4a-4c This is a flow chart of the preparation of the MEMS sensor of the second embodiment provided by the present invention.
[0029] Explanation of the figure markings: 1-bottom electrode layer, 2-top electrode layer, 21-opening, 3-cavity, 4-device layer, 41-movable mass block, 411-first movable mass block, 412-first preset gap, 413-second movable mass block, 414-second preset gap, 415-third movable mass block, 416-third preset gap, 42-anchor point, 5-sacrificial layer, 51-groove. DETAILED DESCRIPTION
[0030] The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, but should not be construed as limiting the present invention.
[0031] like Figure 1 as well as Figure 3 As shown, an embodiment of the present invention provides a MEMS sensor, including:
[0032] A bottom electrode layer 1 and a top electrode layer 2 are arranged at intervals, and a cavity 3 is formed between the bottom electrode layer 1 and the top electrode layer 2 .
[0033] The device layer 4 is accommodated in the cavity 3, and at least a portion of the device layer 4 is conductive, so that a capacitor is formed between the device layer 4 and the top electrode layer 2 opposite to the device layer 4. Specifically, when the MEMS sensor is used as a microphone, when the microphone is powered on, the top electrode layer 2 and the device layer 4 will carry charges of opposite polarities, thereby forming a capacitor. When the device layer 4 vibrates under the action of sound waves, the distance between the top electrode layer 2 and the device layer 4 will change, thereby causing the capacitance of the capacitor to change, and then converting the sound wave signal into an electrical signal, thereby realizing the corresponding function of the microphone.
[0034] In the embodiment provided by the present application, the device layer 4 includes a plurality of movable mass blocks 41 arranged at intervals, and the movable mass blocks 41 are supported on the bottom electrode layer 1 through anchor points 42, and a preset gap is formed between the movable mass blocks 41 and the top electrode layer 2. There are differences in the preset gaps formed by different movable mass blocks 41, thereby forming a differential output electrical signal. This structure allows greater design flexibility, and provides the sensor with higher sensitivity and greater driving force, and can also achieve a reduction in mold size, while achieving a more complex design, with higher precision and miniaturization. Specifically, when the MEMS sensor is used for a microphone, the capacitive microphone can obtain a higher signal-to-noise ratio, improve the ability to suppress linear distortion, and at the same time improve the anti-interference ability of the microphone, so that the signal transmission distance is longer and the audio performance of the microphone is better.
[0035] Furthermore, the plurality of movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415. The second movable mass block 413 is located between the first movable mass block 411 and the third movable mass block 415. A first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2. There are differences in the height values of the first preset gap 412, the second preset gap 414 and the third preset gap 416.
[0036] A first capacitor is formed between the first movable mass block 411 and the top electrode layer 2. When the height value of the first preset gap 412 formed between the first movable mass block 411 and the top electrode layer 2 changes, the capacitance of the first capacitor changes accordingly. A second capacitor is formed between the second movable mass block 413 and the top electrode layer 2. When the height value of the second preset gap 414 formed between the second movable mass block 413 and the top electrode layer 2 changes, the capacitance of the second capacitor changes accordingly. A third capacitor is formed between the third movable mass block 415 and the top electrode layer 2. When the height value of the third preset gap 416 formed between the third movable mass block 415 and the top electrode layer 2 changes, the capacitance of the third capacitor changes accordingly. The electrical signals output by the first capacitor, the second capacitor and the third capacitor form a differential output, and the sensor has higher sensitivity.
[0037] Two embodiments are listed below to provide a more specific description of the MEMS sensor provided by the present invention when used as a microphone. Those skilled in the art will appreciate that variations can be made based on these embodiments, all of which fall within the protection scope of the present invention.
[0038] Embodiment 1
[0039] Reference Figure 1 As shown, in this embodiment, the height value of the first preset gap 412, the height value of the third preset gap 416 and the height value of the second preset gap 414 increase in sequence. Since the value of the capacitor is proportional to the area of the capacitor between the two plates and inversely proportional to the distance between the two plates, that is, C = kε0ε r S / d, k is a constant, ε0 is a constant, ε r is a constant. When the condenser microphone is manufactured, ε0ε r The value of is fixed, S is the area directly opposite to the two plates of the capacitor, d is the distance between the two plates, and when the surfaces of the first movable mass block 411, the second movable mass block 413 and the third movable mass block 415 are roughly the same, the larger the height value of the preset gap, the smaller the capacitance. In this embodiment, the initial capacitance value of the first capacitor formed by the first movable mass block 411 is the largest, the initial capacitance value of the third capacitor formed by the third movable mass block 415 is the second largest, and the initial capacitance value of the third capacitor formed by the second movable mass block 413 is the smallest. The second movable mass block 413 is located in the middle of the device layer 4, which is the most violently deformed part, thereby providing higher sensitivity and greater driving force.
[0040] In this embodiment, refer to Figure 1As shown, the bottom of the first movable mass block 411 and the third movable mass block 415 are connected to an anchor point 42, and the bottom of the second movable mass block 413 is connected to two anchor points 42. The first movable mass block 411, the second movable mass block 413, the third movable mass block 415 and the anchor points 42 can all be made of conductive materials.
[0041] Since the bottom support of the second movable mass block 413 has two anchor points 42 set at intervals, the movable part of the second movable mass block 413 is located between the two anchor points 42. When the device layer 4 vibrates under the action of sound waves, the movable part of the second movable mass block 413 is bent and deformed, thereby changing the distance from the top electrode layer 2, and the capacitance of the second capacitor changes accordingly, and a differential output electrical signal is formed between the first capacitor, the second capacitor and the third capacitor.
[0042] In a feasible implementation, when the device layer 4 vibrates under the action of sound waves, the first movable mass block 411 and the third movable mass block 415 can also pivot around the anchor point 42, so that one end of the first movable mass block 411 and the third movable mass block 415 tilts upward and the other end tilts downward, thereby changing the distance between the top electrode layer 2, and the capacitance of the first capacitor and the third capacitor changes accordingly, forming a differential output electrical signal.
[0043] In this embodiment, a plurality of openings 21 are formed on the top electrode layer 2. The plurality of openings 21 are distributed at intervals along the radial direction of the top electrode layer 2. The openings 21 are evenly distributed to provide channels for sound waves to pass through and to provide structural support for subsequent molding processes.
[0044] Reference Figure 2a-2c As shown, Figure 2a-2c : is a flow chart of the preparation of the MEMS sensor of the embodiment provided by the present invention. The preparation method of the MEMS sensor includes the following steps:
[0045] Step S1: Refer to Figure 2a As shown, a bottom electrode layer 1, a sacrificial layer 5, a device layer 4 and a top electrode layer 2 are sequentially formed from bottom to top. In a feasible implementation, the following steps are specifically included:
[0046] Step 101: a bottom electrode layer 1 is formed on a silicon substrate by electron beam stripping or magnetron sputtering. The bottom electrode layer 1 is connected to a bottom electrode pad (not shown) via a bottom electrode lead (not shown). The material of the bottom electrode layer 1 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good electrical conductivity.
[0047] Step 102: forming a sacrificial layer 5 on the bottom electrode layer 1, and etching the top surface of the sacrificial layer 5 to form a step interface and a plurality of grooves 51. The material of the sacrificial layer 5 may be PSG. A patterned hard mask is made on the sacrificial layer 5, and the grooves 51 are etched on the sacrificial layer 5 by dry etching or wet etching.
[0048] Step 103: forming a device layer 4 on the sacrificial layer 5, wherein the material of the device layer 4 is lead zirconium titanate, aluminum nitride, barium titanate or a mixture of the above materials, and the movable mass block 41 of the device layer 4 is stacked on the step interface to form a device layer 4 with a height difference, and the anchor point 42 of the device layer 4 is formed in the groove 51 and filled in the groove 51 until an electrical coupling is formed between the device layer 4 and the bottom electrode layer 1;
[0049] Step 104: forming a top electrode layer 2, wherein the top electrode layer 2 is connected to a top electrode pad (not shown) via a bottom electrode lead (not shown), and the material of the top electrode layer 2 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good conductive properties. A patterned hard mask is made on the top electrode layer 2, and an opening 21 is formed by etching the top electrode layer 2 by dry etching or wet etching.
[0050] Step S2: Refer to Figure 2b As shown, the device layer 4 is etched to form a number of movable mass blocks 41 spaced apart. Preferably, the device layer 4 is etched by a DRIE (deep reactive ion etching) process. By using this innovation of DRIE to isolate and create movable mass blocks at different heights, a device layer with a multi-layer height structure can be achieved, allowing greater design flexibility and providing higher sensitivity and greater driving force for the sensor. It can also achieve a reduction in mold size while achieving more complex designs with higher precision and miniaturization. The same DRIE process steps can also be used to pattern the device layer while avoiding an increase in the number of thermal cycles. Since DRIE creates a device step height, the gap between the electrodes can also be changed, which is particularly useful for sensors using a parallel plate electrode structure. The sacrificial layer 5 can be used as a hard mask to prevent the DRIE process from etching the bottom electrode layer 1.
[0051] Specifically, the plurality of movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415, a first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2, and the height values of the first preset gap 412, the third preset gap 416 and the second preset gap 414 increase sequentially.
[0052] Step S3: Refer to Figure 2c As shown, the sacrificial layer 5 within the device layer 4 is released to allow the device layer 4 to move.
[0053] Embodiment 2
[0054] Reference Figure 3 As shown, the difference between this embodiment and embodiment one is that the height value of the first preset gap 412 is the same as the height value of the third preset gap 416, and the height value of the second preset gap 414 is greater than the height values of the first preset gap 412 and the third preset gap 416. In this embodiment, the initial capacitance value of the first capacitor formed by the first movable mass block 411 is the same, and the initial capacitance value of the third capacitor formed by the second movable mass block 413 is relatively small. The second movable mass block 413 is located in the middle of the device layer 4, which is the most violently deformed part, thereby providing higher sensitivity and greater driving force.
[0055] Reference Figure 4a-4c As shown, Figure 4a-4c : is a flow chart of the preparation of the MEMS sensor of the embodiment provided by the present invention. The preparation method of the MEMS sensor includes the following steps:
[0056] Step S1: Refer to Figure 4a As shown, a bottom electrode layer 1, a sacrificial layer 5, a device layer 4 and a top electrode layer 2 are sequentially formed from bottom to top. In a feasible implementation, the following steps are specifically included:
[0057] Step 101: a bottom electrode layer 1 is formed on a silicon substrate by electron beam stripping or magnetron sputtering. The bottom electrode layer 1 is connected to a bottom electrode pad (not shown) via a bottom electrode lead (not shown). The material of the bottom electrode layer 1 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good electrical conductivity.
[0058] Step 102: forming a sacrificial layer 5 on the bottom electrode layer 1, and etching the top surface of the sacrificial layer 5 to form a step interface and a plurality of grooves 51. The material of the sacrificial layer 5 may be PSG. A patterned hard mask is made on the sacrificial layer 5, and the grooves 51 are etched on the sacrificial layer 5 by dry etching or wet etching.
[0059] Step 103: forming a device layer 4 on the sacrificial layer 5, wherein the material of the device layer 4 is lead zirconium titanate, aluminum nitride, barium titanate or a mixture of the above materials, and the movable mass block 41 of the device layer 4 is stacked on the step interface to form a device layer 4 with a height difference, and the anchor point 42 of the device layer 4 is formed in the groove 51 and filled in the groove 51 until an electrical coupling is formed between the device layer 4 and the bottom electrode layer 1;
[0060] Step 104: forming a top electrode layer 2, wherein the top electrode layer 2 is connected to a top electrode pad (not shown) via a bottom electrode lead (not shown), and the material of the top electrode layer 2 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good conductive properties. A patterned hard mask is made on the top electrode layer 2, and an opening 21 is formed by etching the top electrode layer 2 by dry etching or wet etching.
[0061] Step S2: Refer to Figure 4b As shown, the device layer 4 is etched to form a number of movable mass blocks 41 spaced apart. Preferably, the device layer 4 is etched by a DRIE (deep reactive ion etching) process. By using this innovation of DRIE to isolate and create movable mass blocks at different heights, a device layer with a multi-layer height structure can be achieved, allowing greater design flexibility and providing higher sensitivity and greater driving force for the sensor. It can also achieve a reduction in mold size while achieving more complex designs with higher precision and miniaturization. The same DRIE process steps can also be used to pattern the device layer while avoiding an increase in the number of thermal cycles. Since DRIE creates a device step height, the gap between the electrodes can also be changed, which is particularly useful for sensors using a parallel plate electrode structure. The sacrificial layer 5 can be used as a hard mask to prevent the DRIE process from etching the bottom electrode layer 1.
[0062] Specifically, the plurality of movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415. A first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2. The height value of the first preset gap 412 is the same as the height value of the third preset gap 416, and the height value of the second preset gap 414 is greater than the height values of the first preset gap 412 and the third preset gap 416.
[0063] Step S3: Refer to Figure 4c As shown, the sacrificial layer 5 within the device layer 4 is released to allow the device layer 4 to move.
[0064] The above describes in detail the structure, features and effects of the present invention based on the embodiments shown in the drawings. The above is only a preferred embodiment of the present invention, but the present invention is not limited to the scope of implementation shown in the drawings. Any changes made according to the concept of the present invention, or modifications to equivalent embodiments with equivalent changes, which still do not exceed the spirit covered by the description and drawings, should be within the protection scope of the present invention.
Claims
1. A MEMS sensor, characterized in that: include: A bottom electrode layer and a top electrode layer are arranged at intervals, and a cavity is formed between the bottom electrode layer and the top electrode layer; The device layer is accommodated in the cavity, and the device layer includes a plurality of movable mass blocks arranged at intervals. The movable mass blocks are supported on the bottom electrode layer through anchor points. A preset gap is formed between the movable mass blocks and the top electrode layer. There are differences in the preset gaps formed by different movable mass blocks.
2. The MEMS sensor according to claim 1, characterized in that: The several movable mass blocks include a first movable mass block, a second movable mass block and a third movable mass block, the second movable mass block is located between the first movable mass block and the third movable mass block, a first preset gap is formed between the first movable mass block and the top electrode layer, a second preset gap is formed between the second movable mass block and the top electrode layer, and a third preset gap is formed between the third movable mass block and the top electrode layer, and there are differences in height values of the first preset gap, the second preset gap and the third preset gap.
3. The MEMS sensor according to claim 2, characterized in that: The height value of the first preset gap, the height value of the third preset gap, and the height value of the second preset gap increase in sequence.
4. The MEMS sensor according to claim 2, characterized in that: The height value of the first preset gap is the same as the height value of the third preset gap, and the height value of the second preset gap is greater than the height values of the first preset gap and the third preset gap.
5. The MEMS sensor according to claim 2, characterized in that: The bottom of the first movable mass block and the third movable mass block is connected to an anchor point, and the bottom of the second movable mass block is connected to two anchor points.
6. The MEMS sensor according to claim 1, characterized in that: A plurality of openings are formed on the top electrode layer, and the openings are distributed at intervals along the radial direction of the top electrode layer.
7. A method for preparing a MEMS sensor, used for preparing the MEMS sensor according to any one of claims 1 to 6, characterized in that: The following steps are involved: Step S1: forming a bottom electrode layer, a sacrificial layer, a device layer and a top electrode layer in sequence from bottom to top; Step S2: etching the device layer to form a plurality of movable mass blocks arranged at intervals; Step S3: releasing the sacrificial layer in the device layer.
8. The method for preparing a MEMS sensor according to claim 7, characterized in that: The step S1 includes: Step 101: forming a bottom electrode layer; Step 102: forming a sacrificial layer on the bottom electrode layer, and etching a top surface of the sacrificial layer to form a stepped interface and a plurality of grooves; Step 103: forming a device layer on the sacrificial layer, wherein the movable mass block of the device layer is stacked on the step interface, and the anchor point of the device layer is formed in the groove; Step 104: Form the top electrode layer, and form a plurality of openings on the top electrode layer.
9. The method for preparing a MEMS sensor according to claim 7, characterized in that: In the step S2, the device layer is etched by a DRIE process to form a plurality of movable mass blocks arranged at intervals.
10. The method for preparing a MEMS sensor according to claim 7, characterized in that: The material of the device layer is lead zirconate titanate, aluminum nitride, barium titanate or a mixture of the above materials.