Resin PC307 for separating germanium from sodium germanate solution as well as preparation method and application of resin PC307
By preparing a porous sodium germanate solution separation resin PC307, the problems of high cost and environmental unfriendliness of germanium extraction in the prior art have been solved, and efficient and low-cost germanium separation effect has been achieved.
Patent Information
- Application Number
- CN202411086702.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-26
AI Technical Summary
Existing technologies for extracting germanium from lead-zinc deposits, germanium-bearing lignite, and copper ores suffer from high costs, large acid consumption, and environmental problems, making it difficult to efficiently separate germanium.
A porous sodium germanate solution separation resin PC307 was prepared by using styrene as the backbone, introducing polar monomers acrylamide and diethylenetriamine as crosslinking agents, and combining pore-forming agents and dispersants, and carrying out a polymerization reaction under a nitrogen atmosphere.
Selective adsorption of germanium was achieved. The process is simple, low-cost, and environmentally friendly, with a germanium extraction rate of 85-90%.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of metallurgy and chemical industry, and specifically relates to a resin PC307 for separating germanium from a sodium germanate solution, and a preparation method and application thereof. Background Art
[0002] As an important material for semiconductors, germanium is widely used in fiber optic communications, solar cells, chemical catalysts, infrared optics, aerospace and other fields. However, global germanium resources are relatively scarce, and there are no independent deposits. They are mainly associated with lead-zinc deposits, germanium-containing lignite and copper mines, in which the germanium content is relatively low, and it is mostly enriched as a by-product in the main metal recovery process. Because germanium enrichment is difficult and is restricted by the process used to treat minerals, a lot of energy has been invested in the research on germanium extraction at home and abroad. Different germanium-containing materials have different methods for extracting and separating germanium. Traditional processes such as tannin precipitation of germanium, neutralization precipitation, and chlorination distillation have problems such as high cost, large acid consumption, and environmental unfriendliness. Therefore, it is very necessary to develop a product and method that can solve the above technical problems. Summary of the invention
[0003] The first purpose of the present invention is to provide a resin PC307 for separating germanium from a sodium germanate solution; the second purpose is to provide a preparation method of the resin PC307 for separating germanium from a sodium germanate solution; and the third purpose is to provide an application of the resin PC307 for separating germanium from a sodium germanate solution.
[0004] The first object of the present invention is achieved in that the resin PC307 for separating germanium from the sodium germanate solution is prepared by polymerization reaction with styrene as the skeleton and polar monomers acrylamide and diethylenetriamine as crosslinking agents.
[0005] The second object of the present invention is achieved by using styrene as a skeleton, introducing polar monomers acrylamide and diethylenetriamine as crosslinking agents, adding pore-forming agents, dispersants and initiators, stirring and reacting in a water bath at 60-80° C. under a nitrogen atmosphere for 5-8 hours, filtering, washing and drying to obtain the target germanium separation resin PC307.
[0006] The specific operation is as follows: take styrene (St) as the skeleton, introduce polar monomer acrylamide (AM), diethylenetriamine (DTA) as the crosslinking agent, toluene as the pore-forming agent, gelatin as the dispersant, and benzoyl peroxide as the initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA is 15-30:5-10:1, and toluene, gelatin and benzoyl peroxide are 1% of the monomer mass. Nitrogen is introduced into the system, and stirred in a water bath at 70℃ for 5-8h. After the reaction is completed, the system is filtered and washed, and placed in a vacuum drying oven at 70℃ for 8-12h to obtain the resin PC307 for separating germanium.
[0007] The third object of the present invention is achieved by applying the resin PC307 for separating germanium from a sodium germanate solution to a process for extracting germanium from a sodium germanate solution.
[0008] The resin PC307 for separating germanium of the present invention has the characteristics of simple process, low cost, environmental friendliness, etc. for selectively adsorbing germanium.
[0009] The technical principle of the resin PC307 for separating germanium from the sodium germanate solution described in the present invention is: in a water bath at 60-80°C, the initiator decomposes to generate free radicals, and the free radicals react with the styrene monomer to generate active chain initiation units: subsequently, the active chain initiation units continue to react with other styrene monomers to form long-chain polystyrene. During the growth of the polystyrene chain, the acrylamide monomer also participates in the reaction to form a copolymer chain. Diethylenetriamine is used as a cross-linking agent to react with the polymer chain through its multiple amino groups to form a cross-linked network structure. The pore-forming agent forms a porous structure through phase separation and solvent evaporation during the reaction; the dispersant ensures the uniform distribution of the reaction system to prevent agglomeration. After 5-8 hours of reaction, the unreacted monomers and by-products are removed by suction filtration and washing, and then dried to obtain the target product, the resin PC307 for separating germanium. DETAILED DESCRIPTION
[0010] The present invention is further described below in conjunction with the embodiments, but the present invention is not limited in any way. Any changes or substitutions made based on the teachings of the present invention belong to the protection scope of the present invention.
[0011] The resin PC307 for separating germanium from a sodium germanate solution of the present invention is prepared by polymerization reaction with styrene as a skeleton and polar monomers acrylamide and diethylenetriamine as crosslinking agents.
[0012] The molar ratio of styrene, acrylamide and diethylenetriamine is (15-30): (5-10): 1.
[0013] The preparation method of the resin PC307 for separating germanium from a sodium germanate solution of the present invention is to use styrene as a skeleton, introduce polar monomers acrylamide and diethylenetriamine as crosslinking agents, add a pore-forming agent, a dispersant and an initiator, stir and react in a water bath at 60-80° C. under a nitrogen atmosphere for 5-8 hours, and then filter, wash and dry to obtain the target resin PC307 for separating germanium.
[0014] The pore-forming agent is toluene, and the added amount is 0.5-1.5% of the mass of the polar monomer.
[0015] The dispersant is gelatin, and the added amount is 0.5-1.5% of the mass of the polar monomer.
[0016] The initiator is benzoyl peroxide, and the added amount is 0.5-1.5% of the mass of the polar monomer.
[0017] The drying is vacuum drying, the drying temperature is 60-80°C, and the drying time is 8-12 hours.
[0018] The application of the resin PC307 for separating germanium from a sodium germanate solution of the present invention is the application of the resin PC307 for separating germanium from a sodium germanate solution in a process for extracting germanium from a sodium germanate solution.
[0019] The application of the resin PC307 for separating germanium from the sodium germanate solution in the process of extracting germanium from the sodium germanate solution is to stir and adsorb the sodium germanate solution using the resin PC307 for separating germanium from the sodium germanate solution.
[0020] The stirring adsorption is carried out at a temperature of 40-50°C and for a time of 20-24 hours.
[0021] The present invention is further described below with specific implementation cases: Example 1 With styrene (St) as the skeleton, polar monomer acrylamide (AM) was introduced, diethylenetriamine (DTA) was used as a crosslinker, toluene was used as a pore-forming agent, gelatin was used as a dispersant, and benzoyl peroxide was used as an initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA was 15:5:1, and toluene, gelatin and benzoyl peroxide were 0.5% of the monomer mass. Nitrogen was introduced into the system, and stirred in a water bath at 60-70°C for 8 hours. After the reaction was completed, the system was filtered and washed, and then placed in a vacuum drying oven at 60°C for 12 hours to obtain the resin PC307 for separating germanium.
[0022] Example 2 With styrene (St) as the skeleton, polar monomer acrylamide (AM) was introduced, diethylenetriamine (DTA) was used as a crosslinker, toluene was used as a pore-forming agent, gelatin was used as a dispersant, and benzoyl peroxide was used as an initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA was 30:10:1, and toluene, gelatin and benzoyl peroxide were 1% of the monomer mass. Nitrogen was introduced into the system, and stirred in a water bath at 70~80℃ for 5h. After the reaction was completed, it was filtered and washed, and placed in a vacuum drying oven at 70℃ for 10h to obtain the resin PC307 for separating germanium.
[0023] Example 3 With styrene (St) as the skeleton, polar monomer acrylamide (AM) was introduced, diethylenetriamine (DTA) was used as a crosslinker, toluene was used as a pore-forming agent, gelatin was used as a dispersant, and benzoyl peroxide was used as an initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA was 20:8:1, and toluene, gelatin and benzoyl peroxide were 1.5% of the monomer mass. Nitrogen was introduced into the system, and stirred in a water bath at 65-70°C for 6 hours. After the reaction was completed, the system was filtered and washed, and then placed in a vacuum drying oven at 80°C for 8 hours to obtain the resin PC307 for separating germanium.
[0024] Example 4 With styrene (St) as the skeleton, polar monomer acrylamide (AM) was introduced, diethylenetriamine (DTA) was used as a crosslinker, toluene was used as a pore-forming agent, gelatin was used as a dispersant, and benzoyl peroxide was used as an initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA was 25:7:1, and toluene, gelatin and benzoyl peroxide accounted for 0.8% of the monomer mass. Nitrogen was introduced into the system, and stirred in a water bath at 68~72℃ for 7h. After the reaction was completed, the system was filtered and washed, and then placed in a vacuum drying oven at 65℃ for 10h to obtain the resin PC307 for separating germanium.
[0025] Example 5 With styrene (St) as the skeleton, polar monomer acrylamide (AM) was introduced, diethylenetriamine (DTA) was used as a crosslinker, toluene was used as a pore-forming agent, gelatin was used as a dispersant, and benzoyl peroxide was used as an initiator to initiate the polymerization reaction. Among them, the molar ratio of St, AM and DTA was 18:6:1, and toluene, gelatin and benzoyl peroxide accounted for 1.2% of the monomer mass. Nitrogen was introduced into the system, and stirred in a water bath at 72~75℃ for 6h. After the reaction was completed, it was filtered and washed, and placed in a vacuum drying oven at 75℃ for 9h to obtain the resin PC307 for separating germanium.
[0026] Comparative Example 1 The School of Chemistry of Liaoning University used AB-8 macroporous adsorption resin to adsorb germanium-containing sulfuric acid solution, controlled the temperature at 25°C and pH at 1.0, and adsorbed for 2 hours under stirring and oscillating conditions, with an extraction rate of germanium of about 77%; the School of Materials Science and Engineering of Huazhong University of Science and Technology used methylglucamine resin to selectively adsorb germanium in germanium-containing solution under alkaline conditions (pH ≥ 9), with a stirring temperature of 20~65°C and a time of 30 minutes, and the effective recovery rate of germanium was above 70%.
[0027] Example 6 The test was conducted using the resin PC307 for separating germanium prepared in Example 1, as follows: Accurately measure 6% (mass of sodium germanate) of resin PC307 and add it to 100g / L sodium germanate solution. Stir and adsorb at 40-50℃ for 20-24h. After the reaction is completed, desorb the adsorbed product with anhydrous ethanol. The extraction rate of germanium reaches 85-90%.
[0028] Example 7 The resin PC307 for separating germanium from the sodium germanate solution prepared in Example 2, Example 3, Example 4, and Example 5 was tested respectively, using the same method as Example 6. The results all showed that the extraction rate of germanium by the resin PC307 for separating germanium from the sodium germanate solution of the present invention reached 85-90%.
Claims
1. A resin PC307 for separating germanium from a sodium germanate solution, characterized in that: The resin PC307 for separating germanium from the sodium germanate solution is prepared by polymerization reaction with styrene as the skeleton and polar monomers acrylamide and diethylenetriamine as crosslinking agents.
2. The resin PC307 for separating germanium from sodium germanate solution according to claim 1, characterized in that: The molar ratio of styrene, acrylamide and diethylenetriamine is (15-30): (5-10):
1.
3. A method for preparing resin PC307 for separating germanium from sodium germanate solution according to 1 or 2, characterized in that: The method is based on styrene as the skeleton, and polar monomers acrylamide and diethylenetriamine are introduced as cross-linking agents. Pore-forming agents, dispersants and initiators are added. Under a nitrogen atmosphere, the reaction is stirred in a water bath at 60-80°C for 5-8 hours. After filtration, washing and drying, the target resin PC307 for separating germanium is obtained.
4. The preparation method according to claim 3, characterized in that: The pore-forming agent is toluene, and the added amount is 0.5-1.5% of the mass of the polar monomer.
5. The preparation method according to claim 3, characterized in that: The dispersant is gelatin, and the added amount is 0.5-1.5% of the mass of the polar monomer.
6. The preparation method according to claim 3, characterized in that: The initiator is benzoyl peroxide, and the added amount is 0.5-1.5% of the mass of the polar monomer.
7. The preparation method according to claim 3, characterized in that: The drying is vacuum drying, the drying temperature is 60-80°C, and the drying time is 8-12 hours.
8. Use of resin PC307 for separating germanium from sodium germanate solution according to claim 1 or 2, characterized in that: The resin PC307 for separating germanium from a sodium germanate solution is used in a process for extracting germanium from a sodium germanate solution.
9. The use according to claim 8, characterized in that: The application of the resin PC307 for separating germanium from the sodium germanate solution in the process of extracting germanium from the sodium germanate solution is to stir and adsorb the sodium germanate solution using the resin PC307 for separating germanium from the sodium germanate solution.
10. The use according to claim 8, characterized in that: The stirring adsorption is carried out at a temperature of 40-50°C and for a time of 20-24 hours.