High-efficiency collagen cleaning agent without surfactant component and preparation method of high-efficiency collagen cleaning agent

Through the method of adsorption and emulsion formation of natural collagen at the oil-water interface and dispersed and used directly in the aqueous solution, the harm problems of traditional detergents to the human body and the environment are solved, and high-efficiency and green cleaning effects and low-cost Preparation process.

CN119020120APending Publication Date: 2024-11-26FUJIAN UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410983078.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The surfactants used in traditional cleaning and cleaning agents are harmful to the human body and the environment, and their preparation process is complex and costly, which cannot meet market demand.

Method used

Natural collagen molecules with high aspect ratio are used to clean oil stains by adsorption and emulsion formation at the oil-water interface, and directly disperse and use in aqueous solution, avoiding the chemical modification process, and using a high-speed homogenizer to homogenize collagen Quality treatment.

Benefits of technology

It realizes efficient cleaning, low toxicity, low irritation, green and environmentally friendly detergent, reduces environmental pollution, reduces wastewater treatment burden, and has moisturizing and water-locking skin care effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119020120A_ABST
    Figure CN119020120A_ABST
Patent Text Reader

Abstract

The invention discloses a high-efficiency collagen cleaning agent without a surfactant component and a preparation method of the high-efficiency collagen cleaning agent. The preparation method comprises the following steps: extracting spongy collagen from cow leather, adding the spongy collagen into an aqueous solution, and homogenizing by using a high-speed homogenizer to obtain the collagen cleaning agent. According to the invention, the limitation of cleaning by using a traditional surfactant is broken through, collagen molecules with natural high length-diameter ratio are continuously adsorbed to an oil-water interface in the cleaning process to reduce the tension of the oil-water interface, and finally, tightly wrapped emulsion droplets are formed to realize oil stain cleaning.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of detergents, and in particular to a high-efficiency collagen cleaning agent without surfactant components and a preparation method thereof. Background Art

[0002] In traditional cleaning agents, the selection of surfactants only considers how to achieve the best effect, such as cleaning, foaming, emulsification, etc., and rarely considers its impact on the natural state of skin, hair or fabrics. In recent years, people have gradually realized that the hazards of chemical surfactants are mainly concentrated in irritation to human mucous membranes, skin sensitization, hemolysis and environmental pollution. People have begun to attach great importance to the safety of washing daily necessities and the harm to the environment. At present, the surfactants in mainstream household cleaning agents on the market are mainly extracted from fatty alcohols of plants, natural fats or oils, and a small part is produced by microbial metabolism. Therefore, the development of safer and more sustainable household cleaning agents has gradually attracted people's attention.

[0003] Collagen is widely available and has good biodegradability, biocompatibility, regeneration and emulsion stability. These characteristics make collagen an ideal candidate material for detergents. In addition, collagen is also the main structural component of human skin. Therefore, collagen detergents have natural affinity, which is of great significance for improving the safety of cleaning products. Patent application CN2011101086203 reports a collagen surfactant modified by anhydride grafting. The combination includes 10 parts of undenatured natural collagen, 1 to 30 parts of long-chain anhydrides, 2 to 8 parts of short-chain anhydrides, 10-500 parts of organic solvents, and 50-500 parts of deionized water. The surfactant prepared by this patent has low toxicity, low irritation, and can be miscible with water in a neutral environment, laying the foundation for expanding the application range of collagen.

[0004] Collagen surfactants prepared by existing technology mainly impart surface activity to collagen by grafting hydrophilic and hydrophobic groups through chemical modification. This process usually involves an acylation reaction in an organic solvent to graft hydrophilic and hydrophobic groups on both sides of the collagen molecule; and during the modification process, the pH value needs to be adjusted at any time to maintain the alkaline conditions of the reaction system. In addition, in order to avoid side reactions such as denaturation of collagen and hydrolysis of hydrophilic and hydrophobic groups, the modification process usually needs to react at room temperature, resulting in a very slow reaction rate for chemical modification, making the production cycle of collagen surfactants very long. At the same time, the cleaning effect of the produced surfactants is also poor, which cannot meet the market demand for cleaning agents.

[0005] Compared with collagen surfactants obtained by chemical modification, natural collagen has outstanding characteristics such as low time and economic cost, good emulsion stability, and good cleaning effect. Therefore, the development of natural collagen as a green, efficient and surfactant-free cleaning agent can not only improve the safety performance of existing cleaning agents and obtain high-performance cleaning agents, but also has important significance for promoting innovation and sustainable development in the field of cleaning agents. Summary of the invention

[0006] Traditional detergents usually contain a large amount of surfactants, which bring great harm to the human body and the environment. The purpose of the present invention is to provide a highly efficient collagen cleaning agent without surfactant ingredients and a preparation method thereof. The present invention takes the oil stain removal mechanism of surfactants into consideration, utilizes the adsorption characteristics of natural collagen molecules with a high aspect ratio at the oil-water interface, and achieves the cleaning purpose by tightly wrapping the oil stains to form an emulsion and dispersing it in water.

[0007] In order to achieve the above object, the technical solution adopted by the present invention is as follows: A method for preparing a high-efficiency collagen cleaning agent without surfactant components comprises the following steps: 1) Preparation of collagen Cutting defatted and protein-free calfskin into small pieces and crushing them with a grinder, extracting the obtained powder with 0.5 mol / L acetic acid containing 2.8-3.2% pepsin at 4°C for 70-75 h to obtain a mixture, wherein the mass ratio of the powder to the acetic acid is 1-1.5:3000, then centrifuging the mixture at 8000-10000 g at 4°C to collect the supernatant, adding NaCl to the supernatant to a final concentration of 0.7-0.75 mol / L to precipitate collagen, dissolving it with 0.1 mol / L acetic acid and dialyzing it for 72-80 h, and finally freeze-drying the dialyzed collagen to obtain sponge collagen and storing it at 4°C; 2) Preparation of collagen detergent solution Add sponge-like collagen into pure water solution with a collagen concentration of 0.1-10%, and use a high-speed homogenizer to homogenize at a speed of 5000-15000 r / min for 30-180 s to obtain a collagen cleaning agent.

[0008] The present invention breaks the limitation of using traditional surfactants for cleaning, and uses collagen molecules with a natural high aspect ratio to reduce the oil-water interfacial tension by continuously adsorbing to the oil-water interface during the cleaning process, and finally forms tightly wrapped emulsion droplets to achieve oil stain cleaning. The present invention uses a method of destroying the hydrogen bonds between collagen molecules by high-speed shearing to directly disperse the natural collagen sponge in an aqueous solution, and can be directly used as a cleaning agent without further chemical modification to a surfactant, breaking through the limitation of relying on surfactants to achieve cleaning in traditional methods. In addition, collagen has extremely high natural moisturizing and water-locking properties, which enables it to protect the loss of skin moisture while removing oil stains, and plays a role in water retention and skin care. Most importantly, the wastewater after collagen cleaning is non-toxic and non-irritating, and will not cause any adverse effects on the ecological environment after discharge, and also greatly reduces the burden of wastewater treatment. The present invention provides a feasible way to prepare a fully green and eco-friendly collagen cleaning agent.

[0009] Compared with the common cleaning agents currently on the market, the collagen cleaning agent provided by the present invention has the following advantages: 1. The collagen raw material is green and environmentally friendly, and has a high affinity to human skin, leather, etc.; 2. No chemical modification is required, the preparation process is green and environmentally friendly, and the cost is low; 3. While efficiently cleaning, it has a wide range of applications, high safety, good water retention and water locking capabilities, is green and degradable, and greatly reduces environmental pollution after use. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 Comparison chart of collagen cleaner and commercial cleaner, where (a), (b), (c), and (d) are cleaning pictures of cowhide, human skin, fabric, and dishes, respectively.

[0011] Figure 2 Provides collagen cleansers with the moisture-locking ability of commercial skin cleansers. DETAILED DESCRIPTION Example 1

[0012] The defatted and protein-free cowhide was cut into small pieces and crushed with a grinder. The obtained powder was extracted with 0.5 mol / L acetic acid containing 3% pepsin at 4°C for 70 hours to obtain a mixture, the mass ratio of the powder to the acetic acid was 1:3000, and then the mixture was centrifuged at 8000 g at 4°C to collect the supernatant. NaCl was added to the supernatant to a final concentration of 0.7 mol / L to precipitate collagen, which was then dissolved with 0.1 mol / L acetic acid and dialyzed for 72 hours. Finally, the dialyzed collagen was freeze-dried to obtain spongy collagen and stored at 4°C.

[0013] 0.05 g of sponge collagen was added to 20 ml of pure water solution and homogenized at 5000 r / min for 30 s using a high-speed homogenizer to obtain a 0.25% w / v collagen detergent. Example 2

[0014] The defatted and protein-free cowhide was cut into small pieces and crushed with a grinder. The obtained powder was extracted with 0.5 mol / L acetic acid containing 3.2% pepsin at 4°C for 72 hours to obtain a mixture, the mass ratio of the powder to the acetic acid was 1.25:3000, and then the mixture was centrifuged at 9000 g at 4°C to collect the supernatant. NaCl was added to the supernatant to a final concentration of 0.75 mol / L to precipitate collagen, which was then dissolved with 0.1 mol / L acetic acid and dialyzed for 76 hours. Finally, the dialyzed collagen was freeze-dried to obtain spongy collagen and stored at 4°C.

[0015] 0.2 g of sponge collagen was added to 20 ml of pure water solution and homogenized at 10000 r / min for 90 s using a high-speed homogenizer to obtain a 1.0% w / v collagen detergent. Example 3

[0016] The defatted and protein-free cowhide was cut into small pieces and crushed with a grinder. The obtained powder was extracted with 0.5 mol / L acetic acid containing 3% pepsin at 4 °C for 75 h to obtain a mixture, the mass ratio of the powder to acetic acid was 1.5:3000, and then the mixture was centrifuged at 10000 g at 4 °C to collect the supernatant. Collagen was precipitated by adding NaCl to a final concentration of 0.7 mol / L. It was then dissolved with 0.1 mol / L acetic acid and dialyzed for 80 h. Finally, the dialyzed collagen was freeze-dried to obtain spongy collagen and stored at 4 °C.

[0017] 2 g of sponge collagen was added to 20 ml of pure water solution and homogenized at 15000 r / min for 180 s using a high-speed homogenizer to obtain a 10% w / v collagen detergent. Example 4

[0018] Cleaning experiment 1. Fabric cleaning Cut textile fabrics (polyester and cotton) into 5×5 cm 2The fabric surface was stained with an equal amount of chili oil or tomato sauce to simulate dirty stains on clothes. After the fabric was dried for 4 h, 3 mL of the collagen detergent prepared in Example 1 and commercial laundry detergent were added to the surface respectively, and deionized water without any detergent was used as a blank control. Then, the fabric was manually scrubbed for 60 s at the same angle and speed as the actual cleaning process to simulate the actual cleaning process, and then rinsed with deionized water for 3 times.

[0019] 2. Tableware cleaning Various tableware such as plates (ceramic, stainless steel, glass and plastic plates) were coated with the same amount of chili oil. Then, 3 mL of the collagen cleaner prepared in Example 1 and commercial dishwashing liquid were dripped onto the surface of the plates, and deionized water without any detergent was used as a blank control. The plates were wiped in a circular motion for 30 s at room temperature using a cleaning sponge, and then rinsed with deionized water three times.

[0020] 3.Leather cleaning Cut the purchased cowhide into 4×4 cm 2 The cowhide surface was stained with equal amounts of chili oil and ketchup to simulate stains on daily leather materials. After drying at room temperature for 4 h, 3 mL of the collagen cleaner prepared in Example 1 and commercial leather cleaner were added to the surface, and deionized water without any detergent was used as a blank control. The cleaning sponge was wiped in a circular motion for 30 s, and then rinsed with deionized water 3 times.

[0021] 4. Skin cleansing A clean area was marked on the flexion side of the left and right forearms, and then an equal amount of edible oil (such as corn oil and soybean oil) was stained on the area, and the oil stain was evenly spread into a circle (Φ2×2 cm). Then, 3 ml of the collagen cleanser prepared in Example 1 and the commercial skin cleanser were dripped on the surface of the arm, and rubbed in a circular motion with fingers for 30 seconds, and then rinsed with deionized water 3 times.

[0022] Phenomenon: The cleaning effect of the collagen cleanser of the present invention is compared with the common cleansers on the market. Figure 1 As shown. Figure 1 It is known that collagen cleaners are as effective or better than commonly used cleaners on the market for cleaning cowhide, human skin, fabrics and dishes.

[0023] The water-retaining and water-locking effect of the collagen cleanser of the present invention is compared with that of common cleansers on the market. Figure 2 As shown. Figure 2 It can be seen that collagen cleansers have lower transepidermal water loss and higher stratum corneum water content.

Claims

1. A method for preparing a highly effective collagen cleaning agent without surfactant components, characterized in that: The following steps are involved: 1) Preparation of collagen The defatted and protein-free calfskin was cut into small pieces and crushed with a grinder. The obtained powder was extracted with 0.5 mol / L acetic acid containing pepsin at 4°C for 70-75 h to obtain a mixture. The mixture was then centrifuged at 4°C, the supernatant was collected, NaCl was added to the supernatant to a final concentration of 0.7-0.75 mol / L to precipitate collagen, and then dissolved with 0.1 mol / L acetic acid and dialyzed for 72-80 h. Finally, the dialyzed collagen was freeze-dried to obtain sponge collagen. 2) Preparation of collagen detergent solution The sponge-like collagen is added into the aqueous solution and homogenized by using a high-speed homogenizer to obtain a collagen cleaning agent.

2. The method for preparing a surfactant-free high-efficiency collagen cleaning agent according to claim 1, characterized in that: In step 1), the mass content of pepsin in acetic acid is 2.8-3.2%.

3. The method for preparing a surfactant-free high-efficiency collagen cleaning agent according to claim 1, characterized in that: In step 1), the mass ratio of the powder to acetic acid is 1-1.5:3000.

4. The method for preparing a surfactant-free high-efficiency collagen cleaning agent according to claim 1, characterized in that: In step 1), the centrifugal force of the centrifugation is 8000~1000g.

5. The method for preparing a surfactant-free high-efficiency collagen cleaning agent according to claim 1, characterized in that: In step 2), the collagen concentration in the collagen cleaning agent is 0.1-10%.

6. The method for preparing a surfactant-free high-efficiency collagen cleaning agent according to claim 1, characterized in that: In step 2), the speed of the high-speed homogenizer is 5000~15000 r / min, and the homogenization time is 30~180 s.

7. A collagen cleaning agent obtained according to the preparation method according to any one of claims 1 to 6.