Electromagnetic coupling three-coil differential metal layer thickness measuring device and manufacturing method

Through the electromagnetically coupled three-coil differential metal layer thickness measurement device, the problem of long testing time and only one metal can be measured in the prior art is solved, and the thickness measurement distinction between iron, stainless steel and aluminum is achieved at a single frequency, improving the improvement of The detection speed and sensitivity are suitable for the thickness detection of a variety of metal materials.

CN119022773AActive Publication Date: 2024-11-26DALIAN MARITIME UNIVERSITY
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411272095.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-26
Estimated Expiration
2044-09-11

AI Technical Summary

Technical Problem

The existing metal thickness measurement technology has a long test time and can only measure ferromagnetic or non-ferromagnetic metals, and requires a large amount of data to be complex after-processed, making it difficult to distinguish metals such as iron, stainless steel and aluminum at a single frequency. .

Method used

The electromagnetically coupled three-coil differential metal layer thickness measurement device is used. The detection coil is connected in parallel through filter capacitors. The excitation coil is closely attached to the detection coil. The signal processing is performed using a phase-locked amplifier and an operational amplifier to generate alternating currents of the same frequency, amplitude and phase. The signal is electromagnetically coupled to extract the thickness characteristics of iron, stainless steel and aluminum.

Benefits of technology

The thickness measurement distinction between iron, stainless steel and aluminum is achieved under a single AC excitation frequency, the detection speed and sensitivity are improved, and the thickness-related characteristics can be extracted at different lifting distances, which is suitable for thickness detection of a variety of metal materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119022773A_ABST
    Figure CN119022773A_ABST
Patent Text Reader

Abstract

The invention provides an electromagnetic coupling three-coil differential metal layer thickness measuring device and a manufacturing method, the device comprises a three-coil differential metal layer thickness measuring sensor, a signal processor and an alternating current signal generator, the sensor comprises a filter capacitor, an excitation coil and a detection coil, the filter capacitor is connected in parallel with the detection coil, and the excitation coil is connected in parallel with the detection coil. The excitation coil is tightly attached to the lower portion of the detection coil. The detection coil comprises two planar coils which are connected in series; the signal processor comprises a lock-in amplifier and an operational amplifier, and the lock-in amplifier is provided with two signal channels and used for removing noise similar to an excitation signal in a pickup signal; the operational amplifier gains and amplifies the direct-current signal; the alternating current signal generator is used for generating two identical alternating current signals, one signal is connected to the excitation coil, and the other signal and the detection coil are jointly connected to the lock-in amplifier. The method has high sensitivity and detection speed, can evaluate various characteristics of the material, and is suitable for detecting the thickness of the metal material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of non-destructive thickness measurement and sensor technology, and in particular to an electromagnetically coupled three-coil differential metal layer thickness measurement device and a manufacturing method thereof. Background Art

[0002] In the field of mechanical manufacturing, due to corrosion and friction during the use of various equipment, the walls of equipment and parts will gradually become thinner. Regularly measuring the wall thickness of equipment is an effective means to achieve real-time control of equipment status, ensure healthy operation of equipment, and reduce the risk of failure.

[0003] The eddy current detection method has the advantages of not needing to destroy or change the surface of the material, high sensitivity, fast detection speed, and the ability to evaluate multiple material properties. It is particularly suitable for detecting the thickness of metal materials. In many industrial scenarios, internal thickness measurement of metal machinery is mandatory, and regular thickness measurement helps monitor the wear of equipment parts. It also plays an important role in ensuring the safety and efficient participation of equipment in production. In recent years, the thickness measurement of metal layers is mostly based on the principle that metals of different thicknesses have different impedance values ​​at different frequencies, and the metal thickness is distinguished by frequency sweeping, and the overall experiment is complicated.

[0004] The current research on metal thickness measurement of lithium battery balancing technology has the following problems:

[0005] The phase characteristics are measured and analyzed using a swept frequency test. Although this method can ignore the influence of some lift-off effects, the test time is long; the metal thickness measurement using a single frequency can mostly only measure one of the ferromagnetic metal and non-ferromagnetic metal, and the analyzed characteristics mostly need to be further extracted from the original data; the method of using algorithms to extract features from the original data to distinguish metals of different thicknesses often requires a large amount of data as support, and still requires relatively complex post-processing. Summary of the invention

[0006] According to the technical problems raised above, an electromagnetically coupled three-coil differential metal layer thickness measuring device and a manufacturing method are provided. The present invention provides an electromagnetically coupled three-coil differential metal layer thickness measuring sensor, which can measure the thickness of ferromagnetic and non-ferromagnetic metals such as iron, stainless steel, and aluminum under a single AC excitation frequency. At the same time, it can also use the original data at different lift-off distances to extract one or more thickness-related features of metals of different properties that are little affected by the lift-off distance.

[0007] The technical means adopted by the present invention are as follows:

[0008] An electromagnetically coupled three-coil differential metal layer thickness measuring device comprises: a three-coil differential metal layer thickness measuring sensor, a signal processor and an AC signal generator, wherein:

[0009] The three-coil differential metal layer thickness sensor comprises a filter capacitor, an excitation coil and a detection coil, wherein the filter capacitor is connected in parallel to the detection coil, and the excitation coil is closely attached to the bottom of the detection coil; the detection coil comprises two planar coils connected in series;

[0010] The signal processor includes a phase-locked amplifier and an operational amplifier, wherein the phase-locked amplifier has two signal channels, and the two input signals have the same frequency and amplitude, and is used to remove noise similar to the excitation signal in the pickup signal and extract a response signal related to the excitation signal; the operational amplifier receives the DC signal output by the phase-locked amplifier and is used to gain amplify the DC signal;

[0011] The AC signal generator is used to generate two AC signals with the same frequency, amplitude and phase. One AC signal is connected to the excitation coil, and the other AC signal and the detection coil are connected to the phase-locked amplifier. The phase-locked amplifier compares, processes and amplifies the input signal, and then outputs a DC signal to the operational amplifier for secondary amplification.

[0012] Furthermore, the excitation coil is used to electromagnetically couple with the detection coil to obtain information of the three-coil differential metal layer thickness measurement sensor and transmit energy to the three-coil differential metal layer thickness measurement sensor.

[0013] Furthermore, the two planar coils are connected in series and then connected in parallel with a filter capacitor to achieve filtering and regulating functions in the circuit.

[0014] Furthermore, the excitation coil is wound by enameled copper wire with a wire diameter of 70 μm, the coil is a single layer with 79 turns, an inner diameter of 1 mm, and an outer diameter of 15 mm.

[0015] Furthermore, the two planar coils are both wound with enameled copper wires with a wire diameter of 70 μm, and the coils are both single-layer 35 turns, with an inner diameter of 1 mm and an outer diameter of 5 mm.

[0016] Furthermore, both ends of the excitation coil and the detection coil are connected with leads, but there is no wire connection between the excitation coil and the detection coil, and the leads are all arranged on one side of the three-coil differential metal layer thickness sensor.

[0017] Furthermore, the electromagnetically coupled three-coil differential metal layer thickness measuring device also includes a data acquisition card and a LabVIEW data acquisition unit. The data acquisition card is connected to the operational amplifier, and the LabVIEW data acquisition unit is connected to the data acquisition card. The data acquisition card is used to collect the signal after secondary amplification and input the collected signal into the LabVIEW data acquisition unit.

[0018] The present invention also provides a method for manufacturing the electromagnetic coupling three-coil differential metal layer thickness measuring device, comprising:

[0019] S1. Place the large diameter coil in the lower layer as the excitation coil; place two small diameter coils on the upper layer of the large diameter coil as the detection coils, and there is no wire connection between the excitation coil and the detection coil;

[0020] S2. Clean and inspect the excitation coil to ensure that it meets the requirements. Select an acrylic plate of appropriate size to raise the excitation coil. Fit the excitation coil tightly to the acrylic plate and fix it at the center of the slide to achieve the best measurement effect.

[0021] S3. Clean and inspect the detection coil to ensure that it meets the requirements. Fix the filter capacitor on the glass slide. Place the two detection coils horizontally opposite to each other so that the detection coils fit closely with the excitation coils. Connect one end of the two detection coils and connect the other end to the filter capacitor in parallel and weld them firmly.

[0022] S4. Use an AC signal generator to generate two AC signals with exactly the same frequency, amplitude, and phase; one signal is input into the excitation coil, and the other signal and the detection coil are connected to the two signal channels of the phase-locked amplifier respectively; the phase-locked amplifier processes and amplifies the two signals and outputs a stable DC signal to the operational amplifier, which is then sent to the data acquisition card for data collection after secondary amplification.

[0023] Compared with the prior art, the present invention has the following advantages:

[0024] 1. The electromagnetically coupled three-coil differential metal layer thickness measuring device provided by the present invention can measure the thickness of ferromagnetic and non-ferromagnetic metals such as iron, stainless steel, and aluminum at a single AC excitation frequency.

[0025] 2. The electromagnetically coupled three-coil differential metal layer thickness measuring device provided by the present invention can use raw data at different lift-off distances to extract one or more thickness-related features of metals of different properties that are little affected by the lift-off distance.

[0026] 3. The electromagnetically coupled three-coil differential metal layer thickness measuring device provided by the present invention has high sensitivity and detection speed, can evaluate various material properties, and is particularly suitable for detecting the thickness of metal materials.

[0027] 4. The electromagnetically coupled three-coil differential metal layer thickness measuring device provided by the present invention adopts a three-coil structure. The winding methods of the two pickup coils are opposite, so that the signals generated by the coils cancel each other out. The initial value of the superimposed signal is at 0, thereby increasing its relative change value.

[0028] Based on the above reasons, the present invention can be widely promoted in the fields of sensors and the like. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0030] Figure 1 It is a schematic structural diagram of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention.

[0031] Figure 2 This is a schematic diagram of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention.

[0032] Figure 3 This is a structural diagram of the three-coil differential metal layer thickness sensor of the present invention.

[0033] Figure 4 This is a structural diagram of the signal processor of the present invention.

[0034] Figure 5 A diagram of the detection signal amplitudes of different metal samples of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention.

[0035] Figure 6 The magnetic flux mode density inside the coil of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention.

[0036] Figure 7 This is a coil signal simulation diagram of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention.

[0037] Figure 8 A simplified schematic diagram of a detection system for an electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention.

[0038] Fig. 9 This is a diagram showing the detection results of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention at a 1mm lifting distance for different stainless steel plate samples.

[0039] Fig.10 This is a diagram of the detection results of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention at different iron plate samples with a lifting distance of 1 mm.

[0040] Fig.11This is a diagram of the detection results of the electromagnetically coupled three-coil differential metal layer thickness measuring device provided in an embodiment of the present invention at a lifting distance of 1 mm for different aluminum plate samples.

[0041] In the figure: 1. Three-coil differential metal layer thickness sensor; 2. Signal processing circuit; 3. AC signal generator (RIGOL DG812 10MHZ dual channel); 4. Filter capacitor; 5. Excitation coil; 6. Detection coil; 7. Phase-locked amplifier; 8. Operational amplifier; 9. Data acquisition card (DAQ) (NI USB_6211, National Instruments, USA); 10. LabVIEW data acquisition unit; 11. Test sample support platform; 12. Dual-axis linear synchronous belt slip test bench. DETAILED DESCRIPTION

[0042] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0043] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0044] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit exemplary embodiments according to the present invention. As used herein, unless the context clearly indicates otherwise, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "comprising" and / or "including" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof.

[0045] Unless otherwise specifically stated, the relative arrangement of the parts and steps described in these embodiments, the numerical expressions and numerical values ​​do not limit the scope of the present invention. At the same time, it should be clear that, for ease of description, the sizes of the various parts shown in the drawings are not drawn according to the actual proportional relationship. The technology, methods and equipment known to ordinary technicians in the relevant field may not be discussed in detail, but in appropriate cases, the technology, methods and equipment should be regarded as part of the authorization specification. In all examples shown and discussed here, any specific value should be interpreted as merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar numbers and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further discussed in subsequent drawings.

[0046] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by directional words such as "front, back, up, down, left, right", "lateral, vertical, perpendicular, horizontal" and "top, bottom" are usually based on the directions or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the device or element referred to must have a specific direction or be constructed and operated in a specific direction. Therefore, they cannot be understood as limiting the scope of protection of the present invention: the directional words "inside and outside" refer to the inside and outside relative to the contours of each component itself.

[0047] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used here to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below their position devices or structures". Thus, the exemplary term "above" can include both "above" and "below". The device can also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used here are interpreted accordingly.

[0048] In addition, it should be noted that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. If not otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present invention.

[0049] like Figure 1As shown, the present invention provides an electromagnetically coupled three-coil differential metal layer thickness measuring device, comprising: a three-coil differential metal layer thickness measuring sensor 1, a signal processor 2 and an AC signal generator 3, wherein:

[0050] The three-coil differential metal layer thickness sensor 1 comprises a filter capacitor 4, an excitation coil 5 and a detection coil 6, wherein the filter capacitor 4 is connected in parallel to the detection coil 6, and the excitation coil 5 is closely attached to the bottom of the detection coil 6; the detection coil 6 comprises two planar coils connected in series; Figure 2 , 3 As shown, the two planar coils are connected in series and then connected in parallel with the filter capacitor 4 to achieve specific filtering and regulating functions in the circuit.

[0051] The signal processor 2 includes a phase-locked amplifier 7 and an operational amplifier 8, wherein the phase-locked amplifier 7 has two signal channels, and the two input signals have exactly the same frequency and amplitude, and is used to remove noise similar to the excitation signal in the pickup signal and extract a response signal related to the excitation signal; the operational amplifier 8 receives the DC signal output by the phase-locked amplifier 7 and is used to gain amplify the DC signal; to meet the input requirements of the subsequent data acquisition system, ensure signal strength and accuracy, so as to carry out effective data acquisition and detailed signal analysis.

[0052] The AC signal generator 3 is used to generate two AC signals with the same frequency, amplitude and phase, such as Figure 4 As shown, one AC signal is connected to the excitation coil 5, and the other AC signal and the detection coil 6 are connected together to the phase-locked amplifier 7. The phase-locked amplifier 7 compares, processes and amplifies the input signal, and then outputs a DC signal to the operational amplifier 8 for secondary amplification.

[0053] In specific implementation, as a preferred embodiment of the present invention, the excitation coil 5 is used to electromagnetically couple with the detection coil 6 to obtain information of the three-coil differential metal layer thickness sensor 1 and transmit energy to the three-coil differential metal layer thickness sensor 1.

[0054] In specific implementation, as a preferred embodiment of the present invention, the excitation coil 5 is wound by enameled copper wire with a wire diameter of 70 μm, the coil is a single layer with 79 turns, an inner diameter of 1 mm, and an outer diameter of 15 mm.

[0055] In specific implementation, as a preferred embodiment of the present invention, the two planar coils are both wound by enameled copper wire with a wire diameter of 70 μm, and the coils are both single-layer 35 turns, with an inner diameter of 1 mm and an outer diameter of 5 mm.

[0056] In a specific implementation, as a preferred embodiment of the present invention, both ends of the excitation coil 5 and the detection coil 6 are connected with leads, but there is no wire connection between the excitation coil 5 and the detection coil 6, and the leads are all arranged on one side of the three-coil differential metal layer thickness sensor 1.

[0057] In specific implementation, as a preferred embodiment of the present invention, the electromagnetically coupled three-coil differential metal layer thickness measuring device also includes a data acquisition card 9 and a LabVIEW data acquisition unit 10. The data acquisition card 9 is connected to the operational amplifier 8, and the LabVIEW data acquisition unit 10 is connected to the data acquisition card 9. The data acquisition card 9 is used to collect the signal after secondary amplification and input the collected signal to the LabVIEW data acquisition unit 10. In this embodiment, the LabVIEW data acquisition unit 10 is a software for data acquisition and instrument control, which can control the application of excitation to the coil and simultaneously collect its signal changes. The entire process from the AC signal generator generating the signal to the final signal being written from the data acquisition card 9 (DAQ) is connected by an RF radio frequency line, so the signal interference is small and no filtering is required.

[0058] The present invention also provides a method for manufacturing the electromagnetic coupling three-coil differential metal layer thickness measuring device, comprising:

[0059] S1. The large diameter coil is arranged in the lower layer as the excitation coil 5; two small diameter coils are arranged in the upper layer of the large diameter coil as the detection coil 6, and there is no wire connection between the excitation coil 5 and the detection coil 6;

[0060] S2. Clean and inspect the excitation coil 5 to ensure that it meets the requirements, select an acrylic plate of appropriate size to raise the excitation coil 5, fit the excitation coil 5 tightly to the acrylic plate, and fix it at the center of the slide to achieve the best measurement effect;

[0061] S3, clean and check the detection coil 6 to ensure that the detection coil 6 meets the requirements, fix the filter capacitor 4 on the slide, place the two detection coils 6 horizontally opposite to each other, make the detection coil 6 fit closely with the excitation coil 5, and connect one end of the two detection coils 6, and the other end is connected in parallel with the filter capacitor 4 and welded firmly;

[0062] S4. Use the AC signal generator 3 to generate two AC signals with exactly the same frequency, amplitude and phase; one signal is input into the excitation coil 5, and the other signal and the detection coil 6 are respectively connected to the two signal channels of the phase-locked amplifier 7; the phase-locked amplifier 7 processes and amplifies the two signals and outputs a stable DC signal to the operational amplifier 8, which is then sent to the data acquisition card 9 for data collection after secondary amplification.

[0063] Example 1

[0064] like Figure 5 As shown in the figure, it is a signal amplitude diagram of different metal samples detected by the electromagnetic coupling three-coil differential metal layer thickness measuring device of the present invention. When the sample begins to approach the sensor, the iron sample and the aluminum sample are ferromagnetic material and non-ferromagnetic material respectively, so the induced voltage of the two changes in the opposite direction. When the first pickup coil is completely passed, the induced voltage of the aluminum sample and the iron sample reaches the peak and trough values ​​respectively. When the sensor is completely close to the sample, the influence of the secondary magnetic field disturbance of the aluminum sample gradually tends to be stable, the magnetic flux density is basically unchanged, and the induced electromotive force returns to the level before approaching the sample. Since the reverse disturbance of the secondary magnetic field of the iron sample gradually increases during the process of approaching the sensor, the coupling of the primary magnetic field enhancement and the secondary magnetic field disturbance still exists, the magnetic flux density changes are still occurring, and the induced electromotive force is different from that before approaching the sample. The magnetic permeability of the stainless steel sample is smaller than that of the iron sample, so the primary magnetic field enhancement is smaller than that of the iron sample, and the electrical conductivity is smaller than that of the aluminum sample, so the secondary magnetic field disturbance intensity is smaller than that of the aluminum sample. When the stainless steel sample begins to approach the sensor, the primary magnetic field enhancement rate is greater than the secondary magnetic field disturbance rate, and the induced voltage begins to change. When the sensor completely passes through the first pickup coil, the induced electromotive force reaches the trough value. When the sensor is completely close to the sample, the secondary magnetic field disturbance rate is greater than the primary magnetic field enhancement rate, and the induced electromotive force curve reaches the peak value. Then the secondary magnetic field disturbance tends to be stable and the curve decreases. Since the coupling between the primary magnetic field enhancement and the secondary magnetic field disturbance still exists, the magnetic flux density is still changing. At this time, the induced electromotive force of the detection coil is different from that before approaching the sample, but it is less than the change of the iron sample.

[0065] Example 2

[0066] like Figure 6 As shown, the internal magnetic flux mode density of the coil of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention is shown. The sensor parameters are that the excitation coil is a single-layer planar coil with 79 turns, an outer diameter of 15mm and an inner diameter of 1mm, and the two planar coils in the detection coil are both single-layer planar coils with 35 turns, an outer diameter of 5mm and an inner diameter of 1mm.

[0067] Example 3

[0068] like Figure 7 As shown in the figure, it is a coil signal simulation diagram of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention. When a single coil is used, no matter which plane coil in the detection coil, its initial value is not 0, which also makes the relative change value of the signal smaller. Therefore, we use a three-coil structure, and the winding methods of the two pickup coils are opposite, so that the signals generated by the coils cancel each other out, and the initial value of the superimposed signal is 0. Because the order of the signals is different, the time when the superimposed signal changes is different, which in turn causes the change of the superimposed signal and increases its relative change value.

[0069] Example 4

[0070] like Figure 8 As shown, it is a schematic diagram of the detection system of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention. The present invention tests aluminum, iron, and stainless steel materials of different thicknesses. In order to ensure the stability of the sample properties, the same metal samples of different thicknesses are processed from the same piece of metal. The types, thicknesses, and numbers of the samples are shown in the following table.

[0071]

[0072] Example 5

[0073] like Fig. 9 As shown in the figure, the electromagnetic coupling three-coil differential metal layer thickness measuring device of the present invention is tested at different 1mm lifting distances of stainless steel plate samples. The 1-5 stainless steel plate samples are tested at 50kHz excitation frequency and 1mm lifting distance. The test results are as follows: Fig. 9 As shown in the figure, when the sensor passes through the steel plate sample, a peak and a trough are generated. When the sensor is about to enter the sample, the absolute value of the induced voltage from the base value to the trough gradually increases. And it can be clearly seen that the thicker the stainless steel plate sample, the smaller the absolute value of the change amplitude. At the same time, it can be seen that the stainless steel plate samples of different thicknesses reach the peak at different times. The thinner the stainless steel plate sample, the earlier it reaches the peak. The thickness of the stainless steel plate sample can be measured and distinguished through these two signal characteristics.

[0074] Example 6

[0075] like Fig.10 As shown in the figure, the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention is used for different iron plate samples at a 1mm lift-off distance. The iron plate samples No. 6-9 are tested at a 50kHz excitation frequency and a 1mm lift-off distance. The induced voltage signal of the iron plate sample has only one trough when the sensor completely enters the sample area. When the sensor is about to enter the test piece, the absolute value of the induced voltage changes from the base value to the trough and gradually increases. The thicker the iron plate sample, the smaller the absolute value of the change amplitude. The thickness of the iron plate sample can be measured and distinguished by the amplitude of the induced voltage change.

[0076] Example 7

[0077] like Fig.11As shown in the figure, it is the detection result diagram of the electromagnetically coupled three-coil differential metal layer thickness measuring device of the present invention at different 1mm lifting distances of aluminum plate samples. The aluminum plate samples No. 10-15 are tested at an excitation frequency of 50kHz and a lifting distance of 1mm. The aluminum plate sample has only one peak when the sensor completely enters the sample area. When the sensor is about to enter the test piece, the absolute value of the induced voltage changes from the base value to the peak and gradually increases. The thicker the aluminum plate sample, the smaller the absolute value of the change amplitude. At the same time, when the sensor is about to approach the aluminum plate sample and the induced voltage value begins to change, the curvature of this part of the curve gradually decreases as the thickness of the aluminum plate sample increases. The thickness of the aluminum plate sample is measured and distinguished by these two signal characteristics.

[0078] In summary, the electromagnetically coupled three-coil differential metal layer thickness measuring device provided by the present invention has a special double-vortex coil structure, which can perform multi-feature differentiation on three metals, iron, aluminum, and stainless steel, and their thicknesses at the same frequency, and still has a good differentiation detection effect at the farthest lift-off distance of 9 mm. The present invention can perform thickness measurement and differentiation on ferromagnetic and non-ferromagnetic metals such as iron, stainless steel, and aluminum at a single AC excitation frequency. At the same time, it is also possible to use the original data at different lift-off distances to extract one or more thickness-related features of metals of different properties that are little affected by the lift-off distance. The sensor of the present invention has a simple structure, obvious signal characteristics, and high detection sensitivity, which is of great significance to the selection of thickness differentiation features and the application of metal thickness measurement technology in the field of metal thickness measurement.

[0079] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. An electromagnetically coupled three-coil differential metal layer thickness measuring device, characterized in that: include: A three-coil differential metal layer thickness sensor (1), a signal processor (2) and an AC signal generator (3), wherein: The three-coil differential metal layer thickness sensor (1) comprises a filter capacitor (4), an excitation coil (5) and a detection coil (6), wherein the filter capacitor (4) is connected in parallel to the detection coil (6), and the excitation coil (5) is tightly fitted below the detection coil (6); the detection coil (6) comprises two planar coils connected in series; The signal processor (2) comprises a phase-locked amplifier (7) and an operational amplifier (8), wherein the phase-locked amplifier (7) has two signal channels, and the two input signals have completely the same frequency and amplitude, and is used to remove noise similar to the excitation signal in the pickup signal, and extract a response signal related to the excitation signal; the operational amplifier (8) receives the DC signal output by the phase-locked amplifier (7), and is used to gain-amplify the DC signal; The AC signal generator (3) is used to generate two AC signals with the same frequency, amplitude and phase, one AC signal is connected to the excitation coil (5), and the other AC signal and the detection coil (6) are connected to the phase-locked amplifier (7). The phase-locked amplifier (7) compares, processes and amplifies the input signal, and then outputs a DC signal to the operational amplifier (8) for secondary amplification.

2. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 1, characterized in that: The excitation coil (5) is used to electromagnetically couple with the detection coil (6), obtain information from the three-coil differential metal layer thickness measurement sensor (1), and transmit energy to the three-coil differential metal layer thickness measurement sensor (1).

3. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 1, characterized in that: The two planar coils are connected in series and then connected in parallel with a filter capacitor (4) to achieve filtering and regulating functions in the circuit.

4. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 1, characterized in that: The excitation coil (5) is wound from an enameled copper wire with a wire diameter of 70 μm, and the coil has 79 turns in a single layer, an inner diameter of 1 mm, and an outer diameter of 15 mm.

5. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 3, characterized in that: The two planar coils are both wound with enameled copper wires with a wire diameter of 70 μm. The coils are both single-layer 35 turns, with an inner diameter of 1 mm and an outer diameter of 5 mm.

6. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 1, characterized in that: Both ends of the excitation coil (5) and the detection coil (6) are connected with lead wires, but there is no wire connection between the excitation coil (5) and the detection coil (6), and the lead wires are arranged on one side of the three-coil differential metal layer thickness sensor (1).

7. The electromagnetically coupled three-coil differential metal layer thickness measuring device according to claim 1, characterized in that: The electromagnetically coupled three-coil differential metal layer thickness measuring device further comprises a data acquisition card (9) and a LabVIEW data acquisition unit (10); the data acquisition card (9) is connected to the operational amplifier (8); the LabVIEW data acquisition unit (10) is connected to the data acquisition card (9); the data acquisition card (9) is used to collect signals after secondary amplification and input the collected signals into the LabVIEW data acquisition unit (10).

8. A method for manufacturing the electromagnetically coupled three-coil differential metal layer thickness measuring device according to any one of claims 1 to 7, characterized in that: include: S1, placing a large diameter coil in the lower layer as an excitation coil (5); Two small diameter coils are arranged on the upper layer of the large diameter coil to serve as detection coils (6), and no wire is connected between the excitation coil (5) and the detection coil (6); S2. Clean and inspect the excitation coil (5) to ensure that the excitation coil (5) meets the requirements, select an acrylic plate of suitable size to raise the excitation coil (5), fit the excitation coil (5) tightly to the acrylic plate, and fix it at the center of the slide to achieve the best measurement effect; S3, cleaning and inspecting the detection coil (6) to ensure that the detection coil (6) meets the requirements, fixing the filter capacitor (4) on the glass slide, placing the two detection coils (6) horizontally opposite to each other, making the detection coil (6) and the excitation coil (5) fit tightly, and connecting one end of the two detection coils (6) and the other end in parallel with the filter capacitor (4) and welding them firmly; S4. Use an AC signal generator (3) to generate two AC signals with exactly the same frequency, amplitude and phase; one signal is input into the excitation coil (5), and the other signal and the detection coil (6) are respectively connected to the two signal channels of the phase-locked amplifier (7); the phase-locked amplifier (7) processes and amplifies the two signals and outputs a stable DC signal to the operational amplifier (8), which is then sent to the data acquisition card (9) for data collection after secondary amplification.

Citation Information

Patent Citations

  • Electromagnetic sensor-based metal film thickness measuring device and method

    CN101876528A

  • Double-layer symmetrical differential plane eddy current detection sensor

    CN111398413A

  • Determination of axial position and rotational position of body

    CN114158272A

  • Pulsed eddy current probe for eliminating lift-off effect and detection method

    CN115825219A