Packaging processing method for ceramic substrate component and device

CN119028834AActive Publication Date: 2024-11-26JIANGXI WANNIANXIN MICROELECTRONICS CO LTD

Patent Information

Application Number
CN202411137686.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-26
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

In the prior art, the welding quality of ceramic substrates, metal frames and radiators is poor, resulting in uneven solder thickness, offset position, insufficient contamination, and reducing welding strength, conductivity and heat dissipation performance.

Method used

The welding sheet groove is opened on the copper layer on the front of the ceramic substrate, the small welding sheet and the large welding sheet are placed, and the reflow combined sheet vehicle is heated to fix the frame through the metal cover plate to ensure that the solder is stable in the welding sheet groove and form a uniform solder layer.

Benefits of technology

The welding strength and electrical characteristics between the pins in the frame and the ceramic substrate are improved, ensuring uniformity of solder thickness and device reliability, while improving heat dissipation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028834A_ABST
    Figure CN119028834A_ABST
Patent Text Reader

Abstract

The invention discloses a packaging processing method for a ceramic substrate component and a device, and the packaging processing method comprises the steps: forming a soldering lug groove in a front copper layer of a ceramic substrate, and sequentially placing a radiator, a large soldering lug and the ceramic substrate in a groove in the center of a backflow chip combination carrier, the small soldering lug is placed in the soldering lug groove, the inner pin of the frame is placed in the area above the soldering lug groove, then a metal cover plate is used for covering the soldering lug groove, the soldering lug groove is placed in a heating environment for formic acid treatment, hot air backflow and vacuumizing, and an obtained initial product with a formed solder welding layer is subjected to plastic package to form a plastic package body; and performing rib cutting forming on the pins of the outer frame of the plastic package body to obtain the device. According to the packaging processing method, the soldering lug groove is arranged to place the small soldering lug, and the boss is arranged to limit the position of the large soldering lug, so that the risk of soldering lug drifting is greatly reduced, enough solder is ensured to be infiltrated and wrapped between the back surface of the pin in the frame and the ceramic substrate after chip combination, and the heat dissipation performance and the reliability of the processed device are greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of electronic device packaging, and in particular to a packaging processing method and device for ceramic substrate components. Background Art

[0002] The ceramic substrate is composed of a front copper layer, a back copper layer and a ceramic layer. In order to firmly and evenly weld and fix the inner pins in the metal frame to the front copper layer and the heat sink to the back copper layer, it is necessary to set a small solder sheet between the front copper layer and the metal frame, and a large solder sheet between the back copper layer and the heat sink, and heat and reflow in a reflow furnace. However, in the prior art method, after the components are assembled, they are affected by vibration or impact during transportation, as well as vibration and airflow in the reflow furnace, which makes some small solder sheets easily shift in position before melting. The partially melted small solder sheets continue to flow due to the vibration and airflow in the reflow furnace, and the bubbles in the molten welding material are discharged during the reflow and vacuuming process, which causes the ceramic substrate to fluctuate up and down, and may cause problems such as uneven solder thickness, positional offset, insufficient wetting, and unstable tin creep height on each side of the inner pin between the back of the inner pin in the frame and the front copper layer of the ceramic substrate (such as Figure 1 and Figure 2 As shown, it can be clearly seen that the solder is not fully wetted after the welding process, including the frame, solder, front copper layer, back copper layer, ceramic layer, and ceramic substrate); the emergence of the above problems reduces the bonding strength, conductivity, and reliability between the pins in the frame and the front copper layer of the ceramic substrate; similarly, the thickness of the solder between the ceramic substrate and the heat sink is difficult to accurately control during the heating and reflow process after the assembly, which affects the heat dissipation performance and reliability of the device. Therefore, the existing technical method has the problem of poor welding quality when welding the ceramic substrate to the metal frame and the heat sink. Summary of the invention

[0003] The embodiment of the present invention provides a packaging processing method and device for ceramic substrate components, aiming to solve the problem of poor welding quality when welding the ceramic substrate to a metal frame and a heat sink in the prior art method.

[0004] In a first aspect, an embodiment of the present application provides a packaging method for ceramic substrate components, wherein the packaging method comprises:

[0005] A soldering slot is provided in the pin welding area of ​​the frame corresponding to the copper layer on the front side of the ceramic substrate; the soldering slot includes a conjoined soldering slot and / or an independent single soldering slot; an island is provided in the center of some of the conjoined soldering slots, and an island is provided in the center of some of the single soldering slots;

[0006] Place the heat sink in the groove in the center of the reflow wafer carrier, and then place a large solder pad with solder pad through holes on the top surface of the heat sink;

[0007] After printing the adhesive material on the surface of the ceramic substrate, mounting the chip, and welding the metal wire, the ceramic substrate is placed on the top surface of the large soldering piece, and a boss corresponding to the through hole of the soldering piece is provided on the back of the ceramic substrate; the thickness of the large soldering piece is greater than the height of the boss;

[0008] Assembling a small soldering piece matching the shape of the soldering piece slot in the soldering piece slot, some of the small soldering pieces are provided with an island through hole matching the island; the thickness of the small soldering piece is greater than the depth of the soldering piece slot;

[0009] Assemble the frame in the groove in the center of the reflow wafer carrier, with the inner pins of the frame placed in the area above the soldering slot or in contact with the surface of the island on the ceramic substrate;

[0010] The metal cover plate is covered on the top of the frame and the metal cover plate is fixedly connected to the flange of the reflow wafer carrier to obtain a wafer assembly structure; the outer edge of the frame is clamped and fixed between the metal cover plate and the flange of the reflow wafer carrier;

[0011] Placing the laminated structure in a formic acid vacuum reflow furnace, subjecting the laminated structure to formic acid treatment, hot air reflow and vacuuming in a heating environment, thereby forming a soldering layer between the inner pins of the frame and the front copper layer of the ceramic substrate and between the front side of the heat sink and the back copper layer of the ceramic substrate; the temperature of the heating environment is higher than the melting points of the large solder piece and the small solder piece;

[0012] The initial product with the solder welding layer is plastic-sealed to form a plastic-sealed body, and the pins of the outer frame of the plastic-sealed body are cut and formed to obtain the final device.

[0013] In a second aspect, an embodiment of the present application further provides a device, wherein the device is processed by the packaging processing method described in the first aspect, and the device includes a ceramic substrate, a heat sink, a frame and a plastic package;

[0014] The ceramic substrate comprises a front copper layer, a back copper layer, and a ceramic layer sandwiched between the front copper layer and the back copper layer;

[0015] A soldering slot is provided on the front copper layer, and the inner pin of the frame penetrates into the top of the soldering slot and is tightly welded to the soldering slot through the solder welding layer; the soldering slot includes a conjoined soldering slot and / or an independent single soldering slot; adjacent soldering slots in the conjoined soldering slot are provided with connected elongated grooves, and an island is provided in the center of some of the conjoined soldering slots, and an island is provided in the center of some of the single soldering slots, and the top surface of the island is in contact with the inner pin of the frame;

[0016] The back copper layer is provided with a boss, and the gap between the boss and the top surface of the heat sink is filled with a solder welding layer for tightly welding the heat sink and the back copper layer;

[0017] The chip is bonded to the upper end surface of the front copper layer by an adhesive material, and the chip and the front copper layer are electrically connected by a metal wire;

[0018] The plastic package is wrapped around the outside of a combination of the ceramic substrate, the heat sink, the chip and the metal wire, and the outer edge of the frame extends outward from the plastic package.

[0019] The embodiment of the present invention provides a packaging and processing method and device for ceramic substrate components. The packaging and processing method includes opening a solder piece groove on the front copper layer of the ceramic substrate, placing a heat sink, a large solder piece and a ceramic substrate in the groove in the center of a reflow wafer carrier in sequence, placing a small solder piece in the solder piece groove, placing the inner pins of the frame in the area above the solder piece groove and then covering it with a metal cover, placing it in a heating environment for formic acid treatment, hot air reflow and vacuuming, plastic-sealing the initial product forming the solder welding layer to form a plastic package body, and cutting the ribs of the frame pins outside the plastic package to obtain a device. The above-mentioned packaging processing method greatly reduces the risk of solder piece drift by setting a solder piece groove to place a small solder piece and setting a boss to limit the position of a large solder piece. When the solder piece is melted to form liquid solder, it is stably controlled in the integrated solder piece groove or the single solder piece groove until it solidifies, ensuring that there is sufficient solder infiltration and wrapping between the back of the pins in the frame and the ceramic substrate after the assembly, and the solder thickness is accurately controlled and more uniform; because the liquid solder is gathered in the integrated solder piece groove or the single solder piece groove, its surface tension causes the liquid solder to climb to the four sides of the pins in the frame, thereby greatly improving the welding strength and solder volume between the pins in the frame and the ceramic substrate, and also ensuring the electrical characteristics and device reliability between the pins in the frame and the front of the ceramic substrate; at the same time, a controllable solder thickness is also formed between the back of the ceramic substrate and the front of the radiator through the boss, which greatly improves the heat dissipation performance and reliability of the processed device. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying any creative work.

[0021] Figure 1 This is a front structural diagram of a device obtained by processing using a prior art method;

[0022] Figure 2 This is a side structural diagram of a device obtained by processing using a prior art method;

[0023] Figure 3 A method flow chart of a packaging and processing method for ceramic substrate components provided by an embodiment of the present invention;

[0024] Figure 4 A front structural diagram of a ceramic substrate provided by an embodiment of the present invention;

[0025] Figure 5 A side structural diagram of a ceramic substrate provided in an embodiment of the present invention;

[0026] Figure 6 A front structural diagram of another ceramic substrate provided by an embodiment of the present invention;

[0027] Figure 7 A side structural diagram of another ceramic substrate provided by an embodiment of the present invention;

[0028] Figure 8 A partial structural diagram of a device provided in an embodiment of the present invention;

[0029] Fig. 9 A front structural diagram of another ceramic substrate provided by an embodiment of the present invention;

[0030] Fig.10 A side structural diagram of another ceramic substrate provided by an embodiment of the present invention;

[0031] Fig.11 A front structural diagram of another ceramic substrate provided by an embodiment of the present invention;

[0032] Fig.12 A side structural diagram of another ceramic substrate provided in an embodiment of the present invention;

[0033] Fig.13 A front structural diagram of a device provided by an embodiment of the present invention;

[0034] Fig.14 A back structural diagram of a ceramic substrate provided in an embodiment of the present invention;

[0035] Fig.15 A cross-sectional structural diagram of a ceramic substrate provided in an embodiment of the present invention;

[0036] Fig.16 Another partial structural diagram of a device provided by an embodiment of the present invention;

[0037] Fig.17 A structural diagram of a heat sink provided by an embodiment of the present invention;

[0038] Fig.18 A structural diagram of a large welding piece provided in an embodiment of the present invention;

[0039] Fig.19 A structural diagram of a small soldering piece provided in an embodiment of the present invention;

[0040] Fig. 20 A structural diagram of a framework provided for an embodiment of the present invention;

[0041] Fig.21 A schematic diagram of a processing process of a device provided by an embodiment of the present invention;

[0042] Fig. 22 A schematic diagram of another processing process of a device provided by an embodiment of the present invention;

[0043] Fig.23 A schematic diagram of another processing process of a device provided by an embodiment of the present invention;

[0044] Fig.24 A partial structural diagram of a device provided in an embodiment of the present invention.

[0045] Figure numerals: 1. Ceramic substrate; 2. Radiator; 3. Frame; 4. Plastic package; 12. Front copper layer; 13. Back copper layer; 11. Ceramic layer; 5. Solder; 121. Solder pad slot; 122. Island; 61. Reflow assembly carrier; 7. Large solder pad; 8. Chip; 81. Metal wire; 71. Solder pad through hole; 131. Boss; 14. Small solder pad; 141. Island through hole; 31. Inner pin; 62. Metal cover. DETAILED DESCRIPTION

[0046] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0047] It should be understood that when used in this specification and the appended claims, the terms "include" and "comprises" indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or combinations thereof.

[0048] It should also be understood that the terms used in the present specification are only for the purpose of describing specific embodiments and are not intended to limit the present invention. As used in the present specification and the appended claims, the singular forms "a", "an" and "the" are intended to include the plural forms unless the context clearly indicates otherwise. It should also be further understood that the term "and / or" used in the present specification and the appended claims refers to any combination of one or more of the associated listed items and all possible combinations, and includes these combinations.

[0049] See also Figure 3 As shown in the figure, an embodiment of the present application discloses a packaging and processing method for ceramic substrate components, wherein the packaging and processing method includes steps S110 to S180.

[0050] S110, a soldering slot is formed in a pin soldering area in the frame corresponding to the copper layer on the front side of the ceramic substrate.

[0051] A soldering slot 121 is provided in the soldering area of ​​the pin 31 in the frame 3 corresponding to the copper layer 12 on the front side of the ceramic substrate 1. The soldering slot 121 includes a conjoined soldering slot and / or an independent single soldering slot; an island 122 is provided in the center of some of the conjoined soldering slots, and an island 122 is provided in the center of some of the single soldering slots.

[0052] The ceramic substrate 1 is obtained by laminating a front copper layer 12, a ceramic layer 11 and a back copper layer 13. The front copper layer 12 needs to be welded to the inner lead of the frame 3. Therefore, a soldering slot 121 can be opened in the welding area corresponding to the front copper layer 12 and the inner lead 31 of the frame 3. The soldering slot 121 opened on the front copper layer 12 is as follows: Figures 4 to 7 As shown. Among them, Figure 4 and Figure 5 The diagram shows a connected soldering slot formed by three soldering slots 121 arranged in sequence, wherein adjacent soldering slots 121 in the connected soldering slot are provided with interconnected elongated grooves (the elongated grooves are used to balance the amount of molten solder in each groove in the connected soldering slot). Figure 6 and Figure 7 A single soldering slot formed by a soldering slot 121 is shown, and two single soldering slots are arranged side by side.

[0053] Furthermore, an island 122 may be provided in the center of a portion of the conjoined welding slots. The specific configuration structure is as follows: Fig. 9 and Fig.10 As shown in FIG. 1 , the island 122 is a protrusion formed by the upward bulge of the concave cavity in the center of the soldering slot 121 in the conjoined soldering slot. In the specific embodiment of the present application, an island 122 is provided in each of the two soldering slots 121 at both ends of the conjoined soldering slot. The island 122 can also be provided in the center of some single soldering slots. The specific configuration structure is as follows: Fig.11 and Fig.12 As shown, the island 122 is a protrusion formed by the upward protrusion of the concave cavity in the center of the single soldering slot. Specifically, the island 122 can be set to be circular, elliptical or polygonal.

[0054] S120, placing the heat sink in the groove in the center of the reflow wafer carrier, and then placing a large solder sheet with solder sheet through holes on the top surface of the heat sink.

[0055] Place the heat sink 2 in the groove in the center of the reflow wafer carrier 61, and then place the large solder piece 7 with the solder piece through hole 71 on the top surface of the heat sink 2. Place the heat sink 2 in the groove in the center of the reflow wafer carrier 61, then the heat sink 2 is placed at the bottom layer of the groove in the reflow wafer carrier 61, and the large solder piece 7 with the solder piece through hole 71 is placed on the top surface of the heat sink 2.

[0056] S130, after printing the adhesive material on the surface of the ceramic substrate, mounting the chip, and welding the metal wire, the ceramic substrate is placed on the top surface of the large welding sheet.

[0057] After printing the adhesive material on the surface of the ceramic substrate 1, mounting the chip 8, and welding the metal wire 81, the ceramic substrate 1 is placed on the top surface of the large soldering piece 7. The back of the ceramic substrate 1 is provided with a boss 131 corresponding to the soldering piece through hole 71; the thickness of the large soldering piece 7 is greater than the height of the boss 131.

[0058] After step 110, the surface of the ceramic substrate obtained by processing is printed with adhesive material, and the adhesive material is laid in the central area of ​​the front copper layer, and the chip is attached to the adhesive material, so as to achieve a stable mounting of the chip; then the metal wires are welded between the chips and between the chip and the front copper layer. After the chip mounting and metal wire welding are completed, the ceramic substrate can be placed on the top surface of the large soldering piece. In order to limit the large soldering piece through the ceramic substrate, a boss can be set on the back copper layer of the ceramic substrate, the boss is matched with the soldering piece through hole on the large soldering piece, and the thickness of the large soldering piece is set to be greater than the height of the boss.

[0059] The outer dimensions of the large soldering piece 7 are larger than the outer dimensions of the back copper layer 13 of the ceramic substrate 1; the large soldering piece 7 is a rectangular soldering piece, and soldering piece through holes 71 are provided at the four vertex corners of the large soldering piece 7. Furthermore, the horizontal spacing between the inner wall of the soldering piece through hole 71 and the side wall of the boss 131 is 0.10 to 0.20 mm; the horizontal spacing between the outer wall of the large soldering piece 7 and the outer wall of the ceramic substrate 1 is 0.05 to 0.10 mm. The thickness of the large soldering piece 7 is 0.05 to 0.10 mm greater than the height of the boss 131.

[0060] The outer dimensions of the large soldering piece 7 are larger than the outer dimensions of the back copper layer 13 of the ceramic substrate 1. Specifically, the horizontal spacing between the outer wall of the large soldering piece 7 and the outer wall of the ceramic substrate 1 can be set to 0.05-0.10 mm, that is, the periphery of the ceramic substrate 1 is 0.05-0.10 mm wider than the periphery of the large soldering piece 7.

[0061] Furthermore, the large soldering piece 7 can be set as a rectangular soldering piece, and soldering piece through holes 71 are set at the four corners of the large soldering piece 7, and the four corners of the back copper layer 13 of the corresponding ceramic substrate 1 are also provided with bosses 131. The specific structure of the back copper layer 13 of the ceramic substrate 1 is as follows: Fig.14 and Fig.15 The specific structure of the large welding piece 7 is as shown in FIG. Fig.18 As shown, the specific structure of the radiator 2 is as follows Fig.17 shown.

[0062] Furthermore, the horizontal spacing between the inner wall of the soldering plate through hole and the side wall of the boss can be set to 0.10-0.20 mm, and the outer dimensions of the soldering plate through hole are larger than the outer dimensions of the boss.

[0063] Furthermore, in order to improve the welding quality of the solder welding layer, the thickness of the large welding piece can be set to be 0.05 to 0.10 mm greater than the height of the boss.

[0064] S140, assembling small soldering pieces that match the shape of the soldering piece slot into the soldering piece slot, and some of the small soldering pieces are provided with island through holes that match the island.

[0065] A small soldering piece 14 matching the shape of the soldering piece slot 121 is assembled in the soldering piece slot 121, and some of the small soldering pieces 14 are provided with through holes of the isolated island 122 matching the isolated island 122. The thickness of the small soldering piece 14 is greater than the depth of the soldering piece slot 121.

[0066] Further, a small soldering piece 14 matching the shape of the soldering piece slot 121 is assembled in the soldering piece slot 121, wherein the specific structure of the small soldering piece 14 is as follows: Fig.19As shown, a one-piece small welding piece is placed in the one-piece welding piece groove, and a one-piece small welding piece is placed in the one-piece welding piece groove. Among them, the small welding piece 14 is a small welding piece 14 with a through hole of an isolated island 122 or a small welding piece 14 without a through hole of an isolated island 122. The small welding piece 14 with a through hole of an isolated island 122 is adapted to the welding piece groove 121 with the isolated island 122, and the small welding piece 14 without a through hole of an isolated island 122 is adapted to the welding piece groove 121 without the isolated island 122. The depths of the welding piece grooves 121 are all equal, and the thickness of the small welding piece 14 is greater than the depth of the welding piece grooves 121; specifically, the thickness of the small welding piece 14 is 0.02 to 0.05 mm greater than the depth of the welding piece grooves 121. The combined structure formed by placing the small welding piece 14 in the welding piece groove 121 and combining it with the frame 3 is as shown in FIG. Figure 8 and Fig.16 shown.

[0067] Specifically, the outer dimensions of the small solder tab 14 are smaller than the outer dimensions of the solder tab slot 121, and the horizontal spacing between the outer side wall of the small solder tab 14 and the inner side wall of the solder tab slot 121 can be set to 0.2 mm, that is, the outer periphery of the solder tab slot 121 is 0.2 mm wider than the small solder tab 14. The size of the small solder tab 14 can be set based on the edges of each solder tab slot 121, for example, the width of the solder tab slot 121 is X and the length is Y, the width of the small solder tab 14 is X1 and the length is Y1, then X=X1+0.2×2mm, Y=Y1+0.2×2mm.

[0068] S150, assembling the frame into the groove in the center of the reflow wafer carrier.

[0069] The frame 3 is assembled in the groove in the center of the reflow wafer carrier 61. The inner pin 31 of the frame 3 is placed in the area above the solder slot 121 or in contact with the surface of the island 122 on the ceramic substrate 1. The inner pin 31 of the frame 3 can be properly recessed and processed. The recessed inner pin 31 can be used to make the back of the inner pin 31 of the frame 3 directly contact the front copper layer 12 of the ceramic substrate 1, and can make the inner pin 31 of the frame 3 contact the surface of the island 122 on the ceramic substrate 1. The structure of the frame 3 is as follows: Fig. 20 shown.

[0070] S160, covering the frame with a metal cover plate and fixing the metal cover plate to a flange of the reflow wafer assembly carrier to obtain a wafer assembly structure.

[0071] The metal cover plate 62 is covered on the top of the frame 3 and the metal cover plate 62 is fixedly connected to the flange of the reflow wafer carrier 61 to obtain a wafer structure. The outer edge of the frame 3 is clamped and fixed between the metal cover plate 62 and the flange of the reflow wafer carrier 61. The device structure to be packaged is assembled together by the reflow wafer carrier 61 and the metal cover plate 62 to obtain a wafer structure. The specific structure of the wafer structure is as follows: Fig.21 shown.

[0072] S170, placing the assembled structure in a formic acid vacuum reflow furnace, performing formic acid treatment, hot air reflow and vacuuming on the assembled structure in a heating environment, so as to form a solder welding layer between the inner pins of the frame and the front copper layer of the ceramic substrate and between the front side of the heat sink and the back copper layer of the ceramic substrate.

[0073] The laminated structure is placed in a formic acid vacuum reflow furnace, and the laminated structure is subjected to formic acid treatment, hot air reflow and vacuuming in a heating environment, so that a soldering layer is formed between the inner pins 31 of the frame 3 and the front copper layer 12 of the ceramic substrate 1, and between the front of the heat sink 2 and the back copper layer 13 of the ceramic substrate 1. The temperature of the heating environment is higher than the melting point of the large solder piece 7 and the small solder piece 14.

[0074] Furthermore, the combined structure obtained by combining the sheets is placed in a formic acid vacuum reflow furnace, and the combined structure is subjected to formic acid treatment, hot air reflow and vacuuming in a heated environment. At high temperature, the small solder sheet 14 melts into liquid solder 5, and the liquid solder 5 gathers in the conjoined solder sheet slot and / or the single solder sheet slot. A connected elongated groove is provided between adjacent solder sheet slots 121 in the conjoined solder sheet slot to balance the amount of molten solder in each slot in the conjoined solder sheet slot. The back of the pin 31 in the frame 3 is soaked and wrapped by the solder 5; under the action of the surface tension of the liquid solder 5, the liquid solder 5 continuously climbs and bites the four sides of the inner pin 31 of the frame 3. At the same time, the large solder piece 7 is also melted into liquid solder 5 at high temperature. Under the gravity of the metal cover plate 62 and the frame 3, not only the back of the inner pin 31 of the frame 3 is pressed against the surface of the island 122 in the integrated solder piece slot and / or the single solder piece slot, but also the gravity of the metal cover plate 62 and the frame 3 is transmitted through the inner pin 31 of the frame 3 and the ceramic substrate 1 and pressed against the front of the heat sink 2, so that during the reflow and vacuum process, the inner pin 31 of the frame 3 is always pressed against the ceramic substrate 1, and the ceramic substrate 1 is also always in close contact with the front of the heat sink 2, forming a uniform solder between the inner pin 31 of the frame 3 and the ceramic substrate 1 after being taken out of the furnace. The thickness, solder wetting rate, and the tin crawling and biting around the sides of the inner pin 31 of the frame 3 form a solid solder welding layer, ensuring that there is sufficient solder infiltration and wrapping between the back of the inner pin 31 of the frame 3 and the front copper layer 12 of the ceramic substrate 1 after assembly, and the solder thickness is also stably controlled (i.e. the depth of the soldering slot 121), thereby effectively improving the welding strength, electrical connection and reliability between the inner pin 31 of the frame 3 and the front copper layer 12 of the ceramic substrate 1; at the same time, a controllable solder thickness is also formed between the back copper layer 13 of the ceramic substrate 1 and the front of the heat sink 2 through a boss 131. The combined structure formed after the above process is as follows Fig. 22 As shown, the initial product is taken out from the reflow wafer carrier 61, and the structure of the initial product is as shown in FIG. Fig.23 shown.

[0075] S180, plastic-encapsulating the initial product with the solder welding layer to form a plastic-encapsulated body, and cutting the outer frame pins of the plastic-encapsulated body to obtain a final device.

[0076] The initial product with the solder welding layer is plastic-encapsulated to form a plastic-encapsulated body 4, and the pins of the outer frame 3 of the plastic-encapsulated body 4 are cut and shaped to obtain the final device. The initial product with the solder welding layer is plastic-encapsulated to form a plastic-encapsulated body 4, and the plastic-encapsulated body 4 is wrapped around the outer side of the assembly formed by the ceramic substrate 1, the heat sink 2, the chip 8 and the metal wire 81, and the outer edge of the frame 3 extends outward from the plastic-encapsulated body 4. The local structure of the final finished device obtained after the pins of the outer frame 3 of the plastic-encapsulated body 4 are cut and shaped is as follows: Fig.24 shown.

[0077] The embodiment of the present invention further provides a device, which is obtained by using the packaging processing method described in the above embodiment. Fig.23 and Fig.24 As shown, the device includes a ceramic substrate 1, a chip 8, a wire, a heat sink 2, a frame 3 and a plastic package 4; the ceramic substrate 1 includes a front copper layer 12, a back copper layer 13, and a ceramic layer 11 sandwiched between the front copper layer 12 and the back copper layer 13; a soldering plate groove 121 is opened on the front copper layer 12, and the inner pin 31 of the frame 3 penetrates into the top of the soldering plate groove 121 and is tightly welded to the soldering plate groove 121 through a solder welding layer, and the solder welding layer is also the solder 5 shown in the figure; the soldering plate groove 121 includes a conjoined soldering plate groove and / or an independent single soldering plate groove; an island 122 is set in the center of some of the conjoined soldering plate grooves, and an island 122 is set in the center of some of the single soldering plate grooves. An island 122, the top surface of the island 122 is in contact with the inner pin 31 of the frame 3; a boss 131 is provided on the back copper layer 13, and a solder welding layer for tightly welding the radiator 2 and the back copper layer 13 is filled in the gap between the boss 131 and the top surface of the radiator 2; the chip 8 is bonded to the upper end surface of the front copper layer 12 by an adhesive material, and the chip 8 is electrically connected to the front copper layer 12 by a metal wire 81; the plastic package 4 is wrapped and arranged on the outside of the combination formed by the ceramic substrate 1, the radiator 2, the chip 8, and the metal wire 81, and the outer edge of the frame 3 extends outward from the plastic package 4.

[0078] In a more specific embodiment, the soldering slots 121 are arranged on both sides of the front copper layer 12 of the ceramic substrate 1 to form two parallel rows of soldering slots; and the number of the soldering slots 121 with isolated islands 122 is not less than three; at least one isolated island 122 is arranged in each row of soldering slots; the two connected soldering slots with isolated islands 122 in a row of soldering slots are respectively arranged at both ends of the row of soldering slots; and the two isolated islands 122 in the connected soldering slots are respectively arranged in the soldering slots 121 at both ends of the connected soldering slots; the two single soldering slots with isolated islands 122 in a row of soldering slots are respectively arranged at both ends of the row of soldering slots. The specific structure is as follows Fig.13 shown.

[0079] Specifically, the number of the soldering slots 121 of the island 122 is not less than three, that is, the number of the islands 122 is not less than three. And at least one island 122 is set in each row of soldering slots. The two conjoined soldering slots of the island 122 in the same row of soldering slots are respectively set at the two ends of the row of soldering slots, for example Fig.13The row of soldering slots on the right side of the middle includes two connected soldering slots with isolated islands 122, and the two connected soldering slots with isolated islands 122 are respectively located at the two ends of the row of soldering slots. If two isolated islands 122 are provided in the connected soldering slot, the two isolated islands 122 are respectively provided in the soldering slots 121 at the two ends of the connected soldering slot. Fig.13 An island 122 is provided in each of the soldering slots 121 at both ends of a connected soldering slot in a row of soldering slots on the left side.

[0080] Two single soldering slots of the island 122 are respectively arranged at the two ends of the soldering slot row. Fig.13 As shown, the row of soldering slots on the left side includes two single soldering slots with isolated islands 122, and the two single soldering slots with isolated islands 122 are respectively located at two ends of the row of soldering slots.

[0081] The packaging processing method and device for ceramic substrate components provided in the embodiments of the present invention include opening a soldering plate groove on the front copper layer of the ceramic substrate, placing a heat sink, a large soldering plate and a ceramic substrate in the groove in the center of a reflow wafer carrier in sequence, placing a small soldering plate in the soldering plate groove, placing the inner pins of the frame in the area above the soldering plate groove, and then covering it with a metal cover plate, placing it in a heating environment for formic acid treatment, hot air reflow and vacuuming, plastic-sealing the initial product forming the solder welding layer to form a plastic-sealed body, and cutting the ribs of the frame pins outside the plastic-sealed body to obtain a device. The above-mentioned packaging processing method greatly reduces the risk of solder piece drift by setting a solder piece groove to place a small solder piece and setting a boss to limit the position of a large solder piece. When the solder piece is melted to form liquid solder, it is stably controlled in the integrated solder piece groove or the single solder piece groove until it solidifies, ensuring that there is sufficient solder infiltration and wrapping between the back of the pins in the frame and the ceramic substrate after the assembly, and the solder thickness is accurately controlled and more uniform; because the liquid solder is gathered in the integrated solder piece groove or the single solder piece groove, its surface tension causes the liquid solder to climb to the four sides of the pins in the frame, thereby greatly improving the welding strength and solder volume between the pins in the frame and the ceramic substrate, and also ensuring the electrical characteristics and device reliability between the pins in the frame and the front of the ceramic substrate; at the same time, a controllable solder thickness is also formed between the back of the ceramic substrate and the front of the radiator through the boss, which greatly improves the heat dissipation performance and reliability of the processed device.

[0082] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed by the present invention, and these modifications or replacements should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.

Claims

1. A packaging method for ceramic substrate components, characterized in that: The packaging processing method comprises: A soldering slot is provided in the pin welding area of ​​the frame corresponding to the copper layer on the front side of the ceramic substrate; the soldering slot includes a conjoined soldering slot and / or an independent single soldering slot; an island is provided in the center of some of the conjoined soldering slots, and an island is provided in the center of some of the single soldering slots; Place the heat sink in the groove in the center of the reflow wafer carrier, and then place a large solder pad with solder pad through holes on the top surface of the heat sink; After printing the adhesive material on the surface of the ceramic substrate, mounting the chip, and welding the metal wire, the ceramic substrate is placed on the top surface of the large soldering piece, and a boss corresponding to the through hole of the soldering piece is provided on the back of the ceramic substrate; the thickness of the large soldering piece is greater than the height of the boss; Assembling a small soldering piece matching the shape of the soldering piece slot in the soldering piece slot, some of the small soldering pieces are provided with an island through hole matching the island; the thickness of the small soldering piece is greater than the depth of the soldering piece slot; Assemble the frame in the groove in the center of the reflow wafer carrier, with the inner pins of the frame placed in the area above the soldering slot or in contact with the surface of the island on the ceramic substrate; The metal cover plate is covered on the top of the frame and the metal cover plate is fixedly connected to the flange of the reflow wafer carrier to obtain a wafer assembly structure; the outer edge of the frame is clamped and fixed between the metal cover plate and the flange of the reflow wafer carrier; Placing the laminated structure in a formic acid vacuum reflow furnace, subjecting the laminated structure to formic acid treatment, hot air reflow and vacuuming in a heating environment, thereby forming a soldering layer between the inner pins of the frame and the front copper layer of the ceramic substrate and between the front side of the heat sink and the back copper layer of the ceramic substrate; the temperature of the heating environment is higher than the melting points of the large solder piece and the small solder piece; The initial product with the solder welding layer is plastic-sealed to form a plastic-sealed body, and the pins of the outer frame of the plastic-sealed body are cut and formed to obtain the final device.

2. The packaging method for ceramic substrate components according to claim 1, characterized in that: The outer dimensions of the small welding piece are smaller than the outer dimensions of the welding piece groove.

3. The packaging method for ceramic substrate components according to claim 2, characterized in that: The thickness of the small welding piece is 0.02-0.05 mm greater than the depth of the welding piece groove.

4. The packaging method for ceramic substrate components according to any one of claims 1 to 3, characterized in that: The outer dimensions of the large soldering piece are larger than the outer dimensions of the back copper layer of the ceramic substrate.

5. The packaging method for ceramic substrate components according to claim 4, characterized in that: The large welding piece is a rectangular welding piece, and welding piece through holes are arranged at the four top corners of the large welding piece.

6. The packaging method for ceramic substrate components according to claim 5, characterized in that: The horizontal distance between the inner wall of the soldering plate through hole and the side wall of the boss is 0.10-0.20 mm.

7. The packaging method for ceramic substrate components according to claim 4, characterized in that: The horizontal distance between the outer side wall of the large welding piece and the outer side wall of the ceramic substrate is 0.05-0.10 mm.

8. The packaging method for ceramic substrate components according to claim 4, characterized in that: The thickness of the large welding piece is 0.05 to 0.10 mm greater than the height of the boss.

9. A device, characterized in that The device is obtained by using the packaging method according to any one of claims 1 to 8, and the device comprises a ceramic substrate, a heat sink, a frame and a plastic package; The ceramic substrate comprises a front copper layer, a back copper layer, and a ceramic layer sandwiched between the front copper layer and the back copper layer; A soldering slot is provided on the front copper layer, and the inner pin of the frame penetrates into the top of the soldering slot and is tightly welded to the soldering slot through the solder welding layer; the soldering slot includes a conjoined soldering slot and / or an independent single soldering slot; adjacent soldering slots in the conjoined soldering slot are provided with connected elongated grooves, and an island is provided in the center of some of the conjoined soldering slots, and an island is provided in the center of some of the single soldering slots, and the top surface of the island is in contact with the inner pin of the frame; The back copper layer is provided with a boss, and the gap between the boss and the top surface of the heat sink is filled with a solder welding layer for tightly welding the heat sink and the back copper layer; The chip is bonded to the upper end surface of the front copper layer by an adhesive material, and the chip and the front copper layer are electrically connected by a metal wire; The plastic package is wrapped around the outside of a combination of the ceramic substrate, the heat sink, the chip and the metal wire, and the outer edge of the frame extends outward from the plastic package.

10. The device according to claim 9, characterized in that The soldering slots are arranged on both sides of the front copper layer of the ceramic substrate to form two parallel rows of soldering slots; and the number of the soldering slots arranged in the isolated island is not less than three; At least one island is provided in each row of welding lug slots; The two connected soldering slots with isolated islands in a row of soldering slots are respectively arranged at the two ends of the row of soldering slots; and the two isolated islands in the connected soldering slots are respectively arranged in the soldering slots at the two ends of the connected soldering slots; The two single soldering slots of the isolated islands in a row of soldering slots are respectively arranged at the two ends of the row of soldering slots.

Citation Information

Patent Citations

  • A perimeter millimeter-level eutectic element welding device and welding method

    CN109256337A

  • Ceramic substrate structure, intelligent power module and preparation method thereof

    CN113380719A

  • Welding groove forming process of substrate and substrate thereof

    CN114446795A

  • TO series packaging structure with high reliability

    CN211428159U

  • Power module and heat dissipation base plate thereof

    CN214254416U

Cited By

  • Stacked stepping welding method for plastic package power device

    CN120502804A