UV / IR heterojunction dual-phase detector based on polarity enhancement and preparation method of UV / IR heterojunction dual-phase detector

By introducing Janus two-dimensional material with intrinsic polarity, the plane mirror symmetry is broken and the intrinsic electric field is introduced in the layer, and the problem of insufficient separation of electrons and holes in β-Ga2O3/BP biphase photodetectors is solved. The light response and detection band performance of the detector are significantly improved.

CN119029079APending Publication Date: 2024-11-26XIDIAN UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411128529.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-16
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing β-Ga2O3/BP biphase photodetectors have a small built-in electric field at the interface, resulting in insufficient separation of electrons and holes, which leads to lower light responsiveness and narrower detection bands, especially in infrared. The light response is low under band light.

Method used

Use Janus two-dimensional materials with intrinsic polarity (such as Janus-AsP) to replace the traditional two-dimensional material BP, break the plane mirror symmetry through surface selenization, and introduce the intrinsic electric field in the layer, which is β-Ga2O3/AsP differentiation. The junction interface introduces additional carrier driving effect to achieve effective separation of electrons and holes.

Benefits of technology

The secondary separation rate of electron holes is improved, the carrier life is extended, the dark current is reduced, the optical response and detection band of the detector are improved, and the performance of the detector is significantly improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119029079A_ABST
    Figure CN119029079A_ABST
Patent Text Reader

Abstract

The invention discloses a UV / IR heterojunction dual-phase detector based on polarity enhancement and a preparation method thereof. The UV / IR heterojunction dual-phase detector comprises a substrate, a wide bandgap semiconductor layer, a narrow bandgap two-dimensional material layer and a metal electrode which are arranged in sequence, the narrow-band-gap two-dimensional material layer is made of a material with intrinsic polarity, and intrinsic electric field polarity driving is introduced to a heterojunction interface. The narrow band gap two-dimensional material layer can be made of a Janus two-dimensional material with intrinsic polarity, and the wide band gap semiconductor layer is made of beta-Ga2O3 or wide band gap hexagonal AlN. And the Janus two-dimensional material with the intrinsic polarity can be Janus-AsP, Bi < 2 > TeO < 5 >, MoTe2 or In < 2 > Se < 3 >. The intrinsic polarity in the layer is introduced, so that the electron performance of the UV / IR dual-phase detector is further improved, sensitive detection of deep ultraviolet and near-infrared band optical signals is realized, and the detector can be applied to the fields of ray measurement and detection, industrial automatic control, photometric measurement and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of semiconductor technology, relates to a photoelectric device, and in particular to a UV / IR heterojunction dual-phase detector based on polarity enhancement and a preparation method thereof. Background Art

[0002] Photoelectric detectors have the function of converting light signals into electrical signals, while ultraviolet / infrared (UV / IR) dual-phase detectors are electronic devices that have both ultraviolet and infrared detection capabilities. This type of detector combines the advantages of UV and IR sensors and can provide more comprehensive information and higher detection accuracy.

[0003] In the prior art, Tao He et al. published a sapphire substrate-based β-Ga2O3 / BP UV / IR dual-phase photodetector in their paper “Metalorganic Chemical VaporDeposition Heteroepitaxialβ-Ga2O3 and Black Phosphorus Pn Heterojunction forSolar-Blind Ultraviolet and Infrared Dual-Band Photodetector” (physica statussolidi(a),vol.217,pp.2020). Compared with the traditional AlGaN / GaN UV / IR dual-phase photodetector, this detector is more resistant to visible light interference, and the detection wavelength range is 238nm in the ultraviolet band, with a detection rate of 88.5mAW. -1 The detection rate at 1030nm wavelength in the infrared band reaches 1.24mAW -1 .

[0004] TiWei Chen et al. published a paper titled "Ultrahigh Responsivity β-Ga2O3 / BP Junction Field Effect Phototransistors for UV / IR Dual-Band Detection" (IEEE Sensors Journal, vol. 23, pp. 15504-15511, 2023) that discloses a β-Ga2O3 / BP three-terminal UV / IR dual-phase photodetector based on a sapphire substrate. Compared with the traditional ZnS / MoS2 three-terminal UV / IR dual-phase photodetector, the detector has a detection rate of 2.39×10 at a wavelength of 254nm in the ultraviolet band under the built-in electric field and negative gate voltage. 6 MW -1, the detection rate at 808nm wavelength in the infrared band reaches 535mAW -1 , with higher light response.

[0005] Including the above two existing technologies, the existing β-Ga2O3 / BP two-phase photodetector has a small built-in electric field at the interface, resulting in a narrow depletion region, which cannot effectively separate electrons and holes, resulting in lower photoresponsivity and a narrow detection band. Under infrared light, a large number of holes that cannot drift will be generated at the interface of β-Ga2O3 / BP and form recombination centers, resulting in relatively low photoresponsivity in the infrared band. Summary of the invention

[0006] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a UV / IR heterojunction dual-phase detector based on polarity enhancement and a preparation method thereof, introduce intrinsic polarity within the layer to further improve the performance of UV / IR dual-phase detector electronics, and realize sensitive detection of deep ultraviolet and near-infrared optical signals, which can be used in the fields of ray measurement and detection, industrial automatic control, photometry, etc.

[0007] In order to achieve the above object, the technical solution adopted by the present invention is:

[0008] A UV / IR heterojunction dual-phase detector based on polarity enhancement comprises a substrate, a wide bandgap semiconductor layer, a narrow bandgap two-dimensional material layer and a metal electrode arranged in sequence; the narrow bandgap two-dimensional material layer adopts a material with intrinsic polarity to introduce intrinsic electric field polarity drive to the heterojunction interface.

[0009] In one embodiment, the narrow bandgap two-dimensional material layer is made of Janus two-dimensional material with intrinsic polarity, and the wide bandgap semiconductor layer is made of β-Ga2O3 or wide bandgap hexagonal AlN.

[0010] In one embodiment, the Janus two-dimensional material with intrinsic polarity is Janus-AsP, Bi2TeO5, MoTe2 or In2Se3.

[0011] The present invention also provides a method for preparing the UV / IR heterojunction dual-phase detector based on polarity enhancement, preparing a wide bandgap semiconductor layer on a substrate, and transferring the prepared narrow bandgap two-dimensional material layer to the wide bandgap semiconductor layer, and flipping the narrow bandgap two-dimensional material layer to achieve regulation of its polarity direction, and finally preparing a metal electrode on the narrow bandgap two-dimensional material layer.

[0012] In one embodiment, the narrow bandgap two-dimensional material layer is a two-dimensional material Janus-AsP with intrinsic polarity, which is prepared by the following method:

[0013] Place a layered black phosphorus sheet on a substrate, connect the Ar gas path and the As gas path under sealing conditions for surface selenization, set the temperature at 800-1000°C, the heating time at 90-120 min, and the constant temperature selenization time at 180-240 min. Then place it in a tubular furnace, anneal at 400-500°C, and anneal for 60-120 min to obtain the two-dimensional material Janus-AsP.

[0014] In one embodiment, the layered black phosphorus flakes are obtained by:

[0015] The layered black phosphorus block is placed on a tape and repeatedly pasted and peeled off to thin it to obtain a layered flake with a thickness of less than 2nm. The layered flake on the tape is transferred to a substrate. After a period of rest, the tape is peeled off to leave the material on the substrate.

[0016] In one embodiment, the wide bandgap semiconductor layer is β-Ga2O3, and the method for preparing the wide bandgap semiconductor layer on the substrate is as follows:

[0017] The substrate is placed in a reaction chamber and β-Ga2O3 is prepared by magnetron sputtering.

[0018] In one embodiment, the narrow bandgap two-dimensional material layer is transferred to the wide bandgap semiconductor layer by the following method:

[0019] A two-dimensional material self-alignment transfer table is used to place a narrow bandgap two-dimensional material layer on the transfer polymer and fix it, and then transfer it to the top platform. The substrate prepared with a wide bandgap semiconductor layer is placed on the bottom platform, and the distance between the wide bandgap semiconductor layer and the narrow bandgap two-dimensional material layer is adjusted. The bottom platform is heated to fit the two together to complete the transfer; annealing is then performed to improve adhesion. During this process, the polarity direction of the narrow bandgap two-dimensional material layer is regulated by flipping it.

[0020] In one embodiment, the transfer polymer is polydimethylsiloxane (PDMS) or polymethyl methacrylate (PMMA).

[0021] In one embodiment, the annealing improves adhesion under the following conditions: annealing at 200° C. for 120 min.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] The present invention replaces the traditional two-dimensional material BP by using Janus-AsP with intrinsic polarity. Due to the surface selenization of Janus-AsP, the plane mirror symmetry is broken and an intrinsic electric field is introduced into the layer, thereby introducing an additional carrier driving effect for the β-Ga2O3 / AsP heterojunction interface, reducing the high electron-hole recombination of the β-Ga2O3 / BP structure photodetector, so that the polarity-enhanced β-Ga2O3 / AsP heterojunction two-phase detector of the present invention has a higher electron-hole secondary separation rate, a longer carrier lifetime, and a smaller dark current, thereby effectively improving the detector's properties such as the light response and detection band. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic structural diagram of the UV / IR heterojunction dual-phase detector based on polarity enhancement of the present invention.

[0025] Figure 2 It is a preparation flow chart of the polarity-enhanced UV / IR heterojunction dual-phase detector of the present invention. DETAILED DESCRIPTION

[0026] The embodiments of the present invention are described in detail below with reference to the accompanying drawings and examples.

[0027] like Figure 1 As shown, the present invention is a UV / IR heterojunction dual-phase detector based on polarity enhancement, comprising a substrate 1, a wide bandgap semiconductor layer 2, a narrow bandgap two-dimensional material layer 3 and a metal electrode 4. As is common knowledge, the above layers can be arranged in sequence from bottom to top.

[0028] Among them, the narrow bandgap two-dimensional material layer 3 of the present invention adopts a material with intrinsic polarity, thereby introducing an intrinsic electric field polarity drive for the heterojunction interface, providing an additional driving effect for the interface carrier transport. The detailed principle is that by constructing the heterojunction interface of the wide bandgap semiconductor layer 2 and the narrow bandgap two-dimensional material layer 3, due to the difference in work function, the built-in electric field of the interface can effectively drive the separation of photogenerated electrons and holes. On this basis, the present invention introduces a material with intrinsic polarity as the narrow bandgap two-dimensional material layer 3. Due to the existence of its intrinsic polarity, it can provide an additional driving effect for the carrier separation and transmission of the interface, and the holes driven and separated into the narrow bandgap two-dimensional material layer 3 are further transferred to the side away from the interface, realizing the secondary separation of electrons and holes in the layer, thereby greatly improving the efficiency of the interface photoelectric effect, reducing exciton recombination, and improving the carrier lifetime and device performance.

[0029] In the present invention, the substrate 1 is a silicon substrate or a sapphire substrate. The narrow bandgap two-dimensional material layer 3 is a Janus two-dimensional material with intrinsic polarity, and the wide bandgap semiconductor layer 2 is β-Ga2O3 or wide bandgap hexagonal AlN. Among them, the Janus two-dimensional material with intrinsic polarity can be Janus-AsP, Bi2TeO5, MoTe2 or In2Se3.

[0030] The present invention focuses on β-Ga2O3 and Janus-AsP as examples, and the situations of other materials are basically similar. When the wide bandgap semiconductor layer 2 uses β-Ga2O3 and the narrow bandgap two-dimensional material layer 3 uses Janus-AsP, compared with the traditional β-Ga2O3 / BP heterojunction UV / IR dual-phase photodetector in the past, the present invention introduces Janus-AsP with intrinsic polarity to replace the traditional two-dimensional material BP. Janus-AsP breaks the plane mirror symmetry due to its surface selenization, introduces the intrinsic electric field in the layer, and thus introduces additional carrier driving effect to the β-Ga2O3 / AsP heterojunction interface, which can realize the effective separation of photogenerated electrons and holes at its interface, thereby effectively improving the properties of the detector such as the light response and detection band.

[0031] The present invention also provides a method for preparing the UV / IR heterojunction dual-phase detector based on polarity enhancement, referring to Figure 2 As shown, the main process includes: pre-treating the substrate 1, then preparing a wide bandgap semiconductor layer 2 on the pre-treated substrate 1, preparing a narrow bandgap two-dimensional material layer 3, transferring it to the wide bandgap semiconductor layer 2, and flipping the narrow bandgap two-dimensional material layer 3 to achieve regulation of its polarity direction, and finally preparing a metal electrode 4 on the narrow bandgap two-dimensional material layer 3.

[0032] In an embodiment of the present invention, the method for pre-treating the substrate 1 is as follows:

[0033] A SiC substrate was selected and sequentially cleaned with deionized water, acetone, isopropanol, deionized water and 50° C. ultrasonic cleaning, with each cleaning time being 20 min.

[0034] The ultrasonically cleaned substrate 1 was dried with nitrogen and treated with ultraviolet ozone UV-zone for 15 minutes to obtain a pretreated substrate 1 for subsequent use.

[0035] In an embodiment of the present invention, the narrow bandgap two-dimensional material layer 3 is a two-dimensional material Janus-AsP having intrinsic polarity, which is prepared by the following method:

[0036] Place the layered black phosphorus flakes on the substrate, push them into the middle of the tubular furnace, and seal them. Connect the Ar gas path and the As gas path for surface selenization, set the temperature at 800-1000°C, the heating time at 90-120min, and the constant temperature selenization time at 180-240min, preferably 800°C, 90min, 180min. Then put it into the tubular furnace, anneal at 400-500°C, anneal for 60-120min, preferably 400°C, 60min, to obtain the two-dimensional material Janus-AsP.

[0037] Layered black phosphorus flakes can be prepared by placing the layered black phosphorus block to be peeled off on a transparent tape, repeatedly sticking and peeling the block material to thin it to obtain a layered flake with a thickness of less than 2nm, transferring the layered flake on the tape to the target substrate (such as SiO2 / Si), and peeling off the tape after a period of rest, leaving the material on the substrate.

[0038] In an embodiment of the present invention, the wide bandgap semiconductor layer 2 is β-Ga2O3, and the method for preparing the wide bandgap semiconductor layer 2 on the substrate 1 is as follows:

[0039] The pretreated SiC substrate was placed in the reaction chamber, and the β-Ga2O3 semiconductor material was prepared by magnetron sputtering. First, a high-purity β-Ga2O3 semiconductor target was placed in the reaction chamber, and the distance between the target and the SiC substrate was adjusted to 50 mm. The reaction chamber was evacuated to a vacuum of 6×10 -4 Pa, the substrate temperature was heated to 800°C, and 99.99% high-purity Ar gas was introduced to stabilize the vacuum degree of the sputtering process at 0.6 Pa. The sputtering power was 150 W, the sputtering film thickness was 200 nm, and a wide bandgap semiconductor layer β-Ga2O3 was prepared.

[0040] In an embodiment of the present invention, the narrow bandgap two-dimensional material layer 3 is transferred to the wide bandgap semiconductor layer 2 by the following method:

[0041] Using a two-dimensional material self-aligned transfer platform, the two-dimensional material Janus-AsP is placed on the transfer polymer and fixed with tape or other means, and then transferred to the top platform, the substrate / β-Ga2O3 structure is placed on the bottom platform, and the vertical knob is continuously adjusted to change the distance between the wide bandgap semiconductor layer 2 and the narrow bandgap two-dimensional material layer 3 until it can be seen on the screen, and the bottom platform is heated to about 85°C, and the two are bonded to complete the transfer. Subsequently, annealing at 200°C for 120 minutes in a tube furnace improves the adhesion between Janus-AsP and β-Ga2O3. In this process, the polar two-dimensional material Janus-AsP is flipped to achieve the regulation of its polar direction.

[0042] The transfer polymer may be polydimethylsiloxane (PDMS) or polymethyl methacrylate (PMMA).

[0043] In an embodiment of the present invention, the metal electrode 4 is prepared by the following method:

[0044] Two metal electrode areas were photolithographically formed and the vacuum degree of the chamber was 10 -5 Pa below Ti / Au (20 / 100 nm) was evaporated at a rate of 1000 nm to obtain a metal electrode 4, and finally the preparation of the β-Ga2O3 / AsP heterojunction dual-phase detector was completed.

[0045] The above describes the specific technical solutions of the present invention. It should be understood that the present invention is not limited to the above specific implementations, and those skilled in the art can make various modifications or variations within the scope of the claims, which do not affect the essential content of the present invention.

Claims

1. A UV / IR heterojunction dual-phase detector based on polarity enhancement, characterized in that: It comprises a substrate (1), a wide bandgap semiconductor layer (2), a narrow bandgap two-dimensional material layer (3) and a metal electrode (4) which are arranged in sequence; the narrow bandgap two-dimensional material layer (3) is made of a material with intrinsic polarity, so as to introduce intrinsic electric field polarity drive for the heterojunction interface.

2. The UV / IR heterojunction dual-phase detector based on polarity enhancement according to claim 1, characterized in that: The narrow bandgap two-dimensional material layer (3) is made of Janus two-dimensional material with intrinsic polarity, and the wide bandgap semiconductor layer (2) is made of β-Ga2O3 or wide bandgap hexagonal AlN.

3. The UV / IR heterojunction dual-phase detector based on polarity enhancement according to claim 1, characterized in that: The Janus two-dimensional material with intrinsic polarity is Janus-AsP, Bi2TeO5, MoTe2 or In2Se3.

4. The method for preparing the polarity-enhanced UV / IR heterojunction dual-phase detector according to any one of claims 1 to 3, characterized in that: A wide bandgap semiconductor layer (2) is prepared on a substrate (1), and a prepared narrow bandgap two-dimensional material layer (3) is transferred onto the wide bandgap semiconductor layer (2). The polarity direction of the narrow bandgap two-dimensional material layer (3) is regulated by flipping the narrow bandgap two-dimensional material layer (3), and finally a metal electrode (4) is prepared on the narrow bandgap two-dimensional material layer (3).

5. The preparation method according to claim 4, characterized in that: The narrow bandgap two-dimensional material layer (3) is a two-dimensional material Janus-AsP with intrinsic polarity, which is prepared by the following method: Place a layered black phosphorus sheet on a substrate, connect the Ar gas path and the As gas path under sealing conditions for surface selenization, set the temperature at 800-1000°C, the heating time at 90-120 min, and the constant temperature selenization time at 180-240 min. Then place it in a tubular furnace, anneal at 400-500°C, and anneal for 60-120 min to obtain the two-dimensional material Janus-AsP.

6. The preparation method according to claim 5, characterized in that: The layered black phosphorus flakes are obtained by: The layered black phosphorus block is placed on a tape and repeatedly pasted and peeled off to thin it to obtain a layered flake with a thickness of less than 2nm. The layered flake on the tape is transferred to a substrate. After a period of rest, the tape is peeled off to leave the material on the substrate.

7. The preparation method according to claim 4, characterized in that: The wide bandgap semiconductor layer (2) is β-Ga2O3, and the method for preparing the wide bandgap semiconductor layer (2) on the substrate (1) is as follows: The substrate (1) is placed in a reaction chamber, and β-Ga2O3 is prepared by magnetron sputtering.

8. The preparation method according to any one of claims 5 to 7, characterized in that: The method of transferring the narrow bandgap two-dimensional material layer (3) onto the wide bandgap semiconductor layer (2) is as follows: A two-dimensional material self-alignment transfer platform is used to place a narrow bandgap two-dimensional material layer (3) on a transfer polymer and fix it, and then transfer it to the top platform, and a substrate (1) prepared with a wide bandgap semiconductor layer (2) is placed on the bottom platform, and the distance between the wide bandgap semiconductor layer (2) and the narrow bandgap two-dimensional material layer (3) is adjusted, and the bottom platform is heated to fit the two together to complete the transfer; and then annealing is performed to improve adhesion.

9. The preparation method according to claim 8, characterized in that: The transfer polymer is polydimethylsiloxane (PDMS) or polymethyl methacrylate (PMMA).

10. The preparation method according to claim 8, characterized in that: The annealing improves the adhesion, and the conditions are: annealing at 200° C. for 120 minutes.