Carbon fiber reinforced modified polytetrafluoroethylene microporous membrane and manufacturing method thereof
By enhancing the sintering process of carbon fiber and double-pull film in the polytetrafluoroethylene microporous membrane, the problems of short blocking period and poor strength of conventional microporous membranes are solved, and higher tensile strength and filtration accuracy are achieved, which extends the Lifespan and reduce costs.
Patent Information
- Application Number
- CN202411319521.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-23
- Publication Date
- 2024-11-29
AI Technical Summary
Conventional porous polytetrafluoroethylene microporous membranes break due to short blocking cycle and poor film wire strength, resulting in short service life, low backwashing efficiency and high cost.
Using carbon fiber reinforced modification of polytetrafluoroethylene microporous membrane, the polytetrafluoroethylene double-pull film and carbon fiber wire are coated on the porous polytetrafluoroethylene hollow fiber tube, and bonded through the sintering process to form enhanced modification microporous membrane.
The tensile strength of the membrane is improved, the membrane wire breakage is avoided, the anti-fouling period is extended, the filtration accuracy and flux are improved, and the use cost is reduced.
Smart Images

Figure CN119034510A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of polytetrafluoroethylene microporous membranes, and in particular relates to a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane and a manufacturing method thereof. Background Art
[0002] Polytetrafluoroethylene, or PTFE, has excellent comprehensive properties such as high temperature resistance, corrosion resistance, non-stickiness, self-lubrication, excellent dielectric properties, and very low friction coefficient. The hollow fiber membrane made of it has the advantages of oxidation resistance, acid and alkali resistance, temperature resistance, and good biocompatibility. After hydrophilic treatment, it is particularly suitable for microporous membrane filtration technology. As a key process in sewage treatment, its high-efficiency filtration and low-cost maintenance directly affect the direct interests of sewage treatment companies. The polytetrafluoroethylene microporous membrane has excellent chemical stability, small micropore diameter, and high filtration accuracy. However, during use, conventional porous polytetrafluoroethylene microporous membranes face the problems of short clogging cycle, poor membrane fiber strength, and broken fibers.
[0003] By filling and modifying polytetrafluoroethylene with carbon fiber, the mechanical properties of polytetrafluoroethylene can be improved, which is helpful to solve the problem of broken wires in polytetrafluoroethylene microporous membranes. This is because carbon fiber, as an important load-bearing unit, can play a role in sharing stress, and the interface of the composite material is a stress transmission bridge between the matrix and the filler. The interface performance determines the various mechanical properties. Excessive filling will lead to a decrease in the interface bonding performance of the composite material, thereby reducing the tensile performance of the composite material. Therefore, although the comprehensive performance of the carbon fiber polytetrafluoroethylene membrane is improved under actual working conditions, the tensile performance of the composite material is significantly reduced, and it is more prone to deformation and wear. Therefore, it is necessary to perform surface modification on the carbon fiber to improve the surface adhesion and wettability of the carbon fiber, improve the interface bonding ability of the carbon fiber composite material, and then improve the mechanical properties of the composite material.
[0004] Therefore, there is an urgent need for an enhanced carbon fiber reinforced modified polytetrafluoroethylene microporous membrane and a manufacturing method thereof that can prevent membrane filament breakage, has higher backwash efficiency, longer service life, and lower cost. Summary of the invention
[0005] In view of this, the technical problem to be solved by the present invention is to provide a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane and a manufacturing method thereof, so as to avoid the problems of short clogging period, poor membrane filament strength and filament breakage faced by conventional porous polytetrafluoroethylene microporous membranes.
[0006] In order to solve the above technical problems, the present invention discloses a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane, which comprises: A supporting tube portion, wherein the supporting tube portion is configured as a porous polytetrafluoroethylene hollow fiber tube; A filter membrane is covered on the outer surface of the supporting tube, wherein the filter membrane is a polytetrafluoroethylene double-stretch membrane; and Carbon fiber filaments wound around the outer surface of the filter membrane; The carbon fiber filaments and the filter membrane are coated on the surface of the supporting tube through a sintering process.
[0007] The present invention also discloses a method for manufacturing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane, comprising: Step 1: pre-impregnate the carbon fiber filaments in a polytetrafluoroethylene dispersion suspension at a speed of 1 m / min, and dry them at 120°C for later use; Step 2: Weigh 20% wt of kerosene and polytetrafluoroethylene fine powder, and prepare a porous polytetrafluoroethylene hollow fiber tube with a porosity greater than 80% through processes such as blending, compacting, extrusion, degreasing, stretching and curing to obtain a support tube; Step 3: Weigh 22% wt of kerosene and polytetrafluoroethylene powder, and prepare a polytetrafluoroethylene double-stretched membrane with a pore size of 0.1µm to 0.2µm and a porosity of ≥85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing to obtain a filter membrane; wherein the biaxial stretching process can effectively control the size and uniformity of the micropore diameter of the filter membrane.
[0008] Step 4: Use winding equipment with an outer diameter less than 3 mm to wind the pre-impregnated carbon fiber filaments and the filter membrane with uniform slitting width on the outer surface of the support tube; sinter and bond the carbon fiber filaments and the filter membrane to the support tube at a temperature higher than the melting temperature of polytetrafluoroethylene to obtain a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane.
[0009] According to one embodiment of the present invention, the carbon fiber filaments in the above step 1 are selected from any one of T600, T800 and T1000.
[0010] According to one embodiment of the present invention, the solid content of the polytetrafluoroethylene suspension pre-impregnated with the carbon fiber filaments in the above step 1 is greater than 60%, ensuring that the PTFE nanoparticles are maximized and evenly attached to the surface, and the adhesion between the sintered carbon fiber filaments and the polytetrafluoroethylene microporous tube is optimal.
[0011] According to one embodiment of the present invention, the overlap width of the filtration membrane in the above step 4 is in the range of 2 mm to 3 mm. The membrane has high filtration accuracy and large filtration flux.
[0012] According to an embodiment of the present invention, the sintering process in step 4 applies a load to the filter membrane, thereby improving the bonding force between the carbon fiber filaments and the filter membrane.
[0013] According to an embodiment of the present invention, the winding spacing of the carbon fiber filaments in the above step 4 is controlled at 1 mm ± 0.5, which can improve the optimal tensile strength performance without affecting the filtered water flux.
[0014] Compared with the prior art, the present invention can achieve the following technical effects: By reinforcing carbon fiber and polytetrafluoroethylene double-stretched membrane, winding and sintering it in a porous polytetrafluoroethylene hollow fiber tube, a reinforced modified polytetrafluoroethylene microporous membrane is prepared. It has ideal tensile strength, avoiding membrane filament breakage during use, and at the same time has high filtration accuracy and a longer anti-fouling and clogging cycle.
[0015] Of course, any product implementing the present invention does not necessarily need to achieve all of the above-mentioned technical effects at the same time. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings: Figure 1 A microscopic schematic diagram of a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the winding process of the carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to an embodiment of the present invention. DETAILED DESCRIPTION
[0017] The following will describe the implementation methods of the present invention in detail with reference to the accompanying drawings and embodiments, so that the implementation process of how the present invention applies technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.
[0018] Please refer to Figure 1 and Figure 2 , Figure 1 A microscopic schematic diagram of a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the winding process of the carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to an embodiment of the present invention.
[0019] A carbon fiber reinforced modified polytetrafluoroethylene microporous membrane comprises: a supporting tube portion, which is configured as a porous polytetrafluoroethylene hollow fiber tube; a filter membrane coated on the outer surface of the supporting tube portion, which is configured as a polytetrafluoroethylene double-stretched membrane; and carbon fiber filaments wound on the outer surface of the filter membrane; wherein the carbon fiber filaments and the filter membrane are coated on the surface of the supporting tube portion by a sintering process.
[0020] The specific manufacturing method is: Step 1: Pre-impregnate the carbon fiber filaments in a polytetrafluoroethylene dispersion suspension at a speed of 1m / min, and dry at 120°C for standby use; the carbon fiber filaments are selected from any one of T600, T800, and T1000; the solid content of the polytetrafluoroethylene suspension pre-impregnated with the carbon fiber filaments is greater than 60%. Ensure that the PTFE nanoparticles are maximized and evenly attached to its surface, and the adhesion between the sintered carbon fiber filaments and the polytetrafluoroethylene microporous tube is optimal.
[0021] Step 2: Weigh 20% wt of kerosene and polytetrafluoroethylene fine powder, and prepare a porous polytetrafluoroethylene hollow fiber tube with a porosity greater than 80% through processes such as blending, compacting, extrusion, degreasing, stretching and curing to obtain a support tube; Step 3: Weigh 22% wt of kerosene and polytetrafluoroethylene powder, and prepare a polytetrafluoroethylene double-stretched membrane with a pore size of 0.1µm to 0.2µm and a porosity of ≥85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing to obtain a filter membrane; wherein the biaxial stretching process can effectively control the size and uniformity of the micropore diameter of the filter membrane.
[0022] Step 4: Use winding equipment with an outer diameter of less than 3mm, and wind the pre-impregnated carbon fiber filaments and the filter membrane with uniform slitting width on the outer surface of the support tube; at a temperature higher than the melting temperature of polytetrafluoroethylene, sinter and bond the carbon fiber filaments and the filter membrane to the support tube to obtain a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane. The overlap width of the filter membrane ranges from 2mm to 3mm. The membrane has high filtration accuracy and large filtration flux. During the sintering process, a load is applied to the filter membrane. It can improve the adhesion between the carbon fiber filaments and the filter membrane. The winding spacing of the carbon fiber filaments is controlled at 1mm±0.5. It can not only improve the optimal tensile strength performance, but also does not affect the filtration water flux.
[0023] Comparative Case 1 20% wt of kerosene and polytetrafluoroethylene fine powder were weighed, and a porous polytetrafluoroethylene hollow fiber tube with a porosity of 80% was prepared through the processes of blending, pressing, extrusion, degreasing, stretching and curing; 22% wt of kerosene and polytetrafluoroethylene powder were weighed, and a polytetrafluoroethylene double-stretched membrane with a pore size of 0.1µm and a porosity of 85% was prepared through the processes of blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing, and the membrane was cut into narrow membranes with a width of 10 mm; a special microporous tube winding equipment was used to evenly wind the ePTFE narrow membrane on the outer surface of the microporous tube; the filter membrane was sintered and bonded to the support tube under conditions higher than the melting temperature and load of polytetrafluoroethylene, and the polytetrafluoroethylene microporous membrane could be used for sewage filtration after hydrophilic treatment.
[0024] Implementation Case 1 A polytetrafluoroethylene suspension with a solid content of 60% was selected, and T600 carbon fiber filaments were pre-impregnated at a speed of 1m / min, and dried at 120°C for standby use; 20% wt of kerosene and polytetrafluoroethylene fine powder were weighed, and a porous polytetrafluoroethylene hollow fiber tube with a porosity of 80% was prepared through blending, pressing, extrusion, degreasing, stretching and curing; 22% wt of wt% kerosene and polytetrafluoroethylene powder are prepared into polytetrafluoroethylene double-stretched membrane with pore size of 0.1µm and porosity of 85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing, and then cut into narrow membranes with a width of 10mm; special microporous tube winding equipment is used to evenly wind the pre-impregnated carbon fiber filaments and ePTFE narrow membrane on the outer surface of the microporous tube (carbon fiber filaments inside, ePTFE membrane outside), and the spacing between the carbon fiber filaments is 1mm; under conditions higher than the melting temperature and load of polytetrafluoroethylene, the carbon fiber filaments and the filter membrane are sintered and bonded to the support tube, and the enhanced modified polytetrafluoroethylene microporous membrane can be used for sewage filtration after hydrophilic treatment.
[0025] Implementation Case 2 A polytetrafluoroethylene suspension with a solid content of 60% was selected, and T800 carbon fiber filaments were pre-impregnated at a speed of 1m / min, and dried at 120°C for standby use; 20% wt of kerosene and polytetrafluoroethylene fine powder were weighed, and a porous polytetrafluoroethylene hollow fiber tube with a porosity of 80% was prepared through blending, pressing, extrusion, degreasing, stretching and curing; 22% wt of wt% kerosene and polytetrafluoroethylene powder are prepared into polytetrafluoroethylene double-stretched membrane with pore size of 0.1µm and porosity of 85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing, and then cut into narrow membranes with a width of 10mm; special microporous tube winding equipment is used to evenly wind the pre-impregnated carbon fiber filaments and ePTFE narrow membrane on the outer surface of the microporous tube (carbon fiber filaments inside, ePTFE membrane outside), and the spacing between the carbon fiber filaments is 1mm; under conditions higher than the melting temperature and load of polytetrafluoroethylene, the carbon fiber filaments and the filter membrane are sintered and bonded to the support tube, and the enhanced modified polytetrafluoroethylene microporous membrane can be used for sewage filtration after hydrophilic treatment.
[0026] Implementation Case 3 A polytetrafluoroethylene suspension with a solid content of 60% was selected, and T1000 carbon fiber filaments were pre-impregnated at a speed of 1m / min, and dried at 120°C for standby use; 20% wt of kerosene and polytetrafluoroethylene fine powder were weighed, and a porous polytetrafluoroethylene hollow fiber tube with a porosity of 80% was prepared through the processes of blending, pressing, extrusion, degreasing, stretching and curing; 22% wt of wt% kerosene and polytetrafluoroethylene powder are prepared into polytetrafluoroethylene double-stretched membrane with pore size of 0.2µm and porosity of 85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing, and then cut into narrow membranes with a width of 10mm; special microporous tube winding equipment is used to evenly wind the pre-impregnated carbon fiber filaments and ePTFE narrow membrane on the outer surface of the microporous tube (carbon fiber filaments inside, ePTFE membrane outside), and the spacing between the carbon fiber filaments is 1mm; under conditions higher than the melting temperature and load of polytetrafluoroethylene, the carbon fiber filaments and the filter membrane are sintered and bonded to the support tube, and the enhanced modified polytetrafluoroethylene microporous membrane is subjected to hydrophilic treatment and can be used for sewage filtration.
[0027] Implementation Case 4 A polytetrafluoroethylene suspension with a solid content of 60% was selected, and T1000 carbon fiber filaments were pre-impregnated at a speed of 1m / min, and dried at 120°C for standby use; 20% wt of kerosene and polytetrafluoroethylene fine powder were weighed, and a porous polytetrafluoroethylene hollow fiber tube with a porosity of 80% was prepared through the processes of blending, pressing, extrusion, degreasing, stretching and curing; 22% wt of wt% kerosene and polytetrafluoroethylene powder are prepared into polytetrafluoroethylene double-stretched membrane with pore size of 0.2µm and porosity of 85% through processes such as blending, pressing, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing, and then cut into narrow membranes with a width of 10mm; special microporous tube winding equipment is used to evenly wind the pre-impregnated carbon fiber filaments and ePTFE narrow membrane on the outer surface of the microporous tube (carbon fiber filaments inside, ePTFE membrane outside), and the spacing between the carbon fiber filaments is 1.5mm; under conditions higher than the melting temperature and load of polytetrafluoroethylene, the carbon fiber filaments and the filter membrane are sintered and bonded to the support tube, and the enhanced modified polytetrafluoroethylene microporous membrane can be used for sewage filtration after hydrophilic treatment.
[0028] The properties of the enhanced modified polytetrafluoroethylene microporous membranes prepared in the above comparative cases and example cases are shown in the following table: Project Name Tensile strength / N Filter turbidity / NTU Pure water flux / LMH Comparative Case 1 67 0.182 2125 Implementation Case 1 85 0.167 2046 Implementation Case 2 88 0.172 1989 Implementation Case 3 91 0.185 2027 Implementation Case 4 86 0.239 2103 It can be seen from the data in the above table that the mechanical properties of the carbon fiber reinforced modified polytetrafluoroethylene microporous tube are significantly improved, and at the same time, the effect on the pure water flux is not significant.
[0029] In summary, the present invention prepares a reinforced modified polytetrafluoroethylene microporous membrane by reinforcing carbon fiber and polytetrafluoroethylene double-stretched membrane, winding and sintering it in a porous polytetrafluoroethylene hollow fiber tube. The reinforced modified polytetrafluoroethylene microporous membrane has ideal tensile strength, which can avoid membrane filament breakage during use, and at the same time has high filtration accuracy and a longer anti-fouling and clogging cycle.
[0030] The above description shows and describes several preferred embodiments of the present invention, but as mentioned above, it should be understood that the present invention is not limited to the form disclosed herein, and should not be regarded as excluding other embodiments, but can be used in various other combinations, modifications and environments, and can be modified within the scope of the invention concept described herein through the above teachings or the technology or knowledge of the relevant field. Changes and variations made by those skilled in the art do not depart from the spirit and scope of the present invention, and should be within the scope of protection of the claims attached to the present invention.
Claims
1. A carbon fiber reinforced modified polytetrafluoroethylene microporous membrane, It is characterized in that include: A supporting tube portion, wherein the supporting tube portion is configured as a porous polytetrafluoroethylene hollow fiber tube; A filter membrane covered on the outer surface of the support tube, wherein the filter membrane is a polytetrafluoroethylene double-stretch membrane; as well as Carbon fiber filaments wound on the outer surface of the filter membrane; Wherein, the carbon fiber filaments and the filter membrane are coated on the surface of the supporting tube portion through a sintering process.
2. A method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane as claimed in claim 1, It is characterized in that include: Step 1: pre-impregnate the carbon fiber filaments in a polytetrafluoroethylene dispersion suspension at a speed of 1 m / min, and dry them at 120°C for later use; Step 2: Weigh 20% wt of kerosene and polytetrafluoroethylene fine powder, and prepare a porous polytetrafluoroethylene hollow fiber tube with a porosity greater than 80% through processes such as blending, compacting, extrusion, degreasing, stretching and curing to obtain a support tube; Step 3: Weigh 22% wt of kerosene and polytetrafluoroethylene powder, and prepare a polytetrafluoroethylene double-stretched membrane with a pore size of 0.1µm to 0.2µm and a porosity of ≥85% through the processes of blending, compacting, extrusion, calendering, degreasing, uniaxial stretching, biaxial stretching and curing to obtain a filter membrane; Step 4: Use winding equipment with an outer diameter less than 3 mm to wind the pre-impregnated carbon fiber filaments and the filter membrane with uniform slitting width on the outer surface of the support tube; sinter and bond the carbon fiber filaments and the filter membrane to the support tube at a temperature higher than the melting temperature of polytetrafluoroethylene to obtain a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane.
3. The method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to claim 2, It is characterized in that The carbon fiber filaments in step 1 are selected from any one of T600, T800 and T1000.
4. The method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to claim 2, It is characterized in that The solid content of the polytetrafluoroethylene suspension pre-impregnated with carbon fiber filaments in step 1 is greater than 60%.
5. The method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to claim 2, It is characterized in that The overlapping width of the filter membrane in step 4 is in the range of 2 mm to 3 mm.
6. The method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to claim 2, It is characterized in that The sintering process in step 4 applies a load to the filter membrane.
7. The method for producing a carbon fiber reinforced modified polytetrafluoroethylene microporous membrane according to claim 2, It is characterized in that The winding spacing of the carbon fiber filaments in step 4 is controlled at 1 mm ± 0.5.
Citation Information
Cited By
Preparation process of polyvinylidene fluoride air filtering membrane capable of rapidly thickening in low-temperature environment
CN122183399A