Laser cutting die and die processing technology

By designing grooves and air guide holes on the laser cutting mold and combining surface treatment technology, the heat accumulation problem in laser cutting is solved, the cutting accuracy is improved and the cost is reduced, and the efficient laser cutting effect is achieved.

CN119035803APending Publication Date: 2024-11-29CYMMETRIK SHENZHEN PRINTING
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411395271.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

Traditional laser cutting molds are prone to heat accumulation during the cutting process, resulting in problems such as degradation of cutting quality, rough cutting edges, and deformation of materials. High-precision femtosecond laser equipment is expensive and has a high failure rate.

Method used

A subject laser cutting mold is designed, including a first groove and a air guide hole formed in the first direction of the base plate. The air guide hole is in communication with the groove for conducting heat and cutting impurities, and the adsorption hole is used to adsorb the material to be cut, through CNC machining forms grooves and air guide holes, and grinds and chrome plating on the surface to ensure rapid heat conduction and residual material removal.

Benefits of technology

It reduces the thermal effect of laser cutting, improves product accuracy and wear resistance of the mold, reduces manufacturing costs, and extends the service life of the mold.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035803A_ABST
    Figure CN119035803A_ABST
Patent Text Reader

Abstract

The invention discloses a laser cutting mold and a mold machining process, and relates to the technical field of mold machining, the laser cutting mold comprises a bottom plate, a first groove is formed in the bottom plate in the first direction, and an air guide hole and an adsorption hole are further formed in the bottom plate in a penetrating mode; wherein the air guide holes are communicated with the first groove and used for conducting heat and impurities generated by laser cutting, and the adsorption holes are used for adsorbing materials to be cut; the invention aims to reduce the heat effect of laser cutting and improve the product precision while reducing the manufacturing cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of mold processing, and in particular to a laser cutting mold and a mold processing technology. Background Art

[0002] Laser cutting is widely used for processing metals, plastics, and other materials due to its high precision and efficiency. However, traditional laser cutting molds are prone to heat buildup during the cutting process, leading to reduced cutting quality, rough edges, and material deformation. These issues not only affect production efficiency but also increase the difficulty of subsequent processing.

[0003] Currently, most manufacturers use femtosecond lasers for cutting and forming to minimize the impact of thermal effects, but this high-precision femtosecond laser equipment is expensive and has a relatively high failure rate. Summary of the Invention

[0004] The main purpose of the present invention is to provide a mold and a mold processing process, which aims to reduce the thermal effect of laser cutting and improve product precision while reducing manufacturing costs.

[0005] To achieve the above-mentioned object, the subject laser cutting mold proposed in the present invention includes a bottom plate, wherein the bottom plate is formed with a first groove along a first direction, and the bottom plate is further provided with at least one air guide hole and at least one adsorption hole;

[0006] The air guide hole is connected to the first groove for conducting heat and cutting impurities, and the adsorption hole is used for adsorbing the material to be cut.

[0007] In one embodiment, the bottom plate is made of steel, and the hardness H of the steel satisfies: 58HRC <H<64HRC。

[0008] In one embodiment, the depth of the first groove along the first direction is greater than 1 mm.

[0009] In one embodiment, the depth of the first groove in the first direction gradually increases along the second direction.

[0010] In one embodiment, a second groove is formed on the bottom plate along the first direction, the second groove is communicated with the first groove, and the air guide hole is communicated with the first groove through the second groove.

[0011] In one embodiment, the second groove comprises a plurality of grooves, and the plurality of second grooves are spaced around the first groove;

[0012] There are multiple air guide holes, and the multiple air guide holes are connected to each other corresponding to the second grooves.

[0013] In one embodiment, a protrusion is provided on the bottom surface of the inner cavity of the first groove, an upper end surface of the protrusion is flush with the surface of the bottom plate, and the protrusion is spaced apart from the inner peripheral wall of the first groove.

[0014] The present invention also proposes a mold processing process, based on the above-mentioned laser cutting mold, comprising the following steps:

[0015] providing a bottom plate;

[0016] Design mold structure through software;

[0017] Forming air guide holes and adsorption holes on the bottom plate by wire cutting;

[0018] A first groove is machined on the bottom plate by CNC numerical control, and the first groove is connected to the air guide hole;

[0019] The bottom plate is surface treated.

[0020] In one embodiment, the step of “machining a first groove on the bottom plate by CNC numerical control, and making the first groove communicate with the air guide hole” further includes:

[0021] In the process of machining the first groove, a bump is formed on the bottom wall of the inner cavity of the first groove, and the distance between the bump and the laser cutting path is greater than 250 μm;

[0022] The distance between the air guide hole and the laser cutting path is between 250 μm and 600 μm.

[0023] In one embodiment, the step of "performing surface treatment on the mold" includes:

[0024] Grinding the surface of the base plate using a grinder; and

[0025] The mold surface is chrome plated.

[0026] In the technical solution of the present invention, a first groove is formed on the base plate, so that the residual gas and impurities generated by laser cutting are collected in the first groove, and are promptly sucked out through the air guide holes connected to the first groove, so that the heat on the laser cutting path is quickly conducted and the residual substances are effectively removed by suction. The adsorption holes running through the base plate can well fit the cutting material tightly on the mold, thereby improving the accuracy of the product cutting size; by arranging the first groove, air guide holes and adsorption holes on the base plate, the thermal effect of laser cutting is reduced, so that the picosecond laser cutting process can be downgraded, thereby reducing the manufacturing cost and improving the product accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying any creative work.

[0028] Figure 1 A schematic structural diagram of an embodiment of a laser cutting mold provided by the present invention;

[0029] Description of Figure Numbers:

[0030] 100. Laser cutting mold; 1. Bottom plate; 11. First groove; 12. Second groove; 2. Air guide hole; 3. Adsorption hole.

[0031] The purpose, features and advantages of the present invention will be further described with reference to the accompanying drawings and in conjunction with the embodiments. DETAILED DESCRIPTION

[0032] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making any creative efforts shall fall within the scope of protection of the present invention.

[0033] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture. If the specific posture changes, the directional indications will also change accordingly.

[0034] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present invention, the descriptions of "first", "second", etc. are only for descriptive purposes and cannot be understood as indicating or suggesting their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features limited to "first" and "second" may explicitly or implicitly include at least one of such features. In addition, if "and / or" or "and / or" appears in the full text, its meaning includes three parallel solutions. Taking "A and / or B" as an example, it includes solution A, solution B, or solutions that satisfy both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in this field to implement. When the combination of technical solutions is mutually contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0035] The present invention provides a laser cutting mold 100 .

[0036] It should be noted that yellowing refers to the situation in which local high temperatures during the laser cutting process cause thermal decomposition, oxidation reaction or chemical bond breakage of the material to be cut. When the laser cutting object is a circuit board (PCB) or other material with a conductive layer, the high temperature may cause the metal to melt or splash, especially at the position of the silver chloride reference electrode, which is more obvious, directly affecting the measurement accuracy of the test piece. In severe cases, it may cause the cut object to short-circuit and fail.

[0037] Furthermore, it is understood that during the laser cutting process, the laser beam interacts with the surface of the material being cut, generating high temperatures that cause the material to rapidly melt or evaporate, leading to yellowing and short circuits. During this process, the molten material and vapor diffuse with the airflow, forming residual gases and impurities. These gases and impurities may accumulate in the cutting area, affecting the cut quality and resulting in rough or unclear cut edges. The high temperatures and high pressures during cutting may also promote the generation of gases and solid particles, further exacerbating the generation of residues. For this reason, please refer to Figure 1 In one embodiment of the present invention, the laser cutting mold 100 includes a base plate 1, wherein the base plate 1 is formed with a first groove 11 along a first direction, and the base plate 1 is further provided with an air guide hole 2 and an adsorption hole 3; wherein the air guide hole 2 is connected with the first groove 11 to conduct heat and impurities generated by laser cutting, and the adsorption hole 3 is used to adsorb the material to be cut; by forming the first groove 11 in the first direction of the base plate 1, the residual gas and impurities generated during cutting are deposited in the first groove 11, the air guide hole 2 is connected with the first groove 11, and an air suction device is connected to the air guide hole 2 on the other side of the base plate 1 in the first direction, so that the residual gas and impurities are sucked out in time through the air guide hole 2, thereby eliminating the laser cutting. The heat on the path is quickly conducted and the residual materials are effectively removed by suction, thereby improving the cutting quality; in addition, the base plate 1 is also provided with adsorption holes 3, and the adsorption holes 3 are connected to the negative pressure device on the other side of the base plate 1 in the first direction to form negative pressure, thereby adsorbing the material to be cut during the cutting process, improving the stability during cutting, and thus improving the cutting quality; wherein, the first direction is the depth direction of the first groove 11; it can be understood that the negative pressure device can be a vacuum pump or a vacuum suction cup, and the present invention does not impose any restrictions on this, as long as the material to be cut can be stably adsorbed on the mold; the present invention does not impose any restrictions on the number of the adsorption holes 3. In order to further improve the stability, the number of the adsorption holes 3 can be adaptively increased.

[0038] In the technical solution of the present invention, a first groove 11 is formed on the base plate 1, so that the residual gas and impurities generated by laser cutting are collected in the first groove 11, and are promptly sucked out through the air guide hole 2 connected to the first groove 11, so that the heat on the laser cutting path is quickly conducted and the residual matter is effectively removed by suction. The adsorption holes 3 provided on the base plate 1 can well fit the material to be cut tightly on the mold, thereby improving the accuracy of the product cutting size; by arranging the first groove 11, the air guide hole 2 and the adsorption hole 3 on the base plate 1, the thermal effect of laser cutting is reduced, so that the picosecond laser cutting process can be downgraded, thereby reducing the manufacturing cost and improving the product accuracy.

[0039] It should be understood that the high temperature generated during the laser cutting process may cause the base plate 1 to soften or deform. In addition, the base plate 1 will repeatedly contact the material to be cut, causing severe wear. For this reason, in one embodiment of the present invention, the base plate 1 is made of steel, so that the base plate 1 has good high temperature resistance and thermal conductivity, so as to effectively dissipate the heat generated during the laser cutting process, reduce the heat accumulation effect, and thus avoid damage to the mold and the material to be cut. The hardness of the steel is 58-64HRC, so that the base plate 1 also has high hardness and wear resistance, increasing the accuracy and reliability during cutting; in this embodiment, the hardness of the base plate 1 is 62-63HRC, so as to better meet the processing requirements. The present invention does not limit the specific hardness of the steel, and can be adjusted according to the properties of the actual material to be cut.

[0040] In one embodiment of the present invention, the depth of the first groove 11 along the first direction is greater than 1 mm. This depth design prevents the laser from cutting the material to be cut into the metal mold and the residual gas and impurities from being promptly discharged through the mold suction, while reducing the heat accumulation effect.

[0041] It can be understood that when the bottom surface of the first groove 11 is flat, the residual gas is likely to form turbulence or dead corners inside the first groove 11, thereby affecting the discharge effect of the residue. Therefore, in one embodiment of the present invention, the depth of the first groove 11 in the first direction gradually deepens along the second direction. Through such a setting, the residual gas deposited in the first groove 11 flows in the direction of gradually deepening depth, thereby helping to improve the exhaust efficiency.

[0042] Specifically, the depth of the first groove 11 can be deepened by forming a multi-step bottom surface of the first groove 11, with the multi-step steps gradually deepening along the second direction. Each step is connected to an unconnected air guide hole 2, guiding airflow at different heights to flow outward layer by layer, ensuring that gas from different areas can be effectively sucked out during the cutting process. In another embodiment of the present invention, a multi-step annular airflow guide channel is designed around the laser cutting path to ensure that high-temperature gas can quickly flow out along the guide structure and prevent it from accumulating in the cutting area.

[0043] In one embodiment of the present invention, the bottom plate 1 is formed with a second groove 12 along the first direction, the second groove 12 is connected to the first groove 11, and the air guide hole 2 is connected to the first groove 11 through the second groove 12. By setting the second groove 12, the residual gas and impurities in the first groove 11 are discharged through the second groove 12, thereby guiding the flow direction of the residual gas and impurities, preventing them from gathering in the dead corner of the groove and causing a heat accumulation effect.

[0044] Specifically, in one embodiment of the present invention, the second groove 12 includes a plurality of second grooves 12, and the plurality of second grooves 12 are arranged at intervals around the first groove 11; the air guide holes 2 are provided in plurality, and the plurality of air guide holes 2 are respectively connected to the second grooves 12. By setting a plurality of second grooves 12 and the air guide holes, the specific distribution of the second grooves 12 can be optimized according to the residual gas and impurities generated during actual cutting, and more second grooves 12 are distributed in the part where more residual gas and impurities are generated. In addition, the present invention does not limit the shape of the air guide holes 2, which can be square, conical or bell-shaped, so as to reduce resistance when the air flow is discharged and improve exhaust efficiency.

[0045] In one embodiment of the present invention, a protrusion is provided on the bottom surface of the inner cavity of the first groove 11, the upper end surface of the protrusion is flush with the surface of the base plate 1, and the protrusion is spaced apart from the inner wall of the first groove 11. This design can accelerate the heat conduction of cutting and avoid the adsorption of cutting residues on the first groove 11. At the same time, it can provide support for the material to be cut during the cutting process, prevent it from being deformed and concave due to the heat effect during the cutting process, and ensure cutting accuracy.

[0046] The present invention further proposes a mold processing process, based on the above-mentioned laser cutting mold 100, the mold processing process includes the following steps:

[0047] S10 provides a base plate 1;

[0048] S20. Design the mold structure through software;

[0049] S30 by wire cutting to form air guide holes 2 and adsorption holes 3 on the bottom plate 1;

[0050] S40. A first groove 11 is machined on the bottom plate 1 by CNC numerical control, and the first groove 11 is connected to the air guide hole 2;

[0051] S50. Perform surface treatment on the bottom plate 1.

[0052] A locally recessed and partially perforated mold structure is designed on the laser cutting optical path, and then a precision mold is manufactured using wire cutting, CNC machining, CNC grinding, and coating processes. Picosecond laser combined with this mold technology can completely solve industry problems such as silver chloride yellowing, short circuit of upper and lower conductive electrodes, uneven cutting cross-section, and unstable dimensions caused by the laser processing of precision flexible multi-layer conductive printed CGM electrodes. This breakthrough in the leapfrog manufacturing technology of using low-level picosecond laser equipment to produce high-precision products has reduced manufacturing costs while improving product precision.

[0053] In one embodiment of the present invention, the step of “machining the first groove 11 on the bottom plate 1 by CNC numerical control, and making the first groove 11 communicate with the air guide hole 2” further includes:

[0054] S41. In the process of machining the first groove 11, a bump is formed on the bottom wall of the inner cavity of the first groove 11, wherein the distance between the bump and the laser cutting path is greater than 250 μm;

[0055] S42. The distance between the air guide hole 2 and the laser cutting path is between 250 μm and 600 μm.

[0056] The distance between the bump and the laser cutting path is greater than 250 μm, which can accelerate the heat conduction of the cutting section and prevent the adsorption of cutting residue on the cutting section. The distance between the air guide hole 2 and the laser cutting path is between 250 μm and 600 μm, which can quickly conduct heat on the laser cutting path and effectively remove residual materials through suction.

[0057] In addition, since laser cutting generates a large amount of heat energy, if the air guide hole 2 is too close to the cutting path, the mold surface may be subject to excessive heat accumulation, resulting in local overheating or damage to the material to be cut. By keeping the bump and the air guide hole 2 at a reasonable distance from the laser cutting path, the heat can be effectively dispersed, the mold can be prevented from overheating and damage, the cutting accuracy can be improved, and the mold life can be extended.

[0058] In one embodiment of the present invention, the step of “performing surface treatment on the mold” includes:

[0059] S51 using a grinder to grind the surface of the bottom plate 1; and,

[0060] S52. Chrome-plating the mold surface.

[0061] The surface of the base plate 1 is ground by a grinder to improve the flatness of the surface of the base plate 1, so that the material to be cut fits tightly with the base plate 1, which is more conducive to heat conduction and control of processing accuracy; and in order to further improve the wear resistance of the mold, the mold surface is chrome-plated so that it can withstand high-intensity, repetitive friction and impact, thereby extending the service life of the mold.

[0062] Furthermore, it is understood that molds may be exposed to corrosive substances such as moisture and chemicals in their working environment. Chrome plating forms a dense protective film that effectively prevents chemical reactions between the mold surface and external substances, preventing rust and corrosion, and further extending the life of the mold.

[0063] The above description is merely an exemplary embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformation made by utilizing the contents of the present invention's description and drawings under the technical concept of the present invention, or directly / indirectly applied in other related technical fields, is included in the patent protection scope of the present invention.

Claims

1. A laser cutting mold, characterized in that: include: A bottom plate, wherein the bottom plate is formed with a first groove along a first direction, and the bottom plate is also provided with at least one air guide hole and at least one adsorption hole; The air guide hole is connected to the first groove to conduct heat and cut impurities, and the adsorption hole is used to adsorb the material to be cut.

2. The mold according to claim 1, characterized in that The bottom plate is made of steel, and the hardness H of the steel satisfies: 58HRC <H<64HRC。 3. The laser cutting mold according to claim 1, characterized in that: The depth of the first groove along the first direction is greater than 1 mm.

4. The laser cutting mold according to claim 1, characterized in that: The depth of the first groove in the first direction gradually increases along the second direction.

5. The laser cutting mold according to claim 1, characterized in that: The bottom plate is formed with a second groove along the first direction, the second groove is communicated with the first groove, and the air guide hole is communicated with the first groove through the second groove.

6. The laser cutting mold according to claim 5, characterized in that: The second grooves include a plurality of grooves, and the plurality of second grooves are arranged around the first groove at intervals; There are a plurality of air guide holes, and the plurality of air guide holes are respectively connected to and correspond to the second grooves.

7. The laser cutting mold according to claim 1, characterized in that: A convex block is provided on the bottom surface of the inner cavity of the first groove, the upper end surface of the convex block is flush with the surface of the bottom plate, and the convex block is spaced apart from the inner peripheral wall of the first groove.

8. A mold processing process, based on the laser cutting mold according to claim 1, characterized in that: The following steps are involved: Providing a bottom plate; Design mold structure through software; Forming air guide holes and adsorption holes on the bottom plate by wire cutting; Processing a first groove on the bottom plate by CNC numerical control, and making the first groove communicate with the air guide hole; The bottom plate is subjected to surface treatment.

9. The mold processing process according to claim 8, characterized in that: The step of "machining a first groove on the bottom plate by CNC numerical control, and making the first groove communicate with the air guide hole" also includes: In the process of machining the first groove, a convex block is formed on the bottom wall of the inner cavity of the first groove, and the distance between the convex block and the laser cutting path is greater than 250 μm; The distance between the air guide hole and the laser cutting path is between 250 μm and 600 μm.