Process for preparing epoxypropane by oxidizing propylene with hydrogen peroxide
Through quantitative mixing of propylene, tert-butanol and hydrogen peroxide and epoxidation reaction of titanium silicon molecular sieve fixed bed reactor, the problem of difficulty in monitoring propylene oxide in the prior art is solved, and effective monitoring of propylene oxide and The stability of the conversion rate ensures the quality of the preparation process.
Patent Information
- Application Number
- CN202411125404.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure CN119039249A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of propylene oxide preparation, and in particular to a process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide. Background Art
[0002] Propylene oxide, also known as propylene oxide, methyl ethylene oxide, and 1,2-propylene oxide, is an organic compound and a very important raw material for organic compounds. It is the third largest propylene derivative after polypropylene and acrylonitrile. Propylene oxide is a colorless ether-smelling liquid with a low boiling point, flammable, and chiral. Industrial products are generally racemic mixtures of two enantiomers. It is partially miscible with water and miscible with ethanol and ether. It forms a binary azeotropic mixture with pentane, pentene, cyclopentane, cyclopentene, and dichloromethane. It is toxic and irritating to mucous membranes and skin, can damage the cornea and conjunctiva, cause respiratory pain, skin burns and swelling, and even tissue necrosis. Propylene oxide is mostly made by epoxidation of hydrogen peroxide and propylene oxide.
[0003] In the prior art, when hydrogen peroxide and propylene oxide are used to prepare propylene oxide, it is not convenient to monitor the prepared propylene oxide and the preparation conversion rate cannot be monitored. Therefore, we propose a process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide to solve the above problems. Summary of the invention
[0004] The purpose of the present invention is to solve the shortcomings of the prior art that when preparing propylene oxide from hydrogen peroxide and propylene oxide, it is inconvenient to monitor the prepared propylene oxide and the preparation conversion rate cannot be monitored, and a process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide is proposed.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide comprises the following steps:
[0007] S1. Weigh and quantify propylene, tert-butyl alcohol and hydrogen peroxide, and then calculate the total amount data, which is recorded as data A;
[0008] S2, fully mixing propylene, tert-butyl alcohol and hydrogen peroxide solution, and then performing epoxidation reaction in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product;
[0009] S3, conveying the crude propylene oxide product to a crude separation tower for crude separation of light components and heavy components;
[0010] S4, the light components separated from the coarse fractionation tower are compressed and enter the non-condensable gas separation tower, and then enter the recovery and reuse system;
[0011] S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product;
[0012] S6. Weigh and quantify the propylene oxide obtained in S5, and calculate the proportion of propylene oxide in data A;
[0013] S7. Perform data analysis on the percentage of propylene oxide obtained each time, and issue an early warning if the percentage data is abnormal.
[0014] Preferably, in S5, the roughly separated heavy components enter a propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product, and the heavy components separated in the propylene oxide separation tower enter a solvent recovery system to achieve solvent recovery.
[0015] Preferably, in S1, propylene, tert-butyl alcohol and hydrogen peroxide are weighed respectively by an electronic weighing device, and the weight data of propylene, tert-butyl alcohol and hydrogen peroxide are recorded respectively, and then the data of the three are added together to calculate the total amount data, which is counted as data A.
[0016] Preferably, in S2, a certain amount of propylene, tert-butanol and hydrogen peroxide solution are fully mixed, and the certain amount of propylene, tert-butanol and hydrogen peroxide added subsequently is ensured to be the same each time.
[0017] Preferably, in S2, propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, the mixing time is 20-30 min, the mixing speed is 200-300 r / min, and the mixing temperature is 20-30° C., and then an epoxidation reaction is carried out in a fixed bed reactor equipped with titanium silicalite to generate a crude propylene oxide product.
[0018] Preferably, in S7, data analysis is performed on the propylene oxide percentage obtained each time, and the obtained percentage data is compared with the preset percentage data. When the obtained percentage data is lower than the preset percentage data by more than 3-5%, an early warning is issued.
[0019] Preferably, in S2, the temperature of the epoxidation reaction is 45-115°C.
[0020] Preferably, in S3, propylene oxide is pumped into the coarse fractionation tower, and the delivery rate is monitored by a flow meter.
[0021] Preferably, in S5, the roughly separated heavy components enter the propylene oxide separation tower, the conveying speed of the heavy components is monitored, and propylene oxide is separated from the solvent and water to obtain a propylene oxide product.
[0022] Preferably, in S6, the propylene oxide obtained in S5 is weighed and quantified, and calculated as data B, and the proportion = data B / data A.
[0023] In the present invention, the beneficial effects of the process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide are as follows:
[0024] Propylene, tert-butyl alcohol and hydrogen peroxide are weighed and quantified, and then the total amount is calculated as data A; the obtained propylene oxide is weighed and quantified, and the proportion of propylene oxide in data A is calculated; the proportion of propylene oxide obtained each time is analyzed, and if the proportion data is abnormal, an early warning is issued;
[0025] The present invention quantifies the raw materials and then calculates the proportion of propylene oxide obtained each time. When an abnormality occurs, an early warning can be given in time to avoid the conversion rate being too low and affecting the processing quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 The present invention discloses a flow chart of a process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide. DETAILED DESCRIPTION
[0027] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0028] Embodiment 1
[0029] Reference Figure 1 A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide comprises the following steps:
[0030] S1. Weigh and quantify propylene, tert-butyl alcohol and hydrogen peroxide, and then calculate the total amount data, which is recorded as data A;
[0031] S2, fully mixing propylene, tert-butyl alcohol and hydrogen peroxide solution, and then performing epoxidation reaction in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product;
[0032] S3, conveying the crude propylene oxide product to a crude separation tower for crude separation of light components and heavy components;
[0033] S4, the light components separated from the coarse fractionation tower are compressed and enter the non-condensable gas separation tower, and then enter the recovery and reuse system;
[0034] S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product;
[0035] S6. Weigh and quantify the propylene oxide obtained in S5, and calculate the proportion of propylene oxide in data A;
[0036] S7. Perform data analysis on the percentage of propylene oxide obtained each time, and issue an early warning if the percentage data is abnormal.
[0037] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product, and the heavy components separated in the propylene oxide separation tower enter the solvent recovery system to achieve solvent recovery and utilization.
[0038] In this embodiment, in S1, propylene, tert-butyl alcohol and hydrogen peroxide are weighed respectively by an electronic weighing device, and the weight data of propylene, tert-butyl alcohol and hydrogen peroxide are recorded respectively. Then, the data of the three are added together to calculate the total amount data, which is counted as data A.
[0039] In this embodiment, in S2, a certain amount of propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, and this certain amount of data is the subsequent addition amount of propylene, tert-butyl alcohol and hydrogen peroxide, ensuring that the addition amount of propylene, tert-butyl alcohol and hydrogen peroxide is the same each time.
[0040] In this embodiment, in S2, propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, the mixing time is 20 minutes, the mixing speed is 200r / min, and the mixing temperature is 20°C, and then an epoxidation reaction is carried out in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product.
[0041] In this embodiment, in S7, data analysis is performed on the propylene oxide percentage obtained each time, and the obtained percentage data is compared with the preset percentage data. When the obtained percentage data is lower than the preset percentage data by more than 3%, an early warning is issued.
[0042] In this embodiment, in S2, the temperature of the epoxidation reaction is 45°C.
[0043] In this embodiment, in S3, propylene oxide is pumped into the coarse fractionation tower, and the delivery rate is monitored by a flow meter.
[0044] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower, the conveying speed of the heavy components is monitored, and propylene oxide is separated from the solvent and water to obtain a propylene oxide product.
[0045] In this embodiment, in S6, the propylene oxide obtained in S5 is weighed and quantified, which is calculated as data B, and the proportion = data B / data A.
[0046] Embodiment 2
[0047] A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide comprises the following steps:
[0048] S1. Weigh and quantify propylene, tert-butyl alcohol and hydrogen peroxide, and then calculate the total amount data, which is recorded as data A;
[0049] S2, fully mixing propylene, tert-butyl alcohol and hydrogen peroxide solution, and then performing epoxidation reaction in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product;
[0050] S3, conveying the crude propylene oxide product to a crude separation tower for crude separation of light components and heavy components;
[0051] S4, the light components separated from the coarse fractionation tower are compressed and enter the non-condensable gas separation tower, and then enter the recovery and reuse system;
[0052] S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product;
[0053] S6. Weigh and quantify the propylene oxide obtained in S5, and calculate the proportion of propylene oxide in data A;
[0054] S7. Perform data analysis on the percentage of propylene oxide obtained each time, and issue an early warning if the percentage data is abnormal.
[0055] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product, and the heavy components separated in the propylene oxide separation tower enter the solvent recovery system to achieve solvent recovery and utilization.
[0056] In this embodiment, in S1, propylene, tert-butyl alcohol and hydrogen peroxide are weighed respectively by an electronic weighing device, and the weight data of propylene, tert-butyl alcohol and hydrogen peroxide are recorded respectively. Then, the data of the three are added together to calculate the total amount data, which is counted as data A.
[0057] In this embodiment, in S2, a certain amount of propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, and this certain amount of data is the subsequent addition amount of propylene, tert-butyl alcohol and hydrogen peroxide, ensuring that the addition amount of propylene, tert-butyl alcohol and hydrogen peroxide is the same each time.
[0058] In this embodiment, in S2, propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, the mixing time is 25 minutes, the mixing speed is 250r / min, and the mixing temperature is 25°C, and then an epoxidation reaction is carried out in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product.
[0059] In this embodiment, in S7, data analysis is performed on the propylene oxide percentage obtained each time, and the obtained percentage data is compared with the preset percentage data. When the obtained percentage data is lower than the preset percentage data by more than 4%, an early warning is issued.
[0060] In this embodiment, in S2, the temperature of the epoxidation reaction is 70°C.
[0061] In this embodiment, in S3, propylene oxide is pumped into the coarse fractionation tower, and the delivery rate is monitored by a flow meter.
[0062] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower, the conveying speed of the heavy components is monitored, and propylene oxide is separated from the solvent and water to obtain a propylene oxide product.
[0063] In this embodiment, in S6, the propylene oxide obtained in S5 is weighed and quantified, which is calculated as data B, and the proportion = data B / data A.
[0064] Embodiment 3
[0065] A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide comprises the following steps:
[0066] S1. Weigh and quantify propylene, tert-butyl alcohol and hydrogen peroxide, and then calculate the total amount data, which is recorded as data A;
[0067] S2, fully mixing propylene, tert-butyl alcohol and hydrogen peroxide solution, and then performing epoxidation reaction in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product;
[0068] S3, conveying the crude propylene oxide product to a crude separation tower for crude separation of light components and heavy components;
[0069] S4, the light components separated from the coarse fractionation tower are compressed and enter the non-condensable gas separation tower, and then enter the recovery and reuse system;
[0070] S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product;
[0071] S6. Weigh and quantify the propylene oxide obtained in S5, and calculate the proportion of propylene oxide in data A;
[0072] S7. Perform data analysis on the percentage of propylene oxide obtained each time, and issue an early warning if the percentage data is abnormal.
[0073] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product, and the heavy components separated in the propylene oxide separation tower enter the solvent recovery system to achieve solvent recovery and utilization.
[0074] In this embodiment, in S1, propylene, tert-butyl alcohol and hydrogen peroxide are weighed respectively by an electronic weighing device, and the weight data of propylene, tert-butyl alcohol and hydrogen peroxide are recorded respectively. Then, the data of the three are added together to calculate the total amount data, which is counted as data A.
[0075] In this embodiment, in S2, a certain amount of propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, and this certain amount of data is the subsequent addition amount of propylene, tert-butyl alcohol and hydrogen peroxide, ensuring that the addition amount of propylene, tert-butyl alcohol and hydrogen peroxide is the same each time.
[0076] In this embodiment, in S2, propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, the mixing time is 30 minutes, the mixing speed is 300r / min, and the mixing temperature is 30°C, and then an epoxidation reaction is carried out in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product.
[0077] In this embodiment, in S7, data analysis is performed on the propylene oxide percentage obtained each time, and the obtained percentage data is compared with the preset percentage data. When the obtained percentage data is lower than the preset percentage data by more than 5%, an early warning is issued.
[0078] In this embodiment, in S2, the temperature of the epoxidation reaction is 115°C.
[0079] In this embodiment, in S3, propylene oxide is pumped into the coarse fractionation tower, and the delivery rate is monitored by a flow meter.
[0080] In this embodiment, in S5, the roughly separated heavy components enter the propylene oxide separation tower, the conveying speed of the heavy components is monitored, and propylene oxide is separated from the solvent and water to obtain a propylene oxide product.
[0081] In this embodiment, in S6, the propylene oxide obtained in S5 is weighed and quantified, which is calculated as data B, and the proportion = data B / data A.
[0082] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide, It is characterized in that The following steps are involved: S1. Weigh and quantify propylene, tert-butyl alcohol and hydrogen peroxide, and then calculate the total amount data, which is recorded as data A; S2, fully mixing propylene, tert-butyl alcohol and hydrogen peroxide solution, and then performing epoxidation reaction in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product; S3, conveying the crude propylene oxide product to a crude separation tower for crude separation of light components and heavy components; S4, the light components separated from the coarse fractionation tower are compressed and enter the non-condensable gas separation tower, and then enter the recovery and reuse system; S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product; S6. Weigh and quantify the propylene oxide obtained in S5, and calculate the proportion of propylene oxide in data A; S7. Perform data analysis on the percentage of propylene oxide obtained each time, and issue an early warning if the percentage data is abnormal.
2. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 1, It is characterized in that In S5, the roughly separated heavy components enter the propylene oxide separation tower to separate propylene oxide from the solvent and water to obtain a propylene oxide product. The heavy components separated in the propylene oxide separation tower enter the solvent recovery system to achieve solvent recovery.
3. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 2, It is characterized in that In S1, propylene, tert-butyl alcohol and hydrogen peroxide are weighed respectively by an electronic weighing device, and the weight data of propylene, tert-butyl alcohol and hydrogen peroxide are recorded respectively. Then, the data of the three are added together to calculate the total amount data, which is counted as data A.
4. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 3, It is characterized in that In S2, a certain amount of propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed. The certain amount of propylene, tert-butyl alcohol and hydrogen peroxide added subsequently is used to ensure that the amount of propylene, tert-butyl alcohol and hydrogen peroxide added each time is the same.
5. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 4, It is characterized in that In S2, propylene, tert-butyl alcohol and hydrogen peroxide solution are fully mixed, the mixing time is 20-30 minutes, the mixing speed is 200-300r / min, and the mixing temperature is 20-30°C, and then an epoxidation reaction is carried out in a fixed bed reactor equipped with titanium silicon molecular sieve to generate a crude propylene oxide product.
6. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 5, It is characterized in that In the above S7, data analysis is performed on the propylene oxide percentage obtained each time, and the obtained percentage data is compared with the preset percentage data. When the obtained percentage data is lower than the preset percentage data by more than 3-5%, an early warning is issued.
7. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 6, It is characterized in that In S2, the temperature of the epoxidation reaction is 45-115°C.
8. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 7, It is characterized in that In S3, propylene oxide is pumped into the coarse fractionation tower, and the delivery rate is monitored by a flow meter.
9. A process for preparing propylene oxide by oxidizing propylene with hydrogen peroxide according to claim 8, It is characterized in that In S5, the roughly separated heavy components enter the propylene oxide separation tower, the conveying speed of the heavy components is monitored, and propylene oxide is separated from the solvent and water to obtain a propylene oxide product.