Organosilicon supramolecular ion salt with hair care effect and preparation method thereof

By using the silicone supramolecular ion salt prepared by maleic acid and end aminosiloxane, the hair scales are filled and the disulfide bond is repaired, the problem of perm damage is solved, the hair is smooth and the strength is improved, and the production is environmentally friendly and simple. Better than existing products.

CN119039339AActive Publication Date: 2024-11-29JIANGNAN UNIV

Patent Information

Application Number
CN202411136932.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-29
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

Existing hair care products are difficult to effectively repair hair damage caused by perm, and have environmental problems and production complexity, so they cannot stay on the hair for a long time and cannot repair severely damaged hair.

Method used

Silicone supramolecular ion salt is prepared by mixing maleic acid with end aminosiloxane. The siloxane structure is used to fill the hair scales and repair the disulfide bonds to form a protective film to improve hair flexibility and strength.

Benefits of technology

It significantly reduces the friction coefficient and dry combing function of the hair, repairs damage and hair loss, improves hair flexibility and damage resistance, is better than existing compounds, and the production process is environmentally friendly and simple.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119039339A_ABST
    Figure CN119039339A_ABST
Patent Text Reader

Abstract

The invention discloses an organic silicon supramolecular ion salt with a hair care effect and a preparation method thereof, and belongs to the technical field of supramolecules. According to the organic silicon supramolecular ion salt, a siloxane chain is used as a central framework to be connected with a diene bond structure, a siloxane structure is introduced while the hair repairing capacity is provided for a product, the product can repair hair fundamentally, meanwhile, a siloxane protection film can be formed on the surface of the hair, and the hair repairing effect is improved. The treated hair is softer, and further damage can be prevented. The organic silicon supramolecular ionic salt belongs to supramolecular ionic salt, and a completely hydrophobic siloxane chain is treated to be water-soluble, so that the design of a formula is more convenient; in addition, no extra solvent is added or water is directly used as the solvent in the production process, the reaction rate and the yield are high, and the method can be directly applied to the formula design of the product end from the product end.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an organosilicon supramolecular ion salt with hair care effect and a preparation method thereof, belonging to the technical field of supramolecular. Background Art

[0002] Nowadays, people have an increasing demand for hair care, and the frequency of hair washing, perming, dyeing and styling is high; and environmental stress can easily cause hair damage. These factors often lead to problems such as dry and frizzy hair, decreased smoothness, damaged hair quality, and easy breakage.

[0003] The destructiveness of perming is well known, and involves the breaking and reforming of disulfide bonds in the hair. The general perming process is divided into two steps. In the first step, a reducing agent (such as thioglycolate and bisulfite) is used to cleave the disulfide bonds into free sulfhydryl groups. Sometimes, for the efficiency of perming, a strong oxidant such as hydrogen peroxide is added in the second oxidation step, which will aggravate the damage to the hair surface and reduce the strength of the hair fiber.

[0004] Studies have shown that prolonged exposure to reducing or oxidizing agents during the perming process reduces the content of α-helical proteins in hair, which can be observed in the wide-angle X-ray diffraction (WAXD) pattern, that is, the intensity of the signal associated with accumulation is reduced at the level of individual keratin fibers.

[0005] The perming process will transform the hydrophobic hair surface into a more hydrophilic surface, so the lipid loss of the hair cuticle will be aggravated in the interaction with shampoo. Keratin, disulfide bonds and lipid content are closely related to the tensile properties of hair, so perming can easily affect the tensile properties of hair.

[0006] At present, polysiloxane with a silicon-oxygen-silicon structure is also commonly used in hair care products. Although the silicon-oxygen-silicon structure cannot directly repair the hair structure, it can form a protective film on the surface of the hair, effectively reducing external damage and reducing water loss in the hair. At the same time, it can fill the hair scales, improve hair frizziness, and reduce breakage and damage caused by combing. However, even if the polysiloxane structure has only two silicon atoms, it is a strongly hydrophobic structure. When applied to the formula, it needs to be processed into an emulsion system, which increases the cost of use and is difficult to stay on the hair for a long time. In addition, the hair care principle of polysiloxane is to reduce the damage to the hair, and it cannot repair the hair that has been severely damaged.

[0007] Patent CN102525845B discloses the use of organopolysiloxane and maleic anhydride to prepare hair care cosmetics, wherein maleic anhydride is connected to the side chain of organopolysiloxane by grafting reaction, and the prepared hair care cosmetics are covalent compounds bonded by covalent bonds, and the hair care effect is specifically a softening effect. The above technology needs to use organic solvents in the actual production process, which is not environmentally friendly. At the same time, there is a problem of reaction rate in the amidation reaction, and the product purification process is relatively complicated. The existing compound bisaminopropyl diglycol dimaleate discloses the function of repairing disulfide bonds in hair through a double olefin bond structure C=C, but the compound structure is a carbon chain polyether structure, which can improve the water solubility of the compound, but can only provide smoothness to the hair by repairing the hair. At the same time, the compound is in liquid state and is subject to certain restrictions during storage and transportation.

[0008] Therefore, it is of great practical and economic value to prepare a supramolecular compound which has good hair repairing effect, can make hair smooth, and is easy to store and transport. Summary of the invention

[0009] In view of the shortcomings of the prior art, the present invention uses maleic acid and amino-terminated siloxane to mix and prepare an organosilicon supramolecular ion salt. The organosilicon supramolecular ion salt provided by the present invention has the functions of hair repair and softening, and can also fill damaged hair scales in the hair.

[0010] The first object of the present invention is to provide an organosilicon supramolecular ion salt, the structural formula of which is as follows:

[0011]

[0012] Among them, the structural formula of A is as follows:

[0013]

[0014] n is an integer greater than or equal to 1.

[0015] Preferably, n is an integer of 1 to 5; more preferably, n is 1.

[0016] The second object of the present invention is to provide a method for preparing the above-mentioned organosilicon supramolecular ion salt, comprising the following steps:

[0017] Maleic acid is mixed with amino-terminated siloxane to prepare an organosilicon supramolecular ion salt.

[0018] In one embodiment, the method for preparing an organosilicon supramolecular ionic salt comprises:

[0019] Dissolving maleic acid in a solvent and mixing it with amino-terminated siloxane to obtain an organosilicon supramolecular ion salt;

[0020] or,

[0021] The maleic acid is ground, mixed with amino-terminated siloxane, and further ground to obtain an organosilicon supramolecular ionic salt.

[0022] In one embodiment, the amino-terminated siloxane structure is as follows:

[0023]

[0024] n is an integer greater than or equal to 1.

[0025] In one embodiment, the amino-terminated silicone comprises one or both of 1,3-bis(3-aminopropyl)-1,1,3,3-tetramethyldisiloxane (CAS No.: 2469-55-8, n=1) or amino-terminated polydimethylsiloxane (CAS: 97917-34-5, n≥2) or aminosilicone water-soluble emulsion system (product model: Silsoft AM 1021N LV PMF emulsion).

[0026] In one embodiment, after the organosilicon supramolecular ion salt is prepared, it can be washed with ethyl acetate and dried to obtain a high-purity organosilicon supramolecular ion salt.

[0027] In one embodiment, the solvent includes but is not limited to water, methanol, ethanol, n-propanol, isopropanol, ethylene glycol, propylene glycol and other solvents that can dissolve maleic acid, but does not include carboxyl-containing or highly acidic solvents.

[0028] Preferably, the solvent is deionized water, methanol, ethanol or other solvents with a low boiling point.

[0029] In one embodiment, the molar ratio of maleic acid to amino groups in amino-terminated siloxane is 1:0.8-1.3.

[0030] Preferably, the molar ratio of maleic acid to the amino group in the amino-terminated siloxane is 1:1 to 1.1.

[0031] In one embodiment, the mass ratio of maleic acid to solvent is 1 to 2:4.

[0032] In one embodiment, the system temperature during the preparation process is 25-40°C.

[0033] In one embodiment, the grinding is performed at room temperature for 0.1 to 1 hour until the system becomes a white uniform solid.

[0034] In one embodiment, the method of preparing the organosilicon supramolecular ionic salt comprises the following steps:

[0035] (1) mixing maleic acid and deionized water in a mass ratio of 1-2:2-6, stirring at room temperature for 5-30 minutes until the maleic acid is completely dissolved, thereby preparing a maleic acid aqueous solution;

[0036] (2) weighing an amino double-capped head (the molar ratio of the amino double-capped head to maleic acid is 1:1-5), slowly dropping the amino double-capped head into the aqueous maleic acid solution under stirring conditions, and continuing to stir the reaction for 1-3 hours after the dropwise addition is completed;

[0037] (3) After the reaction is completed, the solvent water in the system is volatilized, washed with ethyl acetate, filtered, and dried to obtain an organosilicon supramolecular ion salt (i.e., amino double-capped maleate).

[0038] In one embodiment, the method of preparing the organosilicon supramolecular ionic salt comprises the following steps:

[0039] Grind the maleic acid and add the amino double head (the molar ratio of the amino double head to maleic acid is 1:1-5); continue grinding until there is no obvious wet part, continue to drip the amino double head until the amino double head is completely added, continue grinding for 10-30 minutes until the system becomes fine and dry, add ethyl acetate for washing, filter, and dry to obtain the organosilicon supramolecular ion salt (i.e., amino double head maleate).

[0040] The third object of the present invention is to provide the use of the above-mentioned organosilicon supramolecular ion salt in the preparation of daily chemical products and medicines.

[0041] In one embodiment, the daily chemical products include: hair care cosmetics and detergents.

[0042] In one embodiment, the hair care cosmetics include: hair conditioner, hair oil, hair milk, hair wax, hair lotion, after-wash sunscreen lotion, steam-free hair milk, sunscreen shampoo, medicinal hair milk, conditioning shampoo, shampoo, and aftershave.

[0043] The fourth object of the present invention is to provide a product, which contains the organosilicon supramolecular ion salt according to claim 1; the product is a daily chemical product or a medicine.

[0044] In one embodiment, the hair care cosmetics include: hair conditioner, hair oil, hair milk, hair wax, hair lotion, after-wash sunscreen lotion, steam-free hair milk, sunscreen shampoo, medicinal hair milk, conditioning shampoo, shampoo, and aftershave.

[0045] A fifth object of the present invention is to provide a hair care product comprising the organosilicon supramolecular ion salt according to claim 1.

[0046] In one embodiment, the amount of the organosilicon supramolecular ion salt added is 0.01 to 20% w / w;

[0047] Preferably, the addition amount of the organosilicon supramolecular ion salt is 0.01 to 15% w / w.

[0048] In one embodiment, the organosilicon supramolecular ionic salt can be added to commercially available hair care products without dispersibility issues.

[0049] In one embodiment, the above-mentioned organosilicon supramolecular ion salt is used as an effective ingredient to prepare a hair care product, the components of which include: sodium dodecyl sulfate (SDS), cocamidopropyl betaine, an effective ingredient, citric acid and water;

[0050] The preparation method comprises: mixing SDS and water, adding cocamidopropyl betaine and functional ingredients, mixing evenly, and adjusting the pH value to be close to the natural pH value of the scalp with citric acid to obtain a hair care product.

[0051] In one embodiment, the content of sodium lauryl sulfate is 0.05-1% w / w, the content of cocamidopropyl betaine is 0.01-1% w / w, the content of the functional ingredient is 0.01-1% w / w, the content of citric acid is 0.1-0.5% w / w, and water is supplemented to 100%.

[0052] Beneficial effects of the present invention

[0053] The present invention uses maleic acid and 1,3-bis(3-aminopropyl)-1,1,3,3-tetramethyldisiloxane (amino double-capped) to prepare an organosilicon supramolecular ion salt. The organosilicon supramolecular ion salt provided by the present invention can repair the disulfide bonds in the hair from the structural point of view, and the siloxane structure can fill the damaged hair scales in the hair to achieve the purpose of repairing the hair and making the hair smooth.

[0054] (1) Structurally, the organosilicon supramolecular ion salt (amino dicapped maleate) of the present invention uses a siloxane chain as a central skeleton to connect a diene bond structure, which not only provides the product with the ability to repair hair, but also introduces a siloxane structure, so that the product can fundamentally repair hair, and at the same time can form a siloxane protective film on the surface of the hair, making the treated hair more supple and preventing further damage;

[0055] Specifically, the organosilicon supramolecular ion salt of the present invention reduces the static friction coefficient and dynamic friction coefficient of hair by 25.49% and 29.20% respectively, and reduces the dry combing work by 11.7%; the repair and softening effects on damaged hair are significantly better than the existing compound (bisaminopropyl diglycol dimaleate).

[0056] (2) In terms of properties, the organosilicon supramolecular ionic salt (amino dicapped maleate) of the present invention is a supramolecular ionic salt, which processes the completely hydrophobic siloxane chain into water-soluble, making it more convenient to design the formula; and the production process does not require the addition of additional solvents or directly uses water as a solvent, the reaction rate and yield are both high, and can be directly applied from the product end to the product end formula design. BRIEF DESCRIPTION OF THE DRAWINGS

[0057] Figure 1 This is the Fourier transform infrared spectrum of the organosilicon supramolecular ion salt prepared in Example 1.

[0058] Figure 2 This is the hydrogen NMR spectrum of the organosilicon supramolecular ion salt prepared in Example 1.

[0059] Figure 3 This is the Fourier transform infrared spectrum of the organosilicon supramolecular ion salt prepared in Example 2.

[0060] Figure 4 This is the hydrogen NMR spectrum of the organosilicon supramolecular ion salt prepared in Example 2.

[0061] Figure 5 These are photos of original hair (a), hair reduced with thioglycolic acid (b), and hair treated with repair solution A (c) in Example 3, taken under a fluorescence microscope.

[0062] Figure 6 The SEM images are of the original hair (a) in Example 3, the hair reduced with thioglycolic acid (b), the hair treated with repair solution E in Comparative Example 4 (c), and the hair treated with repair solution A (d).

[0063] Figure 7 The products obtained in Comparative Example 1, Comparative Example 2 and Comparative Example 4 were used to prepare repair solutions C, D and E, and the hair was treated with the repair solutions C, D and E respectively, and photos of the treated hair under a fluorescence microscope were obtained. DETAILED DESCRIPTION

[0064] The preferred embodiments of the present invention are described below. It should be understood that the embodiments are for better explanation of the present invention and are not intended to limit the present invention. The technical scheme of the present invention is further described below by specific examples. It should be understood that the implementation of the present invention is not limited to the following examples, and any formal modifications and / or changes made to the present invention will fall within the scope of protection of the present invention. In the present invention, unless otherwise specified, all parts and percentages are weight units, and the equipment and raw materials used can be purchased from the market or are commonly used in the art. The methods in the following embodiments, unless otherwise specified, are conventional methods in the art.

[0065] The raw materials used in the examples are:

[0066] 1,3-bis(3-aminopropyl)-1,1,3,3-tetramethyldisiloxane (referred to as amino dicapped in the subsequent examples; wherein n=1 in the siloxane chain) was purchased from Shanghai Haohong Biopharmaceutical Technology Co., Ltd.; CAS number: 2469-55-8;

[0067] Aminopropyl-terminated polydimethylsiloxane was purchased from Huangshan Qiangli Chemical Co., Ltd.; CAS number: 99904-16-2;

[0068] Bisaminopropyl diglycol dimaleate was purchased from Jining Tangyi Chemical Co., Ltd., CAS No.: 1629579-82-3;

[0069] Silsoft AM 1021N LV PMF emulsion (hereinafter referred to as aminosilicone water-soluble emulsion system 1201) was purchased from Guangzhou Best Chemical Co., Ltd.

[0070] The original hair mentioned in the embodiment is: dyed damaged straight hair (22.5cmx5.5cmx7g, free19.5cm), purchased from Shanghai Canyu Trading Co., Ltd.

[0071] The reduced hair mentioned in the embodiment is obtained by soaking the purchased hair in an aqueous solution of thioglycolic acid with a mass fraction of 8% and a pH value of 8.5, and shaking it at 50° C. for 30 minutes.

[0072] The repaired hair mentioned in the examples is a hair sample obtained by immersing the restored hair in the repair solution prepared in the corresponding examples and shaking at 50° C. for 30 minutes. The real human hair piece mentioned in the examples is a real healthy hair piece (25 cm×2.5 cm×3 g, free 22.5 cm) purchased from Shanghai Canyu Trading Co., Ltd.

[0073] The aminopolysiloxane water-soluble system mentioned in the embodiments is: various aminopolysiloxane water-soluble systems commonly available in the market, such as aminosilicone water-soluble emulsion system 1201.

[0074] Test method:

[0075] 1. Infrared test:

[0076] Liquid sample test: Take 20-30 mg of sample, dilute with 3-5 mL of dichloromethane, drop about 0.2 mL of the diluted solution on the potassium bromide window that has been cleaned and dried with anhydrous ethanol in advance, and bake with an infrared lamp until the sample forms a thin film on the window. Place the window in a Nicolet iS5 Fourier infrared spectrometer for testing to obtain the results.

[0077] Solid sample test: Take a solid sample and potassium bromide crystals in a mass ratio of 2:98, mix them evenly with a mortar and grind them into a solid system with finer particles, bake them dry with an infrared lamp, and then press them into tablets with a tablet press. Then place them in a Nicoleti S5 Fourier infrared spectrometer for testing to obtain the results.

[0078] 2. MRI test:

[0079] Deuterated chloroform was used as a deuterated reagent for double-capped amino groups, and deuterated DMSO was used as a deuterated reagent for maleic acid. 5 to 10 mg of the sample was dissolved in a nuclear magnetic resonance tube, respectively, and the results were obtained by testing with an AVANCEⅢHD 400MHz nuclear magnetic resonance spectrometer.

[0080] 3. Repair effect test:

[0081] When hair is damaged, the disulfide bonds in the hair keratin will be cut, resulting in loss of elasticity and luster, becoming dry and brittle, etc. The cleavage of the disulfide bonds will produce two free thiol groups, so measuring the thiol content in damaged hair can more intuitively determine the degree of hair damage.

[0082] Rhodamine B (RB) is one of the most commonly used fluorescent dyes. 3- ) can react with RB to quench its fluorescence and weaken its fluorescence intensity, while the thiol group can 3- Restore to I - , thereby enhancing the fluorescence intensity. Through the fluorescence interaction between iodine solution and rhodamine B, the residual thiol groups in the hair can be reduced to I 3- , and then observe the fluorescence intensity of the hair under a fluorescence microscope. If the repair goes smoothly, the fluorescence intensity on the repaired hair should be much smaller than the fluorescence intensity of the damaged hair, thereby visualizing the repair effect of the thiol group.

[0083] Pre-configuration 10 -3 mol / L iodine standard solution, 10 -4 mol / L rhodamine B solution and acetic acid-sodium acetate buffer were kept aside.

[0084] In this experiment, the hair was placed in a reducing agent, thioglycolic acid, and shaken in a constant temperature shaking incubator for 3 hours, taken out, dried, and stored in nitrogen to obtain the reduced hair. An appropriate amount of the reduced hair was cut, and different repair solutions (prepared in the examples or comparative examples) were used to incubate and repair for 20 minutes, and then taken out and dried in a nitrogen atmosphere to obtain the repaired hair.

[0085] Several repaired hairs were taken from each group and placed in 2 mL of iodine standard solution, vortexed for 5 minutes, and then 3 mL of rhodamine B solution and 5 mL of acetic acid-sodium acetate buffer were added. After standing for 10 minutes, the hairs were taken out and soaked in deionized water. After vortexing for 5 minutes, the hairs were taken out and rinsed several times with deionized water to wash away the residual rhodamine B. After drying, the hairs were observed under a fluorescence microscope at 360 nm.

[0086] 4. Friction coefficient test

[0087] The experiment was conducted at a temperature of (25±2)°C and a humidity of (50±5)%. Each group of hair was immersed in different repair solutions (prepared in the examples or comparative examples) for 30 seconds, and then placed in a constant temperature and humidity environment for 4 hours to dry naturally. The friction coefficient of each group of hair was tested using a fiber friction coefficient tester, and the dynamic friction coefficient and static friction coefficient of each group of hair before and after using the repair solution were compared. Each group measured 15 sets of relatively concentrated data and took the average value.

[0088] 5. Dry combing test

[0089] The experiment was conducted at a temperature of (25+2)℃ and a RH of (50+5)%. A 40cm long, 25g human hair piece was selected and fully moistened with 40℃ warm water. 5mL of 10% SDS aqueous solution was taken with a dropper and evenly applied to the front and back of the hair piece and rubbed to produce foam. When rubbing, avoid folding the hair bundle in half or twisting it together to prevent the hair from tangling. Then rinse off the foam with warm water. Repeat the above operation twice and place it in a constant temperature and humidity environment to dry naturally.

[0090] Prepare 10g of different repair liquids (prepared in the examples or comparative examples) with a mass fraction of 1%, spray them evenly on each hair bundle, and use a comb to perform simple combing. After the hair bundles are naturally dried at a constant temperature, use a combing instrument to test the dry combing work of each hair bundle. Each group uses 2 hair pieces of the same specification for testing, and the test is repeated seven times. The combing curve is obtained by data processing, and the dry combing work can be obtained by integrating the combing curve.

[0091] 6. Scanning electron microscope (SEM) test

[0092] The treated and dried hair was cut into small sections of about 0.3 cm, fixed on an electron microscope table with conductive glue, and the hair morphology was observed using a Hitachi S-4800 field emission scanning electron microscope.

[0093] The room temperature mentioned in the present invention is 15-30° C.; the stirring is 300-500 rpm for 5-10 minutes; within the above range, parameter changes will not affect product synthesis.

[0094] Example 1: Preparation of organosilicon supramolecular ion salt by solvent method

[0095] An organosilicon supramolecular ion salt, the structure of which is as follows:

[0096]

[0097] in,

[0098] n=1.

[0099] The preparation method of the above-mentioned organosilicon supramolecular ion salt is as follows:

[0100] 18.7 g of maleic acid and 40 g of deionized water were mixed in a reaction bottle equipped with a stirring device, and stirred at room temperature for 10 min. After the maleic acid was completely dissolved, a maleic acid aqueous solution was prepared;

[0101] Accurately weigh 20g of amino double head (the molar ratio of amino double head to maleic acid is 1:2), slowly drop the amino double head into the maleic acid aqueous solution (about one drop of liquid per second) under stirring conditions, keep the system temperature at room temperature, and continue stirring for 2h after the addition is completed; after the reaction is completed, evaporate the solvent water in the system, wash with ethyl acetate, filter, and dry to obtain 38.7g of organosilicon supramolecular ion salt (i.e., amino double head maleate).

[0102] The amino double-capped maleate prepared in Example 1 was subjected to structural analysis, and the test results are as follows:

[0103] Infrared spectrum Figure 1 As shown. Figure 1 It can be seen that the amino double-capped maleate and maleic acid prepared in Example 1 have a -1 The characteristic peaks of silicon-oxygen-silicon appeared at the position, which proved that the siloxane structure was successfully introduced into the product.

[0104] Comparison of the amino double-capped maleate and amino double-capped maleate prepared in Example 1 shows that 3350cm -1 The double peaks attributable to the amino group disappeared and turned into a strong and broad peak. This is because the carboxyl peak introduced in the maleic acid structure covered the original amino peak. At the same time, the product peak at 2100cm -1 A broad peak appeared at , which indicated the presence of protonated amino groups, so the reaction process achieved the process of proton transfer.

[0105] NMR spectra Figure 2 As shown, specifically:

[0106] NMR data of amino double-capped maleate: 1H NMR (400MHz, d-DMSO) δ7.65(s,6H),6.03(m,4H),2.77(t,4H),1.534(m,4H),0.52(m,4H),0.067(s,12H).

[0107] Amino double head NMR data: 1 H NMR (400MHz, CDCl3) δ2.653(t,4H),1.395~1.482(m,8H),0.493(m,4H),0.041(s,12H).

[0108] In the amino double-capped maleate 1 In the H-NMR spectrum, the characteristic peak of protonated amino group appears at e (δ=7.8ppm), and the integral area is 6. At the same time, the integral area of ​​c (δ=1.5ppm) is reduced by 4 compared with g (δ=1.5ppm), which indicates that the two terminal amino groups of the amino double-capped head have successfully become protonated amino groups through the process of proton transfer. The peaks at a (δ=0.1ppm) are the characteristic peaks of Si-CH3, and the three peaks at b (δ=0.5ppm), c (δ=1.5ppm), and d (δ=2.75ppm) are the characteristic peaks of methylene in the amino double-capped head. The integral areas of these four characteristic peaks remain unchanged before and after the reaction, which indicates that the structure of the amino double-capped head is retained. The peak at f (δ=6ppm) is the characteristic peak of -CH=CH-, and the integral area is 4, which indicates that there are two maleic acid structures in the product structure. It can be seen that the amino dicapped group and maleic acid undergo proton transfer to form amino dicapped maleate, and at the same time, the amino groups at both ends of the amino dicapped group exchange protons with one maleic acid each to form a molecule with a diene bond structure.

[0109] The above structural analysis shows that Example 1 successfully carried out the proton exchange reaction between the amino double-capped group and maleic acid, and successfully synthesized the organosilicon supramolecular ion salt containing a diene bond structure.

[0110] Example 2: Preparation of organosilicon supramolecular ionic salt by grinding method

[0111] An organosilicon supramolecular ion salt, the structure of which is as follows:

[0112]

[0113] in,

[0114] n=1.

[0115] The preparation method of organosilicon supramolecular ion salt is as follows:

[0116] Put 18.7g of maleic acid into a mortar and grind it with the mortar; accurately weigh 20g of amino double head, slowly drip it into the mortar (about one drop of liquid per second) at room temperature, and continue grinding. When there is no obvious wet part in the system, continue to drip the amino double head until the amino double head is completely added, and continue grinding for 10 minutes until the system becomes fine and dry. Add ethyl acetate to wash, filter, and dry to obtain 38.7g of organosilicon supramolecular ion salt (i.e., amino double head maleate).

[0117] The structure analysis of the organosilicon supramolecular ion salt obtained in Example 2 was performed, and the results were as follows:

[0118] Infrared spectrum Figure 3 As shown. Figure 3 It can be seen that the amino double-capped maleate and maleic acid prepared in Example 2 have a -1 The characteristic peak of silicon-oxygen-silicon appeared at 3350cm -1 The double peaks attributable to the amino group disappeared and turned into a strong and broad peak. This is because the carboxyl peak introduced in the maleic acid structure covered the original amino peak. At the same time, the product peak at 2100cm -1 A broad peak appeared at , which indicated the presence of protonated amino groups, so the reaction process achieved the process of proton transfer.

[0119] NMR spectra Figure 4 As shown, specifically:

[0120] NMR data of amino double-capped maleate:

[0121] 1 H NMR (400MHz, d-DMSO) δ7.65(s,6H),6.03(m,4H),2.77(t,4H),1.534(m,4H),0.52(m,4H),0.067(s,12H).

[0122] Amino double head NMR data

[0123] 1 H NMR (400MHz, CDCl3) δ2.653(t,4H),1.395~1.482(m,8H),0.493(m,4H),0.041(s,12H).

[0124] In the 1H-NMR spectrum of amino dicapped maleate, the characteristic peak of protonated amino group appears at e (δ=7.8ppm), and the integral area is 6. At the same time, the integral area of ​​c (δ=1.5ppm) is reduced by 4 compared with g (δ=1.5ppm), which indicates that the two terminal amino groups of amino dicapped maleate have successfully become protonated amino groups through the process of proton transfer. The peaks at a (δ=0.1ppm) are the characteristic peaks of Si-CH3, and the three peaks at b (δ=0.5ppm), c (δ=1.5ppm), and d (δ=2.75ppm) are the characteristic peaks of methylene in amino dicapped maleate, respectively. The integral areas of these four characteristic peaks remain unchanged before and after the reaction, which indicates that the structure of amino dicapped maleate is retained. The peak at f (δ=6ppm) is the characteristic peak of -CH=CH-, and the integral area is 4, which indicates that there are two maleic acid structures in the product structure. It can be seen that the amino dicapped group and maleic acid undergo proton transfer to form amino dicapped maleate, and at the same time, the amino groups at both ends of the amino dicapped group exchange protons with one maleic acid each to form a molecule with a diene bond structure.

[0125] The above structural analysis shows that the proton exchange reaction between the amino double capping and maleic acid was successfully carried out, and the organosilicon supramolecular ion salt containing a diene bond structure was successfully synthesized. From the data of nuclear magnetic resonance, the organosilicon supramolecular ion salt prepared in Example 2 and Example 1 is the same, and the only difference between the two is the preparation method.

[0126] Example 3: Performance testing of organosilicon supramolecular ion salt

[0127] The repair effect and friction coefficient of the organosilicon supramolecular ionic salt (amino double-capped maleate) prepared in Example 1 (the organosilicon supramolecular ionic salts prepared in Example 2 and Example 1 are the same substance, and Example 1 is used as an example when testing the performance) on damaged hair were tested.

[0128] 1. Hair repair

[0129] The organosilicon supramolecular ion salt (amino dicapped maleate) prepared in Example 1 and water were mixed in a mass ratio of 1:99, stirred at 20°C and 500 rpm for 3 min, and after fully dissolved, the pH was adjusted to 8 with 1M NaOH solution to obtain a repair solution A (subsequently used for hair restoration).

[0130] Thioglycolic acid and deionized water were prepared into a thioglycolic acid solution with a mass fraction of 8%, and the pH was adjusted to 8.5 with 1M NaOH solution to obtain reducing agent A (used to cut the disulfide bonds in the original hair to form free thiol groups to simulate damaged hair).

[0131] Cut an appropriate amount of original hair (untreated damaged hair), soak it in reducing agent A, reduce it at 50°C for 30 minutes, take it out and dry it to obtain reduced hair.

[0132] Cut about 20 restored hairs of about 2 cm in length, soak them in repair solution A, treat them at 50°C for 20 minutes, take them out and dry them to obtain repaired hair, and test the repair effect.

[0133] The results of fluorescence detection of hair are as follows Figure 5 As shown, the results show that the untreated damaged hair (a) has strong fluorescence under a fluorescence microscope, and the gaps in the hair scales can be clearly seen, which means that the hair scales of the damaged hair will open, exposing the thiol-containing keratin structure inside the hair.

[0134] The fluorescence of the reduced hair (b) treated with thioglycolic acid is also strong. At the same time, the gaps between the hair scales are enlarged, and large fluorescent spots appear on the hair surface where the hair scales have peeled off. This indicates that treating the hair with thioglycolic acid will break the disulfide bonds in the hair, causing the hair scales to open or even break, and increase the content of free thiol groups.

[0135] However, the fluorescence of the hair (c) treated with silicone supramolecular ion salt (amino dicapped maleate) was significantly reduced, and the gaps in the hair scales on the surface were basically unobservable. This indicates that after the hair is treated with the product, the free thiol groups on the hair surface are reduced, and the damaged or opened hair scales are filled, making the hair surface smoother.

[0136] Scanning electron microscopy results of hair Figure 6 As shown, the results show that the surface of untreated damaged hair (a) is relatively rough, with more damaged sites, and it can be seen from the figure that the hair scales tend to lift and peel off. The surface of the reduced hair (b) treated with thioglycolic acid is even rougher, with more damaged sites, and the hair scales are more obviously lifted and peeled off, and some hair scales have been damaged and peeled off. The surface of the reduced hair (d) treated with the product can obviously be seen to have a reduced degree of damage, fewer damaged sites, and a smoother hair scale with a reduced tendency to lift. This shows that from a macroscopic point of view, the degree of damage to the hair is reduced after the product treatment.

[0137] 2. Dynamic and static friction coefficient

[0138] The organosilicon supramolecular ion salt obtained in Example 1 and water were mixed in a mass ratio of 1:99, stirred at 20° C. and 500 rpm for 3 min, and after being fully dissolved, the pH was adjusted to 8 with a 1 M NaOH solution to obtain a repair solution A;

[0139] Thioglycolic acid and deionized water were prepared into a thioglycolic acid solution with a mass fraction of 8%, and the pH was adjusted to 8.5 with a 1M NaOH solution to obtain a reducing agent A (which was subsequently used to treat hair as it was to obtain reduced hair).

[0140] 90 hairs of 5 cm to 7 cm in length were cut and divided into three groups.

[0141] Group 1: No treatment was performed on the hair, leaving it as is.

[0142] Group 2: Soaked in reducing agent A, reduced at 50°C for 30 minutes, taken out and dried to obtain reduced hair.

[0143] Group 3: Soak in reducing agent A, reduce at 50℃ for 30min, take out and dry, then soak in repairing solution A, treat at 50℃ for 20min, take out and dry to obtain repaired hair.

[0144] The friction coefficient results are shown in Table 1. The results show that after the original hair was restored, the static friction coefficient increased by 4.24%, and the dynamic friction coefficient increased by 5.29%. The dynamic friction coefficient of the repaired hair treated with repair fluid A was reduced by 25.49% and 29.20% respectively compared with the restored hair, and the static friction coefficient and dynamic friction coefficient of the original hair were reduced by 22.15% and 25.25% respectively. The above results show that the smoothness of the hair treated with organosilicon supramolecular ion salt is significantly improved compared with the restored hair and the original hair.

[0145] Table 1 Friction coefficient test

[0146]

[0147] 3. Combing test

[0148] The organosilicon supramolecular ion salt obtained in Example 1 and water were mixed in a mass ratio of 1:99, stirred at 20° C. and 500 rpm for 3 min, and after being fully dissolved, the pH was adjusted to 8 with a 1 M NaOH solution to obtain a repair solution A;

[0149] The real human hair pieces were treated with a 10% SDS solution to obtain SDS-treated hair pieces, and the dry combing work was measured after natural drying; the hair pieces were then treated with repair solution A, and the dry combing work after treatment was measured again after natural drying. The test results are shown in Table 2.

[0150] It can be seen from Table 2 that the dry combing work of the hair after being treated with Repair Fluid A is reduced by 11.7% compared with that before treatment, which indicates that the hair is more supple and combable after being treated with the product.

[0151] Table 2 Dry combing work

[0152]

[0153]

[0154] Example 4: Preparation of supramolecular ionic salt using long-chain aminopolysiloxane

[0155] Since long-chain aminopolysiloxane has poor water solubility, it will form gel when directly reacted with maleic acid, which makes it difficult to use in water-based shampoo and hair care products. Therefore, before the reaction, aminopolysiloxane must be prepared into a water-soluble system or a purchased water-soluble system must be used. Taking aminosilicone water-soluble emulsion system 1201 as an example, organosilicon supramolecular ion salt is prepared.

[0156] The method of preparing an organosilicon supramolecular ionic salt using an aminosiloxane water-soluble emulsion system 1201 comprises the following steps:

[0157] 9 g of maleic acid was mixed with 30 g of aminosilicone water-soluble emulsion system 1201, and the mixture was stirred and reacted at room temperature for 30 min to obtain 39 g of aminosilicone maleate water-soluble emulsion system.

[0158] Repairing liquid B was prepared in the same manner as in Example 3, and the dry combing work of the hair was tested for the original hair, the hair treated only with the 1201 water-soluble system (aminosilicone water-soluble emulsion system 1201), and the hair treated with the repairing liquid B. The results are shown in Table 3.

[0159] Table 3 Dry combing work

[0160]

[0161] The results showed that the repair solution prepared using the aminosilicone water-soluble emulsion system and maleate also had good hair smoothing ability, which was better than the hair pieces treated with SDS and treated only with the aminosilicone water-soluble emulsion system 1201.

[0162] Example 5: Preparation of hair care products using organosilicon supramolecular ionic salts.

[0163] The organosilicon supramolecular ion salt prepared in Example 1 was used to prepare shampoo, and the formula was shown in Table 4:

[0164] Table 4

[0165]

[0166] The preparation method is as follows:

[0167] In a beaker, the main surfactant sodium dodecyl sulfate (SDS) is mixed with an appropriate amount of water, cocamidopropyl betaine and functional ingredients are added to the mixture, and the mixture is stirred evenly. The pH value of the mixture is adjusted to a value close to the natural pH value of the scalp (about 5.5) with citric acid, and water is added to the designed system mass to prepare a shampoo.

[0168] The organosilicon supramolecular ion salt prepared in Example 1 was added to the shampoo prepared above as an effective ingredient as a comparative sample, and no effective ingredient was added as a blank sample. The dry combing work of the comparative sample and the blank sample after treating the human hair was tested according to the method of Example 3, and the results are shown in Table 5.

[0169] Table 5 Dry combing work

[0170]

[0171] The results show that the shampoo prepared using the organosilicon supramolecular ion salt of Example 1 has the effect of smoothing hair. Comparative Example 1: Preparation of organosilicon supramolecular ion salt using glacial acetic acid

[0172] On the basis of Example 1, deionized water was replaced by glacial acetic acid, and the remaining steps were consistent with Example 1 to prepare 29.67 g of liquid product.

[0173] Comparative Example 2: Preparation of organosilicon supramolecular ion salt by changing the amount of maleic acid

[0174] On the basis of Example 1, the amount of maleic acid was changed to 13.09 g, the molar ratio of amino double-capped maleate to maleic acid was 1:1.4, and the remaining steps were consistent with Example 1 to prepare 29.45 g of amino double-capped maleate.

[0175] Comparative Example 3: Preparation of organosilicon supramolecular ionic salt using aminopropyl-terminated polydimethylsiloxane

[0176] The main structure of aminopropyl-terminated polydimethylsiloxane is a compound with aminopropyl at the terminal and polydimethylsiloxane as the main chain. Here, the aminopropyl-terminated polydimethylsiloxane with CAS number 99904-16-2 is used to prepare the organosilicon supramolecular ion salt, which includes the following steps:

[0177] 0.15 g of maleic acid and 10.78 g of amino-terminated polydimethylsiloxane were mixed (the molar ratio of maleic acid to amino group was 1:1), and the mixture was stirred at room temperature. As the reaction proceeded, the viscosity of the system gradually increased, while the amount of maleic acid gradually decreased. After stirring for half an hour, the system was basically solidified, and white solid still remained.

[0178] It can be seen that since the amino groups in the overly long-chain aminopropyl siloxane are far apart, an environment is provided for cross-linking between the dicarboxyl groups in maleic acid and different aminosiloxanes, which causes the system to solidify and be unable to continue reacting; at the same time, since the aminopropyl-terminated polydimethylsiloxane has extremely poor water solubility, even if it is modified to be water-soluble through a salt-forming reaction, the viscosity after the reaction is still high, resulting in the entire system being unable to form a uniform phase in water.

[0179] Comparative Example 4: Comparison of repair effects of similar raw materials

[0180] On the basis of Example 3, the organosilicon supramolecular ion salt (amino dicapped maleate) is replaced by the existing compound bisaminopropyl diglycol dimaleate, and the remaining steps are consistent with Example 3.

[0181] The products prepared in Comparative Example 1, Comparative Example 2, and Comparative Example 4 were respectively mixed with water in a mass ratio of 1:99, stirred at 20°C and 500rpm for 3 min, and after fully dissolved, the pH was adjusted to 8 with 1M NaOH solution to obtain repair solution C (Comparative Example 1), repair solution D (Comparative Example 2), and repair solution E (Comparative Example 4), respectively.

[0182] Part of the restored hair was taken and immersed in the repair solution C, the repair solution D and the repair solution E respectively, treated at 50°C for 20 minutes, taken out and dried to obtain the repaired hair C, D and E respectively.

[0183] The obtained hair samples were observed under a fluorescence microscope, and the results were as follows: Figure 7 The results show that the repair solution C corresponding to comparative example 1 has almost no repair effect. This is because the acidic protonating agent used competes with maleic acid for reaction sites, and the product obtained is the reaction product of acetic acid and double capping. There is no unsaturated bond in the structure of acetic acid, so the product has no effect on repairing damaged hair.

[0184] In Example 1, one amino double head is combined with two maleic acid molecules, while in Comparative Example 2, since the preparation was not strictly in accordance with the reactant ratio, there was an excess of amino double head, resulting in part of the product being one amino double head combined with one maleic acid, thereby affecting the hair repair effect of repair liquid D.

[0185] Comparative Example 4 has a repairing effect on the hair, but the gaps in the hair scales with fluorescence can still be seen, which means that it has no silicone structure and its ability to repair the hair scales is weak. The electron microscopy results of the hair E repaired by Comparative Example 4 are as follows: Figure 6 As shown in c, the results show that comparative example 4 has a certain degree of repair on the hair surface, but the hair scales are still lifted, which is consistent with the results of fluorescence microscopy.

[0186] The above results show that the organosilicon supramolecular ion salt prepared in Example 1 has excellent hair repairing function, and its effect is significantly better than existing products.

[0187] Although the present invention has been disclosed as above in the form of a preferred embodiment, it is not intended to limit the present invention. Anyone familiar with this technology can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be based on the definition of the claims.

Claims

1. An organosilicon supramolecular ion salt, characterized in that: The structural formula is as follows: Wherein, the structural formula of A is as shown in Formula II: n is an integer greater than or equal to 1; Preferably, n is an integer of 1-5.

2. A method for preparing the organosilicon supramolecular ion salt according to claim 1, characterized in that: The steps include: Maleic acid is mixed with amino-terminated siloxane to obtain an organosilicon supramolecular ionic salt.

3. The method according to claim 2, characterized in that The method for preparing the organosilicon supramolecular ion salt comprises: Dissolving maleic acid in a solvent and mixing it with amino-terminated siloxane to obtain an organosilicon supramolecular ion salt; or, The maleic acid is ground, mixed with amino-terminated siloxane, and further ground to obtain an organosilicon supramolecular ionic salt.

4. The method according to claim 2 or 3, characterized in that: The amino-terminated siloxane includes one or more of 1,3-bis(3-aminopropyl)-1,1,3,3-tetramethyldisiloxane (n=1), amino-terminated polydimethylsiloxane (n≥2) or aminosiloxane water-soluble emulsion system.

5. The method according to claim 2 or 3, characterized in that: The molar ratio of maleic acid to amino groups in amino-terminated siloxane is 1:0.8-1.

3.

6. The method according to claim 2 or 3, characterized in that: The system temperature during the preparation process is 25-40°C.

7. Use of the organosilicon supramolecular ion salt according to claim 1 in the preparation of daily chemical products or medicines.

8. The use according to claim 7, characterized in that: The daily chemical products include: hair care cosmetics, detergents; the hair care cosmetics include: hair conditioner, hair oil, hair milk, hair wax, hair dew, after-wash sunscreen lotion, steam-free hair milk, sunscreen shampoo, medicinal hair milk, conditioning shampoo, shampoo, and aftershave.

9. A product, characterized in that The product contains the organosilicon supramolecular ion salt according to claim 1; the product is a daily chemical product or a medicine.

10. The product according to claim 9, characterized in that The hair care cosmetics include: hair conditioner, hair oil, hair milk, hair wax, hair dew, after-wash sunscreen lotion, steam-free hair milk, sunscreen shampoo, medicinal hair milk, conditioning shampoo, shampoo, and aftershave.

Citation Information

Patent Citations

  • Copolymerization transparent nylon and preparation method for same

    CN107286340A

  • Puncture-resistant biaxially oriented nylon film and preparation method thereof

    CN116039196A

  • Synthesis method and application of repairing agent capable of repairing damaged hair and preventing dyed hair from decolorizing

    CN116120180A

  • Azelaic acid organic silicon supramolecular ion salt and preparation method thereof

    CN117551125A

  • Block copolymer maleimide-based resin and method of producing the same

    JP2002161137A

Cited By