Shaft sand washing fluid as well as preparation method and application thereof
The sand-pulling liquid prepared by mixing emulsion-type agents with clean water and mixed with nitrogen into the wellbore, solving the waste and complexity of the existing foam sand-pulling process, achieving low-cost, low-complexity sand suspension and separation effects, suitable for low-cost, low-complexity Pressure well.
Patent Information
- Application Number
- CN202310620085.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-29
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2043-05-29
AI Technical Summary
The existing foam sand crushing process has problems such as waste, environmental pollution and high costs, especially in low-pressure wells, and the commonly used methods are complex and have high safety risks.
The sand-pulling liquid is prepared by mixing emulsion agent with clean water, and mixed with nitrogen to inject it into the wellbore. The low viscosity of the emulsion and surfactant characteristics of the emulsion can achieve suspension and rapid separation of the sand, avoid defoaming and recycling.
Under low viscosity conditions, the sand in the wellbore is effectively flushed out, achieving a suspension rate of 90% or more. The process is simple, the cost is low, and there is no need for defoaming treatment. It quickly realizes liquid-sand separation, which is suitable for low-pressure wells.
Smart Images

Figure CN119039954A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of oil and gas well repair operations, and in particular relates to a wellbore sand flushing fluid and a preparation method and application thereof. Background Art
[0002] In the process of oil and gas reservoir development, the problem of sand production in the formation often occurs. If the fluid in the well cannot carry all the sand out of the wellbore, the sand will continue to deposit in the wellbore, which will cause sand to bury the reservoir, increase the fluid flow resistance, and reduce production. Therefore, it is necessary to carry out wellbore sand cleaning operations for oil and gas wells that produce sand. Common sand cleaning methods include mechanical sand bailing and tubing sand flushing. Commonly used sand flushing fluids include clean water, glue, foam, etc. For wells with long-term production bottom deficits or wells with relatively low formation pressure coefficients, using clean water or glue to flush sand often results in serious leakage, inability to establish effective circulation, and difficulty in returning sand to the wellhead. Therefore, sand flushing is performed in wells or formations with low pressure coefficients.
[0003] Commonly used sand flushing media are mainly clean water (including seawater) and foam. Since foam fluid has the advantages of low density, high viscosity, low filtration loss, strong sand carrying capacity, and with the long-term exploitation of oil fields, the oil layer pressure is greatly reduced. In this case, foam is often used as sand flushing medium. However, the existing foam sand flushing process generally does not realize the recycling and reuse of foam base fluid. There are problems such as large waste of foam in one-time use and easy pollution of the environment by the returned foam, which not only increases the cost of foam sand flushing and well washing, but also is not conducive to environmental protection.
[0004] At present, methods such as changing the pH value of the foam base liquid and adding organic defoaming agents are commonly used in nitrogen foam sandblasting construction to achieve the purpose of defoaming and re-foaming. The method of changing the pH value of the foam base liquid is selective for the foaming agent and is limited to amphoteric foaming agents. In addition, corrosive strong acids and strong alkalis need to be repeatedly added during the circulation process to adjust the pH value. There are safety risks during transportation and construction, and the construction equipment requirements are high and the construction process is relatively complicated. Although the addition of conventional organic defoaming agents can quickly defoam, it is easy to affect the performance of the foaming agent, inhibiting its ability to re-foam, and cannot achieve the recycling of the foam base liquid.
[0005] Chinese invention patent application CN102031098A discloses a recyclable foam base fluid for sand flushing and well washing. The sand flushing and well washing fluid includes an N-alkyl-β-aminopropionic acid type amphoteric surfactant and water. The amphoteric surfactant is sensitive to acid and alkali, and the pH value of the base fluid is adjusted to achieve the recycling of the foam. Although the invention achieves the recycling of the foam, it needs to be equipped with corresponding acid tanks, alkali tanks, and corresponding stirring and mixing equipment during application. Strong acid and alkali need to be added repeatedly during the circulation process, which has the disadvantages of complex recycling process and high application cost.
[0006] Chinese invention patent application CN112240173A discloses a foam cycle-based sand flushing and well washing method for oil and gas wells, and a defoaming liquid and a foaming liquid used for sand flushing and well washing for oil and gas wells. The invention adds a defoaming liquid to the sand-carrying foam fluid obtained after well washing to defoam, separate the sand particles, and then add a foaming agent to the obtained liquid for use. The invention has the disadvantages of repeatedly adding a foaming agent and a defoaming agent, and a large amount of the agent is used. The defoaming agent will inhibit the re-foaming performance of the sand flushing fluid.
[0007] Chinese invention patent application CN115725287A discloses a heat-resistant and salt-resistant nitrogen foam sand-washing liquid and a preparation and use method thereof, wherein the former comprises a nitrogen foam stock solution, a sedimentation aid and a sand-carrying agent, and the nitrogen foam stock solution comprises: 0.01% to 0.2% sodium polyacrylate, 0.01% to 1% carboxymethyl cellulose, 0.01% to 0.1% carrageenan, 0.01% to 0.2% polyvinyl pyrrolidone, 0.1% to 1% sodium carbonate, 0.1% to 2% sodium bicarbonate, 0.01% to 0.1% triethanolamine, 0.01% to 0.1% sodium dodecylbenzene sulfonate, 0.01% to 0.5% octadecylphenol polyoxyethylene ether, 0.01% to 0.5% dodecyl dimethyl betaine, and the balance is water. The sand-carrying capacity of the sand-washing liquid in the invention is strong, the silt and the foam liquid can be quickly separated, and it can be recycled for many times, but there are many additives and the cost is high.
[0008] Therefore, it is necessary to develop a sand flushing liquid that has a simple preparation process, low cost, can quickly separate liquid sand without defoaming treatment, and can be recycled. Summary of the invention
[0009] In order to solve the above problems, the present invention provides a wellbore sand flushing fluid and its preparation method and application. The sand flushing fluid can be quickly prepared by directly mixing an emulsion-type agent with clean water. The sand flushing fluid is mixed with nitrogen and injected into the wellbore. The sand flushing fluid flushes the sand in the wellbore, and the settled sand in the wellbore can be flushed out to the ground under the condition of low viscosity or flow rate.
[0010] In order to achieve the above-mentioned purpose of the present invention, the specific technical solution adopted by the present invention is:
[0011] A wellbore sand flushing fluid consists of emulsion A and water, wherein the raw materials of emulsion A include tetradecyl primary amine, didodecylamine, hydrochloric acid, white oil and water.
[0012] Preferably, the emulsion A comprises solution B and solution C, wherein the raw materials of solution B comprise tetradecyl primary amine, hydrochloric acid and water; the raw materials of solution C comprise didodecylamine and white oil.
[0013] Preferably, the sand washing liquid comprises 1-4 parts of emulsion A and 96-99 parts of water by weight.
[0014] Preferably, the emulsion A comprises 40-50 parts of solution B and 50-60 parts of solution C by weight.
[0015] Preferably, the raw materials of the solution B include 2-5 parts of tetradecyl primary amine, 1-3 parts of hydrochloric acid and 92-97 parts of water in parts by weight.
[0016] Preferably, the raw materials of the solution C include 2-8 parts of didodecylamine and 92-98 parts of white oil by weight.
[0017] The present invention also relates to a method for preparing a wellbore sand flushing fluid, comprising the following steps:
[0018] (1) Tetradecyl primary amine is added to water, and hydrochloric acid is added during stirring to obtain solution B;
[0019] (2) adding didodecylamine to white oil and stirring to obtain solution C;
[0020] (3) Mixing solution B and solution C, heating and stirring, to obtain emulsion A;
[0021] (4) Emulsion A is mixed with water to obtain sand washing liquid.
[0022] Preferably, in step (1), hydrochloric acid is added to adjust the pH to 7-8, and the mass concentration of the hydrochloric acid is 10-20%.
[0023] Preferably, the heating temperature in step (3) is 50-70° C., and the heating and stirring time is 8-10 min.
[0024] The present invention also relates to the application of the sand flushing fluid or the sand flushing fluid prepared by the preparation method in sand flushing and well washing.
[0025] Preferably, during the sand flushing and well washing process, a sand flushing fluid or a sand flushing fluid and nitrogen are simultaneously introduced into the well to flush the sand, and the fluid returned from the well is re-introduced into the well as a sand flushing fluid after sedimentation or filtration to remove sand.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] (1) The present invention can achieve surface modification of sand deposited in the wellbore. Even in a static state, the sand adsorbed / encapsulated with nitrogen can still be suspended in the sand flushing liquid. The sand flushing liquid is mixed with an appropriate amount of sand and fully shaken in a closed container, so that the suspension rate of the sand in clean water can reach 90% or more;
[0028] (2) The sand flushing liquid has low viscosity and is easy to separate from the liquid and sand. It does not require defoaming and can be quickly reused after standing or filtering;
[0029] (3) Compared with conventional foam sand washing, this technology has the advantages of simple process and low cost. It can achieve stable suspension of sand at low viscosity and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 The conventional foam sand washing fluid (left) and the sand washing fluid of Example 1 (middle and right). DETAILED DESCRIPTION
[0031] The technical solutions in the embodiments of the present invention are further clearly described. The described embodiments are only a part of the present invention and are used to explain the present invention but not to limit the present invention. Therefore, other embodiments obtained by other technicians in the field without creative work all belong to the protection scope of the present invention.
[0032] The experimental methods without specific conditions in the examples are usually carried out under conventional conditions. The materials, reagents, etc. used in the following examples are all commercially available unless otherwise specified.
[0033] Example 1
[0034] The wellbore sand flushing fluid of this embodiment is prepared from tetradecyl primary amine, didodecyl amine, hydrochloric acid, white oil and water.
[0035] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0036] (1) Add 3 parts of tetradecyl primary amine to 95 parts of water, add 2 parts of hydrochloric acid (hydrochloric acid concentration is 15%), stir thoroughly until completely dissolved, pH is 7, to prepare solution B;
[0037] (2) Add 5 parts of didodecylamine to 95 parts of white oil and stir thoroughly to prepare solution C;
[0038] (3) 50 parts of solution B and 50 parts of solution C were heated at 60° C. for 10 min and stirred for 10 min to prepare emulsion A;
[0039] (4) Mix 97 parts of clean water with 3 parts of emulsion A to obtain a sand washing solution.
[0040] Weigh 10 parts of quartz sand (particle size < 0.5 mm) and mix with 90 parts of sand washing liquid. Shake thoroughly in a closed container and take a photo immediately. The suspension rate of sand in clean water can reach 95%. Figure 1 As shown in the middle figure, the lower clear liquid can be reused.
[0041] Weigh 10 parts of quartz sand (particle size < 0.5 mm) and mix with 90 parts of the above lower layer of clear water. Shake thoroughly in a sealed container and take a picture immediately. The suspended state of the sand can be seen. Figure 1As shown in the right picture, more than 60% of the sand can still float on the water surface.
[0042] Example 2
[0043] The wellbore sand flushing fluid of this embodiment is prepared from tetradecyl primary amine, didodecyl amine, hydrochloric acid, white oil and water.
[0044] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0045] (1) Add 5 parts of tetradecyl primary amine to 92 parts of water, add 3 parts of hydrochloric acid (concentration is 20%), stir thoroughly until completely dissolved, pH is 8, to prepare solution B;
[0046] (2) Add 8 parts of didodecylamine to 92 parts of white oil and stir thoroughly to prepare solution C;
[0047] (3) 40 parts of solution B and 60 parts of solution C were heated at 70° C. for 8 min and stirred for 8 min to prepare emulsion A;
[0048] (4) Mix 99 parts of clean water with 1 part of emulsion A to obtain a sand washing solution.
[0049] Example 3
[0050] The wellbore sand flushing fluid of this embodiment is prepared from tetradecyl primary amine, didodecyl amine, hydrochloric acid, white oil and water.
[0051] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0052] (1) Add 2 parts of tetradecyl primary amine to 97 parts of water, add 1 part of hydrochloric acid (concentration is 10%), stir thoroughly until completely dissolved, pH is 7, to prepare solution B;
[0053] (2) Add 2 parts of didodecylamine to 98 parts of white oil and stir thoroughly to prepare solution C;
[0054] (3) 45 parts of solution B and 55 parts of solution C were heated at 50° C. for 10 min and stirred for 10 min to prepare emulsion A;
[0055] (4) Mix 96 parts of clean water with 4 parts of emulsion A to obtain a sand washing solution.
[0056] Comparative Example 1
[0057] The raw materials of the wellbore sand flushing fluid in this comparative example are hexadecyl dimethyl ammonium chloride, didodecyl amine, white oil and water.
[0058] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0059] (1) Add 3 parts of hexadecyl dimethyl ammonium chloride to 97 parts of water and stir thoroughly until it is completely dissolved to prepare solution B;
[0060] (2) Add 5 parts of didodecylamine to 95 parts of white oil and stir thoroughly to prepare solution C;
[0061] (3) 50 parts of solution B and 50 parts of solution C were heated at 60° C. for 10 min and stirred for 10 min to prepare emulsion A;
[0062] (4) Mix 97 parts of clean water with 3 parts of emulsion A to obtain a sand washing solution.
[0063] Comparative Example 2
[0064] The raw materials of the wellbore sand flushing fluid in this comparative example are tetradecyl primary amine, dioctadecyl amine, hydrochloric acid, white oil and water.
[0065] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0066] (1) Add 3 parts of tetradecyl primary amine to 95 parts of water, add 2 parts of hydrochloric acid (hydrochloric acid concentration is 15%), stir thoroughly until completely dissolved, pH is 7, to prepare solution B;
[0067] (2) Add 5 parts of dioctadecylamine to 95 parts of white oil and stir thoroughly to prepare solution C;
[0068] (3) 50 parts of solution B and 50 parts of solution C were heated at 60° C. for 10 min and stirred for 10 min to prepare emulsion A;
[0069] (4) Mix 97 parts of clean water with 3 parts of emulsion A to obtain a sand washing solution.
[0070] Comparative Example 3
[0071] The raw materials of the wellbore sand flushing fluid in this comparative example are tetradecyl primary amine, didodecyl amine, hydrochloric acid, kerosene and water.
[0072] The preparation method of the wellbore sand flushing fluid is specifically performed as follows:
[0073] (1) Add 3 parts of tetradecyl primary amine to 95 parts of water, add 2 parts of hydrochloric acid (hydrochloric acid concentration is 15%), stir thoroughly until completely dissolved, pH is 7, to prepare solution B;
[0074] (2) Add 5 parts of didodecylamine to 95 parts of kerosene and stir thoroughly to prepare solution C;
[0075] (3) 50 parts of solution B and 50 parts of solution C were heated at 60° C. for 10 min and stirred for 10 min to prepare emulsion A;
[0076] (4) Mix 97 parts of clean water with 3 parts of emulsion A to obtain a sand washing solution.
[0077] Example 4 Sand flushing fluid effect test
[0078] Viscosity test
[0079] The sand flushing liquid and nitrogen are pumped into the well at the same time for sand flushing. After the sand flushing liquid is discharged from the wellbore to the ground, no reagents need to be added. Liquid sand separation can be achieved by standing or filtering. After the sand flushing liquid is returned to the ground tank and left to stand for 10 seconds, the viscosity of the lower layer of clear water is measured. The specific operation process is as follows:
[0080] Measure 350 mL of the lower layer of clear water and transfer it to a rotary viscosity measuring cup. Use a Fann-type six-speed rotary viscometer to measure the shear rate at 170 s. -1 The apparent viscosity at .
[0081] Sand blasting efficiency
[0082] Weigh m0 = 50g of sand and spread it evenly in a simulated horizontal tube (inner diameter 3.67cm). Use a PVC hose (inner diameter 2.00cm) as a sand flushing tube. Prepare 200L of sand flushing liquid and stir evenly. Adjust the gas-liquid volume ratio to 3:7 and the sand flushing displacement to 3L / min. Weigh the mass m1 of the sand flushed out and calculate the sand flushing performance of the sand flushing liquid. The calculation formula is as follows:
[0083]
[0084] Where: Ψ—sand flushing efficiency, %;
[0085] m1—mass of sand flushed out, g;
[0086] m0—mass of sand filled in, g.
[0087] Liquid sand separation time
[0088] The time required for the sand to completely float to the surface of the sand flushing liquid or settle to the bottom of the sand flushing liquid after the sand is returned to the ground storage tank and left to stand.
[0089] Table 1 shows the test data of Examples 1-3 and Comparative Examples 1-3 at 25°C.
[0090] Table 1 Test results
[0091]
[0092] In combination with the above embodiments, it can be seen that after the sand flushing fluid of the present invention is returned from the wellbore to the ground, the rapid separation of gas, liquid and sand can be automatically achieved without adding any reagents. The sand particles float on the surface of the sand flushing fluid, and the viscosity of the lower clear night is measured to be ≤3mPa·s.
[0093] The above detailed description is a specific description of one feasible embodiment of the present invention. The embodiment is not intended to limit the patent scope of the present invention. Any equivalent implementation or modification that does not deviate from the present invention should be included in the scope of the technical solution of the present invention.
Claims
1. A wellbore sand flushing fluid, characterized in that: The sand washing liquid comprises emulsion A and water, wherein the raw materials of emulsion A comprise tetradecyl primary amine, didodecyl amine, hydrochloric acid, white oil and water.
2. The sand washing fluid according to claim 1, characterized in that: The emulsion A comprises solution B and solution C, wherein the raw materials of solution B comprise tetradecyl primary amine, hydrochloric acid and water; the raw materials of solution C comprise didodecylamine and white oil.
3. The sand washing fluid according to claim 1, characterized in that: The sand washing liquid comprises 1-4 parts of emulsion A and 96-99 parts of water by weight.
4. The sand washing liquid according to claim 2, characterized in that: In parts by weight, the emulsion A includes 40-50 parts of solution B and 50-60 parts of solution C.
5. The sand washing liquid according to any one of claim 2, characterized in that: In terms of weight, the raw materials of the solution B include 2-5 parts of tetradecyl primary amine, 1-3 parts of hydrochloric acid and 92-97 parts of water.
6. The sand washing liquid according to any one of claim 2, characterized in that: In parts by weight, the raw materials of the solution C include 2-8 parts of didodecylamine and 92-98 parts of white oil.
7. A method for preparing the sand washing liquid according to any one of claims 1 to 6, characterized in that: The following steps are involved: (1) Add tetradecyl primary amine to water and add hydrochloric acid to obtain solution B; (2) adding didodecylamine to white oil and stirring to obtain solution C; (3) Mixing solution B and solution C, heating and stirring, to obtain emulsion A; (4) Emulsion A is mixed with water to obtain sand washing liquid.
8. The preparation method according to claim 7, characterized in that: In step (1), hydrochloric acid is added to adjust the pH to 7-8, and the mass concentration of the hydrochloric acid is 10-20%.
9. The preparation method according to claim 7, characterized in that: The heating temperature in step (3) is 50-70° C., and the heating and stirring time is 8-10 min.
10. Use of the sand flushing fluid according to any one of claims 1 to 6 or the sand flushing fluid prepared by the preparation method according to any one of claims 7 to 9 in sand flushing and well washing.
11. The use according to claim 10, characterized in that: During the sand flushing and well washing process, a sand flushing fluid or a sand flushing fluid and nitrogen are simultaneously introduced into the well to flush the sand, and the fluid returned from the well is re-introduced into the well as a sand flushing fluid after sedimentation or filtration to remove sand.
Citation Information
Patent Citations
Recyclable foam base fluid for sand-washing well
CN102031098A
Oil-gas well sand washing method based on foam circulation and defoaming liquid and foaming liquid for oil-gas well sand washing
CN112240173A
Temperature-resistant and salt-resistant nitrogen foam sand washing fluid as well as preparation and use methods thereof
CN115725287A
Sand-flushing well-cleaning agent for oil well
CN102399545A
Sand flushing foam liquid for low-pressure absorption oil wells and preparation method of foam liquid
CN109722231A