Atomic layer deposition coating method

By adopting an atomic layer deposition coating method with alternating gas inlet and purge treatment on the cutting surface of the battery, combined with the heat diffusion step, the poor passivation effect and winding problems in the prior art are solved, and a more complete and uniform Passivation film deposition improves battery performance.

CN119040856APending Publication Date: 2024-11-29JIANGSU MICROVIA NANO EQUIP TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411183116.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The existing atomic layer deposition coating technology has poor passivation effect and winding on the cutting surface of the battery, which affects the battery performance.

Method used

Using a new coating method, by alternately passing the first and second process gases into the reaction device and performing purge treatment after sufficient sealing, the pass time of the reaction source is controlled to avoid winding plating. , in combination with the thermal diffusion step to ensure the integrity and uniformity of the passivation film.

Benefits of technology

It effectively reduces the winding phenomenon, ensures the integrity and uniformity of the passivation film, improves the performance of the battery cutting surface coating, and ensures the deposition effect at a lower reaction source concentration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119040856A_ABST
    Figure CN119040856A_ABST
Patent Text Reader

Abstract

The invention discloses an atomic layer deposition coating method, the coating method comprises at least one coating circulation process, the coating circulation process comprises: introducing a first process gas into a reaction device containing a substrate, the first process gas comprising a first reaction gas and an inert gas, and the introduction duration of the first process gas being 0.1 s to 5 s; sealing the reaction device to diffuse and adsorb the first process gas to the surface to be coated of the substrate; carrying out first purging treatment on the reaction device; second process gas is introduced into the reaction device, the second process gas comprises second reaction gas and inert gas, and the introduction duration of the second process gas ranges from 0.1 s to 5 s; the reaction device is closed, so that the second process gas is diffused and adsorbed to the to-be-coated surface of the substrate; and carrying out second purging treatment on the reaction device. In this way, the effect of depositing a passivation film can be guaranteed, and meanwhile the problem of winding plating is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the photovoltaic field, the semiconductor field and the battery field, and in particular to an atomic layer deposition coating method. Background Art

[0002] With the rise of new module technologies such as half-cell modules and shingled modules, a cell needs to be split into two or more pieces when making modules. The recombination rate on the surface of the split section of the cell is very high, which will have a great impact on the electrical performance of the solar cell. In order to reduce this cutting loss, one method is to passivate the cut edge of the cell. Edge passivation refers to the formation of a passivation film on the surface of the cell cut surface by deposition, which plays a role in reducing minority carrier recombination, providing field passivation effect, and reducing reflectivity.

[0003] At present, when ALD (Atomic Layer Deposition) technology is applied to edge passivation technology or deposition technology on the cut surface of sliced ​​cells, there are problems such as poor passivation effect and passivation film deposited on non-cut surfaces, resulting in wrap-around plating. Summary of the invention

[0004] The main technical problem solved by the present application is to provide an atomic layer deposition coating method, which can ensure the effect of depositing a passivation film while reducing the problem of circumferential plating.

[0005] In order to solve the above technical problems, a technical solution adopted in the present application is: to provide an atomic layer deposition coating method, the coating method includes at least one coating cycle process, and the coating cycle process includes: introducing a first process gas into a reaction device containing a substrate, wherein the first process gas includes a first reaction gas and an inert gas, and the introduction time of the first process gas is in the range of 0.1s-5s; closing the reaction device to allow the first process gas to diffuse and adsorb to the surface of the substrate to be coated; performing a first purge treatment on the reaction device; introducing a second process gas into the reaction device, wherein the second process gas includes a second reaction gas and the inert gas, and the introduction time of the second process gas is in the range of 0.1s-5s; closing the reaction device to allow the second process gas to diffuse and adsorb to the surface of the substrate to be coated; performing a second purge treatment on the reaction device.

[0006] Preferably, before entering the first coating cycle process, the coating method further comprises: performing a vacuum treatment on the reaction device, and stopping the vacuum treatment when the first process gas is subsequently introduced into the reaction device.

[0007] Preferably, the step of performing a first purge treatment on the reaction device includes: turning on the vacuum pump to perform a vacuum treatment on the reaction device; during the vacuum treatment, introducing the inert gas into the reaction device at least twice, wherein the air inlet of the reaction device is closed between two adjacent introductions of the inert gas.

[0008] Preferably, before the step of introducing the second process gas into the reaction device, the step further includes: closing the vacuum pump.

[0009] Preferably, the step of performing a second purge treatment on the reaction device includes: turning on the vacuum pump to perform a vacuum treatment on the reaction device; during the vacuum treatment, introducing the inert gas into the reaction device at least twice, wherein the air inlet of the reaction device is closed between two adjacent introductions of the inert gas.

[0010] Preferably, the step of closing the reaction device to allow the first process gas to diffuse and adsorb to the surface of the substrate to be coated, comprises: closing the reaction device for 0.1s to 10s, allowing the first process gas to diffuse and adsorb to the surface of the substrate to be coated; and / or, the step of closing the reaction device to allow the second process gas to diffuse and adsorb to the surface of the substrate to be coated, comprises: closing the reaction device for 0.1s to 10s, allowing the second process gas to diffuse and adsorb to the surface of the substrate to be coated.

[0011] Preferably, the temperature in the reaction device ranges from 100°C to 400°C.

[0012] Preferably, the first reaction gas includes any one of trimethylaluminum, titanium tetrachloride or hafnium tetrachloride.

[0013] Preferably, the second reaction gas includes any one of water vapor, titanium nitride or hafnium dioxide.

[0014] Preferably, the inert gas includes any one of nitrogen, argon, helium or neon.

[0015] The above technical solution changes the original source-passing method by shortening the time for the reaction source to be introduced to less than 5s. Since the filling time is short enough, the concentration of the reaction source can be conveniently controlled, so that the reaction source is not easy to enter the gap of the substrate, and therefore it is not easy to cause plating around. After the reaction source is introduced, there is a thermal diffusion step, in which all air inlets and outlets need to be closed so that the interior of the reaction device is in a closed state. At this time, the first process gas or the second process gas in the reaction device will diffuse to the surface of the substrate to be coated in the reaction device due to the thermal effect in the cavity, which can be specifically the cutting surface of the sliced ​​battery. The passivation film deposited under the condition of a lower reaction source concentration has a more complete structure, a more uniform film layer, and ensures the effect of depositing the passivation film. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic flow chart of an embodiment of a coating method provided by the present application;

[0017] Figure 2 It is a comparison table of performance parameters of different coating methods;

[0018] Figure 3 It is a schematic flow chart of another embodiment of the coating method provided by the present application;

[0019] Figure 4 It is a flow chart of an implementation of step S230 in the coating method provided in the present application. DETAILED DESCRIPTION

[0020] In order to make the purpose, technical solutions and advantages of the present application clearer, the technical solutions in the embodiments of the present application will be clearly and completely described below in combination with the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0021] Atomic layer deposition is a technology that forms a deposited film by alternately passing gaseous precursor pulses into the reactor and chemically adsorbing and reacting on the deposition substrate; when the precursors reach the surface of the deposition substrate, they will chemically adsorb on its surface and react on the surface; the atomic layer deposition reactor needs to be cleaned with an inert gas between different precursor pulses. The atomic layer deposition reaction mode is that two different gases are alternately saturated with chemical adsorption to grow into a thin film.

[0022] The existing coating method usually includes at least one coating cycle process. In one coating cycle process, a reaction source needs to be introduced into the reaction device. The existing source introduction method is to continuously introduce reactants into the reaction device for a long time. However, the inventors have found through research that continuous source introduction leads to excessive source concentration in the reaction device and excessive reaction rate. Part of the reaction source will enter the substrate through the gaps between the substrates (such as sliced ​​cells), thereby causing the deposition of the film on the non-cut area of ​​the substrate, resulting in a wrap-around plating phenomenon, which affects product performance.

[0023] In view of this, the present application provides a coating method to solve the above technical problems. Figure 1 , Figure 1 1 is a schematic diagram of a coating method according to an embodiment of the present invention. The coating method has at least one coating cycle process, and a coating cycle process includes the following steps:

[0024] Step S110: introducing a first process gas into a reaction device containing a substrate, wherein the first process gas includes a first reaction gas and an inert gas, and the first process gas is introduced for a time period ranging from 0.1s to 5s.

[0025] Specifically, in this embodiment, the component of the coating product is aluminum oxide, the first reaction gas can be TMA, the inert gas can be nitrogen, the nitrogen flow value is 1-10000sccm, and the nitrogen is used to carry TMA into the reaction device. Therefore, the first reaction gas and the inert gas enter the reaction device through the air inlet at the same time.

[0026] Step S120: closing the reaction device to allow the first process gas to diffuse and adsorb onto the surface of the substrate to be coated.

[0027] Optionally, in step S120, the specific duration of the closure of the reaction device is 0.1s to 10s. Specifically, in this step, the closure of the reaction device can be achieved by closing the air inlet and the air outlet of the reaction device.

[0028] Step S130: Perform a first purge process on the reaction device. Specifically, in this step, the reaction residues of the previous steps can be removed from the reaction device by purging with an inert gas. In order to improve the purge efficiency, a larger flow rate can be used for purge, such as 10000 sccm.

[0029] Step S140: introducing a second process gas into the reaction device, wherein the second process gas includes a second reaction gas and an inert gas, and the second process gas is introduced for a time period ranging from 0.1s to 5s.

[0030] Specifically, in this embodiment, the second reaction gas may be water vapor, and the inert gas may be nitrogen. The nitrogen is used to carry the water vapor into the reaction device, so the second reaction gas and the inert gas enter the reaction device through the gas inlet at the same time.

[0031] Step S150: Close the reaction device to allow the second process gas to diffuse and adsorb onto the surface of the substrate to be coated. This step is the same as the operation method of step S120. Optionally, in step S150, the specific duration of closing the reaction device is 0.1s to 10s.

[0032] Step S160: Perform a second purge process on the reaction device. Specifically, in this step, the reaction products, reaction byproducts and reaction residues of the previous steps can be removed from the reaction device by purging with an inert gas. In order to improve the purge efficiency, a larger flow rate can be used for purge, such as 10000 sccm.

[0033] Step S110-step S160 is a coating cycle process for depositing a single layer of passivation film. The complete coating method may include multiple continuous coating cycle processes, that is, after completing step S160, returning to step S110 again. Specifically, for example, it may include 30 consecutive cycle processes to achieve the deposition of multiple layers or passivation films of corresponding thickness.

[0034] The present invention changes the original source-passing method by shortening the time for introducing the reaction source to less than 5s. Since the filling time is short enough, the concentration of the reaction source in the reaction chamber can be conveniently controlled, so that the reaction source is not easy to enter the gap of the substrate, and therefore it is not easy to cause the plating-around phenomenon. After the reaction source is introduced, a heat diffusion step is performed. In this step, all air inlets and outlets need to be closed so that the interior of the reaction device is in a closed state. At this time, the first process gas or the second process gas in the reaction device will diffuse to the surface of the substrate to be plated in the reaction device due to the thermal effect in the cavity, which can be specifically the cutting surface of the sliced ​​battery. The passivation film deposited under the condition of a lower reaction source concentration has a more complete structure, a more uniform film layer, and ensures the effect of depositing the passivation film. It should be noted that the thermal diffusion step will not cause the reaction source to enter the gaps in the substrate. The specific reasons are: first, due to the short source charging time, the concentration of the reaction source in the reaction device will not be too high, and the reaction source has been deposited on the surface of the substrate during the source charging; second, the thermal diffusion step is after the source charging step, and the concentration in the reaction device is already very low at this time. The thermal diffusion step at this time only serves as a supplementary deposition; finally, the self-gravity of the stacked substrates has a compacting effect, making it difficult for the reaction source to diffuse into the gaps in the substrate during the thermal diffusion step.

[0035] In addition, it should be noted that, see Figure 2 , Figure 2 It is a comparison table of performance parameters of different coating methods. Figure 2 The coating performance parameters of four charging methods, including long-time charging (charging time is 5s-10s, and there is no subsequent heat diffusion step), short-time charging (charging time is 0.1s-5s, and there is no subsequent heat diffusion step), long-time charging plus heat diffusion step, and short-time charging plus heat diffusion step, are compared. As can be seen from the figure, in the case of long-time charging, regardless of whether the heat diffusion step is superimposed, a larger winding width will be formed, that is, the winding phenomenon is more serious. Short-time charging alone will cause incomplete coating structure due to too little control of the source amount charged into the reaction device, so the passivation effect is poor. Only when short-time charging is used together with subsequent heat diffusion can the purpose of directional coating be achieved while ensuring the uniformity of coating on the cut surface of the sliced ​​battery during the deposition process, the integrity of the coating film structure and the passivation effect, thereby solving the abnormal winding.

[0036] In other embodiments, the first reaction gas and the second reaction gas may be TiCl4 and NH3 respectively, and the coating product is TiN; the first reaction gas and the second reaction gas may be HfCl4 and H2O respectively, and the coating product is HfO2. The inert gas may also be any one of argon, helium or neon.

[0037] See also Figure 3 , Figure 3 : is a schematic flow chart of another embodiment of the coating method provided by the present application. Before entering the first coating cycle process, the coating method further includes:

[0038] Step S210: Vacuum the reaction device. Specifically, the vacuum treatment step can reduce the pressure in the reaction device to 0-1mbar by turning on the vacuum pump. Optionally, this step also includes preheating the reaction device. Specifically, the duration of the preheating treatment ranges from 1s to 3600s, and the temperature in the reaction device is maintained at 100℃-400℃. At this temperature, the reaction source can have a certain thermal diffusion coefficient to increase the reaction rate. The preheating treatment requires opening the air inlet and outlet at the same time to ventilate the reaction device to ensure that the flow field in the reaction chamber is stable when the passivation film is subsequently deposited. The flow value is 1-10000sccm.

[0039] Step S220: When the first process gas is introduced into the reaction device containing the substrate, the vacuum treatment is stopped. Specifically, after the preheating is completed, the passivation film deposition process on the substrate is started. In this step, the vacuum pump needs to be turned off when the first process gas is introduced to avoid the reaction source (the first reaction gas in this step) being drawn away, resulting in insufficient reaction source concentration, thereby ensuring the integrity of the coating and the passivation effect.

[0040] Step S230: Close the reaction device to allow the first process gas to diffuse and adsorb to the surface of the substrate to be coated. This step is the same as step S120 in the previous embodiment, and utilizes the thermal effect to allow the first reaction gas that has not yet been deposited to diffuse to the surface of the substrate to be coated, perform chemical adsorption, and achieve supplementary deposition of the first reaction source.

[0041] Step S240: performing a first purge treatment on the reaction device. This step is the same as step S130 and is used to remove reaction residues through a purge treatment.

[0042] Step S250: After the vacuum pump is turned off, the second process gas is introduced into the reaction device. In step S240, the vacuum pump needs to be turned on because the reaction residues in the reaction device need to be removed by purging. Therefore, this step prevents the second process gas introduced later from being extracted by turning off the vacuum pump, thereby ensuring the concentration of the reaction source in the reaction device.

[0043] Step S260: Close the reaction device to allow the second process gas to diffuse and adsorb onto the surface of the substrate to be coated. This step is the same as step S150 in the previous embodiment, and realizes the supplementary deposition of the second reaction source.

[0044] Step S270: performing a second purge treatment on the reaction device. This step is the same as step S160 and is used to remove reaction products, reaction by-products and reaction residues through a purge treatment.

[0045] Optionally, see Figure 4 , Figure 4 1 is a flow chart of an implementation of step S230 in the coating method provided by the present application. Step S230 specifically includes the following steps:

[0046] Step S231: Turn on the vacuum pump to perform vacuum treatment on the reaction device. During the purge treatment, the vacuum pump is always in the turned-on state.

[0047] Step S232: During the process of vacuum treatment, an inert gas is introduced into the reaction device at least twice, wherein the air inlet of the reaction device is closed between two adjacent inert gas introductions. Specifically, this step specifically includes at least two purge treatments, and a vacuum treatment is also included between two adjacent purge treatments. During the first purge treatment, it is necessary to open the air inlet for the introduction of inert gas, and at the same time open the air outlet, and remove part of the excess first reaction gas and part of the product by the vacuum pump. The inert gas flow rate can be less than 10000sccm, and the purge time is 0-15s. Since the substrate in the reaction device is in a stacked state, and the volume of the substrate accounts for too large a proportion of the volume of the cavity in the reaction device, therefore, by adding a vacuum step after the purge treatment, the positions that are difficult to purge, such as the dead corners, are strongly extracted to fully ensure the cleaning power of the purge. At this time, it is necessary to close the air inlet to stop the introduction of gas, and the excess first reaction gas, part of the product and part of the inert gas are discharged from the reaction device. The specific time of vacuuming is 0-10s. After the vacuum treatment, a purge treatment is performed again to extract the remaining first reaction gas and product, and to keep the flow field in the reaction device stable after the vacuum treatment, and to further improve the cleanliness of the purge. The parameters of this purge treatment can be the same as or different from those of the first purge treatment. In other embodiments, the number of purge treatments can be increased, and a vacuum treatment can be performed between two adjacent purge treatments. This step can also be performed only once.

[0048] Optionally, step S270 may also include at least two purge treatments and a vacuum treatment arranged between the purge treatments, like step S230, wherein the first purge treatment removes part of the excess second reaction gas and part of the product through a vacuum pump, and the vacuum treatment discharges the excess second reaction gas, part of the product and part of the inert gas out of the reaction device, and the purge treatment is performed again after the vacuum treatment to remove the remaining second reaction gas and product, and to ensure that the flow field in the reaction device remains stable after the vacuum treatment. In other embodiments, only one purge treatment may be included.

[0049] The above coating process can be applied to the preparation of a passivation film on the cut surface of a sliced ​​battery, and can also be applied to other products such as silicon wafers or wafers that require a passivation film to be deposited on the stacked cross-section.

[0050] The above are only implementation methods of the present application, and are not intended to limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. An atomic layer deposition coating method, characterized in that: The coating method comprises at least one coating cycle process, wherein the coating cycle process comprises: Introducing a first process gas into a reaction device containing a substrate, wherein the first process gas includes a first reaction gas and an inert gas, and the first process gas is introduced for a time period ranging from 0.1s to 5s; Closing the reaction device to allow the first process gas to diffuse and adsorb onto the surface of the substrate to be coated; performing a first purge treatment on the reaction device; Introducing a second process gas into the reaction device, wherein the second process gas includes a second reaction gas and the inert gas, and the second process gas is introduced for a duration ranging from 0.1s to 5s; Closing the reaction device to allow the second process gas to diffuse and adsorb onto the surface of the substrate to be coated; The reaction device is subjected to a second purge treatment.

2. The coating method according to claim 1, characterized in that: Before entering the first coating cycle process, the coating method further comprises: The reaction device is subjected to a vacuum pumping process, and when the first process gas is subsequently introduced into the reaction device, the vacuum pumping process is stopped.

3. The method according to claim 2, characterized in that The step of performing a first purge treatment on the reaction device comprises: Turning on the vacuum pump to vacuum the reaction device; During the gas extraction process, the inert gas is introduced into the reaction device at least twice, wherein the gas inlet of the reaction device is closed between two adjacent introductions of the inert gas.

4. The method according to claim 3, characterized in that Before the step of introducing the second process gas into the reaction device, the method further includes: closing the vacuum pump.

5. The method according to any one of claims 1 to 4, characterized in that: The step of performing a second purge treatment on the reaction device comprises: Turning on the vacuum pump to vacuum the reaction device; During the gas extraction process, the inert gas is introduced into the reaction device at least twice, wherein the gas inlet of the reaction device is closed between two adjacent introductions of the inert gas.

6. The method according to any one of claims 1 to 4, characterized in that: The step of closing the reaction device to allow the first process gas to diffuse and adsorb onto the surface of the substrate to be coated includes: The reaction device is closed for 0.1s to 10s to allow the first process gas to diffuse and adsorb onto the surface of the substrate to be coated; and / or, The step of closing the reaction device to allow the second process gas to diffuse and adsorb onto the surface of the substrate to be coated includes: The reaction device is closed for 0.1s to 10s to allow the second process gas to diffuse and adsorb onto the surface of the substrate to be coated.

7. The method according to claim 1, characterized in that The temperature in the reaction device ranges from 100°C to 400°C.

8. The method according to claim 1, characterized in that The first reaction gas includes any one of trimethylaluminum, titanium tetrachloride or hafnium tetrachloride.

9. The method according to claim 1, characterized in that: The second reaction gas includes any one of water vapor, titanium nitride or hafnium dioxide.

10. The method according to claim 1, characterized in that The inert gas includes any one of nitrogen, argon, helium or neon.