Adjustable optical waveguide based on ferroelectric domain electro-optical effect

Through the domain structure and domain reversal process, the domain wall of the ferroelectric crystal is modulated by electric field, and the ferroelectric domain electro-optical effect is realized, solving the problems of complex and high cost of waveguide preparation in the prior art, and achieving simple and low-cost possible Dimming waveguide improves the flexibility and efficiency of laser transmission.

CN119045260AActive Publication Date: 2024-11-29NANJING NANZHI INST OF ADVANCED OPTOELECTRONIC INTEGRATION NANJING
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411180424.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-29
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

In the prior art, the preparation process of ferroelectric crystal waveguides is complex, expensive, and requires a high modulation voltage, making it difficult to achieve simple and low-cost dimmable optical waveguides.

Method used

Using a domain structure, positive and negative domains are formed through the domain inversion process, metal electrodes are used to conduct conduction with the domain wall, and an electric field is generated by applying voltage to generate an electric field, achieving an electro-optical effect, increasing the refractive index and achieving total reflection constraints of the laser, forming an adjustable Planar or bar waveguide.

Benefits of technology

It realizes a dimmable optical waveguide with simple preparation process and low cost, reduces the modulation voltage, and improves the flexibility and efficiency of laser transmission.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119045260A_ABST
    Figure CN119045260A_ABST
Patent Text Reader

Abstract

The invention discloses a ferroelectric domain electro-optical effect-based adjustable optical waveguide, which comprises a domain structure, a first domain wall, a second domain wall, a positive electrode, a negative electrode and an insulating layer, and is characterized in that the domain structure is divided into positive domains and negative domains, the negative domains are clamped in the middle, two sides are respectively provided with one positive domain, and the first domain wall and the second domain wall are respectively formed at the junctions of the positive domains and the negative domains; the first domain wall and the second domain wall are covered with metal electrodes, the metal electrodes are communicated with the first domain wall and the second domain wall, voltage is applied to the positive electrode and the negative electrode so that an electric field can be applied to the negative domain, total reflection is generated in the negative domain to restrain the laser, when the voltage is very small, the waveguide disappears, and modulation of transmission of the laser in the waveguide is achieved. According to the invention, electric field modulation is carried out, a photoelectric effect is generated and a reversed crystal refractive index between domain walls is increased by utilizing the domain wall conduction characteristic of the ferroelectric crystal, so that a planar or strip-shaped waveguide is formed, the preparation process is simple, the cost is low, and modulation of laser in waveguide transmission is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an adjustable optical waveguide, in particular to an adjustable optical waveguide based on ferroelectric domain electro-optical effect. Background Art

[0002] The electro-optic effect can be regulated by an electric field, and a change in the refractive index can be produced through the Pockels effect or the Pockels cell effect. Although the change in the refractive index caused by the electric field is very small, it can be accurately displayed and measured by interference and other methods, and has led to many important applications, such as optical communication, ranging, display, information processing, and sensors. Most of the commonly used electro-optic crystals are ferroelectric crystals, such as KDP, KDA, KTP, LiNbO3, LiTaO3, etc. In order to produce a sufficiently large electro-optic effect, the commonly used bulk crystals require a higher modulation voltage, usually several thousand volts to tens of thousands of volts. In order to reduce the modulation voltage and increase the modulation speed, waveguides can be prepared on the crystal, such as buried proton exchange waveguides, titanium diffusion waveguides, or ridge waveguides. By shortening the distance between the positive and negative electrodes to increase the electric field strength and reduce the voltage, the modulation voltage can be reduced to less than a few volts. However, the light-passing area and power of the strip waveguide are limited by the cross-sectional area, and the voltage applied to the planar waveguide requires a large area of ​​conductive electrodes to be embedded in the material, which makes the preparation process complicated and costly.

[0003] In nonlinear optics, one phase matching method of ferroelectric crystals is quasi-phase matching (QPM). The characteristic of this phase matching is that it utilizes the inversion characteristics of ferroelectric domains in ferroelectrics to perform periodic ferroelectric domain inversion, thereby compensating for the phase mismatch caused by the nonlinear coupling process. How to form a planar or strip waveguide with simple preparation process, low cost and adjustable laser transmission is an urgent problem to be solved. Summary of the invention

[0004] Purpose of the invention: The purpose of the present invention is to provide a tunable optical waveguide based on the electro-optic effect of ferroelectric domains.

[0005] Technical solution: The present invention includes a domain structure, a first domain wall, a second domain wall, a positive electrode, a negative electrode and an insulating layer. The domain structure is divided into a positive domain and a negative domain. The negative domain is sandwiched in the middle, and a positive domain is arranged on each side. The first domain wall and the second domain wall are formed at the junction of the positive domain and the negative domain, respectively. The first domain wall and the second domain wall are covered with metal electrodes, and the metal electrodes are conductively connected to the first domain wall and the second domain wall. By applying voltage to the positive electrode and the negative electrode, an electric field is applied to the negative domain, and an electro-optical effect is generated under the action of the electric field. The positive and negative voltages are set to the crystal axis so that the refractive index of the electro-optical effect increases and is greater than the refractive index of the positive domains on both sides, and total reflection is generated in the negative domain to constrain the laser. When the voltage is zero or the voltage is very small, the waveguide disappears, thereby realizing the modulation of the laser transmission in the waveguide.

[0006] Furthermore, the positive domain and the negative domain are both ferroelectric crystals, and the ferroelectric crystals include any one of lithium niobate, lithium tantalate and potassium titanyl phosphate.

[0007] Furthermore, the domain structure is domain-inverted through a domain inversion process, the inverted portion is called a negative domain, and the uninverted portion is called a positive domain.

[0008] Furthermore, the covered area under the positive electrode is a positive domain, and the uncovered area is a negative domain.

[0009] Furthermore, the domain inversion process adopts any one of a room temperature electric field polarization method, a growth stripe method and a poly-sheet multi-domain method.

[0010] Furthermore, the structural size range of the domain inversion is: domain inversion thickness 0.1μm≤D≤100μm; waveguide width 1μm≤H≤10mm; positive and negative electrode thickness 1nm≤T≤100μm.

[0011] Furthermore, the positive and negative voltages range from 1V to 1000V.

[0012] Furthermore, the crystal axis is a direction selected according to the electro-optic coefficient of the material so as to increase the refractive index of the domain inversion part.

[0013] Furthermore, the waveguide includes but is not limited to curved, circular and crossed structures.

[0014] Furthermore, the positive electrode and the negative electrode are insulated and filled with insulating material.

[0015] Beneficial effects: Compared with the prior art, the present invention has the following significant advantages: utilizing the conductive properties of the domain walls of ferroelectric crystals to perform electric field modulation, generate a photoelectric effect, increase the inverted crystal refractive index between domain walls, thereby forming a planar or strip waveguide, with a simple preparation process and low cost, and realizes the modulation of laser in waveguide transmission. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a structural schematic diagram of the present invention;

[0017] Figure 2 It is a cross-sectional schematic diagram of the present invention;

[0018] Figure 3 Schematic diagram of the 2×2 waveguide beam splitter structure. DETAILED DESCRIPTION

[0019] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.

[0020] like Figure 1As shown, the present invention includes a domain structure, a first domain wall 1, a second domain wall 2, a positive electrode 5, a negative electrode 6 and an insulating layer 7. The domain structure is divided into a positive domain 3 and a negative domain 4. The negative domain 4 is sandwiched in the middle, and a positive domain 3 is arranged on each side. The first domain wall 1 and the second domain wall 2 are formed at the junction of the positive domain 3 and the negative domain 4, respectively. The first domain wall 1 and the second domain wall 2 are covered with metal electrodes, and the metal electrodes are conductively connected to the first domain wall 1 and the second domain wall 2. By applying voltage to the positive electrode 5 and the negative electrode 6, an electric field is applied to the negative domain 4, and an electro-optical effect is generated under the action of the electric field. The positive and negative voltages are set to the crystal axis, so that the refractive index of the electro-optical effect increases and is greater than the refractive index of the positive domains 3 on both sides, and total reflection is generated in the negative domain 4 to constrain the laser. When the voltage is zero or the voltage is very small, the waveguide disappears, thereby realizing the modulation of the laser transmission in the waveguide.

[0021] The optical material used to prepare the present invention is a ferroelectric crystal, such as lithium niobate (LiNbO3), lithium tantalate (LiTaO3), potassium titanyl phosphate (KTiOPO4), etc., which can be domain-reversed by room temperature electric field polarization. As shown in the figure below, the reversed part is called the negative domain, and the unreversed part is called the positive domain. A domain wall with a certain conductivity is formed between the positive domain and the negative domain.

[0022] The present invention covers metal electrodes on the two domain walls of the negative domain, and applies voltage through the metal electrodes and the domain walls. Under the action of the voltage, the domain walls are turned on so that an electric field is applied to the negative domain, and an electro-optical effect is generated under the action of the electric field. By selecting appropriate positive and negative voltages and appropriate directions of the crystal axis, the refractive index of the electro-optical effect is increased and is greater than the refractive index of the positive domains on both sides, thereby generating total reflection in the negative domain to confine the laser.

[0023] In addition, the waveguide is formed when voltage is applied and disappears when the voltage is zero or very small. Therefore, this characteristic can be used to realize the modulation of laser transmission in the waveguide. When the waveguide is formed, the tail end outputs laser, and when the waveguide disappears, the light intensity at the tail end is very weak, forming an intensity modulation effect of the output laser.

[0024] like Figure 2 The figure shows a cross-sectional schematic diagram of the present invention, wherein the thickness of the positive and negative electrodes is T, the width of the waveguide is H, and the thickness of the waveguide is D. Lithium niobate is a uniaxial crystal, whose optical axis c-axis is along the Z direction, and the refractive index ellipsoids in the X and Y directions are symmetrical. In order to maintain insulation between the positive and negative electrodes, insulating materials such as photoresist are used for filling.

[0025] The above-mentioned ferroelectric materials include lithium niobate (LiNbO3), lithium tantalate (LiTaO3), potassium titanyl phosphate (KTiOPO4), etc., and the preferred material is lithium niobate.

[0026] The above-mentioned ferroelectric domain inversion process includes room temperature electric field polarization method, growth stripe method, poly-sheet multi-domain method, etc., and room temperature electric field polarization method is preferred.

[0027] The structural size range of the domain inversion is: domain inversion thickness 0.1μm≤D≤100μm; waveguide width 1μm≤H≤10mm; positive and negative electrode thickness 1nm≤T≤100μm. The preferred size is D≈1μm, H≈1mm, T≈100nm.

[0028] The voltage applied to the positive and negative electrodes is in the range of 1V to 1000V.

[0029] According to the electro-optic effect, under the action of an external electric field E, the refractive index principal axis of the lithium niobate crystal changes, causing the refractive index to change in all directions. According to the linear electro-optic effect matrix of lithium niobate, an electric field E is applied along the X-axis direction, then E y =E x =E, the refractive index ellipsoid equation of lithium niobate crystal becomes:

[0030]

[0031] After two coordinate transformations and ignoring the second-order small quantity, the new refractive index can be obtained as follows:

[0032]

[0033] n′ z =n e (4)

[0034] like Figure 1 As shown, the polarization direction of the input light is in the Y direction, so here we only focus on equation (3). In equation (3), the electric field in the X direction is generated by the charges on the positive and negative domain walls. After applying voltage to the positive and negative electrodes, the positive and negative charges are distributed on the adjacent domain walls, thus forming an electric field E in the X direction. The refractive index changes according to equation (3), generating electro-optic modulation

[0035] The axial direction of the above crystal is, according to the sign of the electro-optic coefficient of the material, the direction in which the refractive index of the domain inversion part is increased is selected to apply voltage. For example, the thickness of the domain inversion of lithium niobate crystal D = 1μm, the electro-optic coefficient γ 22 =3.4pm / v, so when the voltage difference between the positive and negative electrodes is V=1000V, according to formula (5)

[0036]

[0037] It can be concluded that this increase in refractive index is similar to that of a proton exchange waveguide, and can form a waveguide similar to that of a proton exchange or titanium diffusion waveguide.

[0038] In addition, the waveguide can be formed into curved, circular, cross-shaped structures, such as the curved cross-shaped waveguide shown in the figure below, which forms a 2×2 waveguide beam splitter after voltage is applied. The negative domain part in the figure is prepared by making a beam splitter mask, photolithography, and room temperature electric field polarization method. The covered area under the prepared positive electrode is the positive domain, and the uncovered area is the negative domain area. The arrangement of the above electrodes is as follows Figure 3 As shown, a curved waveguide with an increased refractive index is formed in a waveguide beam splitter.

[0039] Embodiment 1:

[0040] Using lithium niobate as the substrate, the room temperature electric field polarization process is carried out. Figure 1 The domains shown are reversed and retained Figure 1 The dimensions of the above-mentioned processing structure are: waveguide width D = 1μm, waveguide width H = 1mm, electrode material is copper, and coating thickness is 100nm. Figure 1 A 1000V voltage is applied to the positive electrode shown, and the negative electrode is grounded, forming a high-intensity electric field in the domain inversion part. The input laser wavelength is 1.5μm, and the polarization state is along the X axis. The refractive index is increased by about 0.018 through the electro-optical effect. Waveguide coupling is performed through the optical fiber, and the light intensity at the output port is approximately equal to the input light intensity; when the voltage is removed, the electro-optical effect disappears, the waveguide disappears, the laser cannot be transmitted in the waveguide, and the light intensity at the output port is approximately equal to zero, thus forming voltage-controlled light intensity modulation.

[0041] Embodiment 2:

[0042] like Figure 3 As shown, the 2×2 waveguide is prepared according to the above steps. Figure 3 Apply positive and negative voltages to the positive and negative electrodes to form Figure 3 The 2×2 waveguide coupler shown. After all voltages are removed, Figure 3 The waveguide structure shown disappears, and the waveguide coupler disappears. Only the corresponding voltage is applied to the positive electrode 1, the negative electrode 5, and the negative electrode 2, forming a structure with only the left curved waveguide, and only the left input port to the left output port has an output signal. Only the corresponding voltage is applied to the positive electrode 1, the negative electrode 5, the positive electrode 3, and the negative electrode 4, forming a curved strip waveguide from the lower left to the upper right, and only the left input port to the right output port has an output signal.

[0043] Through the combination of the above-mentioned straight waveguide, 2×2 coupler and other similar waveguide devices, electrical signals can be converted into optical signals to realize a hybrid electro-optical chip for electrical signal operation and optical signal operation.

Claims

1. A tunable optical waveguide based on ferroelectric domain electro-optical effect, characterized in that: The invention comprises a domain structure, a first domain wall (1), a second domain wall (2), a positive electrode (5), a negative electrode (6) and an insulating layer (7). The domain structure is divided into a positive domain (3) and a negative domain (4). The negative domain (4) is sandwiched in the middle, and a positive domain (3) is arranged on each side. The first domain wall (1) and the second domain wall (2) are formed at the junction of the positive domain (3) and the negative domain (4). The first domain wall (1) and the second domain wall (2) are covered with metal electrodes. The metal electrodes are connected to the first domain wall (1) and the second domain wall (2). By applying voltage to the positive electrode (5) and the negative electrode (6), an electric field is applied to the negative domain (4), and an electro-optical effect is generated under the action of the electric field. The positive and negative voltages are arranged in the crystal axis so that the refractive index of the electro-optical effect increases and is greater than the refractive index of the positive domains (3) on both sides, and total reflection is generated in the negative domain (4) to constrain the laser. When the voltage is zero or the voltage is very small, the waveguide disappears, thereby realizing the modulation of the laser transmission in the waveguide.

2. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The positive domain (3) and the negative domain (4) are both ferroelectric crystals, and the ferroelectric crystals include any one of lithium niobate, lithium tantalate and potassium titanyl phosphate.

3. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The domain structure is domain-inverted by a domain inversion process, and the inverted portion is called a negative domain (4), and the uninverted portion is called a positive domain (3).

4. The tunable optical waveguide based on ferroelectric domain electro-optical effect according to claim 1, characterized in that: The covered area below the positive electrode (5) is a positive domain (3), and the uncovered area is a negative domain (4).

5. The tunable optical waveguide based on ferroelectric domain electro-optical effect according to claim 3, characterized in that: The domain inversion process adopts any one of a room temperature electric field polarization method, a growth stripe method and a poly-sheet multi-domain method.

6. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 3, characterized in that: The structural size range of the domain inversion is: domain inversion thickness 0.1 μm ≤ D ≤ 100 μm; Waveguide width 1μm≤H≤10mm; positive and negative electrode thickness 1nm≤T≤100μm.

7. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The positive and negative voltages range from 1V to 1000V.

8. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The crystal axis is a direction selected according to the electro-optic coefficient of the material so as to increase the refractive index of the domain inversion part.

9. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The waveguides include, but are not limited to, curved, circular, and crossed structures.

10. The tunable optical waveguide based on ferroelectric domain electro-optic effect according to claim 1, characterized in that: The positive electrode (5) and the negative electrode (6) are insulated and filled with insulating material.

Citation Information

Patent Citations

  • Electro-optic element

    JP1998039265A

  • Ridge type optical waveguide element and its manufacture

    JP1998206810A

  • Directional coupler

    JP2000347149A

  • Optical control device

    JP2003098494A

  • Domain-structured ferroic element, method and apparatus for generating and for controlling the electrical conductivity of domain walls at room temperature in the elements and applications of the element

    WO2011120495A1