Power metal oxide semiconductor field effect transistor and electronic circuit
By designing the drain side of silicon germanium heterojunction structure and oxide layer in metal oxide semiconductor field effect transistors, the problem of poor reverse recovery performance of traditional devices is solved, and shorter reverse recovery time and lower Reverse charge recovery further improves the device's reverse recovery performance.
Patent Information
- Application Number
- CN202411166938.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-29
AI Technical Summary
The reverse recovery performance of traditional metal oxide semiconductor field effect transistors is poor. The existing improvement methods are mainly concentrated on the source side and drift region, and are rarely improved from the drain side, resulting in insufficient reverse recovery performance.
A power metal oxide semiconductor field effect transistor is designed, including drain metal layer, silicon germanium heterojunction structure, conduction region, body region and heavily doped contact region, through the design of silicon germanium heterojunction structure and oxide layer , so as to make holes easier to enter the silicon germanium region from the drift region, thereby reducing the hole concentration in the drift region and improving the reverse recovery performance.
It realizes the effect of shorter reverse recovery time, shorter reverse recovery time, and lower reverse recovery charge, improves the reverse recovery performance of C-MOS, and can be combined with existing source side improvement technology to further Improve the reverse recovery performance of the device.
Smart Images

Figure CN119050145A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of power semiconductor electronic devices, and in particular to a power metal oxide semiconductor field effect transistor and an electronic circuit. Background Art
[0002] With the advancement of power integrated circuit technology, the field of power semiconductor devices is also developing rapidly. These devices usually operate in the third quadrant of the current-voltage characteristic, which places high standards on the reverse recovery characteristics of the built-in diode. The body diode in the traditional vertical diffused metal oxide semiconductor field effect transistor (C-MOS) is a bipolar structure. Due to the presence of a large number of minority carriers inside the body diode, large losses will be generated during the reverse recovery process, so its reverse recovery performance is relatively poor.
[0003] At present, there are some methods for improving the reverse recovery performance of traditional metal oxide semiconductor field effect transistors, such as introducing a Schottky diode as a built-in diode on the source side, changing the carrier lifetime by irradiation, etc. to improve the reverse recovery performance of the device.
[0004] However, most of the current methods focus on solving the problem on the source side or drift region of the metal oxide semiconductor field effect transistor, and rarely consider improving the drain side to further improve the reverse recovery performance of the device. Therefore, how to improve the reverse recovery performance of C-MOS from the drain side is an urgent problem to be solved. Summary of the invention
[0005] In view of the above-mentioned shortcomings of the prior art, the present invention provides a power metal oxide semiconductor field effect transistor and an electronic circuit to solve at least one of the problems in the prior art.
[0006] To achieve the above and other purposes, the present invention provides a power metal oxide semiconductor field effect transistor, comprising:
[0007] Drain metal layer 1;
[0008] A germanium-silicon heterojunction structure disposed on the drain metal layer 1;
[0009] A conducting region 5 disposed on the germanium-silicon heterojunction structure;
[0010] A body region 6 disposed on the germanium-silicon heterojunction structure and located at both sides of the conductive region 5;
[0011] heavily doped contact regions 7 respectively embedded in the body regions 6;
[0012] An oxide layer 8 disposed on the conductive region 5 and in contact with the body region 6 and the heavily doped contact region 7;
[0013] A heavily doped gate polysilicon layer 9 wrapped in the oxide layer 8;
[0014] A source metal layer 10 covers the oxide layer 8 .
[0015] In one embodiment of the present invention, the germanium-silicon heterojunction structure includes:
[0016] A heavily doped silicon germanium layer 3 is disposed on the drain metal layer 1 ; and a lightly doped drift region 4 is disposed on the heavily doped silicon germanium layer 3 .
[0017] In one embodiment of the present invention, the germanium-silicon heterojunction structure further includes:
[0018] The heavily doped substrate layer 2 is disposed between the heavily doped silicon-germanium layer 3 and the lightly doped drift region 4 .
[0019] In one embodiment of the present invention, the oxide layer 8 contacts a portion of the body region 6 , and the oxide layer 8 contacts a portion of the heavily doped contact region 7 .
[0020] In one embodiment of the present invention, the source metal layer 10 is in contact with the non-contact region between the oxide layer 8 and the body region 6 , and is in contact with the non-contact region between the oxide layer 8 and the heavily doped contact region 7 .
[0021] In one embodiment of the present invention, the thickness of the oxide layer (8) in contact with the body region 6, the heavily doped contact region 7, and the conductive region 5 is in the range of 30-80 nm; the doping concentration of the conductive region 5 is in the range of 5×10 15 cm -3 Up to 3×10 16 cm -3 ; The doping concentration of the lightly doped drift region 4 ranges from 8×10 14 cm -3 Up to 2×10 15 cm -3 ; The doping concentration of the heavily doped gate polysilicon layer 9 ranges from 1×10 19 cm -3 Up to 1×10 20 cm -3 .
[0022] In one embodiment of the present invention, the material of the heavily doped silicon germanium layer 3 is SiGe, and the doping concentration and the molar composition of the Ge element are adjustable.
[0023] In one embodiment of the present invention, the doping concentration of the heavily doped germanium silicon layer 3 is in the range of 1×10 19 cm-3 Up to 5×10 19 cm -3 The molar composition of the Ge element ranges from 0.1 to 0.8, and the thickness of the heavily doped germanium silicon layer 3 ranges from 0.5 μm to 2.5 μm.
[0024] In one embodiment of the present invention, the doping concentration of the heavily doped germanium silicon layer 3 is in the range of 1×10 18 cm -3 Up to 1×10 19 cm -3 The molar composition of the Ge element ranges from 0.1 to 0.5, and the thickness of the heavily doped germanium silicon layer 3 ranges from 0.5 μm to 1 μm.
[0025] To achieve the above objectives and other objectives, the present invention provides an electronic circuit, which includes the field effect transistor.
[0026] Beneficial effects of the present invention:
[0027] A power metal oxide semiconductor field effect transistor of the present invention comprises: a drain metal layer 1; a germanium silicon heterojunction structure arranged on the drain metal layer 1; a conduction region 5 arranged on the germanium silicon heterojunction structure; a body region 6 arranged on the germanium silicon heterojunction structure and respectively located on both sides of the conduction region 5; a heavily doped contact region 7 respectively embedded in the body region 6; an oxide layer 8 arranged on the conduction region 5 and in contact with the body region 6 and the heavily doped contact region 7 at the same time; a heavily doped gate polysilicon layer 9 wrapped in the oxide layer 8; and a source metal layer 10 covering the oxide layer 8. When the transistor is subjected to a reverse voltage, that is, when the metal oxide semiconductor field effect transistor is operating in a reverse conduction state, holes injected from the source will flow to the drain; however, the heterojunction structure on the source side of the device will cause a difference in energy bands, making it easier for holes to enter the germanium silicon region from the inside of the drift region, thereby reducing the hole concentration inside the drift region and improving the reverse recovery performance. Compared with the existing metal oxide semiconductor field effect transistor, the field effect transistor of the present invention has the characteristics of smaller reverse recovery time, shorter reverse recovery time and lower reverse recovery charge, which improves the reverse recovery performance of C-MOS and can be adapted to the existing source side improvement technology to further improve the reverse recovery performance of the device.
[0028] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The drawings herein are incorporated into the specification and constitute a part of the specification, showing embodiments consistent with the present application, and together with the specification, are used to explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application, and for those of ordinary skill in the art, other drawings can be obtained based on these drawings without creative work. In the drawings:
[0030] Figure 1 It is a schematic diagram of the cross-sectional structure of an existing metal oxide semiconductor field effect transistor;
[0031] Figure 2 It is a schematic cross-sectional structure diagram of a power metal oxide semiconductor field effect transistor device according to an exemplary embodiment of the present application;
[0032] Figure 3 It is a schematic cross-sectional structure diagram of a power metal oxide semiconductor field effect transistor device according to an exemplary embodiment of the present application;
[0033] Figure 4 is a reverse recovery characteristic comparison diagram of an exemplary embodiment of the present application;
[0034] In the figure: drain metal layer 1, heavily doped substrate layer 2, heavily doped germanium silicon layer 3, lightly doped drift region 4, conduction region 5, body region 6, heavily doped contact region 7, oxide layer 8, heavily doped gate polysilicon layer 9, source metal layer 10. DETAILED DESCRIPTION
[0035] The following describes the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the following embodiments and features in the embodiments can be combined with each other without conflict.
[0036] It should be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present invention, and thus the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0037] Although the terms "first", "second", "A", "B", etc. may be used herein to describe various elements, these elements should not be limited by these terms and are only used to distinguish one element from another. For example, a first element may be referred to as a second element, and similarly, a second element may be referred to as a first element without departing from the scope of the following technology. The term "and / or" includes a combination of multiple related items or any item in the multiple related items.
[0038] As used herein, unless the context indicates otherwise, the singular form is intended to include the plural form, and it will be understood that the term "comprising" means the presence of stated features, quantities, steps, operations, elements, or combinations thereof, but does not exclude the presence or addition of one or more other features, quantities, steps, operations, elements, components, or combinations thereof.
[0039] Before describing the drawings in detail, it is intended to clarify that the division of components in this specification is divided only by the main function of each component. That is, two or more components to be described below can be combined into one component, or can be divided into two or more components according to more detailed functions. In addition to the main function of the component, each component to be described below can also perform some or all of the functions of other components, and some of the main functions of each component can be exclusively performed by other components.
[0040] With the advancement of power integrated circuit technology, the field of power semiconductor devices is also developing rapidly. These devices usually operate in the third quadrant of the current-voltage characteristic, which places high standards on the reverse recovery characteristics of the built-in diode. The body diode in the traditional vertical diffused metal oxide semiconductor field effect transistor (C-MOS) is a bipolar structure. Due to the presence of a large number of minority carriers inside the body diode, large losses will be generated during the reverse recovery process, so its reverse recovery performance is relatively poor.
[0041] At present, there are some methods for improving the reverse recovery performance of traditional metal oxide semiconductor field effect transistors, such as introducing a Schottky diode as a built-in diode on the source side, changing the carrier lifetime by irradiation, etc. to improve the reverse recovery performance of the device.
[0042] However, most of the current methods focus on solving the problem on the source side or drift region of the metal oxide semiconductor field effect transistor, and rarely consider improving the drain side to further improve the reverse recovery performance of the device. Therefore, how to improve the reverse recovery performance of C-MOS from the drain side is an urgent problem to be solved.
[0043] See also Figure 2 , Figure 2This is a schematic diagram of the cross-sectional structure of a power metal oxide semiconductor field effect transistor device according to an embodiment of the present application. Figure 2 The power metal oxide semiconductor field effect transistor includes:
[0044] Drain metal layer 1;
[0045] A germanium-silicon heterojunction structure disposed on the drain metal layer 1;
[0046] A conducting region 5 disposed on the germanium-silicon heterojunction structure;
[0047] A body region 6 disposed on the germanium-silicon heterojunction structure and located at both sides of the conductive region 5;
[0048] heavily doped contact regions 7 respectively embedded in the body regions 6;
[0049] An oxide layer 8 disposed on the conductive region 5 and in contact with the body region 6 and the heavily doped contact region 7;
[0050] A heavily doped gate polysilicon layer 9 wrapped in the oxide layer 8;
[0051] A source metal layer 10 covers the oxide layer 8 .
[0052] Compared with the existing metal oxide semiconductor field effect transistor, the field effect transistor of the present invention has the characteristics of smaller reverse recovery time, shorter reverse recovery time and lower reverse recovery charge, which improves the reverse recovery performance of C-MOS and can be adapted to the existing source side improvement technology to further improve the reverse recovery performance of the device.
[0053] The following is a detailed description of the various parts that make up the transistor.
[0054] The drain metal layer 1, the germanium-silicon heterojunction structure, the conductive region 5, the body region 6, the heavily doped contact region 7, and the oxide layer 8 all have a first plane and a second plane; preferably, the first plane and the second plane are parallel to each other and the first plane is above the second plane.
[0055] The germanium-silicon heterojunction structure is arranged on the drain metal layer 1 , wherein a first plane of the drain metal layer contacts a second plane of the germanium-silicon heterojunction structure to form a contact surface.
[0056] The conductive region 5 is disposed on the germanium-silicon heterojunction structure, and the second plane of the conductive region contacts the first plane of the germanium-silicon heterojunction structure; preferably, the conductive region 5 is disposed in the middle of the germanium-silicon heterojunction structure.
[0057] An integral region 6 is provided on both sides of the conductive region 5, the body region 6 contacts the conductive region 5, a first plane of the body region 6 and a first plane of the conductive region 5 are on the same plane, and a second plane of the conductive region 5 contacts the first plane of the germanium-silicon heterojunction structure.
[0058] A heavily doped contact region 7 is provided in each body region 6; specifically, the heavily doped contact region 7 extends from the first plane of the body region 6 into the body region 6 and does not contact the second plane of the body region 6. It should be noted that the first plane of the heavily doped contact region 7 is on the same plane as the first plane of the body region 6; and except that the first plane of the heavily doped contact region 7 is on the same plane as the first plane of the body region 6, other planes do not contact each other; for example, the second plane of the heavily doped contact region 7 is not in contact with the second plane of the body region 6, and the two surfaces close to the heavily doped contact region 7 and the body region 6 are not in contact either, such as Figure 2 As shown, the left side wall of the heavily doped contact region 7 does not contact the left side wall of the body region 6 , and the right side wall of the heavily doped contact region 7 does not contact the right side wall of the body region 6 .
[0059] The oxide layer 8 is disposed on the conductive region 5, and its second plane is in contact with the first plane of the conductive region 5, and is also in contact with the first plane of the body region 6 and the first plane of the heavily doped contact region 7; it should be noted that the oxide layer 8 is only partially in contact with the heavily doped contact region 7, and does not completely cover the first plane of the heavily doped contact region 7. The portion of the oxide layer in contact with the heavily doped contact region 7 and the body region 6 is a contact surface, and the portion not in contact with the heavily doped contact region 7 and the body region 6 is a non-contact surface.
[0060] When the transistor operates in a forward conduction state, a current conduction channel is formed at the contact between the oxide layer 8 and the body region 6 .
[0061] The heavily doped gate polysilicon layer 9 is disposed in the oxide layer 8 and is completely wrapped by the oxide layer 8 .
[0062] The source metal layer 10 covers the oxide layer 8. Preferably, the source metal layer 10 contacts the first plane of the heavily doped contact region 7 and the first plane of the body region 6. Specifically, the source metal layer 10 contacts the non-contact region between the oxide layer 8 and the body region 6, and contacts the non-contact region between the oxide layer 8 and the heavily doped contact region 7.
[0063] See also Figure 2 In the embodiment of the present application, the germanium-silicon heterojunction structure includes: a heavily doped germanium-silicon layer 3 disposed on the drain metal layer 1; and a lightly doped drift region 4 disposed on the heavily doped germanium-silicon layer 3.
[0064] It should be noted that the heavily doped silicon germanium layer 3 and the lightly doped drift region 4 both include a first plane and a second plane, the first plane is above the second plane, and the first plane and the second plane are parallel to each other. The second plane of the heavily doped silicon germanium layer 3 contacts the first plane of the drain metal layer 1, the first plane of the heavily doped silicon germanium layer 3 contacts the second plane of the lightly doped drift region 4, and the first plane of the lightly doped drift region 4 serves as the first plane of the silicon germanium heterojunction structure.
[0065] It should also be noted that the lightly doped drift region 4 and the heavily doped germanium silicon layer 3 constitute a heterojunction structure of the power metal oxide semiconductor field effect transistor in the reverse conduction working state, which is conducive to the discharge of holes from the drift region and improves the reverse recovery performance of the device. Among them, the material of the heavily doped germanium silicon layer 3 is SiGe, and the doping concentration and the molar composition of the Ge element are adjustable. The doping concentration ranges from 1×10 19 cm -3 Up to 5×10 19 cm -3 The molar composition of Ge ranges from 0.1 to 0.8. The thickness of the heavily doped first conductivity type germanium silicon layer 3 ranges from 0.5 μm to 2.5 μm.
[0066] See also Figure 3 In the embodiment of the present application, the germanium-silicon heterojunction structure further includes: a heavily doped substrate layer 2 disposed between the heavily doped germanium-silicon layer 3 and the lightly doped drift region 4 .
[0067] It should be noted that the heavily doped substrate layer 2 also includes a first plane and a second plane, the first plane is above the second plane and the first plane and the second plane are parallel to each other. The heavily doped substrate layer 2 is disposed on the drain metal layer 1 and the second plane of the heavily doped substrate layer 2 is in contact with the first plane of the drain metal layer 1, and the first plane of the heavily doped substrate layer 2 is in contact with the second plane of the heavily doped germanium silicon layer 3.
[0068] The lightly doped drift region 4 and the heavily doped germanium silicon layer 3 form a lightly doped silicon / heavily doped germanium silicon heterojunction structure; the heavily doped germanium silicon layer 3 and the heavily doped substrate layer 2 form a heavily doped germanium silicon / heavily doped silicon heterojunction structure; the lightly doped drift region 4, the heavily doped germanium silicon layer 3 and the heavily doped substrate layer 2 constitute a heterojunction structure of the power metal oxide semiconductor field effect transistor in the reverse conduction working state, which is conducive to the discharge of holes from the drift region and improves the reverse recovery performance of the device. Among them, the material of the heavily doped germanium silicon layer 3 is SiGe, and the doping concentration and the molar composition of the Ge element are adjustable. The doping concentration ranges from 1×10 18 cm -3 Up to 1×10 19 cm -3The molar composition of Ge is in the range of 0.1 to 0.5. The thickness of the heavily doped germanium silicon layer 3 is in the range of 0.5 μm to 1 μm.
[0069] In the embodiment of the present application, the thickness of the oxide layer 8 in contact with the body region 6, the heavily doped contact region 7, and the conductive region 5, that is, the oxide layer located below the heavily doped gate polysilicon layer 9, is in the range of 30-80 nm, preferably 50 nm; the doping concentration of the conductive region 5 is in the range of 5×10 15 cm -3 Up to 3×10 16 cm -3 ; The doping concentration of the lightly doped drift region 4 ranges from 8×10 14 cm -3 Up to 2×10 15 cm -3 ; The doping concentration of the heavily doped gate polysilicon layer 9 ranges from 1×10 19 cm -3 Up to 1×10 20 cm -3 .
[0070] Figure 4 The device of Example 1 and Figure 1 A comparison chart of reverse recovery characteristics of existing power metal oxide semiconductor field effect transistor devices;
[0071] Compared to Figure 1 The existing power MOSFET device structure, combined with Figure 4 The reverse recovery characteristics comparison diagram shows that the reverse recovery time of the present invention is smaller, the reverse recovery time is shorter, and the reverse recovery charge is lower.
[0072] In summary, a power metal oxide semiconductor field effect transistor of the present invention comprises: a drain metal layer 1; a germanium silicon heterojunction structure arranged on the drain metal layer 1; a conduction region 5 arranged on the germanium silicon heterojunction structure; a body region 6 arranged on the germanium silicon heterojunction structure and respectively located on both sides of the conduction region 5; a heavily doped contact region 7 respectively embedded in the body region 6; an oxide layer 8 arranged on the conduction region 5 and in contact with the body region 6 and the heavily doped contact region 7 at the same time; a heavily doped gate polysilicon layer 9 wrapped in the oxide layer 8; and a source metal layer 10 covering the oxide layer 8. When the transistor is subjected to a reverse voltage, that is, when the metal oxide semiconductor field effect transistor is operating in a reverse conduction state, the holes injected from the source will flow to the drain; however, the heterojunction structure on the source side of the device will cause a difference in the energy band, making it easier for holes to enter the germanium silicon region from the inside of the drift region, thereby reducing the hole concentration inside the drift region and improving the reverse recovery performance. Compared with the existing metal oxide semiconductor field effect transistor, the field effect transistor of the present invention has the characteristics of smaller reverse recovery time, shorter reverse recovery time and lower reverse recovery charge, which improves the reverse recovery performance of C-MOS and can be adapted to the existing source side improvement technology to further improve the reverse recovery performance of the device.
[0073] The present application provides an electronic circuit, the electronic circuit comprising: Figure 2 , 3 The field effect transistor shown.
[0074] It should be noted that the electronic circuit provided in this embodiment and the power metal oxide semiconductor field effect transistor provided in the above embodiment belong to the same concept, and the specific methods of the various components of the transistor of the electronic circuit have been described in detail in the power metal oxide semiconductor field effect transistor embodiment, which will not be repeated here.
[0075] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present invention. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A power metal oxide semiconductor field effect transistor, characterized in that: The field effect gold tube comprises: Drain metal layer (1); A germanium-silicon heterojunction structure arranged on the drain metal layer (1); A conducting region (5) disposed on the germanium-silicon heterojunction structure; Body regions (6) disposed on the germanium-silicon heterojunction structure and located respectively on both sides of the conduction region (5); heavily doped contact regions (7) respectively embedded in the body regions (6); An oxide layer (8) disposed on the conductive region (5) and in contact with the body region (6) and the heavily doped contact region (7); A heavily doped gate polysilicon layer (9) encapsulated in the oxide layer (8); A source metal layer (10) covers the oxide layer (8).
2. The power metal oxide semiconductor field effect transistor according to claim 1, characterized in that: The germanium-silicon heterojunction structure comprises: A heavily doped germanium silicon layer (3) disposed on the drain metal layer (1); A lightly doped drift region (4) is arranged on the heavily doped germanium silicon layer (3).
3. The power metal oxide semiconductor field effect transistor according to claim 2, characterized in that: The germanium-silicon heterojunction structure further includes: A heavily doped substrate layer (2) is arranged between the heavily doped germanium silicon layer (3) and the lightly doped drift region (4).
4. The power metal oxide semiconductor field effect transistor according to claim 1, characterized in that: The oxide layer (8) contacts a portion of the body region (6), and the oxide layer (8) contacts a portion of the heavily doped contact region (7).
5. The power metal oxide semiconductor field effect transistor according to claim 1, characterized in that: The source metal layer (10) contacts the non-contact region between the oxide layer (8) and the body region (6), and contacts the non-contact region between the oxide layer (8) and the heavily doped contact region (7).
6. The power metal oxide semiconductor field effect transistor according to claim 4, characterized in that: The thickness of the oxide layer (8) in contact with the body region (6), the heavily doped contact region (7), and the conductive region (5) is in the range of 30-80 nm; the doping concentration of the conductive region (5) is in the range of 5×10 15 cm -3 Up to 3×10 16 cm -3 ; The doping concentration of the lightly doped drift region (4) ranges from 8×10 14 cm -3 Up to 2×10 15 cm -3 The doping concentration of the heavily doped gate polysilicon layer (9) is in the range of 1×10 19 cm -3 Up to 1×10 20 cm -3 .
7. The power metal oxide semiconductor field effect transistor according to claim 2, characterized in that: The material of the heavily doped germanium silicon layer (3) is SiGe, and the doping concentration and the molar composition of the Ge element are adjustable.
8. The power metal oxide semiconductor field effect transistor according to claim 7, characterized in that: The doping concentration of the heavily doped germanium silicon layer (3) is in the range of 1×10 19 cm -3 Up to 5×10 19 cm -3 The molar composition of the Ge element ranges from 0.1 to 0.8, and the thickness of the heavily doped germanium silicon layer (3) ranges from 0.5 μm to 2.5 μm.
9. The power metal oxide semiconductor field effect transistor according to claim 7, characterized in that: The doping concentration of the heavily doped germanium silicon layer (3) is in the range of 1×10 18 cm -3 Up to 1×10 19 cm -3 The molar composition of the Ge element ranges from 0.1 to 0.5, and the thickness of the heavily doped germanium silicon layer (3) ranges from 0.5 μm to 1 μm.
10. An electronic circuit, characterized in that: The electronic circuit comprises a field effect transistor as claimed in any one of claims 1 to 9.