Magnesium alloy forging equipment capable of continuously heating and forging method
By introducing intermediate frequency heating coils and hydraulic rods into magnesium alloy forging equipment, continuous heating in forging molds is achieved, and the problem of rapid heat dissipation of magnesium alloys is solved, shortening the forging time and improving the quality of finished products.
Patent Information
- Application Number
- CN202411105091.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-08-13
AI Technical Summary
In the existing magnesium alloy processing technology, magnesium alloy dissipates rapidly, resulting in frequent furnace recovery and insulation, extending forging time and affecting quality.
A magnesium alloy forging equipment that can continuously heat is designed, using the intermediate frequency heating coil and hydraulic rod to realize self-heating in the forging mold, maintaining the high temperature state of the rod material in the molding cavity, and reducing the number of furnace insulation times.
It shortens the forging time, improves the plasticity of magnesium alloy, reduces the time and energy consumption required forging, and improves the quality of finished products.
Smart Images

Figure CN119056994A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of magnesium alloy processing, and in particular to a magnesium alloy forging device and a forging method capable of continuous heating. Background Art
[0002] Magnesium alloy is an alloy composed of magnesium and other elements. Its characteristics are: low density, high strength, large elastic modulus, good heat dissipation, good shock absorption, greater impact load bearing capacity than aluminum alloy, good resistance to organic and alkali corrosion, the main alloy elements are aluminum, zinc, manganese, cerium, thorium and a small amount of zirconium or cadmium, etc. The most widely used is magnesium aluminum alloy, followed by magnesium manganese alloy and magnesium zinc zirconium alloy, which are widely used in portable equipment and the automotive industry.
[0003] As disclosed in a Chinese patent: A magnesium alloy forging forming method and equipment, application number: CN202310541404.0, including a frame, a stamping machine and a forging die, the forging die includes a bottom plate, a lower template, a die sleeve, a connecting plate, a pad, an upper die, a punch piece, an upper Latin and a lower Latin, the upper Latin is removed, the stamping machine is started, the upper template, the pad and the connecting plate are moved upward, and the punch piece is separated from the stamping cavity, and the stamping cavity and the forming cavity are sprayed with oil-based graphite lubricant for lubrication, the magnesium alloy bar is placed in the stamping cavity, the stamping machine is started, and the bar is extruded and forged by the punch piece, after the forming is completed, the upper Latin is assembled, the lower Latin is taken out, and then the stamping machine is started, so that the upper template, the pad, the connecting plate and the die sleeve are moved upward, and the formed parts on the lower template are taken out. With the above structure, there is no need to perform multiple forming and heating on the magnesium alloy forgings, thereby reducing the impact on the performance of the magnesium alloy forgings.
[0004] However, in the above technical scheme, the current magnesium alloy processing is mostly to put the heated magnesium alloy into a mold, and then use forging equipment to extrude and forge the heated magnesium alloy. However, the magnesium alloy dissipates heat quickly, which results in that each time the magnesium alloy is extruded and forged, it is necessary to put the magnesium alloy back into the heating furnace from time to time for reheating and insulation. Only after the reheating and insulation is completed can the forging be continued. This not only prolongs the time required for forging, but also repeatedly reheating the magnesium alloy will cause the internal grains of the magnesium alloy to grow, affecting the quality of the magnesium alloy. Summary of the invention
[0005] In view of the deficiencies in the prior art, the present invention provides a magnesium alloy forging device and a forging method capable of continuous heating, which can effectively solve the problems in the background technology.
[0006] To achieve the above objectives, the present invention is implemented through the following technical scheme: a magnesium alloy forging equipment capable of continuous heating, comprising a base and a plurality of support columns, the base is provided with a forging die and a mounting groove, input wires and output wires are respectively provided on both sides of the forging die, a power supply is provided in the mounting groove, the forging die is connected to the power supply through the input wire, a top cover is provided on one side above the support column, and a hydraulic rod is provided on the top cover.
[0007] Preferably, the forging die includes a die base, an upper die plate is arranged on one side above the die base, a die sleeve is arranged between the upper die plate and the die base, two first Latin grooves are arranged on the outer wall surface on the side where the die base and the die sleeve are close to each other, two second Latin grooves are arranged on the outer wall surface on the side where the upper die plate and the die sleeve are close to each other, a lower Latin and an upper Latin are respectively arranged in the first Latin groove and the second Latin groove, a punch is arranged on the upper die plate, and the punch is movably arranged in a feed groove located on the die sleeve, and the feed groove and the die base are closed to form a forming cavity.
[0008] Preferably, a first power connector is fixedly provided on the inner wall below the first Latin groove on the mold base, a second power connector is fixedly provided on the inner wall above the first Latin groove on the mold sleeve, first card slots are provided on the upper and lower inner walls of the second Latin groove, a Latin structure and a medium frequency heating coil are provided on the mold sleeve, and the medium frequency heating coil surrounds the molding cavity.
[0009] Preferably, the upper template is fixedly connected to the hydraulic rod, and the second power connector is located directly above the second power connector of the first Latin slot.
[0010] Preferably, the lower Latin includes a Latin base, a slide groove is arranged on the Latin base, a first slide column and a second slide column are slidably arranged in the slide groove, a first round ball and a second round ball are fixedly arranged on the side of the first slide column and the second slide column away from each other, two insulating partitions and a conductive column are arranged between the first slide column and the second slide column, and a first spring is fixedly arranged between the two insulating partitions.
[0011] Preferably, the Latin structure has a first rotating column and a second rotating column rotatably arranged in the mold sleeve, and the first gear and the second gear are fixedly arranged at the ends of the first rotating column and the second rotating column that are away from each other, and the first umbrella wheel and the second umbrella wheel are fixedly arranged at the ends of the first rotating column and the second rotating column that are close to each other, and a third umbrella wheel is arranged between the first umbrella wheel and the second umbrella wheel, and the first rack and the second rack are slidably arranged in the mold sleeve.
[0012] Preferably, the first power connector includes a connector base, a groove is provided on the connector base, a conductive sheet is fixedly provided in the groove, a second slot is provided on the side of the conductive sheet close to the lower Latin, a through slot is provided on the side of the groove close to the medium frequency heating coil, an electric wire is provided in the through slot, an insulating baffle is slidably provided on the side of the connector base close to the lower Latin, and a second spring is fixedly provided on the outer wall of the insulating baffle close to the medium frequency heating coil.
[0013] Preferably, the Latin base and the joint base are made of insulating materials, the first sliding column, the second sliding column, the first round ball and the second round ball are made of conductive materials, the two insulating partitions are fixedly connected to the first sliding column and the second sliding column respectively, and the two ends of the conductive column pass through the insulating partitions and are slidably connected to the first sliding column and the second sliding column; The conductive sheet is fixedly connected to the electric wires, the first slot and the second slot are semicircular, and the electric wires of different first power connectors are respectively connected to the input wire, the output wire and the medium frequency heating coil.
[0014] Preferably, the first gear and the second gear are respectively meshed with the first rack and the second rack, the third umbrella wheel is respectively meshed with the first umbrella wheel and the second umbrella wheel on both sides, the structure of the upper Latin is the same as that of the lower Latin, the structure of the second power connector is the same as that of the first power connector, and the third umbrella wheel is rotatably connected to the mold sleeve.
[0015] A magnesium alloy forging method comprises the following steps: Step 1: Place the bar into the heating furnace for heating to 250-450℃, and keep it warm for more than 3 hours according to the size of the bar to ensure that the bar blank is heated through and the temperature is uniform; Step 2: Open the forging die and spray lubricate the working inner cavity of the die with oil-based graphite lubricant; Step 3: Place the lower Latin into the first Latin slot, fix the mold base and the mold sleeve, and the medium frequency heating coil automatically starts to continuously heat the molding cavity through the medium frequency heating coil.
[0016] Step 4: Place the bar into the forming cavity through the feed trough, and then perform multiple extrusion forging on the bar; Step 5: After the bar is formed, put the upper Latin into the second Latin slot, fix the upper template and the die sleeve, and the lower Latin leaves the first Latin slot, and then the medium frequency heating coil is automatically shut down due to power loss; Step 6: The mold sleeve is driven to move by the hydraulic rod and the upper mold plate, so that the mold sleeve is separated from the mold base. The molding bar in the molding cavity is automatically separated under the action of gravity and falls on the mold base, and then the molding bar is taken away.
[0017] The present invention provides a magnesium alloy forging device and forging method capable of continuous heating, which has the following beneficial effects: The present invention first opens the upper part of the forging die by a hydraulic rod, then sprays and lubricates the working inner cavity of the forging die with an oil-based graphite lubricant, then fixes and connects the lower part and the middle part of the forging die, then the power source starts the internal components of the forging die through the input wire, so that the inner cavity of the forging die is continuously self-heated, then the bar material is placed in the inner cavity of the forging die, and then the hydraulic rod is started again, and the bar material in the inner cavity of the forging die is extruded and forged by the hydraulic rod and the forging components inside the forging die, and safety protection is performed during the forging process, and the cooling speed of the bar material is reduced by the continuous self-heating of the inner cavity of the forging die, thereby extending the forging time of the bar material, thereby eliminating the need for re-furnace insulation, and significantly shortening the complex forming process flow, thereby reducing the time required for forging.
[0018] Among them, during the bar forming process, the blank is always in a closed mold cavity, forming a stress state similar to extrusion, which greatly improves the plasticity of the bar and significantly shortens the complex forming process.
[0019] Among them, when the lower Latin is placed in the first Latin slot, the first power connector and the second power connector are electrically connected through the first round ball, the second round ball, the first sliding column, the second sliding column and the conductive column. When the lower Latin needs to leave the first Latin slot, the Latin base is pushed hard to make the lower Latin leave the first Latin slot, and the electrical connection between the first power connector and the second power connector is released at the same time. After that, the medium frequency heating coil is automatically shut down due to loss of power, and the molding cavity is no longer continuously heated, saving energy.
[0020] Among them, when the lower Latin is placed in the first Latin slot, the second slot, the first round bead and the second round bead are used to fix the position of the lower Latin to a certain extent. When the upper Latin enters the second Latin slot, the first slot and the first round bead and the second round bead on the upper Latin are used to fix the position of the upper Latin to a certain extent in the same way as the above principle. When the lower Latin leaves the first Latin slot, the second spring rebounds, so that the insulating baffle re-closes the groove to prevent accidental touching of the conductive sheet.
[0021] Among them, when the upper Latin is inserted into the second Latin slot, the second rack is used to push the lower Latin to move, so that the lower Latin automatically detaches from the first Latin slot. When the lower Latin is inserted into the first Latin slot, the lower Latin squeezes the second rack, and then the first rack pushes the upper Latin to move, so that the upper Latin automatically detaches from the second Latin slot. There is no need for staff to manually disassemble the lower Latin or the upper Latin, which facilitates subsequent forging operations. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the overall structure of the present invention; Figure 2 It is a front view structural schematic diagram of the present invention; Figure 3 It is a schematic diagram of the cross-sectional structure of the forging die in the present invention; Figure 4 It is a schematic diagram of the cross-sectional three-dimensional structure of the forging die in the present invention; Figure 5 For the present invention Figure 4 A schematic diagram of the local enlarged structure at point A in the middle; Figure 6 For the present invention Figure 4 A schematic diagram of the local enlarged structure at B in the middle; Figure 7 It is a schematic diagram of the cross-sectional structure of the lower Latin in the present invention; Figure 8 It is a structural schematic diagram of the Latin structure in the present invention; Fig. 9 is a schematic diagram of a cross-sectional three-dimensional structure of a first electrical connector in the present invention; Fig.10 It is a schematic diagram of the forging process of the present invention.
[0023] Among them, 1. base; 2. support column; 3. forging mold; 301. mold base; 302. upper mold plate; 303. mold sleeve; 304. first Latin groove; 305. second Latin groove; 306. lower Latin; 30601. Latin base; 30602. slide groove; 30603. first slide column; 30604. second slide column; 30605. first round ball; 30606. second round ball; 30607. insulating partition; 30608. conductive column; 30609. first spring; 307. upper Latin; 308. first power connector; 30801. connector base; 30802. groove; 30803. conductive sheet; 30804. second slot; 30805. through slot ; 30806, electric wire; 30807, insulating baffle; 30808, second spring; 309, second power connector; 3010, first slot; 3011, punch; 3012, Latin structure; 30121, first rotating column; 30122, second rotating column; 30123, first gear; 30124, second gear; 30125, first umbrella wheel; 30126, second umbrella wheel; 30127, third umbrella wheel; 30128, first rack; 30129, second rack; 3013, medium frequency heating coil; 3014, feed trough; 3015, molding cavity; 4, mounting slot; 5, input wire; 6, output wire; 7, power supply; 8, top cover; 9, hydraulic rod. DETAILED DESCRIPTION
[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example
[0025] like Figure 1 and Figure 2 As shown, an embodiment of the present invention provides a magnesium alloy forging device capable of continuous heating, including a base 1 and a plurality of support columns 2, wherein a forging die 3 and a mounting groove 4 are provided on the base 1, input wires 5 and output wires 6 are respectively provided on both sides of the forging die 3, a power supply 7 is provided in the mounting groove 4, the forging die 3 is connected to the power supply 7 via the input wire 5, a top cover 8 is provided on one side above the support column 2, and a hydraulic rod 9 is provided on the top cover 8.
[0026] like Figures 3 to 6 As shown, the forging die 3 includes a die base 301, an upper die plate 302 is arranged on one side above the die base 301, a die sleeve 303 is arranged between the upper die plate 302 and the die base 301, two first Latin grooves 304 are arranged on the outer wall surface of the side where the die base 301 and the die sleeve 303 are close to each other, two second Latin grooves 305 are arranged on the outer wall surface of the side where the upper die plate 302 and the die sleeve 303 are close to each other, a lower Latin 306 and an upper Latin 307 are respectively arranged in the first Latin groove 304 and the second Latin groove 305, a punch 3011 is arranged on the upper die plate 302, and the punch 3011 is movably arranged in a feed groove 3014 located on the die sleeve 303, and the feed groove 3014 and the die base 301 are closed to form a forming cavity 3015; A first power connector 308 is fixedly provided on the inner wall below the first Latin groove 304 on the mold base 301, a second power connector 309 is fixedly provided on the inner wall above the first Latin groove 304 on the mold sleeve 303, first card slots 3010 are provided on the upper and lower inner walls of the second Latin groove 305, and a Latin structure 3012 and a medium frequency heating coil 3013 are provided on the mold sleeve 303, and the medium frequency heating coil 3013 surrounds the molding cavity 3015.
[0027] According to the above technical solution, when the bar needs to be forged, the upper mold plate 302 is first separated from the mold sleeve 303 by the hydraulic rod 9, and then the feed groove 3014 and the inner cavity of the molding cavity 3015 are sprayed and lubricated with an oil-based graphite lubricant, and the lower Latin 306 is placed in the first Latin groove 304, and the mold base 301 and the mold sleeve 303 are fixedly connected by the lower Latin 306 and the first Latin groove 304, and at the same time, the surfaces of both ends of the lower Latin 306 are connected to the first power connector 308. The internal components are fitted, and the power supply 7 can start the medium frequency heating coil 3013 through the input wire 5, the first power connector 308, the lower Latin 306, and the second power connector 309, and the forming cavity 3015 is continuously heated by the medium frequency heating coil 3013, and then the bar material is placed into the forming cavity 3015 through the feed trough 3014, and then the upper template 302 drives the punch 3011 to move toward the bar material through the hydraulic rod 9, and the punch 3011 is used to perform multiple extrusion forging on the bar material; Under the action of the punch 3011, the bar material is firstly roughened and deformed. As the punch 3011 continues to move downward, the bar material begins to deform radially and the ribs begin to form. When the rib forming is nearing the end, the bar material is formed by the extrusion effect. During the bar forming process, the forming cavity 3015 is continuously heated by the medium frequency heating coil 3013, thereby reducing the cooling speed of the bar material and extending the one-time forging time of the bar material, so that there is no need to return to the furnace for heat preservation. In addition, the blank is always in the closed die cavity, forming a radial stress state similar to extrusion, which greatly improves the plasticity of the bar material and significantly shortens the complex forming process flow. After the bar is formed, the upper Latin 307 is placed in the second Latin slot 305, and the upper template 302 is fixedly connected to the mold sleeve 303 through the upper Latin 307 and the second Latin slot 305. The upper Latin 307 squeezes some components of the Latin structure 3012, and at the same time, the Latin structure 3012 pushes the lower Latin 306 to move, so that the lower Latin 306 gradually leaves the first Latin slot 304. When the upper Latin 307 completely enters the second Latin slot 305, the Latin structure 3012 also completely pushes the lower Latin 306 away from the first Latin slot 304. At this time, the lower Latin 306 is separated from the first power connector 308 and the second power connector 309, and then the intermediate frequency heating coil 3013 is lost. The power is cut off and the molding cavity 3015 is automatically closed, and the molding cavity 3015 is no longer continuously heated, which saves energy. Subsequently, the mold sleeve 303 is driven to move by the hydraulic rod 9 and the upper mold plate 302, so that the mold sleeve 303 is separated from the mold base 301, and the molding bar in the molding cavity 3015 is automatically separated under the action of gravity and falls on the mold base 301. Then the molding bar is taken away, so that the mold sleeve 303 and the mold base 301 are fitted again, and the lower Latin 306 is placed in the first Latin groove 304. The lower Latin 306 squeezes some components of the Latin structure 3012, and the Latin structure 3012 pushes the upper Latin 307 away from the second Latin groove 305. Repeat the above steps to perform repeated forging.
[0028] like Figure 7 As shown, the lower Latin 306 includes a Latin base 30601, and a slide groove 30602 is arranged on the Latin base 30601, and a first slide column 30603 and a second slide column 30604 are slidably arranged in the slide groove 30602, and a first round ball 30605 and a second round ball 30606 are fixedly arranged on the side of the first slide column 30603 and the second slide column 30604 away from each other, respectively, and two insulating partitions 30607 and a conductive column 30608 are arranged between the first slide column 30603 and the second slide column 30604, and a first spring 30609 is fixedly arranged between the two insulating partitions 30607.
[0029] By means of the above technical solution, when it is necessary to put the lower Latin 306 into the first Latin slot 304, the Latin base 30601 is pushed, and then the inner wall of the first Latin slot 304 squeezes the first round ball 30605 and the second round ball 30606, so that the first round ball 30605 and the second round ball 30606 enter the slide slot 30602, and the first spring 30609 contracts. Subsequently, when the Latin base 30601 moves between the first power-on connector 308 and the second power-on connector 309, the first round ball 30605 and the second round ball 30606 are no longer squeezed, and the first spring 30609 rebounds, so that the first round ball 30605 and the second round ball 30606 enter the second power-on connector 309 and the first power-on connector 309, respectively. 08, the first round bead 30605 and the second round bead 30606 are used to fix the position of the lower Latin 306 to a certain extent, preventing the lower Latin 306 from shifting due to slight vibrations, and the first electrical connector 308 and the second electrical connector 309 can be electrically connected through the first round bead 30605, the second round bead 30606, the first sliding column 30603, the second sliding column 30604 and the conductive column 30608. When it is necessary to make the lower Latin 306 leave the first Latin slot 304, the Latin base 30601 is pushed forcefully to make the lower Latin 306 leave the first Latin slot 304, and at the same time, the electrical connection between the first electrical connector 308 and the second electrical connector 309 is released, thereby saving energy.
[0030] like Figure 8As shown, the Latin structure 3012 is rotatably provided with a first rotating column 30121 and a second rotating column 30122 in the mold sleeve 303, and the ends of the first rotating column 30121 and the second rotating column 30122 that are away from each other are fixedly provided with a first gear 30123 and a second gear 30124 respectively, and the ends of the first rotating column 30121 and the second rotating column 30122 that are close to each other are fixedly provided with a first umbrella wheel 30125 and a second umbrella wheel 30126 respectively, and a third umbrella wheel 30127 is provided between the first umbrella wheel 30125 and the second umbrella wheel 30126, and a first rack 30128 and a second rack 30129 are slidably provided in the mold sleeve 303.
[0031] Through the above technical solution, when the upper Latin 307 is inserted into the second Latin slot 305, the upper Latin 307 squeezes the first rack 30128, the first rack 30128 drives the first gear 30123 to rotate, the first gear 30123 drives the first rotating column 30121 to rotate, the first rotating column 30121 drives the first umbrella wheel 30125 to rotate, the first umbrella wheel 30125 makes the second umbrella wheel 30126 rotate in the opposite direction through the third umbrella wheel 30127, the second umbrella wheel 30126 drives the second gear 30124 to rotate through the second rotating column 30122, and the second gear 30124 drives the second gear 30123 to rotate. Wheel 30124 moves the second rack 30129 toward the lower Latin 306, and uses the second rack 30129 to push the lower Latin 306 to move, so that the lower Latin 306 automatically disengages from the first Latin groove 304. When the lower Latin 306 is inserted into the first Latin groove 304, the lower Latin 306 squeezes the second rack 30129, and then the first rack 30128 pushes the upper Latin 307 to move, so that the upper Latin 307 automatically disengages from the second Latin groove 305. There is no need for staff to manually disassemble the lower Latin 306 or the upper Latin 307, which facilitates subsequent forging operations.
[0032] like Fig. 9 As shown, the first power connector 308 includes a connector base 30801, a groove 30802 is provided on the connector base 30801, a conductive sheet 30803 is fixedly provided in the groove 30802, a second slot 30804 is provided on the side of the conductive sheet 30803 close to the lower Latin 306, a through slot 30805 is provided on the side of the groove 30802 close to the medium frequency heating coil 3013, a wire 30806 is provided in the through slot 30805, an insulating baffle 30807 is slidably provided on the side of the connector base 30801 close to the lower Latin 306, and a second spring 30808 is fixedly provided on the outer wall of the insulating baffle 30807 close to the medium frequency heating coil 3013.
[0033] Through the above technical solution, when the lower Latin 306 is placed in the first Latin groove 304, the lower Latin 306 squeezes the insulating baffle 30807, the second spring 30808 contracts, and the insulating baffle 30807 is released from the sealing of the groove 30802, and then the first round ball 30605 and the second round ball 30606 enter the second card slot 30804 on the second power connector 309 and the second card slot 30804 on the first power connector 308 respectively, and then the current can be transported to the specified position through the wire 30806, and at the same time, the second card slot 30804 and the first card slot 30804 are used to connect the electric wire 30806 to the electric wire 30806. The round ball 30605 and the second round ball 30606 fix the position of the lower Latin 306 to a certain extent. When the upper Latin 307 enters the second Latin groove 305, the same as the above principle is used. The first card slot 3010 and the first round ball 30605 and the second round ball 30606 on the upper Latin 307 fix the position of the upper Latin 307 to a certain extent. When the lower Latin 306 leaves the first Latin groove 304, the second spring 30808 rebounds, so that the insulating baffle 30807 re-seals the groove 30802 to prevent accidental touching of the conductive sheet 30803.
[0034] A magnesium alloy forging method comprises the following steps: Step 1: Place the bar into the heating furnace for heating to 250-450℃, and keep it warm for more than 3 hours according to the size of the bar to ensure that the bar blank is heated through and the temperature is uniform; Step 2: Open the forging die 3 and spray lubricate the working inner cavity of the die with oil-based graphite lubricant; Step 3: Place the lower Latin 306 into the first Latin groove 304, fix the mold base 301 and the mold sleeve 303, and automatically start the intermediate frequency heating coil 3013 to continuously heat the molding cavity 3015; Step 4: Place the bar material into the forming cavity 3015 through the feed slot 3014, and then perform multiple extrusion forging on the bar material; Step 5: After the bar material is formed, the upper Latin 307 is placed in the second Latin slot 305, the upper mold plate 302 is fixedly connected to the mold sleeve 303, the lower Latin 306 leaves the first Latin slot 304, and then the medium frequency heating coil 3013 is automatically turned off due to power loss; Step 6: The mold sleeve 303 is moved by the hydraulic rod 9 and the upper mold plate 302 to separate the mold sleeve 303 from the mold base 301. The molding bar in the molding cavity 3015 is automatically separated under the action of gravity and falls on the mold base 301. Then the molding bar is taken away.
[0035] Working principle: The present invention first opens the upper part of the forging die 3 through the hydraulic rod 9, then sprays and lubricates the working inner cavity of the forging die 3 with an oil-based graphite lubricant, then fixes and connects the lower part and the middle part of the forging die 3, and then the power supply 7 starts the internal components of the forging die 3 through the input wire 5, so that the inner cavity of the forging die 3 is continuously self-heated, and then the bar material is placed in the inner cavity of the forging die 3, and then the hydraulic rod 9 is started again, and the bar material in the inner cavity of the forging die 3 is extruded and forged by the hydraulic rod 9 and the forging components inside the forging die 3, and the cooling speed of the bar material is reduced by the continuous self-heating of the inner cavity of the forging die 3, thereby extending the forging time of the bar material, thereby eliminating the need for re-melting for heat preservation, which can significantly shorten the complex forming process and reduce the time required for forging.
[0036] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not limitations on the implementation methods of the present invention. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made on the basis of the above description. It is impossible to list all the implementation methods here. All obvious changes or modifications derived from the technical solution of the present invention are still within the protection scope of the present invention.
Claims
1. A magnesium alloy forging device capable of continuous heating, comprising a base (1) and a plurality of support columns (2), characterized in that: The base (1) is provided with a forging die (3) and a mounting groove (4), an input wire (5) and an output wire (6) are respectively provided on both sides of the forging die (3), a power supply (7) is provided in the mounting groove (4), the forging die (3) is connected to the power supply (7) via the input wire (5), a top cover (8) is provided on one side above the support column (2), and a hydraulic rod (9) is provided on the top cover (8).
2. The magnesium alloy forging equipment capable of continuous heating according to claim 1, characterized in that: The forging die (3) comprises a die base (301), an upper die plate (302) is arranged on one side above the die base (301), a die sleeve (303) is arranged between the upper die plate (302) and the die base (301), two first Latin grooves (304) are arranged on the outer wall surface of the side where the die base (301) and the die sleeve (303) are close to each other, two second Latin grooves (305) are arranged on the outer wall surface of the side where the upper die plate (302) and the die sleeve (303) are close to each other, a lower Latin (306) and an upper Latin (307) are arranged in the first Latin groove (304) and the second Latin groove (305), respectively, a punch (3011) is arranged on the upper die plate (302), the punch (3011) is movably arranged in a feed groove (3014) located on the die sleeve (303), and the feed groove (3014) and the die base (301) are closed to form a forming cavity (3015).
3. The magnesium alloy forging equipment capable of continuous heating according to claim 2, characterized in that: A first power connector (308) is fixedly provided on an inner wall below one side of the first Latin groove (304) on the mold base (301), a second power connector (309) is fixedly provided on an inner wall above one side of the first Latin groove (304) on the mold sleeve (303), first clamping grooves (3010) are provided on the inner walls on both upper and lower sides of the second Latin groove (305), and a Latin structure (3012) and a medium-frequency heating coil (3013) are provided on the mold sleeve (303), and the medium-frequency heating coil (3013) surrounds the molding cavity (3015).
4. The magnesium alloy forging equipment capable of continuous heating according to claim 3, characterized in that: The upper template (302) is fixedly connected to the hydraulic rod (9), and the second power connector (309) is located directly above the second power connector (309) of the first Latin slot (304).
5. The magnesium alloy forging equipment capable of continuous heating according to claim 4, characterized in that: The lower Latin (306) comprises a Latin base (30601), a slide groove (30602) is arranged on the Latin base (30601), a first slide column (30603) and a second slide column (30604) are slidably arranged in the slide groove (30602), a first round ball (30605) and a second round ball (30606) are fixedly arranged on the side of the first slide column (30603) and the second slide column (30604) away from each other, two insulating partitions (30607) and a conductive column (30608) are arranged between the first slide column (30603) and the second slide column (30604), and a first spring (30609) is fixedly arranged between the two insulating partitions (30607).
6. The magnesium alloy forging equipment capable of continuous heating according to claim 5, characterized in that: The Latin structure (3012) is rotatably provided with a first rotating column (30121) and a second rotating column (30122) in the mold sleeve (303); the ends of the first rotating column (30121) and the second rotating column (30122) that are away from each other are respectively fixedly provided with a first gear (30123) and a second gear (30124); the ends of the first rotating column (30121) and the second rotating column (30122) that are close to each other are respectively fixedly provided with a first umbrella wheel (30125) and a second umbrella wheel (30126); a third umbrella wheel (30127) is provided between the first umbrella wheel (30125) and the second umbrella wheel (30126); and the mold sleeve (303) is slidably provided with a first rack (30128) and a second rack (30129).
7. The magnesium alloy forging equipment capable of continuous heating according to claim 6, characterized in that: The first electrical connector (308) comprises a connector base (30801), a groove (30802) is provided on the connector base (30801), a conductive sheet (30803) is fixedly provided in the groove (30802), a second slot (30804) is provided on the side of the conductive sheet (30803) close to the lower Latin (306), a through slot (30805) is provided on the side of the groove (30802) close to the medium-frequency heating coil (3013), a wire (30806) is provided in the through slot (30805), an insulating baffle (30807) is slidably provided on the side of the connector base (30801) close to the lower Latin (306), and a second spring (30808) is fixedly provided on the outer wall of the insulating baffle (30807) close to the medium-frequency heating coil (3013).
8. The magnesium alloy forging equipment capable of continuous heating according to claim 7, characterized in that: The Latin base (30601) and the joint base (30801) are made of insulating materials, the first sliding column (30603), the second sliding column (30604), the first round ball (30605) and the second round ball (30606) are made of conductive materials, the two insulating partitions (30607) are fixedly connected to the first sliding column (30603) and the second sliding column (30604) respectively, and the two ends of the conductive column (30608) pass through the insulating partitions (30607) and are slidably connected to the first sliding column (30603) and the second sliding column (30604); The conductive sheet (30803) is fixedly connected to the electric wire (30806); the first slot (3010) and the second slot (30804) are semicircular; the electric wires (30806) of different first power connectors (308) are respectively connected to the input wire (5), the output wire (6) and the medium frequency heating coil (3013).
9. The magnesium alloy forging equipment capable of continuous heating according to claim 8, characterized in that: The first gear (30123) and the second gear (30124) are respectively meshed with the first rack (30128) and the second rack (30129); the third umbrella wheel (30127) is respectively meshed with the first umbrella wheel (30125) and the second umbrella wheel (30126); the structure of the upper Latin (307) is the same as that of the lower Latin (306); the structure of the second power connector (309) is the same as that of the first power connector (308); and the third umbrella wheel (30127) is rotatably connected to the mold sleeve (303).
10. A method for forging a magnesium alloy using the magnesium alloy forging equipment according to claim 9, characterized in that: The following steps are involved: Step 1: Place the bar into the heating furnace for heating to 250-450℃, and keep it warm for more than 3 hours according to the size of the bar to ensure that the bar blank is heated through and the temperature is uniform; Step 2: Open the forging die (3) and spray lubricate the working inner cavity of the die with an oil-based graphite lubricant; Step 3: placing the lower Latin (306) into the first Latin groove (304), fixing the mold base (301) and the mold sleeve (303) together, and automatically starting the intermediate frequency heating coil (3013), and continuously heating the molding cavity (3015) through the intermediate frequency heating coil (3013); Step 4: placing the bar material into the forming cavity (3015) through the feed trough (3014), and then performing multiple extrusion forging on the bar material; Step 5: After the bar material is formed, the upper Latin (307) is placed in the second Latin slot (305), the upper template (302) is fixedly connected to the mold sleeve (303), the lower Latin (306) leaves the first Latin slot (304), and then the medium frequency heating coil (3013) is automatically turned off due to power loss; Step 6: The mold sleeve (303) is driven to move by the hydraulic rod (9) and the upper mold plate (302), so that the mold sleeve (303) is separated from the mold base (301), and the molded bar in the molding cavity (3015) is automatically separated under the action of gravity and falls on the mold base (301), and then the molded bar is taken away.
Citation Information
Patent Citations
Four-post vertical hydraulic equipment used for liquid metal casting and forging molding
CN101774006A
Manufacturing process and equipment for nickel-chromium-molybdenum alloy cast iron composite roller in forged steel roller neck
CN105328168A
Isothermal forging forming device and method of wrought magnesium alloy universal joint pin
CN109434004A
Magnesium alloy forge piece forming method and equipment
CN116274788A
Method and device for compression forming of magnesium alloy material
JP2000167636A