Smoke agent for thermal smoke sprayer as well as preparation method and application of smoke agent
By using smoke agents made of alcohols and ultrafine carbon black, the existing smoke method has solved the problem of short smoke duration and open flame hazards in low temperature protection, and achieved the generation of non-toxic and harmless smoke with high-effect tree insulation, ensuring that Use safety.
Patent Information
- Application Number
- CN202410948304.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-12-03
AI Technical Summary
The existing smoke smoke method has problems such as short smoke duration, small smoke volume, fast combustion speed and open flame hazards in low temperature protection, which is difficult to effectively use for large-area fruit tree insulation.
Using aerosol made of glycerol, propylene glycol, ethylene glycol, ethanol and ultrafine carbon black aqueous dispersion, it decomposes non-toxic and harmless smoke through high temperature through hot smoke machine, and uses alcohols and ultrafine carbon black. Improve the diffusion rate and settlement time of smoke, and enhance the scattering and reflection effect on infrared radiation.
It achieves long-term diffusion and settlement of smoke, improves the insulation effect of fruit trees, and does not have open flames during use, which is safe and reliable.
Smart Images

Figure CN119059858A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of materials, and in particular relates to an aerosol and a preparation method and application thereof. Background Art
[0002] Crops, especially fruit trees, are easily affected by low temperatures in the second half of the night during their growth process. In the spring of each year, due to the influence of cold air from the north, the temperature in some orchards will drop below zero degrees Celsius in the second half of the night due to different terrain and topography. The flowers of fruit trees will be injured or wither due to the low temperature.
[0003] In general, fruit farmers use methods such as irrigation, covering, fertilization, and fumigation to keep fruit trees warm. Among these methods, fumigation is to produce smoke by burning fuel before the low temperature arrives, so as to reduce the heat loss around the fruit trees. After fumigation, the temperature around the fruit trees can generally increase by 1-2°C to prevent the fruit trees from freezing. After the aerosol is ignited, smoke particles will be formed in the air. These particles can be suspended in the air for a long time, and at the same time, they will diffuse and sink irregularly. Smoke particles can be scattered in different positions of the fruit trees. The particle size of the aerosol particles is generally 1-14 microns, which can form an aerosol, which has the effect of absorbing, reflecting and scattering infrared thermal radiation, thereby keeping crops warm.
[0004] At present, the materials used in conventional fumigation methods burn very quickly, the smoke lasts for a short time, the amount of smoke is small, there may be open flames during combustion, there are fire hazards, and the cost is high, so it is not conducive to large-scale use. Summary of the invention
[0005] The purpose of the present invention is to provide an aerosol for heat preservation of crops. The smoke generated by high-temperature decomposition using a hot smoke machine is non-toxic and harmless, and has a high smoke diffusion rate, a long settling time and an excellent heat preservation effect. The use process does not require open flames and is safe and reliable.
[0006] In order to achieve the above purpose, the technical solutions adopted are as follows:
[0007] An aerosol for a hot smoke machine, the composition of which is as follows by weight:
[0008] 1-15 parts of glycerol; 1-3 parts of propylene glycol; 1-3 parts of ethylene glycol; 1-5 parts of ethanol; 1-5 parts of an aqueous dispersion of ultrafine carbon black; the carbon black concentration in the aqueous dispersion of ultrafine carbon black is 1-10wt%.
[0009] According to the above scheme, the ultrafine carbon black has a particle size range of 5-30 μm, has good hydrophilicity and is easily dispersed in water at room temperature.
[0010] The method for preparing the aerosol for the hot fog machine comprises the following steps:
[0011] (1) Preheating the aqueous dispersion of raw materials glycerol, propylene glycol, ethylene glycol, ethanol, and ultrafine carbon black to 30-50° C.;
[0012] (2) adding glycerol into the reaction kettle;
[0013] (3) Slowly add ethylene glycol into propylene glycol and stir evenly;
[0014] (4) Slowly add propylene glycol to the mixture of glycerol and ethylene glycol and stir evenly;
[0015] (5) Then, ethanol and the aqueous dispersion of ultrafine carbon black are added in sequence, and the mixture is stirred and mixed to obtain an aerosol.
[0016] According to the above scheme, step 2 includes stirring at 30-50°C for 10-30 minutes.
[0017] According to the above scheme, step 3 includes stirring at 30-50°C for 10-30 minutes.
[0018] According to the above scheme, step 4 includes stirring at 30-50°C for 10-30 minutes.
[0019] According to the above scheme, step 5 includes stirring at 30-50°C for 10-30 minutes.
[0020] According to the above scheme, the stirring rate is 100-300 rpm.
[0021] According to the above scheme, the aerosol obtained in step 5 is sealed and left to stand for 1-2 hours without phase separation.
[0022] The application of the above-mentioned aerosol agent in cold protection and heat preservation of fruit trees comprises adding the aerosol agent into a hot aerosol machine to produce smoke.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] The invention uses alcohol substances as raw materials to prepare smoke agents, which has the advantages that smoke generated after high-temperature decomposition is non-toxic and harmless, and there is no open flame during the use process, which is safe and reliable.
[0025] By screening and adjusting alcohols, propylene glycol is selected as the main smoke-forming material. The reaction performance of propylene glycol is improved by adding ethylene glycol, propylene glycol and ethanol. The high volatility of ethanol is used to enhance the smoke diffusion rate, while also increasing the smoke settling time.
[0026] By adding ultrafine carbon black particles, the adsorption of water vapor and particulate matter in the surrounding environment is enhanced, the amount of smoke is increased by increasing the number of smoke nucleating particles and the smoke concentration is increased, the penetration ability of infrared radiation is reduced, and its scattering and reflection effects are improved.
[0027] By controlling the carbon black content and the particle size of the carbon black particles, the particle size, diffusion and sedimentation rate of the smoke aerosol particles can be well controlled to meet the insulation needs of fruit trees. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 : Actual photo of the aerosol prepared in Example 5.
[0029] Figure 2 : Actual photo of the heat preservation test of the aerosol prepared in Example 5 released by a hot smoke machine. DETAILED DESCRIPTION
[0030] The technical scheme of the present invention will be further described in detail below in conjunction with specific examples. It should be understood that the following examples are only exemplary descriptions and explanations of the present invention, and should not be construed as limiting the scope of protection of the present invention. All technologies implemented based on the above content of the present invention are included in the scope that the present invention is intended to protect. Unless otherwise specified, the raw materials and reagents used in the following examples are all commercially available products, or can be prepared by known methods.
[0031] Example 1
[0032] (1) Screening of raw materials for aerosol composite materials: propylene glycol, ethylene glycol, ethanol, ultrafine carbon black, and distilled water.
[0033] (2) Preparation of composite materials: The selected materials propylene glycol, propylene glycol, ethylene glycol, and distilled water were heated at 30°C respectively; propylene glycol was added to the reactor, and then continued to heat and stir to reduce its viscosity to facilitate subsequent composite operations, and stirred for 10 minutes; ethylene glycol was slowly added to propylene glycol, and continued to stir for 10 minutes. Propylene glycol was slowly added to the mixed solution of propylene glycol and ethylene glycol, and continued to stir for 10 minutes. Ethanol was heated to 30°C, and then ethanol was added to the mixed solution and continued to stir; ultrafine carbon black was added to distilled water and continued to stir and disperse; finally, the carbon black dispersion was added to the mixed solution and heated and stirred for 10 minutes to obtain an aerosol. The aerosol composite material was transferred to a polyethylene barrel for static storage. Among them, the volume ratio of propylene glycol, propylene glycol, ethylene glycol, ethanol, and carbon black dispersion (5wt.%) was 5:2:3:3:1.
[0034] (3) The prepared aerosol composite material is added into a hot aerosol machine to produce aerosol, which is used to keep apricot trees warm in cold spring weather.
[0035] The performance of the smoke agent was tested for heat preservation of apricot trees. Compared with the control group (no smoke environment), the temperature of the surrounding environment of the fruit trees increased significantly, from -5°C to -4°C. 2 ) The time required is 1 minute, the smoke diffusion height is 4 meters, and the time required for smoke settlement is 1 hour.
[0036] Example 2
[0037] (1) Screening of raw materials for aerosol composite materials: propylene glycol, ethylene glycol, ethanol, ultrafine carbon black, and distilled water.
[0038] (2) Preparation of composite materials: Heat the selected materials propylene glycol, propylene glycol, ethylene glycol, and distilled water at 30°C respectively; add propylene glycol to the reactor, and then continue to heat and stir to reduce its viscosity to facilitate subsequent composite operations, and stir for 10 minutes; slowly add ethylene glycol to propylene glycol and continue to stir for 10 minutes. Slowly add propylene glycol to the mixed solution of propylene glycol and ethylene glycol, and continue to stir for 10 minutes. Heat ethanol to 30°C, then add ethanol to the mixed solution and continue to stir; add ultrafine carbon black to distilled water and continue to stir and disperse; finally, add the carbon black dispersion to the mixed solution and heat and stir for 10 minutes to obtain an aerosol, and transfer the aerosol composite material to a polyethylene barrel for static storage. The volume ratio of propylene glycol, propylene glycol, ethylene glycol, ethanol, and carbon black dispersion (5wt.%) is 8:2:3:3:1.
[0039] (3) The prepared aerosol composite material is added to a hot smoke machine to produce smoke, which is used to keep apricot trees warm in cold spring weather.
[0040] The performance of the smoke agent was tested for heat preservation of apricot trees. Compared with the control group (no smoke environment), the temperature of the surrounding environment of the fruit trees increased significantly, from -5℃ to -3.5℃. 2 ) The time required is 1.6 minutes, the smoke diffusion height is 4 meters, and the time required for smoke settlement is 3 hours.
[0041] Example 3
[0042] (1) Screening of raw materials for aerosol composite materials: propylene glycol, ethylene glycol, ethanol, ultrafine carbon black, and distilled water.
[0043] (2) Preparation of composite materials: Heat the selected materials propylene glycol, propylene glycol, ethylene glycol, and distilled water at 30°C respectively; add propylene glycol to the reactor, and then continue to heat and stir to reduce its viscosity to facilitate subsequent composite operations, and stir for 10 minutes; slowly add ethylene glycol to propylene glycol and continue to stir for 10 minutes. Slowly add propylene glycol to the mixed solution of propylene glycol and ethylene glycol, and continue to stir for 10 minutes. Heat ethanol to 30°C, then add ethanol to the mixed solution and continue to stir; add ultrafine carbon black to distilled water and continue to stir and disperse; finally, add the carbon black dispersion to the mixed solution and heat and stir for 10 minutes to obtain an aerosol, and transfer the aerosol composite material to a polyethylene barrel for static storage. The volume ratio of propylene glycol, propylene glycol, ethylene glycol, ethanol, and carbon black dispersion (5wt.%) is 9:2:3:3:1.
[0044] (3) The prepared aerosol composite material is added to a hot smoke machine to produce smoke, which is used to keep apricot trees warm in cold spring weather.
[0045] The performance of the smoke agent was tested for heat preservation of apricot trees. Compared with the control group (no smoke environment), the temperature of the surrounding environment of the fruit trees increased significantly, from -5°C to -3°C. 2 ) The time required is 2 minutes, the smoke diffusion height is 4 meters, and the time required for smoke settlement is 3.6 hours.
[0046] Example 4
[0047] (1) Screening of raw materials for aerosol composite materials: propylene glycol, ethylene glycol, ethanol, ultrafine carbon black, and distilled water.
[0048] (2) Preparation of composite materials: Heat the selected materials propylene glycol, propylene glycol, ethylene glycol, and distilled water at 30°C respectively; add propylene glycol to the reactor, and then continue to heat and stir to reduce its viscosity to facilitate subsequent composite operations, and stir for 10 minutes; slowly add ethylene glycol to propylene glycol and continue to stir for 10 minutes. Slowly add propylene glycol to the mixed solution of propylene glycol and ethylene glycol, and continue to stir for 10 minutes. Heat ethanol to 30°C, then add ethanol to the mixed solution and continue to stir; add ultrafine carbon black to distilled water and continue to stir and disperse; finally, add the carbon black dispersion to the mixed solution and heat and stir for 10 minutes to obtain an aerosol, and transfer the aerosol composite material to a polyethylene barrel for static storage. The volume ratio of propylene glycol, propylene glycol, ethylene glycol, ethanol, and carbon black dispersion (5wt.%) is 10:2:3:3:1.
[0049] (3) The prepared aerosol composite material is added to a hot smoke machine to produce smoke, which is used to keep apricot trees warm in cold spring weather.
[0050] The performance of the smoke agent was tested for heat preservation of apricot trees. Compared with the control group (no smoke environment), the temperature of the surrounding environment of the fruit trees increased significantly, from -5°C to -3°C. 2 ) The time required is 2.3 minutes, the smoke diffusion height is 4 meters, and the time required for smoke settlement is 4.3 hours.
[0051] Example 5
[0052] (1) Screening of raw materials for aerosol composite materials: propylene glycol, ethylene glycol, ethanol, ultrafine carbon black, and distilled water.
[0053] (2) Preparation of composite materials: Heat the selected materials propylene glycol, propylene glycol, ethylene glycol, and distilled water at 30°C respectively; add propylene glycol to the reactor, and then continue to heat and stir to reduce its viscosity to facilitate subsequent composite operations, and stir for 10 minutes; slowly add ethylene glycol to propylene glycol and continue to stir for 10 minutes. Slowly add propylene glycol to the mixed solution of propylene glycol and ethylene glycol, and continue to stir for 10 minutes. Heat ethanol to 30°C, then add ethanol to the mixed solution and continue to stir; add ultrafine carbon black to distilled water and continue to stir and disperse; finally, add the carbon black dispersion to the mixed solution and heat and stir for 10 minutes to obtain an aerosol, and transfer the aerosol composite material to a polyethylene barrel for static storage. The volume ratio of propylene glycol, propylene glycol, ethylene glycol, ethanol, and carbon black dispersion (5wt.%) is 12:3:1:1:3.
[0054] (3) The prepared aerosol composite material is added to a hot smoke machine to produce smoke, which is used to keep apricot trees warm in cold spring weather.
[0055] The performance of the smoke agent was tested for heat preservation of apricot trees. Compared with the control group (no smoke environment), the temperature of the surrounding environment of the fruit trees increased significantly, from -5℃ to -2.5℃. 2 ) The time required is 2.5 minutes, the smoke diffusion height is 4 meters, and the time required for smoke settlement is 5 hours.
[0056] Figure 1 This is a photo of the aerosol prepared in Example 5. Figure 1 It can be seen that the composite material is a black translucent liquid.
[0057] Figure 2 This is a real-life photo of a heat preservation test on fruit trees using the aerosol prepared in Example 5 to produce smoke using a hot smoke machine.
[0058] By adjusting the process parameters described in the present invention, the preparation of the aerosol composite material can be achieved, and the performance is basically the same as that of Example 5. The above is a description of the embodiments of the present invention. However, the present invention is not limited to the above embodiments. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A smoke spray for a hot smoke machine, characterized in that The composition is calculated by weight as follows: 1-15 parts of glycerol; 1-3 parts of propylene glycol; 1-3 parts of ethylene glycol; 1-5 parts of ethanol; 1-5 parts of an aqueous dispersion of ultrafine carbon black; the carbon black concentration in the aqueous dispersion of ultrafine carbon black is 1-10wt%.
2. The aerosol for a hot smoke machine as claimed in claim 1, characterized in that The ultrafine carbon black has a particle size range of 5-30 μm and has good hydrophilicity and is easily dispersed in water at room temperature.
3. The method for preparing the aerosol for the hot smoke machine according to claim 1, characterized in that The following steps are involved: (1) Preheating the aqueous dispersion of raw materials glycerol, propylene glycol, ethylene glycol, ethanol, and ultrafine carbon black to 30-50° C.; (2) adding glycerol into the reaction kettle; (3) Slowly add ethylene glycol into propylene glycol and stir evenly; (4) Slowly add propylene glycol to the mixture of glycerol and ethylene glycol and stir evenly; (5) Then, ethanol and the aqueous dispersion of ultrafine carbon black are added in sequence, and the mixture is stirred and mixed to obtain an aerosol.
4. The method for preparing the aerosol for the hot smoke machine according to claim 3, characterized in that Step 2 includes stirring at 30-50°C for 10-30 minutes.
5. The method for preparing the aerosol for the hot smoke machine according to claim 3, characterized in that Step 3 includes stirring at 30-50°C for 10-30 minutes.
6. The method for preparing aerosol for a hot fog machine as claimed in claim 3, characterized in that Step 4 includes stirring and incubating at 30-50°C for 10-30 minutes.
7. The method for preparing aerosol for a hot fog machine as claimed in claim 3, characterized in that Step 5 includes stirring and incubating at 30-50°C for 10-30 minutes.
8. The method for preparing aerosol for a hot fog machine as claimed in claim 3, characterized in that The stirring rate is 100-300 rpm.
9. The method for preparing aerosol for a hot smoke machine as claimed in claim 3, characterized in that The aerosol obtained in step 5 is sealed and allowed to stand for 1-2 hours without phase separation.
10. Use of the aerosol according to claim 1 in cold protection and heat preservation of fruit trees, comprising adding the aerosol into a hot aerosol machine to produce smoke.
Citation Information
Patent Citations
Preparation and application of smoke agent
CN102301998A
Red smoke agent
CN103044174A
Smoke forming agent for hot smoke type pesticide application technology
CN103299995A
Special smoke agent for preventing oilseed rape freeze injury and preparation method thereof
CN106699411A
Visible light shielding smoke agent and preparation method thereof
CN116102388A
Cited By
High-stability black non-toxic smoke oil and preparation method thereof
CN117510290A
A highly stable black non-toxic vapor oil and its preparation method
CN117510290B