Method for treating polyester-containing release film and method for manufacturing polyester-containing article
The polyester material on the release film is removed through pickling or alkaline washing steps, which solves the problems of resource waste and environmental pollution in the existing technology, and realizes efficient recycling and reuse of polyester, improves resource utilization efficiency, and conforms to environmental protection. Require.
Patent Information
- Application Number
- CN202310864527.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-02
- Filing Date
- 2023-07-14
- Publication Date
- 2024-12-03
AI Technical Summary
The existing release film treatment methods have failed to effectively recycle and reuse polyester materials, resulting in waste of resources and environmental pollution. Especially in the context of increasing environmental awareness, how to effectively deal and recycle useful polyester materials has become a research topic.
The release layer is removed by pickling or alkaline washing steps, and the release film is treated by immersing in an acid solution or alkali solution (such as acid solution of dodecylbenzenesulfonic acid and paraffin oil or 7% to 13% aqueous sodium hydroxide solution). , the release layer is removed and a solid substance containing polyester is obtained, and the use of volatile organic solvents is avoided, so as to achieve the recovery and reproduction of the polyester.
The recovery rate of polyester is improved, the processing process is simplified, and the obtained recycled and remade polyester is reusable, and the treatment method is environmentally friendly, meets environmental protection requirements, and improves resource utilization efficiency.
Smart Images

Figure CN119060407A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a release film processing method and an object manufacturing method, in particular to a release film processing method containing polyester and an object manufacturing method containing polyester. Background Art
[0002] A release film usually includes a corresponding substrate and a release layer thereon, wherein the release layer can be adhered to an object and can separate the object from the release layer after proper use. Therefore, release films are often widely used in life or manufacturing. Generally speaking, the used release films are often discarded as general waste and then treated as waste by incineration or landfill.
[0003] In 1990, the United Nations Environment Programme (UNEP) proposed the concept of "cleaner production". Cleaner production includes reducing pollutants or waste in the product manufacturing process, or saving energy or materials in the product manufacturing process to achieve reasonable resource utilization. In addition, the European Parliament and the Council of the European Union passed a directive on reducing plastic products and plastic waste (i.e., Directive (EU) 2019 / 904) in 2019. Therefore, with the rise of environmental awareness today, how to effectively recycle the useful materials has become a current research topic. Summary of the invention
[0004] The present invention is directed to a method for processing a release film containing polyester and a method for manufacturing an object containing polyester.
[0005] According to an embodiment of the present invention, a method for processing a release film containing polyester includes the following steps: providing a release film, which includes a substrate and a release layer, wherein at least the material of the substrate includes polyester; and subjecting the release film to an acid washing step or an alkaline washing step to remove the release layer to obtain a solid containing polyester.
[0006] According to one embodiment of the present invention, the method for processing a release film containing polyester further comprises the following steps: subjecting the release film to an acid washing step to obtain a first solid containing polyester; and subjecting the first solid to an alkali washing step to obtain a second solid containing polyester.
[0007] According to one embodiment of the present invention, the method for processing a release film containing polyester further comprises the following steps: subjecting the release film to an alkali washing step to obtain a first solid containing polyester; and subjecting the first solid to an acid washing step to obtain a second solid containing polyester.
[0008] According to one embodiment of the present invention, the pickling step comprises the following steps: pickling is performed at least by immersing in an acid solution, wherein the acid equivalent of the acid solution is the same as a mixture of dodecylbenzene sulfonic acid and paraffin oil in a weight ratio of 20:80 to 30:70.
[0009] According to one embodiment of the present invention, the alkali washing step comprises the following steps: alkali washing is performed at least by immersing in alkali solution, wherein the alkali equivalent of the alkali solution is the same as a sodium hydroxide aqueous solution with a weight ratio of 7wt% to 13wt%.
[0010] According to an embodiment of the present invention, the alkali washing step further comprises the following steps: heating to 50°C to 70°C.
[0011] According to an embodiment of the present invention, the release layer is formed by a water-based release agent.
[0012] According to an embodiment of the present invention, the aqueous release agent includes hydrophilic silica gel.
[0013] According to an embodiment of the present invention, a method for treating a release film containing polyester does not use volatile organic solvents during the treatment process.
[0014] According to an embodiment of the present invention, a method for manufacturing a polyester-containing article comprises the following steps: using the recycled polyester obtained or produced by the aforementioned method for processing a release film containing polyester.
[0015] Based on the above, the polyester-containing release film treatment method of the present invention can improve the recovery rate of polyester and / or is relatively simple and / or environmentally friendly. In addition, the obtained or produced recycled polyester can be reused. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 is a schematic diagram of a release film according to an embodiment of the present invention.
[0017] Figure 2 It is a schematic flow chart of the post-use treatment steps of a release film containing polyester or the manufacturing steps of a release film containing polyester according to an embodiment of the present invention.
[0018] Description of Reference Numerals
[0019] 100: Release film;
[0020] 110: base material;
[0021] 120: release layer;
[0022] S11, S12, S20, S30, S40, S51, S52: steps. DETAILED DESCRIPTION
[0023] In the following detailed description, for the purpose of illustration and not limitation, exemplary embodiments that disclose specific details are set forth to provide a thorough understanding of the various principles of the present invention. However, it will be apparent to one of ordinary skill in the art that, with the benefit of this disclosure, the present invention may be practiced in other embodiments that depart from the specific details disclosed herein. In addition, descriptions of well-known devices, methods, and materials may be omitted to avoid obscuring the description of the various principles of the present invention.
[0024] Ranges may be expressed herein as from "about" one particular value to "about" another particular value, which may also be expressed directly as one particular value and / or to another particular value. When expressing the range, another embodiment includes from the one particular value and / or to the other particular value. Similarly, when a value is expressed as an approximation by using the antecedent "about," it will be understood that the particular value forms another embodiment. It will be further understood that the endpoints of each range may be expressly related to or independent of the other endpoint.
[0025] In this document, non-limiting terms (such as: may, can, for example or other similar terms) mean that implementation, inclusion, addition or existence are optional or necessary.
[0026] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by those of ordinary skill in the art to which the present invention belongs. It will also be understood that terms (such as those defined in commonly used dictionaries) should be interpreted as having a meaning consistent with their meaning in the relevant technical context and should not be interpreted in an idealized or overly formal sense unless explicitly defined as such herein.
[0027] [Release film]
[0028] Figure 1 It is a cross-sectional schematic diagram of a release film according to an embodiment of the present invention.
[0029] Please refer to Figure 1 The release film 100 includes a substrate 110 and a release layer 120 . The release layer 120 is located on the substrate 110 .
[0030] In one embodiment, the material of the substrate 110 may include polyester.
[0031] It should be noted that the term "polyester" herein includes polymers commonly referred to as polyesters, particularly aromatic polyesters, and particularly refers to polyesters derived from purified terephthalic acid (PTA) and ethylene glycol (EG) (i.e., polyethylene terephthalate (PET)).
[0032] In addition, the polyester herein may also be, for example, poly(trimethylene terephthalate), poly(butylene terephthalate), polyethylene naphthalate, or a combination thereof. In this embodiment, the polyester is preferably polyethylene terephthalate, poly(trimethylene terephthalate), or a combination thereof. In addition, copolymers may also be used, which particularly refer to copolymers that can be obtained by using two or more dicarboxylic acids and / or two or more diol components.
[0033] In one embodiment, the material of the substrate 110 does not include polyurethane (e.g., polyurethane resin or the like containing polyurethane) or polyacrylic acid (e.g., acrylic resin, polymethyl methacrylate or the like containing polyacrylic acid). In the case where a polyester substrate is used as the substrate 110, if the material of a substrate similar to the substrate 110 includes polyurethane (PU) or polyacrylate, the recycling difficulty or complexity may be increased.
[0034] In one embodiment, the release layer 120 may be formed of a water-based release agent.
[0035] In one embodiment, the solubility of the aqueous release agent in water or an aqueous solution (e.g., an acidic aqueous solution, an alkaline aqueous solution, or a neutral aqueous solution) is greater than its solubility in the lipophilic organic solution. If the aforementioned lipophilic organic solution is mixed with pure water in a normal state (e.g., without any surfactant, without any reactant, without violent or prolonged shaking or stirring), there may be a corresponding interface (interface; often referred to as: organic-aqueous interface) between the aforementioned lipophilic organic solution and the pure water. The aforementioned lipophilic organic solution may include, but is not limited to: toluene, methyl isobutyl ketone (MIBK), hexane, methylethyl ketone (MEK), or a co-solvent including the aforementioned.
[0036] In one embodiment, the aqueous release agent may include hydrophilic silica gel. The hydrophilic silica gel may include a polymeric main body as shown in the following [Formula 1].
[0037] [Formula 1]
[0038]
[0039] In [Formula 1], n may be a positive integer from 5 to 200. Each R1 may be the same or different. Each R2 may be the same or different. R1 and R2 may be the same or different.
[0040] In one embodiment, R1 or R2 may include a hydrophilic side chain. The hydrophilic side chain may include a functional group having an amide bond, a phosphorylcholine functional group, or a hydroxyl group, but the present invention is not limited thereto.
[0041] In one embodiment, the end of [Formula 1] may include a hydroxyl group or other suitable hydrophilic groups, but the present invention is not limited thereto.
[0042] In one embodiment, the release film 100 may be manufactured as follows: providing a substrate 110; forming a water-based release agent on the substrate by coating, laminating or other suitable methods; and curing the water-based release agent formed on the substrate by drying, standing or other suitable methods to form a corresponding release layer (i.e., the cured water-based release agent) 120. In one embodiment, the aforementioned manufacturing method may be performed by a common roll-to-roll manufacturing device, but the present invention is not limited thereto. In one embodiment, a corresponding easy-to-peel layer may be attached to the release layer 120, but the present invention is not limited thereto.
[0043] In one embodiment, the release film 100 may be used in ways including but not limited to: with the release layer 120 of the release film 100 facing the object to be attached, the release layer 120 of the release film 100 is attached to the appropriate part of the object. Taking the manufacture of multi-layer ceramic capacitors (MLCC) as an example, a ceramic sheet may be attached to the release film 100 first. The release film 100 may be used to carry the ceramic sheet thereon and provide a subsequent release effect, so as to be suitable for the corresponding multi-layer ceramic capacitor manufacturing process on the ceramic sheet attached thereon. However, after the aforementioned manufacturing process is completed, the release film 100 will be peeled off.
[0044] In one embodiment, before the release layer 120 is attached to a suitable object, the easy-to-peel layer (if any) attached thereto may be peeled off first.
[0045] [Release film treatment after use]
[0046] Compared to the release film before use (e.g., the same or similar to the release film 100 described above), the release film after use may have slight changes in appearance or material. For example, the release film after use may have slight signs of use such as damage and creases in appearance; and / or, the release film after use may have changes in the detailed structure and / or material surface due to heating, ventilation, lighting, etc. in the corresponding manufacturing process, but the above changes do not basically affect the overall nature (e.g., a release layer composed of hydrophilic silicone and / or a substrate composed of polyester) and / or the subsequent processing methods. Therefore, for the sake of simplicity, the same terms are still used in the subsequent processing methods. For example, the release film after use can still be called a release film, and the release film after use still includes the corresponding substrate and release layer.
[0047] The release film after use can be removed from the substrate by acid washing or alkali washing.
[0048] In one embodiment, before the aforementioned acid washing or alkali washing, the used release film can be reduced in size by a quick or simple physical method (such as shearing, cutting, slicing or dicing, but not limited to).
[0049] In one embodiment, the used release film can be immersed in an alkali solution to remove the release layer on the substrate. In one embodiment, the alkali solution can be, for example, an aqueous solution of sodium hydroxide of about 7wt% to 13wt% or an alkaline aqueous solution of the same alkali equivalent. In one embodiment, the alkali solution can be, for example, an aqueous solution of sodium hydroxide of about 10wt% or an alkaline aqueous solution of the same alkali equivalent. In one embodiment, the alkali solution can be an alkaline aqueous solution of the same alkali equivalent (alkali equivalent) or hydroxyl ion equivalent (hydroxyl ion equivalent) as the aforementioned aqueous solution of sodium hydroxide.
[0050] In one embodiment, the used release film may be appropriately heated during the process of being immersed in the alkaline solution. In one embodiment, the temperature may be heated to about 50° C. to 70° C. In one embodiment, the temperature may be heated to about 60° C.
[0051] In one embodiment, the temperature may be about 50° C. to 70° C. for about 0.5 to 2 hours. In one embodiment, the temperature may be about 60° C. for about 0.5 to 2 hours.
[0052] In one embodiment, the aforementioned alkali washing method may cause a corresponding chain cleavage reaction between silicon and oxygen in the release layer. In one embodiment, the residue generated after the aforementioned alkali washing chain cleavage reaction may further produce a corresponding depolymerization by backbiting to form a silicon-oxygen compound suitable for removal by water washing.
[0053] In one embodiment, the polyester-containing substrate is substantially insoluble (eg, the dissolved mass is less than or equal to 100 ppm) in the alkaline solution used for alkaline washing.
[0054] In one embodiment, the release film after use can be immersed in an acid solution to remove the release layer on the substrate. In one embodiment, the acid solution can be, for example, an acidic oil solution of dodecylbenzene sulfonic acid and paraffin oil, wherein the weight ratio of dodecylbenzene sulfonic acid and paraffin oil is about 20:80 to 30:70. In one embodiment, the acid solution can be, for example, an acidic oil solution of dodecylbenzene sulfonic acid and paraffin oil, wherein the weight ratio of dodecylbenzene sulfonic acid and paraffin oil is about 25:75. In one embodiment, the acid solution can be an acidic oil solution with the same acid equivalent (acid equivalent) or hydrogen ion equivalent (hydrogen ion equivalent) as the aforementioned mixed solution containing dodecylbenzene sulfonic acid and paraffin oil.
[0055] In one embodiment, the aforementioned acid washing method may cause a corresponding chain cleavage reaction between silicon and oxygen in the release layer. In one embodiment, the residue generated after the aforementioned acid washing chain cleavage reaction may further produce a corresponding depolymerization by backbiting to form a silicon-oxygen compound suitable for removal by water washing.
[0056] In one embodiment, the polyester-containing substrate is substantially insoluble (eg, the dissolved mass is less than or equal to 100 ppm) in the acid solution used for pickling.
[0057] In one embodiment, the above-mentioned corresponding backbiting depolymerization generates a silicon-oxygen compound suitable for being removed by washing with water, and its chemical formula can be shown as the following [Formula 2].
[0058] [Formula 2]
[0059]
[0060] In one embodiment, after the aforementioned acid or alkaline cleaning, most of the release layer on the original substrate can be removed. In one embodiment, for example, a comparison can be made by weighing to understand the removal rate of the release layer. For example, by comparing before and after the aforementioned acid or alkaline cleaning, the removal rate of the release layer can be more than 95%.
[0061] In one embodiment, the release film after use can be removed from the substrate by acid washing and alkali washing. In addition, the acid washing and alkali washing are not performed at the same time.
[0062] For example, the acid wash can be first performed with an acidic oil solution; then, the solid after the acid wash (which can be referred to as the first solid) can be separated by an appropriate method (such as filtering with a mesh, but not limited to); then, the solid after the acid wash can be selectively rinsed with water (such as pure water or reverse osmosis water); then, the solid after the acid wash can be alkaline washed with an alkaline aqueous solution; then, the solid after the alkaline wash (which can be referred to as the second solid) can be separated by an appropriate method (such as filtering with a mesh, but not limited to).
[0063] For another example, an alkaline washing can be first performed with an alkaline aqueous solution; then, the solid after the alkaline washing (which can be referred to as: the first solid) can be separated by an appropriate method (such as: filtering with a mesh; but not limited to); then, the solid after the alkaline washing is rinsed with water (such as: pure water or reverse osmosis water); then, the solid after the alkaline washing is acid-washed with an acidic oil solution; then, the solid after the acid washing (which can be referred to as: the second solid) can be separated by an appropriate method (such as: filtering with a mesh; but not limited to).
[0064] In one embodiment, taking the comparison before and after the aforementioned acid cleaning and alkali cleaning as an example, the removal rate of the release layer can be above 98%; even above 99%; even closer to 100%.
[0065] In one embodiment, after the aforementioned acid washing and / or alkali washing, the solid matter remaining is a recycled material substantially comprising polyester (eg, recycled polyester-containing substrate in the form of flakes, granules or powder).
[0066] It should be noted that the term "solid" in this article is not limited to the object being completely solid. For example, the "solid" may include a solid in the form of flakes, strips, powders and / or granules; and a liquid attached to the solid or located between two solids by capillary phenomena. The "solid" can be dried in an appropriate manner (such as heating and / or drying under reduced pressure) to obtain a solid that is almost free of liquid. Based on the total weight of the "solid", the weight of the solid after drying can be about 80% or more; preferably about 90% or more; and more preferably about 95% or more.
[0067] In one embodiment, the post-use release film treatment process substantially does not use common volatile organic solvents. Volatile organic solvents are substantially organic solvents or co-solvents containing volatile organic compounds (VOCs). Common volatile organic solvents may include, but are not limited to, formaldehyde, methanol, formic acid, toluene, methyl isobutyl ketone (MIBK), dichloromethane (DCM), trichloroethylene, acetonitrile (ACN), ethyl acetate (EA), hexane, acetone (DMK), isopropanol (IPA), methyl ethyl ketone (MEK), dimethylacetamide (DMAC), dimethylformamide (DMF), proprylene glycol monomethyl ether (PM), diethyl ether, butanol, methyl tert-butyl ether (MTBE), chloroform, or a co-solvent thereof. Therefore, the processing can be simpler (eg, easier to comply with relevant laws and regulations) and / or eco-friendly.
[0068] [Recycling of polyester]
[0069] Recycled materials including polyester can basically be recycled and reused by appropriate means (such as polyester granulation, but not limited to). The recycling methods include, but are not limited to, the manufacture of fabrics, containers, plates, packaging materials, films and other polyester-containing objects. For example, the recycled polyester can be properly remade to make a substrate (such as the same or similar to the aforementioned release film) suitable for release films (such as the same or similar to the aforementioned release films).
[0070] The processing methods of recycled polyester include physical reprocessing or chemical reprocessing. Physical reprocessing includes using an extruder to melt the treated polyester and then extrude it into granules. Chemical reprocessing includes using a chemical depolymerization liquid to depolymerize the recycled polyester, and then repolymerizing the monomers and / or oligomers obtained after depolymerization under specific conditions, and then granulating; the chemical depolymerization liquid can be water, methanol, ethanol, ethylene glycol, diethylene glycol or any combination.
[0071] In one embodiment, the polyester recovery rate can be greater than or equal to 90% by weight. In one example, the polyester recovery rate can be greater than or equal to 92.4%.
[0072] [Step of manufacturing a release film containing polyester or step of treating a release film containing polyester after use]
[0073] Figure 2 It is a schematic flow chart of the manufacturing steps of a release film containing polyester or the post-use processing steps of a release film containing polyester according to an embodiment of the present invention, and the process may include the following steps.
[0074] Step S11: providing a release agent.
[0075] Step S12: providing a substrate containing polyester.
[0076] Step S20: forming a release agent on the substrate to manufacture a release film. The release film includes a substrate and a release layer on the substrate.
[0077] Step S30: using the release film; and recycling the used release film.
[0078] Step S40: removing the release layer on the substrate by acid washing or alkali washing.
[0079] Step S51: Wastewater after acid washing or alkali washing
[0080] Step S52: Recycling / reusing the solids after acid washing or alkali washing to recover polyester
[0081] In addition, the recycled-PET (r-PET) obtained or produced in step S52 can be (but not limited to) used in the subsequent step S12.
[0082] Based on the above, the method for treating the release film containing polyester of the present invention can improve the recovery rate of polyester and / or is relatively simple and / or environmentally friendly.
[0083] [Practicality]
[0084] By using the method of the present invention, the polyester in the release film after use can be recovered. Furthermore, the recovered polyester can be reused. The reuse method includes, but is not limited to, the manufacture of polyester-containing objects such as fabrics, containers, plates, packaging materials, and films.
[0085] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for treating a release film containing polyester, characterized in that: include: A release film is provided, comprising a substrate and a release layer, wherein at least the substrate is made of polyester; and The release film is subjected to an acid washing step or an alkali washing step to remove the release layer, so as to obtain a solid object containing polyester.
2. The method for processing a release film containing polyester according to claim 1, characterized in that: Also includes: The release film is subjected to the acid washing step to obtain a first solid containing polyester; as well as The first solid is subjected to the alkali washing step to obtain a second solid containing polyester.
3. The method for processing a release film containing polyester according to claim 1, characterized in that: Also includes: The release film is subjected to the alkali washing step to obtain a first solid containing polyester; as well as The first solid is subjected to the acid washing step to obtain a second solid containing polyester.
4. The method for treating a release film containing polyester according to any one of claims 1 to 3, characterized in that: The pickling step comprises: The pickling is performed at least by immersing in an acid solution, wherein the acid equivalent of the acid solution is the same as a mixture of dodecylbenzenesulfonic acid and paraffin oil in a weight ratio of 20:80 to 30:
70.
5. The method for treating a release film containing polyester according to any one of claims 1 to 3, characterized in that: Wherein the alkali washing step comprises: The alkali washing is carried out at least by immersing in alkali solution, wherein the alkali equivalent of the alkali solution is the same as that of a sodium hydroxide aqueous solution with a weight ratio of 7wt% to 13wt%.
6. The method for treating a release film containing polyester according to claim 5, characterized in that: The alkali washing step further comprises: Heat to 50℃~70℃.
7. The method for treating a release film containing polyester according to claim 1, characterized in that: The release layer is formed by a water-based release agent.
8. The method for treating a release film containing polyester according to claim 7, characterized in that: The aqueous release agent comprises hydrophilic silica gel.
9. The method for treating a release film containing polyester according to claim 1, characterized in that: No volatile organic solvents are used in the process.
10. A method for producing an article containing polyester, characterized in that: include: The recycled polyester obtained or produced by the method for treating a release film containing polyester as described in claim 1.