Well cementation method, well cementation structure and fracturing method for preventing casing deformation in fracturing process
By injecting conventional and foam cement slurry into the casing string of the oil and gas well to form an annular space, and using the buffering effect of the foam cement ring and the blocking function of the packer, the problem of casing deformation during fracturing is solved, and the improvement of the Recovery and wellbore sealing.
Patent Information
- Application Number
- CN202310651962.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-02
- Publication Date
- 2024-12-03
AI Technical Summary
Oil and gas wells are prone to casing deformation during fracturing, resulting in a decrease in the number of fracturing sections and a decrease in recovery rate. The existing prevention and control methods are not effective.
Install the packer at the preset position of the casing string, and inject conventional cement slurry and foam cement slurry into the vertical, oblique and horizontal sections of the wellbore to form an annular space to solidify, and the foam cement ring occurs during fracturing. The strength damage forms a buffer zone, reducing the shear load on the casing by the formation slip, and blocking the flow channels in the third annex through the packer to prevent fracturing fluid from flowing.
It effectively prevents casing deformation, ensures the smooth implementation of fracturing operations and wellbore sealing, and improves the recovery rate of oil and gas wells.
Smart Images

Figure CN119062278A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of oil and gas well drilling and production, and in particular to a cementing method for preventing casing deformation during fracturing and a cementing structure formed by the cementing method. On this basis, the present invention also relates to a fracturing method for preventing casing deformation during fracturing. Background Art
[0002] The development of oil and gas has a positive significance in alleviating the increasing demand for energy. Staged fracturing is an important means to improve the development results of oil and gas wells. However, during the fracturing process, oil and gas wells are prone to serious casing deformation problems. In some shale gas blocks, the number of oil and gas wells with casing deformation even exceeds 50%. Casing deformation causes a reduction in the number of fracturing stages, which ultimately leads to a serious reduction in the production and recovery rate of a single oil and gas well.
[0003] The current research results on the problem of casing deformation during fracturing show that the main reason for casing deformation is that when the fracturing fluid activates the formation, the formation slips and shears the casing of the oil and gas well, resulting in shear deformation of the casing. At present, a variety of methods for preventing and controlling casing deformation in oil and gas wells during fracturing have been proposed, mainly by reducing formation slip and reducing casing shear load to achieve the purpose of reducing casing deformation.
[0004] Among them, by optimizing the fracturing process to reduce formation activation and slippage, the effect of reducing casing shear deformation is not obvious due to the great influence of natural geological conditions; by taking measures such as: wrapping the casing with rubber, increasing the strength of the casing steel, increasing the casing wall thickness, reducing the casing inner diameter and floating bead cement slurry system to reduce the casing shear load, but the problem of casing shear deformation still exists in large numbers, indicating that the prevention and control effects of the above-mentioned methods are still not obvious.
[0005] Therefore, how to effectively prevent and control casing deformation during the fracturing process is an urgent problem to be solved. Summary of the invention
[0006] The purpose of the present invention is to overcome the problem of casing deformation during oil and gas well fracturing in the prior art and to provide a cementing method for preventing and controlling casing deformation during fracturing. The cementing method can effectively solve the problem of casing deformation during oil and gas well fracturing.
[0007] In order to achieve the above object, the present invention provides a cementing method for preventing casing deformation during fracturing, comprising the following steps:
[0008] S1, installing a packer at a preset position of the casing string;
[0009] S2, running the casing string into a wellbore including a vertical section, a deflection section, and a horizontal section, so that the casing string is close to the bottom of the wellbore;
[0010] S3, injecting conventional cement slurry into a first annulus formed by the inner wall of the vertical section and the outer wall of the casing string and a second annulus formed by the inner wall of the deflection section and the outer wall of the casing string, and injecting foam cement slurry into a third annulus formed by the inner wall of the horizontal section and the outer wall of the casing string;
[0011] S4, opening the packer to isolate the third annulus;
[0012] S5, waiting for solidification, so that the conventional cement slurry solidifies into a conventional cement ring, and the foam cement slurry solidifies into a foam cement ring, and the foam cement ring can undergo strength destruction to form a buffer zone in the third annulus.
[0013] Preferably, the casing string in the horizontal section includes a fracturing section and a non-fracturing section, and the packer is installed on the non-fracturing section.
[0014] Preferably, step S3 includes the following sub-steps:
[0015] S31, respectively calculating the volume V of the first annulus 1 , the volume of the second annulus V 2 and the volume V of the third annulus 3 ;
[0016] S32, injecting a volume of V into the casing string from the wellhead of the wellbore 1 +V 2 The conventional cement paste and volume V 3 The foamed cement slurry;
[0017] S33, inserting a pressure-holding and impact-pressure integrated plug from the wellhead into the casing string;
[0018] S34, injecting a slurry displacement fluid into the casing string from the wellhead, the slurry displacement fluid moves toward the bottom of the well by pushing the pressure-holding and impact-pressure integrated plug, thereby pushing the conventional cement slurry and the foam cement slurry to move, until the conventional cement slurry moves into the first annulus and the second annulus, and the foam cement slurry moves into the third annulus.
[0019] Preferably, the pressure-holding and impact-pressure integrated plug comprises a pressure-holding plug and a impact-pressure plug which are arranged at two axial ends opposite to each other, the pressure-holding plug can cooperate with a pressure-holding coupling arranged at the bottom of the casing string, the impact-pressure plug is in contact with the slurry displacement fluid and can isolate the slurry displacement fluid from the foam cement slurry.
[0020] Preferably, in step S4, the slurry displacement fluid is continuously injected into the casing string to open the packer.
[0021] Preferably, an open pressure step for returning the pressure at the wellhead of the wellbore to zero is further included between step S4 and step S5.
[0022] Preferably, the foamed cement slurry comprises a foamed cement slurry base slurry, a gas for foaming the foamed cement slurry base slurry, and an additive for stabilizing bubbles.
[0023] A second aspect of the present invention provides a cementing structure for preventing casing deformation during a fracturing process. The cementing structure is formed by the above-mentioned cementing method. The cementing structure includes the wellbore, the casing string, the packer, the conventional cement ring filled in the first annulus and the second annulus, and the foam cement ring filled in the third annulus.
[0024] A third aspect of the present invention provides a fracturing method for preventing casing deformation during the fracturing process. The fracturing method is applicable to the above-mentioned cementing structure, and fracturing cracks are formed in the formation by performing perforation fracturing operations at positions other than the preset positions of the casing string.
[0025] Preferably, after the perforation and fracturing operation, a fracturing bridge plug is lowered into the casing string to prevent the fracturing fluid in the fracturing cracks from flowing into the casing string.
[0026] Foam cement slurry is usually used to solve the formation leakage problem during cementing construction. By utilizing its low density and high compressive strength, the foam cement ring formed by its solidification can neither cause formation leakage nor self-strength damage during the fracturing process. However, in the above technical scheme of the present invention, by using foam cement slurry with low elastic modulus and low compressive strength to form a foam cement ring, the formation slip caused by the fracturing process acts on the foam cement ring, and the strength of the foam cement ring may be damaged, thereby forming a buffer zone between the formation and the casing string, reducing the shear load of the formation slip on the casing string, and finally reducing the shear deformation of the casing. At the same time, after the foam cement ring is damaged in strength, a flow channel can be formed in the third annulus, which is easy to cause the fracturing fluid to flow in the third annulus during the subsequent fracturing process. Therefore, a packer is installed at a preset position of the casing string, and the third annulus is sealed by opening the packer, blocking the flow channel in the third annulus, and finally preventing the fracturing fluid from flowing in the third annulus, ensuring the smooth implementation of the fracturing operation and the integrity of the wellbore seal. Ultimately, the technical effect of ensuring the effective implementation of fracturing operations and the sealing capability of the wellbore annulus, and preventing casing deformation during the fracturing process of oil and gas wells is achieved. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 is a flow chart of an embodiment of the cementing method of the present invention;
[0028] Figure 2is a schematic diagram of the injection foam cement slurry and conventional cement slurry of the present invention;
[0029] Figure 3 It is a schematic diagram of the packer of the present invention opening and separating the third annulus;
[0030] Figure 4 It is a schematic diagram of the perforation and fracturing operation of the present invention.
[0031] Description of Reference Numerals
[0032] 1- casing string; 2- conventional cement slurry; 3- wellhead;
[0033] 4-Foam cement slurry; 5-Packer; 6-Pressure-holding and impact-pressure integrated plug;
[0034] 7-Fracturing bridge plug; 8-Fracturing crack. DETAILED DESCRIPTION
[0035] The following is a further detailed description of the embodiments of the present invention in conjunction with the accompanying drawings and examples. The detailed description of the following embodiments and the accompanying drawings are used to exemplarily illustrate the principles of the present invention, but cannot be used to limit the scope of the present invention. The present invention can be implemented in many different forms and is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.
[0036] The present invention provides these embodiments to make the present invention thorough and complete, and fully express the scope of the present invention to those skilled in the art. It should be noted that unless otherwise specifically stated, the relative arrangement of the parts and steps, the composition of materials, numerical expressions and numerical values set forth in these embodiments should be interpreted as being merely exemplary, rather than as limiting.
[0037] It should be noted that, in the description of the present invention, unless otherwise specified, the meaning of "multiple" is greater than or equal to two; the terms "front", "rear", "inside", "outside" and the like indicate directions or positional relationships only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.
[0038] In addition, the words "first", "second", "third" and the like used in the present invention do not indicate any order, quantity or importance, but are only used to distinguish different parts. "Vertical" is not strictly vertical, but is within the tolerance range. "Horizontal" is not strictly horizontal, but is within the tolerance range. "Include" or "comprising" and the like mean that the elements before the word include the elements listed after the word, and do not exclude the possibility of including other elements.
[0039] It should also be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances. When a specific device is described as being located between a first device and a second device, there may or may not be an intermediate device between the specific device and the first device or the second device.
[0040] All terms used in the present invention have the same meanings as those understood by ordinary technicians in the field to which the present invention belongs, unless otherwise specifically defined. It should also be understood that terms defined in general dictionaries, such as general dictionaries, should be interpreted as having meanings consistent with their meanings in the context of the relevant technology, and should not be interpreted in an idealized or extremely formal sense, unless explicitly defined herein.
[0041] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered part of the specification.
[0042] The first aspect of the present invention provides a cementing method for preventing casing deformation during fracturing, referring to Figures 1 to 3 , the cementing method may include the following steps:
[0043] S1, installing a packer 5 at a preset position of the casing string 1;
[0044] S2, running a casing string 1 into a wellbore including a vertical section, a deflection section, and a horizontal section, so that the casing string 1 is close to the bottom of the wellbore;
[0045] S3, injecting conventional cement slurry 2 into the first annulus formed by the inner wall of the vertical section and the outer wall of the casing string 1 and the second annulus formed by the inner wall of the deflection section and the outer wall of the casing string 1, and injecting foam cement slurry 4 into the third annulus formed by the inner wall of the horizontal section and the outer wall of the casing string 1;
[0046] S4, opening the packer 5 to seal the third annulus;
[0047] S5, waiting for solidification, so that the conventional cement slurry 2 solidifies into a conventional cement annulus, and the foamed cement slurry 4 solidifies into a foamed cement annulus, and the foamed cement annulus can undergo strength destruction to form a buffer zone in the third annulus.
[0048] In the above technical scheme of the present invention, a foam cement ring is formed by using a foam cement slurry with a low elastic modulus and low compressive strength. The formation slip caused by the fracturing process acts on the foam cement ring, which may cause the strength of the foam cement ring to be destroyed, thereby forming a buffer zone between the formation and the casing string, reducing the shear load of the formation slip on the casing string, and finally reducing the shear deformation of the casing. At the same time, after the foam cement ring is damaged in strength, a flow channel can be formed in the third annulus, which is easy to cause the fracturing fluid to flow in the third annulus during the subsequent fracturing process. Therefore, a packer is installed at a preset position of the casing string, and the third annulus is sealed by opening the packer, blocking the flow channel in the third annulus, and finally preventing the fracturing fluid from flowing in the third annulus, ensuring the smooth implementation of the fracturing operation and the integrity of the wellbore seal. Finally, the technical effect of ensuring the effective implementation of the fracturing operation and the wellbore annulus sealing capacity and preventing the casing deformation during the fracturing process of the oil and gas well is achieved.
[0049] like Figure 3 As shown, the casing string 1 in the horizontal section includes a fracturing section and a non-fracturing section, and the packer 5 is installed on the non-fracturing section. That is, the preset position on the casing string 1 for installing the packer 5 is the non-fracturing section, and the number of packers 5 is equal to the number of non-fracturing sections. It should be noted that there are multiple fracturing sections and non-fracturing sections, and the fracturing sections and non-fracturing sections are arranged alternately on the casing string 1 in the horizontal section, that is, the packers 5 and the fracturing sections are arranged alternately. It should also be noted that the packer 5 has a closed and an open state. When the pressure in the casing string 1 reaches the activation pressure of the packer 5, the packer 5 opens, and at this time the packer 5 can isolate the annulus where it is located. Therefore, in the present invention, by opening the packer 5, multiple fracturing sections can be isolated in the third annulus, so that no fluid flow channel can be formed between the multiple fracturing sections.
[0050] In addition, refer to Figures 2 to 3 , step S3 may include the following sub-steps:
[0051] S31, calculate the volume V of the first annulus respectively 1 , the volume of the second annulus V 2 and the volume of the third annulus V 3 ;
[0052] S32, inject a volume of V into the casing string 1 from the wellhead 3 of the wellbore. 1 +V 2 The conventional cement paste and volume V 3 Foam cement slurry 4;
[0053] S33, inserting the pressure holding and impact pressure integrated plug 6 from the wellhead 3 into the casing string 1;
[0054] S34, inject slurry replacement fluid into the casing string 1 from the wellhead 3, and the slurry replacement fluid moves toward the bottom of the well by pushing the pressure-holding and impact-pressure integrated plug 6, thereby pushing the conventional cement slurry 2 and the foam cement slurry 4 to move, until the conventional cement slurry 2 moves into the first annulus and the second annulus, and the foam cement slurry 4 moves into the third annulus.
[0055] In the above, the volume of the first annulus V 1 , the volume of the second annulus V 2 and the volume of the third annulus V 3 The calculation formula can be:
[0056]
[0057]
[0058]
[0059] Among them, D 01 is the inner diameter of the vertical section of the wellbore, D 11 is the outer diameter of the casing string in the vertical section, L 1 is the wellbore depth of the vertical section, D 02 D is the inner diameter of the wellbore’s deflection section, 12 L is the outer diameter of the casing string in the deflection section, 2 is the depth of the wellbore in the deflection section, D 03 is the inner diameter of the horizontal section of the wellbore, D 13 is the outer diameter of the casing string in the horizontal section, L 3 is the wellbore depth of the horizontal section.
[0060] In addition, in sub-steps S32 to S34, the pressure-holding and impact-pressure integrated plug 6 between the slurry replacement fluid and the foam cement slurry 4 can isolate the slurry replacement fluid from the foam cement slurry 4. The slurry replacement fluid is injected into the casing string 1 to form a slurry replacement fluid column in the casing string 1. Under the gravity of the slurry replacement fluid column, the pressure-holding and impact-pressure integrated plug 6 can be pushed to move toward the bottom of the well, thereby pushing the conventional cement slurry 2 and the foam cement slurry 4 to move, until the pressure-holding and impact-pressure integrated plug 6 moves to the bottom of the casing string 1, and a sealing structure is formed at the bottom of the casing string 1, so that the slurry replacement fluid cannot continue to flow to the bottom of the well. At this time, the conventional cement slurry 2 moves to the first annulus and the second annulus, and the foam cement slurry 4 moves to the third annulus. The slurry replacement fluid is any liquid that can push the pressure-holding and impact-pressure integrated plug 6 to move, for example, the slurry replacement fluid can be a liquid such as drilling fluid or clean water.
[0061] Further, the pressure-holding and impact-pressure integrated plug 6 may include a pressure-holding plug and a impact-pressure plug that are arranged at two axial ends opposite to each other, and it is stipulated that along the wellbore direction, the position close to the bottom of the well is the front, and the position away from the bottom of the well is the rear. The pressure-holding plug is located at the front of the pressure-holding and impact-pressure integrated plug 6, and the impact-pressure plug is located at the rear of the pressure-holding and impact-pressure integrated plug 6. The pressure-holding plug can cooperate with the pressure-holding coupling arranged at the bottom of the casing string 1. The impact-pressure plug contacts the displacement fluid, and the displacement fluid can be isolated from the foam cement slurry 4, and the casing string 1 can be sealed. When the displacement fluid pushes the pressure-holding plug to the pressure-holding coupling arranged at the bottom of the casing string 1, the conventional cement slurry 2 moves to the first annulus and the second annulus, the foam cement slurry moves to the third annulus, and the pressure-holding and impact-pressure integrated plug 6 and the pressure-holding coupling at the bottom of the casing string 1 form a sealing structure, and the displacement fluid cannot continue to flow to the bottom of the well.
[0062] Further, refer to Figure 3 In step S4, the slurry displacement fluid is continuously injected into the casing string 1. At this time, the pressure-holding and impact-pressure integrated plug 6 forms a sealing structure at the bottom of the casing string 1, so that the slurry displacement fluid cannot continue to flow to the bottom of the well. Therefore, the slurry displacement fluid is continuously injected into the casing string 1, so that the pressure in the casing string 1 continues to increase. When the pressure in the casing string 1 increases to the activation pressure of the packer 5, the packer 5 opens to isolate the third annulus.
[0063] Furthermore, between step S4 and step S5, there is also an open pressure step for returning the pressure of the wellhead 3 of the wellbore to zero. In step S4, the pressure in the casing string 1 is increased to the activation pressure of the packer 5 by continuing to inject the displacement fluid, and after the packer 5 is opened, the injection of the displacement fluid is stopped. At this time, since the pressure of the wellhead 3 is higher than the atmospheric pressure, the displacement fluid in the casing string 1 can flow back to the wellhead 3, and the pressure of the wellhead 3 continues to decrease until the pressure of the wellhead 3 is equal to the atmospheric pressure, and then step S5 is prepared.
[0064] It should also be noted that the conventional cement slurry 2 used in the embodiment of the present invention includes dry cement, water and admixtures, and the admixtures may be one or more of weighting agents, lightening agents, retarders, accelerators, drag reducers, fluid loss agents and leakage control agents, or other admixtures not listed above but which can make the conventional cement slurry 2 have certain special functions. Conventional cement slurry 2 that meets the requirements of cementing operations is prepared by mixing water and dry cement in a certain proportion and adding appropriate admixtures. Conventional cement slurry 2 can be divided into conventional low-density cement slurry, conventional density cement slurry and high-density cement slurry according to its density.
[0065] Furthermore, the foamed cement slurry 4 includes a foamed cement slurry base slurry, a gas for foaming the foamed cement slurry base slurry, and an additive for stabilizing bubbles.
[0066] It should also be noted that the foamed cement slurry base slurry can be one of conventional low-density cement slurry, conventional density cement slurry and high-density cement slurry, and the gas used for foaming the foamed cement slurry base slurry can be air or other gases, preferably nitrogen. In addition, the gas used for foaming the foamed cement slurry base slurry can be obtained by chemical reaction, for example, a gas-generating substance is added to dry cement ash, and when the dry cement ash mixture meets water, the gas-generating substance reacts chemically with the foamed cement slurry base slurry to produce gas, and these gases are dispersed in the foamed cement slurry base slurry to form foamed cement slurry 4, and finally additives are added to extend the life of the bubbles and improve the stability of the foamed cement slurry 4. Preferably, an air supply device is provided, and the gas in the air supply device is injected into the foamed cement slurry base slurry by mechanical inflation to form the foamed cement slurry 4.
[0067] In addition, the density of the foam cement slurry 4 can be adjusted according to the formation conditions and the need to prevent casing deformation during the fracturing process, so that the formation slip caused by the fracturing process acts on the foam cement ring formed by the foam cement slurry 4, which can cause the strength of the foam cement ring to be destroyed, thereby forming a buffer zone between the formation and the casing. Based on the set density of the foam cement slurry 4, the amount of gas that needs to be injected into the foam cement slurry base slurry can be calculated, wherein the calculation formula for the gas volume injected into the foam cement slurry base slurry is as follows:
[0068]
[0069] In the above formula, V g is the gas volume under standard conditions, ρ s is the density of foam cement slurry base, ρ f is the density of foam cement slurry, ρ g is the gas density, V s is the volume of foam cement slurry base slurry, P st is the pressure under standard conditions, P is the pressure in the wellbore, T st is the temperature under standard pressure, T is the temperature inside the wellbore, and Z is the gas compressibility factor.
[0070] The cementing method of the present invention is described below by taking a horizontal well located in a mining area where casing deformation is serious as an example:
[0071] Well W1 is a horizontal shale gas well. Through drilling operations, its drilling parameters are as follows: completion depth is 6325.0m, of which the vertical section is 0.0~3320.0m, the deflection section is 3320.0~4630.0m, the horizontal section is 4630.0~6325.0m, the A target well depth is 4630.0m, the B target well depth is 6320.0m, and 17 fracturing sections are designed for the horizontal section. Since Well W1 is located in a shale gas block with severe casing deformation, and the shale gas horizontal wells adjacent to Well W1 in the shale gas block have already experienced casing deformation during the fracturing process, it is planned to adopt the cementing method for preventing and controlling casing deformation during the fracturing process provided by the present invention for Well W1, with reference to Figures 1 to 4 The specific implementation process is as follows:
[0072] (1) Install the packer 5 at the preset position of the casing string 1. The preset position for installing the packer 5 is the non-fracture section on the casing string 1 in the horizontal section. The casing string 1 in the horizontal section is designed with 17 fracturing sections and 17 non-fracture sections. The fracturing sections and non-fracture sections are arranged alternately, and 17 packers 5 are required. The first packer 5 on the casing string 1 is located at a well depth of 6200.0m after the casing string 1 is lowered, and the second packer 5 on the casing string 1 is located at a well depth of 6100.0m after the casing string 1 is lowered, and so on. A packer 5 is installed every 100m on the casing string 1, and a total of 17 packers 5 are installed, and the activation pressure of the packer is 75-85MPa.
[0073] (2) The casing string 1 is lowered, one end of which is connected to the wellhead 3 and the other end is close to the bottom of the well. The drilling fluid is circulated in the wellbore so that the working conditions in the wellbore meet the cementing conditions. The density of the drilling fluid is 1.65 g / cm 3 .
[0074] (3) Calculate the volume V of the first annulus based on the inner diameter of the vertical section, the outer diameter of the casing string 1 in the vertical section, and the wellbore depth of the vertical section. 1 , V is obtained by calculation 1 75m 3 Calculate the volume V of the second annulus according to the inner diameter of the deflection section, the outer diameter of the casing string 1 in the deflection section, and the wellbore depth of the deflection section. 2 , V is obtained by calculation 2 33m 3 ; Calculate the volume V of the third annulus according to the inner diameter of the horizontal section, the outer diameter of the casing string 1 in the horizontal section, and the wellbore depth of the horizontal section 3 , V is obtained by calculation 3 43m 3 .
[0075] (4) According to the formation conditions and the need to prevent casing deformation during fracturing, conventional cement slurry 2 and foam cement slurry 4 are prepared, wherein the conventional cement slurry 2 used for injection into the first annulus described later is prepared to have a density of 1.63 g / cm 3 The conventional low-density cement slurry used for injection into the second annulus described later is configured to have a density of 1.88g / cm 3 The foam cement slurry 4 for injection into the third annulus described later is configured to have a density of 1.70g / cm 3 Foam cement slurry.
[0076] The foam cement slurry 4 is prepared by injecting a certain amount of nitrogen into the foam cement slurry base slurry in a mechanical aeration manner. The amount of nitrogen injected can be calculated by the following calculation formula:
[0077]
[0078] (5) Before starting to inject cement slurry, an isolation fluid is first injected into the casing string 1 to isolate the cement slurry to be injected later from the drilling fluid in the well. Then, a 1.63 g / cm 3 And the volume is 75m 3 Conventional low-density cement slurry with a density of 1.88 g / cm 3 And the volume is 33m 3 High-density cement slurry with a density of 1.70g / cm 3 、Volume 43m 3 of foam cement slurry.
[0079] (6) Insert the pressure-holding and impact-pressure integrated plug 6 into the casing string 1.
[0080] (7) Clean water is injected into the casing string 1. The pressure-holding and pressure-impacting integrated plug 6 can isolate the clean water and cement slurry. Continuous injection of clean water into the casing string 1 can push the pressure-holding and pressure-impacting integrated plug 6 to move toward the bottom of the well until the pressure-holding and pressure-impacting integrated plug 6 moves to the bottom of the casing string 1 and cooperates with the pressure-holding coupling provided at the bottom of the casing string 1 to form a sealing structure. At this time, conventional low-density cement slurry moves into the first annulus, high-density cement slurry moves into the second annulus, and foam cement slurry moves into the third annulus.
[0081] (8) Clean water is continuously injected into the casing string 1. Since the pressure-holding and impact-pressure integrated plug 6 and the pressure-holding coupling of the casing string 1 form a sealing structure, the clean water cannot flow to the bottom of the well, causing the pressure in the casing string 1 to continue to increase. The ground operator observes the pump pressure of the clean water injection pump. When the pump pressure reaches 85 MPa, the packer 5 is activated, and the injection of clean water is stopped at this time.
[0082] (9) Open pressure, clean water reflux, the pressure at the wellhead 3 continues to drop until the pressure at the wellhead 3 is equal to the atmospheric pressure.
[0083] (10) Remove the cementing equipment at the wellhead 3, wait for the conventional low-density cement slurry in the first annulus to solidify into a conventional low-density cement ring, the high-density cement slurry in the second annulus to solidify into a high-density cement ring, and the foam cement slurry in the third annulus to solidify into a foam cement ring, and then complete the cementing operation.
[0084] The second aspect of the present invention provides a cementing structure for preventing casing deformation during fracturing. The cementing structure is formed by adopting the above-mentioned cementing method, and includes a wellbore, a casing string 1, a packer 5, a conventional cement ring filled in the first annulus and the second annulus, and a foam cement ring filled in the third annulus.
[0085] In addition, the third aspect of the present invention provides a fracturing method for preventing casing deformation during fracturing, and the fracturing method is applicable to the above-mentioned cementing structure, referring to Figure 4 , by performing perforation and fracturing operations at positions other than the preset positions of the casing string 1, a fracturing crack 8 is formed in the formation.
[0086] Further, refer to Figure 4 After the perforating and fracturing operation, a fracturing bridge plug 7 is lowered into the casing string 1 to prevent the fracturing fluid in the fracturing cracks 8 from flowing into the casing string 1 .
[0087] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications. Including the combination of various specific technical features in any appropriate manner, in order to avoid unnecessary repetition, the present invention will not further describe various possible combinations. However, these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.
Claims
1. A cementing method for preventing casing deformation during fracturing, characterized in that: The following steps are involved: S1, installing a packer (5) at a preset position of the casing string (1); S2, lowering the casing string (1) into a wellbore including a vertical section, a deflection section, and a horizontal section, so that the casing string (1) is close to the bottom of the wellbore; S3, injecting conventional cement slurry (2) into a first annulus formed by the inner wall of the vertical section and the outer wall of the casing string (1) and a second annulus formed by the inner wall of the deflection section and the outer wall of the casing string (1), and injecting foam cement slurry (4) into a third annulus formed by the inner wall of the horizontal section and the outer wall of the casing string (1); S4, opening the packer (5) to seal the third annulus; S5, waiting for solidification, so that the conventional cement slurry (2) solidifies into a conventional cement ring, and the foam cement slurry (4) solidifies into a foam cement ring, and the foam cement ring can undergo strength destruction to form a buffer zone in the third annulus.
2. The cementing method for preventing casing deformation during fracturing according to claim 1, characterized in that: The casing string (1) in the horizontal section comprises a fracturing section and a non-fracturing section, and the packer (5) is installed on the non-fracturing section.
3. The cementing method for preventing casing deformation during fracturing according to claim 1, characterized in that: Step S3 includes the following sub-steps: S31, respectively calculating the volume V1 of the first annulus, the volume V2 of the second annulus, and the volume V3 of the third annulus; S32, injecting the conventional cement slurry with a volume of V1+V2 and the foam cement slurry (4) with a volume of V3 into the casing string (1) in sequence from the wellhead (3) of the wellbore; S33, inserting a pressure-holding and impact-pressure integrated plug (6) from the wellhead (3) into the casing string (1); S34, injecting a slurry displacement fluid into the casing string (1) from the wellhead (3), the slurry displacement fluid pushes the pressure-holding and impact-pressure integrated plug (6) to move toward the bottom of the well, thereby pushing the conventional cement slurry (2) and the foam cement slurry (4) to move, until the conventional cement slurry (2) moves into the first annulus and the second annulus, and the foam cement slurry (4) moves into the third annulus.
4. The cementing method for preventing casing deformation during fracturing according to claim 3, characterized in that: The pressure-holding and impact-pressure integrated plug (6) comprises a pressure-holding plug and an impact-pressure plug which are arranged at two axial ends opposite to each other, the pressure-holding plug can cooperate with a pressure-holding coupling arranged at the bottom of the casing string (1), and the impact-pressure plug is in contact with the slurry displacement fluid and can isolate the slurry displacement fluid from the foam cement slurry (4).
5. The cementing method for preventing casing deformation during fracturing according to claim 3, characterized in that: In step S4, the grout displacement fluid is continuously injected into the casing string (1) to open the packer (5).
6. The cementing method for preventing casing deformation during fracturing according to claim 1, characterized in that: Between step S4 and step S5, there is also included an open pressure step for returning the pressure of the wellhead (3) of the wellbore to zero.
7. The cementing method for preventing casing deformation during fracturing according to claim 1, characterized in that: The foamed cement slurry (4) comprises a foamed cement slurry base slurry, gas for foaming the foamed cement slurry base slurry, and an additive for stabilizing bubbles.
8. A cementing structure for preventing casing deformation during fracturing, characterized in that: The cementing structure is formed by the cementing method described in any one of claims 1 to 7, and the cementing structure includes the wellbore, the casing string (1), the packer (5), the conventional cement ring filled in the first annulus and the second annulus, and the foam cement ring filled in the third annulus.
9. A fracturing method for preventing casing deformation during fracturing, characterized in that: The cementing structure according to claim 8 is applicable to forming a fracturing crack (8) in the formation by performing a perforation fracturing operation at a position other than the preset position of the casing string (1).
10. The fracturing method for preventing casing deformation during fracturing according to claim 9, characterized in that: After the perforation and fracturing operation, a fracturing bridge plug (7) is lowered into the casing string (1) to prevent the fracturing fluid in the fracturing cracks (8) from flowing into the casing string (1).