Construction method of concrete fiber interface bonding strength prediction model and bonding strength prediction method

Through near-field dynamics simulation and response surface analysis, a prediction model of bond strength of concrete fiber interface was constructed, which solved the problem of measuring interface mechanical parameters and crack evolution in the existing technology, and realized the accurate measurement and evaluation of concrete fiber interface, and made breakthroughs Grid dependency has wide application prospects.

CN119069027APending Publication Date: 2024-12-03QINGDAO UNIV OF TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411045244.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The prior art is difficult to effectively measure the mechanical parameters and crack evolution of concrete fiber interfaces, and the numerical simulation method based on the theory of continuous medium mechanics has grid dependence, which limits its application scope.

Method used

Construct a concrete fiber interface bond strength prediction model, establish a prediction model of interface bond strength through near-field dynamics simulation and response surface analysis, and use computer simulation technology to simulate the fiber extraction process, record displacement, mechanical load and bond break information. The influence of porosity and thickness of the interface transition zone on bond strength is analyzed.

Benefits of technology

Accurate measurement and evaluation of the interface of concrete fibers is achieved, the limitations of difficult to characterize interface mechanical parameters and the evolution of internal cracks in fiber extraction experiments are overcome, and the grid dependence of traditional finite element analysis methods is broken through, and it has broad application prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069027A_ABST
    Figure CN119069027A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of civil engineering materials and near-field dynamics simulation, and particularly relates to a construction method of a concrete fiber interface bonding strength prediction model and a bonding strength prediction method. The method comprises the following steps: 1) constructing a concrete-fiber interface model; 2) setting near-field dynamics simulation parameters; (3) carrying out analogue simulation calculation on the interface bonding performance by utilizing a near-field dynamics method; 4) data processing; and 5) establishing a prediction model F = f (interface parameter) of the bonding strength of the concrete-fiber interface by using a response surface analysis method. According to the method, accurate measurement and evaluation of the concrete-fiber interface bonding strength are realized by utilizing a computer simulation technology, the limitation that interface mechanical parameters and material internal crack evolution are difficult to represent in a fiber pull-out experiment is overcome, and the dependency of a traditional finite element analysis method on grids is broken through.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of civil engineering materials and peridynamic simulation, and particularly relates to a method for constructing a concrete fiber interface bonding strength prediction model and a bonding strength prediction method. Background Art

[0002] As the most widely used building material in the world, the mechanism of action of its various components has always been a hot topic of research. At the microscopic level, concrete can be regarded as a three-phase composite material composed of aggregate, cement mortar and the interface (Interfacial Transition Zone, ITZ) between the two. Its macroscopic mechanical properties depend on the properties of each component, and ITZ is the weakest link in concrete. However, due to the quasi-brittle nature of ordinary concrete materials, it has the following shortcomings: low tensile strength, which is only 1 / 10 to 1 / 20 of its compressive strength, and brittle failure will occur when the tensile limit is reached; low fracture toughness, even a large number of matching steel bars cannot avoid cracking. When cracks exist, water and corrosive chemicals enter the interior of the concrete, causing the steel bars to rust and expand, driving the cracks to continue to expand, leading to the failure of the concrete structure, causing significant economic losses.

[0003] Therefore, in civil engineering structures, it is extremely important to improve the ductility and control cracks of concrete materials. In order to improve the ITZ strength of ordinary concrete to meet the requirements of building structures and overcome the above shortcomings, researchers mixed fibers into concrete materials to form fiber reinforced concrete (FRC), allowing the fibers to provide bridging effects for cracks and absorb certain deformation energy. As a result, steel fiber reinforced concrete (SFRC) has also been popularized. However, the addition of fibers introduces a matrix / fiber interface transition zone, which has the characteristics of high porosity, low hardness and crystal preferential orientation, and is a weak layer of FRC materials. At the same time, the interface acts as a bridge between the matrix and the fiber, and its bonding properties directly affect the transfer and distribution of stress between the matrix and the fiber, thereby affecting the strengthening, toughening and crack resistance of the FRC material. Therefore, in order to effectively exert the fiber effect in FRC, it is necessary to conduct direct quantitative testing of the concrete / fiber interface bonding properties.

[0004] At present, the research methods of domestic and foreign scholars on the bonding performance of concrete-fiber interface mainly include: single-filament pull-out test and numerical simulation method based on continuous medium mechanics theory. However, due to the non-transparency of concrete fiber system and the small scale of interface, the single-filament pull-out test method cannot observe the initiation and evolution of cracks inside the material, and it is difficult to effectively and intuitively determine the mechanical parameters of the interface transition zone and the fiber inside during fiber pull-out. The numerical simulation method based on continuous medium mechanics theory must know the existence, location and size of cracks in advance when analyzing the failure problem, and must re-divide the grid after the crack propagates. The calculation results will also have strong grid dependence and a small scope of application. Summary of the invention

[0005] In view of this, the purpose of the present invention is to provide a method for constructing a concrete fiber interface bonding strength prediction model and a method for predicting bonding strength. The method provided by the present invention can solve the problem in the prior art that the fiber pull-out experiment is difficult to characterize the interface mechanical parameters and the grid dependence of the numerical simulation method based on the continuum mechanics theory.

[0006] In order to achieve the above object, the present invention provides the following technical solutions:

[0007] The present invention provides a method for constructing a concrete fiber interface bonding strength prediction model, comprising the following steps:

[0008] 1) Constructing a concrete-fiber interface model: constructing a model system of size L×L×(L+h), in which peridynamic voxels are stacked in a cubic manner, and the volume of each voxel is set to a×a×a; taking the origin of the XOY plane as the center, selecting voxels within a diameter range of D around the center and setting them as the fiber region, setting voxels within a diameter range of D to D+w as the interface transition region, and setting the remaining voxels as the concrete region, deleting redundant voxels greater than L in the Z direction in the interface transition region and the concrete region, and exposing the fiber pull-out end with a length of h; randomly deleting n% of the voxels in the interface transition region to describe the porosity of the interface transition region;

[0009] 2) Set peridynamic simulation parameters:

[0010] Set the micromodulus constant c, and the calculation formula is shown in formula (1):

[0011]

[0012] In the formula (1), K is the bulk modulus of the material, and the material includes a fiber region, a concrete region, and an interface transition region; the near field range δ is three times the voxel side length;

[0013] The calculation formula of K is shown in formula (2):

[0014]

[0015] In the formula (2), E is the elastic modulus of the material, and υ is the Poisson's ratio of the material;

[0016] Set s0, the critical stretch value, as shown in formula (3):

[0017] s0(t,η,ξ)=s 00 -αs min (t,η,ξ), (3)

[0018] In the formula (3), s 00 and α are parameters related to the critical elongation, and their values ​​are 0.0005 and 0.25 respectively;

[0019] Among them, s min , which is the minimum stretch value, and the calculation formula is shown in formula (4):

[0020]

[0021] In the formula (4), t is time, η is relative position, and ξ is displacement vector;

[0022] 3) Carry out simulation calculation of interface bonding performance:

[0023] The near-field dynamics simulation parameters set in the step 2) are assigned to the concrete-fiber interface model in the step 1) to perform dynamic calculations; a virtual site is set at L+h / 2 in the Z direction, and the moving speed of the virtual site along the Z direction is set to v; a virtual spring with a stiffness coefficient k is placed at the center of mass of the virtual site and the fiber pull-out end to simulate the fiber pull-out process under load, and the displacement and mechanical load of the fiber pull-out end and the stress, atomic coordinates and bond breaking information of the concrete-fiber interface model are recorded and saved in the output trajectory file;

[0024] 4) Data processing:

[0025] Processing the displacement and mechanical load data of the fiber pull-out end obtained in step 3) to obtain a load-displacement curve during the fiber pull-out process, and taking the peak value on the load-displacement curve to evaluate the bonding performance of the concrete-fiber interface;

[0026] The bond breaking information data obtained in step 3) is processed to obtain the law of the change of the number of bond breaking in the concrete-fiber interface model over time during the fiber pulling process, and the acoustic emission phenomenon in the pulling process is analyzed according to the bond breaking situation of the voxels during the fiber pulling process, and the number of bond breaking is the number of acoustic emissions;

[0027] Read the trajectory file generated in step 3), analyze the crack development process in the concrete area and the interface transition area and the stress distribution in the axial direction of the fiber area,

[0028] The atomic coordinates and bond breaking information are used to analyze the internal crack evolution during fiber pull-out.

[0029] The stress of the concrete-fiber interface model is used to analyze the mechanical response during fiber pullout.

[0030] 5) Based on the peak data on the load-displacement curve obtained in step 4), a prediction model F=f (interface parameters) of the concrete-fiber interface bond strength is established using the response surface analysis method; the interface parameters include the thickness and porosity of the interface transition zone.

[0031] Preferably, in step 1), the concrete-fiber interface model is constructed by simulation software LAMMPS.

[0032] Preferably, in step 1), the value of L is 50 cm, the value of h is 10 cm, the value of a is 1 cm, the D=15 cm, the values ​​of w are 1 cm, 3 cm, 5 cm, 7 cm and 9 cm, and the values ​​of n are 5, 10, 15, 20, 25 and 30.

[0033] Preferably, in step 3), the interface bonding performance simulation calculation is implemented by LAMMPS software.

[0034] Preferably, in step 3), the kinetic calculation is performed by a canonical simulation system, and the simulation temperature T of the kinetic calculation is 300K.

[0035] Preferably, in step 3), the moving speed v is 0.05 m / s, and the stiffness coefficient k is 1 nN / m.

[0036] Preferably, in step 4), data processing is performed by Matlab software.

[0037] Preferably, in step 4), the trajectory file generated in step 3) is read using OVITO software.

[0038] Preferably, the fiber is polypropylene alcohol fiber.

[0039] The present invention also provides a method for predicting the bond strength of a concrete-fiber interface using the concrete fiber interface bond strength prediction model obtained by the construction method described in the above technical solution, comprising the following steps:

[0040] The interface parameters of the concrete-fiber interface to be tested are substituted into the concrete-fiber interface bonding strength prediction model to predict the bonding strength of the concrete-fiber interface to be tested, wherein the interface parameters include the thickness and porosity of the interface transition zone.

[0041] The present invention provides a method for constructing a concrete fiber interface bonding strength prediction model. The present invention includes the following steps: 1) constructing a concrete-fiber interface model; 2) setting peridynamic simulation parameters; 3) using peridynamic methods to simulate and calculate the interface bonding performance; 4) data processing; 5) using the response surface analysis method to establish a concrete-fiber interface bonding strength prediction model F=f (interface parameters). The present invention uses computer simulation technology to propose a method for constructing a concrete fiber interface bonding strength prediction model, which achieves accurate measurement and evaluation of the concrete-fiber interface bonding strength, overcomes the limitations of fiber pull-out experiments that are difficult to characterize interface mechanical parameters and internal crack evolution of materials, breaks through the grid dependence of traditional finite element analysis methods, and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 is a schematic diagram of a concrete-fiber interface model constructed in Example 1 of the present invention;

[0043] Figure 2 AA-direction cross-sectional structural schematic diagram of the concrete-fiber interface model constructed in Example 1 of the present invention;

[0044] Figure 3 is a stress-strain relationship diagram during the fiber extraction process in Example 1 of the present invention;

[0045] Figure 4 is a graph showing the number of acoustic emissions during the process of calculating fiber pull-out in Example 1 of the present invention;

[0046] Figure 5 is a schematic diagram of crack development state 1 during the calculation of fiber pull-out in Example 1 of the present invention;

[0047] Figure 6 is a schematic diagram of crack development state 2 during the calculation of fiber pull-out in Example 1 of the present invention;

[0048] Figure 7 is a schematic diagram of crack development state 3 during the calculation of fiber pull-out in Example 1 of the present invention;

[0049] Figure 8 Schematic diagram of crack development state 4 during the calculation of fiber pull-out in Example 1 of the present invention;

[0050] Fig. 9Schematic diagram of the first force state of the fiber in the pulling-out direction during the calculation of the fiber pulling-out process in Example 1 of the present invention;

[0051] Fig.10 It is a schematic diagram of the second force state of the fiber in the pulling-out direction during the calculation of the fiber pulling-out process in Example 1 of the present invention;

[0052] Fig.11 Schematic diagram of the third force state of the fiber in the pulling-out direction during the calculation of the fiber pulling-out process in Example 1 of the present invention;

[0053] Fig.12 Schematic diagram of the fourth force state of the fiber in the pulling-out direction during the calculation of the fiber pulling-out process in Example 1 of the present invention;

[0054] In the figure: 1-concrete area; 2-interface transition area; 3-fiber area. DETAILED DESCRIPTION

[0055] The present invention provides a method for constructing a concrete fiber interface bonding strength prediction model, comprising the following steps:

[0056] 1) Constructing a concrete-fiber interface model: constructing a model system of size L×L×(L+h), in which peridynamic voxels are stacked in a cubic manner, and the volume of each voxel is set to a×a×a; taking the origin of the XOY plane as the center, selecting voxels within a diameter range of D around the center and setting them as the fiber region, setting voxels within a diameter range of D to D+w as the interface transition region, and setting the remaining voxels as the concrete region, deleting redundant voxels greater than L in the Z direction in the interface transition region and the concrete region, and exposing the fiber pull-out end with a length of h; randomly deleting n% of the voxels in the interface transition region to describe the porosity of the interface transition region;

[0057] 2) Set peridynamic simulation parameters:

[0058] Set the micromodulus constant c, and the calculation formula is shown in formula (1):

[0059]

[0060] In the formula (1), K is the bulk modulus of the material, and the material includes a fiber region, a concrete region, and an interface transition region; the near field range δ is three times the voxel side length;

[0061] The calculation formula of K is shown in formula (2):

[0062]

[0063] In the formula (2), E is the elastic modulus of the material, and υ is the Poisson's ratio of the material;

[0064] Set s0, the critical stretch value, as shown in formula (3):

[0065] s0(t,η.ξ)=s 00 -αs min (t,η,ξ), (3)

[0066] In the formula (3), s 00 and α are parameters related to the critical elongation, and their values ​​are 0.0005 and 0.25 respectively;

[0067] Among them, s min , which is the minimum stretch value, and the calculation formula is shown in formula (4):

[0068]

[0069] In the formula (4), t is time, η is relative position, and ξ is displacement vector;

[0070] 3) Simulation calculation of interface bonding performance:

[0071] The near-field dynamics simulation parameters set in the step 2) are assigned to the concrete-fiber interface model in the step 1) to perform dynamic calculations; a virtual site is set at L+h / 2 in the Z direction, and the moving speed of the virtual site along the Z direction is set to v; a virtual spring with a stiffness coefficient k is placed at the center of mass of the virtual site and the fiber pull-out end to simulate the fiber pull-out process under load, and the displacement and mechanical load of the fiber pull-out end and the stress, atomic coordinates and bond breaking information of the concrete-fiber interface model are recorded and saved in the output trajectory file;

[0072] 4) Data processing:

[0073] Processing the displacement and mechanical load data of the fiber pull-out end obtained in step 3) to obtain a load-displacement curve during the fiber pull-out process, and taking the peak value on the load-displacement curve to evaluate the bonding performance of the concrete-fiber interface;

[0074] The bond breaking information data obtained in step 3) is processed to obtain the law of the change of the number of bond breaking in the concrete-fiber interface model over time during the fiber pulling process, and the acoustic emission phenomenon in the pulling process is analyzed according to the bond breaking situation of the voxels during the fiber pulling process, and the number of bond breaking is the number of acoustic emissions;

[0075] Read the trajectory file generated in step 3), analyze the crack development process in the concrete area and the interface transition area and the stress distribution in the axial direction of the fiber area,

[0076] The atomic coordinates and bond breaking information are used to analyze the internal crack evolution during fiber pull-out.

[0077] The stress of the concrete-fiber interface model is used to analyze the mechanical response during fiber pullout.

[0078] 5) Based on the peak data on the load-displacement curve obtained in step 4), a prediction model F=f (interface parameters) of the concrete-fiber interface bond strength is established using the response surface analysis method; the interface parameters include the thickness and porosity of the interface transition zone.

[0079] The present invention first constructs a concrete-fiber interface model: constructs a model system with a size of L×L×(L+h), in which peridynamic voxels are stacked in a cubic manner, and the volume of each voxel is set to a×a×a; with the origin of the XOY plane as the center, voxels within a diameter range of D around the center are selected and set as fiber areas, voxels within a diameter range of D to D+w are set as interface transition areas, and the remaining voxels are set as concrete areas, and redundant voxels greater than L in the Z direction are deleted in the interface transition area and the concrete area to expose the fiber pull-out end with a length of h; and n% of the voxels are randomly deleted in the interface transition area to describe the porosity of the interface transition area.

[0080] Figure 1 is a schematic diagram of a concrete-fiber interface model constructed in Example 1 of the present invention; Figure 2 AA-direction cross-sectional structural schematic diagram of the concrete-fiber interface model constructed in Example 1 of the present invention;

[0081] In the figure: 1-concrete area; 2-interface transition area; 3-fiber area. Figure 1 and 2 As shown, a model system of size L×L×(L+h) is first constructed, in which the voxels within the diameter range of D are set as the fiber area, the voxels within the diameter range of D to D+w are set as the interface transition zone, and the voxels are set as the concrete area. In the interface transition zone and the concrete area, the redundant voxels greater than L in the Z direction are deleted to expose the fiber pull-out end with a length of h.

[0082] In the step 1), the concrete-fiber interface model is preferably constructed by simulation software LAMMPS.

[0083] LAMMPS software can perform classical molecular dynamics simulations of solid, liquid and gas states and is easy to expand, such as adding new force fields, atom types and boundary conditions; in addition, it also supports C++ with MPI, FFT library functions and GPU and OpenMP. LAMMPS simulates the entire model as a particle, reduces the calculation of degrees of freedom, increases the space and time scales of the computable system, and simplifies data processing and analysis. The present invention uses the simulation software LAMMPS to construct a concrete-fiber interface model. This method is easy to operate, and the constructed concrete-fiber interface model is more realistic, which is conducive to subsequent simulation, calculation and analysis.

[0084] In the present invention, in the step 1), the value of L is preferably 50 cm, the value of h is preferably 10 cm, the value of a is preferably 1 cm, the value of D is preferably = 15 cm, the value of w is preferably 1 cm, 3 cm, 5 cm, 7 cm and 9 cm, and the value of n is preferably 5, 10, 15, 20, 25 and 30.

[0085] The side lengths of the system selected in the present invention are 50 cm, 50 cm and 60 cm respectively, and the peridynamic voxels stacked therefrom are cubes with a side length of 1 cm, forming a fiber region, an interface transition region and a concrete region, setting interface transition regions of different thicknesses, and randomly deleting some voxels in the interface transition region to form the porosity of the interface transition region, so as to well construct a concrete-fiber interface model.

[0086] The present invention is used to set the peridynamic simulation parameters in the model:

[0087] Set the micromodulus constant c, and the calculation formula is shown in formula (1):

[0088]

[0089] In the formula (1), K is the bulk modulus of the material, and the material includes a fiber region, a concrete region, and an interface transition region; the near field range δ is three times the voxel side length;

[0090] The calculation formula of K is shown in formula (2):

[0091]

[0092] In the formula (2), E is the elastic modulus of the material, and υ is the Poisson's ratio of the material;

[0093] Set s0, the critical stretch value, as shown in formula (3):

[0094] s0(t,η,ξ)=s 00 -αs min (t,η,), (3)

[0095] In the formula (3), s 00 and α are parameters related to the critical elongation, and their values ​​are 0.00055 and 0.25 respectively;

[0096] Among them, s min , which is the minimum stretch value, and the calculation formula is shown in formula (4):

[0097]

[0098] In the formula (4), t is time, η is relative position, and ξ is displacement vector.

[0099] In the present invention, the determination of the near-field range δ being three times the voxel side length refers to the prior art "Cracknucleation in brittle and quasi-brittle materials: A peridynamic analysis" (Niazi S, Chen Z, Bobaru F. Theoretical and Applied Fracture Mechanics, 2020).

[0100] In Example 1 of the present invention, E is taken as the elastic modulus of C30 concrete, which is 30 GPa, and the Poisson's ratio υ of the concrete is taken as 0.25; the elastic modulus of the fiber, which is polypropylene alcohol fiber, is taken as 40 GPa.

[0101] The present invention constructs a model and selects parameters to perform interface bonding performance simulation calculation:

[0102] The near-field dynamics simulation parameters set in the step 2) are assigned to the concrete-fiber interface model in the step 1) to perform dynamic calculations; a virtual site is set at L+h / 2 in the Z direction, and the moving speed of the virtual site along the Z direction is set to v; a virtual spring with a stiffness coefficient k is placed at the center of mass of the virtual site and the fiber pull-out end to simulate the pull-out process of the fiber under load, and the displacement and mechanical load of the fiber pull-out end as well as the stress, atomic coordinates and bond breaking information of the concrete-fiber interface model are recorded and saved in the output trajectory file.

[0103] In the present invention, in step 3), the simulation calculation of the interface bonding performance is preferably implemented by LAMMPS software. The present invention uses LAMMPS software for simulation calculation, which has a high degree of simulation, high calculation efficiency, and accurate and reliable results.

[0104] In step 3) of the present invention, the kinetic calculation is preferably performed by a canonical simulation system, and the simulation temperature T of the kinetic calculation is preferably 300K. The simulation system used in the kinetic calculation process of the present invention selects a canonical system (NVT), which means a system with a certain number of particles (N), volume (V), and temperature (T). The canonical ensemble is a typical representative of the Monte Carlo method simulation process. Assume that N particles are in a simulation box with a volume of V, bury them in a heat bath with a constant temperature of T, and perform kinetic calculations.

[0105] In step 3) of the present invention, the moving speed v is preferably 0.05 m / s, and the stiffness coefficient k is preferably 1 nN / m. The present invention controls the moving speed of the virtual site along the Z-axis direction and the stiffness coefficient of the virtual spring at the center of mass of the virtual site and the fiber pull-out end to better simulate the crack development process of the concrete and the interface transition zone and the stress distribution of the fiber in the axial direction.

[0106] In Example 1 of the present invention, the stiffness coefficient of the virtual spring at the center of mass of the virtual site and the fiber pulling end is 1 nN / m.

[0107] After the interface bonding performance simulation calculation obtains data, the present invention processes the obtained data; the displacement and mechanical load data of the fiber pull-out end obtained in the step 3) are processed to obtain a load-displacement curve during the fiber pull-out process, and the peak value on the load-displacement curve is taken to evaluate the bonding performance of the concrete-fiber interface;

[0108] The bond breaking information data obtained in step 3) is processed to obtain the law of the change of the number of bond breaking in the concrete-fiber interface model during the fiber pulling process over time, and the acoustic emission phenomenon in the pulling process is analyzed according to the bond breaking situation of the voxels during the fiber pulling process, and the number of bond breaking is the number of acoustic emissions;

[0109] Read the trajectory file generated in step 3), analyze the crack development process in the concrete area and the interface transition area and the stress distribution in the axial direction of the fiber area,

[0110] The atomic coordinates and bond breaking information are used to analyze the internal crack evolution during fiber pull-out.

[0111] The stress of the concrete-fiber interface model is used to analyze the mechanical response during fiber pull-out.

[0112] In step 4) of the present invention, data processing is preferably performed by Matlab software.

[0113] The present invention utilizes Matlab software to process data. This data processing method is easy to operate, highly efficient, and has accurate processing results and is easy to use. Matlab is a set of powerful engineering calculation software that is widely used in engineering fields such as automatic control, mechanical design, fluid mechanics, and mathematical statistics. By using the toolbox provided by Matlab, engineering and technical personnel can efficiently solve complex engineering problems, dynamically simulate the system, and display the numerical calculation results with powerful graphics functions.

[0114] In step 4) of the present invention, the trajectory file generated in step 3) is preferably read using OVITO software. The present invention preferably uses OVITO software to read the trajectory file, which has a high recognition rate, fast reading and high efficiency. OVITO software has the characteristics of open source and free, and is compatible with mainstream computer platforms. It is more and more widely used in research related to computer simulation.

[0115] In the present invention, the fiber is preferably polypropylene alcohol fiber; the elastic modulus of the polypropylene alcohol fiber is preferably 40 GPa. The polypropylene alcohol fiber used in the present invention is widely used in reinforced concrete materials, has strong representativeness, and can better model the bonding performance of the concrete fiber interface.

[0116] After the data processing, the present invention uses the response surface analysis method based on the peak data on the load-displacement curve obtained in step 4) to establish a prediction model F=f (interface parameters) of the concrete-fiber interface bonding strength; the interface parameters include the thickness and porosity of the interface transition zone.

[0117] The present invention also provides a method for predicting the bond strength of a concrete-fiber interface using the concrete fiber interface bond strength prediction model obtained by the construction method described in the above technical solution, comprising the following steps:

[0118] The interface parameters of the concrete-fiber interface to be tested are substituted into the concrete-fiber interface bonding strength prediction model to predict the bonding strength of the concrete-fiber interface to be tested, wherein the interface parameters include the thickness and porosity of the interface transition zone.

[0119] The present invention preferably verifies the concrete fiber interface bonding strength prediction model obtained by the construction method described in the above technical solution; the verification process preferably substitutes the interface parameters characterized by the actual concrete-fiber interface into the concrete fiber interface bonding performance prediction model for verification.

[0120] It is difficult to observe the internal crack evolution of the material in the traditional test process, and the traditional finite element analysis method must divide the grid when studying the material failure problem, and must re-divide the grid after the crack expands, and the calculation result will also have a strong grid dependence. The present invention uses computer simulation technology to propose a test method for calculating the concrete-fiber interface bonding performance, and combines the peri-field dynamics theory with the computer method to study the concrete-fiber interface bonding performance. By constructing a concrete-fiber interface structure model, simulating the interface bonding performance of the interface structure model, and using the peri-field dynamics theory to propose a prediction model for the concrete-fiber interface bonding performance, the crack evolution inside the material can be observed intuitively, and the precise measurement and evaluation of the concrete-fiber interface bonding strength are achieved. The limitation of the fiber pull-out experiment that it is difficult to characterize the interface mechanical parameters and the internal crack evolution of the material is overcome, and the numerical simulation method based on the continuous medium mechanics theory, that is, the grid dependence of the traditional finite element analysis method, has a broad application prospect.

[0121] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention.

[0122] Example 1

[0123] The present invention provides a method for testing the interfacial bonding performance of concrete fibers, comprising the following steps:

[0124] 1) Construct the concrete-fiber interface model. The simulation software LAMMPS is used to construct the concrete-fiber interface model. First, a concrete-fiber interface model with a size of 50×50×(50+10)cm is selected. 3 The system is a simple cubic stacking of peridynamic voxels, with the volume of each voxel set to 1×1×1cm 3 ; Secondly, with the origin of the XOY plane as the center, select the voxels within a diameter of 15 cm around the center and set them as fiber region 3, set the voxels within a diameter range of 15 cm to 15+w cm (where w is 1 cm, 3 cm, 5 cm, 7 cm, and 9 cm, respectively) as interface transition region 2, and set the remaining voxels as concrete region 1; in interface transition region 2 and concrete region 1, delete the redundant voxels greater than 50 cm in the Z direction to expose the fiber pull-out end with a length of 10 cm; finally, randomly delete n% (where n is 5, 10, 15, 20, 25, and 30, respectively) of the voxels in interface transition region 2 to describe the porosity of interface transition region 2, as shown in FIG. Figure 1 and Figure 2 As shown;

[0125] 2) Set the parameters of peridynamic simulation. In peridynamic simulation, four parameters need to be set, namely, micromodulus constant c, near-field range δ, and parameter s related to critical elongation.00 and α, where c is calculated as shown in equations (1) and (2), and the critical tensile value is expressed by equation (3):

[0126]

[0127] s0(t,η,ξ)=s 00 -αs min (t,η,ξ), (3);

[0128]

[0129] Where K is the bulk modulus of the material, E is the elastic modulus of the material, υ is the Poisson's ratio of the material, during the peridynamic simulation, the near-field range δ is three times the voxel side length, and the critical elongation-related parameter s 00 and α are taken as 0.0005 and 0.25 respectively; E is taken as 30 GPa of elastic modulus of C30 concrete, and Poisson's ratio υ of concrete is taken as 0.25; the elastic modulus of the fiber is 40 GPa of polypropylene alcohol fiber; in the formula (4), t is time, η is relative position, ξ is displacement vector, since η and ξ in the formula (4) are both in vector form and are used to characterize the telekinetic changes of material points at each time node, it is not convenient to give specific values ​​here;

[0130] After calculation, the elastic constants of the voxels in the concrete region 1 and the interface transition region 2, and the elastic constants of the fiber region 3 are obtained; in addition, in order to simulate the influence of different interface bonding parameters, the elastic constants between the concrete region 1 or the interface transition region 2 and the fiber region 3 are set respectively, so as to obtain the peridynamic simulation parameters of the concrete and fiber system.

[0131] 3) Simulation calculation of interface bonding performance: The concrete fiber interface bonding performance is simulated and calculated based on LAMMPS software. First, the force field parameters set in step 2) are assigned to the concrete-fiber interface model system constructed in step 1), and the simulation temperature is set to 300K. Under the NVT system, dynamic calculation is performed; secondly, a virtual site is set at 50+10 / 2 in the Z direction, and the moving speed of the virtual site along the Z direction is set to 0.05m / s; then, a virtual spring with a stiffness coefficient of 1nN / m is placed at the virtual site and the center of mass of the fiber pull-out end to simulate the pull-out process of the fiber under load, and the displacement and mechanical load of the fiber pull-out end as well as the stress, atomic coordinates and bond breaking information of the concrete-fiber interface model are recorded and saved in the output trajectory file.

[0132] 4) Data processing: The data is processed using Matlab software to obtain the load-displacement curve during fiber pull-out, such as Figure 3As shown in the figure, the peak value of the load-displacement curve is taken to evaluate the bonding performance of the concrete-fiber interface; the voxel bond breaking situation during the fiber pull-out process is obtained, and the acoustic emission phenomenon during the pull-out process is analyzed, such as Figure 4 As shown; the trajectory file generated in the dynamic process of step 3) is read using OVITO software to analyze the crack development process of the concrete region 1 and the interface transition zone 2 and the stress distribution of the fiber in the axial direction, and the crack development process of the concrete region 1 and the interface transition zone 2 is analyzed as shown. Figures 5 to 8 As shown, the stress distribution of fiber region 3 in the axial direction is as follows Figures 9 to 12 As shown, the internal crack evolution law and mechanical response during fiber pull-out are analyzed, the bonding performance of the concrete-fiber interface and the bond breaking of the voxels during fiber pull-out are evaluated; and the concrete-fiber interface bonding strength of different thicknesses and porosities of the interface transition zone 2 is obtained;

[0133] 5) Based on the data obtained in step 4), a prediction model F=f (interface parameter) of concrete-fiber interface bond strength is established by using response surface analysis method, and the influence law and mechanism of interface parameter on concrete-fiber interface bond strength are obtained, that is, the greater the thickness of the interface transition zone, the weaker the mechanical properties of the model, the lower the bond strength, and the greater the porosity, the weaker the mechanical properties of the model, the lower the bond strength;

[0134] 6) Substitute the interface parameters characterized by the actual concrete fiber interface into the prediction model, and predict the bond strength of the concrete-fiber interface through the prediction model in step 5). According to the literature (Xu L, Deng F, Chi Y. Nano-mechanical behavior of the interfacial transition zone between steel-polypropylene fiber and cement paste [J]. Construction and Building Materials, 2017, 145: 619-638.), the interface transition zone of the actual concrete fiber interface is about 15 μm and the porosity is about 20%. In the literature (Pakravan HR, Jamshidi M, Latifi M. Polymeric fibers pull-out behavior and microstructure as cementitious composites reinforcement [J]. Journal of the Textile Institute, 2013, 104 (10): 1056-1064.), the bond strength of the concrete-fiber interface is 1.3 MPa, while the bond strength of the concrete-fiber interface predicted by the prediction model in step 5) is 1.27 MPa, and the relative error between the two is 2%. Therefore, the prediction model in step 5) has good accuracy.

[0135] Although the above embodiment describes the present invention in detail, it is only a part of the embodiments of the present invention rather than all the embodiments. People can also obtain other embodiments based on this embodiment without creativity, and these embodiments all fall within the protection scope of the present invention.

Claims

1. A method for constructing a concrete fiber interface bond strength prediction model. It is characterized in that The following steps are involved: 1) Constructing a concrete-fiber interface model: constructing a model system of size L×L×(L+h), in which peridynamic voxels are stacked in a cubic manner, and the volume of each voxel is set to a×a×a; taking the origin of the XOY plane as the center, selecting voxels within a diameter range of D around the center and setting them as the fiber region, setting voxels within a diameter range of D to D+w as the interface transition region, and setting the remaining voxels as the concrete region, deleting redundant voxels greater than L in the Z direction in the interface transition region and the concrete region, and exposing the fiber pull-out end with a length of h; randomly deleting n% of the voxels in the interface transition region to describe the porosity of the interface transition region; 2) Set peridynamic simulation parameters: Set the micromodulus constant c, and the calculation formula is shown in formula (1): In the formula (1), K is the bulk modulus of the material, and the material includes a fiber region, a concrete region, and an interface transition region; the near field range δ is three times the voxel side length; The calculation formula of K is shown in formula (2): In the formula (2), E is the elastic modulus of the material, and υ is the Poisson's ratio of the material; Settings 0 , that is, the critical tensile value, and the calculation formula is shown in formula (3): s 0 (t,η,ξ)=s 00 -as min (t,η,ξ), (3) In the formula (3), s 00 and α are parameters related to the critical elongation, and their values ​​are 0.0005 and 0.25 respectively; Among them, s min , which is the minimum stretch value, and the calculation formula is shown in formula (4): In the formula (4), t is time, η is relative position, and ξ is displacement vector; 3) Carry out simulation calculation of interface bonding performance: The near-field dynamics simulation parameters set in the step 2) are assigned to the concrete-fiber interface model in the step 1) to perform dynamic calculations; a virtual site is set at L+h / 2 in the Z direction, and the moving speed of the virtual site along the Z direction is set to v; a virtual spring with a stiffness coefficient k is placed at the center of mass of the virtual site and the fiber pull-out end to simulate the fiber pull-out process under load, and the displacement and mechanical load of the fiber pull-out end and the stress, atomic coordinates and bond breaking information of the concrete-fiber interface model are recorded and saved in the output trajectory file; 4) Data processing: Processing the displacement and mechanical load data of the fiber pull-out end obtained in step 3) to obtain a load-displacement curve during the fiber pull-out process, and taking the peak value on the load-displacement curve to evaluate the bonding performance of the concrete-fiber interface; The bond breaking information data obtained in step 3) is processed to obtain the law of the change of the number of bond breaking in the concrete-fiber interface model over time during the fiber pulling process, and the acoustic emission phenomenon in the pulling process is analyzed according to the bond breaking situation of the voxels during the fiber pulling process, and the number of bond breaking is the number of acoustic emissions; Read the trajectory file generated in step 3), analyze the crack development process in the concrete area and the interface transition area and the stress distribution in the axial direction of the fiber area, The atomic coordinates and bond breaking information are used to analyze the internal crack evolution during fiber pull-out. The stress of the concrete-fiber interface model is used to analyze the mechanical response during fiber pullout. 5) Based on the peak data on the load-displacement curve obtained in step 4), a prediction model F=f (interface parameters) of the concrete-fiber interface bond strength is established using the response surface analysis method; the interface parameters include the thickness and porosity of the interface transition zone.

2. The construction method according to claim 1, It is characterized in that In the step 1), the concrete-fiber interface model is constructed by the simulation software LAMMPS.

3. The construction method according to claim 1 or 2, It is characterized in that In the step 1), the value of L is 50 cm, the value of h is 10 cm, the value of a is 1 cm, the D=15 cm, the values ​​of w are 1 cm, 3 cm, 5 cm, 7 cm and 9 cm, and the values ​​of n are 5, 10, 15, 20, 25 and 30.

4. The construction method according to claim 1, It is characterized in that In the step 3), the interface bonding performance simulation calculation is implemented by LAMMPS software.

5. The construction method according to claim 1 or 4, It is characterized in that In the step 3), the kinetic calculation is performed by a canonical simulation system, and the simulation temperature T of the kinetic calculation is 300K.

6. The construction method according to claim 1, It is characterized in that In the step 3), the moving speed v is 0.05 m / s, and the stiffness coefficient k is 1 nN / m.

7. The construction method according to claim 1, It is characterized in that In the step 4), data processing is performed by Matlab software.

8. The construction method according to claim 1, It is characterized in that In the step 4), the trajectory file generated in the step 3) is read by using OVITO software.

9. The construction method according to claim 1, It is characterized in that The fiber is polypropylene alcohol fiber.

10. A method for predicting the bond strength of a concrete-fiber interface using the concrete fiber interface bond strength prediction model obtained by the construction method according to any one of claims 1 to 9, The following steps are involved: The interface parameters of the concrete-fiber interface to be tested are substituted into the concrete-fiber interface bonding strength prediction model to predict the bonding strength of the concrete-fiber interface to be tested, wherein the interface parameters include the thickness and porosity of the interface transition zone.

Citation Information

Cited By

  • Concrete strength prediction method based on deep learning

    CN120355675A