Development of egg white-based nanofiber treatment material

The double-layer nanofiber material produced by electrospinning uses super absorbent PAA and flexible PCL combined with egg white protein to solve the shortcomings of existing burn dressings in the treatment of second-degree burns, achieving rapid healing and safe wounds Nursing, providing efficient burn treatment materials.

CN119072320APending Publication Date: 2024-12-03SÜLEYMAN DEMİREL ÜNİVERSİTESİ İDARİ VE MALİ İŞLER DAİRE BAŞKANLIĞI GENEL SEKRETERLİK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380036715.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-12-11
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Existing burn wound dressings lack effective nanofiber materials when treating second-degree burns, and often contain toxic substances, which are difficult to heal quickly, and are not mechanically strong enough to support daily activities.

Method used

The first layer is composed of super absorbent polyacrylic acid (PAA) nanofibers, and the second layer contains polycaprolactone (PCL) and egg white protein, which is formed by thermal physical crosslinking. , ensure the biocompatibility and flexibility of the material.

Benefits of technology

Accelerate the healing process of burn wounds, keep the wounds moist, avoid adhesion, provide environmentally friendly, high-value-added biomedical materials, significantly improving the effect of burn treatment.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The subject matter of the present invention relates to the production of nanofiber materials based on biopolymers and egg white active ingredients for the treatment of secondary burns. In the invention, design, production, characterization and in-vivo application of the double-layer nanofiber burn wound material with different functional properties are provided. The electrostatic spinning method is used for producing the material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The subject matter of the present invention relates to the production of nanofiber materials based on biopolymers and egg white active ingredients for the treatment of second-degree burns. In the present invention, the design, production, characterization and in vivo application of double-layer nanofiber burn wound materials with different functional properties are provided. Electrospinning is used for the production of the material. Background Art

[0002] Nowadays, many methods and tools are used for the treatment of burn wounds. Although the care of burn wounds requires great attention, ideal dressings and dressing materials are particularly important for the care and rapid wound healing of second-degree burns. The ideal healing or wound treatment material that helps in treatment should protect the burn wound from bacteria and foreign matter, absorb fluids in the wound and keep the wound area moist, and should not contain toxic or allergenic substances. At the same time, it should be easy to apply without damaging the wound and surrounding skin, and then be removed from the wound area during the replacement process without causing any damage. In addition, the mechanical strength of the treatment material must be good. For this strength, it is necessary that it does not interfere with the patient's daily activities and does not cause any tearing, twisting or curling to the wound. However, burn wound dressings are used in the prior art. These dressings are aluminum film burn dressings that are only used to maintain body temperature when the burn wound is first formed. These wound dressings are only used to protect the injured area. In addition, they also contain toxic active substances such as silver (Ag). In addition to protecting the wound surface, there are commercial burn wound dressings that contain harmless substances that accelerate wound healing. These dressings are usually in the form of meshes, hydrogels or films, and do not use nanofibers or add materials with different properties. In addition to this, the lack of materials containing natural active ingredients that are more easily available than chemicals or drugs in wound and burn treatment also poses a problem for the existing technology.

[0003] In the prior art document numbered CA2640197A1, a wound dressing is described. The wound dressing comprises a first absorbent layer and a second absorbent layer of a fabric woven from viscose fibers and polyester fibers. Each absorbent layer has an operational inner surface and an operational outer surface. The wound dressing also comprises a third layer sandwiched between the first absorbent layer and the second absorbent layer and bonded to the first absorbent layer and the second absorbent layer. The third layer is in the form of cotton gauze. The invention does not include a layer formed by nanofibers or polymers in any way, nor does it include a method for making a wound dressing and a method for treating a wound.

[0004] Prior art document numbered US4361552A describes a method for treating wounds or burns, which involves covering the surface of the wound or burn with a cross-linked amniotic membrane dressing. An amniotic membrane wound dressing is provided and the wound is treated to essentially become a more permanent dressing until the wound heals. Fresh amniotic membrane from any animal source is stabilized with a glutaraldehyde solution or any other fixing or tanning solution to cross-link its proteins.

[0005] In the prior art document numbered CN209392237U, a facial burn wound dressing set is described. The burn patch includes a burn patch and an elastic mesh dressing. The burn patch contacts the inner side of the elastic mesh dressing; the burn patch is in the form of a facial mask, formed with two eye openings, a nose opening and a mouth opening. The burn patch of the facial burn wound dressing set is made in the shape of a facial mask. In addition, the burn label includes a dressing layer and a cotton pad layer, one side of the cotton pad layer is fixedly attached to the dressing layer, and the other side of the cotton pad layer contacts the inner side of the elastic mesh. The facial burn wound dressing set is constructed to be used only as a bandaging material.

[0006] The prior art document numbered CN108404191A describes a graphene oxide / lidocaine sponge dressing and a preparation method thereof. The medical sponge dressing combines the excellent properties of graphene oxide, lidocaine, polyvinyl alcohol, etc., and has a structure with fast liquid absorption, large liquid absorption, large moisture retention, antibacterial activity, analgesia and flexibility; it describes a dressing developed using graphene oxide and used for wounds and burns.

[0007] The prior art document numbered CN108261557A describes a nanofiber membrane for wound healing, its preparation method and application. It uses polycaprolactone, gelatin and calcium disilicate phosphate bioceramics as raw materials, and uses mixed electrospinning technology to prepare a composite nanofiber membrane for wound healing. The composite nanofiber membrane can significantly shorten the healing time of chronic soft tissue wounds, especially diabetic wounds, and promote angiogenesis, epidermal regeneration and collagen formation in the wound area. It is constructed to reduce the inflammatory response of chronic wounds and promote the healing of soft tissue wounds.

[0008] Prior art document No. 2016 / 11396 describes a medical wound dressing for use in the healthcare industry, which comprises a cross-linking agent, a natural and / or leaf-like polymer, and a thin exit submucosal layer that accelerates the healing process of various wounds and burn wounds. Because it contains a certain dose of growth factors that are effective for wound healing, such as TGF-β, FGF-2, VEGF, and EGF, the sponge structure acts as a scaffold for new tissue formation while repairing natural reorganization. Under cell stimulation, host cells provide new vascular structures, peripheral differentiation, and regional specific tissue regeneration.

[0009] In the prior art document No. 2015 / 17118, an antibacterial PCL / chitosan wound dressing material is described. It is a composite biocompatible wound dressing material applied to the use of artificial tissue scaffolds, which are considered as an alternative solution to tissue transplantation for the treatment of tissue damage (especially burn cases). The developed composite biomaterial is constructed to support the healing process of tissue damage exceeding a critical defect size.

[0010] There are no studies at home and abroad on the production, detailed characterization, in vitro and in vivo applications of wound treatment materials containing polyacrylic acid, polycaprolactone and egg white protein active ingredients in their structure. Summary of the invention

[0011] The main purpose of the present invention is to develop a nanofiber wound treatment material containing egg white active ingredients for burn wound healing, and to provide healing of second-degree burn wounds using the material produced by electrospinning.

[0012] Another object of the present invention is to absorb wound exudate and keep the wound moist through polyacrylic acid (PAA), which is the first of two layers and is a nanofiber wound treatment material specially developed for treating second-degree burn wounds.

[0013] Another object of the present invention is to accelerate wound healing by adding polycaprolactone (PCL) polymer and egg white as a wound healing active ingredient in the second layer in contact with the wound surface. The polycaprolactone polymer does not adhere to the wound surface and does not interfere with the patient's daily life due to its high strength.

[0014] Another object of the present invention is to accelerate the healing process using a burn healing material containing PAA, PCL and egg white protein as healing active ingredients and developed by electrospinning.

[0015] Another object of the present invention is to obtain an environmentally friendly, sustainable and high value-added biomedical material through the developed nanofiber burn treatment material and the polymers and active ingredients used.

[0016] The purpose of the present invention is to develop a burn wound material containing nanofiber egg white protein active ingredients for treating burn wounds. Electrospinning is used for the production of the nanofiber material, and the design, production and characterization of a double-layer nanofiber wound burn material are carried out. The first layer of the developed nanofiber wound burn material is composed of polyacrylic acid (PAA)-based nanofibers with super absorbent properties, and the PAA-based nanofibers are expected to absorb wound exudate and keep the injured area moist. In the production of the second layer in contact with the wound, polycaprolactone (PCL) polymers are used in view of their flexibility, high strength and the fact that they do not adhere to the wound due to their hydrophobic structure. In this layer, as a wound healing active ingredient, protein-based egg white is preferred. As a result of histopathological analysis of the surface of the double-layer nanofibers produced according to the present invention, it has been determined that the nanofiber wound treatment material has the potential to accelerate the healing of second-degree burn wounds. DETAILED DESCRIPTION

[0017] In the present study, the design, production and characterization of a two-layer nanofiber wound treatment material was performed. Subsequently, in vivo studies were conducted on experimental animals to determine the burn wound healing properties of the developed nanofiber material. The subject of the present invention describes a burn treatment material containing polyacrylic acid (PAA) and polycaprolactone (PCL) polymers and egg white as active ingredients, which accelerates the healing process in burn treatment.

[0018] In the experimental study, optimization studies were first conducted in terms of fiber tensile properties and fiber morphology. Then, in the production of nanofibers by electrospinning, solution properties such as conductivity, surface tension and viscosity, which are closely related to fiber spinning properties and fiber morphology, were determined. Electrospinning technology is a method for producing nanofibers. In this method, a polymer solution / melt is subjected to an electric field. Under the influence of the electric field, the fibers are dispersed and fine and dry polymer fibers of nanometer diameter are formed on the surface of the collector. In this method, a polymer solution is first prepared and placed in a syringe. With the help of a feed pump, a droplet of the polymer solution is formed at the tip of a needle / device connected to the syringe. In this case, the droplet is at the tip of the device, maintaining a balance between its own surface tension and gravity. When the applied potential exceeds the surface tension of the droplet, the polymer jet leaves the device and starts moving towards the opposite collector. During the movement of the polymer jet, the solvent evaporates and the polymer jet becomes longer and thinner.

[0019] For the first layer in the production of the nanofiber wound treatment material, a PAA-based super absorbent nanofiber layer was produced under optimal conditions and then cross-linked. In the cross-linking study, thermophysical cross-linking was applied and water solubility was prevented. The first layer of the wound treatment material is important for its ability to absorb wound exudate and keep the wound surface moist. Then, the surface of the cross-linked super absorbent PAA nanofiber layer was coated with PCL-based nanofibers containing egg white to form the second layer.

[0020] PCL polymer is an ideal polymer for wound healing materials due to its characteristics such as biocompatibility and biodegradability, flexibility and durability. In addition, due to its hydrophobic structure, it does not adhere to the wound surface and is therefore preferred.

[0021] In the present study, egg white protein was used as the main active ingredient in the surface of nanofibers produced as wound healing materials, and was used to treat second-degree burn wounds by utilizing the properties of protein, such as growth, reproduction and self-repair processes (which are all basic characteristics of life).

[0022] After the optimization study was completed and the nanofiber production was concluded, the morphological, chemical and thermal characterization of the PCL-based nanofibers was completed by SEM, FT-IR, TGA, DSC, DTG and XRD analysis. Then, the release properties of the active substances were determined from the produced nanofibers. After the optimization study was conducted and the characterization process was completed, the water vapor permeability analysis of the double-layer nanofiber surface was performed.

[0023] In the final stage of the study, in vivo analysis of the two-layer produced nanofiber surface was performed on experimental animals, and the healing performance of the present invention on second-degree burn wounds was evaluated from a histopathological perspective. As a result of the histopathological analysis, it was determined that the nanofiber wound treatment material has the potential to accelerate the healing of second-degree burn wounds.

[0024] The invention relates to a burn treatment material for burn treatment developed by an electrostatic spinning method, comprising polyacrylic acid (PAA), polycaprolactone (PCL) and protein. The protein used is an active component of egg white.

[0025] The burn treatment and healing material was obtained using an electrospinning method. In this method, a solution of polyacrylic acid, ethanol and pure water was prepared to form a first layer. Then, the solution was injected into a syringe, and the solution was injected through an injection needle with high pressure by applying pressure with a pump. After the fiber structure was accumulated on a collection plate, the first layer was formed by thermal physical crosslinking. The second layer was formed on top of the first layer located on the collection layer. For this purpose, a polycaprolactone, protein and chloroform:DMF solution was prepared. Polycaprolactone was used as a polymer, egg white active ingredient was used as protein, and chloroform and DMF (dimethylformamide) were used as solvents. Then, the prepared solution was injected into a syringe, and the solution was injected through an injection needle with high pressure by applying pressure with a pump. By combining the fiber structure with the polyacrylic acid-based nanofiber layer on the collection plate, the production of a double-layer burn treatment material was completed.

[0026] The present invention is a burn treatment material for treating second-degree burns developed by electrospinning, comprising polyacrylic acid (PAA), polycaprolactone (PCL) and protein. The protein used is an active ingredient of egg white. The subject of the present invention is an electrospinning method, which is a method for obtaining a burn treatment material for treating burns developed by electrospinning. In order to prepare the first layer, a solution of polyacrylic acid, ethanol and pure water is prepared and the solution is injected into a syringe. After the syringe is placed at a pump that feeds it into the system, a polymer solution droplet is generated at the tip of a needle connected to the syringe with the help of a feed pump. By applying an electric potential, the surface tension of the droplet increases, and the solution droplet becomes longer and thinner. After the fiber droplets accumulate on a collection plate, the accumulated fibers are physically cross-linked by heat and remain on the collection plate. The second layer is formed on the produced first layer. After preparing a polycaprolactone, protein and chloroform:DMF solution, the solution is injected into a syringe. The syringe is placed in a pump that feeds it into the system, and then a polymer solution droplet is formed at the tip of a needle connected to the syringe with the help of a feed pump. By applying an electric potential, the surface tension of the droplets increases and the solution droplets become longer and thinner. When the fiber droplets accumulate on the collecting plate, the first and second layers combine on the collecting plate.

[0027] In this method, first, a polymer solution consisting of ethanol, pure water and polyacrylic acid, which is about to form the first layer, is prepared and injected into a syringe. With the help of a feed pump, a droplet of the polymer solution is formed at the tip of the needle / device connected to the syringe. In this case, the droplet is at the tip of the device, in balance with its own surface tension and gravity. Then, an electric potential is started to be supplied to the system with the help of a power supply. When the applied potential exceeds the surface tension of the droplet, the polymer jet leaves the device and begins to move toward the relative collector. During the movement of the polymer jet, the solvent evaporates and the polymer jet becomes longer and thinner. When the polymer jet reaches the collector, the solvent is completely removed and the dried nanometer diameter fibers remain on the collector. The last step in the nanofiber formation stage of the electrospinning method is the solidification of the sprayed polymer solution in the form of nanofibers. At this stage, the polymer jet reaches the collector and settles on the surface. The fibers that reach the collector are structures in the form of a two-dimensional nonwoven surface, which is composed of short fibers completely removed from the solvent. Thereafter, the first layer produced using heat is cross-linked and placed on a collecting plate. Following the same procedure, a solution containing polycaprolactone, chloroform:DMF, and egg white active ingredient protein was prepared to form a second layer. Then, it was injected into a syringe, and exactly the same procedure was repeated. This time, a second layer was formed on top of the first layer containing polyacrylic acid on the collection material. Thus, a second-degree burn treatment material was prepared.

[0028] In the step of forming the first layer, the solution content comprises 5 wt % of polyacrylic acid and a total of 95 wt % of pure water and ethanol. The solution for preparing the second layer comprises 7 wt % of polycaprolactone, 9 wt % of egg white active ingredient and a total of 84 wt % of solvent (chloroform and DMF). According to different preferred embodiments of the present invention, the 84 wt % of solvent constituting the solution forming the second layer is 80 wt % of chloroform and 20 wt % of DMF.

[0029] According to various preferred embodiments of the present invention, the solvent constituting 95 wt % of the solution for forming the first layer is 70 wt % of pure water and 30 wt % of ethanol.

Claims

1. A second degree burn treatment material for burn treatment developed by electrospinning, characterized in that Contains polyacrylic acid (PAA), polycaprolactone (PCL) and protein.

2. The second degree burn treatment material for burn treatment prepared by electrospinning according to claim 1, characterized in that Contains the active ingredient protein from egg white.

3. A second degree burn treatment material for burn treatment prepared by electrospinning according to any one of the preceding claims, characterized in that It contains 5 wt% of polyacrylic acid, 7 wt% of polycaprolactone and 9 wt% of egg white active ingredient protein.

4. A method for obtaining a second degree burn treatment material for burn treatment prepared by electrospinning, characterized in that The process includes the following steps: a. Prepare a solution using polyacrylic acid and a solvent, b. injecting the solution into a syringe, c. Place the syringe on the pump that will feed it into the system. d. generating polymer solution droplets at the tip of a needle connected to a syringe with the aid of a feed pump, e. Increase the surface tension of the droplets by applying an electric potential, thereby making the solution droplets longer and thinner, f. Fiber droplets accumulate on the collecting plate, g. Physical cross-linking of the accumulated fibers by heat, h. preparing a solution with polycaprolactone, protein and solvent, i. Inject the solution into the syringe, j. Place the syringe on the pump that will feed it into the system. k. generating droplets of the polymer solution at the tip of a needle connected to a syringe with the aid of a feed pump, l. Increase the surface tension of the droplets by applying an electric potential, thereby making the solution droplets longer and thinner, m. Fiber droplets accumulate on the collection plate, and n. Joining the first layer and the second layer on the collecting plate.

5. The method for obtaining a second degree burn treatment material for burn treatment prepared by electrospinning according to claim 4, characterized in that In process step "a", the polyacrylic acid is 5% by weight.

6. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 5, characterized in that In step "a", the solvent amounts to 95% by weight.

7. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 6, characterized in that In step "a", 95% by weight of the solvent used is 70% by weight of pure water.

8. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 7, characterized in that In step "a", 95% by weight of the solvent used was 30% by weight of ethanol.

9. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 8, characterized in that In step "h", 7% by weight of polycaprolactone is present.

10. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 9, characterized in that The protein used in step "h" is an egg white active ingredient.

11. The method for obtaining a second-degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 10, characterized in that The active ingredient of egg white in step "h" is 9% by weight.

12. The method for obtaining a second degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 11, characterized in that The solvent in step "h" was 84% ​​by weight.

13. The method for obtaining a second degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 11, characterized in that In step "h", 84% by weight of the solvent used was 80% by weight of chloroform.

14. The method for obtaining a second degree burn treatment material for burn treatment prepared by electrospinning according to any one of claims 4 to 11, characterized in that In step "h", 84% by weight of the solvent used was 20% by weight of DMF.