Processing method of maltitol crystal
Through press molding and cladding technology, the problem of maltitol crystals is easily agglomerated, and its storage stability and industrial application are improved.
Patent Information
- Application Number
- CN202411111032.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-12-06
AI Technical Summary
Maltitol crystals have poor stability during storage and are prone to agglomeration, resulting in additional crushing operations during application, affecting their industrial application.
By pressing the powdered maltitol crystals into molding, a molded body with a smaller specific surface area is formed, and a cladding layer is formed on its surface, and stored using polysaccharides and grease coatings with opposite charges, combined with vacuum drying and protective gas sealing.
Effectively prevent maltitol crystals from agglomerating, reduce their contact area and hygroscopicity, improve storage stability, and promote its industrial application.
Smart Images

Figure CN119073439A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of maltitol processing, and in particular to a method for processing maltitol crystals. Background Art
[0002] As a new type of functional sweetener, maltitol has no free hydroxyl groups in its structure, does not cause the Maillard reaction when heated with amino acids and proteins, and has good heat and acid stability. Therefore, it can be used in foods such as chewing gum, chocolate, dairy products, ice cream, low-sugar foods and beverages.
[0003] However, the above maltitol has poor stability during storage and is easy to agglomerate, which requires additional crushing operations when used. In addition, the agglomerated maltitol is difficult to crush, which is not conducive to its industrial application. Summary of the invention
[0004] In view of the above technical problems, the present application provides a method for processing maltitol crystals, which can effectively prevent the storage and agglomeration of maltitol crystals, and is conducive to its industrial application.
[0005] The present application provides a method for processing maltitol crystals, comprising: A pressing step, pressing the powdered maltitol crystals into a molded body; A slurrying step, dispersing a coating material in a solvent to obtain a coating slurry, wherein the coating material comprises a first polysaccharide having a charge opposite to that of the maltitol crystals and fat; A coating step of mixing the molded body and the coating slurry to form a coating slurry layer on the surface of the molded body; A drying step of drying the molded body having the coating slurry layer formed thereon to form a coating layer on the surface of the molded body; The storage step is to seal and store the molded body with the coating layer under protective gas conditions.
[0006] According to any of the aforementioned embodiments of the present application, in the pressing step, the specific surface area of the molded body is 10 -5 m 2 / g~10 -3 m 2 / g.
[0007] According to any of the foregoing embodiments of the present application, in the pressing step, the maltitol content in the maltitol crystals is greater than or equal to 99.5% on a dry basis.
[0008] According to any of the foregoing embodiments of the present application, in the pressing process, the shape of the molded body includes one or more combinations of spherical, square and cylindrical shapes.
[0009] According to any of the aforementioned embodiments of the present application, in the pulping process, the mass ratio of the polysaccharide to the oil is (10-20):1.
[0010] According to any of the foregoing embodiments of the present application, in the pulping process, the polysaccharide includes one or more combinations of chitin, chitosan, chitosan and xanthan gum.
[0011] According to any of the foregoing embodiments of the present application, in the pulping process, the oil includes vegetable hydrogenated oil.
[0012] According to any of the aforementioned embodiments of the present application, in the pulping process, the coating material further includes a second polysaccharide containing starch, and the mass ratio of the first polysaccharide, the second polysaccharide and the oil is (10-20): (2-5):1.
[0013] According to any of the foregoing embodiments of the present application, in the drying step, the drying treatment includes vacuum drying.
[0014] According to any of the foregoing embodiments of the present application, in the storage process, the protective gas includes one or more combinations of nitrogen and carbon dioxide.
[0015] The present application provides a processing method for maltitol crystals, by pressing and molding powdered maltitol crystals to reduce its contact area, so that the occurrence of caking between maltitol crystals can be reduced. Moreover, a coating layer is formed on the surface of a molded body by using a coating material including a first polysaccharide and grease having an electric charge opposite to that of the maltitol crystals, wherein the first polysaccharide having an electric charge opposite to that of the maltitol crystals can make the coating layer tightly coated, and the same electric charge carried by the coating layer in each molded body can further prevent the occurrence of maltitol crystal caking. In addition, by placing the above-mentioned molded body in a sealed storage under protective gas conditions, the occurrence of caking of external environmental factors can be reduced. Therefore, the processing method for maltitol crystals provided by the present application can effectively prevent maltitol crystal storage caking, which is conducive to its industrial application. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 A schematic flow chart of a method for processing maltitol provided in some embodiments of the present application is shown. DETAILED DESCRIPTION
[0018] The "range" disclosed in this application is defined in the form of a lower limit and an upper limit, and a given range is defined by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundaries of the particular range. The range defined in this way can be inclusive or exclusive of the end values, and can be arbitrarily combined, that is, any lower limit can be combined with any upper limit to form a range.
[0019] In this article, specific surface area generally refers to the total area per unit mass of material, with the unit of m 2 / g.
[0020] See also Figure 1 As shown, the present application provides a method for processing maltitol crystals, comprising: S100, a pressing step of pressing the powdered maltitol crystals into a molded body; S200, a slurry preparation step of dispersing the coating material in a solvent to obtain a coating slurry, wherein the coating material includes a first polysaccharide having a charge opposite to that of the maltitol crystals and fat; S300, a coating step of mixing the molded body and the coating slurry to form a coating slurry layer on the surface of the molded body; S400, a drying step of drying the molded body having the coating slurry layer formed thereon to form a coating layer on the surface of the molded body; S500, a storage step, wherein the molded body with the coating layer is sealed and stored under protective gas conditions.
[0021] The present application provides a processing method for maltitol crystals, by pressing and molding powdered maltitol crystals to reduce its contact area, so that the occurrence of caking between maltitol crystals can be reduced. Moreover, a coating layer is formed on the surface of a molded body by using a coating material including a first polysaccharide and grease having an electric charge opposite to that of the maltitol crystals, wherein the first polysaccharide having an electric charge opposite to that of the maltitol crystals can make the coating layer tightly coated, and the same electric charge carried by the coating layer in each molded body can further prevent the occurrence of maltitol crystal caking. In addition, by placing the above-mentioned molded body in a sealed storage under protective gas conditions, the occurrence of caking of external environmental factors can be reduced. Therefore, the processing method for maltitol crystals provided by the present application can effectively prevent maltitol crystal storage caking, which is conducive to its industrial application.
[0022] In the pressing process of the above embodiment, the pressing and molding can be performed by using instruments and equipment well known in the art, such as a granulator, etc. Through the pressing and molding, the powdered maltitol crystals are formed into a molded body with a small specific surface area, which can reduce the contact area of the maltitol crystals, thereby reducing the occurrence of agglomeration. When the specific surface area of the molded body is within a suitable range, it can not only further reduce the occurrence of agglomeration, but also facilitate its transportation and storage.
[0023] In some embodiments of the present application, the specific surface area of the molded body is 10 -5 m 2 / g~10 -3 m 2 / g.
[0024] In the embodiments of the present application, the specific surface area of the molded body can be measured using instruments and methods well known in the art. For example, the gas adsorption amount measured by a gas adsorption method (constant volume adsorption method) using nitrogen (N2) gas as an adsorption medium is analyzed using the BET method.
[0025] In the above embodiment, when the specific surface area of the molded body is within the above range, the contact area can be further reduced, and the contact area can be further reduced by the coating layer, thereby further reducing the occurrence of agglomeration.
[0026] For example, the specific surface area of the molded body may be, but is not limited to, 10 -5 m 2 / g, 1.5×10 -5 m 2 / g, 2×10 -5 m 2 / g, 2.5×10 -5 m 2 / g, 3×10 -5 m 2 / g, 3.5×10 -5 m 2 / g, 4×10 -5 m 2 / g, 4.5×10 -5 m 2 / g, 5×10 -5 m 2 / g, 5.5×10 -5 m 2 / g, 6×10 -5 m 2 / g, 6.5×10 -5 m 2 / g, 7×10 -5 m 2 / g, 7.5×10 -5 m2 / g, 8×10 -5 m 2 / g, 8.5×10 - 5 m 2 / g, 9×10 -5 m 2 / g, 9.5×10 -5 m 2 / g, 10 -4 m 2 / g, 1.5×10 -4 m 2 / g, 2×10 -4 m 2 / g, 2.5×10 -4 m 2 / g, 3×10 -4 m 2 / g, 3.5×10 -4 m 2 / g, 4×10 -4 m 2 / g, 4.5×10 -4 m 2 / g, 5×10 -4 m 2 / g, 5.5×10 -4 m 2 / g, 6×10 - 4 m 2 / g, 6.5×10 -4 m 2 / g, 7×10 -4 m 2 / g, 7.5×10 -4 m 2 / g, 8×10 -4 m 2 / g, 8.5×10 -4 m 2 / g, 9×10 -4 m 2 / g, 9.5×10 -4 m 2 / g, 10 -3 m 2 / g or a range consisting of any two of the above values. For example, the range of the specific surface area of the molded body can be, but is not limited to, 1.5×10 -5 m 2 / g~9.5×10 -4 m 2 / g, 2.5×10 -5 m 2 / g~8×10-4 m 2 / g, 4×10 -4 m 2 / g~7×10 -4 m 2 / g.
[0027] In the embodiments of the present application, the higher the maltitol content in the maltitol crystals, the lower the water absorption will be, and thus the probability of agglomeration will be greatly reduced.
[0028] In some embodiments of the present application, in the pressing process, the maltitol content in the maltitol crystals is greater than or equal to 99.5% on a dry basis.
[0029] In the embodiments of the present application, the maltitol content in the maltitol crystals can be measured by the method described in the national standard GB28307-2012 "National Food Safety Standard Food Additive Maltitol and Maltitol Liquid".
[0030] In the above embodiment, when the maltitol content in the maltitol crystals is within the above range, the hygroscopicity of the molded body formed by pressing the maltitol crystals is relatively low, which helps to reduce the occurrence of agglomeration.
[0031] Exemplarily, the maltitol content in the maltitol crystals may be, but is not limited to, 99.5%, 99.6%, 99.7%, 99.8%, 99.9% or a range consisting of any two of the above values.
[0032] In the embodiments of the present application, the molded body has a suitable shape, which can further reduce the contact area between adjacent molded bodies, thereby reducing the occurrence of agglomeration.
[0033] In some embodiments of the present application, in the pressing process, the shape of the formed body includes one or more combinations of sphere, square and column.
[0034] For example, the shape of the formed body may be, but is not limited to, a polyhedron, a cube, a cuboid, a cone, a prism, a sphere, a hemisphere, a cylinder, or a mixture thereof.
[0035] In some embodiments of the present application, the shape of the molded body may be a sphere, and its diameter is 1 mm to 15 mm. The diameter of the spherical molded body within the above range can further reduce the contact area between the molded bodies, thereby reducing the occurrence of agglomeration.
[0036] Exemplarily, the diameter of the spherical molded body can be 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, 7 mm, 8 mm, 9 mm, 10 mm, 11 mm, 12 mm, 13 mm, 14 mm, 15 mm, or a range consisting of any two of the above values.
[0037] In the pulping process of the above embodiment, selecting a suitable coating material can not only help to coat the molded body, but also reduce the occurrence of agglomeration. Moreover, the mass ratio of each component in the coating material within a suitable range can further reduce the occurrence of agglomeration.
[0038] In some embodiments of the present application, in the pulping process, the mass ratio of polysaccharide to oil is (10-20):1.
[0039] In the above embodiment, when the mass ratio of polysaccharide to fat is within the above range, it can help to form a strong coating layer and can also make the molded bodies repel each other to prevent the occurrence of agglomeration.
[0040] Exemplarily, the mass ratio of polysaccharide to fat can be, but is not limited to, 10:1, 11:1, 12:1, 13:1, 14:1, 15:1, 16:1, 17:1, 18:1, 19:1, or 20:1.
[0041] In some embodiments of the present application, in the pulping process, the polysaccharide includes one or more combinations of chitin, chitosan, chitosan and xanthan gum. The above types of polysaccharides are selected, and the positive charge carried by them can attract the negative charge carried by the maltitol crystals, which can contribute to stable coating, and the coating layers formed by the above polysaccharides are all positively charged, so that the molded bodies can be mutually repelled, thereby reducing the occurrence of agglomeration. In addition, the above polysaccharides are all edible grade polysaccharides, which can help maintain the quality of the maltitol crystals.
[0042] In some embodiments of the present application, in the pulping process, the oil includes vegetable hydrogenated oil. The vegetable hydrogenated oil can make the coating layer have a suitable wetting angle, so that the coating layer has a certain hydrophobicity, thereby reducing the contact between water and maltitol crystals, thereby further reducing the occurrence of agglomeration.
[0043] In some embodiments of the present application, in the pulping process, the coating material further includes a second polysaccharide containing starch, and the mass ratio of the first polysaccharide, the second polysaccharide and the oil is (10-20): (2-5):1.
[0044] In the above embodiment, the addition of the second polysaccharide containing starch can further help the coating layer to reduce the occurrence of maltitol crystal agglomeration. Moreover, the mass ratio of the first polysaccharide, the second polysaccharide and the oil is within the above range, which can make the coating layer have sufficient positive charge and a suitable wetting angle, thereby further reducing the occurrence of agglomeration.
[0045] Exemplarily, the mass ratio of the first polysaccharide, the second polysaccharide and the oil can be, but is not limited to, 10:2:1, 11:2:1, 12:2:1, 13:2:1, 14:2:1, 15:2:1, 16:2:1, 17:2:1, 18:2:1, 19:2:1, 20:2:1, 11:3:1, 11:3:1, 11:4:1, 11:5:1, 12:4:1, 13:4:1, 13:5:1, etc.
[0046] In some embodiments of the present application, the starch may include one or more combinations of corn starch and pea starch. The above-mentioned starch can further help reduce the occurrence of maltitol crystal agglomeration.
[0047] In the embodiments of the present application, the coating layer has a suitable thickness which can help to further prevent the agglomeration of maltitol crystals. In this article, the thickness of the coating layer refers to the thickness of the material layer coated on the core shaped body in the radial direction of the core.
[0048] In some embodiments of the present application, the thickness of the coating layer may be 5µm to 20µm.
[0049] Exemplarily, the thickness of the coating layer may be, but is not limited to, 5µm, 6µm, 7µm, 8µm, 9µm, 10µm, 11µm, 12µm, 13µm, 14µm, 15µm, 16µm, 17µm, 8µm, 19µm, 20µm or a range consisting of any two of the above values.
[0050] In some embodiments of the present application, in the drying process, the drying process includes vacuum drying. Vacuum drying can reduce the oxygen content during drying, thereby preventing the dried material from oxidizing and deteriorating.
[0051] Furthermore, in some embodiments of the present application, the vacuum degree during vacuum drying is 90 KPa~100 KPa, the drying temperature is 60°C~70°C, and the drying time is 1h~5h.
[0052] In some embodiments of the present application, during the storage process, the protective gas includes one or more combinations of nitrogen and carbon dioxide.
[0053] The following embodiments describe the contents disclosed in the present application in more detail, and these embodiments are only used for illustrative explanations, because it is obvious to those skilled in the art that various modifications and changes are made within the scope of the present application disclosure. Unless otherwise stated, all parts, percentages and ratios reported in the following embodiments are based on mass, and all reagents used in the embodiments are commercially available or synthesized according to conventional methods, and can be used directly without further processing, and the instruments used in the embodiments are commercially available.
[0054] Example 1 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0055] Example 2 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 5 mm and the specific surface area was 4×10 -4 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0056] Example 3 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 10 mm and the specific surface area was 1.5×10 -4 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0057] Example 4 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 15 mm and the specific surface area was 7×10 -5 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0058] Example 5 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 8 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 8 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 12 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0059] Example 6 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 10 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 10 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer formed thereon is dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 20 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0060] Example 7 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0061] Example 8 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of chitosan and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0062] Example 9 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of xanthan gum and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0063] Example 10 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of chitosan, 1 kg of corn starch and 0.5 kg of vegetable hydrogenated oil in 8 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 12 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0064] Embodiment 11 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 6 kg of chitosan, 1 kg of corn starch and 0.5 kg of vegetable hydrogenated oil in 8 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 12.5 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0065] Example 12 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10-4 m 2 / g; Disperse 8 kg of chitosan, 1 kg of corn starch and 0.5 kg of vegetable hydrogenated oil in 10 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 15 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0066] Comparative Example 1 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; The molded body was put into a PE bag (30 kg / bag), and then the bag was filled with nitrogen for protection and sealed for storage.
[0067] Comparative Example 2 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of glucose and 0.5 kg of vegetable hydrogenated oil in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0068] Comparative Example 3 This embodiment provides a method for processing maltitol crystals, comprising: 25 kg of maltitol crystals with a particle size of 0.5 mm and a purity of 99.5% were pressed into spherical molded bodies at 25°C using a granulator. The diameter of the molded body was 2 mm and the specific surface area was 9.5×10 -4 m 2 / g; Disperse 5 kg of chitosan in 6 L of water to obtain a coating slurry; The molded body and the coating slurry are mixed to form a coating slurry layer on the surface of the molded body; The molded body with the coating slurry layer was dried in a vacuum oven at a vacuum degree of 95 KPa, a temperature of 60° C., and a drying time of 5 h, to form a coating layer with a thickness of 10 μm on the surface of the molded body; The molded body with the coating layer formed is put into a PE bag (30 kg / bag), and then the bag is filled with nitrogen for protection and sealed for storage.
[0069] Test Section The samples processed in Examples 1-12 and Comparative Examples 1-3 were exposed to a controlled environment at 25° C. and a relative humidity of 60%, and the degree of agglomeration was observed after 5 days, as shown in Table 1.
[0070] Table 1 Test results of Examples 1-12 and Comparative Examples 1-3 According to Table 1, by comparing the test results of Examples 1-12 and Comparative Examples 1-3, it can be seen that the processing method of maltitol crystals provided in the present application can effectively prevent maltitol crystals from agglomerating during storage, which is beneficial to its industrial application.
[0071] Finally, it should be noted that the above experimental examples are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned experimental examples, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned experimental examples, or replace some or all of the technical features therein with equivalents. These modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the experimental examples of the present application.
Claims
1. A method for processing maltitol crystals, characterized in that: include: A pressing step, pressing the powdered maltitol crystals into a molded body; A slurrying step, dispersing a coating material in a solvent to obtain a coating slurry, wherein the coating material comprises a first polysaccharide having a charge opposite to that of the maltitol crystals and fat; A coating step of mixing the molded body and the coating slurry to form a coating slurry layer on the surface of the molded body; A drying step of drying the molded body having the coating slurry layer formed thereon to form a coating layer on the surface of the molded body; The storage step is to seal and store the molded body with the coating layer under protective gas conditions.
2. The method for processing maltitol crystals according to claim 1, characterized in that: In the pressing step, the specific surface area of the molded body is 10 -5 m 2 / g~10 -3 m 2 / g.
3. The method for processing maltitol crystals according to claim 1, characterized in that: In the pressing process, the maltitol content in the maltitol crystals is greater than or equal to 99.5% on a dry basis.
4. The method for processing maltitol crystals according to claim 1, characterized in that: In the pressing process, the shape of the molded body includes one or more combinations of spherical, square and cylindrical shapes.
5. The method for processing maltitol crystals according to claim 1, characterized in that: In the pulping process, the mass ratio of the polysaccharide to the oil is (10-20):
1.
6. The method for processing maltitol crystals according to claim 5, characterized in that: In the pulping process, the polysaccharide includes one or more combinations of chitin, chitosan, chitosan and xanthan gum.
7. The method for processing maltitol crystals according to claim 5, characterized in that: In the pulping process, the oil includes vegetable hydrogenated oil.
8. A method for processing maltitol crystals according to any one of claims 1 to 7, characterized in that: In the pulping process, the coating material further includes a second polysaccharide containing starch, and the mass ratio of the first polysaccharide, the second polysaccharide and the oil is (10-20):(2-5):
1.
9. The method for processing maltitol crystals according to claim 1, characterized in that: In the drying step, the drying process includes vacuum drying.
10. The method for processing maltitol crystals according to claim 1, characterized in that: In the storage process, the protective gas includes one or more combinations of nitrogen and carbon dioxide.