Large-size composite material launching box and preparation method thereof

By wrapping fiber cloth on the mold and bonding metal frames and ring ribs, large-size composite material emission boxes are prepared, which solves the problems of complex, long cycle and high cost in the existing composite square box preparation methods, and simplified operation is achieved and cost-reducing effects.

CN119078224AActive Publication Date: 2024-12-06XIAN KANGBEN MATERIAL
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411410735.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-12-06
Estimated Expiration
2044-10-10

AI Technical Summary

Technical Problem

The existing composite square box preparation methods are too complex, have large process cycles and high costs, and cannot meet the preparation needs.

Method used

Using the methods of lining layer preparation, composite material layer preparation and composite solid material preparation, by applying rubber or composite material to the mold, wrapping fiber cloth, using rigid pressurization, and bonding metal frames and ring ribs to the outer surface to form Large-size composite material launch box.

Benefits of technology

It reduces operation difficulty, improves production efficiency, shortens manufacturing cycle, and to a certain extent reduces production costs, meeting the preparation needs of composite square boxes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119078224A_ABST
    Figure CN119078224A_ABST
Patent Text Reader

Abstract

The invention relates to a large-size composite material launching box and a preparation method thereof, and the preparation method comprises the following steps: smearing rubber or a first composite material on a pretreated mold, and curing to form a lining layer; coating the second composite material on the surface of fiber cloth to prepare prepreg cloth; after the prepreg cloth is wound on the outer surface of the lining layer, the prepreg cloth is cured in a rigid pressurization mode, and a composite material layer is obtained; a tool positioning mode is adopted, a plurality of metal frames are wound and bonded to the outer surface of the composite material layer through an adhesive, a plurality of ring ribs are wound on the outer surface of the composite material layer and arranged among the metal frames at intervals, a rigid pressurizing mode is adopted, the metal frames and the ring ribs are solidified on the outer surface of the composite material layer, and the composite material layer is formed. A composite solid material is obtained, and then the large-size composite material launching box is obtained. According to the method, special manufacturing equipment is not needed, the operation difficulty is greatly reduced, the production efficiency is effectively improved, and the manufacturing period is shortened.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of composite material preparation, and in particular relates to a large-size composite material launch box and a preparation method thereof. Background Art

[0002] Carbon fiber reinforced composite materials have the characteristics of light weight, high strength, high temperature resistance, corrosion resistance, excellent thermodynamic properties, and strong designability. Square structural parts are one of their representative structural forms and are widely used in civil, aerospace, military and other fields. In the field of intelligent manufacturing, they can be used as mechanical arms to achieve excellent characteristics such as light weight, high strength, small motion inertia, and excellent thermal stability. With the rapid development of related technologies, more stringent requirements are also put forward for the volume, quality, environmental adaptability, low cost and batch manufacturing capabilities of composite square boxes.

[0003] However, the existing preparation methods of composite square boxes are too complicated, have a long process cycle, and are costly, and cannot meet the preparation requirements well. Summary of the invention

[0004] In order to solve the above problems existing in the prior art, the present invention provides a large-size composite material launch box and a preparation method thereof. The technical problem to be solved by the present invention is achieved through the following technical solutions:

[0005] In the first aspect, the present invention provides a method for preparing a large-size composite launch box, comprising: preparing an inner lining layer: applying rubber or a first composite material to a pretreated mold, and curing and forming the inner lining layer; preparing a composite material layer: applying a second composite material formed by mixing epoxy resin and epoxy curing agent to the surface of a fiber cloth to prepare a prepreg cloth; according to a cycle of wet fiber winding and wet prepreg cloth laying, the prepreg cloth is wound on the outer surface of the inner lining layer, and then the prepreg cloth is cured by rigid pressurization to obtain a composite material layer; preparing a composite solid material: surface treating the composite material layer, using a tooling positioning method, using an adhesive to wrap and bond a plurality of metal frames on the outer surface of the composite material layer, wrapping a plurality of annular ribs on the outer surface of the composite material layer, and arranging them at intervals between the plurality of metal frames, and using the rigid pressurization method to cure the plurality of metal frames and the plurality of annular ribs on the outer surface of the composite material layer to obtain a composite solid material; processing: processing the structure consisting of the inner lining layer, the composite material layer and the composite solid material to obtain a large-size composite launch box.

[0006] In some embodiments, the first composite material is a composite material prepared by mixing epoxy resin, filler and ethanol.

[0007] In some embodiments, the mass ratio of the epoxy resin, the filler and the ethanol is: 100:(20-50):(10-30).

[0008] In some embodiments, the mass ratio of the second composite material to the fiber cloth is: (2-4): (6-8).

[0009] In some embodiments, the rigid pressurizing plate that performs the rigid pressurizing operation is composed of a plurality of pressure equalizing plates and a plurality of hard fillets; wherein the plurality of pressure equalizing plates and the plurality of hard fillets are connected by detachable bolts.

[0010] In some embodiments, the adhesive is a mixture of epoxy resin, a curing agent, and a filler.

[0011] In some embodiments, the mass ratio of the epoxy resin, the curing agent and the filler is: 100:(20-50):(10-40).

[0012] In some embodiments, the pretreated mold is obtained through the following steps: surface cleaning: using an organic solvent to wipe the mold; multiple heating: using a curing furnace to repeatedly heat the wiped mold, and applying a layer of silicone oil on the mold surface before each heating; applying a release agent: after completing the multiple heating steps, applying a release agent on the mold surface to obtain the pretreated mold.

[0013] In some embodiments, before performing the processing step, the method further includes: annealing the large-size composite material launch box, wherein the annealing temperature is 120° C. to 150° C., and the annealing time is 2 h to 4 h.

[0014] In a second aspect, the present invention further provides a large-sized composite launch box, which is prepared by the preparation method described in the first aspect. The large-sized composite launch box comprises: a box body and a composite solid material; the box body comprises an inner lining layer and a composite material layer, the composite material layer is wound and formed on the outer surface of the inner lining layer; the composite solid material is wound and formed on the outer surface of the composite material layer to enhance the load-bearing capacity of the box body.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: in view of the problem that the existing preparation method of the composite square box is too complicated, has a long process cycle, and is costly, and cannot well meet the preparation requirements, the present invention provides a large-size composite launch box and a preparation method thereof. The method first prepares an inner lining layer, and then prepares a composite material layer on the outer surface of the inner lining layer to form the body of the launch box. This method does not require the use of special manufacturing equipment, greatly reduces the difficulty of operation, and uses a mixture of carbon fiber and epoxy resin to prepare the composite material layer, which can effectively improve production efficiency, shorten the manufacturing cycle, reduce production costs to a certain extent, and meet preparation requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The invention provides a method for preparing a large-size composite material launch box.

[0017] Figure 2 is an overall deformation cloud diagram of a composite material layer attached to an inner lining layer under a load of 0.18 MPa provided in an embodiment of the present invention;

[0018] Figure 3 is a full cross-sectional schematic diagram of tooling positioning provided by an embodiment of the present invention;

[0019] Figure 4 Schematic diagram of the components of the rigid pressure plate provided by an embodiment of the present invention;

[0020] Figure 5 It is a schematic structural diagram of a large-size composite material launch box provided in an embodiment of the present invention.

[0021] Reference numerals:

[0022] 1: Upper positioning plate; 2: Lower positioning plate; 3: Bolts; 4: Box body; A: Steel plate pressure block; B: Hard rounded corner pressure block; C: Ring rib pressure plate; D: Metal parts pressure plate. DETAILED DESCRIPTION

[0023] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.

[0024] In the description of the present invention, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0025] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine different embodiments or examples described in this specification.

[0026] Although the present invention is described herein in conjunction with various embodiments, in the process of implementing the claimed invention, those skilled in the art may understand and implement other variations of the disclosed embodiments by viewing the drawings, the disclosure, and the appended claims. In the claims, the word "comprising" does not exclude other components or steps, and "one" or "an" does not exclude multiple situations. A single processor or other unit may implement several functions listed in the claims. Certain measures are recorded in different dependent claims, but this does not mean that these measures cannot be combined to produce good results.

[0027] The large-size composite material launch box and its preparation method proposed by the present invention are now described in conjunction with the accompanying drawings. Figure 1 This is a method for preparing a large-size composite material launch box provided by an embodiment of the present invention. Figure 1 As shown, the method includes the steps of: preparing the inner lining layer, preparing the composite material layer, preparing the composite solid material and processing. Specifically, the content of each step includes:

[0028] Step 1: Preparation of the inner lining layer: Apply the rubber or the first composite material to the pre-treated mold and solidify to form the inner lining layer.

[0029] Here, the first composite material or rubber is applied to the pretreated mold by knife coating or spraying.

[0030] Here, the first composite material is a composite material prepared by mixing epoxy resin, filler and ethanol, and the mass ratio of epoxy resin, filler and ethanol is: 100: (20-50): (10-30).

[0031] In a possible implementation, the types of fillers include: short-cut viscose carbon fiber, short-cut high-silica fiber, graphite, white carbon black, etc. Epoxy resin can be replaced by phenolic resin, epoxy phenolic resin, etc., and ethanol can be replaced by acetone, dichloromethane, ethyl acetate, etc.

[0032] It should be noted that the mass ratio of each material in the first composite material is constant and does not change with the type of material.

[0033] In a possible implementation, the types of rubber include natural rubber, styrene-butadiene rubber, nitrile rubber, fluororubber, etc.

[0034] In a possible implementation, the inner lining layer is in the shape of a rectangular tube.

[0035] In one possible implementation, the pretreated mold is obtained through the following steps: surface cleaning: using an organic solvent to wipe the mold; multiple heating: using a curing furnace to repeatedly heat the wiped mold, and applying a layer of silicone oil on the mold surface before each heating; applying a release agent: after completing the multiple heating steps, applying a release agent on the mold surface to obtain a pretreated mold.

[0036] Here, the organic solvent used is ethanol, ethyl acetate, acetone, dichloromethane, petroleum ether, etc. The release agent used is silicone oil release agent, amide release agent, polyurethane release agent, organic fluoride release agent, silicone grease release agent, etc.

[0037] Here, when performing the step of heating multiple times, the number of heating times in the curing oven is 2 to 4 times, and the temperature of the curing oven is 110° C. to 150° C.

[0038] By using low-cost, high-carbon residual rate rubber or a first composite material to form an integral lining layer, the lining layer has the characteristics of ablation resistance and greatly reduces the production cost compared to commercially available coatings; compared to the method of generating an inner lining layer by splicing multiple modules, the inner lining layer provided by the present invention has a more uniform thickness, more consistent performance, higher reliability in use, and can be reused many times, thereby greatly reducing the overall production cost of the launch box.

[0039] Step 2: Preparation of composite material layer: Apply a second composite material formed by mixing epoxy resin and epoxy curing agent on the surface of the fiber cloth to prepare a prepreg cloth; wind the prepreg cloth on the outer surface of the lining layer according to the cycle of wet fiber winding and wet prepreg cloth laying, and then cure the prepreg cloth by rigid pressure to obtain a composite material layer.

[0040] Here, the mass ratio of the second composite material to the fiber cloth is: (2-4): (6-8).

[0041] In a possible implementation, the carbon fiber is one or a combination of T300 grade carbon fiber, T700 grade carbon fiber, T800 grade carbon fiber, etc.; the epoxy resin can be replaced by phenolic resin, epoxy phenolic resin, etc.

[0042] Here, the fiber cloth is a large-tow high-density fiber cloth, which is one or a combination of unidirectional carbon fiber cloth with a surface density of 200g (400g), satin carbon fiber cloth with a surface density of 250g (400g), twill carbon fiber cloth with a surface density of 250g (400g), and the like.

[0043] In a possible implementation, the epoxy curing agent includes an amine curing agent, an acid anhydride curing agent, and an imidazole curing agent.

[0044] Here, after the second composite material is prepared, the second composite material is applied to the fiber cloth several times to obtain a prepreg, and the fiber cloth is laid on the inner lining layer, and the laying angles include but are not limited to 0°, ±20°, ±45° and 90°. After the second composite material is prepared, the second composite material is applied to the fiber cloth several times to obtain a prepreg; then, according to the cycle of wet fiber winding and wet prepreg laying, specifically, the prepreg is wound on the outer surface of the inner lining layer, and after standing for 2 hours, the prepreg is prepared again and continued to be wound on the outer surface of the inner lining layer, and the cycle is stopped after the feeler gauge and steel ruler confirm that the outer dimensions reach the required thickness of the composite material layer. Among them, fillet filling is performed every two cycles.

[0045] Here, in order to ensure that the thickness of each surface of the composite material layer is uniform, rigid pressurization or equalizing plate vacuum pressurization is used to solidify the composite structure of the composite material layer and the lining layer. Specifically, when rigid pressurization is used, the rigid pressurization plate that performs the rigid pressurization operation is composed of multiple equalizing plates and multiple hard fillets; wherein, the multiple equalizing plates and the multiple hard fillets are connected by detachable bolts. Removable bolts (for example, square steel bolts) are used to pressurize the composite material layer attached to the lining layer. When using an equalizing plate vacuum pressurization, the box fixed with the equalizing plate and the hard fillets is placed in a vacuum bag, and the vacuum bag is evacuated to pressurize the whole. Among them, the vacuum degree is -0.085MPa to -0.092MPa.

[0046] Figure 2 It is a cloud diagram of the overall deformation of the composite material layer attached to the inner lining layer under a load of 0.18 MPa provided in an embodiment of the present invention. Figure 2 U, magnitude, refers to the equivalent displacement in the x, y, and z directions. Under a load of 0.18 MPa, the deformation is 20.32 mm. Relative to the size of the entire box, the deformation is within a controllable range.

[0047] By using a second composite material mixed with carbon fiber and epoxy resin to prepare the composite material layer of the launch box on the inner lining layer, compared with the existing method of first preparing the composite material layer and then preparing the inner lining layer inside the composite material layer, the preparation method provided by the present invention is simpler to operate, does not require specific equipment, reduces the operating difficulty of the operator, effectively improves production efficiency, and reduces production costs to a certain extent.

[0048] Step 3: Preparation of composite solid materials: Surface treatment is performed on the composite material layer, and a plurality of metal frames are wrapped and bonded to the outer surface of the composite material layer using an adhesive by means of tooling positioning, and a plurality of ring ribs are wrapped around the outer surface of the composite material layer and spaced between the plurality of metal frames, and a rigid pressurization method is used to solidify the plurality of metal frames and the plurality of ring ribs on the outer surface of the composite material layer to obtain a composite solid material.

[0049] Here, before preparing the composite solid material, the outer surface of the composite material layer needs to be processed by grinding and wiping with a cleaning agent.

[0050] Here, the adhesive is mixed with epoxy resin, curing agent and filler. The mass ratio of epoxy resin, curing agent and filler is: 100: (20-50): (10-40). Specifically, the epoxy resin is glycidyl ether epoxy resin, the curing agent is an amine curing agent, and the filler is white carbon black.

[0051] Here, the shape of the metal frame finally wound is a rectangular metal frame, and the shape of the annular rib is also a rectangular frame.

[0052] Figure 3 1 is a schematic cross-sectional view of the tooling positioning provided by an embodiment of the present invention. Figure 3 As shown, the upper positioning plate 1 and the lower positioning plate 2 are connected by bolts 3 to position the box body 4. The box body 4 refers to a composite material layer attached to the inner lining layer. The upper positioning plate 1 and the lower positioning plate 2 can be used to accurately determine the relative position of the metal frame on the upper surface, avoiding the position deviation caused by manual measurement during the assembly process, so that the box body can be smoothly stacked in the later stage. After completing the tooling positioning, use adhesive to fix multiple metal frames, and use tools to tightly fit multiple ring ribs to the box body 4. Subsequently, rigid pressure is used to solidify the multiple metal frames and multiple ring ribs. Figure 4 Schematic diagram of the components of the rigid pressure plate provided by the embodiment of the present invention. Figure 4 As shown, the rigid pressure plate includes: a steel plate pressure block A, a hard rounded corner pressure block B, a ring rib pressure plate C and a metal part pressure plate D. The steel plate pressure block A, the hard rounded corner pressure block B, the ring rib pressure plate C and the metal part pressure plate D are connected by detachable bolts.

[0053] By preparing composite solid materials on the surface of the composite material layer, the load-bearing capacity of the large-size composite launch box can be further strengthened and supplemented.

[0054] Step 4: Processing: Process the structure consisting of the lining layer, composite material layer and composite solid material to obtain a large-sized composite launch box.

[0055] Here, before performing the processing step, the method further includes: annealing the large-size composite material launch box, wherein the annealing temperature is 120°C to 150°C and the annealing time is 2h to 4h. Specifically, after removing the rigid pressure plate, the curing furnace is used again to anneal the large-size composite material launch box to eliminate the residual stress inside the large-size composite material launch box and improve the service life of the large-size composite material launch box.

[0056] Here, the processing includes some conventional processing operations such as machining, demoulding and painting.

[0057] Corresponding to the method for preparing a large-size composite material launch box provided by the present invention, the present invention also provides a large-size composite material launch box. Figure 5 Schematic diagram of the structure of a large-sized composite material launch box provided by an embodiment of the present invention. Figure 5 As shown, the large-size composite launch box includes: a box body and a composite solid material; the box body includes an inner lining layer and a composite material layer, the composite material layer is wound and formed on the outer surface of the inner lining layer; the composite solid material is wound and formed on the outer surface of the composite material layer to enhance the bearing capacity of the box body. The composite solid material includes: multiple metal frames and multiple ring ribs.

[0058] In view of the problem that the existing preparation method of composite square box is too complicated, has a long process cycle, high cost, and cannot well meet the preparation needs, the present invention provides a large-size composite launch box and a preparation method thereof. The method first prepares an inner lining layer, and then prepares a composite material layer on the outer surface of the inner lining layer to form the body of the launch box. There is no need to use special manufacturing equipment, which greatly reduces the difficulty of operation. In addition, the composite material layer is prepared by mixing carbon fiber and epoxy resin, which can effectively improve production efficiency, shorten the manufacturing cycle, reduce production costs to a certain extent, and meet preparation needs.

[0059] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.

Claims

1. A method for preparing a large-size composite material launch box, characterized in that: The method comprises: Preparation of the inner lining layer: applying the rubber or the first composite material to the pre-treated mold and curing to form the inner lining layer; Preparation of composite material layer: applying a second composite material formed by mixing epoxy resin and epoxy curing agent on the surface of fiber cloth to prepare prepreg cloth; winding the prepreg cloth on the outer surface of the inner lining layer according to a cycle of wet fiber winding and wet prepreg cloth laying, and curing the prepreg cloth by rigid pressurization to obtain a composite material layer; Preparation of composite solid material: surface treatment is performed on the composite material layer, a plurality of metal frames are wound and bonded to the outer surface of the composite material layer by an adhesive in a tooling positioning manner, a plurality of annular ribs are wound on the outer surface of the composite material layer and spaced between the plurality of metal frames, and the plurality of metal frames and the plurality of annular ribs are solidified on the outer surface of the composite material layer by the rigid pressurization manner to obtain a composite solid material; Processing: Processing the structure composed of the lining layer, the composite material layer and the composite solid material to obtain a large-sized composite material launch box.

2. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: The first composite material is a composite material prepared by mixing epoxy resin, filler and ethanol.

3. The method for preparing a large-size composite material launch box according to claim 2, characterized in that: The mass ratio of the epoxy resin, the filler and the ethanol is: 100:(20-50):(10-30).

4. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: The mass ratio of the second composite material to the fiber cloth is: (2-4): (6-8).

5. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: The rigid pressurizing plate for performing the rigid pressurizing operation is composed of a plurality of pressure equalizing plates and a plurality of hard fillets; wherein the plurality of pressure equalizing plates and the plurality of hard fillets are connected by detachable bolts.

6. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: The adhesive is prepared by mixing epoxy resin, curing agent and filler.

7. The method for preparing a large-size composite material launch box according to claim 6, characterized in that: The mass ratio of the epoxy resin, the curing agent and the filler is: 100:(20-50):(10-40).

8. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: The pretreated mold is obtained by the following steps: Surface cleaning: Use organic solvent to wipe the mold; Multiple heating: using a curing furnace to repeatedly heat the wiped mold, and applying a layer of silicone oil on the mold surface before each heating; Applying a release agent: After the multiple heating steps are completed, a release agent is applied to the surface of the mold to obtain the pretreated mold.

9. The method for preparing a large-size composite material launch box according to claim 1, characterized in that: Before performing the processing step, the method further includes: annealing the large-size composite material launch box, wherein the annealing temperature is 120° C. to 150° C. and the annealing time is 2 hours to 4 hours.

10. A large-sized composite material launch box, characterized in that: The large-size composite material launch box is prepared by the preparation method of the large-size composite material launch box described in any one of claims 1 to 9 above, and the large-size composite material launch box comprises: a box body and a composite solid material; the box body comprises an inner lining layer and a composite material layer, and the composite material layer is wound and molded on the outer surface of the inner lining layer; the composite solid material is wound and molded on the outer surface of the composite material layer to enhance the bearing capacity of the box body.

Citation Information

Patent Citations

  • Preparation method for seal head-free fiber reinforced resin-based composite material combustion chamber shell of rocket projectile

    CN110978558A

  • Large-size no-lining composite material storage tank mold and using method and application

    CN111152474A

  • Process method for forming large-diameter square launching tube made of composite material

    CN117584483A

  • Manufacturing method of launching box with special-shaped guide rail

    CN118082254A