Semi-permanent curing coating convenient for DLP (Digital Light Processing) 3D (Three-Dimensional) printing demolding and manufacturing method of semi-permanent curing coating

By preparing a polyemulsion coating with butyl acrylate, short glass fibers and glass microbeads as the core components, the problems of material waste and mold damage during the mold release process of DLP 3D printing mold are solved, and efficient and simple mold release is achieved Process and good mechanical properties.

CN119081498APending Publication Date: 2024-12-06GUIZHOU INST OF METALLURGY & CHEM ENG +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411174102.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing DLP 3D printed molds are prone to waste of materials and damage to the mold during the demolding process, and are difficult to clean. They lack a simple, efficient and widely applicable semi-permanent curing coating to solve this problem.

Method used

Polyemulsion coatings with butyl acrylate, short glass fiber, glass microbeads and emulsifiers as core components are prepared through specific dispersion and beating processes to form metallic and oleophobic coatings, combined with ammonium persulfate as the initiation The agent and aqueous sodium bicarbonate solution are used as pH adjusters to form a semi-permanent curing coating by drying and curing.

Benefits of technology

It improves the uniformity, strength and weather resistance of the coating, reduces the adsorption force of the printing contact surface, is easy to release, and maintains the physical and chemical properties and moldability of the surface. It is suitable for DLP 3D printing, and the production process is simple and efficient.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a semi-permanent curing coating convenient for DLP 3D printing demolding and a preparation method thereof, the coating is prepared by taking butyl acrylate, short glass fiber, glass beads, an emulsifier NP-10 and an emulsifier K-12 as cores, butyl acrylate, a silane coupling agent KH-570, an emulsifier NP-10 and an emulsifier K-12 as shells, ammonium persulfate as an initiator, a curing agent as a solvent, a curing agent as a curing agent, a curing agent as a curing agent, a curing agent as a curing agent and a curing agent as a curing agent. A poly-emulsion is formed by taking a sodium bicarbonate aqueous solution as a pH regulator, and the coating is a metal-philic and nylon-hydrophobic coating which is dried and cured after being coated. The problems that in the manufacturing and using process of a DLP 3D printing piece, especially an elastomer, due to difficult demolding, a mold is abraded and corroded, and the surface of a product is torn, scratched and subjected to hole dredging are solved, and the beneficial effects that the production process is simple and efficient, the practical effect for DLP 3D printing is good, the matching performance with an existing device is wide, and semi-curing is easy to repair and maintain are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of additive manufacturing, and in particular to a semi-permanent curing coating for facilitating demolding of DLP 3D printing and a manufacturing method thereof. Background Art

[0002] In the prior art, molds generally used for digital light processing (DLP) 3D printing are made of stainless steel, which is a metal plane. Some devices deliberately make the plane relatively rough or punch holes to facilitate the attachment of photosensitive resin. However, all devices have the problem of difficulty in removing the printed parts after they are formed. Either the material of the basic part of the molding is discarded, resulting in waste and difficulty in cleaning the mold surface, or the printed part is removed by a physical flat shovel, which will also damage the mold.

[0003] Therefore, there is a need in the market for a semi-permanent curing coating and a manufacturing method thereof for DLP 3D printing demolding, which has a simple and efficient production process, good practical effects for DLP 3D printing, wide compatibility with existing devices, and is easy to maintain and repair. Summary of the invention

[0004] The present invention aims to provide a semi-permanent curing coating and a manufacturing method thereof, which is convenient for DLP 3D printing demolding and has a raw material derived from biomass, is green and environmentally friendly, has a simple preparation process, has self-repairing ability, has good mechanical properties and self-repairing properties.

[0005] In order to achieve the above-mentioned object, the present invention adopts the following technical scheme: a semi-permanent curing coating for DLP 3D printing demolding, the coating is a polyemulsion composed of butyl acrylate, short glass fiber, glass microbeads, emulsifier NP-10, emulsifier K-12 as a core, butyl acrylate, silane coupling agent KH-570, emulsifier NP-10, emulsifier K-12 as a shell, ammonium persulfate as an initiator, and sodium bicarbonate aqueous solution as a pH regulator, and the metal-philic and oleophobic coating is cured by drying after coating, and the preparation method thereof comprises the following stages: S1: Raw material preparation ① Raw material preparation: prepare sufficient aluminum chloride, glass microbeads with a particle size of 10μm-20μm, hot-melt fibers with a silicon mass fraction of 1.3%-1.6%, micro-glass fiber wool, silane coupling agent KH-570, emulsifier NP-10, emulsifier K-12, butyl acrylate, ammonium persulfate aqueous solution with a solute mass fraction of 0.6%, and sodium bicarbonate aqueous solution with a solute mass fraction of 0.6%; ② Equipment preparation: prepare a fiber disintegrator, a dehydration device with a spin-drying device, a vacuum device, and a baking device, a pulping device, and a resistance furnace; S2: Nanofiber Preparation ① The hot melt fiber and micro glass fiber wool prepared in step ① of stage S1 are mixed evenly in a mass ratio of 1:(2-3) to obtain a mixed solid A prepared in step ① of stage S1; ② The mixed solid A obtained in step ① is mixed with deionized water in a mass ratio of 1: (450-480) and stirred evenly, and then put into the fiber disintegrator prepared in step ② of stage S1, and physically separated at a speed of 4000 rpm for 7 min-7.5 min to obtain a wet separated fiber slurry; ③ The wet separated fiber slurry obtained in step ② is placed in a dehydrating device, and subjected to spin drying, vacuum dehydration, and drying, respectively, wherein the drying process parameters are: temperature 230° C.-240° C., time 70 min-80 min, to obtain dry cellulose; ④ The cellulose obtained in step ③ is mixed with water in a mass ratio of 1: (45-50) and dispersed for 3-5 minutes, and then the dispersion is put into a pulping machine, and the pulping is performed at a speed of 550-600 rpm for 135-150 seconds, and then the pulped dispersion is put into a dehydrating device, and then dehydrated to obtain dry short fibers; S3: Coating emulsion preparation ① The dried short fibers obtained in step ④ of stage S2 are mixed with the glass microbeads, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 in a mass ratio of 10: (0.5-0.8): (145-150): (2-3): (0.5-0.8) at room temperature for 30-35 minutes to obtain a core emulsion; ② The KH-570, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 were fully mixed at a mass ratio of 10: (75-80): (2-3): (1-1.2) at room temperature for 30 min-35 min to obtain a shell emulsion; ③ Add the ammonium persulfate aqueous solution prepared in step S1① to the core emulsion obtained in step ①, slowly heat it to 82℃-85℃ under stirring, and continue to add the initiator solution until equilibrium after the blue light appears for 10 minutes, and keep the temperature for 80min-90min to obtain a pre-reaction emulsion; ④ Start dripping the shell emulsion into the pre-reaction emulsion obtained in step ③, complete the dripping within 2-2.5 hours, continue to keep warm for 1.5 hours to 2 hours, then use the sodium bicarbonate aqueous solution prepared in step ① of stage S1 to adjust the pH to 5.5-6, and finally cool to no more than 40°C, start discharging, and obtain the desired coating emulsion; S4: Paint curing The coating emulsion obtained in step ④ of stage S3 is coated on the surface of the starting metal plate of DLP 3D printing with a mesh center distance of 5mm×5mm and a width of 1.5-2mm, and dried at 130°C for 3min-5min to obtain the required semi-permanently cured coating.

[0006] Compared with the prior art, the present invention has the following advantages due to the adoption of the above technical solution: (1) The present invention improves the dispersion performance of the micro-glass fiber slurry by controlling the dispersion process and the pulping process. The addition of hot-melt fibers affects the uniformity of the micro-glass fiber composite felt and significantly improves the mechanical properties of the micro-glass fiber composite felt. Therefore, the uniformity, strength and weather resistance of the coating of the present invention are superior to those of existing general coatings.

[0007] (2) The type of coating and the molding method of the coating affect the mechanical properties and surface physical and chemical properties of the coating composite structure. Coatings with a smaller surface roughness have a lower adsorption force as a printing contact surface and are easy to demold. Coatings with a larger surface roughness have a higher adsorption force as a printing contact surface and are easy to mold. The coating synthesized by the present invention has a reasonable distribution of components and a stable structure. The core material has an affinity with the steel surface and thus has a strong adhesion, but is not compatible with the resin, so it is easy to demold. Although the shell material is also not compatible with the resin, it physically has a relatively rough surface with quite a lot of pores and is easy to mold.

[0008] Therefore, the present invention has the characteristics of simple and efficient production process, good practical effect for DLP 3D printing, wide compatibility with existing devices, and easy maintenance of semi-curing. DETAILED DESCRIPTION Example

[0009] A semi-permanent curing coating for easy demolding of DLP 3D printing, the coating is a polyemulsion composed of butyl acrylate, short glass fiber, glass microbeads, emulsifier NP-10, and emulsifier K-12 as a core, butyl acrylate, silane coupling agent KH-570, emulsifier NP-10, and emulsifier K-12 as a shell, ammonium persulfate as an initiator, and sodium bicarbonate aqueous solution as a pH regulator, and is a metal-philic and oleophobic coating that is cured by drying after coating; The preparation method includes the following stages: S1: Raw material preparation ① Raw material preparation: prepare sufficient aluminum chloride, glass microbeads with a particle size of 10μm-20μm, hot-melt fibers with a silicon mass fraction of 1.3%-1.6%, micro-glass fiber wool, silane coupling agent KH-570, emulsifier NP-10, emulsifier K-12, butyl acrylate, ammonium persulfate aqueous solution with a solute mass fraction of 0.6%, and sodium bicarbonate aqueous solution with a solute mass fraction of 0.6%; ② Equipment preparation: prepare a fiber disintegrator, a dehydration device with a spin-drying device, a vacuum device, and a baking device, a pulping device, and a resistance furnace; S2: Nanofiber Preparation ① The hot melt fiber and micro glass fiber wool prepared in step ① of stage S1 are mixed evenly in a mass ratio of 1:(2-3) to obtain a mixed solid A prepared in step ① of stage S1; ② The mixed solid A obtained in step ① is mixed with deionized water in a mass ratio of 1: (450-480) and stirred evenly, and then put into the fiber disintegrator prepared in step ② of stage S1, and physically separated at a speed of 4000 rpm for 7 min-7.5 min to obtain a wet separated fiber slurry; ③ The wet separated fiber slurry obtained in step ② is placed in a dehydrating device, and subjected to spin drying, vacuum dehydration, and drying, respectively, wherein the drying process parameters are: temperature 230° C.-240° C., time 70 min-80 min, to obtain dry cellulose; ④ The cellulose obtained in step ③ is mixed with water in a mass ratio of 1: (45-50) and dispersed for 3-5 minutes, and then the dispersion is put into a pulping machine, and the pulping is performed at a speed of 550-600 rpm for 135-150 seconds, and then the pulped dispersion is put into a dehydrating device, and then dehydrated to obtain dry short fibers; S3: Coating emulsion preparation ① The dried short fibers obtained in step ④ of stage S2 are mixed with the glass microbeads, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 in a mass ratio of 10: (0.5-0.8): (145-150): (2-3): (0.5-0.8) at room temperature for 30-35 minutes to obtain a core emulsion; ② The KH-570, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 were fully mixed at a mass ratio of 10: (75-80): (2-3): (1-1.2) at room temperature for 30 min-35 min to obtain a shell emulsion; ③ Add the ammonium persulfate aqueous solution prepared in step S1① to the core emulsion obtained in step ①, slowly heat it to 82℃-85℃ under stirring, and continue to add the initiator solution until equilibrium after the blue light appears for 10 minutes, and keep the temperature for 80min-90min to obtain a pre-reaction emulsion; ④ Start dripping the shell emulsion into the pre-reaction emulsion obtained in step ③, complete the dripping within 2-2.5 hours, continue to keep warm for 1.5 hours to 2 hours, then use the sodium bicarbonate aqueous solution prepared in step ① of stage S1 to adjust the pH to 5.5-6, and finally cool to no more than 40°C, start discharging, and obtain the desired coating emulsion; S4: Paint curing The coating emulsion obtained in step ④ of stage S3 is coated on the surface of the starting metal plate of DLP 3D printing with a mesh center distance of 5mm×5mm and a width of 1.5-2mm, and dried at 130°C for 3min-5min to obtain the required semi-permanently cured coating.

[0010] The semi-permanently cured coating material prepared by the present invention for DLP 3D printing demolding has the characteristics of simple and efficient production process, good practical effect for DLP 3D printing, wide compatibility with existing devices, and easy maintenance of semi-curing. The above description of the disclosed embodiments is intended only to enable those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A semi-permanent curing coating for DLP 3D printing demolding, characterized in that: The coating is a polyemulsion composed of butyl acrylate, short glass fiber, glass microbeads, emulsifier NP-10 and emulsifier K-12 as a core, butyl acrylate, silane coupling agent KH-570, emulsifier NP-10 and emulsifier K-12 as a shell, ammonium persulfate as an initiator and sodium bicarbonate aqueous solution as a pH regulator. The coating is a metal-philic and oleophobic coating that is cured by drying after coating. The preparation method thereof comprises the following stages: S1: Raw material preparation ① Raw material preparation: prepare sufficient aluminum chloride, glass microbeads with a particle size of 10μm-20μm, hot-melt fibers with a silicon mass fraction of 1.3%-1.6%, micro-glass fiber wool, silane coupling agent KH-570, emulsifier NP-10, emulsifier K-12, butyl acrylate, ammonium persulfate aqueous solution with a solute mass fraction of 0.6%, and sodium bicarbonate aqueous solution with a solute mass fraction of 0.6%; ② Equipment preparation: prepare a fiber disintegrator, a dehydration device with a spin-drying device, a vacuum device, and a baking device, a pulping device, and a resistance furnace; S2: Nanofiber Preparation ① The hot melt fiber and micro glass fiber wool prepared in step ① of stage S1 are mixed evenly in a mass ratio of 1:(2-3) to obtain a mixed solid A prepared in step ① of stage S1; ② The mixed solid A obtained in step ① is mixed with deionized water in a mass ratio of 1: (450-480) and stirred evenly, and then put into the fiber disintegrator prepared in step ② of stage S1, and physically separated at a speed of 4000 rpm for 7 min-7.5 min to obtain a wet separated fiber slurry; ③ The wet separated fiber slurry obtained in step ② is placed in a dehydrating device, and subjected to spin drying, vacuum dehydration, and drying, respectively, wherein the drying process parameters are: temperature 230° C.-240° C., time 70 min-80 min, to obtain dry cellulose; ④ The cellulose obtained in step ③ is mixed with water in a mass ratio of 1: (45-50) and dispersed for 3-5 minutes, and then the dispersion is put into a pulping machine, and the pulping is performed at a speed of 550-600 rpm for 135-150 seconds, and then the pulped dispersion is put into a dehydrating device, and then dehydrated to obtain dry short fibers; S3: Coating emulsion preparation ① The dried short fibers obtained in step ④ of stage S2 are mixed with the glass microbeads, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 in a mass ratio of 10: (0.5-0.8): (145-150): (2-3): (0.5-0.8) at room temperature for 30-35 minutes to obtain a core emulsion; ② The KH-570, butyl acrylate, emulsifier NP-10 and emulsifier K-12 prepared in step ① of stage S1 were fully mixed at a mass ratio of 10: (75-80): (2-3): (1-1.2) at room temperature for 30 min-35 min to obtain a shell emulsion; ③ Add the ammonium persulfate aqueous solution prepared in step S1① to the core emulsion obtained in step ①, slowly heat it to 82℃-85℃ under stirring, and continue to add the initiator solution until equilibrium after the blue light appears for 10 minutes, and keep the temperature for 80min-90min to obtain a pre-reaction emulsion; ④ Start dripping the shell emulsion into the pre-reaction emulsion obtained in step ③, complete the dripping within 2-2.5 hours, continue to keep warm for 1.5 hours to 2 hours, then use the sodium bicarbonate aqueous solution prepared in step ① of stage S1 to adjust the pH to 5.5-6, and finally cool to no more than 40°C, start discharging, and obtain the desired coating emulsion; S4: Paint curing The coating emulsion obtained in step ④ of stage S3 is coated on the surface of the starting metal plate of DLP 3D printing with a mesh center distance of 5mm×5mm and a width of 1.5-2mm, and dried at 130°C for 3min-5min to obtain the required semi-permanently cured coating.