Water seepage prevention treatment method for tunnel secondary lining structure
By performing waterproofing treatment at the tunnel construction joints, including changing the waterproof plate, pre-embedding the grouting pipe and installing water-stop rubber strips, the problem of water seepage after the tunnel lining is damaged is solved, and the effective establishment of the waterproof system and the convenience of later maintenance is achieved. sex.
Patent Information
- Application Number
- CN202411465850.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-21
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the prior art, external forces or other force majeure factors cause damage to tunnel lining and require rework treatment or waterproofing system damage, and a large amount of seepage is formed at the deformation joints and the weak parts of the construction joints, which is difficult to repair and maintain in the later stage.
A method of anti-seepage water treatment at the secondary lining structure of the tunnel, including chiseling and removing the secondary lining plate with large water output along the construction joint, replacing the waterproof plate, pouring new secondary lining concrete, and pre-embedding and grouting at the construction joint The pipe is installed with water stop rubber strips to form a second waterproof system, and clean it with high-pressure water or high-pressure air. It is sealed with elastic sealant and high-elastic wet epoxy resin mortar to ensure the extended water seepage path and weakened pressure.
Effectively seal and diversion, ensure the establishment of a waterproofing system, prevent large amounts of water seepage in the later tunnel, and facilitate later renovation and maintenance.
Smart Images

Figure CN119084043A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of tunnel construction, and in particular to an anti-seepage treatment method for a secondary lining structure of a tunnel. Background Art
[0002] At present, tunnel waterproofing is one of the important links in the tunnel construction process. Tunnel waterproofing not only concerns the safety and stability of the tunnel structure, but also directly affects the service life of the tunnel and subsequent maintenance costs. At every stage of tunnel construction, from survey and design, construction to later operation and management, it is necessary to attach great importance to and carefully implement waterproofing measures.
[0003] However, in the prior art, external forces or other force majeure factors may cause the tunnel lining to be damaged and require rework or damage the waterproofing system, resulting in a large amount of water seepage at the weak points of the deformation joints and construction joints, making it difficult to carry out repairs and maintenance at a later stage. Summary of the invention
[0004] The purpose of the present invention is to provide a method for anti-seepage treatment at the secondary lining structure of a tunnel, aiming to solve the technical problems in the prior art that the tunnel lining is damaged due to external force or other force majeure factors and needs to be reworked or the waterproof system is destroyed, resulting in a large amount of seepage at the weak points of the deformation joints and construction joints, which makes it difficult to carry out repairs and maintenance in the later stage.
[0005] To achieve the above object, the present invention adopts a method for anti-seepage treatment at a secondary lining structure of a tunnel, comprising the following steps:
[0006] Chisel out the secondary lining panels with large water discharge along the construction joints, replace the damaged waterproof panels, and chisel the tongue-and-groove joints in the middle of the secondary lining;
[0007] Place a 2cm thick foam board at the bottom of the tongue-and-groove joint and pour new secondary lining concrete. After the new secondary lining concrete reaches the designed strength, clean the inside and both sides of the construction joint, and use a manual grinder to grind and chamfer the two positive corners on the outside of the deformation joint;
[0008] Use a wire brush to remove sand and concrete slag from the construction joint surface within the laying range, then use high-pressure water or high-pressure wind to blow it clean, embed the pre-buried grouting pipe along the construction joint, select a 25mm diameter water-stop rubber strip according to the division of the grouting pipe, and combine them to form a second waterproof system for local drainage of leakage;
[0009] After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, and tamp it with a stick. After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections. The joints or pores will no longer accept more slurry, and the grouting can be completed. After reaching a certain strength, cut off the grouting pipe opening and the exhaust pipe opening, clean them, and seal them with elastic sealant.
[0010] A water receiving box is installed on the outside of the expansion joint. Water-stop rubber pads are placed on both sides of the water receiving box and it is fixed to the secondary lining of the tunnel with expansion bolts. The outside is sealed with highly elastic moist epoxy resin mortar. The water receiving box is extended to the top of the longitudinal drainage ditch for centralized drainage.
[0011] The height of the tongue-and-groove seam is 10 cm, the depth is 5 cm, and the groove is kept vertical as much as possible to increase the water flow path of the seepage water and reduce the seepage pressure.
[0012] Among them, the steps of cleaning both sides of the construction joint include the following steps:
[0013] At the lower end of the tongue-and-groove joint, a 2cm thick foam board is placed to pour new secondary lining concrete. The grade of the new secondary lining concrete is one grade higher than that of the old secondary lining concrete. Alternatively, micro-expansion concrete is used at the end. After the new secondary lining concrete reaches the design strength, clean the inside and both sides of the construction joint.
[0014] Adjust the width of the expansion joint to 17-20mm;
[0015] Use electric pick and cutting machine to expand the trench along the outside of the construction joint. The left and right widths of the trench are controlled at 5 cm in length and 2 to 3 cm in depth for the subsequent installation of the water collection box.
[0016] Use a manual grinder to grind and chamfer the two outer corners of the expansion joint to protect the water-stop rubber strip from being scratched by the outer corners of the expansion joint during the embedding construction.
[0017] The step of forming the second waterproof system includes the following steps:
[0018] Use a wire brush to remove sand and concrete residue from the construction joint surface within the laying range, and then use high-pressure water to wash or high-pressure air to blow clean;
[0019] After the construction joints are treated, the pre-buried grouting pipe is embedded along the construction joints. The inner diameter of the grouting pipe is 8mm, the outer diameter is 20mm, and the inner diameter tolerance is ±0.3mm. The grouting pipe is used for one-time grouting. The grouting pipe is divided into sections every 6 to 8m. Grouting ports and exhaust holes are set at both ends. According to the division of the grouting pipe, a 25mm diameter water-stop rubber strip is selected accordingly.
[0020] Nylon chisels and hammers are used to drive into the repaired deformation joints and close to the pre-buried grouting pipes. The combination of the two forms a second waterproofing system for local drainage of leakage.
[0021] Wherein, the grouting step includes the following steps:
[0022] After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, use a stick to compact it, and apply the interface agent to the sealant and the inner surface of the groove;
[0023] Prepare elastic sealant and apply it with a scraper until it is 2 cm away from the structure surface;
[0024] After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections, and the grouting material is ultra-fine silicate cement;
[0025] Use compressed air or water to test the sealing of the grouting pipe, use low-pressure grouting to fill the pipe with slurry, and when the slurry flows out from one end of the grouting pipe, seal it with a grouting nozzle;
[0026] A certain amount of slurry is injected into the grouting pipe. The flow rate of the grouting liquid can be controlled by the pressure gauge located in front of the grouting nozzle on the pump;
[0027] When the setting time of the grouting material reaches half, fresh slurry is injected until the pressure remains constant. At this point, the joints or pores will no longer accept more slurry, and the grouting can be completed;
[0028] After the slurry reaches a certain strength, cut off the grouting pipe and the exhaust pipe opening, clean them, and seal them with elastic sealant.
[0029] The beneficial effect of the anti-seepage treatment method for the secondary lining structure of a tunnel of the present invention is: the anti-seepage treatment method of the present invention is used to play a role in blocking and diversion, which is convenient for later repair and maintenance, ensures the effective establishment of the waterproof system, and prevents a large amount of water seepage in the tunnel in the later period. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0031] Figure 1 It is a flow chart of the steps of a method for anti-seepage treatment at a secondary lining structure of a tunnel according to the present invention.
[0032] Figure 2 It is a cross-sectional view of treatment measures for a seepage section of a method for anti-seepage treatment at a secondary lining structure of a tunnel according to the present invention.
[0033] Figure 3 It is a partial cross-sectional view of the seepage section treatment measures of a method for anti-seepage treatment at a secondary lining structure of a tunnel according to the present invention.
[0034] Figure 4 It is a schematic diagram of the division of sections of a method for anti-seepage treatment at a secondary lining structure of a tunnel according to the present invention. DETAILED DESCRIPTION
[0035] See also Figures 1 to 4 The present invention provides a method for anti-seepage treatment at a secondary lining structure of a tunnel, comprising the following steps:
[0036] S1: Chisel out the secondary lining slabs with large water discharge along the construction joints, replace the damaged waterproofing boards, and chisel the tongue-and-groove joints in the middle of the secondary lining;
[0037] S2: Place a 2cm thick foam board at the bottom of the tongue-and-groove joint and pour new secondary lining concrete. After the new secondary lining concrete reaches the design strength, clean the inside and both sides of the construction joint, and use a manual grinder to grind and chamfer the two positive corners on the outside of the deformation joint;
[0038] S3: Use a wire brush to remove sand and concrete slag on the construction joint surface within the laying range, then use high-pressure water or high-pressure wind to blow it clean, embed the pre-buried grouting pipe along the construction joint, select a 25mm diameter water-stop rubber strip according to the division of the grouting pipe, and combine them to form a second waterproof system for local drainage of leakage;
[0039] S4: After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, and tamp it with a stick. After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections. The joints or pores will no longer accept more slurry, and the grouting can be completed. After reaching a certain strength, cut off the grouting pipe opening and the exhaust pipe opening, clean them, and seal them with elastic sealant;
[0040] S5: A water receiving box is installed on the outside of the expansion joint. Water-stop rubber pads are placed on both sides of the water receiving box and fixed to the secondary lining of the tunnel with expansion bolts. The outside is sealed with highly elastic wet epoxy resin mortar. The water receiving box is extended to the top of the longitudinal drainage ditch for centralized drainage.
[0041] Furthermore, the height of the tongue-and-groove seam is 10 cm and the depth is 5 cm, and the groove is kept vertical as much as possible to increase the water flow path of the seepage water and reduce the seepage pressure.
[0042] Further, the steps of cleaning both sides of the construction joint include the following steps:
[0043] At the lower end of the tongue-and-groove joint, a 2cm thick foam board is placed to pour new secondary lining concrete. The grade of the new secondary lining concrete is one grade higher than that of the old secondary lining concrete. Alternatively, micro-expansion concrete is used at the end. After the new secondary lining concrete reaches the design strength, clean the inside and both sides of the construction joint.
[0044] Adjust the width of the expansion joint to 17-20mm;
[0045] Use electric pick and cutting machine to expand the trench along the outside of the construction joint. The left and right widths of the trench are controlled at 5 cm in length and 2 to 3 cm in depth for the subsequent installation of the water collection box.
[0046] Use a manual grinder to grind and chamfer the two outer corners of the expansion joint to protect the water-stop rubber strip from being scratched by the outer corners of the expansion joint during the embedding construction.
[0047] Furthermore, the step of forming the second waterproof system includes the following steps:
[0048] Use a wire brush to remove sand and concrete residue from the construction joint surface within the laying range, and then use high-pressure water to wash or high-pressure air to blow clean;
[0049] After the construction joints are treated, the pre-buried grouting pipe is embedded along the construction joints. The inner diameter of the grouting pipe is 8mm, the outer diameter is 20mm, and the inner diameter tolerance is ±0.3mm. The grouting pipe is used for one-time grouting. The grouting pipe is divided into sections every 6 to 8m. Grouting ports and exhaust holes are set at both ends. According to the division of the grouting pipe, a 25mm diameter water-stop rubber strip is selected accordingly.
[0050] Nylon chisels and hammers are used to drive into the repaired deformation joints and close to the pre-buried grouting pipes. The combination of the two forms a second waterproofing system for local drainage of leakage.
[0051] Furthermore, the grouting step includes the following steps:
[0052] After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, use a stick to compact it, and apply the interface agent to the sealant and the inner surface of the groove;
[0053] Prepare elastic sealant and apply it with a scraper until it is 2 cm away from the structure surface;
[0054] After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections, and the grouting material is ultra-fine silicate cement;
[0055] Use compressed air or water to test the sealing of the grouting pipe, use low-pressure grouting to fill the pipe with slurry, and when the slurry flows out from one end of the grouting pipe, seal it with a grouting nozzle;
[0056] A certain amount of slurry is injected into the grouting pipe. The flow rate of the grouting liquid can be controlled by the pressure gauge located in front of the grouting nozzle on the pump;
[0057] When the setting time of the grouting material reaches half, fresh slurry is injected until the pressure remains constant. At this point, the joints or pores will no longer accept more slurry, and the grouting can be completed;
[0058] After the slurry reaches a certain strength, cut off the grouting pipe and the exhaust pipe opening, clean them, and seal them with elastic sealant.
[0059] In this embodiment, the anti-seepage treatment method of the present invention plays a role of blocking and diversion, which is convenient for later repair and maintenance, ensures the effective establishment of the waterproof system, and prevents a large amount of water seepage in the tunnel in the later stage.
[0060] What is disclosed above is only a preferred embodiment of the present invention, and it certainly cannot be used to limit the scope of rights of the present invention. Ordinary technicians in this field can understand that all or part of the processes of the above embodiment and equivalent changes made according to the claims of the present invention still fall within the scope of the invention.
Claims
1. A method for preventing water seepage at the secondary lining structure of a tunnel. It is characterized in that The steps include: Chisel out the secondary lining panels with large water discharge along the construction joints, replace the damaged waterproof panels, and chisel the tongue-and-groove joints in the middle of the secondary lining; Place a 2cm thick foam board at the bottom of the tongue-and-groove joint and pour new secondary lining concrete. After the new secondary lining concrete reaches the designed strength, clean the inside and both sides of the construction joint, and use a manual grinder to grind and chamfer the two positive corners on the outside of the deformation joint; Use a wire brush to remove sand and concrete slag from the construction joint surface within the laying range, then use high-pressure water or high-pressure wind to blow it clean, embed the pre-buried grouting pipe along the construction joint, select a 25mm diameter water-stop rubber strip according to the division of the grouting pipe, and combine them to form a second waterproof system for local drainage of leakage; After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, and tamp it with a stick. After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections. The joints or pores will no longer accept more slurry, and the grouting can be completed. After reaching a certain strength, cut off the grouting pipe opening and the exhaust pipe opening, clean them, and seal them with elastic sealant. A water receiving box is installed on the outside of the expansion joint. Water-stop rubber pads are placed on both sides of the water receiving box and it is fixed to the secondary lining of the tunnel with expansion bolts. The outside is sealed with highly elastic moist epoxy resin mortar. The water receiving box is extended to the top of the longitudinal drainage ditch for centralized drainage.
2. A method for preventing water seepage at a secondary lining structure of a tunnel as claimed in claim 1, It is characterized in that The height of the tongue-and-groove seam is 10 cm and the depth is 5 cm. The groove is kept vertical as much as possible to increase the water flow path of the seepage water and reduce the seepage pressure.
3. A method for preventing water seepage at a secondary lining structure of a tunnel as claimed in claim 1, It is characterized in that The steps for cleaning both sides of the construction joint include the following: At the lower end of the tongue-and-groove joint, a 2cm thick foam board is placed to pour new secondary lining concrete. The grade of the new secondary lining concrete is one grade higher than that of the old secondary lining concrete. Alternatively, micro-expansion concrete is used at the end. After the new secondary lining concrete reaches the design strength, clean the inside and both sides of the construction joint. Adjust the width of the expansion joint to 17-20mm; Use electric pick and cutting machine to expand the trench along the outside of the construction joint. The left and right widths of the trench are controlled at 5 cm in length and 2 to 3 cm in depth for the subsequent installation of the water collection box. Use a manual grinder to grind and chamfer the two outer corners of the expansion joint to protect the water-stop rubber strip from being scratched by the outer corners of the expansion joint during the embedding construction.
4. A method for preventing water seepage at a secondary lining structure of a tunnel as claimed in claim 1, It is characterized in that The steps of forming the second waterproof system include the following steps: Use a wire brush to remove sand and concrete residue from the construction joint surface within the laying range, and then use high-pressure water to wash or high-pressure air to blow clean; After the construction joints are treated, the pre-buried grouting pipe is embedded along the construction joints. The inner diameter of the grouting pipe is 8mm, the outer diameter is 20mm, and the inner diameter tolerance is ±0.3mm. The grouting pipe is used for one-time grouting. The grouting pipe is divided into sections every 6 to 8m. Grouting ports and exhaust holes are set at both ends. According to the division of the grouting pipe, a 25mm diameter water-stop rubber strip is selected accordingly. Nylon chisels and hammers are used to drive into the repaired deformation joints and close to the pre-buried grouting pipes. The combination of the two forms a second waterproofing system for local drainage of leakage.
5. A method for preventing water seepage at a secondary lining structure of a tunnel as claimed in claim 1, It is characterized in that The grouting process includes the following steps: After the waterproof rubber strip is installed, clean the construction joint, fill it with flexible sealant, use a stick to compact it, and apply the interface agent to the sealant and the inner surface of the groove; Prepare elastic sealant and apply it with a scraper until it is 2 cm away from the structure surface; After the newly poured concrete and sealant reach the designed strength, grouting is carried out in sections, and the grouting material is ultra-fine silicate cement; Use compressed air or water to test the sealing of the grouting pipe, use low-pressure grouting to fill the pipe with slurry, and when the slurry flows out from one end of the grouting pipe, seal it with a grouting nozzle; A certain amount of slurry is injected into the grouting pipe. The flow rate of the grouting liquid can be controlled by the pressure gauge located in front of the grouting nozzle on the pump; When the setting time of the grouting material reaches half, fresh slurry is injected until the pressure remains constant. At this point, the joints or pores will no longer accept more slurry, and the grouting can be completed; After the slurry reaches a certain strength, cut off the grouting pipe and the exhaust pipe opening, clean them, and seal them with elastic sealant.