Method of forming source / drain regions

By forming a multi-layered stacked structure in a semiconductor device and performing epitaxial growth, planting and rapid thermal processes, the thermally induced relaxation and performance degradation problems faced by the source/drain region in a semiconductor device are solved, and high density and High performance source/drain region manufacturing.

CN119092466APending Publication Date: 2024-12-06TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410493412.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-08-10
Filing Date
2024-04-23
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

As the minimum feature size of semiconductor devices decreases, the formation of high-density source/drain regions faces problems such as heat-induced relaxation and performance degradation, and the prior art is difficult to effectively solve these problems.

Method used

Improve the source/drain by forming a multi-layered structure on the substrate, including nanostructures and epitaxial growth source/drain regions, and performing a transplanting process and a rapid thermal process to form amorphous phase and recrystallization regions, improving the source/draining electrode by the formation of a multi-layered stacked structure on the substrate, including nanostructures and epitaxial growth source/drain regions, and performing a transplanting process and rapid thermal processes to form an amorphous phase region and a recrystallization region. performance of zone.

Benefits of technology

This method effectively activates dopants, improves device performance, reduces heat-induced relaxation, and improves overall manufacturing simplicity and performance stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092466A_ABST
    Figure CN119092466A_ABST
Patent Text Reader

Abstract

A method of forming a source / drain region includes forming a first nanostructure over a substrate. A second nanostructure is then formed over the first nanostructure. An epitaxially grown first source / drain region is adjacent to the first nanostructure. A second source / drain region is epitaxially grown over the first source / drain region and adjacent to the second nanostructure. An implantation process is performed to implant impurities in the second source / drain region. The implantation process forms an amorphous phase region within the second source / drain region. A rapid thermal process is performed on the second source / drain region that recrystallizes a portion of the amorphous phase region.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a method for forming a source / drain region. Background Art

[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, cell phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor material layers on a semiconductor substrate and patterning the various material layers using photolithography to form circuit components and elements thereon.

[0003] The semiconductor industry continues to increase the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by continuously reducing the minimum feature size, which allows more components to be integrated into a given area. However, as the minimum feature size decreases, other problems arise that need to be solved. Summary of the invention

[0004] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a first nanostructure above a substrate. Then forming a second nanostructure above a plurality of first nanostructures. Epitaxially growing a first source / drain region adjacent to the first nanostructure. Epitaxially growing a second source / drain region above the first source / drain region and adjacent to the second nanostructure. Performing an implantation process to implant impurities in the second source / drain region. The implantation process forms an amorphous phase region in the second source / drain region. Performing at least one rapid thermal process on the second source / drain region. Performing each rapid thermal process to recrystallize a portion of the amorphous phase region.

[0005] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a fin extending from a substrate. The fin includes a lower nanostructure and an upper nanostructure above the lower nanostructure. A lower epitaxial source / drain region is formed on an opposite side of the lower nanostructure. An isolation region is formed on the lower epitaxial source / drain region. An upper epitaxial source / drain region is formed on the isolation region and on an opposite side of the upper nanostructure. An upper region of the upper epitaxial source / drain region is amorphized. A first rapid annealing process is performed to recrystallize a first amorphous portion of an upper region of the upper epitaxial source / drain region. After performing the first rapid annealing process, a second rapid annealing process is performed to recrystallize a remaining amorphous portion of an upper region of the upper epitaxial source / drain region.

[0006] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a multilayer stack over a substrate. Patterning the multilayer stack to form a first channel region and a second channel region over the first channel region. The first channel region and the second channel region include nanostructures. The method includes epitaxially growing a first source / drain region over the substrate. The first channel region extends between the first source / drain regions. The first source / drain region applies stress to the first channel region. The method includes forming a dielectric layer over the first source / drain region. Forming a second source / drain region over the dielectric layer. The second channel region extends between the second source / drain regions. Forming the second source / drain region includes epitaxially growing a crystalline semiconductor material over the dielectric layer. Performing an implantation process that amorphizes a portion of the crystalline semiconductor material to form an amorphous semiconductor material over the crystalline semiconductor material. Performing a rapid thermal process that recrystallizes the amorphous semiconductor material. The method includes forming a first gate structure around the first channel region and a second gate structure around the second channel region. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] When with Figure 1 The disclosure can be best understood from the following detailed description when read together. It should be emphasized that, in accordance with standard practice in the industry, various features are not drawn to scale and are only used for illustration purposes. In fact, the size of various features can be arbitrarily increased or decreased for clarity of discussion.

[0008] Figure 1 An example schematic diagram of a complementary field effect transistor in a three-dimensional view according to some embodiments is shown;

[0009] Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 , Fig. 8A , Figure 8B and Figure 8C is a diagram of an intermediate step in the fabrication of a CFET according to some embodiments;

[0010] Fig.9A , Fig. 9B , Fig. 9C , Fig.9D and Fig.9E depicts an intermediate step in forming epitaxial source / drain regions according to some embodiments;

[0011] Fig.10 , Fig.11 , Fig. 12A , Fig. 12B , Fig. 12C and Fig.13is a diagram of intermediate steps in the fabrication of a CFET according to some embodiments.

[0012]

Explanation of symbols

[0013] 100: Isolation structure

[0014] 108: Source / drain region

[0015] 108L: Lower epitaxial source / drain region

[0016] 108U: epitaxial source / drain region

[0017] 110: doping area

[0018] 111: Amorphous phase

[0019] 112: First CESL

[0020] 114: First ILD

[0021] 116: Implantation process

[0022] 118: Rapid Thermal Process

[0023] 118A: First Rapid Thermal Process

[0024] 118B: Second Rapid Thermal Process

[0025] 118C: The third rapid thermal process

[0026] 122: Second CESL

[0027] 124: Second ILD

[0028] 132: Gate dielectric

[0029] 134: Gate electrode

[0030] 134L: Lower gate electrode

[0031] 134U: Upper gate electrode

[0032] 138: Gate mask

[0033] 142:Metal-Semiconductor Alloy Area

[0034] 144: Upper source / drain contact

[0035] 152:ESL

[0036] 154: Third ILD

[0037] 156: Upper gate contact

[0038] 158: Source / drain vias

[0039] 160: Device layer

[0040] 170: Front side interconnection structure

[0041] 172: Dielectric layer

[0042] 174: Conductive characteristics

[0043] 50:Substrate

[0044] 52:Multi-layer stacking

[0045] 54: Virtual semiconductor layer

[0046] 54A: first virtual semiconductor layer

[0047] 54B: Second virtual semiconductor layer

[0048] 56: Semiconductor layer

[0049] 56L: lower semiconductor layer

[0050] 56U: Upper semiconductor layer

[0051] 62:Semiconductor fins

[0052] 64 / 66: Nanostructure

[0053] 64A: First Virtual Nanostructure

[0054] 64B: Second virtual nanostructure

[0055] 66L: Lower semiconductor nanostructure

[0056] 66M:Medium semiconductor nanostructures

[0057] 66U: Semiconductor Nanostructures

[0058] 66:Semiconductor Nanostructures

[0059] 70: Isolation Area

[0060] 72: Virtual dielectric layer

[0061] 74: Virtual gate layer

[0062] 76: Mask layer

[0063] 82: Virtual Dielectric

[0064] 84: Virtual Gate

[0065] 86:Mask

[0066] 90: Gate spacer

[0067] 92: Fin spacer

[0068] 94: Source / drain groove

[0069] 98:Internal spacer

[0070] A-A', B-B', C-C': cross section DETAILED DESCRIPTION

[0071] The following disclosure provides many different embodiments or examples for implementing different features of the disclosure. In order to simplify the disclosure, specific examples of components and arrangements are described below. Of course, these are just examples and are not meant to be restrictive. For example, in the following description, a first feature formed above or on a second feature may include an embodiment in which the first and second features form direct contact, and may also include an embodiment in which additional features are formed between the first and second features, so that the first and second features may not be in direct contact. In addition, the disclosure may repeat reference numbers and / or symbols in various examples. This repetition is for simplicity and clarity and does not itself specify the relationship between the various embodiments and / or configurations discussed.

[0072] Additionally, for ease of description, spatially relative terms, such as "below," "beneath," "below," "above," "over," and the like, may be used herein to describe the relationship of one element or feature to another element or feature as shown in the figures. Spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be oriented in other orientations (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein may be interpreted accordingly.

[0073] According to various embodiments, a complementary field-effect transistor (CFET) is formed. The CFET includes a lower nanostructure FET and an upper nanostructure FET. The lower source / drain region of the lower nanostructure FET is formed before the upper source / drain region of the upper nanostructure FET is formed. The lower source / drain region and the upper source / drain region can exert pressure on the adjacent channel region to improve performance. The upper source / drain region is formed by implanting dopants to amorphize a portion of the upper source / drain region, followed by recrystallizing the amorphized portion through a rapid thermal process (also referred to as rapid thermal annealing). Forming the upper source / drain region in this manner allows the dopants in the upper source / drain region to be activated while maintaining the lower source / drain region below a relaxation temperature. Activating the dopants in the upper source / drain region by the techniques described herein can improve device performance without causing thermally-induced relaxation of the lower source / drain region that can reduce device performance. Therefore, device performance and ease of fabrication of a complete CFET can be improved.

[0074] Figure 1 An example schematic diagram of a stacked transistor, such as a complementary field effect transistor (CFET), is shown according to some embodiments. Figure 1 It is a three-dimensional view, and some features of the CFET are omitted for clarity.

[0075] The CFET includes a plurality of vertically stacked nanostructure FETs (e.g., nanoFETs, nanowire FETs, nanosheet FETs, multiple bridge channel (MBC) FETs, nanoribbon FETs, gate-all-around (GAA) FETs, or the like). For example, the CFET may include a lower nanostructure FET of a first device type (e.g., n-type / p-type) and an upper nanostructure FET of a second device type (e.g., p-type / n-type) opposite to the first device type. Specifically, in some embodiments, the CFET may include a lower PMOS (p-type metal oxide semiconductor) transistor and an upper NMOS (n-type metal oxide semiconductor) transistor. In other embodiments, the CFET may include a lower NMOS transistor and an upper PMOS transistor. Each nanostructure FET includes a semiconductor nanostructure 66 (labeled as a lower semiconductor nanostructure 66L and an upper semiconductor nanostructure 66U), wherein the semiconductor nanostructure 66 serves as a channel region of the nanostructure FET. The semiconductor nanostructure 66 may be a nanosheet, a nanowire, or the like. The lower semiconductor nanostructure 66L is for the lower nanostructure FET. The upper semiconductor nanostructure 66U is used for the upper nanostructure FET. Figure 1 ) The upper semiconductor nanostructure 66U is separated and electrically isolated from the lower semiconductor nanostructure 66L.

[0076] The gate dielectric 132 is along the top surface, sidewalls and bottom surface of the semiconductor nanostructure 66. The gate electrode 134 (including the lower gate electrode 134L and the upper gate electrode 134U) is above the gate dielectric 132 and around the semiconductor nanostructure 66. The source / drain region 108 (labeled as the lower epitaxial source / drain region 108L and the upper epitaxial source / drain region 108U) is set on the opposite side of the gate dielectric 132 and the gate electrode 134. Depending on the context, the source / drain region 108 can be referred to as a source or a drain individually or collectively. Isolation features can be formed to separate the desired source / drain regions 108 and / or the desired gate electrodes 134. For example, the isolation layer (not explicitly shown) can be selectively formed. Figure 1 Alternatively, the lower gate electrode 134L may be coupled to the upper gate electrode 134U. In addition, one or more dielectric layers (not explicitly shown) may be used to separate the lower gate electrode 134L from the upper gate electrode 134U. Figure 1) separates the upper epitaxial source / drain region 108U from the lower epitaxial source / drain region 108L. The isolation features between the channel region, gate, and source / drain regions allow vertical stacking of transistors, thereby improving device density. Because of the nature of vertically stacked FETs, this schematic may also be referred to as a stacked transistor or a folded transistor.

[0077] Figure 1 Reference cross sections for subsequent figures are further depicted. Cross section AA' is parallel to the longitudinal axis of the semiconductor nanostructure 66 of the CFET and is along, for example, the direction of the current flow between the source / drain regions 108 of the CFET. Cross section BB' is perpendicular to cross section AA' and is along the longitudinal axis of the gate electrode 134 of the CFET. Cross section CC' is parallel to cross section BB' and extends through the source / drain regions 108 of the CFET. For clarity, subsequent figures refer to these reference cross sections.

[0078] Figures 2 to 13 Diagram of intermediate steps in the fabrication of a CFET, according to some embodiments. Figure 2 , Figure 3 and Figure 4 Shown with Figure 1 A 3D view similar to a 3D view of . Figure 7 , Fig. 8A , Fig.9A , Fig. 9B , Fig. 9C , Fig.9D , Fig.9E , Fig.10 , Fig.11 , Fig. 12A and Fig.13 Draw along with Figure 1 A cross-sectional view of a cross section similar to reference cross section AA'. Figure 8B and Fig. 12B Draw along with Figure 1 Cross-sectional view of a cross-section similar to reference cross-section BB'. Figure 8C and Fig. 12C Draw along with Figure 1 Cross-sectional view of a cross section similar to reference cross section CC'.

[0079] exist Figure 2In the invention, a substrate 50 is provided. The substrate 50 may be a semiconductor substrate, such as a bulk semiconductor, a semiconductor on insulator (SOI) substrate, or the like. It may be doped (e.g., with a p-type or n-type dopant) or undoped. The substrate 50 may be a wafer, such as a silicon wafer. Typically, an SOI substrate is a semiconductor material layer formed on an insulator layer. The insulator layer may be, for example, a buried oxide (BOX) layer, a silicon oxide layer, or the like. An insulator layer is provided on a substrate, typically a silicon or glass substrate. Other substrates, such as multilayer or gradient substrates, may also be used. In some embodiments, the semiconductor material of the substrate 50 may include silicon, germanium, a compound semiconductor, an alloy semiconductor, or a combination thereof. Compound semiconductors include carbon-doped silicon, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide. The alloy semiconductor includes silicon germanium, gallium arsenide phosphide, aluminum indium arsenide, aluminum gallium arsenide, gallium indium arsenide, gallium indium phosphide and / or gallium arsenide phosphide or a combination thereof. For example, substrate 50 may be a multi-layer substrate including a semiconductor material layer formed on a silicon germanium layer, wherein the silicon germanium layer is provided on a substrate core, typically a silicon or glass substrate.

[0080] A multilayer stack 52 is formed on a substrate 50. The multilayer stack 52 includes alternating virtual semiconductor layers 54 (including a first virtual semiconductor layer 54A and a second virtual semiconductor layer 54B) and semiconductor layers 56 (including a lower semiconductor layer 56L and an upper semiconductor layer 56U). A subset of the lower semiconductor layer 56L and the first virtual semiconductor layer 54A is disposed below the second virtual semiconductor layer 54B. The upper semiconductor layer 56U and another subset of the first virtual semiconductor layer 54A are disposed above the second virtual semiconductor layer 54B. As described in more detail below, the virtual semiconductor layer 54 will be removed and the semiconductor layer 56 will be patterned to form a channel region of the CFET. Specifically, the lower semiconductor layer 56L will be patterned to form a channel region of the lower nanostructure FET of the CFET. The upper semiconductor layer 56U will be patterned to form a channel region of the upper nanostructure FET of the CFET.

[0081] The multilayer stack 52 is illustrated as including six virtual semiconductor layers 54 and six semiconductor layers 56. It should be understood that the multilayer stack 52 may include any number of virtual semiconductor layers 54 and semiconductor layers 56. Each of the multilayer stacks 52 may be grown by a process such as vapor phase epitaxy (VPE) or molecular beam epitaxy (MBE). Each of the multilayer stacks 52 may be deposited by a process such as chemical vapor deposition (CVD) or atomic layer deposition (ALD) or the like.

[0082] The first virtual semiconductor layer 54A is formed of a first semiconductor material, and the second virtual semiconductor layer 54B is formed of a second semiconductor material. The first and second semiconductor materials can be selected from candidate semiconductor materials of the substrate 50. The first and second semiconductor materials have high etching selectivity to each other. As a result, in subsequent processes, the material of the second virtual semiconductor layer 54B can be removed at a faster rate than the material of the first virtual semiconductor layer 54A. In some embodiments, the first virtual semiconductor layer 54A is formed of silicon germanium with a low germanium concentration (for example, a germanium concentration in the range of about 10% to about 40%). The second virtual semiconductor layer 54B is formed of silicon germanium with a high germanium concentration (for example, a germanium concentration in the range of about 40% to about 50%).

[0083] The semiconductor layer 56 (including the lower semiconductor layer 56L and the upper semiconductor layer 56U) is formed of one or more semiconductor materials. The semiconductor material can be selected from the candidate semiconductor materials of the substrate 50. The lower semiconductor layer 56L and the upper semiconductor layer 56U can be formed of the same semiconductor material or can be formed of different semiconductor materials. In some embodiments, both the lower semiconductor layer 56L and the upper semiconductor layer 56U are formed of semiconductor materials suitable for p-type devices and n-type devices, such as silicon. In some embodiments, the lower semiconductor layer 56L is formed of a semiconductor material suitable for p-type devices, such as germanium or silicon germanium. The upper semiconductor layer 56U is formed of a semiconductor material suitable for n-type devices, such as silicon or carbon-doped silicon. The semiconductor material of the semiconductor layer 56 will be described in more detail below. The semiconductor material of the semiconductor layer 56 has a high etching selectivity compared to the semiconductor material of the virtual semiconductor layer 54. As a result, in subsequent processes, the material of the virtual semiconductor layer 54 can be removed at a faster rate than the material of the semiconductor layer 56. In some embodiments, semiconductor layer 56 is formed of silicon, which may be undoped or lightly doped at this stage of the process. Other materials, combinations of materials, or compositions of materials are possible.

[0084] Some layers of the multilayer stack 52 may be thicker than other layers of the multilayer stack 52. The thickness of the second virtual semiconductor layer 54B may be different from (e.g., greater than or less than) the thickness of each first virtual semiconductor layer 54A. Additionally, the thickness of each semiconductor layer 56 may be different from (e.g., greater than or less than) the thickness of each virtual semiconductor layer 54.

[0085] exist Figure 3 , semiconductor fins 62 are formed in substrate 50. Nanostructures 64 / 66 (including first dummy nanostructures 64A, second dummy nanostructures 64B, lower semiconductor nanostructures 66L, middle semiconductor nanostructures 66M, and upper semiconductor nanostructures 66U) are formed in multilayer stack 52. In some embodiments, nanostructures 64 / 66 and semiconductor fins 62 may be formed in multilayer stack 52 and substrate 50, respectively, by etching trenches in multilayer stack 52 and substrate 50. Etching may be any acceptable etching process, such as reactive ion etching (RIE), neutral beam etching (NBE), the like, or a combination thereof. Etching may be anisotropic. The formation of nanostructures 64 / 66 by etching the multilayer stack 52 may define a first virtual nanostructure 64A in the first virtual semiconductor layer 54A, a second virtual nanostructure 64B in the second virtual semiconductor layer 54B, a lower semiconductor nanostructure 66L in some lower semiconductor layers 56L, an upper semiconductor nanostructure 66U in some upper semiconductor layers 56U, and a middle semiconductor nanostructure 66M in some lower semiconductor layers 56L and some upper semiconductor layers 56U. The first virtual nanostructure 64A and the second virtual nanostructure 64B may be collectively referred to as virtual nanostructures 64. The lower semiconductor nanostructure 66L, the middle semiconductor nanostructure 66M, and the upper semiconductor nanostructure 66U may be collectively referred to as semiconductor nanostructures 66.

[0086] As described in more detail below, the lower semiconductor nanostructure 66L will serve as the channel region of the lower nanostructure FET for the CFET. The upper semiconductor nanostructure 66U will serve as the channel region of the upper nanostructure FET for the CFET. The middle semiconductor nanostructure 66M is a semiconductor nanostructure 66 directly (e.g., in contact) above / below the second virtual nanostructure 64B. Depending on the height of the subsequently formed source / drain regions, the middle semiconductor nanostructure 66M may or may not be combined with any source / drain region and may or may not serve as a functional channel region of the CFET. In addition, in some embodiments, the second virtual nanostructure 64B may be subsequently replaced with an isolation structure. In other embodiments, at least a portion of the second virtual nanostructure 64B may remain in the complete CFET. The isolation structure and the middle semiconductor nanostructure 66M may define the boundaries of the lower nanostructure FET and the upper nanostructure FET.

[0087] The semiconductor fins 62 and nanostructures 64 / 66 may be patterned by any suitable method. For example, the semiconductor fins 62 and nanostructures 64 / 66 may be patterned by one or more photolithography processes, including double patterning or multi-patterning processes. Typically, the double patterning or multi-patterning process combines photolithography and a self-aligned process so that the formed pattern has, for example, a smaller spacing relative to the spacing obtained by a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed above the substrate and the sacrificial layer is patterned by a photolithography process. Spacers are formed next to the patterned sacrificial layer by a self-aligned process, and then the sacrificial layer is removed, and the remaining spacers can then be used to pattern the semiconductor fins 62 and nanostructures 64 / 66. In some embodiments, a mask (or other layer) may remain on the nanostructure 64 / 66.

[0088] Although each semiconductor fin 62 and nanostructure 64 / 66 is illustrated as having a constant width throughout, in other embodiments, the semiconductor fin 62 and / or nanostructure 64 / 66 may have different widths or non-constant widths. For example, in some embodiments, the semiconductor fin 62 and / or nanostructure 64 / 66 may have tapered sidewalls such that the width of each semiconductor fin 62 and / or nanostructure 64 / 66 increases continuously in a direction toward the substrate 50. In such embodiments, each nanostructure 64 / 66 may have different widths and be trapezoidal in shape. Other sidewall shapes or profiles are possible.

[0089] In addition, an isolation region 70 is formed above the substrate 50 and between adjacent semiconductor fins 62. In some embodiments, the isolation region 70 may include a liner and a filling material above the liner. Each liner and filling material may include a dielectric material, such as an oxide (e.g., silicon oxide), a nitride (e.g., silicon nitride), the like, or a combination thereof. The formation of the isolation region 70 may include depositing the dielectric material and performing a planarization process, such as a chemical mechanical polishing (CMP) process, a mechanical polishing process, or the like, to remove excess portions of the dielectric material, such as portions above the nanostructures 64 / 66. The deposition process may include ALD, high-density plasma chemical vapor deposition (HDP-CVD), flowable CVD (FCVD), the like, or a combination thereof. In some embodiments, the isolation region 70 includes silicon oxide formed by an FCVD process followed by an annealing process. The dielectric material is then recessed to define the isolation region 70. The dielectric material may then be recessed such that upper portions of semiconductor fins 62 and nanostructures 64 / 66 extend above isolation regions 70 .

[0090] The aforementioned process is only one example of how to form semiconductor fins 62 and nanostructures 64 / 66. In some embodiments, semiconductor fins 62 and / or nanostructures 64 / 66 may be formed by masking and epitaxial growth processes. For example, a dielectric layer may be formed above the top surface of substrate 50. A groove may be etched through the dielectric layer to expose the substrate 50 thereunder. An epitaxial structure may be epitaxially grown in the groove. The dielectric layer may be recessed so that the epitaxial structure protrudes from the dielectric layer to form semiconductor fins 62 and / or nanostructures 64 / 66. The epitaxial structure may include the aforementioned semiconductor material. In some embodiments of epitaxially grown epitaxial structures, the epitaxially grown material may be in situ doped during growth, which may omit previous and / or subsequent implantation, but in situ doping and implantation doping may also be used together.

[0091] In addition, appropriate well regions (not separately shown) may be formed in the semiconductor nanostructures 66 and / or the semiconductor fins 62. For example, n-type impurity implantation and / or p-type impurity implantation may be performed, or the semiconductor material may be in-situ doped during growth. The n-type impurity may be phosphorus, arsenic, antimony, or the like, with a concentration of 10 17 atoms / cm 3 Up to 10 19 atoms / cm 3 The p-type impurity may be boron, boron fluoride, indium or the like, with a concentration of 1017 atoms / cm 3 Up to 10 19 atoms / cm 3 The well region in the lower semiconductor nanostructure 66L and the semiconductor fin 62 has a conductivity type opposite to that of a lower source / drain region that will be formed adjacent to the lower semiconductor nanostructure 66L later. The well region of the upper semiconductor nanostructure 66U has a conductivity type opposite to that of an upper source / drain region that will be formed adjacent to the upper semiconductor nanostructure 66U later.

[0092] exist Figure 4 In the embodiment of the present invention, a dummy dielectric layer 72 is formed on the semiconductor fin 62 and / or on the nanostructure 64 / 66. The dummy dielectric layer 72 may be, for example, silicon oxide, silicon nitride, a combination thereof, or the like. The dummy dielectric layer 72 may be deposited or thermally grown according to an acceptable technique. A dummy gate layer 74 is formed over the dummy dielectric layer 72. A mask layer 76 is formed over the dummy gate layer 74. The dummy gate layer 74 may be deposited over the dummy dielectric layer 72 and then planarized, for example, by CMP. The mask layer 76 may be deposited over the dummy gate layer 74. The dummy gate layer 74 may be a conductive or non-conductive material. It may be selected from the group consisting of amorphous silicon, polycrystalline silicon (poly-silicon), polycrystalline silicon germanium (poly-SiGe), metal nitrides, metal silicides, metal oxides, and metals. The dummy gate layer 74 may be deposited by physical vapor deposition (PVD), CVD, sputtering deposition, or other techniques for depositing the selected material. The dummy gate layer 74 may be formed of other materials having high etch selectivity compared to etching of the isolation region. The mask layer 76 may include, for example, silicon nitride, silicon oxynitride, or the like. In the illustrated embodiment, the dummy dielectric layer 72 covers the isolation region 70 such that the dummy dielectric layer 72 extends between the dummy gate layer 74 and the isolation region 70. In another embodiment, the dummy dielectric layer 72 only covers the semiconductor fins 62 and / or the nanostructures 64 / 66.

[0093] exist Figure 5 In the embodiment of the present invention, the mask layer 76 can be patterned by acceptable photolithography and etching techniques to form a mask 86. The pattern of the mask 86 can then be transferred to the dummy gate layer 74 and the dummy dielectric layer 72 to form a dummy gate 84 and a dummy dielectric 82, respectively. The dummy gate 84 covers the corresponding channel area of ​​the nanostructure 64 / 66. Each dummy gate 84 can be physically separated from an adjacent dummy gate 84 by the pattern of the mask 86. The dummy gate 84 can also have a length direction that is substantially perpendicular to the length direction of the corresponding semiconductor fin 62. The mask 86 can be selectively removed after patterning, for example by any acceptable etching technique.

[0094] exist Figure 6 In the process, a gate spacer 90 is formed above the nanostructure 64 / 66 and on the sidewalls of the exposed mask 86 (if present), the dummy gate 84, and the dummy dielectric 82. The gate spacer 90 can be formed by conformally forming one or more dielectric materials and then etching the dielectric material. Acceptable dielectric materials may include silicon oxide, silicon nitride, silicon oxynitride, silicon nitride carbon oxide, or the like. The dielectric material may be formed by a deposition process such as chemical vapor deposition (CVD), atomic layer deposition (ALD), or the like. Other dielectric materials that can be formed by any acceptable process may be used. Any acceptable etching process, such as dry etching, wet etching, the like, or a combination thereof, may be performed to pattern the dielectric material. The etching may be anisotropic. When the dielectric material is etched, a portion remains on the sidewalls of the dummy gate 84 (thereby forming the gate spacer 90). The dielectric material will be described in more detail below. When the dielectric material is etched, a portion may also remain on the sidewalls of the semiconductor fin 62 and / or the nanostructure 64 / 66 (thereby forming the fin spacer 92, see Figure 8C ).

[0095] In addition, implantation of lightly doped source / drain (LDD) regions (not shown separately) may be performed. LDD implantation may be performed before forming gate spacers 90. Appropriate types of impurities may be implanted in nanostructures 64 / 66 to a desired depth. The LDD region may have the same conductivity type as the source / drain region of the subsequently formed adjacent lower semiconductor nanostructure 66L. Additionally, the LDD region in the lower semiconductor nanostructure 66L may have a conductivity type opposite to the conductivity type of the LDD region in the upper semiconductor nanostructure 66U. In some embodiments, the lower semiconductor nanostructure 66L has a p-type LDD region and the upper semiconductor nanostructure 66U has an n-type LDD region. In some embodiments, the lower semiconductor nanostructure 66L has an n-type LDD region and the upper semiconductor nanostructure 66U has a p-type LDD region. The n-type impurity may be any of the aforementioned n-type impurities, and the p-type impurity may be any of the aforementioned p-type impurities. The lightly doped source / drain region may have a conductivity type between 10 17 atoms / cm 3 Up to 10 20 atoms / cm 3 Annealing can be used to restore implant damage and to activate implanted impurities. In some embodiments, the growing material of the nanostructure 64 / 66 can be in-situ doped during growth, and implantation can be omitted, but in-situ doping and implantation doping can also be used together.

[0096] It should be noted that the foregoing generally describes the process of forming spacers and LDD regions. Other processes and sequences may be used. For example, fewer or additional spacers may be used, a different sequence of steps may be used, additional spacers may be formed and removed, and / or the like.

[0097] Source / drain recesses 94 are formed in the semiconductor fins 62, the nanostructures 64 / 66, and the substrate 50. Epitaxial source / drain regions are then formed in the source / drain recesses 94. The source / drain recesses 94 may extend through the nanostructures 64 / 66 and into the substrate 50. The semiconductor fins 62 may be etched such that the bottom surface of the source / drain recesses 94 is disposed above, below, or flush with the top surface of the isolation region 70. In the illustrated example, the top surface of the isolation region 70 is above the bottom surface of the source / drain recesses 94. The semiconductor fins 62, the nanostructures 64 / 66, and the substrate 50 may be etched by an anisotropic etching process, such as RIE, NBE, or the like, to form the source / drain recesses 94. During the etching process for forming the source / drain recesses 94, portions of the semiconductor fins 62, the nanostructures 64 / 66, and the substrate 50 are masked with the gate spacers 90 and the dummy gates 84 to form the source / drain recesses 94. A single etching process or multiple etching processes may be used to etch each layer of the nanostructures 64 / 66 and / or the semiconductor fins 62. After the source / drain recesses 94 reach a desired depth, the etching of the source / drain recesses 94 may be stopped using a timed etching process.

[0098] exist Figure 7 In the embodiment of the present invention, an inner spacer 98 is formed on the sidewalls of the remaining portion of the first virtual nanostructure 64A. As described in more detail below, a source / drain region is subsequently formed in the source / drain groove 94, and the first virtual nanostructure 64A is replaced with a corresponding gate structure. The inner spacer 98 serves as an isolation feature between the subsequently formed source / drain region and the subsequently formed gate structure. In addition, the inner spacer 98 can be used to prevent subsequent etching processes, such as etching processes for forming a gate structure, from damaging the subsequently formed source / drain region. In addition, the second virtual nanostructure 64B is replaced with an isolation structure 100 between the middle semiconductor nanostructures 66M. The isolation structure 100 and the middle semiconductor nanostructure 66M define the boundaries of the lower nanostructure FET and the upper nanostructure FET. The isolation structure 100 can have similar dimensions to the replaced second virtual nanostructure 64B.

[0099] As an example, the inner spacer 98 and the isolation structure 100 are formed, and the sidewalls of the first virtual nanostructure 64A exposed by the source / drain groove 94 are recessed to form a sidewall groove. In addition, the second virtual nanostructure 64B is removed to form an opening between the middle semiconductor nanostructures 66M, for example, between the lower semiconductor nanostructure 66L (commonly) and the upper semiconductor nanostructure 66U (commonly). The sidewalls of the first virtual nanostructure 64A can be recessed to form the sidewall grooves with any acceptable etching process. The first virtual nanostructure 64A is selectively etched (for example, the material of the first virtual nanostructure 64A is selectively etched at a faster rate relative to the material of the semiconductor nanostructure 66). The etching can be isotropic. Although the sidewalls of the first virtual nanostructure 64A are shown as straight, after etching, the sidewalls can be concave (concave) or convex (convex). The second virtual nanostructure 64B can be removed with any acceptable etching process to form an opening between the middle semiconductor nanostructures 66M. The second dummy nanostructure 64B is selectively etched (e.g., the material of the second dummy nanostructure 64B is selectively etched at a faster rate relative to the material of the semiconductor nanostructure 66). The etching may be isotropic. After forming the openings between the middle semiconductor nanostructures 66M, the dummy gate 84 may adhere to and support the upper semiconductor nanostructure 66U so that the upper semiconductor nanostructure 66U does not fall over. The middle semiconductor nanostructure 66M is exposed through the opening. In some embodiments, the etching process thins the middle semiconductor nanostructure 66M. Therefore, the thickness of the middle semiconductor nanostructure 66M may be different from (e.g., less than) the thickness of the lower semiconductor nanostructure 66L and the thickness of the upper semiconductor nanostructure 66U.

[0100] In some embodiments, the same etching process is used to recess the sidewall of the first virtual nanostructure 64A and remove the second virtual nanostructure 64B. For example, the second virtual nanostructure 64B may be completely removed without completely removing the first virtual nanostructure 64A. The first virtual nanostructure 64A may be recessed without significantly recessing the semiconductor nanostructure 66. The etching process has selectivity between the materials of the first virtual nanostructure 64A, the second virtual nanostructure 64B, and the semiconductor nanostructure 66. Specifically, the etching process selectively etches the material of the first virtual nanostructure 64A at a faster rate than the material of the semiconductor nanostructure 66, and selectively etches the material of the second virtual nanostructure 64B at a faster rate than the material of the first virtual nanostructure 64A. Therefore, the etching rate of the first virtual nanostructure 64A is lower than the etching rate of the second virtual nanostructure 64B, and greater than the etching rate of the semiconductor nanostructure 66.

[0101] An insulating material is then conformally formed in the source / drain recesses 94, the sidewall recesses, and the openings between the middle semiconductor nanostructures 66M. Etching is then performed. The insulating material may be a carbon-containing dielectric material, such as silicon oxycarbon nitride, silicon oxycarbon, silicon oxynitride, or the like. Other low-k materials having a dielectric constant less than about 3.5 may be used. The insulating material may be formed by a deposition process, such as ALD, CVD, or the like. The etching of the insulating material may be anisotropic. For example, the etching process may be a dry etch such as RIE, NBE, or the like. The insulating material is etched with a remaining portion in the sidewall recesses (thereby forming the inner spacer 98) and a remaining portion in the openings between the middle semiconductor nanostructures 66M (thereby forming the isolation structure 100).

[0102] Although the outer sidewalls of the inner spacers 98 and isolation structures 100 are depicted as being immediately adjacent to the sidewalls of the semiconductor nanostructures 66, the outer sidewalls of the inner spacers 98 and isolation structures 100 may extend beyond or be recessed from the sidewalls of the semiconductor nanostructures 66. Thus, the inner spacers 98 and isolation structures 100 may partially fill, completely fill, or overfill the sidewall recesses and openings between the semiconductor nanostructures 6624. Furthermore, although the sidewalls of the inner spacers 98 and isolation structures 100 are depicted as straight lines, those sidewalls may be concave or convex.

[0103] Next, a lower epitaxial source / drain region 108L is formed in the lower portion of the source / drain recess 94. The lower epitaxial source / drain region 108L only partially fills the source / drain recess 94, so that the lower epitaxial source / drain region 108L contacts the lower semiconductor nanostructure 66L but does not contact the upper semiconductor nanostructure 66U. The lower epitaxial source / drain region 108L is formed in the source / drain recess 94 so that each stack of lower semiconductor nanostructures 66L is disposed between a corresponding adjacent pair of lower epitaxial source / drain regions 108L. In some embodiments, the lower epitaxial source / drain region 108L is separated from the first dummy nanostructure 64A by an inner spacer 98 at an appropriate lateral distance so that the lower epitaxial source / drain region 108L does not short-circuit a subsequently formed gate of the resulting device. The lower epitaxial source / drain region 108L includes one or more semiconductor material layers epitaxially grown in the lower portion of the source / drain recess 94. The lower epitaxial source / drain regions 108L have a conductivity type suitable for the device type of the lower nanostructure FET. In some embodiments, the lower epitaxial source / drain regions 108L apply stress to the corresponding channel region of the lower semiconductor nanostructure 66L to improve performance.

[0104] In some embodiments, the lower nanostructure FET is p-type (e.g., a PMOS transistor) and the lower epitaxial source / drain region 108L is a p-type source / drain region. For example, the p-type lower epitaxial source / drain region 108L may include, for example, silicon germanium, boron-doped silicon germanium, boron-doped silicon, germanium, germanium tin, or a similar material. In some embodiments, the p-type lower epitaxial source / drain region 108L may include a material that applies compressive stress to the lower semiconductor nanostructure 66L, which may include one or more of these example materials. In some embodiments, materials like these may be used with the lower semiconductor nanostructure 66L including silicon germanium. In other embodiments, the lower nanostructure FET is n-type and / or the lower epitaxial source / drain region 108L is an n-type source / drain region. The lower epitaxial source / drain region 108L may have a surface that is raised from the corresponding upper surface of the lower semiconductor nanostructure 66L and may have a facet. Other materials or combinations of materials are possible.

[0105] The epitaxial source / drain region 108L may be implanted with a dopant to form a source / drain region, similar to the process of forming a lightly doped source / drain region described above, followed by annealing. The source / drain region may have an impurity concentration of 10 19 atoms / cm 3 Up to 10 21 atoms / cm 3 The n-type and / or p-type impurities used for the source / drain regions may be any of the impurities described above. In some embodiments, the lower epitaxial source / drain regions 108L are in-situ doped during growth.

[0106] As a result of the epitaxial process for forming lower epitaxial source / drain region 108L, the upper surface of lower epitaxial source / drain region 108L has facets that extend laterally outward beyond the sidewalls of nanostructures 64 / 66. Figure 8C As shown, after the epitaxy process is completed, adjacent lower epitaxial source / drain regions 108L remain separated. In other embodiments, these facets allow adjacent lower epitaxial source / drain regions 108L of the same nanostructure FET to merge (not shown separately). In some embodiments, fin spacers 92 are formed (see Figure 8C ) on the top surface of the isolation region 70, thereby preventing epitaxial growth. In some other embodiments, the fin spacer 92 may cover a portion of the sidewalls of the nanostructures 64 / 66 and / or the semiconductor fin 62, further preventing epitaxial growth. In another embodiment, the spacer etch used to form the gate spacer 90 may be adjusted so that the fin spacer 92 is not formed, so that the lower epitaxial source / drain region 108L extends to the surface of the isolation region 70.

[0107] Next, a first ILD 114 (interlayer dielectric, ILD) is formed over the lower epitaxial source / drain region 108L. The first ILD 114 may be formed of a dielectric material, which may be deposited by any suitable method, such as CVD, plasma enhanced PVD (PECVD), or FCVD. The dielectric material may include phospho-silicate glass (PSG), boro-silicate glass (BSG), boron-doped phospho-silicate glass (BPSG), undoped silicate glass (USG), or the like. Other insulating materials formed by any acceptable process may be used.

[0108] In some embodiments, a first CESL 112 (contact etch stoplayer, CESL) is formed between the first ILD 114 and the lower epitaxial source / drain region 108L. The first CESL 112 may be formed of a dielectric material having a high etching selectivity compared to the first ILD 114, such as silicon nitride, silicon oxide, silicon oxynitride, or the like, and may be formed by any suitable deposition process, such as CVD, ALD, or the like.

[0109] The first CESL 112 and / or the first ILD 114 may be formed by depositing a material for the first CESL 112 and depositing a material for the first ILD 114, followed by an etch-back process. In some embodiments, the first ILD 114 is first etched so that the first CESL 112 is not etched. An anisotropic etching process is then performed to remove a portion of the first CESL 112 that is higher than the first ILD 114. After the recess, the sidewalls of the upper semiconductor nanostructure 66U are exposed.

[0110] exist FIG. 8A to FIG. 8C , and then forming an upper epitaxial source / drain region 108U in the upper portion of the source / drain recess 94. In some embodiments, the upper epitaxial source / drain region 108U is formed by epitaxially growing a source / drain material, implanting dopants in the source / drain material, and then performing a rapid thermal process to recrystallize the source / drain material and activate the implanted dopants. The process will be described in more detail below. The upper epitaxial source / drain region 108U only partially fills the source / drain recess 94, so that the upper epitaxial source / drain region 108U contacts the upper semiconductor nanostructure 66U, but does not contact the lower semiconductor nanostructure 66L.

[0111] The source / drain recess 94 includes an upper epitaxial source / drain region 108U, a first ILD 114, a first CESL 112, and a lower epitaxial source / drain region 108L. The first ILD 114 and the first CESL 112 are between the upper epitaxial source / drain region 108U and the lower epitaxial source / drain region 108L. The lower epitaxial source / drain region 108L is used for the lower nanostructure FET of the CFET. The upper epitaxial source / drain region 108U is used for the upper nanostructure FET of the CFET. The first ILD 114 and the first CESL 112 provide isolation between the upper epitaxial source / drain region 108U and the lower epitaxial source / drain region 108L to avoid short circuits between the lower nanostructure FET and the upper nanostructure FET.

[0112] The upper epitaxial source / drain regions 108U are formed in the source / drain recesses 94 such that each stack of the upper semiconductor nanostructures 66U is disposed between a corresponding adjacent pair of upper epitaxial source / drain regions 108U. In some embodiments, the upper epitaxial source / drain regions 108U and the first dummy nanostructure 64A are separated by inner spacers 98 at an appropriate lateral distance such that the upper epitaxial source / drain regions 108U do not short-circuit a subsequently formed gate of the resulting device.

[0113] Epitaxially grown upper epitaxial source / drain regions 108U are grown in upper portions of source / drain recesses 94. For example, upper epitaxial source / drain regions 108U may be grown laterally from the sidewalls of the exposed upper semiconductor nanostructures 66U. As a result of the epitaxial process used to form the upper epitaxial source / drain regions 108U, the upper surface of the upper epitaxial source / drain regions 108U has facets that extend laterally outward beyond the sidewalls of the nanostructures 64 / 66. In some embodiments, adjacent upper epitaxial source / drain regions 108U remain separated after the epitaxial process is completed. In other embodiments, as the upper epitaxial source / drain regions 108U grow in the source / drain recesses 94, these facets cause adjacent upper epitaxial source / drain regions 108U of the same nanostructure FET to merge (not shown separately). The upper epitaxial source / drain regions 108U may have surfaces that are raised from the corresponding upper surfaces of the upper semiconductor nanostructures 66U. The upper epitaxial source / drain regions 108U may include one or more semiconductor material layers.

[0114] The upper epitaxial source / drain region 108U has a conductivity type suitable for the device type of the upper nanostructure FET. The conductivity type of the upper epitaxial source / drain region 108U can be opposite to the conductivity type of the lower epitaxial source / drain region 108L. In other words, the upper epitaxial source / drain region 108U can be oppositely doped relative to the lower epitaxial source / drain region 108L. For example, in an embodiment where the lower epitaxial source / drain region 108L is p-type, the upper epitaxial source / drain region 108U can be n-type. In some embodiments, the upper epitaxial source / drain region 108U applies stress to the corresponding channel region of the upper semiconductor nanostructure 66U, thereby improving performance.

[0115] In some embodiments, the upper nanostructure FET is n-type (e.g., an NMOS transistor), and the upper epitaxial source / drain region 108U is an n-type source / drain region. For example, the upper epitaxial source / drain region 108U may include, for example, silicon, carbon-doped silicon, phosphorus-doped and carbon-doped silicon, silicon phosphide, silicon arsenide, or similar materials. The upper epitaxial source / drain region 108U may be implanted with a dopant to form a source / drain region, which will be described in more detail below. In some embodiments, the upper epitaxial source / drain region 108U is doped in situ during growth.

[0116] In some embodiments, the n-type upper epitaxial source / drain region 108U may include a material that applies tensile stress to the upper semiconductor nanostructure 66U, which may include one or more of these example materials. In some embodiments, these materials may be used with an upper semiconductor nanostructure 66U that includes silicon. In other embodiments, the upper epitaxial source / drain region 108U is a p-type source / drain region and / or the lower epitaxial source / drain region 108L is an n-type source / drain region.

[0117] In some embodiments, dopants are doped into the epitaxial material by an amorphization implantation process, followed by a rapid thermal process to recrystallize the epitaxial material and activate the implanted dopants to dope the upper epitaxial source / drain region 108U. Forming the upper epitaxial source / drain region 108U in this manner allows doping and activation of dopants within the upper epitaxial source / drain region 108U without subjecting the lower epitaxial source / drain region 108L or the upper epitaxial source / drain region 108U to thermal conditions that cause stress relaxation and thereby degrade device performance. Activating dopants within the upper epitaxial source / drain region 108U can reduce the overall resistance and contact resistance of the upper epitaxial source / drain region 108U, thereby improving device performance.

[0118] As a schematic example, 9A to 9E An example of intermediate steps of a doping and doping activation process of epitaxial source / drain regions 108U is depicted according to some embodiments. 9A to 9EA cross-sectional view of a portion of the epitaxial source / drain region 108U is shown, which may be similar to that shown in FIG. FIG. 8A to FIG. 8C The epitaxial source / drain region 108U is formed, for example, 9A to 9E The upper epitaxial source / drain regions 108U in may be n-type source / drain regions formed of doped silicon, although other materials are possible.

[0119] Fig.9A The upper epitaxial source / drain regions 108U are shown prior to dopant implantation according to some embodiments. The upper epitaxial source / drain regions 108U may be epitaxially grown from the material described above, such as silicon or another material. Fig.9A The epitaxial source / drain regions 108U may be undoped or may be in-situ doped during growth. Fig.9A The upper epitaxial source / drain region 108U may be substantially crystalline.

[0120] exist Fig. 9B In some embodiments, an amorphization implantation process 116 is performed on the epitaxial source / drain region 108U. The amorphization implantation process 116 implants dopants (e.g., impurities, ions, or the like) into the epitaxial source / drain region 108U and at least partially amorphizes the epitaxial source / drain region 108U. Fig. 9B As shown, the amorphization implantation process 116 amorphizes the crystalline material of the epitaxial source / drain region 108U into an amorphous (or relatively amorphous) material, and forms an amorphous phase region 111 in the epitaxial source / drain region 108U. In some cases, because the amorphization implantation process 116 is performed before the epitaxial source / drain region 108U is amorphized, the amorphization implantation process 116 can be regarded as a "pre-amorphous phase implantation". In addition, the amorphization implantation process 116 implants dopants into the epitaxial source / drain region 108U to form a doped region 110, and the doped region 110 can be at least partially in the amorphous phase region 111. Fig. 9B The amorphous phase region 111 and the doped region 110 shown are illustrative examples. The amorphous phase region 111 and / or the doped region 110 may have different locations, sizes or depths within the epitaxial source / drain region 108U. Additionally, the boundaries of the amorphous phase region 111 and the doped region 110 shown are distinct (e.g., abrupt), but in some cases, the boundaries of these regions may be gradual (e.g., gradient). As described herein, amorphizing the epitaxial source / drain region 108U by an amorphization implantation process 116 allows a subsequently performed rapid thermal process 118 to activate dopants while recrystallizing the amorphous phase material, which will be described in more detail below.

[0121] In some embodiments, the parameters of the amorphization implantation process 116 are controlled to implant dopants in a manner that amorphizes the crystalline phase material of the epitaxial source / drain region 108U to form the amorphous phase region 111. For example, in some cases, a lower implantation process temperature may promote amorphization of the target material. Therefore, in some embodiments, the amorphization implantation process 116 may be performed using a low process temperature (e.g., a process temperature in the range of about -100°C to about 28°C), but other temperatures are also possible. In some embodiments, the amorphization implantation process 116 may have an implantation energy in the range of about 1 keV to about 8 keV, but other energies are also possible. In some embodiments, the amorphization implantation process 116 may be performed at about 2×10 15 atoms / cm 2 About 1.4×10 16 atoms / cm 2 The dopant is implanted at an energy in the range of about 2×10 15 atoms / cm 2 About 1.4×10 16 atoms / cm 2 Dopants are implanted at doses in a range of , but other doses are possible.

[0122] In some embodiments, the initial amorphous phase region 111 may have a depth D0 from the top surface of the epitaxial source / drain region 108U, and the depth D0 is in the range of about 5 nanometers to about 15 nanometers. The depth D0 may be between about 10% and about 30% of the total height (e.g., top surface to bottom surface) of the epitaxial source / drain region 108U. But other depths are possible. Below the amorphous phase region 111, the material of the epitaxial source / drain region 108U is substantially crystalline. The transition from the substantially amorphous phase material of the amorphous phase region 111 to the substantially crystalline phase material below it may be steep, irregular or gradual. In some cases, the depth D0 can be measured from the top surface of the epitaxial source / drain region 108U to a depth at which the epitaxial source / drain region 108U is substantially crystalline. In some cases, the depth D0 can be measured from the top surface of the epitaxial source / drain region 108U to a depth where about half of the epitaxial source / drain region 108U is crystalline material and about half is amorphous phase material. In some embodiments, the depth D0 of the amorphous phase region 111 can be controlled by controlling the parameters (e.g., temperature or energy) of the amorphization implantation process 116.

[0123] The amorphization implantation process 116 may implant suitable n-type and / or p-type impurities for the source / drain regions, which may be any of the impurities described above. As an example, for embodiments where the epitaxial source / drain regions 108U are n-type, the implanted impurities may include arsenic, phosphorus, diphosphorus (e.g., P2), or the like. In some cases, implanting relatively large elements such as arsenic or diphosphorus may promote amorphization, especially at relatively low process temperatures. Other impurities are possible.

[0124] In this way, the amorphization implantation process 116 forms the doped region 110 in the epitaxial source / drain region 108U. The doped region 110 may be completely in the amorphous phase region 111, such as Fig. 9B As shown, in other cases, the doped region 110 may extend into the crystalline region of the epitaxial source / drain region 108U. The doped region 110 may have a thickness of about 10 19 atoms / cm 3 to about 10 21 atoms / cm 3 The dopant concentration of the doped region 110 may be within a range of 100, but other concentrations are possible. By controlling the parameters of the amorphization implantation process 116, such as temperature, energy, dosage, or the like, the location, depth, height, boundary, or concentration profile of the doped region 110 may be controlled. The boundary of the doped region 110 may be steep, irregular, or gradual. For example, the dopant concentration profile of the doped region 110 adjacent the boundary may be stepped or gradient. Thus, in some cases, a non-zero concentration of the implanted impurity may exist at the doped region 110. FIG. 9B to FIG. 9E The exemplary doped region 110 is shown outside the region. In some cases, the upper boundary of the doped region 110 can be the top surface of the upper epitaxial source / drain region 108U.

[0125] According to some embodiments, after the amorphization implantation process 116 is formed, one or more rapid thermal processes 118 may be performed. The rapid thermal process 118 is an annealing process or other heating process that heats the structure for a short duration, and will be described in more detail below. Fig. 9C In the process, a first rapid thermal process 118A is performed. Fig.9D In the process, a second rapid thermal process 118B is performed. Fig.9E, a third rapid thermal process 118C is performed. In other embodiments, more or fewer rapid thermal processes 118 may be performed. Multiple rapid thermal processes 118 are performed to recrystallize the amorphous phase region 111 into a crystalline phase material doped with implanted impurities of the doping region 110. For example, impurities may be doped at the lattice sites of the crystalline phase material. In this way, the implanted impurities in the upper epitaxial source / drain region 108U may be "activated", which may improve device performance. In some cases, the rapid thermal process 118 also reduces or eliminates implantation damage to the upper epitaxial source / drain region 108U. In some cases, the use of the rapid thermal process 118 as described herein allows activation of dopants in the upper epitaxial source / drain region 108U while reducing stress relaxation of the lower epitaxial source / drain region 108L and / or the upper epitaxial source / drain region 108U, as will be described in more detail below.

[0126] In some embodiments, the rapid thermal process 118 heats the structure for a short duration, for example, a duration in the range of about 1 millisecond to about 10 milliseconds. In some embodiments, the duration of the rapid thermal process 118 heating the structure may be less than about 5 milliseconds. The duration may be longer or shorter than these examples. In other embodiments. The rapid thermal process 118 may include a heating temperature in the range of about 800°C to about 1250°C, but other temperatures are possible. In some embodiments, the rapid thermal process 118 may heat the structure to a temperature in the range of about 800°C to about 1250°C, but other temperatures are possible. In some embodiments, the rapid thermal process 118 may heat the structure to a temperature below about 1250°C. In some cases, the short duration of the rapid thermal process 118 subjects the structure to lower temperatures and / or less thermal stress, which may reduce epitaxial material relaxation (described in more detail below). For embodiments in which multiple rapid thermal processes 118 are performed, each rapid thermal process 118 may have similar parameters or different parameters (e.g., temperature, duration, ramp-up or ramp-down rate, or the like). For embodiments that perform multiple rapid thermal processes 118, each rapid thermal process 118 may be performed as a separate process. For example, in some embodiments, the structure may be partially or completely cooled before performing a subsequent rapid thermal process 118. The rapid thermal process 118 may be performed by rapid thermal anneal (RTA), laser annealing, or the like.

[0127] In some embodiments, each rapid thermal process 118 causes the lower region of the amorphous material of the amorphous region 111 to recrystallize into a crystalline material. The recrystallization of the amorphous region 111 may be a solid-state epitaxial regrowth process that is "seed" by the crystalline material below it. For example, the transition between the portion of the amorphous region 111 adjacent to the amorphous region 111 and the crystalline region below it may be recrystallized. Therefore, the transition between the amorphous material and the crystalline material moves toward the top surface of the upper epitaxial source / drain region 108U. In other words, the rapid thermal process 118 increases the relative height of the crystalline region and decreases the relative height of the amorphous region 111 above it. This FIG. 9B to FIG. 9E , as each rapid thermal process (first rapid thermal process 118A, second rapid thermal process 118B, third rapid thermal process 118C) is sequentially performed, the depth of the amorphous phase region 111 is reduced from the initial depth D0, which will be described in more detail below. In some embodiments, during a single rapid thermal process 118, the thickness of the portion of the amorphous phase region 111 that is recrystallized may be in the range of about 5 nanometers to about 15 nanometers, but other sizes of the recrystallized amorphous phase region 111 are possible. The thickness of the amorphous phase region 111 that is recrystallized during the rapid thermal process 118 can be controlled by controlling the parameters of the rapid thermal process 118, such as temperature or duration. In some cases, the rapid thermal process 118 can change the concentration profile or boundary of the doping region 110.

[0128] exist Fig. 9C In some embodiments, a first rapid thermal process 118A is performed on the epitaxial source / drain region 108U. Fig. 9C As shown in FIG. 1 , the first rapid thermal process 118A recrystallizes a portion of the amorphous phase region 111, so that the depth of the amorphous phase region 111 is reduced from an initial depth D0 to a smaller depth D1. The difference between D0 and D1 (e.g., D0-D1) corresponds to the thickness of the region recrystallized by the first rapid thermal process 118A. Fig. 9C 1, after the first rapid thermal process 118A is performed, the bottom boundary of the amorphous phase region 111 is above the bottom boundary of the doped region 110. However, in other embodiments, after the first rapid thermal process 118A is performed, the doped region 110 may still be within the amorphous phase region 111. In other embodiments, the first rapid thermal process 118A recrystallizes a larger or smaller portion of the amorphous phase region 111. In other embodiments, the first rapid thermal process 118A recrystallizes all of the amorphous phase region 111.

[0129] exist Fig.9D In some embodiments, a second rapid thermal process 118B is performed on the epitaxial source / drain region 108U. The second rapid thermal process 118B may have similar or different parameters than the first rapid thermal process 118A. Fig.9DAs shown, the second rapid thermal process 118B recrystallizes a portion of the amorphous phase region 111 so that the depth of the amorphous phase region 111 is reduced from a depth D1 to a smaller depth D2. The difference between D1 and D2 (e.g., D1-D2) corresponds to the thickness of the region recrystallized by the second rapid thermal process 118B. In other embodiments, the second rapid thermal process 118B recrystallizes a larger or smaller portion of the amorphous phase region 111. In other embodiments, the second rapid thermal process 118B recrystallizes all of the remaining amorphous phase region 111.

[0130] exist Fig.9E In some embodiments, a third rapid thermal process 118C is performed on the epitaxial source / drain region 108U. The third rapid thermal process 118C may have parameters similar to or different from those of the first rapid thermal process 118A and / or the second rapid thermal process 118B. Fig.9E As shown, the third rapid thermal process 118C recrystallizes the remaining portion of the amorphous phase region 111, so that the epitaxial source / drain region 108U becomes completely or substantially crystalline. The depth D2 corresponds to the thickness of the region recrystallized by the third rapid thermal process 118C. In other embodiments, the third rapid thermal process 118C does not completely recrystallize the remaining amorphous phase region 111. 9A to 9E Three rapid thermal processes 118 are shown to be performed to recrystallize the amorphous phase region 111 , but more or fewer rapid thermal processes 118 may be performed in other embodiments.

[0131] As described herein, recrystallizing the doped amorphous phase material to form the source / drain region can reduce the thermal stress experienced by the structure and improve device performance. In some cases, heating the structure to a sufficient temperature to thermally activate the implanted dopants in the crystalline phase material can cause relaxation of the stressed epitaxial material. For example, a sufficiently high temperature can cause the epitaxial source / drain material to relax, thereby applying channel pressure, which can reduce device performance. In this way, the manufacturing process can have a "thermal budget", which can be determined at least in part by avoiding temperatures high enough to cause relaxation of the epitaxial material. By recrystallizing the upper epitaxial source / drain region 108U through a rapid thermal process 118 as described herein, the dopants in the upper epitaxial source / drain region 108U can be activated by a relatively low temperature, thereby reducing the risk of causing relaxation in the lower epitaxial source / drain region 108L and / or in the upper epitaxial source / drain region 108U. In other words, the technology described herein can activate dopants with little or no epitaxial relaxation. This can improve device performance while avoiding thermal process conditions that can degrade device performance. This can also allow for greater process flexibility in subsequent thermal processes.

[0132] exist Fig.10In the embodiment of the present invention, a second ILD 124 is deposited over the epitaxial source / drain region 108U. The second ILD 124 may be formed of a dielectric material, which may be deposited by any suitable method, such as chemical vapor deposition (CVD), plasma assisted chemical vapor deposition (PECVD), or FCVD. The dielectric material may include phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), or the like. Other dielectric materials formed by any acceptable process may be used.

[0133] The second CESL 122 may be formed between the second ILD 124 and the upper epitaxial source / drain region 108U. The second CESL 122 may be formed of a dielectric material having a high etch selectivity compared to the dielectric material of the second ILD 124, such as silicon nitride, silicon oxide, silicon oxynitride, or the like, which may be formed by any suitable deposition process, such as CVD, ALD, or the like.

[0134] The second CESL 122 and / or the second ILD 124 may be formed by depositing a material for the second CESL 122 and depositing a material for the second ILD 124. A removal process is then performed until the top surface of the second ILD 124 is flush with the top surface of the gate spacer 90 and the mask 86 (if present) or the dummy gate 84. In some embodiments, a planarization process such as chemical mechanical polishing (CMP), an etch-back process, or a combination thereof, or the like may be used. The planarization process may also remove the dummy gate 84 on the mask 86 and a portion of the gate spacer 90 along the sidewall of the mask 86. After the planarization process, the top surfaces of the second ILD 124, the gate spacer 90, and the mask 86 (if present) or the dummy gate 84 are substantially coplanar (within process variations). Accordingly, the top surface of the mask 86 (if present) or the dummy gate 84 is exposed through the second ILD 124. In the embodiment shown, the mask 86 is retained after the removal process. In other embodiments, the mask 86 is removed such that the top surface of the dummy gate 84 is exposed through the second ILD 124 .

[0135] exist Fig.11In one or more etching steps, the dummy gate 84 is removed to form a groove between the gate spacers 90. The portion of the dummy dielectric located in the groove is also removed. In some embodiments, the dummy gate 84 and the dummy dielectric 82 are removed by an anisotropic dry etching process. For example, the etching process may include a dry etching process using a reactive gas that selectively etches the material of the dummy gate 84 at a faster rate than the material of the second ILD 124, the isolation structure 100, the inner spacer 98, and the gate spacer 90. Each groove between the gate spacers 90 exposes and / or covers a portion of the semiconductor nanostructure 66 that is a channel region of the resulting device. The portion of the semiconductor nanostructure 66 that is a channel region is disposed between a pair of adjacent lower epitaxial source / drain regions 108L or between a pair of adjacent upper epitaxial source / drain regions 108U. During the removal, the dummy dielectric 82 may serve as an etch stop layer for etching the dummy gate 84. The dummy dielectric 82 may then be removed after the dummy gate 84 is removed.

[0136] The remaining portion of the first dummy nanostructure 64A is then removed to form an opening in the area between the semiconductor nanostructures 66. The remaining portion of the first dummy nanostructure 64A may be removed by any acceptable etching process, wherein the reaction gas selectively etches the material of the first dummy nanostructure 64A at a faster rate than the material of the semiconductor nanostructure 66, the inner spacer 98, and the isolation structure 100. The etching may be isotropic. For example, when the first dummy nanostructure 64A is formed of silicon germanium, the semiconductor nanostructure 66 is formed of silicon, the inner spacer 98 is formed of silicon oxycarbon, and the isolation structure 100 is formed of silicon oxycarbon. The etching process may be a wet etch using tetramethyl ammonium hydroxide (TMAH), ammonium hydroxide (NH4OH), or the like. In some embodiments, a trimming process (not separately depicted) is performed to reduce the thickness of the exposed portion of the semiconductor nanostructure 66 and expand the opening between the semiconductor nanostructures 66.

[0137] Next, a gate dielectric 132 and a gate electrode 134 (including a lower gate electrode 134L and an upper gate electrode 134U) are formed to replace the gate. Each pair of gate dielectrics 132 and gate electrodes 134 (including an upper gate electrode 134U and / or a lower gate electrode 134L) may be collectively referred to as a "gate structure". Each gate structure extends along at least three sides (e.g., top surface, sidewall, and bottom surface) of the channel region of the semiconductor nanostructure 66. The gate structure may also extend along the sidewalls and / or top surface of the channel region of the semiconductor fin 62.

[0138] The gate dielectric 132 includes one or more gate dielectric layers disposed around the lower semiconductor nanostructure 66L, the upper semiconductor nanostructure 66U, and the isolation structure 100. Specifically, the gate dielectric 132 is disposed on the sidewalls and / or top surface of the semiconductor fin 62, on the top surface and on the top surface, sidewalls, and bottom surface of the semiconductor nanostructure 66, on the sidewalls of the inner spacer 98, and on the sidewalls of the gate spacer 90. The gate dielectric 132 surrounds at least three sides of the semiconductor nanostructure 66. The gate dielectric 132 may be formed of an oxide such as silicon oxide or a metal oxide, a silicate such as a metal silicate, a combination thereof, a multilayer thereof, or the like. Alternatively or additionally, the gate dielectric 132 may be formed of a high-k dielectric material (e.g., a dielectric material having a dielectric constant greater than about 7.0), such as a metal oxide or a silicate of hafnium, aluminum, zirconium, lanthanum, manganese, barium, titanium, lead, and a combination thereof. The gate dielectric 132 of dielectric material may be formed by molecular-beam deposition (MBD), ALD, PECVD, or the like. Although a single layer of gate dielectric 132 is shown, the gate dielectric 132 may include any number of interfacial layers and any number of bulk layers. For example, the gate dielectric 132 may include an interfacial layer and a high-k dielectric layer thereover.

[0139] The lower gate electrode 134L includes one or more gate electrode layers disposed above the gate dielectric 132 and around the lower semiconductor nanostructure 66L. The lower gate electrode 134L is disposed in the lower portion of the recess between the gate spacers 90 and in the opening between the lower semiconductor nanostructures 66L. The lower gate electrode 134L may be formed of a material such as tungsten, titanium, titanium nitride, tantalum, tantalum nitride, tantalum carbide, aluminum, ruthenium, cobalt, combinations thereof, multiple layers thereof, or similar metal-containing materials. Although illustrated as a single-layer gate electrode, the lower gate electrode 134L may include any number of work function tuning layers, any number of barrier layers, any number of glue layers, and filler materials.

[0140] The lower gate electrode 134L is formed of a material suitable for the device type of the lower nanostructure FET. For example, the lower gate electrode 134L may include one or more work function adjustment layers suitable for the device type of the lower nanostructure FET. In some embodiments, the lower gate electrode 134L includes an n-type work function adjustment layer, which may be formed of an n-type work function adjustment metal, such as titanium aluminum, titanium aluminum carbide, aluminum tantalum, tantalum carbide, or a combination thereof or the like. In some embodiments, the lower gate electrode 134L includes a p-type work function adjustment layer, which may be formed of a p-type work function adjustment metal, such as titanium nitride, tantalum nitride, or a combination thereof or the like. Alternatively or additionally, the lower gate electrode 134L may include a dipole-inducing element suitable for the device type of the lower nanostructure FET. Acceptable dipole-inducing elements include lanthanum, aluminum, scandium, ruthenium, zirconium, erbium, magnesium, strontium, and combinations thereof.

[0141] The upper gate electrode 134U includes one or more gate electrode layers disposed above the gate dielectric 132 and around the upper semiconductor nanostructure 66U. The upper gate electrode 134U is disposed in the upper portion of the recess between the gate spacers 90 and in the opening between the upper semiconductor nanostructures 66U. The upper gate electrode 134U may be formed of a material such as tungsten, titanium, titanium nitride, tantalum, tantalum nitride, tantalum carbide, aluminum, ruthenium, cobalt, combinations thereof, multiple layers thereof, or similar metal-containing materials. Although illustrated as a single-layer gate electrode, the upper gate electrode 134U may include any number of work function adjustment layers, any number of barrier layers, any number of glue layers, and filler materials.

[0142] The upper gate electrode 134U is formed of a material suitable for the device type of the upper nanostructure FET. For example, the upper gate electrode 134U may include one or more work function adjustment layers of a work function adjustment metal suitable for the device type of the upper nanostructure FET. In some embodiments, the upper gate electrode 134U includes an n-type work function adjustment layer, which may be formed of an n-type work function adjustment metal, such as titanium aluminum, titanium aluminum carbide, aluminum tantalum, tantalum carbide, or a combination thereof or the like. In some embodiments, the upper gate electrode 134U includes a p-type work function adjustment layer, which may be formed of a p-type work function adjustment metal, such as titanium nitride, tantalum nitride, or a combination thereof or the like. The work function adjustment metal of the upper gate electrode 134U may be different from the work function adjustment metal of the lower gate electrode 134L. Alternatively or additionally, the upper gate electrode 134U may include a dipole-inducing element suitable for the device type of the upper nanostructure FET. Acceptable dipole-inducing elements include lanthanum, aluminum, scandium, ruthenium, zirconium, erbium, magnesium, strontium, and combinations thereof. The dipole-inducing element of the upper gate electrode 134U may be different from the dipole-inducing element of the lower gate electrode 134L.

[0143] In some embodiments, an isolation layer (not separately shown) is formed between the lower gate electrode 134L and the upper gate electrode 134U. The isolation layer serves as an isolation feature between the lower gate electrode 134L and the upper gate electrode 134U. The isolation layer may be formed of a dielectric material. Acceptable dielectric materials may include silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbon nitride, or a combination thereof or the like. The dielectric material may be formed by a deposition process such as chemical vapor deposition (CVD), atomic layer deposition (ALD), or the like. The dielectric material may be formed by any other acceptable process. In an embodiment in which the isolation layer is formed, the isolation layer and the isolation structure 100 together isolate the upper gate electrode 134U from the lower gate electrode 134L. Therefore, the upper nanostructure FET may be isolated from the lower nanostructure FET by the combination of the isolation structure 100 and the isolation layer. In some embodiments in which the isolation layer is omitted, the upper nanostructure FET may be coupled to the lower nanostructure FET. When the isolation layer is omitted, the lower gate electrode 134L may be physically and electrically coupled to the upper gate electrode 134U.

[0144] A removal process is performed to remove excess portions of the upper gate electrode layer, which are on the top surfaces of the gate spacers 90 and the second ILD 1242, so that the upper gate electrode layer remains in the openings between the upper semiconductor nanostructures 66U. In some embodiments, a planarization process such as chemical mechanical polishing (CMP), an etch-back process, a combination thereof, or the like may be used. After the removal process, the gate dielectric layer has portions remaining in the recesses between the gate spacers 90 and in the openings between the semiconductor nanostructures 66 (thereby forming the gate dielectric 132). After the removal process, the lower gate electrode layer has portions remaining in the lower portions of the recesses between the gate spacers 90 and in the openings between the lower semiconductor nanostructures 66L (thereby forming the lower gate electrode 134L). After the removal process, the upper gate electrode layer has portions remaining in the upper portions of the recesses between the gate spacers 90 and in the openings between the upper semiconductor nanostructures 66U (thereby forming the upper gate electrode 134U). When a planarization process is used, the top surfaces of the gate spacer 90 , the second ILD 124 , the gate dielectric 132 , and the upper gate electrode 134U are coplanar (within process variations) after the planarization process.

[0145] In some embodiments, a gate mask 138 is formed over the gate structure (including the gate dielectric 132 and the gate electrode 134). The gate mask 138 may also (or may not) be formed over the gate spacer 90. A gate contact may then be formed through the gate mask 138 to contact the top surface of the upper gate electrode 134U. As an example of forming the gate mask 138, the gate structure may be recessed by any acceptable etching process. In some embodiments (not separately shown), the gate spacer 90 is also recessed. One or more dielectric materials are then conformally deposited in the recess. A dielectric material may also be deposited on the top surface of the second ILD 124 and the gate spacer 90. Acceptable dielectric materials may include silicon nitride, silicon carbonitride, silicon oxynitride, silicon carbonitride, or the like, which may be formed by a conformal deposition process such as chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma assisted atomic layer deposition (PEALD), or the like. Any other dielectric material formed by an acceptable process may be used. A removal process is performed to remove excess portions of the dielectric material that are above the top surfaces of the second ILD 124 and the gate spacer 90, thereby forming the gate mask 138. In some embodiments, a planarization process such as chemical mechanical polishing (CMP), an etch-back process, or a combination thereof, or the like, may be used. When planarized, the dielectric material has a portion remaining in the recess (thereby forming the gate mask 138). After the planarization process, the top surfaces of the gate spacer 90, the second ILD 124, and the gate mask 138 are substantially coplanar (within process variations).

[0146] exist FIG. 12A to FIG. 12C, an upper source / drain contact 144 for the source / drain region 108 is formed. The upper source / drain contact 144 may be physically and electrically coupled to the upper epitaxial source / drain region 108U. As an example of forming the upper source / drain contact 144, an opening for forming the upper source / drain contact 144 passes through the second ILD 124 and the second CESL 122. The opening may be formed by acceptable photolithography and etching techniques. In the illustrated embodiment, the opening is formed by a self-aligned contact (SAC) process. A liner (not separately shown) such as a diffusion barrier layer, an adhesive layer or the like and a conductive material are formed in the opening. The liner may include titanium, titanium nitride, tantalum, tantalum nitride or the like. The conductive material may be cobalt, tungsten, copper, a copper alloy, silver, gold, aluminum, nickel or the like. A removal process may be performed to remove excess material from the top surface of the gate spacer 90 and the second ILD 124. The remaining liner and conductive material form upper source / drain contacts 144 in the openings. In some embodiments, a planarization process such as chemical mechanical polishing (CMP), an etch-back process, or a combination thereof, or the like is used. After the planarization process, the top surfaces of the gate spacer 90, the second ILD 124, the gate mask 138, and the upper source / drain contacts 144 are substantially coplanar (within process variations).

[0147] Optionally, a metal semiconductor alloy region 142 is formed at the interface between the upper epitaxial source / drain region 108U and the upper source / drain contact 144. The metal semiconductor alloy region 142 may be a silicide region formed of a metal silicide (e.g., titanium silicide, cobalt silicide, nickel silicide, or the like), a germanide region formed of a metal germanide (e.g., titanium germanide, cobalt germanide, nickel germanide, etc.), a silicon germanide region formed of both a metal silicide and a metal germanide, etc. The metal semiconductor alloy region 142 may be formed before forming the material of the upper source / drain contact 144 by depositing a metal in the opening of the upper source / drain contact 144 and then performing a thermal annealing process. The metal may be any metal that can react with the semiconductor material (e.g., silicon, silicon, germanium, germanium, etc.) of the upper epitaxial source / drain region 108U to form a low-resistance metal semiconductor alloy, such as nickel, cobalt, titanium, tantalum, platinum, tungsten, other noble metals, other refractory metals, rare earth metals, or alloys thereof. The metal may be deposited by a deposition process such as ALD, CVD, PVD, etc. After the thermal annealing process, a cleaning process such as a wet clean may be performed to remove any residual metal from the opening of the upper source / drain contact 144 (e.g., from the surface of the metal semiconductor alloy region 142). The material of the upper source / drain contact 144 may then be formed on the metal semiconductor alloy region 142.

[0148] In the illustrated embodiment, the upper source / drain contacts 144 are coupled to the upper epitaxial source / drain region 108U. In another embodiment (not separately illustrated), some of the upper source / drain contacts 144 are shared source / drain contacts that are coupled to the upper epitaxial source / drain region 108U and the lower epitaxial source / drain region 108L. For example, a shared source / drain contact may be formed through the upper epitaxial source / drain region 108U, the first ILD 114, and the first CESL 112 to couple to the lower epitaxial source / drain region 108L. When forming such a shared source / drain contact, an opening for the shared source / drain contact may also be formed through the upper epitaxial source / drain region 108U, the first ILD 114, and the first CESL 112. Additionally, a metal semiconductor alloy region 142 may be formed on the sidewalls of the upper epitaxial source / drain region 108U.

[0149] In addition, FIG. 12A to FIG. 12C In the embodiment, the third ILD 154 is deposited over the gate spacer 90, the second ILD 124, the gate mask 138, and the upper source / drain contacts 144. In some embodiments, the third ILD 154 is a flowable film formed by a flow CVD method and then cured. In some embodiments, the third ILD 154 is formed of a dielectric material such as PSG, BSG, BPSG, USG, or the like, which can be deposited by any suitable method such as CVD, PECVD, or the like.

[0150] In some embodiments, an ESL 152 (etch stop layer, ESL) is formed between the third ILD 154, the gate spacer 90, the second ILD 124, the gate mask 138, and the upper source / drain contacts 144. The ESL 152 may include a dielectric material having a high etching selectivity compared to the dielectric material of the third ILD 154, such as silicon nitride, silicon oxide, silicon oxynitride, or the like.

[0151] An upper gate contact 156 and an upper source / drain via 158 are formed through the third ILD 154 to contact the upper gate electrode 134U and the upper source / drain contact 144, respectively. An upper gate contact 156 is also formed through the gate mask 138 (if present). The upper gate contact 156 can be physically and electrically coupled to the upper gate electrode 134U. The upper source / drain via 158 can be physically and electrically coupled to the upper source / drain contact 144.

[0152] As an example of forming an upper gate contact 156 and an upper source / drain via 158, an opening for forming an upper gate contact 156 and an upper source / drain via 158 passes through the third ILD 154 and the ESL 152. The opening can be formed by acceptable photolithography and etching techniques. A liner (not shown separately) and a conductive material are formed in the opening. The liner is, for example, a diffusion barrier layer, an adhesive layer, or the like. The liner may include titanium, titanium nitride, tantalum, tantalum nitride, or the like. The conductive material may be cobalt, tungsten, copper, a copper alloy, silver, gold, aluminum, nickel, or the like. A planarization process, such as CMP, may be performed to remove excess material from the top surface of the third ILD 154. The remaining liner and conductive material form an upper gate contact 156 and an upper source / drain via 158 in the opening. The upper gate contact 156 and the upper source / drain via 158 may be formed by different processes or may be formed by the same process. Although shown as being formed in the same cross-section, it should be understood that each upper gate contact 156 and upper source / drain via 158 may be formed in different cross-sections, which may avoid shorting of the contacts.

[0153] The depicted active devices are collectively referred to as device layer 160. In some embodiments, contacts to lower gate electrode 134L and / or lower epitaxial source / drain regions 108L can be formed through the back side of device layer 160 (eg, opposite side of upper source / drain contacts 144).

[0154] exist Fig.13 In the embodiment of the present invention, a front side interconnect structure 170 is formed on the device layer 160, for example, above the third ILD 154. The front side interconnect structure 170 is called a front side interconnect structure because it is formed on the front side of the device layer 160 (for example, the side on which the device is formed on the substrate 50). The front side interconnect structure 170 includes a dielectric layer 172 and a layer of conductive features 174 in the dielectric layer 172. The dielectric layer 172 can be formed of a suitable dielectric material, such as silicon oxide or the like. The conductive features 174 can include conductive lines and vias. The conductive vias can extend through the corresponding dielectric layer 172 to provide vertical connections between the conductive line layers. The conductive features 174 can be formed by a suitable process, such as a damascene process or the like. The front side interconnect structure 170 includes any desired number of layers of conductive features 174. Conductive features 174 connect to the features of the device below (eg, upper gate electrode 134U and upper epitaxial source / drain regions 108U) through upper gate contacts 156 and source / drain vias 158 to form a functional circuit. In other words, conductive features 174 interconnect the upper nanostructure FETs of device layer 160.

[0155] Embodiments can achieve advantages. The technology described herein allows activation of dopants in the upper epitaxial source / drain region of a CFET without adversely affecting the performance of the lower epitaxial source / drain region. As described herein, by forming an amorphous phase doped portion of the upper source / drain and then performing a rapid thermal process to recrystallize the amorphous phase doped portion to form the upper epitaxial source / drain region, the dopants in the amorphous phase doped portion are allowed to be activated while reducing the risk of stress relaxation in the lower epitaxial source / drain region. In some cases, the rapid nature of the rapid thermal process used to recrystallize the amorphous phase doped portion may not sufficiently heat the lower epitaxial source / drain region to cause relaxation. The technology described herein can therefore improve the doping and dopant activation of the upper epitaxial source / drain region, which can improve device performance.

[0156] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a first nanostructure above a substrate. Then forming a second nanostructure above a plurality of first nanostructures. Epitaxially growing a first source / drain region adjacent to the first nanostructure. Epitaxially growing a second source / drain region above the first source / drain region and adjacent to the second nanostructure. Performing an implantation process to implant impurities in the second source / drain region. The implantation process forms an amorphous phase region in the second source / drain region. Performing at least one rapid thermal process on the second source / drain region. Performing each rapid thermal process to recrystallize a portion of the amorphous phase region.

[0157] In some embodiments, the first source / drain region is p-type and the second source / drain region is n-type. In some embodiments, the impurities include arsenic or diphosphorus. In some embodiments, after performing at least one rapid thermal process, the first source / drain region applies compressive stress to the first nanostructure. In some embodiments, each rapid thermal process heats the second source / drain region to a temperature below 1250°C. In some embodiments, the duration of each rapid thermal process heating the second source / drain region is less than 10 milliseconds. In some embodiments, performing at least one rapid thermal process completely recrystallizes the amorphous phase region. In some embodiments, the implantation process forms an amorphous phase region extending from the top surface of the second source / drain region to a depth between 5 nanometers and 15 nanometers.

[0158] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a fin extending from a substrate. The fin includes a lower nanostructure and an upper nanostructure above the lower nanostructure. A lower epitaxial source / drain region is formed on an opposite side of the lower nanostructure. An isolation region is formed on the lower epitaxial source / drain region. An upper epitaxial source / drain region is formed on the isolation region and on an opposite side of the upper nanostructure. An upper region of the upper epitaxial source / drain region is amorphized. A first rapid annealing process is performed to recrystallize a first amorphous portion of an upper region of the upper epitaxial source / drain region. After performing the first rapid annealing process, a second rapid annealing process is performed to recrystallize the remaining amorphous portion of the upper region of the upper epitaxial source / drain region.

[0159] In some embodiments, amorphizing the upper region of the epitaxial source / drain region includes implanting dopants in the epitaxial source / drain region. In some embodiments, the dopant includes an n-type dopant. In some embodiments, the first rapid annealing process activates the dopant within the first amorphous portion of the upper region of the epitaxial source / drain region. In some embodiments, after performing the first rapid annealing process, a third rapid annealing process is performed to recrystallize the second amorphous portion of the upper region of the epitaxial source / drain region. The second amorphous portion is above the first amorphous portion. In some embodiments, the height of the amorphized upper region of the epitaxial source / drain region is greater than half of the total height of the epitaxial source / drain region. In some embodiments, each of the first rapid annealing process and the second rapid annealing process includes a rapid thermal annealing (RTA).

[0160] In one embodiment of the present disclosure, a method of forming a source / drain region includes forming a multilayer stack over a substrate. Patterning the multilayer stack to form a first channel region and a second channel region over the first channel region. The first channel region and the second channel region include nanostructures. The method includes epitaxially growing a first source / drain region over the substrate. The first channel region extends between the first source / drain regions. The first source / drain region applies stress to the first channel region. The method includes forming a dielectric layer over the first source / drain region. Forming a second source / drain region over the dielectric layer. The second channel region extends between the second source / drain regions. Forming the second source / drain region includes epitaxially growing a crystalline semiconductor material over the dielectric layer. Performing an implantation process that amorphizes a portion of the crystalline semiconductor material to form an amorphous semiconductor material over the crystalline semiconductor material. Performing a rapid thermal process that recrystallizes the amorphous semiconductor material. The method includes forming a first gate structure around the first channel region and a second gate structure around the second channel region.

[0161] In one embodiment, after performing the rapid thermal process, the first source / drain region applies stress in the first channel region. In one embodiment, the first source / drain region includes boron-doped silicon germanium. In one embodiment, the second source / drain region includes phosphorus-doped silicon. In one embodiment, the implantation process includes a process temperature in the range of -100°C to 28°C.

[0162] The foregoing summarizes the features of several embodiments or examples so that those skilled in the art may better understand the various aspects of the present disclosure. Those skilled in the art will recognize that they may easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or achieve the same advantages of the embodiments or examples described herein. Those skilled in the art will also recognize that such equivalent structures do not depart from the spirit and scope of the present disclosure, and that they may make various changes, substitutions, and modifications to the present disclosure without departing from the spirit and scope of the present disclosure.

Claims

1. A method for forming a source / drain region, characterized in that: include: forming a plurality of first nanostructures on a substrate; forming a plurality of second nanostructures above the plurality of first nanostructures; epitaxially growing a first source / drain region adjacent to the plurality of first nanostructures; epitaxially growing a second source / drain region above the first source / drain region and adjacent to the plurality of second nanostructures; Performing an implantation process to implant a plurality of impurities in the second source / drain region, wherein the implantation process forms an amorphous phase region in the second source / drain region; as well as At least one rapid thermal process is performed on the second source / drain region, wherein each of the rapid thermal processes performed recrystallizes a portion of the amorphous phase region.

2. The method according to claim 1, characterized in that After performing at least one of the rapid thermal processes, the first source / drain region applies compressive stress to the plurality of first nanostructures.

3. The method according to claim 1, characterized in that Each of the rapid thermal processes heats the second source / drain region to a temperature below 1250°C.

4. The method according to claim 1, characterized in that Each of the rapid thermal processes heats the second source / drain region for a duration shorter than 10 milliseconds.

5. A method for forming a source / drain region, characterized in that: include: Forming a fin extending from a substrate, wherein the fin includes a lower nanostructure and an upper nanostructure above the lower nanostructure; forming a plurality of lower epitaxial source / drain regions on a plurality of opposite sides of the lower nanostructure; forming an isolation region on the plurality of lower epitaxial source / drain regions; forming a plurality of upper epitaxial source / drain regions on the isolation region and on the plurality of opposite sides of the upper nanostructure; amorphizing a plurality of upper regions of the plurality of epitaxial source / drain regions; performing a first rapid annealing process to recrystallize first amorphous portions of the upper regions of the epitaxial source / drain regions; as well as After performing the first rapid annealing process, a second rapid annealing process is performed to recrystallize the remaining amorphous portions of the upper regions of the epitaxial source / drain regions.

6. The method according to claim 5, characterized in that Amorphizing the upper regions of the epitaxial source / drain regions includes implanting a plurality of dopants in the epitaxial source / drain regions.

7. The method according to claim 6, characterized in that The first rapid annealing process activates the plurality of dopants within the first amorphous portion of the plurality of upper regions of the plurality of epitaxial source / drain regions.

8. A method for forming a source / drain region, characterized in that: include: forming a multi-layer stack over a substrate; patterning the multilayer stack to form a plurality of first channel regions and a plurality of second channel regions above the plurality of first channel regions, wherein the plurality of first channel regions and the plurality of second channel regions include a plurality of nanostructures; epitaxially growing a plurality of first source / drain regions above the substrate, wherein the plurality of first channel regions extend between the plurality of first source / drain regions, wherein the plurality of first source / drain regions apply stress to the plurality of first channel regions; forming a dielectric layer over the plurality of first source / drain regions; forming a plurality of second source / drain regions above the dielectric layer, wherein the plurality of second channel regions extend between the plurality of second source / drain regions, wherein forming the plurality of second source / drain regions comprises: epitaxially growing a crystalline semiconductor material on the dielectric layer; performing an implantation process, wherein the implantation process amorphizes a portion of the crystalline semiconductor material to form an amorphous semiconductor material above the crystalline semiconductor material; and performing a plurality of rapid thermal processes that recrystallize the amorphous semiconductor material; and A first gate structure is formed around the first channel regions and a second gate structure is formed around the second channel regions.

9. The method according to claim 8, characterized in that After performing the plurality of rapid thermal processes, the plurality of first source / drain regions apply stress to the plurality of first channel regions.

10. The method according to claim 8, characterized in that The implantation process includes a process temperature in the range of -100°C to 28°C.