Composite groove type FBAR filter and preparation method thereof
By adopting a composite groove-type structure and process in the FBAR filter, the fracture of the bottom electrode and piezoelectric layer and the collapse of the resonant cavity are solved, and a high-performance and stable FBAR filter is achieved.
Patent Information
- Application Number
- CN202411123201.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-12-06
AI Technical Summary
During the manufacturing process, existing FBAR filters are prone to fracture of the bottom electrode and piezoelectric layer, collapse of the resonant cavity and low performance, and the way of reducing the resonant region will affect the stability and performance of the device.
Using a composite groove-shaped structure, including a composite groove-like substrate, a bottom electrode layer, a pre-deposition layer, a piezoelectric layer and a top electrode layer, the composite groove is etched by a photolithography process, and deposited and etched thereon. A stable structure is formed to avoid the use of support layers or support columns, thereby improving the stability and performance of the device.
The bottom electrode layer is not easy to break and the resonance region is stable, which improves the performance and stability of the FBAR filter, and avoids the problem of affecting the acoustic wave vibration mode due to the support layer or support column.
Smart Images

Figure CN119093900A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductor technology, and in particular relates to a composite groove type FBAR (Film Bulk Acoustic Resonator, FBAR) filter and a preparation method thereof. Background Art
[0002] With the development of modern micro-electro-mechanical system (MEMS) technology and in-depth research on piezoelectric materials, thin film bulk acoustic resonator technology has emerged. Devices based on thin film bulk acoustic resonator (FBAR) (such as filters and multiplexers) can be used in the ultra-high frequency field, and have high quality factor (Q value), strong power handling capacity, and can be integrated with IC (Integrated Circuit) technology, with integration potential, and have advantages that traditional filters cannot match. However, the manufacturing process of FBAR filters is dozens of times more complicated than other filters, and the investment in process equipment and measurement equipment is relatively large. Therefore, the high cost has restricted its popularization speed. At present, the core technology is in the hands of a few countries such as the United States, Germany, and Japan. Domestic research is in the initial stage, and the performance indicators of the manufactured devices are still far behind those of foreign countries. Therefore, the research on high-performance FBAR is of great significance to the development of wireless communications in my country.
[0003] According to the different composition structures of FBAR, it can be divided into three structures: back-etched type, solid-mounted resonator (SMR) and air cavity type. Among them, the air cavity type FBAR has better performance than the solid-mounted type and has a more stable structure than the back-etched type. Therefore, the air cavity type FBAR is currently the most widely used in the commercial field. Its structure is based on the MEMS silicon surface processing technology. A closed cavity is etched on the upper surface of the silicon substrate. The upper electrode interface and this closed cavity together confine the sound waves within the resonance area. There are two ways to form a cavity. One is to etch away part of the silicon surface, fill the sacrificial layer, and then prepare other material layers. Finally, the sacrificial layer is released through the through hole to form a concave air cavity; the second is to directly prepare a sacrificial layer on the silicon surface, then prepare other material layers, and finally release the sacrificial layer to form a convex air cavity structure.
[0004] For the concave air cavity FBAR filter, the bottom electrode and piezoelectric film are prepared on the sacrificial layer material. To ensure the preferred orientation growth of the piezoelectric film, it is required that after the cavity is filled with the sacrificial material, the step height difference inside and outside the cavity is less than 20nm, and the surface roughness is less than 1nm. Therefore, the substrate needs to be flattened by the CMP (Chemical Mechanical Polishing) process. However, since the cavity structure generally has a span ranging from tens of microns to hundreds of microns, it is difficult to avoid cavity depression or over-polishing in the conventional CMP process. Over-polishing will cause the height of the sacrificial layer to be lower than the substrate, and the bottom electrode and piezoelectric layer deposited later will easily break at the edge of the cavity. The cavity depression caused by the different reaction speeds between different areas of the sacrificial layer and the corresponding polishing liquid will make it impossible to carry out the subsequent process flow.
[0005] The most direct and obvious way to prepare FBAR devices with high operating frequencies is to reduce the resonance region, that is, the thickness of the bottom electrode, piezoelectric layer and top electrode. However, a top electrode that is too thin is not conducive to the extraction of the electrode for testing, and it is easy to break when crossing the piezoelectric layer step. Reducing the thickness of the piezoelectric layer is proportional to the parasitic effects introduced, which greatly affects the performance of the device. The thinning of the bottom electrode will make the device fragile and difficult to resist the pressure and stress of the subsequent deposited materials, resulting in the collapse of the device resonance region and the warping of the material after the cavity is released. Some designs have proposed the design of support columns and support layers to avoid the above problems, but these designs all affect the longitudinal vibration mode of the sound wave, thereby causing the performance of the FBAR device to decline.
[0006] Therefore, how to provide a FBAR filter that is not prone to breakage, stable and has high performance has become an urgent problem to be solved. Summary of the invention
[0007] In order to solve the above problems existing in the prior art, the present invention provides a composite groove type FBAR filter and a preparation method thereof.
[0008] The technical problem to be solved by the present invention is achieved through the following technical solutions:
[0009] In a first aspect, the present invention provides a composite groove type FBAR filter, comprising:
[0010] A composite groove-shaped substrate; the composite groove-shaped substrate has a composite groove; the composite groove includes a first bevel groove and a second bevel groove; the second bevel groove is formed in the central area of the bottom of the first bevel groove;
[0011] A bottom electrode layer; the bottom electrode layer fills the composite groove and is separated from the bottom of the second oblique angle groove by a gap;
[0012] A pre-deposition layer; the pre-deposition layer is stacked on a portion of the upper surface of the bottom electrode layer;
[0013] Piezoelectric layer; the piezoelectric layer is stacked on the upper surface of the pre-deposition layer;
[0014] A top electrode layer; the top electrode layer is stacked on the upper surface of the piezoelectric layer.
[0015] Optionally, the top electrode layer is in the shape of a regular pentagonal prism, and a bottom diameter of the top electrode layer is smaller than a bottom length of the second oblique angle groove.
[0016] Optionally, the composite groove-shaped substrate is made of Si; and the thickness of the composite groove-shaped substrate ranges from 524 μm to 526 μm.
[0017] Optionally, the material of the pre-deposition layer is Al; and the thickness of the pre-deposition layer is in the range of 5 nm to 10 nm.
[0018] Optionally, the material of the piezoelectric layer is AlN; the thickness of the piezoelectric layer ranges from 300 nm to 400 nm.
[0019] Optionally, the material of the top electrode layer is Mo; and the thickness of the top electrode layer is in the range of 50 nm to 70 nm.
[0020] Optionally, the bottom electrode layer is made of Mo; and the thickness of the bottom electrode layer is in the range of 50 nm to 70 nm.
[0021] Optionally, the bottom angles of the first bevel groove and the second bevel groove are both 135°.
[0022] Optionally, the depth of the first oblique angle groove ranges from 20nm to 30nm; the depth of the second oblique angle groove ranges from 300nm to 400nm.
[0023] In a second aspect, the present invention provides a method for preparing a composite groove type FBAR filter, the preparation method comprising:
[0024] Selecting an initial substrate;
[0025] Etching downward from the central area of the upper surface of the initial substrate to obtain a first oblique angle groove by using a photolithography process;
[0026] A second bevel groove is further etched downward in the bottom center area of the first bevel groove to obtain a composite groove-shaped substrate; the first bevel groove and the second bevel groove form a composite groove;
[0027] depositing a sacrificial layer at a lower portion of the second bevel groove;
[0028] Growing a bottom electrode layer on the upper surface of the sacrificial layer so that the bottom electrode layer fills the composite groove;
[0029] growing an initial pre-deposition layer on the upper surface of the bottom electrode layer;
[0030] growing an initial piezoelectric layer on the upper surface of the pre-deposited layer;
[0031] Etching downwards on the upper surface of the initial piezoelectric layer until a portion of the bottom electrode layer is exposed to obtain a pre-deposition layer and a piezoelectric layer;
[0032] Growing a top electrode layer in a middle region of the upper surface of the piezoelectric layer;
[0033] The sacrificial layer is released by wet etching.
[0034] The present invention provides a composite groove type FBAR filter. The presence of a first oblique angle groove and a second oblique angle groove in the composite groove of the composite groove-shaped substrate enables the bottom electrode layer to withstand the pressure of the resonance zone located above it, including the pre-deposition layer, the piezoelectric layer and the top electrode layer, without breaking or collapsing. Therefore, there is no need to add a supporting layer or a supporting column to sacrifice device performance in exchange for structural stability, thereby ensuring the high performance of the FBAR filter.
[0035] The present invention will be further described in detail below with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 is a cross-sectional view of a composite groove type FBAR filter provided by an embodiment of the present invention;
[0037] Figure 2 It is a schematic flow chart of a method for preparing a composite groove type FBAR filter provided by an embodiment of the present invention;
[0038] Figure 3 It is a schematic diagram of a preparation process of a composite groove type FBAR filter provided in an embodiment of the present invention.
[0039] Figure numerals: 10, composite groove-shaped substrate; 20, bottom electrode layer; 30, pre-deposition layer; 40, piezoelectric layer; 50, top electrode layer. DETAILED DESCRIPTION
[0040] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.
[0041] In order to solve the problems of easy breakage at the cavity edge, easy collapse of the resonant cavity and low performance of the existing FBAR devices, the embodiment of the present invention provides a composite groove type FBAR filter, see Figure 1 , Figure 1 It is a cross-sectional view of a composite groove type FBAR filter provided by an embodiment of the present invention, which specifically comprises a composite groove-shaped substrate 10 , a bottom electrode layer 20 , a pre-deposition layer 30 , a piezoelectric layer 40 and a top electrode layer 50 .
[0042] In the embodiment of the present invention, the composite groove-shaped substrate 10 has a composite groove, wherein the composite groove includes a first bevel groove and a second bevel groove, and the second bevel groove is formed in the center area of the bottom of the first bevel groove.
[0043] In the embodiment of the present invention, the composite groove-shaped substrate 10 is the base of the semiconductor chip, namely the FBAR filter, and provides a process platform for the subsequent formation of the FBAR filter structure. The composite groove-shaped substrate 10 can be grown in different ways, which are not limited here.
[0044] In the embodiment of the present invention, the composite groove of the composite groove-shaped substrate 10 includes a first oblique angle groove and a second oblique angle groove, wherein the bottom angles of the first oblique angle groove and the second oblique angle groove are equal and greater than 90°.
[0045] In the embodiment of the present invention, the bottom electrode layer 20 fills the composite groove and is separated from the bottom of the second oblique angle groove by a gap.
[0046] In an embodiment of the present invention, the bottom electrode layer 20 completely fills the first bevel groove in the composite groove, and its upper surface is at the same horizontal interface as the upper surface of the first bevel groove, and covers the upper part of the area filling the second bevel groove, and is separated from the bottom of the second bevel groove by a gap, which is the air cavity.
[0047] Specifically, the air cavity may occupy the lower 9 / 10 portion of the second oblique angle groove, and the bottom electrode layer 20 may occupy the upper 1 / 10 portion of the second oblique angle groove.
[0048] In the embodiment of the present invention, the material of the bottom electrode layer 20 may be Mo (molybdenum). Mo has the characteristic of high hardness, which can further improve the supporting capacity of the bottom electrode layer 20 to avoid the risk of the bottom electrode layer 20 being broken.
[0049] In addition, Mo has the characteristics of good high-temperature oxidation resistance and is not easily corroded. Selecting the bottom electrode layer 20 made of Mo can further improve the stability and service life of the device.
[0050] In the embodiment of the present invention, the pre-deposition layer 30 is stacked on a portion of the upper surface of the bottom electrode layer 20 .
[0051] In an embodiment of the present invention, since the upper surface of the bottom electrode layer 20 and the upper surface of the composite grooved substrate 10 are at the same horizontal interface, in order to subsequently lead out the bottom electrode, the pre-deposition layer 30 is configured to be stacked on a portion of the upper surface of the bottom electrode layer 20, that is, the pre-deposition layer 30 does not completely cover the upper surface of the bottom electrode layer 20, but exposes a portion of the bottom electrode layer 20.
[0052] In the embodiment of the present invention, the pre-deposition layer 30 may expose the bottom electrode layer 20 at four corners of the edge.
[0053] In the embodiment of the present invention, the piezoelectric layer 40 is stacked on the upper surface of the pre-deposition layer 30. The material of the pre-deposition layer 30 may be Al (aluminum), and the material of the piezoelectric layer 40 may be AlN (aluminum nitride).
[0054] According to the theoretical lattice constants of Al and AlN, the lattice mismatch rate of Al and AlN is smaller than that of Mo and AlN. Therefore, using the pre-deposition layer 30 made of Al as an induction layer for growing high-quality c-axis oriented single crystal AlN can make the crystallinity of AlN better and obtain a more stable and higher quality piezoelectric layer 40, thereby ensuring better piezoelectric performance of the piezoelectric layer 40 and further improving the device performance.
[0055] In the embodiment of the present invention, the thickness of the pre-deposition layer 30 may be in the range of 5 nm to 10 nm. The thickness of the piezoelectric layer 40 may be in the range of 300 nm to 400 nm.
[0056] In the embodiment of the present invention, the top electrode layer 50 is stacked on the upper surface of the piezoelectric layer 40 .
[0057] The material of the top electrode layer 50 may be Mo (molybdenum). Mo has the characteristics of high hardness, good high temperature oxidation resistance and not easy to be corroded. The top electrode layer 50 made of Mo improves the stability and service life of the device.
[0058] In the embodiment of the present invention, the thickness of the bottom electrode layer 20 and the top electrode layer 50 are both in the range of 50 nm to 70 nm. The top electrode layer 50 and the bottom electrode layer 20 can be used to establish electrical connection and lead out electrical signals.
[0059] In the embodiment of the present invention, the presence of the first bevel groove and the second bevel groove in the composite groove of the composite groove-shaped substrate 10 enables the bottom electrode layer 20 to withstand the pressure of the resonance zone located above it, including the pre-deposition layer 30, the piezoelectric layer 40 and the top electrode layer 50, without breaking or collapsing. Therefore, there is no need to add a supporting layer or a supporting column to sacrifice device performance in exchange for structural stability, thereby ensuring the high performance of the FBAR filter.
[0060] In the embodiment of the present invention, the top electrode layer 50 is in the shape of a regular pentagonal prism, and the bottom diameter of the top electrode layer 50 is smaller than the bottom length of the second oblique angle groove.
[0061] In the embodiment of the present invention, the regular pentagonal prism-shaped top electrode layer 50 can suppress parasitic modes. Specifically, one of the parasitic modes is the RL (Rayleigh-Lamb) lateral vibration mode. The more regular the shape, the easier it is to scatter. The top electrode layer 50 is set to a regular pentagonal prism, and the regular pentagonal boundaries of the surface and bottom are not easy to provide a direct path for lateral vibration. Therefore, the parasitic mode can be well suppressed, thereby improving the performance and stability of the device.
[0062] In the embodiment of the present invention, the bottom area of the top electrode layer 50 (the top electrode layer 50 is in the shape of a regular pentagonal prism, and its bottom area is consistent with its top area) is the resonance region, including the effective areas of the bottom electrode layer 20, the piezoelectric layer 40 and the top electrode layer 50. The bottom length of the second bevel groove is the bottom length of the air cavity. If the effective area of the resonance region is larger than the bottom area of the air cavity, severe lateral vibration will occur, which greatly affects the performance of the FBAR filter. Therefore, in the embodiment of the present invention, the bottom diameter of the top electrode layer 50 is set to be smaller than the bottom length of the second bevel groove.
[0063] In the embodiment of the present invention, the composite groove-shaped substrate 10 may be made of Si (silicon). Preferably, the composite groove-shaped substrate 10 may be a composite groove-shaped substrate 10 of intrinsic state-high resistance state Si single crystal.
[0064] The intrinsic state indicates that the composite grooved substrate 10 of Si single crystal does not have any external impurities or dopants. The high resistance state helps to reduce crosstalk and current leakage in the device, thereby improving the working efficiency and reliability of the device.
[0065] In the embodiment of the present invention, the thickness of the composite groove-shaped substrate 10 is in the range of 524 μm to 526 μm, preferably 525 μm. There is no limitation on the size of the composite groove-shaped substrate 10, preferably 4 inches.
[0066] In an embodiment of the present invention, the bottom angles of the first angled groove and the second angled groove are equal, and in order to ensure the supporting capacity of the first angled groove and the second angled groove, the bottom angles are set to be greater than 90°. Preferably, the bottom angles of the first angled groove and the second angled groove are both 135°.
[0067] In an embodiment of the present invention, the depth of the first oblique angle groove is less than the depth of the second oblique angle groove. Specifically, the depth of the first oblique angle groove ranges from 20nm to 30nm, and the depth of the second oblique angle groove ranges from 300nm to 400nm.
[0068] For example, the depth of the first bevel groove is 20 nm, and the depth of the second bevel groove may be 300 nm.
[0069] In an embodiment of the present invention, a method for preparing a composite groove type FBAR filter is also provided. Figure 2 , Figure 2 1 is a flow chart of a method for preparing a composite groove type FBAR filter provided by an embodiment of the present invention, and the preparation method specifically comprises the following steps:
[0070] Step S201, selecting an initial substrate.
[0071] See also Figure 3 , Figure 3 It is a schematic diagram of a preparation process of a composite groove type FBAR filter provided in an embodiment of the present invention. Figure 3 (a) is the selected initial substrate, wherein the material of the initial substrate can be Si.
[0072] In the embodiment of the present invention, after the initial substrate is selected, the initial substrate may be cleaned to remove contamination, dust, organic impurities, etc. on the surface of the substrate.
[0073] Taking the initial substrate as a 4-inch intrinsic state-high resistance state Si substrate as an example, the specific process of placing the 4-inch intrinsic state-high resistance state Si substrate in a 4-inch flower basket for cleaning may include: placing the 4-inch intrinsic state-high resistance state Si substrate in an acetone solution for ultrasonication for 15 minutes to 20 minutes, then placing it in an ethanol solution for ultrasonication for 15 minutes to 20 minutes, and finally placing it in deionized water for ultrasonication for 10 minutes to 15 minutes and then taking it out. Through the above steps, the contamination, dust and organic impurities on the surface of the 4-inch intrinsic state-high resistance state Si substrate can be removed. Finally, the surface of the 4-inch intrinsic state-high resistance state Si substrate is blown dry with a nitrogen gun, and then dried on a 100°C hot plate for 80 seconds to proceed with the subsequent process flow.
[0074] In the embodiment of the present invention, the temperature of ultrasound in the three solutions can be set to 45° C., and the ultrasound power can be set to 100W.
[0075] Step S202: etching downward from the center area of the upper surface of the initial substrate using a photolithography process to obtain a first oblique angle groove.
[0076] In the embodiment of the present invention, after obtaining the cleaned initial substrate, it is subjected to photolithography and RIE (Reactive Ion Etching) process:
[0077] The photoresist mask morphology with a 60° tilt angle is achieved by adjusting the temperature and time of the post-bake in the photolithography process. The time is preferably 90s. Figure 3 (b) Using fluorine-based gas (SF6) as the etching reaction gas, the etching ratio of Si to photoresist is controlled by adjusting the gas flow rate of RIE etching Si (for example, the O2 flow rate can be adjusted to 7 sccm), and a first bevel groove with a tilt angle of 45°, that is, a bottom angle of 135° is etched, see Figure 3 (c) During etching, the etching time can be set to 30 seconds, and the depth of the first bevel groove can be set to 20 nm.
[0078] Step S203 , etching a second bevel groove downwards in the bottom center area of the first bevel groove to obtain a composite groove-shaped substrate 10 ; the first bevel groove and the second bevel groove form a composite groove.
[0079] In the embodiment of the present invention, the second bevel groove is prepared on the basis of the first bevel groove. Specifically, the exposure area (the photoresist used is a positive photoresist) can be locked in the bottom center area of the second bevel groove by overlay, and then the etching process in step S102 is used to continue etching downward, see Figure 3 (d) The etching time can be set to 450s, and the depth of the second angled groove can be in the range of 300nm to 400nm, preferably 300nm. After the etching is completed, the second angled groove is obtained. Figure 3 (e).
[0080] Step S204 , depositing a sacrificial layer at the bottom of the second bevel groove.
[0081] In an embodiment of the present invention, a PECVD (Plasma Enhanced Chemical Vapor Deposition) method may be used to achieve deposition of the initial sacrificial layer. The material of the initial sacrificial layer may be SiO2 (silicon dioxide). The deposition of the initial sacrificial layer made of SiO2 may be achieved using reaction gases SiH4 (monosilane) and N2O (nitrous oxide):
[0082] SiH4+N2O→SiO2+H2(hydrogen)+N2(nitrogen);
[0083] In an embodiment of the present invention, the frequency of the radio frequency (RF) power supply used during deposition can be set to 13.56 MHz, the RF power can be set to 50 W, the reaction temperature can be set to 200° C., the N2O / SiH4 flow ratio can be set to 1 / 30, and the deposition time can be set to 30 min.
[0084] In the embodiments of the present invention, see Figure 3(f) After the initial sacrificial layer is obtained within the first bevel groove and the second bevel groove, a CMP process can be used to perform a polishing operation on the upper surface to make the upper surface of the composite groove-shaped substrate 10 not covered by the initial sacrificial layer and the upper surface of the initial sacrificial layer as smooth and continuous as possible. It can be noted that since the sacrificial layer of the final structure only exists in the second bevel groove, the polishing requirements for the initial sacrificial layer can be low.
[0085] The CMP process is a polishing process that forms a smooth surface on the surface of the ground medium through the synergistic effect of chemical corrosion and mechanical grinding.
[0086] After polishing, the initial sacrificial layer is etched downward to remove the initial sacrificial layer in the first bevel groove and the upper portion of the initial sacrificial layer in the second bevel groove to obtain a sacrificial layer. Figure 3 (g).
[0087] In the embodiment of the present invention, the initial sacrificial layer etched in the second bevel groove may occupy 1 / 10 of the depth of the entire second bevel groove, and the final sacrificial layer will occupy 9 / 10 of the second bevel groove from bottom to top.
[0088] For example, the depth of the second oblique angle groove ranges from 300 nm to 400 nm. Corresponding to this depth range, the depth of the sacrificial layer may range from 270 nm to 360 nm.
[0089] Step S205 , growing a bottom electrode layer 20 on the upper surface of the sacrificial layer so that the bottom electrode layer 20 fills the composite groove.
[0090] In the embodiment of the present invention, the initial bottom electrode layer can be grown on the upper surface of the sacrificial layer by magnetron sputtering. Figure 3 (h).
[0091] Specifically, during magnetron sputtering, 99.999% pure Mo metal target can be used as the sputtering target, the argon flow rate and nitrogen flow rate are set to 20 sccm and 7 sccm respectively, the chamber pressure is set to 2 mtor, the sputtering power is 150 W, the sputtering temperature is set to 500°C, and the sputtering time is set to 18 min.
[0092] In the embodiment of the present invention, the thickness of the initially grown bottom electrode layer is preferably 150 nm. Specifically, the thickness can be measured using a step profiler.
[0093] After the initial bottom electrode layer is obtained, a mask template 3 μm to 4 μm wider than the first oblique angle groove may be used to overlay the initial bottom electrode layer, and then the initial bottom electrode layer portion except the first oblique angle groove may be etched by ICP (Inductively Coupled Plasma Etching). Figure 3 (i), the etching time can be set to 180s~200s. Then use a coating machine to spin-coat a layer of organic solvent that does not react with the Mo polishing solution on the etched initial bottom electrode layer, so that it covers the upper surface of the etched bottom electrode layer as a protective layer. During the CMP polishing process, the Mo polishing solution does not react with the organic solvent, but due to the existence of mechanical polishing, the part of the bottom electrode layer after etching that is exposed by the organic solvent after being polished away in the horizontal direction will react with the Mo polishing solution, while the organic solvent at the slope of the groove edge will not be completely polished away, and therefore still does not react with the Mo polishing solution. That is, only the horizontal surface of the initial bottom electrode layer where the organic solvent is polished away will react with the Mo polishing solution, and the remaining part will not be affected due to the coverage of the organic solvent, thereby effectively preventing the occurrence of uneven corrosion by the polishing solution. After the polishing is completed, the bottom electrode layer 20 is obtained, see Figure 3 (j).
[0094] It can be noted that before polishing, a reverse etching process is required to perform ICP etching on the initial bottom electrode layer outside the groove, which can be as close to the grooved substrate as possible, thereby shortening the subsequent polishing time.
[0095] In the embodiment of the present invention, since the bottom electrode layer 20 is no longer a structure protruding from the surface of the composite groove-shaped substrate 10, the problem of the bottom electrode layer edge step affecting the growth of the piezoelectric material is eliminated.
[0096] Step S206 , growing an initial pre-deposition layer on the upper surface of the bottom electrode layer 20 .
[0097] In the embodiment of the present invention, after the polished device is cleaned, an initial pre-deposition layer is grown on the upper surface of the bottom electrode layer 20, see Figure 3 (k), the specific process is as follows:
[0098] The polished device is placed in a magnetron sputtering reaction chamber, and a 99.9995% pure aluminum metal target is used as a sputtering target on the upper surface of the bottom electrode layer 20. The argon flow rate is set to 20 sccm, the chamber pressure is set to 0.4 Pa, the sputtering power is set to 250 W, and the sputtering time is set to 36s to 48s for magnetron sputtering to obtain an initial pre-deposition layer.
[0099] Step S207 , growing an initial piezoelectric layer on the upper surface of the initial pre-deposition layer.
[0100] In an embodiment of the present invention, a magnetron sputtering method is used to grow an initial piezoelectric layer on the upper surface of the initial pre-deposition layer, see Figure 3 (l), the specific process is as follows:
[0101] After the sputtering in step S106 is completed, N2 is introduced into the magnetron sputtering reaction chamber, and the N2 flow rate is set to 7 sccm. The pressure in the chamber is modified to 2 mtor, the sputtering power remains unchanged, and then the shutter is closed for pre-sputtering for 5 minutes, and then the shutter is opened, and AlN is used as the sputtering target to start formally sputtering the initial piezoelectric layer. The sputtering time is set to 30 minutes to 32 minutes.
[0102] In the embodiment of the present invention, after the initial pre-deposition layer and the initial piezoelectric layer are sputtered, they can be subjected to high temperature annealing in a high temperature annealing furnace in a pure nitrogen environment. In the high temperature annealing process, the annealing time is set to 3 minutes and the annealing temperature is set to 800°C.
[0103] Step S208 , etching downwards on the upper surface of the initial piezoelectric layer until a portion of the bottom electrode layer 20 is exposed, thereby obtaining the pre-deposition layer 30 and the piezoelectric layer 40 .
[0104] In the embodiment of the present invention, ICP can be used to etch downward on the upper surface of the initial piezoelectric layer, and after etching, the pre-deposition layer 30 and the piezoelectric layer 40 stacked on the upper surface of the bottom electrode layer 20 are obtained, see Figure 3 (m), that is, after the ICP etching process, the pre-deposition layer 30 and the piezoelectric layer 40 will expose a portion of the bottom electrode layer 20 to facilitate the subsequent extraction of the bottom electrode layer 20.
[0105] In an embodiment of the present invention, the photoresist used in ICP etching may be 6130 positive photoresist, and the pre-bake time is set to 100° C. / 90 s, the exposure time is 2.3 s, the development time is 37 s, and the post-bake time is set to 110° C. / 100 s.
[0106] Step S209 , growing a top electrode layer 50 in the middle region of the upper surface of the piezoelectric layer 40 .
[0107] In the embodiment of the present invention, an initial top electrode layer is first grown on the upper surface of the piezoelectric layer 40 by magnetron sputtering, and then the initial top electrode layer is patterned and etched by ICP so that the etched top electrode layer 50 shows a regular pentagonal pattern covering the middle area of the upper surface of the piezoelectric layer 40 when viewed from top to bottom, that is, the initial top electrode layer is etched into a regular pentagonal top electrode layer 50, see Figure 3 (n), and leave part of the area as electrode lead-out.
[0108] Step S210, releasing the sacrificial layer by wet etching.
[0109] In the embodiment of the present invention, by adopting wet etching, the etching solution and the sacrificial layer can be chemically reacted to generate a soluble product, thereby removing the sacrificial layer to be etched, forming an air cavity, and finally obtaining a composite groove type FBAR filter, see Figure 3 (o).
[0110] Specifically, the etching solution involved in the release may be a BOE (Buffered Oxide Etch) solution. After 3 minutes of wet etching, the sacrificial layer is released and an air cavity is formed.
[0111] In the embodiment of the present invention, the presence of the first bevel groove and the second bevel groove in the composite groove of the composite groove-shaped substrate 10 enables the bottom electrode layer 20 to withstand the pressure of the resonance zone located above it, including the pre-deposition layer 30, the piezoelectric layer 40 and the top electrode layer 50, without breaking or collapsing. Therefore, there is no need to add a supporting layer or a supporting column to sacrifice device performance in exchange for structural stability, thereby ensuring the high performance of the FBAR filter.
[0112] In the embodiment of the present invention, the upper surface of the bottom electrode and the upper surface of the composite grooved substrate 10 are located at the same horizontal interface, and the CMP polishing process is mainly targeted at the bottom electrode rather than the sacrificial layer, thereby eliminating the influence on the quality of the grown piezoelectric layer 40 caused by the presence of steps and large roughness at the edge of the bottom electrode of the existing FBAR device, so that the grown piezoelectric layer 40 will not warp due to excessive edge stress, thereby further improving the performance of the FBAR filter.
[0113] In addition, the magnetron sputtering method, PECVD, RIE, ICP and other methods involved in the preparation method provided in the embodiment of the present invention are all common methods in semiconductor MEMS technology, which can effectively reduce the production cost while ensuring the excellent performance of the device, and conform to the development law of Moore's Law. Among them, the magnetron sputtering method can be replaced by atomic layer deposition process and other methods.
[0114] It should be noted that the terms "first", "second", etc. are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchangeable where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein.
[0115] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification.
[0116] Although the present invention is described herein in conjunction with various embodiments, in the process of implementing the claimed invention, those skilled in the art can understand and implement other changes to the disclosed embodiments by viewing the drawings and the disclosed content. In the description of the present invention, the term "comprising" does not exclude other components or steps, "one" or "an" does not exclude multiple situations, and "multiple" means two or more, unless otherwise clearly and specifically limited. In addition, certain measures are recorded in different embodiments, but this does not mean that these measures cannot be combined to produce good results.
[0117] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0118] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0119] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A composite groove type FBAR filter, characterized in that: include: A composite groove-shaped substrate; the composite groove-shaped substrate has a composite groove; the composite groove includes a first bevel groove and a second bevel groove; the second bevel groove is formed in the center area of the bottom of the first bevel groove; A bottom electrode layer; the bottom electrode layer fills the composite groove and is separated from the bottom of the second oblique angle groove by a gap; Pre-deposition layer; The pre-deposition layer is stacked on a portion of the upper surface of the bottom electrode layer; Piezoelectric layer; the piezoelectric layer is stacked on the upper surface of the pre-deposition layer; top electrode layer; The top electrode layer is stacked on the upper surface of the piezoelectric layer.
2. The composite groove type FBAR filter according to claim 1, characterized in that: The top electrode layer is in the shape of a regular pentagonal prism, and the bottom diameter of the top electrode layer is smaller than the bottom length of the second oblique angle groove.
3. The composite groove type FBAR filter according to claim 1, characterized in that: The composite groove-shaped substrate is made of Si; the thickness of the composite groove-shaped substrate is in the range of 524 μm to 526 μm.
4. The composite groove type FBAR filter according to claim 1, characterized in that: The material of the pre-deposition layer is Al; the thickness of the pre-deposition layer is in the range of 5 nm to 10 nm.
5. The composite groove type FBAR filter according to claim 1, characterized in that: The material of the piezoelectric layer is AlN; the thickness of the piezoelectric layer ranges from 300nm to 400nm.
6. The composite groove type FBAR filter according to claim 1, characterized in that: The material of the top electrode layer is Mo; the thickness of the top electrode layer is in the range of 50nm to 70nm.
7. The composite groove type FBAR filter according to claim 1, characterized in that: The material of the bottom electrode layer is Mo; the thickness of the bottom electrode layer is in the range of 50nm to 70nm.
8. The composite groove type FBAR filter according to claim 1, characterized in that: The bottom angles of the first bevel groove and the second bevel groove are both 135°.
9. The composite groove type FBAR filter according to claim 8, characterized in that: The depth of the first oblique angle groove ranges from 20nm to 30nm; the depth of the second oblique angle groove ranges from 300nm to 400nm.
10. A method for preparing a composite groove type FBAR filter, characterized in that: The preparation method comprises: Selecting an initial substrate; Etching downward from the central area of the upper surface of the initial substrate to obtain a first oblique angle groove by using a photolithography process; A second bevel groove is further etched downward in the bottom center area of the first bevel groove to obtain a composite groove-shaped substrate; the first bevel groove and the second bevel groove form a composite groove; depositing a sacrificial layer at a lower portion of the second bevel groove; Growing a bottom electrode layer on the upper surface of the sacrificial layer so that the bottom electrode layer fills the composite groove; growing an initial pre-deposition layer on the upper surface of the bottom electrode layer; growing an initial piezoelectric layer on the upper surface of the pre-deposited layer; Etching downwards on the upper surface of the initial piezoelectric layer until a portion of the bottom electrode layer is exposed to obtain a pre-deposition layer and a piezoelectric layer; Growing a top electrode layer in a middle region of the upper surface of the piezoelectric layer; The sacrificial layer is released by wet etching.
Citation Information
Cited By
Resonator with inductive charge trapping defect structure and preparation method