In-situ sealing structure of ceramic feedthrough and airtight packaging body

By introducing water-absorbing and expansion seals and insulating layers into the ceramic feedthrough, the problems of controlling brittleness and water vapor permeability of ceramic feedthrough materials are solved, and the dehumidification and leakage plugging are achieved, which extends the service life of the device and improves safety performance.

CN119095315APending Publication Date: 2024-12-06ZHEJIANG NUROTRON BIOTECH
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202311620354.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-11-30
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Existing active implantable devices are difficult to achieve long-term air sealing in bodily fluid environments, and the brittleness and water vapor permeability of ceramic feedthrough materials are difficult to fully control, resulting in water vapor leakage, affecting the life of the device and patient safety.

Method used

The ceramic feedthrough in-situ sealing structure is adopted, which includes a water-absorbing and expansion seal and an insulating layer. The gaps and cracks are blocked through the water-absorbing and expansion effects of the water-absorbing and expansion seal, thereby reducing the permeability of water vapor, and achieving dehumidification and leakage plugging effects.

Benefits of technology

It effectively extends the life of active implantable devices, ensures airtightness, reduces water vapor permeability, improves safety performance, and is suitable for leak plugging applications at various leak points.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119095315A_ABST
    Figure CN119095315A_ABST
Patent Text Reader

Abstract

The invention discloses a ceramic feed-through in-situ sealing structure and an airtight packaging body, the ceramic feed-through in-situ sealing structure comprises a shell, and further comprises a ceramic feed-through and a metal flange wrapping the periphery of the ceramic feed-through, the ceramic feed-through comprises a metal feed-through needle and a ceramic piece wrapping the periphery of the metal feed-through needle, and the ceramic piece is in sealed connection with the metal feed-through needle, the metal flange and the shell; the ceramic water heater further comprises a sealing assembly arranged in the shell, the sealing assembly comprises a rigid shell and a water absorption expansion sealing part, the rigid shell is fixedly connected with the shell, the water absorption expansion sealing part is located in the rigid shell and arranged on one side of the ceramic part, and the rigid shell is used for limiting the position of the water absorption expansion sealing part. The in-situ sealing structure of the ceramic feed-through not only has the effects of water absorption and dehumidification, but also has the effect of leakage point leakage stoppage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of medical devices, and in particular relates to an in-situ sealing structure of a ceramic feedthrough and an airtight sealing package. Background Art

[0002] Active implantable devices, such as cochlear implant systems, artificial vision, and implantable drug pumps, are often equipped with components such as chips and electronic circuits to achieve their functions and therapeutic purposes. Since water vapor has a significant impact on the functional failure of components (for example, water vapor accelerates metal corrosion, damages leads and bonding areas, and reduces the insulation performance of components), in order to ensure the long-term effectiveness (>10 years) of active implantable devices in body fluid environments, components often need to be hermetically sealed before they can be implanted in the human body.

[0003] The airtightness of the component housing is often optimized through structure or process to ensure a sufficiently long packaging life, such as optimizing the feedthrough structure, welding process, etc. There are large differences in the permeability of gases in different materials. It is generally believed that: metal < ceramic < glass < fluorocarbon < epoxy resin < silicone rubber. Therefore, the components in active implantable devices are often hermetically packaged with metal (for example, pure titanium, titanium alloy) or ceramic (for example, high-purity alumina or zirconium oxide), and the packaging shell is wrapped with implantable silicone rubber to improve its comfort. Since the components after hermetic packaging also need to be electrically connected to the outside, the use of all metal materials as the packaging shell cannot achieve conductive insulation between the two, that is, the components will form a conductive path between the shell. The optional solution includes hermetic packaging with all ceramic materials, but ceramic materials have hard and brittle characteristics, and will crack or even break under high-intensity impact, resulting in failure of the hermetic packaging. Therefore, the mainstream shells of active implantable devices currently use metal shells combined with ceramic feedthroughs.

[0004] In the existing requirements for implantable devices, the 10-year cumulative water vapor content of the hermetic package should be less than 5000ppm, which is equivalent to 8.1% humidity at 37°C and 16% humidity at 25°C. Under room temperature conditions, the ambient humidity generally ranges from 30% to 80%, so dehumidification is often required during hermetic packaging, and the humidity of the working environment is controlled. In theory, the risk of water vapor leakage in the package shell is extremely low, but it is still difficult to completely avoid it in practical applications. Water vapor leakage will inevitably lead to the failure of the implanted device, causing harm to the patient, and requiring a secondary operation to remove the implanted device. On the one hand, the various materials that constitute the components have different degrees of physical or chemical adsorption of water vapor. Therefore, before hermetic packaging, some of the adsorbed water can be removed by heating. However, considering the temperature tolerance of the components, the temperature should not be too high, so the adsorbed water is difficult to completely remove. The humidity of the working environment should be controlled during hermetic packaging to reduce the water vapor introduced into the package shell by the ambient humidity. On the other hand, the laser welding quality of the hermetic package has an important influence on the airtightness of the package shell. In research and development or processing and production, inert gases such as helium and argon are often introduced into the packaging shell. After the packaging is completed, the packaging shell is tested for airtightness (for example, helium leakage rate) to evaluate the airtightness and packaging life of the packaging shell, and to optimize the process or structure. Finally, although the combined application of metal shell and ceramic feedthrough reduces the risk of water vapor leakage during full ceramic packaging, it is difficult to avoid it completely. The brittleness of ceramics is an inherent property. Through reasonable structural design, the ceramic feedthrough is placed in a position on the packaging shell that is less affected by external impact, which can avoid the fracture of ceramics to a certain extent. Through-type cracks are easily discovered through the airtightness test as described above, but the early non-through-type cracks or defects are difficult to detect effectively and non-destructively. Although non-through-type cracks or defects will not immediately cause water vapor leakage, the defects will develop into through-type cracks under the action of various residual stresses during subsequent processing or long-term use, and cause water vapor leakage. And the development of ceramic cracks is unpredictable. After the hermetic packaging, the packaging shell still has multiple subsequent processing steps to complete the final implant device, such as wrapping with silicone rubber, disinfection and sterilization, transportation, etc. As mentioned above, the subsequent processing may cause ceramic fracture and lead to water vapor leakage, and the airtightness test is not suitable for implant devices wrapped with silicone rubber on the outside.

[0005] In summary, the accumulation of water vapor in the shell of active implantable devices will inevitably lead to the functional failure of components, thereby damaging the implantable device, causing harm to the patient, and requiring a second operation to remove the implantable device. Although the water vapor permeability of the metal and ceramic materials currently selected as airtight packaging is extremely low, it is difficult to achieve complete impermeability. In a body fluid environment that lasts for several years, more than ten years, or even decades, the accumulated water vapor content is still considerable. In the packaging shell, the laser welding between the metal lower shell and the metal upper cover, the laser welding between the metal flange of the ceramic feedthrough and the metal shell, the brazing welding between the metal flange on the ceramic feedthrough, the metal feedthrough needle and the ceramic tube / piece, and the quality of the ceramic have an important impact on the airtightness of the packaging shell, because these are often the main paths for water vapor leakage. Especially for ceramic tubes / pieces, their inherent brittleness and the unpredictability of crack development make it difficult to predict or evaluate the risks and life of airtight packaging.

[0006] In response to this problem, the existing remedial measures are mainly to place a desiccant in the shell. When water vapor penetrates into the shell, the desiccant can absorb water vapor, thereby reducing the humidity in the sealed shell and maintaining it at a low level, thereby protecting the components in the shell and achieving the purpose of extending the service life of the package shell. Patent 201310222678.X discloses a thick film getter slurry composition for moisture control to reduce moisture in electronic devices. Patent 201410334114.X discloses a composition for electronic device packaging, a packaging method and an OLED display device, which can absorb water and oxygen entering the electronic device. Many papers also disclose methods of using such desiccant to reduce the water vapor content in the package shell, thereby increasing its service life. However, such desiccant is often disposable, and will no longer have a dehumidification effect when it reaches saturation. The desiccant can only absorb water vapor entering the shell, but cannot reduce the water vapor permeability, especially when the ceramic in the ceramic feedthrough has a through crack, which increases the water vapor permeability, the dehumidification life of the desiccant will be reduced. Another solution is to wrap the packaging shell with materials such as silicone rubber, which can improve the comfort of the product and reduce the contact between water vapor and the packaging shell. However, the wrapping material is often easy to fall off the packaging shell, and the adhesion is not reliable, especially in long-term solution / body fluid environment, and the water vapor permeability of such materials is relatively high.

[0007] In summary, when ceramic feedthrough sealed packaging is used in active implantable devices, neither the method of placing a desiccant in the shell nor the method of wrapping the packaging shell with silicone rubber materials can achieve an excellent dehumidification effect, which can easily lead to failure of the active implantable device and cause harm to the patient. Summary of the invention

[0008] In order to solve the above problems, the technical solution of the present invention is as follows: an in-situ sealing structure of a ceramic feedthrough, comprising a shell, a ceramic feedthrough and a metal flange coated on the outer periphery of the ceramic feedthrough, the ceramic feedthrough comprising a metal feedthrough needle and a ceramic member coated on the outer periphery of the metal feedthrough needle, the ceramic member is sealedly connected to the metal feedthrough needle, the metal flange and the shell;

[0009] It also includes a sealing component arranged in the shell, the sealing component includes a rigid shell and a water-swellable seal, the rigid shell is fixedly connected to the shell, the water-swellable seal is located in the rigid shell and is arranged on one side of the ceramic component, and the rigid shell is used to limit the position of the water-swellable seal.

[0010] Preferably, the sealing assembly further comprises a first insulating layer covering the outer periphery of the metal feed-through needle, the first insulating layer is located in the rigid shell, and the first insulating layer is located between the water-swellable seal and the metal feed-through needle.

[0011] Preferably, the sealing assembly further comprises a second insulating layer, which is disposed on the inner surface of the rigid shell and surrounds the water-swellable sealing member.

[0012] Preferably, the projection of the water-swellable sealing component in a plane perpendicular to the metal feedthrough pin completely covers the projection of the ceramic component in a plane perpendicular to the metal feedthrough pin.

[0013] Preferably, a confined space is formed in the rigid shell, the water-swellable seal is located in the confined space, and the volume of the confined space is smaller than the volume of the water-swellable seal when it expands to a limit state.

[0014] Preferably, the volume ratio of the confined space to the water-swellable seal when expanded to the limit state is 0.0001-0.5.

[0015] Preferably, the water absorption expansion ratio of the water absorption expansion seal is greater than 5000%.

[0016] An airtight package includes the above-mentioned ceramic feedthrough in-situ sealing structure and a circuit board arranged in the shell, one end of the metal feedthrough needle is electrically connected to the circuit board, and the other end of the metal feedthrough needle extends outside the shell.

[0017] The beneficial effects of the present invention are:

[0018] 1. The in-situ sealing structure of the ceramic feedthrough of the present application is provided with a sealing assembly including a water-absorbing and swelling seal, so that the sealing structure has both the effect of absorbing water and dehumidifying and the effect of plugging leaks, thereby effectively protecting the components in the housing and extending the life of the active implantable device.

[0019] 2. The in-situ sealing structure of the ceramic feedthrough of the present application can block the channels (such as gaps, cracks, etc.) for water vapor to enter from the inside out by in-situ plugging, thereby reducing the water vapor permeability. Therefore, when it no longer has a dehumidification effect, it can still ensure the airtightness of the packaging shell, greatly extending the packaging life of the airtight package.

[0020] 3. The ceramic feedthrough in-situ sealing structure of the present application is simple and easy to implement, and can be flexibly used to plug leaks near various leak points, with a wide range of applications.

[0021] 4. The airtight package including the ceramic feedthrough in-situ sealing structure of the present application has excellent sealing and safety performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a partial structural schematic diagram of an in-situ sealing structure of a ceramic feedthrough according to a specific embodiment of the present invention;

[0023] Figure 2 A cross-sectional view of a ceramic feedthrough peripheral structure of an in-situ sealing structure of a ceramic feedthrough according to a specific embodiment of the present invention;

[0024] Figure 3 It is a partial structural schematic diagram of an in-situ sealing structure of a ceramic feedthrough according to a specific embodiment of the present invention;

[0025] Figure 4 It is a schematic diagram of the overall structure of a hermetic sealing package according to a specific embodiment of the present invention;

[0026] Figure 5 A schematic diagram of pressure changes during water absorption of a water-swellable seal of an in-situ sealing structure of a ceramic feedthrough according to a specific embodiment of the present invention;

[0027] Figure 6 It is a schematic diagram of the gas permeation process inside and outside the shell of the in-situ sealing structure of the ceramic feedthrough according to a specific embodiment of the present invention;

[0028] Figure 7 It is a schematic diagram of the plugging process of the in-situ sealing structure of the ceramic feedthrough according to a specific embodiment of the present invention;

[0029] Figure 8 It is a schematic diagram of the change of water vapor permeability of a ceramic component of an in-situ sealing structure of a ceramic feedthrough according to a specific embodiment of the present invention.

[0030] Fig. 9 The figure is a schematic diagram of the water vapor content in the shell of the in-situ sealing structure of the ceramic feedthrough according to a specific embodiment of the present invention. DETAILED DESCRIPTION

[0031] The preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0032] See also Figure 1 and Figure 2 , is an in-situ sealing structure of a ceramic feedthrough, comprising a shell, a ceramic feedthrough and a metal flange 303 coated on the periphery of the ceramic feedthrough, the ceramic feedthrough comprising a metal feedthrough needle 301 and a ceramic part 302 coated on the periphery of the metal feedthrough needle 301, the ceramic part 302 is sealedly connected to the metal feedthrough needle 301, the metal flange 303 and the shell. The ceramic part 302 and the metal feedthrough needle 301 and the metal flange 303 are all connected by brazing, and there are gaps 601 / 602 that are not visible at a macroscopic level. The shell comprises a metal lower shell 1 and a metal upper shell 2, and the metal upper shell 2 and the metal lower shell 1 are sealedly connected to the periphery of the metal flange 303. The metal flange 303 and the metal upper shell 2, and the metal upper shell 2 and the metal lower shell 1 are connected by laser welding, and there are gaps 603 / 604 that are not visible at a macroscopic level.

[0033] The main ways for water vapor to penetrate the equipment with a shell in an environment such as body fluids are gaps and ceramic parts 302, especially crack defects (not shown) that may exist on the ceramic parts 302. Therefore, the quality of laser welding, brazing and ceramic parts 302 has an important influence on the life of the airtight package. Often, the airtightness of the shell can be determined by non-destructive testing methods such as helium leakage, so as to evaluate its packaging life or optimize the structure and processing technology. However, from the shell to the final product, it still needs to go through multiple subsequent process steps, and the initial non-penetrating cracks of the ceramic part 302 will not cause the helium leakage test to fail, but the cracks will develop in the long term and are unpredictable. At a low water vapor leakage rate, the water vapor in the shell will gradually accumulate at a lower rate, and when it exceeds the upper limit, it will aggravate the corrosion or failure of the components. When a penetrating crack appears in the ceramic part 302, the rate of water vapor leakage will increase, which will shorten the packaging life.

[0034] Reference Figure 1 and Figure 3 A sealing assembly is provided in the shell, so as to play an airtight packaging role, thereby effectively protecting the components. The sealing assembly includes a rigid shell 703 and a water-swelling seal 701, and the rigid shell 703 is fixedly connected to the shell. Specifically, the two are fixedly connected by laser welding or the like, and a confined space is formed in the rigid shell 703. The water-swelling seal 701 is located in the confined space of the rigid shell 703 and is provided on one side of the ceramic part 302, and the rigid shell 703 is used to limit the position of the water-swelling seal 701.

[0035] The sealing assembly also includes an insulating layer 702, and the insulating layer 702 includes a first insulating layer and a second insulating layer. The first insulating layer is coated on the outer periphery of the metal feedthrough needle 301, and the first insulating layer is located in the rigid shell 703. The first insulating layer is located between the water-swelling seal 701 and the metal feedthrough needle 301 to ensure that the metal feedthrough needle 301 does not form a conductive path with the water-swelling seal 701 and / or the rigid shell 703, thereby affecting the communication between the inside and outside of the shell. The second insulating layer is arranged on the inner surface of the rigid shell 703 and surrounds the water-swelling seal 701 to ensure that the water-swelling seal 701 does not form a conductive path with the rigid shell 703, thereby affecting the communication between the inside and outside of the shell. In addition, there should be no insulating layer 702 or other obstacles between the water-swelling seal 701 and the shell, as this area is a leak point prone to water vapor leakage.

[0036] Furthermore, the insulating layer 702 is non-absorbent, non-conductive, and has a certain degree of flexibility. Specifically, it can be selected from polypropylene, polyethylene, polyvinyl chloride, polytetrafluoroethylene, etc. The rigid shell 703 is pure titanium or titanium alloy, etc.

[0037] The projection of the water-swellable sealing member 701 in a plane perpendicular to the metal feedthrough needle 301 completely covers the projection of the ceramic member 302 in a plane perpendicular to the metal feedthrough needle 301 to ensure effective leak plugging.

[0038] The dehumidification effect of the in-situ sealing structure is determined by the water absorption rate and quality of the material used for the water-absorbing and expanding seal 701. The greater the water absorption rate and quality, the more water can be absorbed, and the more significantly the package life is extended. The sealing and plugging effect is also determined by the expansion rate of the material used for the water-absorbing and expanding seal 701. In the case of a confined space and a fixed size of the water-absorbing and expanding component 701, the greater the expansion rate, the better the squeezing and plugging effect, the more obvious the reduction in water vapor permeability, and the more significantly the package life is extended.

[0039] The water-swelling seal 701 is made of a material with a water-swelling rate greater than 5000% and has a certain strength. Specifically, one of highly water-swelling resins / rubbers such as starch-acrylonitrile graft polymer, starch-acrylic acid copolymer, starch-acrylamide graft copolymer, cellulose graft copolymer, cellulose derivative cross-linked product, agarose derivative, chitosan derivative, sodium polyacrylate cross-linked product, polyvinyl alcohol cross-linked polymer, and their combinations can be selected.

[0040] In addition, the volume of the confined space is generally smaller than the volume of the fully expanded water-swellable seal 701, thereby further reducing water vapor penetration. Further, the volume ratio of the confined space to the fully expanded water-swellable seal 701 is 0.0001-0.5.

[0041] The main pathways for water vapor penetration in a device with a housing in an environment such as body fluids are the gaps 601-604 and the ceramic part 302. When a through crack appears in the ceramic part 302, since the size of the water-absorbing and swelling seal 701 that has not absorbed water is smaller than the confined space, it only fills the confined space in the early stage and does not have a leak-proofing effect, that is, it only has a dehumidification effect. When the water-absorbing and swelling seal 701 absorbs water and expands to a size equivalent to the confined space, the continuous water absorption and expansion squeezes the inner wall of the ceramic part 302, and then fills the leak point, achieving in-situ leak-proofing at the water vapor leak point. The above structure has both the effect of absorbing water and dehumidifying, and the effect of leak-proofing, thereby effectively protecting the components in the housing and extending the life of the active implantable device.

[0042] See also Figure 4 , is an airtight package including the in-situ sealing structure of the above-mentioned ceramic feedthrough, which also includes a circuit board 4 arranged in the shell, one end of the metal feedthrough needle 301 is electrically connected to the circuit board 4 through a wire 5, and the other end of the metal feedthrough needle 301 extends to the outside of the shell and is connected to the outside of the shell such as a receiving coil, a stimulation electrode (not shown), etc., so as to realize communication between the inside and the outside of the shell.

[0043] Below, the specific principles of dehumidification and leak plugging will be explained in detail.

[0044] Reference Figure 5 When the pressure sensor is placed between the water-swellable seal 701 and the metal lower shell 1, the pressure characteristics of the inner wall of the confined space formed by the water-swellable seal 701 after water absorption and expansion can be determined. For example, the size of the water-swellable seal 701 without water absorption is 0.5 of the confined space, and the water absorption expansion rate is 5000% (A); the size ratio is 0.05, and the water absorption expansion rate is 5000% (B); the size ratio is 0.05, and the water absorption expansion rate is 3000% (C); the measured pressure results are shown in Figure 5 . Since the size of the water-swellable seal 701 that has not absorbed water is smaller than that of the confined space, it only fills the confined space in the early stage and does not have a leak-proofing effect, that is, it only has a dehumidification effect. When the water-swellable seal 701 absorbs water and swells to a size equivalent to the confined space, the continuous water absorption and expansion will produce pressure on the inner wall, thereby showing a leak-proofing effect. In addition, it can be found that the smaller the size of the water-swellable seal 701 that has not absorbed water is relative to the confined space, the longer the filling stage is and the lower the leak-proofing effect is. The lower the water absorption and expansion rate, the lower the leak-proofing effect. On the other hand, the dehumidification effect is also positively correlated with its size and water absorption rate. Therefore, if the shell space allows, the water-swellable seal 701 should be as large as possible and made of a water-absorbing material with high water absorption and expansion.

[0045] See also Figure 6During the hermetic packaging process, the shell is often filled with 70% argon and 30% helium at a pressure of 1 bar. On the one hand, it serves as a protective gas for internal components, and on the other hand, it is convenient to detect the airtightness of the packaging shell. If the helium leakage rate of the shell is less than 10 -9 Pa m 3 / s, the airtight package is considered qualified, that is, the predicted package life is > 10 years. However, during the use of the package shell, the airtightness will inevitably decrease gradually, especially when cracks appear in the ceramic part 302, the airtightness will be significantly reduced. Therefore, the actual package life of the shell is often lower than the predicted one. - 7 Pam 3 / s, the exchange between the gas inside the shell and the gas in the environment outside the shell is often in a molecular flow state, which is extremely slow. However, since there is basically no water vapor inside the shell, while the external environment contains a large amount of water vapor, the water vapor in the external environment will gradually penetrate into the shell during the slow exchange process. When there is no pressure difference between the inside and outside of the shell, the gas exchange rate inside and outside the shell is roughly equal, so the water vapor in the external environment penetrates into the shell at a stable rate. However, since the molecular size of helium / argon is lower than that of water vapor, the diffusion rate of the former is greater than that of the latter. And the internal components have a certain adsorption effect on the water vapor that penetrates into, converting gaseous water into liquid water. In the actual process, due to the above two effects, there is a pressure difference between the inside and outside of the packaging shell, that is, the external pressure is higher than the internal pressure. When a desiccant is placed in the shell, this pressure difference effect is more significant. Therefore, although the use of a desiccant can reduce the water vapor content in the internal environment of the packaging shell, it will aggravate the penetration of water vapor, that is, the water vapor permeability increases. Figure 6 The example shows the permeation process of the gas inside and outside the shell at the ceramic part 302. The shell as a whole shows that helium / argon permeates from the inside of the shell to the outside of the shell, and water vapor permeates from the outside of the shell to the inside of the shell, and the permeation rate of water vapor is higher than that of helium / argon, and the accumulation of water vapor inside the shell is shown.

[0046] See also Figure 7, showing the plugging effect of the water-absorbing and swelling seal 701 on the cracks of the ceramic part 302. As mentioned above, when the water vapor in the external environment penetrates into the shell through the leak point such as the crack of the ceramic part 302, the water vapor encounters the water-absorbing and swelling seal 701 and is absorbed by it, and the water-absorbing and swelling seal 701 gradually expands. The water-absorbing and swelling seal 701 fills the confined space in the early water absorption process, so it does not have a plugging effect. And this stage will aggravate the pressure difference effect, so that the water vapor penetration is aggravated. However, when the water-absorbing and swelling seal 701 has filled the confined space and exerts pressure on the inner wall with the continuous water absorption and expansion, the water-absorbing and swelling seal 701 will be squeezed and filled into the leak point, realizing the in-situ plugging at the leak point. Under this squeezing and plugging effect, the pressure difference effect between the inside and outside of the leak point will be eliminated, and a positive pressure effect will be formed in the reverse direction, that is, the external pressure is lower than the internal pressure, which reduces the rate of water vapor penetration.

[0047] The experimental effects of the present invention will be described below with reference to specific embodiments.

[0048] The size of the shell is 20×20×5mm. A humidity sensor is placed to monitor the humidity changes in the shell. The internal space after placing the relevant components is 1cm 3 , filled with 70% argon + 30% helium, the pressure is 1 bar, and the initial helium leakage rate after packaging is 10 -10 ~10 -9 Pa m 3 / s. The material of the water-swelling seal 701 is sodium polyacrylate crosslinked material, and the water-swelling rate is 5000%, that is, 50 times. The size of the water-swelling seal 701 is 10×3×0.5mm, and the mass is 35mg. The material of the insulating layer 702 is polytetrafluoroethylene, and the rigid shell 703 is titanium alloy. Physiological saline is used to simulate the human body fluid environment, and 80°C is used as the temperature acceleration (that is, the acceleration factor is 20 times). The shell is placed under the above conditions, taken out after different time periods, and its helium leakage rate is measured.

[0049] Comparative Example 1: The shell is a conventional shell, and no desiccant or other types of water-absorbing materials are placed inside.

[0050] Comparative Example 2: A desiccant is placed in the shell. The desiccant is calcium oxide, has a water absorption rate of 50%, i.e. 0.5 times, and a mass of 400 mg.

[0051] Embodiment 1: A water-swellable seal 701 is placed inside the housing.

[0052] See also Figure 8, are the water vapor permeabilities of the comparative example and the embodiment. When cracks develop on the ceramic part 302, it can be seen that the water vapor permeability in comparative example 1 will increase significantly, and when the internal and external air pressures reach equilibrium, the growth of the water vapor permeability is relatively slow. In comparative example 2, when cracks develop, due to the presence of the desiccant, the water vapor permeability will increase at a faster rate, mainly due to the pressure difference after the desiccant absorbs water vapor. When the dehumidification effect of the desiccant decreases, the water vapor permeability will increase at a slow rate, but the final permeability rate will be higher than that of comparative example 1. In embodiment 1, it can be found that the water-absorbing expansion seal 701 has no obvious plugging effect in the early stage of filling confined space. When the water-absorbing expansion seal 701 expands to a certain extent, it will show an obvious plugging effect. Some of the developed crack leaks are filled with water-absorbing materials, which slows down the growth of the water vapor permeability.

[0053] See also Fig. 9 , are the results of the water vapor content of the comparative example and the embodiment. In the case of no cracks, that is, when the water vapor permeability is maintained at a stable and low level, the cumulative water vapor content in comparative example 1 gradually increases at a substantially constant rate and is less than 5000 ppm. v The corresponding packaging life is about 10 years. In Comparative Example 2, due to the dehumidification effect of the desiccant, the water vapor in the shell is basically maintained at an extremely low level (close to zero) before the desiccant fails, and when the desiccant fails due to water absorption saturation, the water vapor will accumulate at a rate slightly higher than that in Comparative Example 1. Overall, the packaging life is significantly extended. In Example 1, similar to Comparative Example 2, since the water absorption and expansion seal 701 has a dehumidification effect similar to that of a desiccant, the water vapor in the packaging shell is also maintained at an extremely low level before it fails due to water absorption saturation. Another point is that although there are no cracks, the water absorption and expansion seal 701 still has a certain degree of plugging effect after water absorption and expansion. After it fails due to water absorption saturation, water vapor will accumulate at a rate slightly lower than that in Comparative Example 1. In the case of cracks, the cracks will cause a significant increase in water vapor permeability. Therefore, in Comparative Example 1, the accumulated water vapor content in the shell will increase sharply, greatly shortening its packaging life. In Comparative Example 2, due to the dehumidification effect of the desiccant, the increase in water vapor permeability caused by the cracks did not cause obvious water vapor content in the packaging shell in the early stage. However, when the desiccant fails due to water absorption saturation, water vapor will penetrate into the shell at a faster rate due to the pressure difference after dehumidification. When the pressure difference weakens or disappears, water vapor will penetrate at the same rate as in Comparative Example 1. Overall, the life of the packaging shell will be extended to a certain extent. In Example 1, compared with Comparative Example 2, even after the dehumidification effect of the water absorption and expansion seal 701 fails, due to its plugging effect, the water vapor permeability will be improved. Therefore, the subsequent water vapor leakage rate can still be maintained at a low level, greatly extending the packaging life.

[0054] Finally, it should be noted that the above preferred embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail through the above preferred embodiments, those skilled in the art should understand that various changes can be made in form and details without departing from the scope defined by the claims of the present invention.

Claims

1. An in-situ sealing structure of a ceramic feedthrough, comprising a housing, characterized in that: It also includes a ceramic feedthrough and a metal flange coated on the outer periphery of the ceramic feedthrough, the ceramic feedthrough includes a metal feedthrough needle and a ceramic component coated on the outer periphery of the metal feedthrough needle, and the ceramic component is sealedly connected to the metal feedthrough needle, the metal flange and the housing; It also includes a sealing component arranged in the shell, the sealing component includes a rigid shell and a water-swellable seal, the rigid shell is fixedly connected to the shell, the water-swellable seal is located in the rigid shell and is arranged on one side of the ceramic component, and the rigid shell is used to limit the position of the water-swellable seal.

2. The in-situ sealing structure of a ceramic feedthrough according to claim 1, characterized in that: The sealing assembly further comprises a first insulating layer covering the outer periphery of the metal feed-through needle, wherein the first insulating layer is located in the rigid shell and between the water-swellable sealing component and the metal feed-through needle.

3. An in-situ sealing structure of a ceramic feedthrough according to claim 1 or 2, characterized in that: The sealing assembly further comprises a second insulating layer, which is arranged on the inner surface of the rigid shell and surrounds the water-swellable sealing component.

4. The in-situ sealing structure of a ceramic feedthrough according to claim 1, characterized in that: The projection of the water-swellable sealing component in a plane perpendicular to the metal feed-through pin completely covers the projection of the ceramic component in a plane perpendicular to the metal feed-through pin.

5. The in-situ sealing structure of a ceramic feedthrough according to claim 1, characterized in that: A confined space is formed in the rigid shell, the water-swellable seal is located in the confined space, and the volume of the confined space is smaller than the volume of the water-swellable seal when it expands to a limit state.

6. The in-situ sealing structure of a ceramic feedthrough according to claim 5, characterized in that: The volume ratio of the confined space to the water-swellable seal when expanded to the limit state is 0.0001-0.

5.

7. The in-situ sealing structure of a ceramic feedthrough according to claim 1, characterized in that: The water absorption expansion rate of the water absorption expansion seal is greater than 5000%.

8. An airtight package, characterized in that: An in-situ sealing structure comprising the ceramic feedthrough according to any one of claims 1 to 7, further comprising a circuit board arranged in the shell, one end of the metal feedthrough needle being electrically connected to the circuit board, and the other end of the metal feedthrough needle extending outside the shell.

Citation Information

Patent Citations

  • Thick film getter paste compositions for use in moisture control

    CN103319091A

  • Composition for electronic device packaging, packaging method, and OLED display device

    CN104167394A

  • Ceramic feed-through connector for implantable electrical stimulator and method for manufacturing ceramic feed-through connector

    CN102872529A

  • Sealed power source feed-through terminal plate component

    CN103296495A

  • Seal structure of implanted device

    CN106361464A