Production equipment and production process of aluminum foil meal box
By introducing deformation mechanism, stamping components and heat dissipation components into the aluminum foil lunch box production equipment, the problem of fixed mold cavity size and poor heat dissipation effect is solved, and the flexibility and efficient heat dissipation of the production of lunch boxes of different specifications is achieved, reducing the operation complexity and production costs.
Patent Information
- Application Number
- CN202411502503.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-25
- Publication Date
- 2024-12-27
- Estimated Expiration
- 2044-10-25
AI Technical Summary
The mold cavity size of the existing aluminum foil lunch box stamping and forming equipment is fixed, resulting in the need to replace the mold when producing lunch boxes of different specifications, which increases the cumbersome operation and production costs. At the same time, the heat dissipation effect is poor, which affects continuous production, and it is easy to get stuck in the mold of the lunch box. Demolding, and the mold cavity is difficult to clean.
An aluminum foil lunch box production equipment is designed, including deformation mechanism, stamping assembly and heat dissipation assembly. The deformation mechanism moves the corner plate synchronously through the transmission of the tooth ring and gear, adjusts the size of the mold cavity to adapt to the lunch box of different specifications. The stamping component is stamped with lifting rods and screws, and the heat dissipation component is circulated through the coolant flow and the semiconductor refrigeration sheet to improve heat dissipation. efficiency.
It realizes the flexibility of producing lunch boxes of different specifications, facilitates mold release and cleaning, improves heat dissipation efficiency, and reduces production costs and operation complexity.
Smart Images

Figure CN119187385A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum foil tableware processing, in particular to production equipment and a production process for an aluminum foil lunch box. Background Art
[0002] After the aluminum foil is stamped into the shape of a lunch box, the lunch box usually needs to be pressed to the edge. Additional equipment specifically used for pressing the edge is required to complete the pressing operation, which increases the manufacturer's investment cost. A process for preparing a heatable aluminum foil packaging lunch box with application number CN202010876648.0 includes a base plate, a workbench, a mounting frame, a stamping device and a feeding device. During the movement of the aluminum foil, air blowing is used to guide and position the aluminum foil to avoid displacement of the aluminum foil and prevent deformation of the aluminum foil due to extrusion.
[0003] Although the device has the above advantages, it still has the following defects in actual use:
[0004] 1) The mold cavity size of the device is fixed, resulting in that only a single specification of lunch boxes can be produced in the actual production process. If lunch boxes of different specifications need to be produced, molds of different specifications need to be replaced, which increases the complexity of the operation and the production cost;
[0005] 2) The heat dissipation effect of the device is poor when in use, which affects the continuous production of lunch boxes. There are also problems that the lunch boxes are easily stuck in the mold and difficult to demold, and the mold cavity is difficult to clean.
[0006] Therefore, it is necessary to solve the problems that still exist in the above-mentioned device. Summary of the invention
[0007] In view of the deficiencies in the prior art, the present invention provides a production device and a production process for aluminum foil lunch boxes, which solves the problem that when the existing aluminum foil packaging lunch box stamping and forming equipment is used, due to the fixed mold cavity size, different specifications of molds need to be replaced when producing lunch boxes of different specifications, which increases the cumbersomeness of operation and production costs. At the same time, the poor heat dissipation effect affects continuous production, and there are problems such as the lunch box is easily stuck in the mold and difficult to demold, and the mold cavity is difficult to clean.
[0008] To achieve the above purpose, the present invention is implemented by the following technical scheme: a production device for an aluminum foil lunch box, comprising:
[0009] Die base for support and forming;
[0010] A deformation mechanism, the deformation mechanism is arranged on the mold base, the deformation mechanism includes four corner plates, the outer surfaces of the four corner plates are mutually attached and are all arranged on the mold base, the four corner plates are formed by cutting a square plate along two diagonal lines, and the four corner plates can adjust the size of the central area by horizontally moving along the outer surface, and facilitate demoulding of the formed lunch box;
[0011] A stamping assembly, which is arranged on a die base and stamps the aluminum foil material by moving up and down and cooperating with a corner plate;
[0012] The heat dissipation component dissipates heat from the mold base and the angle plate through the flow of coolant, which facilitates continuous production.
[0013] Preferably, the outer part of the angle plate is sleeved with a gear ring, the ring of the gear ring is movably connected with a gear, the outer surface of the gear is meshed with a ruler plate, the outer surface of the ruler plate is fixedly connected to the outer surface of the angle plate, the body of the angle plate is provided with a through slide groove, the inside of the slide groove is movably connected with a pin rod, one end of the pin rod is fixedly connected to the outer surface of the mold base, the outer surface of the gear ring is fixedly connected with a swivel, the outer surface of the swivel is embedded and rotatably connected with the outer surface of the mold base, and the outer surface of the gear ring is fixedly connected with a shift rod.
[0014] Preferably, the stamping assembly includes a bracket, the outer surface of the bracket is fixedly connected to the outer surface of the die base, the outer surface of the bracket is fixedly connected to a lifting rod, a punch is arranged outside the output end of the lifting rod, the outer surface of the punch is fixedly connected to a screw, the outer surface of the screw is threadedly connected to a screw sleeve, and the outer surface of the screw sleeve is fixedly connected to the output end of the lifting rod.
[0015] Preferably, a pneumatic unit is provided on the body of the punch, and the pneumatic unit includes an inner cavity, which is opened on the body of the punch, and a fan is provided inside the inner cavity. The interior of the inner cavity is connected with an air hole, and the air hole is opened on the body of the punch and is in a through state. A square frame is slidably connected to the interior of the inner cavity, and the outer surface of the fan is fixedly connected to the interior of the square frame ring.
[0016] Preferably, the outer surface of the square frame is fixedly connected to a push-pull rod, the outer surface of the push-pull rod is fixedly connected to the interior of the inner cavity, the outer surface of the square frame is fixedly connected to a sliding column, the outer surface of the sliding column is slidably connected to the interior of the inner cavity and the air hole respectively.
[0017] Preferably, the heat dissipation component includes a heat dissipation groove, which is opened on the main body of the mold base and is in a through-state, a partition is fixedly connected to the inside of the heat dissipation groove, a semiconductor refrigeration plate is fixedly connected to the outer surface of the partition, a fin is fixedly connected to the outer surface of the partition, and a liquid pump is arranged inside the heat dissipation groove.
[0018] Preferably, the interior of the heat dissipation groove is connected with a solid cover, the outer surface of the solid cover is fixedly connected to the outer surface of the mold base, the interior of the solid cover is penetrated by a spring tube, and one end of the spring tube is penetrated and connected with the interior of the inner cavity.
[0019] Preferably, a linkage unit is provided on the outside of the semiconductor refrigeration plate, and the linkage unit includes a slide rail, the outer surface of the slide rail is fixedly connected to the outer surface of the mold base, the outer surface of the slide rail is slidably connected to a linear motor, the outer surface of the linear motor is fixedly connected to a connecting plate, the outer surface of the connecting plate is fixedly connected to a sliding rheostat, and the outer surface of the sliding rheostat is fixedly connected to the outer surface of the mold base.
[0020] Preferably, a fixed frame is fixedly connected to the outer surface of the linear motor, an I-shaped wheel is rotatably connected to the body of the fixed frame, a sliding sleeve is fixedly connected to the outer surface of the I-shaped wheel, and the sliding sleeve is sleeved on the outer surface of the shifting rod.
[0021] The present invention also discloses a production process of an aluminum foil lunch box production device, which specifically comprises the following steps:
[0022] Step 1: The gear ring is rotated by the lever, and the four angle plates are moved synchronously by the transmission of the gear and the ruler plate, so that the space between the angle plates is adjusted, and then the aluminum foil raw material is placed on the surface of the angle plate, and then the output end of the lifting rod is extended to drive the punch to descend, and cooperate with the angle plate to punch the aluminum foil raw material into a lunch box shape, and then the angle plate continues to move to break away from the contact with the lunch box, so as to facilitate the demoulding of the formed lunch box;
[0023] Step 2: When the formed lunch box is stuck outside the punch, the output end of the push-pull rod retracts to drive the frame to rise, so that the slide column is free from the blockage of the air hole. Then the fan works through the air pressure to blow the formed lunch box off, and the fan extracts the air inside the heat dissipation groove through the spring tube and the solid cover to dissipate the heat of the hot end of the semiconductor refrigeration plate;
[0024] Step three: The cold end of the semiconductor refrigeration plate cools down the coolant through the partition and the fin plate, and drives the coolant to circulate through the liquid pump to dissipate heat to the mold base and the angle plate. At the same time, when the linear motor moves the lever through the sliding sleeve to adjust the size of the space between the angle plates, the resistance value of the sliding rheostat is synchronously adjusted through the connecting plate, so that the power of the semiconductor refrigeration plate and the liquid pump can be adjusted according to the size of the lunch box.
[0025] Beneficial Effects
[0026] The present invention provides a production device and a production process for an aluminum foil lunch box. Compared with the prior art, it has the following beneficial effects:
[0027] (1) By setting up a deformation mechanism, utilizing the rotation of the gear ring and the meshing transmission of the gear and the ruler plate, the four corner plates move synchronously to adjust the size of the space between the corner plates, so as to facilitate the production of lunch boxes of different specifications. When the space adjustment is larger than the specifications of the lunch box, it is convenient for demoulding the lunch box and cleaning the space between the corner plates.
[0028] (2) By setting up a punching assembly, using a lifting rod to drive the punch to rise and fall, and cooperating with the function of the angle plate, the aluminum foil raw material can be punched into a lunch box, and through the cooperation of the screw and the screw sleeve, it is easy to disassemble and assemble the punch, and replace the punches of different specifications.
[0029] (3) By setting up a pneumatic unit, the push-pull rod is used to drive the square frame to move, so that it drives the sliding column to move away from the obstruction of the air hole, and the fan is operated to blow air through the air hole, so that the lunch box stuck outside the punch can be demolded and the space between the corner plates can be cleaned.
[0030] (4) By setting up a heat dissipation component and using a liquid pump to drive the coolant to circulate, the mold base and the angle plate can be cooled through the action of the semiconductor cooling plate, the partition and the fin plate. At the same time, the inner side of the heat dissipation groove is transparent, which is also convenient for the heat dissipation of the hot end of the semiconductor cooling plate. The spring tube and the solid cover are coordinated to facilitate the fan to drive the air to flow on one side of the inner side of the heat dissipation groove to improve the heat dissipation efficiency.
[0031] (5) By setting up a linkage component, the linear motor slides along the slide rail. Through the cooperation of the fixed frame, the I-wheel and the sliding sleeve, the lever can be moved to drive the gear ring to rotate, so as to drive the angle plate to move to adjust the size of the space, and the sliding end of the sliding rheostat can be pushed to move synchronously through the connecting plate to adjust the power of the liquid pump and the semiconductor refrigeration plate, so that the power is proportional to the volume of the lunch box, so as to improve the heat dissipation effect when producing lunch boxes of different specifications. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a three-dimensional diagram of the external structure of the present invention;
[0033] Figure 2 It is a three-dimensional diagram of the external structure of the corner plate of the present invention;
[0034] Figure 3 A three-dimensional diagram of the internal structure of the mold base of the present invention;
[0035] Figure 4 It is a three-dimensional diagram of the external structure of the slide rail of the present invention;
[0036] Figure 5 A three-dimensional diagram of the external structure of the punch of the present invention;
[0037] Figure 6 It is a three-dimensional diagram of the internal structure of the punch of the present invention.
[0038] In the figure: 1. die base; 2. angle plate; 3. stamping assembly; 31. bracket; 32. lifting rod; 33. punch; 34. pneumatic unit; 341. inner cavity; 342. fan; 343. air hole; 344. frame; 345. push-pull rod; 346. slide column; 35. screw; 36. screw sleeve; 4. heat dissipation assembly; 41. heat dissipation groove; 42. partition; 43. semiconductor cooling plate; 44. linkage unit; 441. slide rail; 442. linear motor; 443. sliding rheostat; 444. connecting plate; 445. fixed frame; 446. I-shaped wheel; 447. sliding sleeve; 45. fin plate; 46. liquid pump; 47. fixed cover; 48. spring tube; 5. gear ring; 6. gear; 7. ruler plate; 8. slide groove; 9. pin rod; 10. swivel; 11. lever. DETAILED DESCRIPTION
[0039] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0040] See also Figure 1-6 The present invention provides a technical solution: a production device for an aluminum foil lunch box:
[0041] Embodiment 1: Refer to the attached manual Figure 1 , Attachment Figure 2 ;
[0042] The mold base 1 includes a mold base 1, and a deformation mechanism is arranged on the outside of the mold base 1. The deformation mechanism includes four isosceles angle plates 2. The angle plates 2 are made of four isosceles triangular cross-section plates formed by equally cutting a square plate along two diagonals. At the same time, the angle plates 2 slide horizontally along the bottom edge. The waist edges of the four angle plates 2 fit each other, and the outer surfaces are all slidably connected to the outer surface of the mold base 1. A notch is arranged at an angle end of one side of the angle plate 2, and one side of the notch is a movement front to avoid collision with the ring of the gear ring 5 and improve the movement range. A gear ring 5 is sleeved on the outside of the angle plate 2. The teeth of the gear ring 5 are arranged on the inner wall of the ring. The ring of the gear ring 5 is movably connected with a gear 6. The outer surface of the wheel 6 is meshed with a ruler plate 7, and the outer surface of the ruler plate 7 is fixedly connected to the outer surface of the angle plate 2. The body of the angle plate 2 is provided with a through slide groove 8, and the inner part of the slide groove 8 is movably connected with a pin rod 9. At least two pin rods 9 are provided inside each slide groove 8 to limit and guide the movement of the angle plate 2. One end of the pin rod 9 is fixedly connected to the outer surface of the mold base 1. The outer surface of the gear ring 5 is fixedly connected to a swivel 10. The cross-section of the swivel 10 is T-shaped to improve the stability of the connection between the gear ring 5 and the mold base 1. The outer surface of the swivel 10 is embedded in the outer surface of the mold base 1 for rotation connection, and the outer surface of the gear ring 5 is fixedly connected to a lever 11.
[0043] In this embodiment, the gear ring 5 is driven by the lever 11 to rotate, and the gear 6 is respectively engaged with the gear ring 5 and the ruler plate 7, so that the ruler plate 7 pushes the four corner plates 2 to move synchronously. During the movement of the corner plates 2, the pin rod 9 slides inside the slide groove 8 to limit and guide the movement of the corner plates 2. At the same time, after the corner plates 2 move, a mold cavity can be formed by the space surrounded by the waist edge to facilitate the forming of the lunch box.
[0044] Embodiment 2: Based on Embodiment 1, refer to the attached Figure 1 , Attachment Figure 5 ;
[0045] A stamping assembly 3 is provided on the outside of the angle plate 2, and the stamping assembly 3 includes a bracket 31. The outer surface of the bracket 31 is fixedly connected to the outer surface of the mold base 1. The outer surface of the bracket 31 is fixedly connected to a lifting rod 32. The lifting rod 32 is made of an existing hydraulic rod and is connected to an external control circuit. As a preferred method, a pressing device of an existing equipment can be provided on the output end of the lifting rod 32 to cut the edge of the formed lunch box. A punch 33 is provided on the outside of the output end of the lifting rod 32. There are multiple punches 33 with different sizes to facilitate the production of lunch boxes of different specifications. A screw 35 is fixedly connected to the outer surface of the punch 33. A screw sleeve 36 is threadedly connected to the outer surface of the screw 35. The sizes of the screw sleeve 36 and the screw 35 are adapted, and they are modularly arranged to facilitate the disassembly, assembly and replacement of the punch 33. The outer surface of the screw sleeve 36 is fixedly connected to the output end of the lifting rod 32.
[0046] In this embodiment, after the position adjustment of the angle plate 2 is completed, the aluminum foil raw material is placed on the angle plate 2, and then a punch 33 of a size corresponding to the required production specification is selected and installed on the output end of the lifting rod 32 through the connection of the screw 35 and the screw sleeve 36. Then the output end of the lifting rod 32 is extended to drive the punch 33 and the edge pressing device to descend. Through the cooperation of the punch 33 and the waist edge of the angle plate 2, the raw material is punched into a lunch box, and the edge of the lunch box can be cut by the edge pressing device.
[0047] Embodiment 3: Based on Embodiment 2, refer to the attached Figure 1 , Attachment Figure 6 ;
[0048] The body of the punch 33 is provided with a pneumatic unit 34, which includes an inner cavity 341, which is opened on the body of the punch 33, and a fan 342 is arranged inside the inner cavity 341. The fan 342 is made of a two-way fan of model DPT20-65B and is electrically connected to an external control circuit. The inner cavity 341 is connected with air holes 343. As a preferred embodiment, the air holes 343 are respectively arranged at the bottom and around the inner wall of the inner cavity 341. When the frame 344 covers the bottom air holes 343, the side air holes 343 can facilitate the normal operation of the fan 342. The air holes 343 are opened on the body of the punch 33 and are in a through state. The inner cavity 341 is slidably connected with the frame 3 44. The frame 344 is square on the outside and circular on the inside, and is made of a material that is resistant to pressure, high temperature, wear and has good sealing properties. The outer surface of the fan 342 is fixedly connected to the inside of the ring of the frame 344. The outer surface of the frame 344 is fixedly connected to a push-pull rod 345. The push-pull rod 345 is made of an electric push rod and is electrically connected to an external control circuit. The outer surface of the push-pull rod 345 is fixedly connected to the inside of the inner cavity 341. The outer surface of the frame 344 is fixedly connected to a slide column 346. The slide column 346 is made of the same material as the frame 344. By filling the air hole 343 below, it is convenient for the punch 33 to punch the aluminum foil raw material. The outer surface of the slide column 346 is slidably connected to the inner cavity 341 and the air hole 343 respectively.
[0049] In this embodiment, when the lunch box is stuck outside the punch 33, or the mold base 1 needs to be cleaned, the output end of the push-pull rod 345 retracts to drive the square frame 344 to rise inside the inner cavity 341, thereby driving the sliding column 346 to follow the movement and slide out from the air hole 343, and then the fan 342 works to drive the air inside the inner cavity 341 to be discharged to the outside through the ring of the square frame 344 and the air hole 343, so that the stuck lunch box can be blown off and the waste chips on the mold base 1 can be cleaned, and at the same time, air heat dissipation of the mold base 1 and the angle plate 2 can be achieved on the outside.
[0050] Embodiment 4: Based on Embodiment 3, refer to the attached Figure 1, Attachment Figure 3 ;
[0051] A heat dissipation component 4 is arranged outside the angle plate 2. The heat dissipation component 4 includes a heat dissipation groove 41. The cross section of the heat dissipation groove 41 is T-shaped, and its protruding part is close to the angle plate 2, and the interior is filled with coolant to perform liquid cooling and heat dissipation on the mold base 1 and the angle plate 2. At the same time, the transverse part is arranged horizontally through the mold base 1 body to facilitate air flow for heat dissipation. The heat dissipation groove 41 is opened on the body of the mold base 1 and is in a through state. The interior of the heat dissipation groove 41 is fixedly connected with a partition 42. The partition 42 is made of a corrosion-resistant material with good thermal conductivity. The outer surface of the partition 42 is fixedly connected with a semiconductor cooling sheet 43. The outer surface of the partition 42 is fixedly connected with a fin plate 45. The fin plate 45 is connected with the partition 42. The heat dissipation groove 41 is made of the same material, and a through grille groove is opened on its main body, which is convenient for the circulation of the coolant on the one hand, and further increases the heat dissipation area on the other hand to improve the heat dissipation efficiency. A liquid pump 46 is arranged inside the heat dissipation groove 41, and the liquid pump 46 can drive the coolant to circulate to improve the heat dissipation efficiency of the mold base 1 and the angle plate 2. The interior of the heat dissipation groove 41 is connected with a solid cover 47, and the outer surface of the solid cover 47 is fixedly connected to the outer surface of the mold base 1. The interior of the solid cover 47 is penetrated and connected with a spring tube 48. The cooperation of the spring tube 48 and the solid cover 47 allows the fan 342 to act on the interior of the heat dissipation groove 41, so as to improve the heat dissipation efficiency. One end of the spring tube 48 is penetrated and connected with the interior of the inner cavity 341.
[0052] In this embodiment, after the semiconductor refrigeration plate 43 is energized, the cold end cools down the coolant through the partition plate 42 and the fin plate 45, and the liquid pump 46 drives the coolant to circulate, thereby improving the heat dissipation efficiency of the mold base 1 and the angle plate 2. At the same time, the hot end of the semiconductor refrigeration plate 43 dissipates heat on the other side of the heat dissipation groove 41, and the fan 342 drives the air from the inside of the heat dissipation groove 41 into the inner cavity 341 through the action of the spring tube 48 and the solid cover 47, and is discharged through the air holes 343 on the side wall, thereby improving the heat dissipation efficiency of the hot end through air flow, so that the semiconductor refrigeration plate 43 can be used continuously.
[0053] Embodiment 5: Based on Embodiment 4, refer to the attached Figure 1 , Attachment Figure 4 ;
[0054] A linkage unit 44 is arranged outside the semiconductor cooling sheet 43, and the linkage unit 44 includes a slide rail 441, and the outer surface of the slide rail 441 is fixedly connected to the outer surface of the mold base 1, and the outer surface of the slide rail 441 is slidably connected to a linear motor 442, and the linear motor 442 is electrically connected to an external control circuit, and the outer surface of the linear motor 442 is fixedly connected to a connecting plate 444, and the connecting plate 444 is made of a pressure-resistant and insulating material, and the outer surface of the connecting plate 444 is fixedly connected to a sliding rheostat 443, and the sliding end of the sliding rheostat 443 is fixedly connected to the connecting plate 444, and the input end of the sliding rheostat 443 is electrically connected to the external control circuit. The sliding end is electrically connected to the input end of the liquid pump 46 and the semiconductor cooling plate 43 respectively, the outer surface of the sliding rheostat 443 is fixedly connected to the outer surface of the mold base 1, the outer surface of the linear motor 442 is fixedly connected to the fixed frame 445, the body of the fixed frame 445 is rotatably connected with an I-shaped wheel 446, the I-shaped wheel 446 can improve the stability of the connection between the fixed frame 445 and the sliding sleeve 447, and it is also convenient for the sliding sleeve 447 to rotate synchronously with the lever 11 when the lever 11 is rotated, so as to maintain the adaptability of the two, the outer surface of the I-shaped wheel 446 is fixedly connected to the sliding sleeve 447, and the sliding sleeve 447 is sleeved on the outer surface of the lever 11.
[0055] In this embodiment, when it is necessary to control the adjustment of the angle plate 2 through the lever 11, the linear motor 442 slides along the slide rail 441. Through the cooperation of the fixed frame 445, the I-wheel 446 and the sliding sleeve 447, the lever 11 can be moved to drive the gear ring 5 to rotate, thereby driving the angle plate 2 to move, and at the same time, the connecting plate 444 pushes the sliding end of the sliding rheostat 443 to move synchronously, so as to adjust the power of the liquid pump 46 and the semiconductor refrigeration plate 43, so that the heat dissipation efficiency provided by the power is proportional to the volume of the lunch box, so as to improve the heat dissipation effect when producing lunch boxes of different specifications.
[0056] The present invention also discloses a production process of an aluminum foil lunch box production device, which specifically comprises the following steps:
[0057] Step 1: The gear ring 5 is rotated by the lever 11, and the four angle plates 2 are moved synchronously by the transmission of the gear 6 and the ruler 7, so that the space between the angle plates 2 is adjusted, and then the aluminum foil raw material is placed on the surface of the angle plate 2, and then the output end of the lifting rod 32 is extended to drive the punch 33 to descend, and cooperate with the angle plate 2 to punch the aluminum foil raw material into a lunch box shape, and then the angle plate 2 continues to move to break away from the contact with the lunch box, so as to facilitate the demoulding of the formed lunch box;
[0058] Step 2: When the formed lunch box is stuck outside the punch 33, the output end of the push-pull rod 345 retracts to drive the frame 344 to rise, so that the slide column 346 is free from the blockage of the air hole 343, and then the fan 342 works to blow the formed lunch box down through the air pressure, and the fan 342 extracts the air inside the heat dissipation groove 41 through the spring tube 48 and the solid cover 47, which can dissipate the heat of the hot end of the semiconductor cooling plate 43;
[0059] Step three: The cold end of the semiconductor refrigeration plate 43 cools the coolant through the partition plate 42 and the fin plate 45, and drives the coolant to circulate through the liquid pump 46 to dissipate heat to the mold base 1 and the corner plate 2. At the same time, when the linear motor 442 moves the lever 11 through the sliding sleeve 447 to adjust the size of the space between the corner plates 2, the resistance value of the sliding rheostat 443 is synchronously adjusted through the connecting plate 444, so that the power of the semiconductor refrigeration plate 43 and the liquid pump 46 is adjusted according to the volume of the lunch box.
[0060] Meanwhile, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.
[0061] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A production equipment for aluminum foil lunch boxes, characterized by: include: A mold base (1) for supporting and forming; A deformation mechanism, the deformation mechanism being arranged on the mold base (1), the deformation mechanism comprising four corner plates (2), the outer surfaces of the four corner plates (2) being mutually abutted and all arranged on the mold base (1), the four corner plates (2) being formed by cutting a square plate along two diagonal lines, the four corner plates (2) being able to adjust the size of the central area by horizontally moving along the outer surfaces, and facilitating demoulding of the formed lunch box; A punching assembly (3), wherein the punching assembly (3) is arranged on the die base (1), and punches and forms the aluminum foil material by moving up and down and cooperating with the angle plate (2); A heat dissipation component (4) is provided, wherein the heat dissipation component (4) dissipates heat from the mold base (1) and the angle plate (2) through the flow of a cooling liquid, thereby facilitating continuous production.
2. The production equipment of an aluminum foil lunch box according to claim 1 is characterized in that: The angle plate (2) is sleeved with a gear ring (5) on the outside, the ring of the gear ring (5) is movably connected to a gear (6), the outer surface of the gear (6) is meshed with a ruler plate (7), the outer surface of the ruler plate (7) is fixedly connected to the outer surface of the angle plate (2), the body of the angle plate (2) is provided with a through slide groove (8), the inside of the slide groove (8) is movably connected to a pin rod (9), one end of the pin rod (9) is fixedly connected to the outer surface of the mold base (1), the outer surface of the gear ring (5) is fixedly connected to a swivel (10), the outer surface of the swivel (10) is embedded and rotatably connected to the outer surface of the mold base (1), and the outer surface of the gear ring (5) is fixedly connected to a shift rod (11).
3. The production equipment of an aluminum foil lunch box according to claim 2 is characterized in that: The punching assembly (3) comprises a bracket (31), the outer surface of the bracket (31) is fixedly connected to the outer surface of the die base (1), the outer surface of the bracket (31) is fixedly connected to a lifting rod (32), a punch (33) is arranged outside the output end of the lifting rod (32), the outer surface of the punch (33) is fixedly connected to a screw rod (35), the outer surface of the screw rod (35) is threadedly connected to a screw sleeve (36), and the outer surface of the screw sleeve (36) is fixedly connected to the output end of the lifting rod (32).
4. The production equipment of an aluminum foil lunch box according to claim 3 is characterized in that: A pneumatic unit (34) is arranged on the body of the punch (33), and the pneumatic unit (34) comprises an inner cavity (341), wherein the inner cavity (341) is provided on the body of the punch (33), and a fan (342) is arranged inside the inner cavity (341), and the interior of the inner cavity (341) is connected with an air hole (343), and the air hole (343) is provided on the body of the punch (33) and is in a through-state, and a square frame (344) is slidably connected inside the inner cavity (341), and the outer surface of the fan (342) is fixedly connected to the inside of the ring of the square frame (344).
5. The production equipment of an aluminum foil lunch box according to claim 4, characterized in that: The outer surface of the square frame (344) is fixedly connected to a push-pull rod (345), and the outer surface of the push-pull rod (345) is fixedly connected to the interior of the inner cavity (341). The outer surface of the square frame (344) is fixedly connected to a sliding column (346), and the outer surface of the sliding column (346) is respectively slidably connected to the interior of the inner cavity (341) and the air hole (343).
6. The production equipment of an aluminum foil lunch box according to claim 4, characterized in that: The heat dissipation component (4) comprises a heat dissipation groove (41), the heat dissipation groove (41) is provided on the main body of the mold base (1) and is in a through-state, a partition (42) is fixedly connected inside the heat dissipation groove (41), a semiconductor cooling plate (43) is fixedly connected to the outer surface of the partition (42), a fin plate (45) is fixedly connected to the outer surface of the partition (42), and a liquid pump (46) is arranged inside the heat dissipation groove (41).
7. The production equipment of an aluminum foil lunch box according to claim 6, characterized in that: The interior of the heat dissipation groove (41) is connected to a solid cover (47), the outer surface of the solid cover (47) is fixedly connected to the outer surface of the mold base (1), the interior of the solid cover (47) is connected to a spring tube (48), and one end of the spring tube (48) is connected to the interior of the inner cavity (341).
8. The production equipment of an aluminum foil lunch box according to claim 6, characterized in that: A linkage unit (44) is arranged outside the semiconductor cooling plate (43), and the linkage unit (44) comprises a slide rail (441), the outer surface of the slide rail (441) is fixedly connected to the outer surface of the mold base (1), the outer surface of the slide rail (441) is slidably connected to a linear motor (442), the outer surface of the linear motor (442) is fixedly connected to a connecting plate (444), the outer surface of the connecting plate (444) is fixedly connected to a sliding rheostat (443), and the outer surface of the sliding rheostat (443) is fixedly connected to the outer surface of the mold base (1).
9. The production equipment of an aluminum foil lunch box according to claim 8, characterized in that: The outer surface of the linear motor (442) is fixedly connected to a fixed frame (445), the body of the fixed frame (445) is rotatably connected to an I-shaped wheel (446), the outer surface of the I-shaped wheel (446) is fixedly connected to a sliding sleeve (447), and the sliding sleeve (447) is sleeved on the outer surface of the shifting rod (11).
10. A production process of an aluminum foil lunch box production device, using the aluminum foil lunch box production device according to any one of claims 1 to 9, characterized in that: The specific steps include: Step 1: The gear ring (5) is rotated by the lever (11), and the four angle plates (2) are moved synchronously by the transmission of the gear (6) and the ruler plate (7), so that the space between the angle plates (2) is adjusted, and then the aluminum foil raw material is placed on the surface of the angle plate (2), and then the output end of the lifting rod (32) is extended to drive the punch (33) to descend, and cooperate with the angle plate (2) to punch the aluminum foil raw material into a lunch box shape, and then the angle plate (2) continues to move to break away from the contact with the lunch box, so as to facilitate the demoulding of the formed lunch box; Step 2: When the formed lunch box is stuck outside the punch (33), the output end of the push-pull rod (345) retracts to drive the frame (344) to rise, so that the slide column (346) is freed from the blockage of the air hole (343), and then the fan (342) works to blow the formed lunch box off through the action of air pressure, and the fan (342) draws air from the heat dissipation groove (41) through the spring tube (48) and the solid cover (47), so as to dissipate heat from the hot end of the semiconductor cooling plate (43); Step three: The cold end of the semiconductor refrigeration plate (43) cools the coolant through the partition (42) and the fin plate (45), and drives the coolant to circulate through the liquid pump (46) to dissipate heat from the mold base (1) and the corner plate (2). At the same time, when the linear motor (442) moves the lever (11) through the sliding sleeve (447) to adjust the size of the space between the corner plates (2), the resistance of the sliding rheostat (443) is synchronously adjusted through the connecting plate (444), so that the power of the semiconductor refrigeration plate (43) and the liquid pump (46) is adjusted according to the size of the lunch box.
Citation Information
Patent Citations
Cold stamping die for aluminium foil container
CN101758139A
Pipe extruding machine for spiral flat pipe
CN102744306A
Forming processing equipment based on aluminum foil meal box
CN116393574A
Cutting edge cooling device for high-speed precision stamping die
CN219786303U
Metallic vacuum double-walled container and manufacturing method thereof
EP0603613A1