External water nozzle base and machining method thereof

Through the external water nozzle base and its processing method, the water nozzle is formed using aluminum profiles and CNC lathes, which solves the problems of cumbersome processing of liquid-cooled plate water nozzles and waste of materials, and realizes simple installation and low-cost processing, meeting the runner requirements .

CN119304539APending Publication Date: 2025-01-14JIANGSU WEITENG COPPER CO LTD

Patent Information

Application Number
CN202411722949.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-28
Publication Date
2025-01-14

AI Technical Summary

Technical Problem

The existing liquid-cooled plate water nozzle processing methods have problems such as cumbersome design welding, difficult cost control and waste of materials, especially during small-piece processing.

Method used

The external water nozzle base and its processing method are adopted. The prototype base block is cut through aluminum profiles, and the CNC lathe is processed by machining the connection holes and inserts. The front plate and base welding are combined to form the water nozzle to avoid opening the original liquid-cooled plate and realize simple installation. and low cost processing.

Benefits of technology

It simplifies the installation process of the water nozzle, avoids material waste, reduces the cost of small parts processing, and effectively controls the length and weight of the liquid-cooled plate to meet the runner requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119304539A_ABST
    Figure CN119304539A_ABST
Patent Text Reader

Abstract

The invention discloses an external water nozzle base and a processing method thereof, the external water nozzle base is applied to the field of machining, the external water nozzle base comprises a liquid cooling plate, a rear plate, a front plate, a front cross beam and two side plates, and the two side plates are symmetrically and fixedly connected to the top of the liquid cooling plate; the rear plate and the front plate are symmetrically and fixedly connected to the top of the liquid cooling plate, and the two ends of the rear plate and the two ends of the front plate are fixedly connected with the two side plates respectively. Two inserting grooves are machined in one side of the front plate, inserting blocks are inserted into the two inserting grooves, two bases are arranged on one side of the front plate, and the two bases and the two inserting blocks are integrally machined. The side, close to the front plate, of the base is welded to the front plate. A connecting hole is further machined in the base. According to the external water nozzle base, the length and the weight of the liquid cooling plate are effectively controlled, the external water nozzle base is welded to the front plate of the liquid cooling plate, the requirement of a flow channel is met, overall machining is easy, and waste of materials in the machining process is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of mechanical processing, and in particular to an external faucet base and a processing method thereof. Background Art

[0002] At present, similar liquid cooling plates are mostly made by drilling holes in the liquid cooling plate and welding water nozzles, or by machining the water nozzle flow channel on a solid block and then welding the water nozzle. The former is cumbersome to design and weld, and cost control is difficult, while the latter takes a long time to machine and wastes materials. In order to solve the above problems, we propose an external water nozzle base and a processing method thereof. Summary of the invention

[0003] The purpose of the present invention is to provide an external faucet base and a processing method thereof, which has the advantage of being easy to process.

[0004] The above technical objectives of the present invention are achieved through the following technical solutions: an external faucet base and a processing method thereof, comprising a liquid cooling plate, a rear plate, a front plate, a front crossbeam and two side plates, wherein the two side plates are symmetrically fixedly connected to the top of the liquid cooling plate; the rear plate and the front plate are symmetrically fixedly connected to the top of the liquid cooling plate, and the two ends of the rear plate and the front plate are respectively fixedly connected to the two side plates; One side of the front plate is processed with two slots, and plug blocks are inserted into the two slots. One side of the front plate is provided with two bases, and the two bases are respectively processed integrally with the two plug blocks; The side of the base close to the front plate is welded to the front plate; A connecting hole is processed inside the base, a water nozzle is inserted inside the connecting hole, and the bottom of the water nozzle is welded to the base.

[0005] By adopting the above technical solution, a connection is formed by using a base, an insert, a water nozzle and a front plate externally connected, and there is no need to drill holes in the original liquid cold plate, making the installation of the water nozzle easier. At the same time, the original liquid cold plate is not processed and there will be no waste of materials. In addition, the processing cost of small parts is lower.

[0006] A method for processing an external faucet base comprises the following steps: S1: Prepare aluminum profiles for processing the base and connecting holes. The length of the aluminum profiles must be at least greater than the sum of the lengths of the two bases and the connecting holes. Cut the aluminum profile according to the length of the drawing. The size of the cut single aluminum profile should include the length of the base and the plug-in block. After cutting, you will get a prototype base block. A single liquid cooling plate needs to be equipped with at least two prototype base blocks, so the aluminum profile needs to be cut into two prototype base blocks of the same size. S2: Move the two prototype base blocks that have been cut to the CNC lathe in turn, and use the CNC lathe to process connecting holes on the two prototype base blocks in turn; the diameter of the connecting hole must be consistent with the diameter of the faucet; according to the length of the plug block on the drawing, the shape drawing of the plug block is milled by the CNC lathe and can be changed according to the size requirements; S3: Mill two slots at the position where the front plate needs to be welded to the base; the size of the slots must be consistent with the size of the insert; S4: insert the two plug-ins into the two slots in sequence, at which point the plug-in on one side of the base is inserted into the slot, the side of the base close to the front plate contacts the front plate, and the side of the base close to the front plate is welded to the front plate; after welding, the bottom welding position of the base and the plug-in is polished so that the base and the bottom of the front plate are on the same horizontal line; S5: Connect the two water nozzles to the two connection holes in sequence, weld the contact position between the water nozzle and the base to form a whole, and complete the processing.

[0007] In summary, the present invention has the following beneficial effects: The external faucet base of the present invention effectively controls the length and weight of the liquid cooling plate, meets the requirements of the flow channel by being welded with the front plate of the liquid cooling plate, is easy to process as a whole, and does not generate waste of materials during processing. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figure 1 It is a schematic diagram of the structure of the present invention; Figure 2 is a schematic diagram of the front panel and slot of the present invention; Figure 3 It is a schematic diagram of the connection between the base and the plug block of the present invention; Figure 4 is a cross-sectional view of the front plate of the present invention; Figure 5 It is a processing flow chart of the present invention.

[0009] Figure numerals: 1, liquid cooling plate; 2, rear plate; 3, front plate; 4, front cross beam; 5, side plate; 6, slot; 7, plug-in block; 8, base; 9, connecting hole; 10, water nozzle. DETAILED DESCRIPTION

[0010] The present invention is further described in detail below in conjunction with the accompanying drawings.

[0011] Embodiment 1: refer to Figure 1-Figure 5, an external faucet base, comprising a liquid cooling plate 1, a rear plate 2, a front plate 3, a front crossbeam 4 and two side plates 5, characterized in that: the two side plates 5 are symmetrically fixedly connected to the top of the liquid cooling plate 1; the rear plate 2 and the front plate 3 are symmetrically fixedly connected to the top of the liquid cooling plate 1, and the two ends of the rear plate 2 and the front plate 3 are respectively fixedly connected to the two side plates 5; one side of the front plate 3 is processed with two slots 6, and the two slots 6 are plugged with plug blocks 7 inside, and one side of the front plate 3 is provided with two bases 8, and the two bases 8 are respectively processed integrally with the two plug blocks 7; the side of the base 8 close to the front plate 3 is welded to the front plate 3; a connecting hole 9 is also processed inside the base 8, and a faucet 10 is plugged inside the connecting hole 9, and the bottom of the faucet 10 is welded to the base 8; the external faucet base effectively controls the length and weight of the liquid cooling plate 1, and meets the requirements of the flow channel by welding with the front plate 3 of the liquid cooling plate 1, and the overall processing is simple and does not generate waste of materials during processing.

[0012] A method for processing an external faucet base comprises the following steps: S1: Prepare an aluminum profile for processing the base 8 and the connecting hole 9, the length of the aluminum profile must be at least greater than the sum of the lengths of the two bases 8 and the connecting holes 9; Cut the aluminum profile according to the length of the drawing. The size of the cut single aluminum profile should include the sum of the length of the base 8 and the plug 7. After cutting, a prototype base block is obtained. A single liquid cooling plate 1 needs to be equipped with at least two prototype base blocks, so the aluminum profile needs to be cut into two prototype base blocks of the same size. S2: The two prototype base blocks that have been cut are moved to the CNC lathe in sequence, and the connecting holes 9 are processed in sequence on the two prototype base blocks by the CNC lathe; the diameter of the connecting hole 9 is required to be consistent with the diameter of the faucet 10; according to the length of the plug block 7 on the drawing, the shape drawing of the plug block 7 is milled by the CNC lathe and can be changed according to the size requirements; S3: Mill two slots 6 at the position where the front plate 3 needs to be welded to the base 8; the size of the slots 6 must be consistent with the size of the insert 7; S4: insert the two plug blocks 7 into the two slots 6 in sequence, at which time the plug block 7 on one side of the base 8 is inserted into the slot 6, the side of the base 8 close to the front plate 3 is in contact with the front plate 3, and the side of the base 8 close to the front plate 3 is welded to the front plate 3; after welding, the bottom welding position of the base 8 and the plug block 7 is polished so that the base 8 and the bottom of the front plate 3 are on the same horizontal line; S5: Insert the two water nozzles 10 into the two connection holes 9 in sequence, weld the contact position between the water nozzle 10 and the base 8 to form a whole, and complete the processing.

[0013] This specific embodiment is merely an explanation of the present invention and is not a limitation of the present invention. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed. However, as long as they are within the scope of the claims of the present invention, they are protected by the patent law.

Claims

1. An external faucet base, comprising a liquid cooling plate (1), a rear plate (2), a front plate (3), a front crossbeam (4) and two side plates (5), characterized in that: The two side plates (5) are symmetrically fixedly connected to the top of the liquid cooling plate (1); the rear plate (2) and the front plate (3) are symmetrically fixedly connected to the top of the liquid cooling plate (1), and the two ends of the rear plate (2) and the front plate (3) are respectively fixedly connected to the two side plates (5); One side of the front plate (3) is processed with two slots (6), and the insides of the two slots (6) are plugged with plug blocks (7); one side of the front plate (3) is provided with two bases (8), and the two bases (8) are respectively processed integrally with the two plug blocks (7); The side of the base (8) close to the front plate (3) is welded to the front plate (3); A connection hole (9) is also machined inside the base (8), a water nozzle (10) is inserted into the connection hole (9), and the bottom of the water nozzle (10) is welded to the base (8).

2. The method for processing an external faucet base according to claim 1, characterized in that: The following steps are involved: S1: preparing an aluminum profile for processing the base (8) and the connecting hole (9), wherein the length of the aluminum profile must be at least greater than the sum of the lengths of the two bases (8) and the connecting hole (9); The aluminum profile is cut according to the length of the drawing. The size of the cut single aluminum profile should include the sum of the length of the base (8) and the plug (7). After cutting, a prototype base block is obtained. A single liquid cooling plate (1) needs to be equipped with at least two prototype base blocks, so the aluminum profile needs to be cut into two prototype base blocks of the same size. S2: The two prototype base blocks that have been cut are moved to a CNC lathe in sequence, and the connecting holes (9) are processed in sequence on the two prototype base blocks by the CNC lathe; the diameter of the connecting hole (9) is required to be consistent with the diameter of the water nozzle (10); according to the length of the plug block (7) on the drawing, the shape of the plug block (7) is milled out by the CNC lathe (the drawing can be changed according to the size requirements); S3: Milling out the shapes of two slots (6) at the positions where the front plate (3) needs to be welded to the base (8); the size of the slots (6) is required to be consistent with the size of the insert (7); S4: inserting the two plug blocks (7) into the two slots (6) in sequence, at which time the plug block (7) on one side of the base (8) is inserted into the slot (6), and the side of the base (8) close to the front plate (3) is in contact with the front plate (3), and the side of the base (8) close to the front plate (3) is welded to the front plate (3); after welding, the bottom welding position of the base (8) and the plug block (7) is polished so that the bottom of the base (8) and the front plate (3) are on the same horizontal line; S5: plugging the two water nozzles (10) into the two connection holes (9) in sequence, and welding the contact positions of the water nozzles (10) and the base (8) to form a whole, thereby completing the processing.

Citation Information

Patent Citations

  • Embedded roller structure in energy storage battery box and processing and mounting method thereof

    CN118919983A

  • Integrated battery box body, battery pack and electric equipment

    CN219123351U

  • Battery box and battery pack

    CN220963576U

  • Water nozzle structure of profile liquid cooling plate

    CN221080122U

  • Battery module

    US20210313643A1

Cited By

  • Flat plate type energy storage box body machining method

    CN120023600A