A polysiloxane-modified polyferric flocculant, its preparation method and application

By constructing a three-dimensional network structure using polysiloxane-modified polyferric flocculant and utilizing the synergistic effect of multiple chemical bonds, the problem of poor performance of traditional flocculants in papermaking wastewater treatment is solved, achieving efficient removal of suspended solids and organic pollutants, and improving the stability and economy of the flocculant.

CN120483359BActive Publication Date: 2026-11-10NANJING UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202510703799.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-05-29
Publication Date
2026-11-10
Estimated Expiration
2045-05-29

AI Technical Summary

Technical Problem

Existing flocculants have several drawbacks when treating papermaking wastewater, including sensitivity to water quality, susceptibility to fluctuations in environmental conditions, limited treatment effectiveness, and the potential for residual toxic substances. They are not efficient at removing suspended solids and organic pollutants from papermaking wastewater.

Method used

Polyferric flocculants modified with polysiloxanes are used to construct a three-dimensional network structure by forming a stable iron-imidazolium coordination complex and crosslinking with functionalized polysiloxanes. This structure achieves efficient flocculation and sedimentation through the synergistic effect of multiple chemical bonds.

Benefits of technology

It improves the removal efficiency of suspended solids and organic pollutants, enhances floc strength and solid-liquid separation speed, reduces the risk of secondary pollution, and improves treatment efficiency and economy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120483359B_ABST
    Figure CN120483359B_ABST
Patent Text Reader

Abstract

This invention discloses a novel polysiloxane-modified polyferric flocculant, its preparation method, and its application, belonging to the field of wastewater treatment agent preparation technology. This invention uses polysiloxane as the main chain material, introducing imidazole groups to combine with ferric ions to form a stable imidazole-ferric coordination complex. This complex is then bonded to the functionalized polysiloxane via hydrogen bonding to form a high-molecular-weight network composite material. The polysiloxane chain structure not only provides a high molecular weight but also enhances the stability and mechanical strength of the flocculant. When treating wastewater containing high concentrations of pollutants, the flocculant of this invention can effectively adsorb and aggregate pollutants through coordination bonds and hydrogen bonds, forming large and strong flocs. Compared with traditional flocculants, the flocculant of this invention has a faster floc formation rate, a higher settling rate, and a better turbidity removal effect, making it particularly suitable for papermaking wastewater treatment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of wastewater treatment agent preparation technology, specifically relating to a polysiloxane-modified polyferric flocculant, its preparation method, and its application. Background Technology

[0002] Currently, with the continuous expansion of the paper industry, the discharge of large amounts of papermaking wastewater has become a major challenge for environmental governance. Papermaking wastewater typically has high color, high chemical oxygen demand (COD), high suspended solids, and a complex composition of organic pollutants, especially containing recalcitrant lignin derivatives and chlorinated organic compounds. These characteristics make it poorly biodegradable and toxic, making it difficult to treat.

[0003] Currently, the main methods for treating papermaking wastewater include physical, chemical, and biological methods. Physical methods (such as screening, sedimentation, and membrane filtration) are mainly for large suspended particles, but their effectiveness in removing dissolved organic matter and color is limited. Chemical methods (such as oxidation, adsorption, and coagulation / precipitation) can effectively degrade some organic matter and remove color, but they are often accompanied by high energy consumption, the generation of reaction byproducts, and the risk of secondary pollution. Biological methods (such as activated sludge processes and sequencing batch reactors) are environmentally friendly and have lower costs, but they are affected by recalcitrant substances in the wastewater, have long reaction cycles, and poor stability.

[0004] Among numerous treatment methods, flocculation is widely used in papermaking wastewater treatment due to its simplicity and cost-effectiveness. Its principle involves adding flocculants to neutralize the negative charge on the surface of suspended particles, achieving adsorption bridging, and causing tiny particles to aggregate into large flocs, facilitating solid-liquid separation. Commonly used flocculants include polyferric sulfate, polyaluminum chloride, polyacrylamide (PAM), and organic-inorganic composite flocculants. These materials achieve flocculation through coordination bonds, hydrogen bonds, and dipole interactions. However, these traditional flocculants have several shortcomings: they are sensitive to pH and ionic strength in the water, and their flocculation efficiency is easily affected by fluctuations in environmental conditions; some flocculants may leave behind toxic metal ions or polymers after treatment, increasing the difficulty of subsequent treatment; furthermore, traditional polymeric flocculants have a simple structure and lack the synergistic effect of multifunctional functional groups, limiting their adsorption and bridging capabilities when facing complex organic pollutants in papermaking wastewater, thus requiring improvement in overall treatment efficiency and economics. Summary of the Invention

[0005] This invention provides a polysiloxane-modified polyferric flocculant, its preparation method, and its application. The prepared flocculant contains coordination bonds, hydrogen bonds, and slight condensation covalent bonds. The synergistic effect of multiple chemical bonds results in a high-density distribution of active sites, thereby possessing excellent adsorption bridging ability, rapid flocculation and sedimentation characteristics, and can efficiently remove organic pollutants and suspended solids from papermaking wastewater.

[0006] To achieve the above objectives, the present invention adopts the following technical solution:

[0007] A polysiloxane-modified polyferric flocculant, using polysiloxane as the chain-like main material, introduces ferric ions to combine with imidazole groups to form a stable iron-imidazolium coordination complex. Simultaneously, through the crosslinking reaction of functionalized polysiloxane with the complex, a highly stable three-dimensional network structure is constructed. The specific structure is as follows:

[0008] .

[0009] The preparation method of the above-mentioned polysiloxane-modified polyferric flocculant includes the following steps:

[0010] Preparation of iron ion solution;

[0011] Add imidazole to the iron ion solution and stir at 400 rpm for 1 to 2 hours at 25 to 30°C to generate a stable imidazole-iron complex.

[0012] Tetraethoxysilane (TEOS) was dissolved in a solvent, and ethylene glycol was added as a catalyst. The mixture was stirred continuously at 300 rpm for 4 hours at 35–40 °C to obtain a functionalized polysiloxane solution.

[0013] The imidazole-iron complex was mixed with a functionalized polysiloxane solution and stirred at 300 rpm for 2 to 4 hours at 30 to 40°C to allow the two to react chemically and construct a polyferric flocculant with a highly stable three-dimensional network structure.

[0014] In the steps described above, the molar ratio of imidazole to iron ions is (30-60):(10-15), preferably 45:12;

[0015] When dissolving tetraethoxysilane, a mixed solvent of water and ethanol at a volume ratio of 1:1 is used; the volume ratio of the imidazole-iron complex to the functionalized polysiloxane solution is (1-2):(1-2), preferably 1:1, and the molar ratio of ethylene glycol to tetraethoxysilane is 1:100.

[0016] The polysiloxane-modified polyferric flocculant prepared above can be used for the treatment of papermaking wastewater. The unique three-dimensional network structure and multiple chemical bonds (including coordination bonds, hydrogen bonds and slight condensation covalent bonds) of the flocculant can achieve efficient adsorption, rapid flocculation and sedimentation in wastewater treatment, effectively improving the removal efficiency of suspended solids and organic pollutants.

[0017] Beneficial effects: This invention provides a polysiloxane-modified polyferric flocculant, its preparation method, and its application, which have the following advantages compared with the prior art:

[0018] 1. The efficient bridging effect of the three-dimensional mesh structure

[0019] This invention constructs a dense three-dimensional network structure by forming a stable coordination complex between imidazole groups and ferric ions, and then crosslinking it with functionalized polysiloxanes. This structure has a large number of dispersed active sites, which can bridge multiple suspended particles at the same time. This not only enhances the physical adsorption and crosslinking between particles, but also forms large and dense flocs, resulting in faster solid-liquid separation and higher floc strength.

[0020] 2. Multiple chemical bonds synergistically enhance adsorption and cross-linking capabilities.

[0021] The flocculant prepared by this invention simultaneously possesses coordinate bonds (Fe-N bonds), hydrogen bonds (between hydroxyl and imidazole groups), and covalent condensation bonds. These different types of chemical bonds coexist, forming a multi-point, multi-layered bonding network. Coordinate bonds provide a strongly stable metal-organic framework, while hydrogen bonds play a flexible regulatory role. This multi-bond synergy greatly enhances the ability to capture and immobilize organic matter, colloids, and metal ions, thereby achieving highly efficient flocculation through multiple mechanisms of action.

[0022] 3. Environmental adaptability and durability of functionalized polysiloxane backbone

[0023] Polysiloxane, as the chain-like host, not only endows the material with high molecular weight and excellent temperature and acid / alkali resistance, but also, through the introduction of hydrophilic functional groups such as hydroxyl groups, enables the entire material to maintain a stable structure under different pH and ionic strengths. The synergistic effect of multiple functional groups enhances the binding with the imidazole-iron complex, while also ensuring that the flocculant maintains excellent long-term stability and reusability under complex water quality conditions.

[0024] 4. Multiple mechanisms of action achieve high-density distribution of active sites

[0025] This invention simultaneously introduces imidazole, an iron center, and a siloxane chain within a single molecule. This design imbues each polymerization unit with multiple active functions. The metal center improves the surface charge of suspended particles through charge neutralization, the imidazole group provides coordination and hydrogen bonding, and the siloxane skeleton forms a broad physical network. This multi-functional mechanism results in a highly uniform and dense distribution of active sites at the molecular level, thereby exhibiting excellent adsorption bridging capabilities, rapid flocculation and sedimentation characteristics, significantly improving flocculation efficiency, and effectively removing organic pollutants and suspended solids from papermaking wastewater. Through dual optimization of structure and function, this invention significantly improves the treatment efficiency of flocculants in papermaking wastewater treatment applications, reduces the risk of secondary pollution, and effectively saves operating costs, achieving efficient, environmentally friendly, and sustainable wastewater treatment. Attached Figure Description

[0026] Figure 1This is a reaction mechanism diagram of the preparation method of the present invention;

[0027] Figure 2 This is a practical diagram of Embodiment 1 of the present invention;

[0028] Figure 3 This is a practical illustration of Embodiment 2 of the present invention;

[0029] Figure 4 This is a practical diagram of Embodiment 3 of the present invention. Detailed Implementation

[0030] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments:

[0031] Example 1

[0032] A method for preparing a polysiloxane-modified polyferric flocculant includes the following steps:

[0033] 12 parts of ferric chloride hexahydrate were dissolved in deionized water, and an appropriate amount of hydrochloric acid was added to adjust the pH to about 4.5 to obtain an iron ion solution. 45 parts of imidazole were added to the above iron ion solution and stirred at 400 rpm for 1 to 2 hours at 25 to 30°C to generate a stable imidazole-iron complex. 20 parts of tetraethoxysilane (TEOS) were dissolved in a mixed solvent of deionized water and ethanol (1:1 volume ratio), and after adjusting the pH to about 4.5, 0.2 parts of ethylene glycol were added as a catalyst. The mixture was stirred at 300 rpm for 4 hours at 35 to 40°C to form a functionalized polysiloxane solution. The imidazole-iron complex obtained in step (2) was mixed with the polysiloxane solution in step (3) at a 1:1 volume ratio and stirred at 300 rpm for 2 to 4 hours at 30 to 40°C to carry out a cross-linking reaction, and finally a highly cross-linked polyferric flocculant was obtained. Finally, the reaction solution was cooled and filtered to obtain the novel polyferric flocculant.

[0034] Example 2

[0035] A method for preparing a polysiloxane-modified polyferric flocculant includes the following steps:

[0036] 15 parts of ferric chloride hexahydrate were dissolved in deionized water and the pH was adjusted to about 4.5 with dilute hydrochloric acid to obtain an iron ion solution. 30 parts of imidazole were added to the above solution and stirred at 400 rpm for 1 to 2 hours at 25 to 30°C to generate an imidazole-iron complex. 15 parts of tetraethoxysilane (TEOS) were dissolved in a mixed solvent of deionized water and ethanol (1:1), the pH was adjusted to about 4.5, and 0.15 parts of ethylene glycol were added as a catalyst. The mixture was stirred at 300 rpm for 4 hours at 35 to 40°C to form a functionalized polysiloxane solution. The imidazole-iron complex obtained in step (2) was mixed with the polysiloxane solution in step (3) at a volume ratio of 1:1 and stirred at 300 rpm for 2 to 4 hours at 30 to 40°C to carry out a crosslinking reaction, and finally, a polyferric flocculant was obtained. After the reaction was completed, the system was cooled and filtered to obtain a novel polyferric flocculant.

[0037] Example 3

[0038] A method for preparing a polysiloxane-modified polyferric flocculant includes the following steps:

[0039] 10 parts of ferric chloride hexahydrate were dissolved in deionized water and the pH was adjusted to about 4.5 to obtain an iron ion solution. 60 parts of imidazole were added to the above solution and stirred at 400 rpm for 1 to 2 hours at 25 to 30°C to generate an imidazole-iron complex. 25 parts of tetraethoxysilane (TEOS) were dissolved in a mixed solvent of deionized water and ethanol (1:1), the pH was adjusted to about 4.5, and 0.25 parts of ethylene glycol were added as a catalyst. The mixture was stirred at 300 rpm for 4 hours at 35 to 40°C to form a functionalized polysiloxane solution. The imidazole-iron complex obtained in step (2) was mixed with the polysiloxane solution in step (3) at a volume ratio of 1:1 and stirred at 300 rpm for 2 to 4 hours at 30 to 40°C to carry out a crosslinking reaction, and finally, a polyferric flocculant was obtained. Finally, the reaction system was cooled and filtered to obtain a novel polyferric flocculant.

[0040] The flocculant prepared in the above examples and the traditional PAC were used for papermaking wastewater treatment, with the mass ratio of the flocculant concentrate to the raw slurry both being 50,000 ppm. The initial COD of the papermaking wastewater was 7642 mg / L, and the initial SS was 6943 mg / L.

[0041] Taking Example 1 as an example, under optimal reaction conditions, the effluent COD and SS were 2941 and 351 mg / L, respectively. At this time, the flocculation time was 45 min, the dosage was 400 mg / L, and the pH was 7.6. Therefore, Examples 1, 2, 3, and 4 were compared under optimal operating conditions, and the comparison results are shown in Table 1 (unit: mg / L).

[0042] Table 1. Effluent COD and SS of wastewater treated with different flocculants

[0043]

[0044] Table 1 shows that the removal rates of various indicators of the novel modified polyferric flocculant in Examples 1, 2, and 3 are compared with those of the traditional PAC, as shown in Table 2.

[0045] Table 2. COD and SS removal rates of wastewater treated with different flocculants

[0046]

[0047] The comparative experimental results show that the novel polyferric flocculants prepared in Examples 1, 2, and 3 are significantly superior to traditional PAC in terms of papermaking wastewater treatment, with Example 1 showing the best performance. Example 1 uses an imidazole to ferric chloride hexahydrate molar ratio of 45:12 and a TEOS content of 20, which ensures the full formation of the iron-imidazolium complex and allows for uniform mixing of the functionalized polysiloxane solution and the complex. The resulting three-dimensional network structure is neither too sparse nor too dense, resulting in a highly uniform and dense distribution of active sites at the molecular level, thus achieving optimal adsorption bridging and sedimentation effects. In contrast, the lower molar ratio (30:10) in Example 2 leads to fewer active sites, resulting in a decrease in flocculation effect; while the higher molar ratio (60:15) in Example 3 generates more active sites, the overly dense system may cause some functional groups to deactivate, reducing overall performance. In summary, the preparation method of Example 1 is optimal, providing a highly efficient, stable, economical, and environmentally friendly solution for papermaking wastewater treatment.

[0048] The above are merely preferred embodiments of the present invention, which will help those skilled in the art to further understand the present invention, but do not limit the present invention in any way. It should be noted that for those skilled in the art, any modifications and improvements made without departing from the concept of the present invention are protected by the present invention.

Claims

1. A polysiloxane-modified polyferric flocculant, characterized in that, Using polysiloxane as the chain matrix, ferric ions are introduced to combine with imidazole groups to form a stable iron-imidazolium coordination complex, which is then bonded to the functionalized polysiloxane via hydrogen bonds to form a three-dimensional network structure; the structure of the flocculant is as follows: 。 2. A method for preparing the polysiloxane-modified polyferric flocculant according to claim 1, characterized in that, Includes the following steps: Preparation of iron ion solution; Imidazole is added to an iron ion solution, wherein the molar ratio of imidazole to iron ions is (30-60):(10-15), and the mixture is stirred to generate an imidazole-iron complex. Tetraethoxysilane was dissolved in a solvent, and a catalyst was added. The mixture was stirred continuously to obtain a functionalized polysiloxane solution. The imidazole-iron complex and the functionalized polysiloxane solution are mixed in a volume ratio of (1-2):(1-2) to react and form a polyferric flocculant with a three-dimensional network structure.

3. The method for preparing the polysiloxane-modified polyferric flocculant according to claim 2, characterized in that, The iron ion solution is formed by dissolving ferric chloride hexahydrate in deionized water.

4. The method for preparing the polysiloxane-modified polyferric flocculant according to claim 2, characterized in that, The reaction temperature for generating the imidazole-iron complex is 25–30 °C, the reaction time is 1–2 hours, and the stirring speed is 400 rpm.

5. The method for preparing the polysiloxane-modified polyferric flocculant according to claim 2, characterized in that, The reaction temperature for preparing the functionalized polysiloxane solution was 35–40 °C, the reaction time was 4 hours, and the stirring speed was 300 rpm; the molar ratio of the catalyst to tetraethoxysilane was 1:

100.

6. The method for preparing the polysiloxane-modified polyferric flocculant according to claim 2, characterized in that, The reaction temperature of the imidazole-iron complex with the functionalized polysiloxane solution is 30-40°C, the reaction time is 2-4 hours, and the stirring speed is 300 rpm.

7. The method for preparing the polysiloxane-modified polyferric flocculant according to claim 2, characterized in that, The catalyst is ethylene glycol.

8. The application of the polysiloxane-modified polyferric flocculant according to claim 1, characterized in that, The polyferric flocculant is used for the treatment of papermaking wastewater.

Citation Information

Patent Citations

  • Preparing method for polymeric ferric silicate polymolecular flocculant

    CN105152297A

  • Guar gum-inorganic salt hybrid green flocculant and preparation method thereof

    CN112919602A