Argon arc welding apparatus and welding method for large-sized curved thin-walled parts
By employing alternating odd and even pressure and elastic component compensation technology in argon arc welding equipment, the challenges of welding positioning and gap control for large-sized curved thin-walled parts were solved, achieving high-precision and low-cost welding results.
Patent Information
- Application Number
- CN202611302022.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-10
AI Technical Summary
In the argon arc welding process of large-sized curved thin-walled parts, there are problems such as poor versatility in positioning and gap control, high cost, and difficulty in ensuring welding accuracy. In particular, cumulative errors and plastic deformation are easily generated in the segmented pressure operation.
An argon arc welding device is used, including a tooling base, a lower mold, an upper mold, an elastic element, and a pressure element. By using an alternating odd and even pressure method, combined with the flexibility compensation of the elastic element and multi-parameter coupled torque calculation, the adaptive correction of the welding gap and the uniform transmission of the pressure are achieved.
It improves the welding precision and quality stability of large-sized curved thin-walled parts, avoids deformation problems caused by rigid pressure, and ensures the accuracy and consistency of the welding process.
Smart Images

Figure CN123060211A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of argon arc welding technology, specifically to an argon arc welding apparatus and welding method for large-sized curved thin-walled parts. Background Technology
[0002] Large-sized, curved, thin-walled parts are widely used in precision manufacturing fields such as aerospace and high-end equipment due to their advantages such as lightweight structure and strong spatial adaptability. The welding quality of these parts directly affects the structural strength and operational stability of the entire machine. Argon arc welding is the mainstream welding process for these parts. It is necessary to strictly control the weld gap to avoid defects such as incomplete penetration and porosity. However, due to the structural characteristics of the parts and the limitations of traditional processing methods, the current welding process still faces many technical bottlenecks.
[0003] In traditional welding processes, large-sized curved thin-walled parts are often positioned and fixed using integral conformal tooling. This type of tooling needs to be custom-made to perfectly fit the curved contour of the part, which not only makes mold design and manufacturing difficult and time-consuming, but also consumes a lot of materials, resulting in a significant increase in production costs. At the same time, tooling needs to be designed separately for parts with different curvatures and sizes, resulting in poor versatility and difficulty in meeting the needs of multi-variety, small-batch production.
[0004] To address the limitations of integral conformal tooling, the industry has gradually adopted segmented pressurization welding fixtures. However, two major challenges exist in actual pressurization operations. Firstly, there's the challenge of controlling the pressurization sequence: while continuous pressurization at each segment ensures the weld gap at the arc-starting end meets requirements, cumulative errors can easily occur during subsequent segmented pressurization, leading to uncontrolled weld gaps at the end and failing to meet welding accuracy. Conversely, if the head and tail sections are pressed and fixed first, the lack of effective constraint in the middle area causes thermal deformation of the part to concentrate at a certain point in the weld, resulting in localized arching and misalignment, ultimately leading to weld discontinuity and severely impacting welding quality. Secondly, there's the challenge of controlling the pressurization pressure: segmented fixtures typically achieve pressurization through screw tightening. Directly tightening the screws to a fixed position can cause excessive local pressure, leading to plastic deformation of curved, thin-walled parts, compromising the original contour accuracy, and causing stress concentration in the weld, which can easily result in cracks and other failures.
[0005] Therefore, the inventors have provided an argon arc welding apparatus and welding method for large-sized curved thin-walled parts. Summary of the Invention
[0006] (1) Technical problems to be solved This invention provides an argon arc welding device and welding method for large-sized curved thin-walled parts, solving the technical problems of poor versatility, high cost, and difficulty in guaranteeing welding accuracy in the positioning and gap control of argon arc welding of large-sized curved thin-walled parts.
[0007] (2) Technical solution This invention provides an argon arc welding device for large-sized curved thin-walled parts, including a tooling base, a base reinforcing rib, a lower die, an upper die, an elastic element, and a pressure element. The lower die is installed on the tooling base through the base reinforcing rib and is used to support the lower surface of the workpiece to be welded. The upper die covers the upper surface of the workpiece to be welded and is installed in conjunction with the lower die to clamp the workpiece to be welded. A plurality of pressure elements are sequentially spaced through the upper die and compress the workpiece to be welded through the elastic element.
[0008] Furthermore, the argon arc welding device also includes an upper mold hanger, which is installed on the upper end face of the upper mold.
[0009] Furthermore, the argon arc welding apparatus also includes a workpiece protection plate, through which the elastic element contacts the upper surface of the workpiece to be welded.
[0010] Furthermore, the elastic element is a spring.
[0011] Furthermore, the pressure-applying component is a screw.
[0012] Furthermore, the upper mold has multiple threaded holes, and the pressure member passes through the threaded holes.
[0013] The present invention also provides a welding method using the above-mentioned argon arc welding apparatus for large-sized curved thin-walled parts, comprising the following steps: Place the workpiece to be welded on the top surface of the lower mold and adjust the position of the workpiece to ensure that the weld seam is aligned with the preset welding path. The upper mold is attached and covered to the upper surface of the workpiece to be welded; Each pressure point on the workpiece to be welded is pressurized twice using an alternating odd and even pressure method. After the two pressurization processes are completed, spot welding is performed using argon arc welding. Then, the workpiece to be welded is welded according to the preset welding path until the weld cools to room temperature.
[0014] Furthermore, during the first pressurization, each pressurizing component is tightened point by point in the order of odd-numbered points, and then each pressurizing component is tightened point by point in the order of even-numbered points.
[0015] Furthermore, during the second pressurization, each pressurizing component is tightened point by point in the order of odd-numbered points, and then each pressurizing component is tightened point by point in the order of even-numbered points.
[0016] Furthermore, during the first pressurization process, the pressurizing torque of each pressurizing component is directly proportional to the total number of pressurizing components, the diameter of the pressurizing components, the distance between two adjacent pressurizing components, the thickness of the workpiece to be welded, and the elastic modulus of the workpiece to be welded, and inversely proportional to the yield strength of the workpiece to be welded.
[0017] (3) Beneficial effects In summary, this invention achieves flexible compensation of the applied pressure and adaptive correction of the welding gap through segmented pressurization and compensation with spring screws. This avoids the deformation problem caused by rigid pressurization of large-sized curved thin-walled parts, and also improves the fitting accuracy and overall quality stability of the welded parts. Furthermore, the precise pre-pressurization calculated by multi-parameter coupled torque in the two-stage pressurization strategy, along with the synergy of subsequent tightening pressurization, ensures accurate gap control and more uniform load transfer, further addressing the technical challenges of welding large-sized curved thin-walled parts. Attached Figure Description
[0018] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the embodiments of the present invention will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0019] Figure 1 This is a schematic diagram of the structure of an argon arc welding device for large-sized curved thin-walled parts provided in an embodiment of the present invention; Figure 2 This is a schematic diagram of the assembly structure of the elastic component and the pressure component of an argon arc welding device for large-sized curved thin-walled parts provided in an embodiment of the present invention; Figure 3 This is a schematic flowchart of an argon arc welding method for large-sized curved thin-walled parts provided in an embodiment of the present invention; Figure 4 This is a schematic diagram of the two-stage pressurization process of an argon arc welding method for large-sized curved thin-walled parts provided in an embodiment of the present invention.
[0020] In the picture: 1- Tooling base; 2- Base reinforcing rib; 3- Lower mold; 4- Upper mold; 401- Threaded hole; 5- Elastic component; 6- Pressure component; 7- Upper mold hanger; 8- Workpiece protection plate; 100- Workpiece to be welded. Detailed Implementation
[0021] The embodiments of the present invention will be further described in detail below with reference to the accompanying drawings and examples. The following detailed description of the embodiments and the accompanying drawings are used to illustrate the principles of the present invention by way of example, but should not be used to limit the scope of the present invention. That is, the present invention is not limited to the described embodiments, and any modifications, substitutions and improvements to the parts, components and connection methods are covered without departing from the spirit of the present invention.
[0022] It should be noted that, unless otherwise specified, the embodiments and features described in this application can be combined with each other. This application will now be described in detail with reference to the accompanying drawings and embodiments.
[0023] In the description of this invention, it should be understood that the terms "upper," "lower," "front," "rear," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product of this invention is in use, or the orientation or positional relationship commonly understood by those skilled in the art. They are only used to facilitate the description of this invention and to simplify the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.
[0024] In the description of this invention, it should also be noted that, unless otherwise explicitly specified and limited, the terms "set" and "install" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0025] A first aspect of this invention provides an argon arc welding apparatus for large-sized curved thin-walled parts, see [link to relevant documentation]. Figure 1 The device may include a tooling base 1, a base reinforcing rib 2, a lower mold 3, an upper mold 4, an elastic element 5, and a pressure element 6. The lower mold 3 is installed on the tooling base 1 through the base reinforcing rib 2 and is used to support the lower surface of the workpiece 100 to be welded. The upper mold 4 covers the upper surface of the workpiece 100 to be welded and is installed in conjunction with the lower mold 3 to clamp the workpiece 100 to be welded. Multiple pressure elements 6 are sequentially spaced through the upper mold 4 and are squeezed by the elastic element 5 to press the workpiece 100 to be welded.
[0026] In the above embodiment, a threaded hole is used to assemble an adjusting screw with a spring. The elastic deformation of the spring is used to achieve flexible compensation of the applied pressure. At the same time, it adaptively compensates for the gap deviation during the assembly and welding of large-sized curved thin-walled parts, avoiding deformation of the parts caused by rigid pressure.
[0027] Furthermore, the argon arc welding device also includes an upper mold hanger 7, which is installed on the upper end face of the upper mold 4. The upper mold 4 can be hoisted via the upper mold hanger 7 for easy installation and disassembly. The argon arc welding device also includes a workpiece protective plate 8, and an elastic element 5 contacts the upper surface of the workpiece 100 to be welded through the workpiece protective plate 8. Among them, the elastic element 5 is a spring, the pressure element 6 is a screw, and the upper mold 4 has multiple threaded holes 401. The pressure element 6 passes through the threaded holes 401. The upper mold 4 is a structure that completely fits the curved contour of the workpiece 100 to be welded. Specifically, it is divided into 10 independent pressure points, which are marked in sequence as point 1, point 2, point 3... point 10. Each point is provided with a threaded hole 401, and the threaded hole 401 matches the screw one by one. The screw is tightened to achieve precise pressure positioning of the workpiece 100 to be welded.
[0028] A second aspect of the present invention provides a welding method using the above-described argon arc welding apparatus for large-sized curved thin-walled parts. Referring to the figure, the method may include the following steps: S100. Place the workpiece to be welded on the top surface of the lower mold and adjust the position of the workpiece to be welded to ensure that the weld seam is aligned with the preset welding path.
[0029] Specifically, the workpiece to be welded (a large-sized curved thin-walled part) is placed on the top surface of the lower mold, and the position of the part is adjusted to ensure that the weld seam is aligned with the preset welding path.
[0030] S200. The upper mold is attached and covered on the upper surface of the workpiece to be welded.
[0031] Specifically, the upper mold is placed over the surface of the workpiece to be welded, so that the upper mold fits tightly against the curved surface of the workpiece, ensuring that the threaded hole is positioned in the pressure area of the workpiece to be welded.
[0032] S300: Each pressure point on the workpiece to be welded is pressurized twice using an alternating odd and even method.
[0033] Specifically, a two-stage pressurization mode is adopted. The first stage is based on the yield strength of the thin-walled part material (workpiece to be welded), the arc length of the single-stage upper die at the weld position, the nominal diameter of the thread of the pressurizing screw, the thickness of the part to be welded, and the number of pressurizing points on the upper die to build a calculation model to achieve precise pre-pressurization. The second stage strengthens the bonding effect through fastening pressurization, taking into account both gap control accuracy and welding stability. First pressurization (torque-controlled pressurization): Tighten the screws segment by segment using a torque wrench in the order of 1 point → 3 point → 5 point → 7 point → 9 point, with the torque applied for each segment (determined by a preset formula) to ensure that the pressurization pressure matches the material properties of the parts and avoids initial deformation; then tighten the screws segment by segment using a torque wrench in the order of 2 point → 4 point → 6 point → 8 point → 10 point, with the torque applied for each segment (determined by a preset formula) to ensure that the pressurization pressure matches the material properties of the parts and avoids initial deformation; Second pressurization (tightening pressurization): After completing the first torque-controlled pressurization, tighten the screws directly segment by segment in the same order to further compact the parts, ensuring that the weld gap is uniform and stable and that no additional plastic deformation occurs.
[0034] S400. After two pressurizations are completed, spot welding is performed using argon arc welding. Then, the workpiece to be welded is welded according to the preset welding path until the weld cools to room temperature.
[0035] Specifically, after all segments are pressurized, argon arc welding is used to automatically spot-fix the welds in the order of 1 point → 3 points → 5 points → 7 points → 9 points to reduce welding stress concentration. Then, welding is carried out according to the preset path. During the welding process, the tooling is kept under pressure until the weld cools to room temperature and then the tooling is removed.
[0036] As an optional implementation, in step S300, the pressure torque of each pressure component during the first pressurization process is directly proportional to the total number of pressure components, the diameter of the pressure components, the distance between two adjacent pressure components, the thickness of the workpiece to be welded, and the elastic modulus of the workpiece to be welded, and inversely proportional to the yield strength of the workpiece to be welded.
[0037] The initial pressurization torque is calculated using the following formula to achieve a precise match between the pressure and the yield strength of the component material. To prevent plastic deformation of the component after pressurization, the target pressure... c Take the yield strength σ s 60~80%, that is: ; In the formula, K c The preload stress coefficient is 0.6 to 0.8.
[0038] Combining the pressure area A of the part (the pressure area corresponding to a single screw) (where D is the equivalent diameter of the pressure zone of the workpiece to be welded), the clamping force F required for a single screw is: ; However, since D is related to the screw distribution span L (when uniformly distributed) (Approximate distribution of regular polygons), after substituting, it simplifies to: ; The torque balance equation for threaded fasteners is: ; In the formula, r f The equivalent radius of friction on the bearing surface is given by adjusting the thread helix angle λ and the equivalent friction angle ρ in the formula. v Friction coefficient f c By taking approximate values, substituting and combining the friction terms, we can obtain: ; In the formula, The coefficient of friction is 0.10 to 0.18.
[0039] Then, deformation constraints (thickness t and elastic modulus E) are introduced for the part, and the elastic deformation of the part under compression is calculated. The tooling pressurization stroke requirement must be met, according to Hooke's Law: ; Combination We can obtain: ; Substituting this into the expression for the clamping force F, we can finally get F, , The correlation relationships are integrated, and a comprehensive correction coefficient K (including) is introduced. , (Tooling stiffness compensation), and considering the influence of the screw distribution span L on the uniformity of force distribution (the larger L is, the greater the force on a single screw), the final torque formula is derived: ; In the formula, M is the required applying torque for a single screw (unit: N·m); K is a comprehensive correction coefficient, ranging from 0.12 to 0.20, adjusted according to the curvature of the part surface; the greater the curvature, the smaller the K value; σ s E is the yield strength of the material of the thin-walled part to be welded (unit: MPa); E is the elastic modulus of the thin-walled part to be welded (unit: MPa); L is the arc length of the single-segment upper die at the weld position (unit: mm); d is the nominal diameter of the thread of the pressure screw (unit: mm); t is the thickness of the part to be welded (unit: mm); n is the number of pressure screws on the upper die.
[0040] Formula design principle: Based on the material yield strength, the compressive stress is limited to avoid plastic deformation of the parts; by matching the length of the upper mold of a single segment with the pressure coverage range, and combined with the thread diameter, the torque transmission efficiency is ensured, and finally, the pressure of each segment is uniform and controllable.
[0041] Example 1 Taking a curved thin-walled part made of 0Cr18Ni9 stainless steel with a thickness of 0.8mm, a weld curvature radius of approximately 460mm, and a weld length of approximately 1100mm as an example, the specific implementation method is as follows: I. Pre-processing stage (Challenge: Datum positioning of curved surface parts) 1. Part datum calibration: Use a coordinate measuring machine to inspect the surface contour of the part and record the curvature deviation of the weld area (allowable deviation ≤0.05mm); mark 3 positioning datum points in the non-welded area of the part and align them with the datum pins preset in the lower mold. Adjust the position of the part with a dial indicator to ensure that the flatness deviation of the datum points is ≤0.02mm.
[0042] 2. Tooling cleaning: Wipe the mating surfaces and threaded holes of the upper and lower molds with anhydrous ethanol to remove oil and metal shavings (difficulty: avoid residual impurities that cause the mating gap of the curved surfaces to be greater than 0.03mm).
[0043] II. Part positioning and pre-fixation (Challenge: Stress-free bonding of curved surfaces) 1. Initial placement: Gently place the part on the top surface of the lower mold to avoid initial deformation caused by hard contact between the part and the lower mold; 2. Gap inspection: Use a feeler gauge to check the fit gap between the part and the lower mold. The gap in the weld area should be 0.05mm. If the gap exceeds the standard, adjust it by locally padding the lower mold with 0.02mm thick copper foil (difficulty: the thickness of the copper foil must match the gap to avoid excessive support). 3. Pre-fixing: Lightly press the two ends of the part (corresponding areas of position 1 and position 10) with temporary clamps. The clamp pressure is ≤5N (only restricts the displacement of the part and does not produce plastic deformation).
[0044] III. Upper mold assembly and precision verification (Challenge: the fit of the curved surfaces of the segmented upper mold) 1. Segmented assembly: The upper mold is placed in the order of "from the middle to both ends" (first install points 5 and 6, then install points 3, 4, 7, and 8, and finally install points 1, 2, 9, and 10) to avoid cumulative errors in segments; 2. Fit Test: Use a dial indicator to test the gap between each section of the upper mold and the part. Select 3 test points for each section (both ends + the middle). The gap must be ≤0.03mm. If the gap of a certain section exceeds the standard, fine-tune the position of the upper mold until it fits (difficulty: avoid local forced pressing that may cause deformation of the upper mold). 3. Thread hole alignment: Use a go / no-go gauge to check the coaxiality of the thread hole and the lower die thread. The coaxiality deviation must be ≤0.1mm (to prevent eccentric force when tightening the screw).
[0045] IV. Segmented pressurization (Core challenges: torque control and sequential coordination) (1) First pressurization (torque control, difficulty: torque accuracy and sequence rhythm) 1. Torque wrench calibration: Use a digital torque wrench with an accuracy of ±2%, and calibrate the 0.123 N·m setting error in advance with a standard torque meter (to ensure that the actual torque deviation is ≤0.002 N·m). 2. Pressurization sequence and rhythm: Pressurize in the order of "1→3→5→7→9→2→4→6→8→10", with each point pressurized in 3 progressive steps: first tighten to 0.05 N·m, pause for 10 seconds (to release the elastic deformation of the part), then tighten to 0.1 N·m, pause for 10 seconds, and finally tighten to 0.123 N·m; after each point of pressurization, use a dial indicator to check the deformation of that section of the part (the allowable deformation is ≤0.05 mm); if the deformation exceeds the limit, reduce the torque to 0.1 N·m, readjust the upper mold fit, and then pressurize again; 3. Segment gap detection: After pressurizing at odd-numbered points (1, 3, 5, 7, 9), check the gap between adjacent segments (≤0.03mm), and then pressurize at even-numbered points.
[0046] (2) Second pressurization (tightening pressurization, difficulty: avoid overpressure deformation) 1. Tightening sequence: Same as the first pressurization sequence, each section adopts the "slow tightening + gap monitoring" method: use a manual Allen wrench to tighten the screw, and check the weld gap every 1 / 2 turn (allowable gap 0.3~0.5mm); stop when the screw is tightened to the state of "no obvious looseness" (torque about 0.5N·m), to avoid over-tightening and causing plastic deformation of the parts; 2. Consistency test of pressure throughout the entire section: Use a pressure sensor to detect the actual pressure of each screw section. The pressure deviation must be ≤10% (challenge: correcting the pressure deviation by fine-tuning the screw tightness).
[0047] V. Welding (Challenges: thermal deformation and gap stability) 1. Welding preheating parameters: Preheat the argon arc welding equipment for 5 minutes in advance, and adjust the welding current (120A), voltage (18V), and argon flow rate (15L / min) to ensure that the parameters are stable; 2. Segmented welding: Weld along the weld from point 1 to point 10, pausing for 30 seconds after welding every 2 points (e.g., points 1 and 2 correspond to the weld seam), and use an infrared thermometer to check the weld temperature (≤200℃) to avoid the accumulation of thermal deformation; 3. Real-time gap monitoring: During the welding process, the weld gap is photographed in real time using an industrial camera. If the gap change is >0.1mm, welding is paused and the tightness of the screws in the corresponding section is fine-tuned (the difficulty is that the fine-tuning range must be ≤1 / 8 turn to prevent sudden pressure changes).
[0048] VI. Post-processing and accuracy testing 1. Cooling control: After welding, keep the tooling pressurized and continue to hold the pressure for 30 minutes after the weld temperature drops to room temperature (25℃) (difficulty: avoid stress concentration caused by rapid cooling). 2. Tooling removal: Remove the upper mold screws in reverse order of "10→8→6→4→2→9→7→5→3→1" to prevent the parts from springing back; 3. Final inspection: Use a coordinate measuring machine to inspect the weld gap (deviation ≤ 0.2 mm) and the surface contour of the part (deformation ≤ 0.1 mm) to ensure that it meets the accuracy requirements.
[0049] It should be noted that the various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referred to mutually. Each embodiment focuses on describing the differences from other embodiments. The present invention is not limited to the specific steps and structures described above and shown in the figures. Furthermore, for the sake of brevity, detailed descriptions of known methods and techniques are omitted here.
[0050] The above are merely embodiments of this application and are not intended to limit the scope of this application. Various modifications and variations can be made to this application by those skilled in the art without departing from the scope of the invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principle of this application should be included within the scope of the claims of this application.
Claims
1. An argon arc welding device for large-sized curved thin-walled parts, characterized in that, The fixture includes a tooling base (1), a base reinforcing rib (2), a lower mold (3), an upper mold (4), an elastic element (5), and a pressure element (6). The lower mold (3) is installed on the tooling base (1) through the base reinforcing rib (2) and is used to support the lower surface of the workpiece (100) to be welded. The upper mold (4) covers the upper surface of the workpiece (100) to be welded and is installed in conjunction with the lower mold (3) to clamp the workpiece (100) to be welded. A plurality of pressure elements (6) are sequentially spaced through the upper mold (4) and squeeze the workpiece (100) to be welded through the elastic element (5).
2. The argon arc welding apparatus for large-size curved thin-walled parts according to claim 1, characterized in that, It also includes an upper mold hanger (7), which is installed on the upper end face of the upper mold (4).
3. The argon arc welding apparatus for large-size curved thin-walled parts according to claim 1, characterized in that, It also includes a workpiece protection sheet (8), through which the elastic element (5) contacts the upper surface of the workpiece (100) to be welded.
4. The argon arc welding apparatus for large-size curved thin-walled parts according to claim 1, characterized in that, The elastic element (5) is a spring.
5. The argon arc welding apparatus for large-size curved thin-walled parts according to claim 1, characterized in that, The pressure-applying component (6) is a screw.
6. The argon arc welding apparatus for large-size curved thin-walled parts according to claim 1, characterized in that, The upper mold (4) has multiple threaded holes (401), and the pressure member (6) passes through the threaded holes (401).
7. A welding method for a large-sized curved thin-walled part using an argon arc welding apparatus as described in any one of claims 1-6, characterized in that, The method includes the following steps: Place the workpiece to be welded on the top surface of the lower mold and adjust the position of the workpiece to ensure that the weld seam is aligned with the preset welding path. The upper mold is attached and covered to the upper surface of the workpiece to be welded; Each pressure point on the workpiece to be welded is pressurized twice using an alternating odd and even pressure method. After the two pressurization processes are completed, spot welding is performed using argon arc welding. Then, the workpiece to be welded is welded according to the preset welding path until the weld cools to room temperature.
8. The welding method of the argon arc welding apparatus for large-size curved thin-walled parts according to claim 7, characterized in that, For the first pressurization, tighten each pressurizing component one by one in the order of odd-numbered points, and then tighten each pressurizing component one by one in the order of even-numbered points.
9. The welding method of the argon arc welding apparatus for large-size curved thin-walled parts according to claim 7, characterized in that, For the second pressurization, tighten each pressurizing component one by one in the order of odd-numbered points, and then tighten each pressurizing component one by one in the order of even-numbered points.
10. The welding method of the argon arc welding apparatus for large-size curved thin-walled parts according to claim 7, characterized in that, During the first pressurization process, the pressurizing torque of each pressurizing component is directly proportional to the total number of pressurizing components, the diameter of the pressurizing components, the distance between two adjacent pressurizing components, the thickness of the workpiece to be welded, and the elastic modulus of the workpiece to be welded, and inversely proportional to the yield strength of the workpiece to be welded.