A herbicide granular formulation containing diuron and its preparation process
By moving the ethanol film-forming and salt-immersion operations to before drug loading in the preparation process, and combining in-core drug loading and surface cleaning, the problem of drug loss and outer coating integrity is solved by using wet continuous construction and segmented cross-linking to form transmembrane gel connections, thus achieving effective drug release and self-repair.
Patent Information
- Application Number
- CN202611515874.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-28
- Publication Date
- 2026-11-17
AI Technical Summary
In the prior art, after the particles are first wetted and repeatedly dried and wetted, residual crystals or defects in the outer coating near the orifice may increase early drug loss, while simply thickening the sealing outer membrane may hinder subsequent effective drug delivery.
Ethanol film formation and salt impregnation were moved to before drug loading. Surface free drug was reduced by in-core drug loading and surface cleaning. Transmembrane gel connections were formed using wet continuous construction and segmented crosslinking. The study investigated how to maintain the integrity of the outer coating during wet-dry cycles.
It reduces drug loss, maintains the drug diffusion pathway, ensures the integrity of the outer coating during wet and dry cycles, and enables on-demand release and self-repair.
Smart Images

Figure CN123100608A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of pesticide formulation and porous particle coating technology, specifically to a herbicide granule containing diuron and its preparation process. Background Technology
[0002] Diuron can be dispersed in porous carriers in crystalline form, and its dissolution and diffusion upon contact with water can be altered by a polymer layer. Published literature CN101773112A has proposed a scheme combining hydroxyapatite particles loaded with diuron under negative pressure with calcium alginate gel. Therefore, the use of negative pressure impregnation, alginate, and calcium salts are all known technical methods.
[0003] For directly applied granules, residual crystals or defects in the outer coating near the orifice after the initial wetting and repeated drying and wetting processes may increase early drug loss; simply thickening the sealing outer membrane may hinder subsequent effective drug delivery. Summary of the Invention
[0004] To address the shortcomings of existing technologies, this invention provides a herbicidal granule containing diuron and its preparation process, which moves the ethanol film-forming and salt-impregnation operations to before drug loading, reducing the chance of these two processes directly contacting diuron; and reduces surface free drug by loading the drug into the core and cleaning the surface.
[0005] To achieve the above objectives, the present invention provides the following technical solution: a herbicide granular agent containing diuron and its preparation process, comprising the following steps: S1. A water-soluble polyvinyl alcohol layer with closed pores is formed on the surface of sintered diatomaceous earth core particles with interconnected pores; sodium chloride microcrystals are attached to the surface of this layer at intervals, and then an ethyl cellulose ethanol solution is sprayed to form a film, such that at least some of the microcrystals have a height greater than the film thickness along the normal direction of their respective surfaces, with the bottom contacting the polyvinyl alcohol layer and the top exposing the film; sodium chloride and polyvinyl alcohol are removed by water extraction, and the particles are dried to obtain a coated blank particle with through pores connecting the core particle pores to the outside. S2. The coated blank particles are impregnated with an aqueous suspension of diuron with a volume reference particle size D90 of 0.3-0.8 μm under reduced pressure and re-pressurization to allow diuron crystals to enter the core particle pores. The surface liquid is removed and the particles are dried to obtain drug-loaded particles. S3. The drug-loaded particles are impregnated with the first sodium alginate aqueous solution under reduced pressure and re-pressurization. After the solution is drained, a second sodium alginate aqueous solution with a higher sodium alginate mass fraction than the first sodium alginate aqueous solution is sprayed on it, so that the two solutions are continuously distributed outside the membrane, in the through holes and in the pores of the connected core particles. S4. Without drying, pre-crosslink the herbicide in a 0.02-0.05 mol / L calcium chloride aqueous solution, then continue crosslinking in a 0.10-0.20 mol / L calcium chloride aqueous solution, rinse, and dry to form a calcium alginate phase in which the outer membrane is continuously connected to the core granule pores via the connecting part in the through-holes, thus obtaining the herbicide granules.
[0006] Preferably, in step S1, the particle size of the core particle is 0.8–1.6 mm, and the open pore volume is 0.4–0.8 mL / g; according to the pore volume distribution measured by mercury intrusion porosimetry, the pore volume with a throat diameter of 3–30 μm accounts for 60%–85% of the total open pore volume; the degree of alcoholysis of the polyvinyl alcohol is 87%–89% (mole fraction); the polyvinyl alcohol layer is formed by spraying a polyvinyl alcohol aqueous solution onto the surface of the core particle in stages and drying it, and its dry average thickness is 2–5 μm; the polyvinyl alcohol layer is dried before spraying the ethyl cellulose ethanol solution.
[0007] Preferably, in step S1, sodium chloride microcrystals are attached to the surface of the polyvinyl alcohol layer in a separate monolayer; according to the volume distribution measured by dry laser diffraction, the D10 of the sodium chloride microcrystals is 30-40 μm and the D90 is not greater than 60 μm; the ethyl cellulose ethanol solution is prepared with anhydrous ethanol and contains 10%-20% of triethyl citrate by mass of ethyl cellulose; fluidized bed intermittent spraying and intermittent drying are used, with the material temperature at 30-40°C, to form an ethyl cellulose membrane with an average dry thickness of 10-25 μm, and the height of the microcrystals exposed on the membrane surface along the normal direction of the surface is not less than 1.2 times the membrane thickness at that point; the membrane is extracted with water at 35-45°C through multiple water changes, and the residual sodium chloride content in the resulting coated blank particles does not exceed 0.2% of its dry basis mass.
[0008] Preferably, in step S2, diuron, polyvinylpyrrolidone, alkyl glycoside and water are mixed and wet-milled to obtain an aqueous suspension with a diuron mass fraction of 20% to 25%; the amounts of polyvinylpyrrolidone and alkyl glycoside are 1% to 3% and 0.2% to 0.5% of the diuron mass, respectively; the volume reference particle size D90 of diuron is determined by wet laser diffraction and is not greater than one-fifth of the volume reference pore throat equivalent diameter distribution D10 of the through-holes before drug loading; the pore throat distribution is determined by three-dimensional reconstruction using focused ion beam continuous slice scanning electron microscopy, with the through-holes separated from each other in the membrane as the statistical unit, the diameter of the circle of equal area of the narrowest cross section along the center line of each pore as the pore throat equivalent diameter, and the pore throat equivalent diameter when the cumulative volume first reaches or exceeds 10% of the total through-hole volume is the weighted pore reconstruction volume in the membrane.
[0009] Preferably, in step S2, the coated blank particles are placed in a sealed container, the air is evacuated to an absolute pressure of 20-40 kPa and maintained for 2-5 minutes, the aqueous suspension is injected under this pressure until the particles are submerged, and then the pressure is restored to normal within 1-3 minutes and maintained for 5-10 minutes; the surface liquid is drained off, and the particles are sprayed with deionized water for 5-15 seconds and then drained immediately, and then dried at 35-45°C; the amount of water used for spraying is 0.5-1.0 mL per gram of coated blank particles.
[0010] Preferably, in step S3, the mass fraction of the first sodium alginate aqueous solution is 0.6% to 1.0%, and the mass fraction of the second sodium alginate aqueous solution is 1.5% to 2.5%. The drug-loaded particles are immersed in the first sodium alginate aqueous solution and kept under an absolute pressure of 15 to 30 kPa for 1 to 3 minutes, then restored to normal pressure and kept under normal pressure for 3 to 8 minutes. Both aqueous solutions are prepared with the same batch of sodium alginate, and no calcium salts are added before contact with the particles. After the impregnation and spraying are completed, step S4 is carried out without intermediate drying.
[0011] Preferably, in step S4, the pre-crosslinking and continued crosslinking are carried out in two separate calcium chloride crosslinking baths. The pre-crosslinking time is 3-10 min, and the continued crosslinking time is 20-40 min. The temperature for both crosslinking is 20-30°C. The initial solution volume of each crosslinking bath is 20-40 mL per gram of wet particles obtained in step S3, and the particles are kept submerged during crosslinking. After crosslinking, the particles are rinsed with a calcium chloride aqueous solution with a concentration of 5-15 mmol / L.
[0012] Preferably, the drying in step S4 includes: first drying in air at 25-30°C and 60%-75% relative humidity for 1-3 hours, and then drying in air at 35-45°C and 30% relative humidity until the moisture content of the granules is 1%-3% by mass; the content of diuron in the resulting granules is 8%-18% by dry basis mass.
[0013] Preferably, the granules include sintered diatomaceous earth core particles with interconnected pores, an ethyl cellulose membrane covering the core particles, diuron crystals distributed within the pores of the core particles, and a calcium alginate phase; the ethyl cellulose membrane has through-holes connecting the core particle pores to the outside; the calcium alginate phase includes an outer membrane portion outside the membrane, a connecting portion penetrating the through-holes, and an embedded portion within the core particle pores, all three being continuously connected and each containing a coordination cross-linking structure formed between carboxyl groups of different alginate chains; the core particles have a particle size of 0.8–1.6 mm, the ethyl cellulose membrane has a dry average thickness of 10–25 μm, and diuron accounts for 8%–18% of the dry basis mass of the granules; the outer membrane portions are interconnected, and their coverage area accounts for not less than 95% of the outer surface area of the ethyl cellulose membrane, excluding the area of the through-hole openings.
[0014] Preferably, the dry average thickness of the outer membrane is 0.3–1.5 μm; the depth L of the embedded portion extending radially inward from the core particle side opening of the corresponding through-hole is not less than twice the equivalent diameter d of the throat of the through-hole, and not less than the dry average thickness of the ethyl cellulose membrane; the embedded portion has a branch extending into the core particle branch hole communicating with the through-hole, and the maximum width of the branch in the plane perpendicular to the radial direction is greater than d; d is the diameter of the equal-area circle of the narrowest cross section of the corresponding through-hole in the dry state along the center line of the channel, which is determined after distinguishing the ethyl cellulose membrane from the calcium alginate phase by continuous slice three-dimensional reconstruction.
[0015] Compared with existing technologies, this invention provides a diuron-containing herbicide granule and its preparation process, which has the following beneficial effects: the ethanol film-forming and salt-impregnation operations are moved to before drug loading, reducing the chance of these two processes directly contacting diuron; the surface free drug is reduced through in-core drug loading and surface cleaning; the transmembrane gel connection is formed through wet continuous construction and segmented crosslinking, and its role in maintaining the integrity of the outer coating in wet-dry cycles is studied, while preserving the diffusion path of dissolved diuron; it does not advocate permanent non-detachment, complete non-leaching, on-demand release or self-repair. Attached Figure Description
[0016] Figure 1 This is a FIB-SEM three-dimensional reconstruction image of the interconnected structure between the through-holes of the coated blank particles and the pores of the core particles in Example 1; Figure 2 This is a FIB-SEM three-dimensional reconstruction of the transmembrane linkage structure of the herbicide granules obtained in Example 1. Detailed Implementation
[0017] The technical solutions of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0018] Please see Figures 1-2 This invention provides a technical solution for a herbicide granule containing diuron and its preparation process: Diuron uses technical grade pesticides with content certification and independently certified reference materials; the technical grade pesticide input is calculated based on the active ingredient. Polyvinylpyrrolidone is graded K30, and alkyl glycosides are graded C8-C10 and calculated based on the active ingredient. Ethyl cellulose is graded to form a homogeneous solution in anhydrous ethanol of this formulation; ethoxylated content and supplier viscosity specifications are recorded. Sodium alginate uses the same low-viscosity batch; a 1.0% aqueous solution at 25°C and a shear rate of 10 s is recommended. -¹The apparent viscosity of 50–100 mPa·s was used as the raw material screening window, and the M / G composition was recorded.
[0019] Each mass percentage is calculated with the total mass of the specified solution or the mass of the active ingredient as the denominator; the dry basis dosage is calculated with the mass of the finished product after removing the water content measured according to the specified method as the denominator. Absolute pressure and gauge pressure are recorded separately, and all given decompression values are absolute pressures. Film thickness, pore throat, and embedding depth are defined in the dry state and are not used interchangeably with the hydrated dimensions; the core particle size is the size before coating, described using the diameter of the equal-area circle from the calibration image. Endpoint trials use narrow-distribution raw materials and report the actual distribution and uncertainty; the sieve aperture size or nominal value cannot be used as the diameter of each particle.
[0020] The temporary sealing layer is considered acceptable if its cross-section continuously covers the pore opening and ethyl cellulose does not significantly penetrate the original core pores. Sacrificial samples with different intermediate nodes are set up in S1; formulation tests are not continued on already cut particles. After water extraction, chloride ions are quantified, and sodium chloride is converted after subtracting the core particle blank. Polyvinyl alcohol (PVA) residues in the final extract and after thorough extraction of whole particles are checked using an iodine-boric acid colorimetric method calibrated for this system. Core particle, ethyl cellulose, and plasticizer blanks are set up. It is recommended that the PVA residue not exceed 0.05% (dry basis) of the blank particles as the R&D control line, and the detection limit must be below this line; low conductivity of the extract cannot be used to determine that PVA has been removed.
[0021] The salt substrate contacts the temporary layer and is exposed, allowing water to reach the soluble template from the outside; however, removing the temporary layer may create a gap between the membrane and the core, and the membrane may collapse during pressure cycling. Membrane integrity and pore connectivity should be checked at three points: after extraction, after drug loading, and after crosslinking and drying. If the pre-fabricated membrane cannot maintain integrity, the membrane formation and extraction conditions should be improved, and a new trial production should be conducted, using the term "through-hole" to replace the actual structure.
[0022] Drug loading mass balance: Let the mass of non-drug dry matter before drug loading be B, the mass of non-drug dry matter added subsequently be G, and the target dry basis drug content be w. Then the required residual mass of diuron is M = w(B + G) / (1 - w). Actual loading must also consider the loss during each round of washing and cross-linking. After each round S2, retain a sample to measure M, and estimate G using a drug-free sacrificial batch of the same process. After S4, determine the final content based on the finished product. The initial pore volume multiplied by the suspension density and mass fraction is only an estimate of an ideal filling, not a guarantee of loading. Repeated loading may clog pores, and the remaining pathways must be checked simultaneously. If the conditions are not met after a maximum of three rounds, the parameter combination is considered unachieved, and drug loading cannot continue until the structure cannot be guaranteed. Structural parameters and finished product content are used as trial production targets and acceptance conditions. The input endpoints are confirmed after actual temperature control, weighing, pressure measurement, and concentration calibration, while the output endpoints can only be identified after obtaining samples.
[0023] Example 1 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 88 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 3.5 μm by cross-sectional sampling, ensuring the surface pores are sealed. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 35 μm and a target D90 of 55 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0024] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 0.75g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, and maintain a material temperature of 35°C. Replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 17.5μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 40°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis mass of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0025] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 112.5g, the dry matter of polyvinylpyrrolidone is 2.25g, the active ingredient of alkyl glycoside is 0.39375g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, stopping when the volume reference D90 target of 0.55μm is reached, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-hole. The blank particles are drawn to an absolute pressure of 30kPa and held for 3.5min, and the suspension is injected under this pressure until completely submerged, with an initial dosage of 3.0mL of suspension per gram of dry particles in this round; restore to normal pressure within 2min and hold for 7.5min. After draining for 60 seconds, spray with 0.75 mL of deionized water per gram of original coated blank particles for 10 seconds, drain immediately, and dry at 40°C to constant weight.
[0026] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (8g of sodium alginate) and 200.00g of the second solution (4g of sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 0.8% and 2%, respectively, without pre-addition of calcium salts, phosphates, or chelating agents. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 22.5kPa for 2 minutes, then restore to normal pressure within 60 seconds and maintain for 5.5 minutes; drain for 60 seconds. In a sealed rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 40g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0027] S4: Two independent crosslinking baths were set up, each prepared with 30 mL of solution per gram of wet S3 particles, resulting in 0.035 mol / L and 0.15 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 25°C, pre-crosslinked for 6.5 min, then transferred to the bath and drained for 10 s without drying, followed by another 30 min of crosslinking. The particles were rinsed twice with 10 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s, followed by 60 s of draining. The particles were first dried at 27.5°C and 67.5% relative humidity for 2 h, then dried at 40°C and 20% relative humidity, with a moisture content of 2% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0028] Example 2 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 87 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 2 μm with sealed surface pores by cross-sectional sampling. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 30 μm and a target D90 of 50 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0029] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 0.5g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, and maintain a material temperature of 30°C. Replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 10μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 35°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis weight of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0030] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 100g, the dry matter of polyvinylpyrrolidone is 1g, the active ingredient of alkyl glycoside is 0.2g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, and stopping after reaching the target volume reference D90 of 0.3μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-hole. Draw the blank particles to an absolute pressure of 20kPa and hold for 2min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 1min and hold for 5min. After draining for 60 seconds, spray with 0.5 mL of deionized water per gram of original coated blank particles for 5 seconds, drain immediately, and dry at 35°C to constant weight.
[0031] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (6g of sodium alginate) and 200.00g of the second solution (3g of sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 0.6% and 1.5%, respectively. No calcium salts, phosphates, or chelating agents are added beforehand. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 15kPa for 1 minute, then restore to normal pressure within 60 seconds and maintain for 3 minutes; drain for 60 seconds. In a sealed, rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 10g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0032] S4: Two independent crosslinking baths were prepared, each using 20 mL of solution per gram of wet S3 particles, resulting in 0.02 mol / L and 0.1 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 20°C for 3 minutes of pre-crosslinking, followed by a 10-second draining period without drying, and then another 20 minutes of crosslinking. The particles were rinsed twice with 5 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 seconds, followed by a 60-second draining period. The particles were first dried at 25°C and 60% relative humidity for 1 hour, then dried again at 35°C and 30% relative humidity, with a moisture content of 1% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0033] Example 3 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 89 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 5 μm with sealed surface pores by cross-sectional sampling. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 40 μm and a target D90 of 60 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0034] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 1g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, maintain a material temperature of 40°C, and replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 25μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 45°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis mass of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0035] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 125g, the dry matter of polyvinylpyrrolidone is 3.75g, the active ingredient of alkyl glycoside is 0.625g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, stopping after reaching the target volume reference D90 of 0.8μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-pore. Draw the blank particles to an absolute pressure of 40kPa and hold for 5min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 3min and hold for 10min. After draining for 60 seconds, spray with 1 mL of deionized water per gram of original coated blank particles for 15 seconds, drain immediately, and dry at 45°C to constant weight.
[0036] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (10g sodium alginate) and 200.00g of the second solution (5g sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 1% and 2.5%, respectively. No calcium salts, phosphates, or chelating agents are added beforehand. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 30kPa for 3 minutes, then restore to normal pressure within 60 seconds and maintain for 8 minutes; drain for 60 seconds. In a sealed, rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 60g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0037] S4: Two independent crosslinking baths were prepared, each using 40 mL of solution per gram of wet S3 particles, resulting in 0.05 mol / L and 0.2 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 30°C, pre-crosslinked for 10 min, then transferred to the bath and drained for 10 s without drying, followed by another 40 min of crosslinking. The particles were rinsed twice with 15 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s, followed by 60 s of draining. The particles were first dried at 30°C and 75% relative humidity for 3 h, then dried again at 45°C and 30% relative humidity, with a moisture content of 3% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0038] Example 4 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 88 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 5 μm by cross-sectional sampling, ensuring the surface pores are sealed. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 40 μm and a target D90 of 60 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0039] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 0.75g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, and maintain a material temperature of 35°C. Replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 25μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 45°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis mass of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0040] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 125g, the dry matter of polyvinylpyrrolidone is 2.5g, the active ingredient of alkyl glycoside is 0.4375g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, stopping after reaching the target volume reference D90 of 0.3μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-pore. Draw the blank particles to an absolute pressure of 20kPa and hold for 5min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 3min and hold for 10min. After draining for 60 seconds, spray with 0.5 mL of deionized water per gram of original coated blank particles for 5 seconds, drain immediately, and dry at 35°C to constant weight.
[0041] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (6g of sodium alginate) and 200.00g of the second solution (4g of sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 0.6% and 2%, respectively, without pre-addition of calcium salts, phosphates, or chelating agents. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 15kPa for 3 minutes, then restore to normal pressure within 60 seconds and maintain for 8 minutes; drain for 60 seconds. In a sealed rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 60g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0042] S4: Two independent crosslinking baths were prepared, each using 40 mL of solution per gram of wet S3 particles, resulting in 0.02 mol / L and 0.15 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 25°C, pre-crosslinked for 10 min, then transferred to the bath and drained for 10 s without drying, followed by another 40 min of crosslinking. The particles were rinsed twice with 10 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s, followed by 60 s of draining. The particles were first dried at 25°C and 75% relative humidity for 3 h, then dried again at 35°C and 20% relative humidity, with a moisture content of 2% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0043] Example 5 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 87 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 2 μm with sealed surface pores by cross-sectional sampling. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 30 μm and a target D90 of 55 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0044] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 1g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, and maintain a material temperature of 30°C. Replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 10μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 35°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis mass of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0045] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 125g, the dry matter of polyvinylpyrrolidone is 3.75g, the active ingredient of alkyl glycoside is 0.625g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, stopping after reaching the target volume reference D90 of 0.8μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-hole. Draw the blank particles to an absolute pressure of 20kPa and hold for 5min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 3min and hold for 10min. After draining for 60 seconds, spray with 0.75 mL of deionized water per gram of original coated blank particles for 10 seconds, drain immediately, and dry at 35°C to constant weight.
[0046] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (6g of sodium alginate) and 200.00g of the second solution (5g of sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 0.6% and 2.5%, respectively. No calcium salts, phosphates, or chelating agents are added beforehand. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 15kPa for 3 minutes, then restore to normal pressure within 60 seconds and maintain for 8 minutes; drain for 60 seconds. In a sealed, rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 9g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0047] S4: Two independent crosslinking baths were prepared, each using 40 mL of solution per gram of wet S3 particles, resulting in 0.035 mol / L and 0.2 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 25°C for 10 min of pre-crosslinking, followed by a 10 s leachate in the bath without drying, and then continued crosslinking for another 40 min. The particles were rinsed twice with 15 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s, followed by a 60 s leachate. The particles were first dried at 25°C and 75% relative humidity for 3 h, then dried again at 35°C and 20% relative humidity, with a moisture content of 1% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0048] Example 6 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 89 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 3.5 μm by cross-sectional sampling, ensuring the surface pores are sealed. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 35 μm and a target D90 of 55 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0049] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 0.5g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, maintain a material temperature of 40°C, and replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 10μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 40°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis weight of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0050] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 100g, the dry matter of polyvinylpyrrolidone is 2g, the active ingredient of alkyl glycoside is 0.2g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, and stopping after reaching the target volume reference D90 of 0.55μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-hole. Draw the blank particles to an absolute pressure of 30kPa and hold for 3.5min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 2min and hold for 7.5min. After draining for 60 seconds, spray with 0.75 mL of deionized water per gram of original coated blank particles for 10 seconds, drain immediately, and dry at 40°C to constant weight.
[0051] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (10g sodium alginate) and 200.00g of the second solution (3g sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 1% and 1.5%, respectively. No calcium salts, phosphates, or chelating agents are added beforehand. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 30kPa for 3 minutes, then restore to normal pressure within 60 seconds and maintain for 8 minutes; drain for 60 seconds. In a sealed, rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 85g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0052] S4: Two independent crosslinking baths were prepared, each using 30 mL of solution per gram of wet S3 particles, resulting in 0.02 mol / L and 0.1 mol / L calcium chloride aqueous solutions, respectively. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 30°C for 10 min of pre-crosslinking, followed by a 10 s draining period without drying, and then another 40 min of crosslinking. The particles were rinsed twice with 5 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s, followed by a 60 s draining period. The particles were first dried at 30°C and 60% relative humidity for 1 h, then dried again at 45°C and 10% relative humidity, with a moisture content of 3% as the target sampling endpoint. The samples were then sealed and cooled for packaging.
[0053] Example 7 specifically includes the following steps: S1: Prepare a 4.00% aqueous solution of polyvinyl alcohol with a degree of hydrolysis of 88 mol%. Dissolve by stirring at 85°C for 30 min, then cool to 25°C. Spray in a fluidized bed at an instantaneous rate of 2.0 g / min per 100 g core particles for 10 s, dry for 20 s, and coat in multiple stages, maintaining the material at 35°C. Determine the target dry average thickness of the polyvinyl alcohol layer as 3.5 μm by cross-sectional sampling, ensuring the surface pores are sealed. Then dry at 35°C for 30 min. Add 0.50 g of water to the uniform micro-mist of the particles, immediately disperse 5.00 g of sodium chloride microcrystals, roll for 20 s, and dry at 35°C for 10 min to remove unattached microcrystals. Select batches of microcrystals with a target D10 of 40 μm and a target D90 of 60 μm based on dry volume distribution. Retain the separated monolayer microcrystals; the actual adhesion height is confirmed by cross-sectional measurements before and after film formation.
[0054] Prepare a 100.00g coating solution by mixing 5.00g ethyl cellulose, 0.75g triethyl citrate, and anhydrous ethanol. Use a soluble grade suitable for anhydrous ethanol and stir at 25°C until homogeneous and transparent. Spray the solution into a closed, inert gas fluidized bed with recoverable ethanol at an instantaneous rate of 3.0g / min per 100g core particles for 20s, dry for 20s, and maintain a material temperature of 35°C. Replenish with the same coating solution until the average dry thickness of the ethyl cellulose membrane reaches the target of 25μm. Sampling is required to confirm that at least some microcrystals have their bottom in contact with the polyvinyl alcohol layer and their top exposed on the membrane surface, with a surface normal height not less than 1.2 times the membrane thickness at that location; if this is not met, the batch cannot be used as a qualified blank particle. Extract with 30mL of deionized water per gram of particle at 40°C for 20min, repeating the extraction three times with water changes; continue water changes and extraction until sodium chloride residue does not exceed 0.2% of the dry basis mass of the blank particle, and the polyvinyl alcohol removal test is passed. Dry at 40℃ to constant weight, weigh the coated blank particles (mB), and retain the sample to measure the perforation.
[0055] S2: Prepare 500.00g of diuron suspension for each round, and supplement with the same proportion if necessary; the equivalent of pure diuron active ingredient is 112.5g, the dry matter of polyvinylpyrrolidone is 2.25g, the active ingredient of alkyl glycoside is 0.39375g, and the remainder is made up with water. When using water-containing adjuvants or non-100% technical grade, the water introduced by them should be deducted and the non-active ingredients should be included, and the total mass should be recalculated based on 500.00g. Wet grinding with 0.1mm zirconia beads at 25℃, segmented sampling, stopping after reaching the target volume reference D90 of 0.55μm, and this value must not be greater than one-fifth of the volume reference throat D10 of the blank membrane through-hole. Draw the blank particles to an absolute pressure of 20kPa and hold for 5min, then inject the suspension under this pressure until completely submerged, with an initial dosage of 3.0mL suspension per gram of dry particles in this round; restore to normal pressure within 3min and hold for 10min. After draining for 60 seconds, spray with 1 mL of deionized water per gram of original coated blank particles for 15 seconds, drain immediately, and dry at 40°C to constant weight.
[0056] S3: Using the same batch of low-viscosity sodium alginate and deionized water, prepare 1000.00g of the first solution (8g of sodium alginate) and 200.00g of the second solution (5g of sodium alginate), respectively. Stir at 25℃ for 2 hours and allow to stand for 1 hour to remove bubbles. The concentrations are 0.8% and 2.5%, respectively. No calcium salts, phosphates, or chelating agents are added beforehand. Immerse the drug-loaded particles in the first solution at a volume of 5.0mL per gram of dry drug-loaded particles. Maintain a pressure of 15kPa for 3 minutes, then restore to normal pressure within 60 seconds and maintain for 8 minutes; drain for 60 seconds. In a sealed, rolling container at 25℃, spray the second solution evenly over 2 minutes at an initial spray volume of 18g per 100g of initial dry core particles, without hot air drying. The spray volume is a fixed input for this round of trial production; the outer film thickness must be verified on the finished product. Subsequent trials requiring adjustments to the spray volume should be recorded in a separate batch number; the original batch record cannot be overwritten. The wet particle mass (mW) is measured and transferred to the first crosslinking bath within 30 seconds after spraying is completed.
[0057] S4: Two independent crosslinking baths were prepared, each containing 40 mL of 0.05 mol / L and 0.2 mol / L calcium chloride aqueous solution per gram of wet S3 particles. The solutions were prepared using anhydrous calcium chloride equivalents, and hydrated salts were converted according to molecular weight and purity. The particles were completely immersed at 20°C for 10 min of pre-crosslinking, followed by a 10 s leachate in the bath without drying, and then continued crosslinking for another 40 min. The particles were rinsed twice with 10 mmol / L calcium chloride aqueous solution, each time with 5.0 mL per gram of wet particles for 30 s and a 60 s leachate. The particles were first dried at 27.5°C and 67.5% relative humidity for 2 h, then dried at 40°C and 20% relative humidity, with a moisture content of 2% as the sampling endpoint. The samples were then sealed and cooled for packaging.
[0058] Unless otherwise stated, the following comparative examples are the same as those in Example 1.
[0059] Comparative Example 1: Only the drying state of the polyvinyl alcohol layer was changed. After salt attachment, the step of drying at 35°C for 10 minutes before spraying with ethyl cellulose in S1 was omitted. After adding 0.50 g of water and rolling for 20 seconds, the polyvinyl alcohol layer was directly coated with ethanol. The remaining steps remained unchanged.
[0060] Comparative Example 2: Only the volume distribution of sodium chloride microcrystals dry method, D10 / D90, was changed from 35 / 55μm to 8 / 15μm, while the dosage was 5.00g and the spraying procedure remained unchanged.
[0061] Comparative Example 3: Only the depressurization / repressurization during the first sodium alginate solution immersion in S3 was cancelled, and the immersion was changed to atmospheric pressure for 8.5 min, so that the total contact time was consistent with the depressurization of 2 min, repressurization of 1 min and atmospheric pressure of 5.5 min in Example 1.
[0062] Comparative Example 4: Only the mass fraction of the second sodium alginate solution in S3 was changed from 2.0% to 0.8%, while the spraying time remained unchanged at 40g, 2min, and other steps.
[0063] Comparative Example 5: Only the calcium chloride concentration in the first independent crosslinking bath of S4 was changed from 0.035 mol / L to 0.15 mol / L, while retaining the first 6.5 min, the bath transfer 10 s, the second 0.15 mol / L crosslinking 30 min, and the volume and temperature of the two baths.
[0064] Comparative Example 6: Only the relative humidity of the first stage dry air in S4 was changed from 67.5% to 20%, while the temperature was 27.5℃, the time was 2h, and the conditions of the second stage remained unchanged.
[0065] Test methods Sampling of commercial pesticides was conducted in accordance with GB / T 1605—2001 "Sampling Methods for Commercial Pesticides". For each research and development batch, samples were prepared independently three times. Samples were taken from different locations within each batch, combined, and separated using a sampler into undisturbed, heat-stored, wet-dry cycle, chemical analysis, and retention samples. The quality of each sample was recorded, and undesirable particles were not pre-screened. At least two independent pretreatment parallel samples were prepared for each chemical assay; these parallel samples were not considered as new preparation batches.
[0066] Moisture content was determined using the procedure applicable to this sample matrix in GB / T 1600—2021 "Methods for Determination of Moisture in Pesticides". This scheme prioritizes the Karl Fischer method, and its applicability was verified using a blank matrix, water recovery, and thorough extraction. The loss on drying at 45℃ cannot be directly used to replace specific moisture content, as volatiles such as ethanol can also cause weight loss. The mass fraction of moisture is denoted as h. When the wet basis pesticide amount is w_wet, the dry basis pesticide amount w_dry = w_wet / (1 - h), with both h and w substituted as decimals.
[0067] Quantitative analysis of diuron was performed using a high-performance liquid chromatography (HPLC) method validated with this matrix. Approximately 0.20 g of a representative whole sample was accurately weighed and added to 20.0 mL of acetonitrile / water (80:20, v / v). The sample was sonicated for 20 min, shaken for 30 min, and centrifuged. The residue was extracted twice more with the same solution; the extracts were combined and diluted to 100.0 mL. The optimal extraction control condition was that the fourth extraction yield was less than 1% of the total yield of the first three extractions. Initial chromatographic conditions were: C18 column 150 mm × 4.6 mm, 5 μm; acetonitrile / water 60:40; flow rate 1.0 mL / min; column temperature 30 °C; detection at 254 nm; injection depth 10 μL. Calibration was performed using a certified diuron standard reference.
[0068] This project pre-spikes the formulation matrix at three levels (low, medium, and high) six times each, with an average recovery rate of 95%–105% and a relative standard deviation not exceeding 5% as the target for the analytical procedure. The mother liquor and washing solution in each round of S2, and the crosslinking bath and rinsing solution in S4 are all analyzed separately to determine drug loss. The finished product recovery rate is calculated by dividing the actual mass of diuron received by the actual mass of active ingredient added.
[0069] Laser diffraction analysis of diuron crystals and sodium chloride microcrystals was performed according to GB / T 19077—2024, "Laser Diffraction Method for Particle Size Analysis". Diuron was analyzed using a wet method to verify that the dispersion process did not alter the original crystals and avoided dissolution during sampling. The medium, refractive index, absorption parameters, opacity, and whether ultrasonication was used were recorded. Sodium chloride was analyzed using a dry method, and it was confirmed that the dispersion pressure did not cause crystal breakage. Volume distributions (D10, D50, D90) and repeatability were output for both.
[0070] The open pore volume and throat distribution of bare core particles were determined according to GB / T 21650.1—2026 "Determination of Pore Size Distribution and Porosity of Solid Materials by Mercury Intrusion Porosimetry and Gas Adsorption Methods - Part 1: Mercury Intrusion Porosimetry". Appropriate blank and compression corrections were applied to the dried bare core particles, and the mercury contact angle, surface tension, pressure range, and methods for eliminating intergranular voids were recorded. The intrusive pore volume in the 3–30 μm throat region was divided by the total open pore volume of the core particles.
[0071] The perforation D10 of the membrane was determined using the three-dimensional reconstruction method of focused ion beam continuous slicing scanning electron microscopy as defined in this paper. This method is a research approach and does not employ laser diffraction standards. At least six particles were randomly selected layer by layer from the dry blank particles before S2, with each particle positioned at three different orientations, to obtain sufficient volume data to penetrate the full thickness of the ethyl cellulose membrane. Large-volume plasma focused ion beam or multi-field stitching was used to calibrate voxel dimensions and record sample shrinkage. Complete pores that are separated from each other and connect the inner and outer surfaces were statistically analyzed; boundary-cut pores were treated separately. Blind pores were not allowed to be counted as perforations. The cumulative number of effective pores should ideally be no less than 100; if this number is not reached, random sampling was expanded.
[0072] For each through hole, find the narrowest normal section along the centerline, and use its equal-area circle diameter d i As the equivalent diameter of the pore throat, V is the reconstructed volume of the pore located within the ethyl cellulose membrane. i Weighting. Press d. i Sort in ascending order, firstly make ΣV i d reaches or exceeds 10% of the total effective through-hole volume i Defined as the volumetric reference pore throat distribution D10.
[0073] Membrane thickness and embedment depth were measured while the finished product was dry. Sample moisture content and conditioning history were recorded before low-damage sectioning. Thickness was measured along the local surface normal; ethyl cellulose membrane and calcium alginate outer membrane were separately statistically analyzed, and the dry-state average thickness was given by weighting the area represented, along with the distribution. For a 0.3 μm outer membrane, the resolution of local cross-sectional analysis should be better than 0.05 μm; for embedment portions ranging from tens to hundreds of micrometers, a larger field of view was used for reconstruction and correspondence with a high-resolution interface image.
[0074] Material phase identification uses pure ethyl cellulose, sodium alginate, calcium alginate, and bare core particles as controls, combined with morphology, elemental distribution, and chemical imaging with sufficient resolution; when necessary, nano-infrared spectroscopy is used to distinguish calcium-containing alginate phases from other calcium-containing impurities. Overall coverage is determined using multi-directional surface chemical imaging and three-dimensional outer surface registration, with stratified sampling of random regions and weighting by representative area; whole-particle reconstruction is prioritized, and confidence intervals and uncertainties in unobserved areas must be provided during sampling estimation. Coverage C = (outer surface area of ethyl cellulose covered by calcium alginate outer membrane / outer surface area of ethyl cellulose) × 100%, with the denominator subtracting the opening of the through-pores; additionally, three-dimensional connectivity is used to check whether the outer membranes are interconnected. High coverage and interconnection are two separate conditions and cannot be substituted for each other.
[0075] In the finished product 3D data, distinguish between the ethyl cellulose backbone and the calcium alginate filling the pores. Calculate the d of the filled pores using the geometric boundary of the former, instead of using the width of the residual water channels as d. For the same pore, trace the connection and embedding parts, measuring L radially from the core-side pore opening, and measuring the maximum width W of the core branch perpendicular to the radial direction. Report L / d, the relationship between L and the average membrane thickness, W / d, and the continuity of the three parts for each pore.
[0076] Crosslinking was assessed using mutually corroborating evidence: co-localization of alginate and calcium in various regions; changes in carboxylate coordination spectra compared to the same batch of sodium alginate; and the water retention of the gel network after sufficient removal of free salts and its response to disintegration after chelation of calcium. For the latter, a sacrificial sample was used for a paired challenge at 25°C with 10 mmol / L calcium chloride solution and 50 mmol / L EDTA solution at pH 7.0 for 30 min each, and the released uronic acid and calcium were analyzed. A blank core membrane without alginate was set up to eliminate interference from calcium release from the core material. The EDTA test was for structural diagnostics, not performance or soil release testing. The equilibrium solubility (Cs) of diuron in the intended release medium was first measured at 25.0 ± 0.5°C, and its stability under light, container, and sampling processes was verified. The main medium was deionized water, and pH and conductivity were recorded. No organic solvents capable of dissolving ethyl cellulose or surfactants were added to improve solubility.
[0077] For each release container, take a random sample of no less than 30 particles and weigh them accurately. Calculate the initial dosage M0 based on the batch dry basis content. Use the same medium volume for all groups, with an initial recommended volume of 5.0 L. If the largest sample M0 still exceeds 0.1 CsV, increase the volume uniformly to ensure that the pre-set leakage conditions of this project are met even if all particles are released; apparent leakage cannot be achieved by reducing the number of particles to one or two. Place the particles in an inert coarse mesh basket that does not impede the passage of solute, and stir at a low speed of 40 r / min at 25.0 ± 0.5℃ in the dark to ensure that the particles are not mechanically ground. Set up two independent release containers for each batch.
[0078] All media were collected at 0.5, 2, 6, 24, 72 h and 7, 14, 28 d and immediately replaced with isothermal fresh media. The actual volume and replacement time were recorded. For each media sample split, one sample was completely dissolved in an organic solvent to release crystals, and the total diuron was measured. The other sample was separated using a 20 nm inorganic membrane with pre-validated recovery and crystal rejection rates, and the dissolved diuron was measured as defined in the operation. Separation validation must be repeated when using different pore sizes or other separation methods. For the complete media replacement procedure, the cumulative total release rate Qtotal,t = Σ(Ctotal,iVt) i The cumulative release rate of dissolved state Q_dissolved, t is calculated according to the corresponding concentration; the amount of particulate matter released is the difference between the two and the measurement error is reported. The total amount cannot be directly referred to as the amount of drug that has been dissolved and is available for use. After 28 days, the remaining particles, basket, and container wall are fully extracted, and the balance between the unreleased amount, the collected amount, and M0 is checked. This project initially sets 90% to 110% as the material balance check window. If it exceeds this range, the cause of recovery, degradation, or adsorption should be investigated and the process repeated.
[0079] For wet-dry cycling, granules that had not undergone release testing were soaked in deionized water at 25°C for 2 hours, drained for 60 seconds, and then dried at 30°C and 40% relative humidity for 22 hours, for a total of five cycles. The water volume and soaking liquid were recorded each time, and the total amount of drug lost was measured cumulatively. Coverage, cracks, and continuity were retested using independent sacrificial samples. After the cycle, a 6-hour release test was performed. The denominator was the remaining mass of diuron after the cycle to obtain Q. At the same time, the cumulative loss / initial drug amount of the five cycles was reported.
[0080] Thermal storage stability was determined according to the applicable procedure in GB / T 19136—2021 "Determination of Thermal Storage Stability of Pesticides". This research pre-set comparative conditions of sealed, identical packaging and 54±2℃ for 14 days. After sample removal and restoration to room temperature, moisture content, diuron content, and membrane structure were compared. Testing institutions must verify these conditions against the standard procedure they employ. The pesticide retention rate was defined using the same dry basis; increased wet basis concentration due to water loss should not be interpreted as increased activity. A 6-hour release test after thermal storage was added to identify cases where the content remained stable but the coating was damaged. Dust testing adopted the applicable procedure selected in GB / T 30360—2013 "Determination of Dust from Particulate Pesticides", following the particle fall conditions, dust collection or detection device, and unit of expression specified in the procedure. The same sampling rules were maintained before and after the test. Soil leaching evaluation was based on GB / T 31270.5—2025 "Test Guidelines for Environmental Safety Evaluation of Chemical Pesticides Part 5: Soil Leaching Test".
[0081] The extended experiment used one batch of sandy loam and one batch of loam soil. Particle size distribution, pH, organic carbon, cation exchange capacity, and maximum water holding capacity were measured and reported. The background concentration of diuron in the soil was below the method limit of quantitation. Glass columns with an inner diameter of 5.0 cm and a soil filling height of 30.0 cm were used. The columns were layered with a dry basis volumetric mass of 1.30 g / cm³, pre-wetted, and equilibrated for 24 h. Particles containing 1.00 mg of diuron were directly and uniformly applied to the surface of each column, and the particle mass and number were recorded. Two soil columns were prepared for each of the three independent formulations. All groups used the same 1 mmol / L calcium chloride solution as the leaching medium with fixed ionic strength. Specific results are only applicable to this medium and are not generalized to all rainwater or soil conditions.
[0082] Apply a medium equivalent to a 20.0 mm water layer on days 1, 3, 7, 14, and 21 after application. The volume for each application is 39.27 mL, calculated based on the cross-sectional area of the soil column, and should be added evenly over 2 hours. Cover the column opening to reduce unintended evaporation and prevent preferential flow from forming on the column side. Collect the bottom liquid in several applications and measure the total diuron and dissolved fraction. After 21 days, divide the soil column into four sections: 0–5 cm, 5–10 cm, 10–20 cm, and 20–30 cm. Extract the parent diuron from each section, and perform material balance analysis along with residual particles, the container wall, and the leachate. Record the early bottom leaching rate and cumulative leaching rate, as well as the surface and deep layer distribution. If no liquid is extracted from the soil column, it cannot be automatically assumed that the formulation has reduced leaching. If the parent diuron recovery is insufficient, it is necessary to investigate degradation or non-extractable residues; the missing amount should not be entirely attributed to particle fixation.
[0083] Indoor bioassay can draw on the test organization and plant inhibition rate evaluation approach of NY / T 1155.3—2006 "Guidelines for Indoor Bioassay of Pesticides - Herbicides Part 3: Activity Assay Test - Soil Spray Method". This formulation uses direct granulation and is specifically designed for expansion of the pot cultivation method as a granular formulation.
[0084] Barnyardgrass seeds with a clear source and no known resistance to diuron were selected. The same batch of seeds was used in the same experiment, and germination rate was measured first. Each pot contained 1.00 kg of dry base soil. The main comparative dose was fixed at 0.50 mg / kg of diuron in dry soil. Granules were weighed according to the content of each formulation, placed directly and evenly, without grinding or preparing a spray solution. Auxiliary doses of 0.25 mg / kg and 1.00 mg / kg were set up using Examples 1 and Comparative Examples 3 and 5 to verify whether the main dose fell within the resolvable range; these were only laboratory study doses. Each batch of formulation was used in four pots per treatment, with three independent batches of formulations constituting twelve pots. Untreated blanks and untreated granule blanks were also set up and randomly placed in blocks.
[0085] Two independent sowing cohorts were set up: In the first cohort, 20 seeds were sown per pot on the day of application and covered with a thin layer of soil; the survival rate and aboveground fresh weight were measured 21 days later. In the second cohort, the seeds were applied and the soil was kept in the same pot for 28 days before sowing 20 seeds from the same batch and continuing cultivation for another 21 days. Soil from the same pots used in the first cohort that had already been harvested was not used to replace soil from the second cohort. Day / night temperatures were controlled at 25 / 20℃, and light / dark hours at 16 / 8h. Moisture was controlled by weighing, with a cycle every 7 days of decreasing the water content from 70% to 30% of the maximum water holding capacity and then replenishing it to 70%. Actual water volume and soil moisture were recorded consistently across all groups. Fresh weight inhibition rate I = (1 - fresh weight of the treatment group / fresh weight of the corresponding control group) × 100%. Early I0, I21, and I2 after 28 days of soil cultivation were reported separately. 28 21. The duration of effectiveness cannot be inferred from a single short-term preventive effect.
[0086] Table 1
[0087] Note: EC stands for ethyl cellulose, and the outer membrane is a calcium alginate membrane. L, d, and W represent the embedment depth, equivalent diameter of the pore throat, and maximum transverse width of the branch at the same connection location, respectively; further verification is required to ensure that L is not less than the EC membrane thickness.
[0088] Table 2
[0089] Note: The release rate 6 hours after cycling is calculated using the remaining mass of diuron after cycling as the denominator, and the other corresponding proportions are calculated using the initial amount of drug in the experiment as the denominator. Total release includes dissolved state and escaped crystals; the total release rate and dissolved state release rate at different times cannot be subtracted to calculate the amount of crystals escaped.
[0090] Table 3
[0091] Note: Using the same dust collection and weighing conditions and sample mass, and taking the dust collection mass of Example 1 as the benchmark, J is defined as 100 × sample dust collection mass / dust collection mass of Example 1.
[0092] Table 4
[0093] Note: I0, 21 The fresh weight inhibition rate was determined by sowing on the day of application and culturing for 21 days. 28 , 21 To determine the fresh weight inhibition rate after 28 days of soil conditioning following pesticide application and 21 days of seed culture, two independent pot cohorts were used.
[0094] As shown in Table 1, the dry basis diuron content of the granules obtained in Example 1 was 13.0%, the thickness of the ethyl cellulose membrane and the outer membrane of the calcium alginate were 17.5 μm and 0.90 μm, respectively, and the continuous coverage of the outer membrane reached 97.5%. The ratio of the core embedding depth L to the equivalent diameter d of the pore throat was 3.0, and the ratio of the maximum transverse width W of the branch to the equivalent diameter d of the pore throat was 1.5, forming a transmembrane connection structure that continuously extends from the calcium alginate outer membrane, the pore connecting part to the core embedding part. In Examples 2 to 7, the continuous coverage of the outer membrane was maintained at 95.0% to 99.0%, L / d was maintained at 2.0 to 4.0, and W / d was maintained at 1.1 to 2.0, indicating that the process window can form a granular structure with continuous outer membrane coverage and geometric anchoring characteristics within the core.
[0095] A comparison of Example 1 with Comparative Examples 1 and 2 shows that the particle size of sodium chloride microcrystals, the matching relationship between sodium chloride microcrystals and the thickness of the ethyl cellulose membrane, and the shaping and drying before coating all affect the formation of transmembrane pores and subsequent drug loading capacity. In Comparative Example 2, after reducing the volume-based particle size (D10 / D90) of sodium chloride microcrystals from 35 μm / 55 μm to 8 μm / 15 μm, the dry-basis diuron content decreased from 13.0% in Example 1 to 4.0%, and L / d and W / d decreased to 1.0 and 0.8, respectively. The transmembrane structure showed only sporadic connections; its 28-day dissolved diuron release rate was only 24%, and the fresh weight inhibition rate after 28 days of soil conditioning was only 41%. This indicates that excessively low release does not necessarily indicate good sustained-release performance, but may be due to insufficient transmembrane pathways leading to a simultaneous decrease in drug loading and effective drug delivery. Example 1 demonstrates how sodium chloride microcrystals at least partially penetrate the ethyl cellulose membrane, and how a polyvinyl alcohol layer isolates the core pores during coating, making it difficult for the ethyl cellulose coating solution to penetrate and clog the core pores, thereby providing a continuous pathway for subsequent negative pressure drug loading and alginate infiltration.
[0096] Example 1 and Comparative Example 3 had the same dry-basis diuron content and similar outer film coverage. However, in Comparative Example 3, after the depressurization-repressurization immersion with sodium alginate solution was omitted, the L / d decreased from 3.0 to 1.0, and the W / d decreased from 1.5 to 0.8, with only shallow connections forming within the core. The cumulative diuron loss rate after five wet-dry cycles increased from 12% to 30%, and the cumulative leaching rate 6 hours after the cycle increased from 7% to 21%. The 21-day diuron leaching rates in sandy loam and loam soils for Example 1 were 0.20% and 0.08%, respectively, while those for Comparative Example 3 were 0.60% and 0.24%, respectively, representing a relative reduction of approximately 66.7% in Example 1. Simultaneously, the fresh weight inhibition rate after 28 days of soil conditioning in Example 1 was 79%, an increase of 12 percentage points compared to 67% in Comparative Example 3. Since the dry-basis drug loading was the same in both groups, the above differences indicate that the performance improvement did not originate from an increase in diuron dosage, but was mainly related to the entry of alginate into the core pores and the formation of embedded portions and lateral branches within the core. This embedded structure improves the mechanical anchoring ability between the outer membrane and the porous core, and reduces the sudden release caused by outer membrane delamination and pore enlargement during wet-dry cycles.
[0097] The comparison between Example 1 and Comparative Example 5 further demonstrates that low-concentration pre-crosslinking and higher-concentration secondary crosslinking have a synergistic effect. In Comparative Example 5, after directly increasing the first crosslinking bath to 0.15 mol / L, although the initial outer membrane coverage remained at 97.5%, the cumulative loss rate after five wet-dry cycles reached 24%, the cumulative escape rate after 6 hours of cycling reached 17%, the outer membrane coverage decreased to 77% after cycling, and the fresh weight inhibition rate after 28 days of soil conditioning was 68%. In Example 1, a low-concentration pre-crosslinking with 0.035 mol / L calcium chloride was used, allowing calcium ions to enter the pore connections and core embeddings before the outer alginate layer was completely densified. Then, a secondary crosslinking with 0.15 mol / L calcium chloride was used to further stabilize the outer membrane; the cumulative loss rate after five cycles decreased to 12%, the cumulative escape rate after 6 hours of cycling decreased to 7%, the outer membrane coverage remained at 95% after cycling, and the fresh weight inhibition rate after 28 days of soil conditioning increased to 79%. This result supports the role of two-step calcium crosslinking in balancing internal connection formation and external membrane structure stability, rather than simply relying on increasing the calcium chloride concentration to increase surface crosslinking.
[0098] Comparative Examples 4 and 6 further illustrate the importance of outer film formation and drying conditions. The fresh weight inhibition rates at the time of application in both groups reached 93% and 94%, respectively, but the cumulative escape rates over 6 hours reached 12% and 13%, respectively, and the cumulative loss rates after five cycles reached 33% and 35%, respectively. After 28 days of soil conditioning, the fresh weight inhibition rates decreased to 65% and 64%, respectively. Specifically, the cumulative escape rate over 6 hours after heat storage in Comparative Example 6 reached 19%, and the outer film coverage rate after cycles was only 65%, while the corresponding values in Example 1 were 6% and 95%, respectively. The diuron content retention rate after heat storage in each group remained between 98% and 99%, indicating that the above differences mainly stemmed from outer film cracking, delamination, and interfacial structural instability, rather than significant chemical degradation of diuron.
[0099] Based on the combined results of release and herbicidal activity, in Example 1, the cumulative release of total diuron over 6 hours was 5%, and the cumulative release of dissolved diuron over 28 days was 72%. The fresh weight inhibition rates at the time of application and after 28 days of soil conditioning were 86% and 79%, respectively. In Examples 2-7, the cumulative release over 6 hours was 3%-9%, the cumulative release of dissolved diuron over 28 days was 54%-82%, and the fresh weight inhibition rate after 28 days of soil conditioning remained at 74%-82%. This indicates that the present invention does not simply block diuron, but rather maintains the continuous release of the active ingredient in the later stages while limiting early crystal release and soil migration. Although Comparative Example 2 had a lower soil column leaching rate, its fresh weight inhibition rates at the two sowing stages were only 48% and 41%, respectively. This further illustrates that when evaluating slow-release granules, it is necessary to simultaneously consider early release, long-term dissolved release, soil migration, and late-stage herbicidal activity; the effectiveness of the technology cannot be judged solely by low leaching or low release rates.
[0100] In summary, this invention utilizes a combination of techniques, including sodium chloride microcrystalline permeabilization, polyvinyl alcohol temporary sealing, depressurized-repressurized drug loading, alginate impregnation, outer layer concentration gradient construction, and two-step calcium crosslinking, to create a loading pathway within the granules that connects the original pores outside the membrane to the interconnected pores inside the membrane to the core pores, and a fixed structure consisting of the calcium alginate outer membrane portion, the pore-connecting portion, and the core-embedded portion and its branches. The former structure addresses the problem of the porous core granules being unable to effectively load the drug again after ethyl cellulose coating, while the latter structure improves the binding stability between the outer membrane and the core granules and regulates the release process of diuron from the core pores to the external environment. This results in a better balance between drug loading, early burst release control, dry-wet cycle structure maintenance, soil migration control, and late-stage herbicidal activity in the resulting granules, avoiding problems such as pore blockage, outer membrane delamination, early burst release, or excessive inhibition of the active ingredient that are common in ordinary surface-coated granules.
[0101] Figure 1In the diagram, 101 represents the sintered diatomaceous earth core skeleton, 102 represents the ethyl cellulose membrane, 103 represents the internal through-hole spanning the entire thickness of the ethyl cellulose membrane, 104 represents the core particle pores connected to the internal through-hole 103, 105 represents the original pores on the outer surface of the membrane, and 106 represents the pores on the inner surface of the membrane. Figure 1 As can be seen from the actual continuous slice sequence verification, it is possible to continuously trace from the original external pore 105 along the internal through-hole 103 to the internal pore 106, and further into the core particle pores 104. This connecting path spans the entire thickness of the ethyl cellulose membrane 102, and does not pass through cutting grooves, field boundaries, membrane cracks, or damaged areas formed during sample preparation. After the sodium chloride microcrystals and polyvinyl alcohol layer are removed by water extraction, a through-structure is formed in the ethyl cellulose membrane that communicates with the internal pores of the sintered diatomaceous earth core particles. Figure 1 The diagram shows the dry geometric connectivity of blank particles before drug loading and coating, illustrating the structural features of "extraction forming through pores" and "through pores communicating with the pores of the core particles".
[0102] Figure 2 In this diagram, 101 represents the sintered diatomaceous earth core skeleton, 102 represents the ethyl cellulose membrane, 201 represents the calcium alginate outer membrane covering the outside of the ethyl cellulose membrane, 202 represents the pore-connecting portion located within the through-holes and spanning the ethyl cellulose membrane 102, and 203 represents the core-embedded portion extending from the pore-connecting portion 202 into the core pores. Figure 2 As can be seen, the calcium alginate outer membrane portion 201 can be continuously traced to the pore-connecting portion 202 within the through-hole, and from the pore-connecting portion 202 to the core-embedded portion 203 within the core particle pores. These three parts constitute a continuous, interconnected phase within the three-dimensional voxel. The pore-connecting portion 202 spans the entire thickness of the ethyl cellulose membrane 102, and the core-embedded portion 203 extends into the interior of the sintered diatomaceous earth core particle. A low-concentration sodium alginate solution enters the core particle pores through the pre-formed through-hole under pressure differential, subsequently connecting with the outer layer of sprayed sodium alginate. After two-step calcium cross-linking, a continuous transmembrane connection structure of "calcium alginate outer membrane portion 201 – pore-connecting portion 202 – core-embedded portion 203" is finally formed in the particle.
[0103] The above are merely specific embodiments of the present invention, but the technical features of the present invention are not limited thereto. Any simple changes, equivalent substitutions, or modifications made based on the present invention to solve essentially the same technical problems and achieve essentially the same technical effects are all covered within the protection scope of the present invention.
Claims
1. A preparation process for a herbicide granular formulation containing diuron, characterized in that: Specifically, the following steps are included: S1. A water-soluble polyvinyl alcohol layer with closed pores is formed on the surface of sintered diatomaceous earth core particles with interconnected pores; sodium chloride microcrystals are attached to the surface of this layer at intervals, and then an ethyl cellulose ethanol solution is sprayed to form a film, such that at least some of the microcrystals have a height greater than the film thickness along the normal direction of their respective surfaces, with the bottom contacting the polyvinyl alcohol layer and the top exposing the film; sodium chloride and polyvinyl alcohol are removed by water extraction, and the particles are dried to obtain a coated blank particle with through pores connecting the core particle pores to the outside. S2. The coated blank particles are impregnated with an aqueous suspension of diuron with a volume reference particle size D90 of 0.3-0.8 μm under reduced pressure and re-pressurization to allow diuron crystals to enter the core particle pores. The surface liquid is removed and the particles are dried to obtain drug-loaded particles. S3. The drug-loaded particles are impregnated with the first sodium alginate aqueous solution under reduced pressure and re-pressurization. After the solution is drained, a second sodium alginate aqueous solution with a higher sodium alginate mass fraction than the first sodium alginate aqueous solution is sprayed on it, so that the two solutions are continuously distributed outside the membrane, in the through holes and in the pores of the connected core particles. S4. Without drying, pre-crosslink the herbicide in a 0.02-0.05 mol / L calcium chloride aqueous solution, then continue crosslinking in a 0.10-0.20 mol / L calcium chloride aqueous solution, rinse, and dry to form a calcium alginate phase in which the outer membrane is continuously connected to the core granule pores via the connecting part in the through-holes, thus obtaining the herbicide granules.
2. The preparation process of a diuron-containing herbicide granule according to claim 1, characterized in that: In step S1, the core particle has a particle size of 0.8–1.6 mm and an open pore volume of 0.4–0.8 mL / g; according to the pore volume distribution measured by mercury intrusion porosimetry, the pore volume with a throat diameter of 3–30 μm accounts for 60%–85% of the total open pore volume; the degree of alcoholysis of the polyvinyl alcohol is 87%–89% (mole fraction); the polyvinyl alcohol layer is formed by spraying a polyvinyl alcohol aqueous solution onto the surface of the core particle in stages and drying it, and its dry average thickness is 2–5 μm; the polyvinyl alcohol layer is dried before spraying the ethyl cellulose ethanol solution.
3. The preparation process of a diuron-containing herbicide granule according to claim 1, characterized in that: In step S1, sodium chloride microcrystals are attached to the surface of the polyvinyl alcohol layer in separate monolayers. According to the volume distribution measured by dry laser diffraction, the D10 of the sodium chloride microcrystals is 30-40 μm and the D90 is no greater than 60 μm. The ethyl cellulose ethanol solution is prepared with anhydrous ethanol and contains 10%-20% triethyl citrate by mass of ethyl cellulose. Fluidized bed intermittent spraying and intermittent drying are used to form an ethyl cellulose membrane with an average dry thickness of 10-25 μm. The height of the microcrystals exposed on the membrane surface along the normal direction of the surface is no less than 1.2 times the membrane thickness at that point. The membrane is extracted with water at 35-45°C through multiple water changes, and the residual sodium chloride in the resulting coated blank particles does not exceed 0.2% of its dry basis mass.
4. The preparation process of a diuron-containing herbicide granule according to claim 3, characterized in that: In step S2, diuron, polyvinylpyrrolidone, alkyl glycosides, and water are mixed and wet-milled to obtain an aqueous suspension with a diuron mass fraction of 20%–25%. The amounts of polyvinylpyrrolidone and alkyl glycosides are 1%–3% and 0.2%–0.5% of the diuron mass, respectively. The volume reference particle size D90 of diuron is determined by wet laser diffraction and is not greater than one-fifth of the volume reference pore throat equivalent diameter distribution D10 of the through-holes before drug loading. The pore throat distribution is determined by three-dimensional reconstruction using focused ion beam continuous section scanning electron microscopy. The through-holes separated from each other in the membrane are used as statistical units. The diameter of the circle with the narrowest cross-section along the center line of each pore is the equivalent diameter of the pore throat. The pore throat equivalent diameter is the pore throat equivalent diameter when the cumulative volume first reaches or exceeds 10% of the total through-hole volume, weighted by the reconstruction volume of each pore in the membrane.
5. The preparation process of a diuron-containing herbicide granule according to claim 4, characterized in that: In step S2, the coated blank particles are placed in a sealed container, and the pressure is evacuated to an absolute pressure of 20-40 kPa and maintained for 2-5 minutes. Under this pressure, the aqueous suspension is injected until the particles are submerged. Then, the pressure is restored to normal within 1-3 minutes and maintained for 5-10 minutes. The surface liquid is drained off, and the particles are sprayed with deionized water for 5-15 seconds and then drained immediately. The particles are then dried at 35-45°C. The amount of water used for spraying is 0.5-1.0 mL per gram of coated blank particles.
6. The preparation process of a diuron-containing herbicide granule according to claim 1, characterized in that: In step S3, the mass fraction of the first sodium alginate aqueous solution is 0.6%–1.0%, and the mass fraction of the second sodium alginate aqueous solution is 1.5%–2.5%. The drug-loaded particles are immersed in the first sodium alginate aqueous solution and maintained at an absolute pressure of 15–30 kPa for 1–3 minutes, then restored to normal pressure and maintained for 3–8 minutes. Both aqueous solutions are prepared with the same batch of sodium alginate, and no calcium salts are added before contact with the particles. After the impregnation and spraying are completed, step S4 is carried out without intermediate drying.
7. The preparation process of a diuron-containing herbicide granule according to claim 6, characterized in that: In step S4, pre-crosslinking and continued crosslinking are carried out in two separate calcium chloride crosslinking baths. The pre-crosslinking time is 3-10 min, and the continued crosslinking time is 20-40 min. The temperature for both crosslinking is 20-30℃. The initial solution volume of each crosslinking bath is 20-40 mL per gram of wet particles obtained in step S3. The particles are kept submerged during crosslinking. After crosslinking, the particles are rinsed with a calcium chloride aqueous solution with a concentration of 5-15 mmol / L.
8. The preparation process of the diuron-containing herbicide granules according to claim 7, characterized in that, The drying process in step S4 includes: first drying in air at 25-30°C and 60%-75% relative humidity for 1-3 hours, and then drying in air at 35-45°C and 30% relative humidity until the moisture content of the granules is 1%-3% by mass; the content of diuron in the resulting granules is 8%-18% by dry basis mass.
9. A diuron-containing herbicide granular agent prepared by the method according to any one of claims 1 to 8, characterized in that: The product comprises sintered diatomaceous earth core particles with interconnected pores, an ethyl cellulose membrane covering the core particles, diuron crystals distributed within the pores of the core particles, and a calcium alginate phase. The ethyl cellulose membrane has through-holes connecting the core particle pores to the outside. The calcium alginate phase includes an outer membrane portion outside the membrane, a connecting portion penetrating the through-holes, and an embedded portion within the core particle pores, all three being continuously connected and containing a coordination cross-linking structure formed between carboxyl groups of different alginate chains by calcium ions. The core particles have a particle size of 0.8–1.6 mm, the ethyl cellulose membrane has a dry average thickness of 10–25 μm, and diuron accounts for 8%–18% of the dry basis mass of the granules. The outer membrane portions are interconnected, and their coverage area accounts for not less than 95% of the outer surface area of the ethyl cellulose membrane, excluding the area of the through-hole openings.
10. The diuron-containing herbicide granules according to claim 9, characterized in that: The dry average thickness of the outer membrane is 0.3–1.5 μm; the depth L of the embedded portion extending radially inward from the core particle side opening of the corresponding through hole is not less than twice the equivalent diameter d of the throat of the through hole, and not less than the dry average thickness of the ethyl cellulose membrane; the embedded portion has a branch extending into a core particle branch hole communicating with the through hole, and the maximum width of the branch in a plane perpendicular to the radial direction is greater than d.
Citation Information
Patent Citations
Preparation method of pesticide diuron slow controlled release nanometer composite material
CN101773112A