An automatic repair device for pipe welding seams
By coordinating the fixed welding head and the welding head, and combining the arc-shaped grinding block and hook plate controlled by the laser sensor and electromagnet, synchronous internal and external repair of pipeline welds is achieved, solving the problem of uneven weld formation, improving repair accuracy and quality, reducing weld slag residue, and enhancing the structural reliability of the pipeline.
Patent Information
- Application Number
- CN202611618872.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-20
- Publication Date
- 2026-11-17
AI Technical Summary
Existing pipeline weld repair equipment is prone to uneven penetration depth during the welding process due to fluctuations in welding parameters and assembly deviations. This results in uneven weld formation, defects such as depressions and excessive weld height, which affect the flatness of the pipeline surface and the flow of the medium, increase corrosion losses, and reduce structural reliability.
Using a combination of a fixed welding head and a welding head, combined with a laser sensor to detect the location of missed welds in real time, the welding head is moved along the outer arc surface of the pipe by a rotating ring to repair the external weld. The weld repair on the inner wall of the pipe is achieved by a fixed motor driving gear transmission. Electromagnets are used to control the magnetic attraction and disengagement of the arc-shaped grinding block and hook plate to avoid interference. A negative pressure suction pump is used to clean the welding slag, so as to achieve simultaneous repair of the internal and external welds.
It improves the accuracy and quality of weld repair, reduces weld defects, enhances the reliability of pipe weld joints and the efficiency of inner wall cleaning, prevents weld slag residue pollution, and ensures long-term stable operation of pipelines.
Smart Images

Figure CN123103301A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of pipeline weld repair technology, specifically an automatic weld repair device for pipeline welding. Background Technology
[0002] Welding technology is widely used in the mechanical and electronic fields. It is a processing technology that joins metal parts by heating, high temperature or high pressure. After welding, the weld seam is formed, which affects the appearance. Some special weld seams also have specifications for the weld reinforcement (the height of the metal on the line connecting the two weld toes on the weld surface).
[0003] A patent with publication number CN120502909A discloses an automatic welding mechanism for pipe annular welds, including a workbench. The workbench has four casters at its bottom corners, and side guards are connected to the top of the workbench at the front and back. A steering shaft is rotatably connected to the upper part of the side guards, and a flip shell is connected between two steering shafts. The flip shell has an opening at its upper end, and a central shaft is rotatably connected to the center of the inner wall of the flip shell. A receiving seat is connected to the top of the central shaft, and several stepped holes are circumferentially opened on the top of the receiving seat. A hollow tube is rotatably connected to the lower part of the inner cavity of the stepped holes, and a tray is connected to the upper part of the outer wall of the hollow tube. A welding frame is connected to the top left side of the workbench.
[0004] However, existing pipeline weld repair equipment suffers from several drawbacks during use. Because the two pipelines are assembled using a ring-shaped butt joint, the welding head acts on the ring-shaped butt joint. The welding heat source melts the base material at the butt joint, and the filler metal melts and flows into the joint to form a molten pool. After the molten pool cools and crystallizes, the connection between the two pipelines is achieved. However, due to fluctuations in welding parameters and assembly deviations, the penetration depth at the joint is difficult to maintain consistently. This results in unevenly formed welds at the ring-shaped butt joint, with defects such as localized depressions and excessive weld height. Consequently, the surface smoothness of the pipe joint is poor. When the pipeline is put into subsequent transportation operations, the uneven surface of the weld disrupts the flow of the medium, easily causing impurities in the medium to accumulate and adhere at the weld. Long-term operation exacerbates corrosion and wear in the weld area, reduces the structural reliability of the pipe joint, and adversely affects the long-term stable operation of the pipeline.
[0005] Therefore, the present invention provides an automatic repair device for weld seams in pipeline welding. Summary of the Invention
[0006] In order to overcome the shortcomings of the prior art, at least one technical problem raised in the background art is solved.
[0007] The technical solution adopted by the present invention to solve its technical problem is as follows: The present invention provides an automatic weld repair device for pipe welding, comprising a machine body, two fixing plates fixedly connected to the upper surface of the machine body, a welded pipe body placed above the two fixing plates, a positioning plate fixedly connected to the upper surface of the machine body, a fixing ring fixedly connected to the upper surface of the positioning plate, a rotating ring rotatably connected inside the fixing ring, a welding head fixedly connected to the inner wall of the rotating ring, an auxiliary component provided on the upper surface of the machine body, the auxiliary component including a positioning box fixedly connected to the upper surface of the machine body, a positioning column fixedly connected to one side of the positioning box, a positioning ring fixedly connected to one end of the positioning column, a connecting ring rotatably connected inside the positioning ring, an arc-shaped grinding block and a fixed welding head provided on the surface of the connecting ring, and a collection pipe opened inside the positioning column.
[0008] Preferably, the auxiliary component further includes a positioning frame fixed to the arc surface of the connecting ring, a plurality of positioning springs are fixed to the inner wall of the positioning frame, the bottom ends of the plurality of positioning springs are fixed to the same positioning rod, the bottom end of the positioning rod is fixed to an arc-shaped grinding block, and an electromagnet is fixed to the top wall of the positioning frame.
[0009] Preferably, the cross-section of the arc-shaped grinding block is one-third of a circular arc, and the end of the arc-shaped grinding block does not abut against the inner wall of the tube, while the middle part of the arc-shaped grinding block abuts against the inner wall of the tube.
[0010] Preferably, the circumferential surface of the connecting ring is further provided with a processing component, the processing component including a hook plate disposed on the circumferential surface of the connecting ring, the hook plate being used to process residual dust and welding slag on the inner wall of the pipe.
[0011] Preferably, the processing component includes a connecting frame fixed to the arc surface of the connecting ring, a plurality of connecting springs fixed inside the connecting frame, the bottom ends of the plurality of connecting springs being fixed to the same hook plate, a guide frame being fixed to one side of the hook plate, and a guide groove being formed on the arc surface of the hook plate.
[0012] Preferably, the connecting ring has a collection groove inside, an auxiliary ring is rotatably connected inside the connecting ring, a guide tube is fixedly connected to the inner wall of the auxiliary ring, the guide tube is fixedly connected to the positioning post, and both the guide tube and the positioning post have fixing grooves inside.
[0013] Preferably, a fixed motor is fixedly connected inside the positioning column, a gear is fixedly connected to the output end of the fixed motor, and a plurality of gear teeth are fixedly connected to the inner wall of the connecting ring, with the gear meshing with the gear teeth.
[0014] Preferably, the electromagnet is initially energized and magnetic, and the magnetically attracted positioning rod and hook plate, that is, the arc-shaped grinding block and the hook plate are not initially in contact with the annular inner wall of the tube.
[0015] Preferably, after the welding of the two tubes is completed, the tubes are placed on the fixed plate on the upper surface of the machine body. The fixed plate has an arc-shaped groove corresponding to the tube. After placement, the built-in guide rail of the positioning plate is activated, driving the rotating ring to drive the welding head fixed to its inner wall to repair the weld. A laser sensor is fixed to the side of the welding head. The laser sensor detects the missed welds during the welding process, thereby completing the weld repair on the outer arc surface of the two tubes. At this time, the fixed motor inside the positioning column is activated. The fixed motor drives the gear to rotate, which in turn drives the connecting ring fixed to the gear to rotate. The rotation of the connecting ring drives the fixed welding head fixed to its arc surface to weld the joint at the inside of the tube, thereby completing the weld generated during the welding of the molten pool. At this time, the arc-shaped grinding block and the hook plate are not in contact with the inner wall of the tube due to the magnetic attraction of the electromagnet. After the weld repair work at the joint of the inner wall of the tube is completed, the electromagnet is de-energized to release the magnetic attraction on the arc-shaped grinding block and the hook plate.
[0016] Preferably, after the arc-shaped grinding block and hook plate are demagnetized one by one, the elastic force of the positioning spring and connecting spring is released, thereby causing the arc-shaped grinding block and hook plate to extend out of the positioning frame and connecting frame. The middle part of the arc-shaped grinding block will abut against the inner wall of the tube, so that when encountering a protruding weld point, the arc-shaped end of the arc-shaped grinding block will not directly push against the weld point, but will contact the weld point with its arc surface to perform grinding work. After the arc-shaped grinding block completes the grinding work, the hook plate on the circumference of the connecting ring is released. The hook plate is arc-shaped, and the arc-shaped tip of the hook plate directly abuts against the inner wall of the tube. Furthermore, during the rotation of the connecting ring, the arc-shaped hook plate will scrape up the metal dust and welding slag inside the pipe. After being scraped up, the metal dust and welding slag will be guided into the guide frame by the guide groove opened on the surface of the hook plate. Then, as the hook plate rotates and the height increases, the metal dust and welding slag will fall to the bottom wall of the collection tank. The metal dust and welding slag ground by the arc-shaped grinding block will always be located at the bottom of the pipe under the action of gravity. Then, by starting the negative pressure suction pump inside the positioning box, the metal dust and welding slag ground in the collection tank will be suctioned under negative pressure, thereby completing the weld repair work of the pipe.
[0017] The beneficial effects of this invention are as follows: 1. The automatic weld repair equipment for pipeline welding described in this invention completes the pipe weld repair operation through the cooperation of a fixed welding head and a welding head. Externally, a rotating ring drives the welding head to move along the outer arc surface of the pipe body. Combined with a laser sensor to detect the location of missed welds in real time, it can specifically repair the welds on the outer wall of the pipe body, effectively identifying weld defects and improving the accuracy of external weld repair. Internally, a fixed motor drives gear transmission to rotate the connecting ring and the fixed welding head, performing repair welding on the inner wall weld at the pipe body joint, thereby compensating for defects that occur during the molten pool formation stage. This system enables simultaneous repair of weld defects inside and outside the pipe. During the internal repair welding process, the arc-shaped grinding block and hook plate are kept detached from the inner wall of the pipe by the magnetic attraction of the electromagnet, avoiding interference and scratches between the arc-shaped grinding block and hook plate and the high-temperature weld. This prevents damage to components and disruption of weld formation during the repair welding process. After the internal wall repair welding process is completed, the arc-shaped grinding block and hook plate can be released by de-energizing the electromagnet, facilitating subsequent internal wall grinding and cleaning processes. This effectively improves the repair quality of the pipe's circumferential butt weld, reduces the retention of weld defects, and enhances the overall reliability of the pipe's welded joints.
[0018] 2. The automatic weld repair equipment for pipeline welding described in this invention utilizes the de-energization of an electromagnet to release an arc-shaped grinding block and a hook plate. Relying on positioning springs and connecting springs to release elastic force, the arc-shaped grinding block and hook plate extend out of the positioning frame and connecting frame respectively, achieving automatic positioning of the grinding and slag removal mechanism. The arc-shaped grinding block adopts an arc-shaped structure with its middle part contacting the inner wall of the pipe. When facing protruding weld points, it grinds with its arc surface in close contact, avoiding hard pushing and bumping of the weld point at the end. This allows for smooth grinding and repair of protruding parts of the inner wall weld, reducing damage to the pipe base material during the grinding process and improving the surface grinding quality of the weld. After grinding, the electromagnet of the hook plate is de-energized, releasing the hook plate and causing it to rotate with the connecting ring. The arc-shaped hook plate adheres to the inner wall of the pipe, scraping away the metal dust and welding slag adhering to the inner wall. The scraped waste is guided into the guide frame through the guide groove of the hook plate. As the hook plate rotates and rises, the welding slag and dust fall into the collection tank by gravity. The debris generated by the arc-shaped grinding block also collects at the lower half of the pipe ring under gravity. Then, a negative pressure suction pump is used to centrally extract and collect the waste in the collection tank, achieving unified recycling and treatment of grinding waste. This reduces welding slag and dust residue, avoids secondary pollution caused by residue remaining in the pipe, and further ensures the processing quality of the welds inside the pipe. Attached Figure Description
[0019] The invention will now be further described with reference to the accompanying drawings.
[0020] Figure 1 This is a perspective view of Embodiment 1 of the present invention; Figure 2 This is a schematic diagram of the structure of the welding head of the present invention; Figure 3 This is a schematic diagram of the structure of the auxiliary component of the present invention; Figure 4 This is a schematic diagram of the internal structure of the connecting ring of the present invention; Figure 5 This is a schematic diagram of the disassembled structure of the connecting ring of the present invention; Figure 6 This is a front view of the connecting ring of the present invention; Figure 7 This is a cross-sectional view of the positioning post of the present invention; In the diagram: 1. Body; 11. Fixing plate; 12. Positioning plate; 13. Fixing ring; 14. Tube body; 15. Rotating ring; 16. Welding head; 17. Laser sensor; 2. Positioning box; 21. Positioning post; 22. Positioning ring; 23. Connecting ring; 24. Gear tooth; 25. Fixed motor; 26. Gear; 27. Fixed welding head; 28. Positioning frame; 29. Positioning spring; 210. Positioning rod; 211. Arc-shaped grinding block; 212. Electromagnet; 213. Connecting frame; 214. Connecting spring; 215. Hook plate; 216. Guide groove; 217. Guide frame; 218. Fixed groove; 219. Guide tube; 220. Auxiliary ring; 221. Collection groove; 222. Collection pipe. Detailed Implementation
[0021] To make the technical means, creative features, objectives and effects of this invention easier to understand, the invention will be further described below in conjunction with specific embodiments.
[0022] Example 1: As Figures 1 to 7 As shown in the embodiment of the present invention, an automatic weld repair device for pipe welding includes two fixed plates 11 fixed to the upper surface of the machine body 1. A welded pipe body 14 is placed above the two fixed plates 11. A positioning plate 12 is also fixed to the upper surface of the machine body 1. A fixing ring 13 is fixed to the upper surface of the positioning plate 12. A rotating ring 15 is rotatably connected inside the fixing ring 13. A welding head 16 is fixed to the inner wall of the rotating ring 15. An auxiliary component is provided on the upper surface of the machine body 1. The auxiliary component includes a positioning box 2 fixed to the upper surface of the machine body 1. A positioning column 21 is fixed to one side of the positioning box 2. A positioning ring 22 is fixed to one end of the positioning column 21. A connecting... Ring 23, the surface of the connecting ring 23 is provided with arc-shaped grinding block 211 and fixed welding head 27, and the positioning column 21 is provided with collection pipe 222; the auxiliary component also includes a positioning frame 28 fixed to the arc surface of the connecting ring 23, a number of positioning springs 29 are fixed to the inner wall of the positioning frame 28, the bottom end of the number of positioning springs 29 is fixed to the same positioning rod 210, the bottom end of the positioning rod 210 is fixed to the arc-shaped grinding block 211, and the top wall of the positioning frame 28 is fixed to an electromagnet 212; the cross section of the arc-shaped grinding block 211 is one-third arc-shaped, and the end of the arc-shaped grinding block 211 does not abut against the inner wall of the tube body 14, while the middle part of the arc-shaped grinding block 211 abuts against the inner wall of the tube body 14.
[0023] Specifically, in the use of existing pipeline weld repair equipment, since two pipelines are assembled in a ring-shaped butt joint, the welding head 16 acts on the ring-shaped butt joint of the pipeline. The welding heat source melts the base material at the pipeline butt joint, and the filler metal melts and flows into the joint to form a molten pool. After the molten pool cools and crystallizes, the connection between the two pipelines is achieved. Affected by factors such as fluctuations in welding parameters and assembly deviations, the penetration depth at the joint is difficult to be consistent, resulting in an uneven weld at the ring-shaped butt joint of the pipeline. Defects such as depressions and excessive height of the weld may appear locally, resulting in poor surface flatness of the pipeline butt joint. When the pipeline is put into subsequent transportation conditions, the uneven surface of the weld will disrupt the flow of the medium and easily cause impurities in the medium to accumulate and adhere at the weld position. Long-term operation will aggravate corrosion and wear in the weld area, reduce the structural reliability of the pipeline butt joint, and have an adverse effect on the long-term stable operation of the pipeline. Therefore, the present invention solves the above problems by setting the above structure. First, after the welding of the two tubes 14 is completed, the tubes 14 are placed on the fixing plate 11 on the upper surface of the machine body 1. The fixing plate 11 has an arc-shaped groove corresponding to the tubes 14. After placement, the built-in guide rail of the positioning plate 12 is activated, and the rotating ring 15 is driven to drive the welding head 16 fixed to its inner wall to repair the weld. A laser sensor 17 is fixed to the side of the welding head 16. The laser sensor 17 detects the weld seam that is missed during the welding process, thereby completing the weld seam repair of the outer arc surface of the two tubes 14. At this time, the positioning column 21 is activated. The internal fixed motor 25 drives the gear 26 to rotate, which in turn drives the connecting ring 23 fixed to the gear 24 to rotate. The rotation of the connecting ring 23 drives the fixed welding head 27 fixed to its arc surface to weld the weld at the joint inside the pipe body 14, thereby repairing the weld generated during the welding process of the molten pool. At this time, the arc-shaped grinding block 211 and the hook plate 215 are not in contact with the inner wall of the pipe body 14 due to the magnetic attraction of the electromagnet 212. After the weld repair work at the joint inside the pipe body 14 is completed, the electromagnet 212 is de-energized to release the magnetic attraction of the arc-shaped grinding block 211 and the hook plate 215. The weld repair work on the pipe body 14 is completed by the cooperation of the fixed welding head 27 and the welding head 16. Externally, the rotating ring 15 drives the welding head 16 to move along the outer arc surface of the pipe body 14. With the help of the laser sensor 17, the location of the missed weld is detected in real time, which can target the repair of the weld seam on the outer wall of the pipe body 14. It can effectively identify weld seam defects and improve the accuracy of external weld seam repair. Internally, the fixed motor 25 drives the gear 26 to rotate the connecting ring 23 and the fixed welding head 27 to repair the weld seam on the inner wall of the pipe body 14 at the joint. This makes up for the weld seam defects generated during the molten pool formation stage and realizes the repair of the inner and outer weld seams of the pipe body 14. The weld seam is repaired simultaneously. During the internal repair welding operation, the arc-shaped grinding block 211 and the hook plate 215 are kept detached from the inner wall of the pipe body 14 by the magnetic attraction of the electromagnet 212. This avoids interference and scratching between the arc-shaped grinding block 211, the hook plate 215 and the high-temperature weld seam, and prevents damage to components and weld formation during the repair welding process. After the inner wall repair welding process is completed, the arc-shaped grinding block 211 and the hook plate 215 can be released by de-energizing the electromagnet 212, which facilitates the subsequent inner wall grinding and cleaning process. This effectively improves the repair quality of the pipe circumferential butt weld seam, reduces the retention of weld defects, and enhances the overall reliability of the welded joint of the pipe body 14.
[0024] Example 2: Figures 1 to 7 As shown in the comparative embodiment one, another embodiment of the present invention is as follows: a processing component is further provided on the circumferential surface of the connecting ring 23. The processing component includes a hook plate 215 disposed on the circumferential surface of the connecting ring 23. The hook plate 215 is used to process residual dust and welding slag on the inner wall of the pipe body 14. The processing component includes a connecting frame 213 fixed to the arc surface of the connecting ring 23. A plurality of connecting springs 214 are fixedly connected inside the connecting frame 213. The bottom end of the plurality of connecting springs 214 is fixedly connected to the same hook plate 215. A guide frame 217 is fixedly connected to one side of the hook plate 215. A guide groove 216 is opened on the arc surface of the hook plate 215. A collection groove is opened inside the connecting ring 23. 221. An auxiliary ring 220 is rotatably connected inside the connecting ring 23. A guide tube 219 is fixedly connected to the inner wall of the auxiliary ring 220. The guide tube 219 is fixedly connected to the positioning post 21. A fixing groove 218 is opened inside both the guide tube 219 and the positioning post 21. A fixed motor 25 is fixedly connected inside the positioning post 21. A gear 26 is fixedly connected to the output end of the fixed motor 25. Several gear teeth 24 are fixedly connected to the inner wall of the connecting ring 23. The gear 26 meshes with the gear teeth 24. The electromagnet 212 is initially energized and magnetic. The magnetically attracted positioning rod 210 and hook plate 215, that is, the arc-shaped grinding block 211 and the hook plate 215 are not initially in contact with the annular inner wall of the tube body 14.
[0025] Specifically, after the arc-shaped grinding block 211 and the hook plate 215 are demagnetized one by one, the elastic force of the positioning spring 29 and the connecting spring 214 is released, thereby causing the arc-shaped grinding block 211 and the hook plate 215 to extend out of the positioning frame 28 and the connecting frame 213. The middle part of the arc-shaped grinding block 211 will abut against the inner wall of the tube body 14, so that when encountering a protruding weld point, the arc-shaped end of the arc-shaped grinding block 211 will not directly push against the weld point, but will contact the weld point with its arc surface to perform grinding work. After the arc-shaped grinding block 211 completes the grinding work, the hook plate 215 on the circumferential surface of the connecting ring 23 is released. The release of the hook plate 215, the hook plate 215 is an arc-shaped hook plate 215, and the arc-shaped tip of the hook plate 215 directly The arc-shaped hook plate 215, which abuts against the inner wall of the pipe body 14, will scrape up the metal dust and welding slag inside the pipe body 14 during the rotation of the connecting ring 23. After being scraped up, the metal dust and welding slag will be guided into the guide frame 217 by the guide groove 216 opened on the surface of the hook plate 215. Then, as the hook plate 215 rotates and the height increases, the metal dust and welding slag will fall to the bottom wall of the collection tank 221. The metal dust and welding slag ground by the arc-shaped grinding block 211 will always be located at the bottom of the pipe body 14 under the action of gravity. Then, by starting the negative pressure suction pump inside the positioning box 2, the metal dust and welding slag ground in the collection tank 221 will be suctioned under negative pressure, thereby completing the weld repair work of the pipe body 14. By de-energizing the electromagnet 212 to release the arc-shaped grinding block 211 and hook plate 215, and relying on the elastic force released by the positioning spring 29 and connecting spring 214, the arc-shaped grinding block 211 and hook plate 215 are driven to extend out of the positioning frame 28 and connecting frame 213 respectively, realizing the automatic positioning of the grinding and slag removal mechanism. The arc-shaped grinding block 211 adopts an arc-shaped structure that contacts the inner wall of the pipe body 14 in the middle. When facing the protruding weld point, it grinds with the arc surface in contact, avoiding hard pushing and bumping of the weld point at the end. It can smoothly grind and repair the protruding part of the inner wall weld, reduce the damage to the base material of the pipe body 14 during the grinding process, and improve the surface grinding quality of the weld. After grinding, the electromagnet 212 of the hook plate 215 is de-energized, releasing the hook plate 215 and causing it to rotate with the connecting ring 23. The arc-shaped hook plate 215 adheres to the inner wall of the pipe body 14, scraping away the metal dust and welding slag adhering to the inner wall of the pipe body 14. The scraped waste slag is guided into the guide frame 217 through the guide groove 216 of the hook plate 215. As the hook plate 215 rotates and rises, the welding slag and dust fall into the collection tank 221 by gravity. The debris generated by the grinding of the arc-shaped grinding block 211 also collects to the lower half of the ring of the pipe body 14 under the action of gravity. Then, the waste slag inside the collection tank 221 is centrally sucked and collected by a negative pressure suction pump, realizing the unified recycling and treatment of grinding waste slag. This reduces the residue of welding slag and dust, avoids secondary pollution caused by residue remaining in the pipe, and further ensures the processing quality of the weld seam inside the pipe body 14.
[0026] Working principle: First, after the welding of the two tubes 14 is completed, the tubes 14 are placed on the fixing plate 11 on the upper surface of the machine body 1. The fixing plate 11 has an arc-shaped groove corresponding to the tube 14. After placement, the built-in guide rail of the positioning plate 12 is activated, driving the rotating ring 15 to move the welding head 16 fixed to its inner wall to repair the weld. A laser sensor 17 is fixed to the side of the welding head 16. The laser sensor 17 detects the weld seam that is missed during the welding process, thereby completing the weld seam repair on the outer arc surface of the two tubes 14. At this time, the fixing motor 2 inside the positioning column 21 is activated. 5. The fixed motor 25 drives the gear 26 to rotate, which in turn drives the connecting ring 23 fixed to the gear 24 to rotate. The rotation of the connecting ring 23 drives the fixed welding head 27 fixed to its arc surface to weld the weld at the joint inside the pipe body 14, thereby repairing the weld generated during the welding of the molten pool. At this time, the arc-shaped grinding block 211 and the hook plate 215 are not in contact with the inner wall of the pipe body 14 due to the magnetic attraction of the electromagnet 212. After the weld repair work at the joint inside the pipe body 14 is completed, the electromagnet 212 is de-energized to release the magnetic attraction of the arc-shaped grinding block 211 and the hook plate 215. The weld repair work on the pipe body 14 is completed by the cooperation of the fixed welding head 27 and the welding head 16. Externally, the rotating ring 15 drives the welding head 16 to move along the outer arc surface of the pipe body 14. With the help of the laser sensor 17, the location of the missed weld is detected in real time, which can target the repair of the weld seam on the outer wall of the pipe body 14. It can effectively identify weld seam defects and improve the accuracy of external weld seam repair. Internally, the fixed motor 25 drives the gear 26 to rotate the connecting ring 23 and the fixed welding head 27 to repair the weld seam on the inner wall of the pipe body 14 at the joint. This makes up for the weld seam defects generated during the molten pool formation stage and realizes the repair of the inner and outer weld seams of the pipe body 14. During the internal repair welding process, the arc-shaped grinding block 211 and the hook plate 215 are kept detached from the inner wall of the pipe body 14 by the magnetic attraction of the electromagnet 212, so as to avoid interference and scratching between the arc-shaped grinding block 211, the hook plate 215 and the high-temperature weld, and prevent damage to components and weld formation during the repair welding process. After the internal wall repair welding process is completed, the arc-shaped grinding block 211 and the hook plate 215 can be released by de-energizing the electromagnet 212, which facilitates the subsequent internal wall grinding and cleaning process. This effectively improves the repair quality of the pipe circumferential butt weld, reduces the retention of weld defects, and improves the overall reliability of the welded joint of the pipe body 14. Furthermore, after the arc-shaped grinding block 211 and hook plate 215 are demagnetized one by one, the elastic force of the positioning spring 29 and connecting spring 214 is released, thereby causing the arc-shaped grinding block 211 and hook plate 215 to extend out of the positioning frame 28 and connecting frame 213. The middle part of the arc-shaped grinding block 211 will abut against the inner wall of the tube body 14, so that when encountering a protruding weld point, the arc-shaped end of the arc-shaped grinding block 211 will not directly push against the weld point, but will contact the weld point with the arc surface to perform grinding work. After the arc-shaped grinding block 211 completes the grinding work, the hook plate 215 on the circumference of the connecting ring 23 is released. The release of the hook plate 215, the hook plate 215 is an arc-shaped hook plate 215, and the arc-shaped tip of the hook plate 215 directly contacts the weld point. The inner wall of the tube body 14 abuts against the ring 23, and the arc-shaped hook plate 215 scrapes up the metal dust and welding slag inside the tube body 14 during the rotation of the ring 23. After being scraped up, the metal dust and welding slag are guided by the guide groove 216 on the surface of the hook plate 215 to the guide frame 217. Then, as the hook plate 215 rotates and the height increases, the metal dust and welding slag fall to the bottom wall of the collection tank 221. The metal dust and welding slag ground by the arc-shaped grinding block 211 will always be located at the bottom of the tube body 14 under the action of gravity. Then, by starting the negative pressure suction pump inside the positioning box 2, the metal dust and welding slag ground in the collection tank 221 are suctioned under negative pressure, thereby completing the weld repair work of the tube body 14. By de-energizing the electromagnet 212 to release the arc-shaped grinding block 211 and hook plate 215, and relying on the elastic force released by the positioning spring 29 and connecting spring 214, the arc-shaped grinding block 211 and hook plate 215 are driven to extend out of the positioning frame 28 and connecting frame 213 respectively, realizing the automatic positioning of the grinding and slag removal mechanism. The arc-shaped grinding block 211 adopts an arc-shaped structure that contacts the inner wall of the pipe body 14 in the middle. When facing the protruding weld point, it grinds with the arc surface in contact, avoiding hard pushing and bumping of the weld point at the end. It can smoothly grind and repair the protruding part of the inner wall weld, reduce the damage to the base material of the pipe body 14 during the grinding process, and improve the surface grinding quality of the weld. After grinding, the electromagnet 212 of the hook plate 215 is de-energized, releasing the hook plate 215 and causing it to rotate with the connecting ring 23. The arc-shaped hook plate 215 adheres to the inner wall of the pipe body 14, scraping away the metal dust and welding slag adhering to the inner wall of the pipe body 14. The scraped waste slag is guided into the guide frame 217 through the guide groove 216 of the hook plate 215. As the hook plate 215 rotates and rises, the welding slag and dust fall into the collection tank 221 by gravity. The debris generated by the grinding of the arc-shaped grinding block 211 also collects to the lower half of the ring of the pipe body 14 under the action of gravity. Then, the waste slag inside the collection tank 221 is centrally sucked and collected by a negative pressure suction pump, realizing the unified recycling and treatment of grinding waste slag. This reduces the residue of welding slag and dust, avoids secondary pollution caused by residue remaining in the pipe, and further ensures the processing quality of the weld seam inside the pipe body 14.
[0027] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of the present invention is defined by the appended claims and their equivalents.
Claims
1. An automatic weld repair device for pipe welding, comprising a body (1), wherein two fixing plates (11) are fixedly connected to the upper surface of the body (1), a welded pipe body (14) is placed above the two fixing plates (11), a positioning plate (12) is also fixedly connected to the upper surface of the body (1), a fixing ring (13) is fixedly connected to the upper surface of the positioning plate (12), a rotating ring (15) is rotatably connected inside the fixing ring (13), and a welding head (16) is fixedly connected to the inner wall of the rotating ring (15), characterized in that: The upper surface of the body (1) is provided with an auxiliary component, which includes a positioning box (2) fixed to the upper surface of the body (1). A positioning column (21) is fixed to one side of the positioning box (2). A positioning ring (22) is fixed to one end of the positioning column (21). A connecting ring (23) is rotatably connected inside the positioning ring (22). An arc-shaped grinding block (211) and a fixed welding head (27) are provided on the surface of the connecting ring (23). A collection pipe (222) is opened inside the positioning column (21). The auxiliary component also includes a positioning frame (28) fixed to the arc surface of the connecting ring (23). The inner wall of the positioning frame (28) is fixed with a number of positioning springs (29). The bottom ends of the positioning springs (29) are fixed with the same positioning rod (210). The bottom end of the positioning rod (210) is fixed with an arc-shaped grinding block (211). The top wall of the positioning frame (28) is fixed with an electromagnet (212).
2. The automatic weld repair equipment for pipeline welding according to claim 1, characterized in that: The cross section of the arc-shaped grinding block (211) is one-third of a circular arc, and the end of the arc-shaped grinding block (211) does not abut against the inner wall of the tube body (14), while the middle part of the arc-shaped grinding block (211) abuts against the inner wall of the tube body (14).
3. The automatic weld repair equipment for pipeline welding according to claim 1, characterized in that: The circumferential surface of the connecting ring (23) is also provided with a processing component, which includes a hook plate (215) provided on the circumferential surface of the connecting ring (23). The hook plate (215) is used to process residual dust and welding slag on the inner wall of the pipe body (14).
4. The automatic weld repair equipment for pipeline welding according to claim 3, characterized in that: The processing component includes a connecting frame (213) fixed to the arc surface of the connecting ring (23), a plurality of connecting springs (214) fixed inside the connecting frame (213), the bottom ends of the plurality of connecting springs (214) are fixed to the same hook plate (215), a guide frame (217) is fixed to one side of the hook plate (215), and a guide groove (216) is opened on the arc surface of the hook plate (215).
5. The automatic weld repair equipment for pipeline welding according to claim 4, characterized in that: The connecting ring (23) has a collection groove (221) inside. An auxiliary ring (220) is rotatably connected inside the connecting ring (23). A guide tube (219) is fixedly connected to the inner wall of the auxiliary ring (220). The guide tube (219) is fixedly connected to the positioning post (21). Both the guide tube (219) and the positioning post (21) have fixing grooves (218).
6. The automatic weld repair equipment for pipeline welding according to claim 5, characterized in that: A fixed motor (25) is fixedly connected inside the positioning column (21), and a gear (26) is fixedly connected to the output end of the fixed motor (25). Several gear teeth (24) are fixedly connected to the inner wall of the connecting ring (23), and the gear (26) meshes with the gear teeth (24).
7. The automatic weld repair equipment for pipeline welding according to claim 1, characterized in that: The electromagnet (212) is initially energized and magnetic, and the magnetically attracted positioning rod (210) and hook plate (215), i.e. the arc-shaped grinding block (211) and hook plate (215) are not initially in contact with the annular inner wall of the tube body (14).
8. The automatic weld repair equipment for pipeline welding according to claim 7, characterized in that: After the welding of the two tubes (14) is completed, the tubes (14) are placed on the fixing plate (11) on the upper surface of the machine body (1). The fixing plate (11) has an arc-shaped groove corresponding to the tubes (14). After placement, the guide rail inside the positioning plate (12) is activated, and the rotating ring (15) is driven to drive the welding head (16) fixed to its inner wall to repair the weld. A laser sensor (17) is fixed to the side of the welding head (16). The laser sensor (17) detects the weld seam that is missed during the welding process, thereby completing the weld seam repair on the outer arc surface of the two tubes (14). At this time, the fixing motor (25) inside the positioning column (21) is activated to fix the weld seam. The motor (25) drives the gear (26) to rotate, which in turn drives the connecting ring (23) fixed to the gear teeth (24) to rotate. The rotation of the connecting ring (23) drives the fixed welding head (27) fixed to its arc surface to weld the weld at the joint inside the pipe body (14), thereby completing the weld generated during the welding process of the molten pool. At this time, the arc-shaped grinding block (211) and the hook plate (215) do not come into contact with the inner wall of the pipe body (14) due to the magnetic attraction of the electromagnet (212). After the weld repair work at the joint inside the pipe body (14) is completed, the electromagnet (212) is de-energized to release the magnetic attraction of the arc-shaped grinding block (211) and the hook plate (215).
9. An automatic weld repair device for pipeline welding according to claim 8, characterized in that: After the arc-shaped grinding block (211) and hook plate (215) are demagnetized one by one, the elastic force of the positioning spring (29) and connecting spring (214) is released, thereby driving the arc-shaped grinding block (211) and hook plate (215) to extend out of the positioning frame (28) and connecting frame (213). The middle part of the arc-shaped grinding block (211) will abut against the inner wall of the tube body (14), so that when encountering a protruding weld point, the arc-shaped end of the arc-shaped grinding block (211) will not directly push the weld point, but will contact the weld point with the arc surface to perform grinding work. After the arc-shaped grinding block (211) completes the grinding work, the hook plate (215) on the circumference of the connecting ring (23) is released. The release of the hook plate (215) results in the hook plate (215) being an arc-shaped hook plate (215), and the arc-shaped tip of the hook plate (215) The ring (23) directly contacts the inner wall of the pipe body (14). During the rotation of the ring (23), the arc-shaped hook plate (215) will scrape up the metal dust and welding slag inside the pipe body (14). After the metal dust and welding slag are scraped up, they will be guided to the guide frame (217) by the guide groove (216) opened on the surface of the hook plate (215). Then, as the height of the hook plate (215) increases, the metal dust and welding slag fall to the bottom wall of the collection tank (221). The metal dust and welding slag ground by the arc-shaped grinding block (211) will always be located at the bottom of the pipe body (14) under the action of gravity. Then, by starting the negative pressure suction pump inside the positioning box (2), the metal dust and welding slag ground in the collection tank (221) will be suctioned under negative pressure, thereby completing the weld repair work of the pipe body (14).
Citation Information
Patent Citations
Automatic welding mechanism for pipeline circumferential welds
CN120502909A