A method and apparatus for high-pressure hot bending forming of 3D curved PC mobile phone back cover

By using a high-pressure hot bending forming device driven by a single cylinder and utilizing a mechanical structure to achieve a self-circulating air path, the problems of high cost, high energy consumption and poor stability of existing devices have been solved, and high-precision 3D curved PC mobile phone back cover processing has been realized.

CN123104038APending Publication Date: 2026-11-17HUIZHOU BAOMEI PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611400046.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing 3D curved PC mobile phone back cover high-pressure hot bending forming processing equipment has problems such as high equipment cost, large space occupation, high energy consumption and poor stability. In particular, the sensor is prone to failure in high temperature and high pressure environment, resulting in insufficient processing accuracy and reliability.

Method used

The high-pressure hot bending forming device driven by a single cylinder achieves time-sharing linkage of cylinder movement through a combination structure of one-way gear and sealed cavity. Combined with negative and positive pressure airflow, it completes the dust collection and cooling functions. The mechanical structure realizes a self-circulating air path, eliminating the need for an external air source and electrical control system.

Benefits of technology

It has achieved cost reduction and energy saving of equipment, improved processing accuracy and product yield, prevented warping and surface defects, ensured high-precision curved surface dimensions, and improved the stability and reliability of the whole machine operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123104038A_ABST
    Figure CN123104038A_ABST
Patent Text Reader

Abstract

This invention relates to the field of molding equipment technology, and in particular to a method and apparatus for high-pressure hot bending forming of a 3D curved PC mobile phone back cover. The technical solution includes a main body and a mounting plate. The mounting plate is fixedly mounted on the main body, and a cylinder is fixedly mounted on the mounting plate. A sliding plate is slidably mounted on the main body, and the piston rod of the cylinder is fixedly connected to the sliding plate. A forming groove is fixedly mounted on the main body, and the forming groove has an arc-shaped design. A heating pressure plate is fixedly mounted at the bottom of the sliding plate, and the heating pressure plate is located directly above the forming groove. A first mounting frame is fixedly mounted on the main body. This invention uses a single cylinder as the power core, and through a purely mechanical time-sharing linkage and air circuit reuse design, it simultaneously completes pressure plate pre-cleaning, 3D curved PC back cover high-pressure hot bending forming, and full-area air cooling shaping within one lifting cycle. No additional drive or electrical control system is required, achieving cost reduction and energy saving of equipment, and simultaneous improvement of product forming accuracy and surface yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of molding equipment technology, and in particular to a high-pressure hot bending forming method and apparatus for 3D curved PC mobile phone back cover. Background Technology

[0002] With the rapid development of smartphone technology and the popularization of 5G communication and wireless charging technology, the materials for mobile phone back covers are gradually shifting from traditional metals to non-metals. Polycarbonate (PC) has become one of the important materials for manufacturing 3D curved mobile phone back covers due to its high impact strength, excellent optical transmittance, ease of processing, and good electromagnetic wave penetration performance. In the high-pressure hot bending process of 3D curved PC mobile phone back covers, the PC sheet (blank) is usually placed in a forming mold. The blank is heated to above the glass transition temperature by a heating plate to soften it. Then, high pressure is applied to make it fit tightly into the curved cavity of the mold. After cooling and shaping, it is demolded and removed. However, the existing high-pressure hot bending forming equipment and processes still have the following technical defects in actual production.

[0003] After hot bending, PC sheets need to be rapidly cooled to below the setting temperature. Existing equipment mostly uses fixed fans for point-to-point cooling. Due to the complex curvature of the 3D curved surface, fixed fans easily lead to uneven heating of the workpiece surface and the creation of local cooling dead zones. This results in large residual internal stresses within the workpiece, causing warping, shrinkage cavities, or dimensional deviations in the PC back cover after demolding. Existing auxiliary cleaning and air-cooling devices mostly require additional independent drive motors, high-pressure fans, and dust pumps, and rely on complex electrical control systems and sensors for timing control. This not only significantly increases the manufacturing cost, space occupation, and energy consumption of the equipment, but also makes the sensors and electrical control components prone to failure or malfunction under the harsh high-temperature and high-pressure processing environment, leading to disordered action timing and reducing the stability and reliability of the entire machine. Therefore, this application proposes a high-pressure hot bending forming method and apparatus for 3D curved PC mobile phone back covers. Summary of the Invention

[0004] The purpose of this invention is to address the problems existing in the background art by proposing a high-pressure hot bending forming method and apparatus for 3D curved PC mobile phone back cover.

[0005] The first invention, this application proposes a high-pressure hot bending forming device for 3D curved PC mobile phone back covers using a cylinder, which adopts the following technical solution: A high-pressure hot bending forming device for 3D curved PC mobile phone back covers using a cylinder includes a main body and a mounting plate. The mounting plate is fixedly mounted on the main body, and a cylinder is fixedly mounted on the mounting plate. A sliding plate is slidably disposed on the main body, and the piston rod of the cylinder is fixedly connected to the sliding plate. A forming groove with an arc-shaped design is fixedly mounted on the main body. A heating pressure plate is fixedly mounted on the bottom of the sliding plate, and the heating pressure plate is located directly above the forming groove. A first mounting frame is fixedly mounted on the main body, and a first reciprocating lead screw is rotatably mounted on the first mounting frame. A first one-way gear is rotatably mounted on one end of the first mounting frame. A first rack is fixedly mounted on the bottom of the sliding plate, and one end of the first rack penetrates the main body. The first rack meshes with the first one-way gear. A slider is slidably mounted on the first mounting frame. The slider is threadedly connected to the first reciprocating lead screw. A fixing plate is fixedly mounted on one side of the slider. A cooling chamber is fixedly mounted on the bottom of the fixing plate. The cooling chamber is hollow. Multiple nozzles are fixedly mounted on the bottom of the cooling chamber. An installation cavity is fixedly mounted on the bottom of the mounting plate. The installation cavity is hollow. A sealing plate is slidably mounted inside the installation cavity. The sliding plate is fixedly connected to the sealing plate. A first one-way valve is fixedly mounted on the sealing plate. One end of the first one-way valve communicates with the cooling cavity. The first one-way valve can only release air in one direction. A dust collection device is provided on the sliding plate to clean the heating pressure plate before use.

[0006] Optionally, the dust collection device includes a second mounting frame fixedly installed at the bottom of the slide plate, a guide block slidably mounted on the second mounting frame, a second reciprocating screw rotatably mounted inside the second mounting frame, the second reciprocating screw being threadedly connected to the guide block, a second one-way gear rotatably mounted at one end of the second mounting frame, a second rack fixedly mounted on the main body, one end of the second rack penetrating the slide plate, the second rack meshing with the second one-way gear, a positioning plate fixedly mounted at the bottom of the guide block, a negative pressure chamber fixedly mounted on the positioning plate, a dust collection groove formed on the negative pressure chamber, a second one-way valve fixedly mounted on one side of the mounting chamber, one end of the second one-way valve communicating with the negative pressure chamber, and the second one-way valve allowing air to enter in only one direction.

[0007] Optionally, a first connecting pipe is fixedly installed at one end of the first one-way valve, and one end of the first connecting pipe is connected to the cooling chamber.

[0008] Optionally, a second connecting pipe is fixedly installed at one end of the second one-way valve, and one end of the second connecting pipe is connected to the negative pressure chamber.

[0009] Optionally, a connecting rod is fixedly installed on the slide plate, and one end of the connecting rod is fixedly connected to the sealing plate.

[0010] Optionally, a filter chamber is fixedly installed on the second connecting pipe, the second connecting pipe is connected to the filter chamber, and a filter bag is provided inside the filter chamber.

[0011] Optionally, a guide post is fixedly installed on the main body, and the slide plate and the guide post are slidably connected.

[0012] Optionally, a sliding groove is provided on the first mounting frame, and the slider is slidably connected to the sliding groove.

[0013] Optionally, a base is fixedly mounted on the main body, and the base is fixedly connected to the first mounting frame.

[0014] Secondly, this application proposes a high-pressure hot bending forming method for 3D curved PC mobile phone back cover, including the following steps; Step 1. Blank preparation: Select optical grade PC sheet and precisely cut it according to the outer dimensions of the target mobile phone back cover to obtain a flat blank. Perform electrostatic dust removal pretreatment on the front and back surfaces of the blank to remove surface dust and cutting burrs. Step 2. Pre-cleaning of the forming working surface: Position the pre-treated blank at the opening of the forming groove on the main body, start the cylinder on the mounting plate to drive the slide plate down along the guide column. During the slide plate's descent, the second rack fixed to the main body meshes with the second one-way gear, driving the second reciprocating screw in the second mounting frame to rotate. Through the guide block and positioning plate, the negative pressure chamber moves laterally back and forth along the bottom surface of the heating plate. At the same time, the slide plate drives the sealing plate to slide in the mounting cavity through the connecting rod to generate negative pressure. The negative pressure is transmitted to the negative pressure chamber in sequence through the second one-way valve, the second connecting pipe and the filter chamber, so that a continuous adsorption airflow is formed at the dust collection groove. Before the heating plate contacts the blank, the dust and impurities on the entire working surface of the heating plate are cleaned. Step 3. High-pressure hot bending: The cylinder continues to drive the slide plate downwards, and the heated pressure plate presses against the upper surface of the blank and heats the blank evenly, raising the blank temperature above the glass transition temperature and softening it fully; under the pressure output by the cylinder, the softened blank gradually conforms to the arc-shaped inner surface of the molding groove, maintaining the heating temperature at 130℃~160℃ and the forming pressure at 0.4MPa~0.8MPa, holding the pressure for 15s~30s, so that the blank is formed into the preset 3D curved surface shape; Step 4. Air Cooling and Shaping: After the pressure holding molding is completed, the cylinder drives the slide plate to move upward and reset. During the upward movement of the slide plate, the first rack moves upward synchronously with the slide plate, meshes with the first one-way gear, and drives the first reciprocating screw in the first mounting frame to rotate. Through the slider and the fixed plate, the cooling chamber is driven to move laterally and reciprocally above the molding groove. At the same time, the slide plate drives the sealing plate to slide upward in the mounting cavity, compressing the air in the mounting cavity to form a high-pressure airflow. The high-pressure airflow is introduced into the cooling cavity through the first one-way valve and the first connecting pipe. It is evenly sprayed onto the surface of the molded PC back cover by multiple nozzles at the bottom of the cooling cavity, and the workpiece is cooled down by air cooling throughout until the workpiece temperature drops below 60°C to complete the shaping. Step 5. Unloading and Removal: After the workpiece has cooled and solidified, remove the formed 3D curved PC mobile phone back cover from the forming groove to complete the single-cycle high-pressure hot bending forming process.

[0015] Compared with the prior art, the present invention has the following beneficial technical effects: This invention uses a single cylinder as the sole power input. By leveraging the unidirectional transmission characteristics of the first and second unidirectional gears and the switching between positive and negative pressure in the sealed cavity, the linear motion of the cylinder's lifting and lowering is simultaneously converted into the negative pressure power for suction and the lateral reciprocating motion of the suction mechanism during downward movement, and the positive pressure power for cooling and the lateral reciprocating motion of the cooling mechanism during upward movement. Through a purely mechanical structure, a time-sharing linkage of one power source and four outputs is achieved without the need for additional drive components.

[0016] Furthermore, through the combined structure of a single mounting cavity, a sealing plate, a first check valve, and a second check valve, the same mounting cavity can act as a negative pressure generating cavity to provide dust suction power during the downward stroke and as a positive pressure generating cavity to provide cooling air source during the upward stroke. One mounting cavity has two pneumatic functions, realizing a high degree of integration and self-circulation of the air circuit system, without the need for external air source and vacuum equipment.

[0017] Furthermore, the cooling chamber is driven to move laterally and reciprocally above the forming groove by the first reciprocating screw. High-pressure airflow is evenly swept across the workpiece surface through multiple nozzles, achieving rapid and uniform cooling of the entire 3D curved back cover. This eliminates the internal stress concentration caused by local temperature differences, effectively preventing warping, deformation, or surface annealing shrinkage of the PC back cover after demolding, ensuring high-precision curved surface contour dimensions, and improving processing results.

[0018] This invention uses a single cylinder as the power core and, through a purely mechanical time-sharing linkage and air circuit reuse design, simultaneously completes the pre-cleaning of the pressure plate, high-pressure hot bending of the 3D curved PC back cover, and full-area air-cooling shaping within one lifting cycle. It requires no additional drive or electronic control system, thus achieving cost reduction and energy saving of equipment, and simultaneous improvement of product forming accuracy and surface yield. Attached Figure Description

[0019] Figure 1A schematic diagram of a high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover. Figure 1 ; Figure 2 A schematic diagram of a high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover. Figure 2 ; Figure 3 A schematic diagram of a high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover. Figure 3 ; Figure 4 A schematic diagram of a high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover. Figure 4 ; Figure 5 for Figure 1 A magnified schematic diagram of the local structure at point A; Figure 6 for Figure 2 A magnified view of the structure at point B in the middle; Figure 7 for Figure 3 A magnified schematic diagram of the local structure at point C; Figure 8 for Figure 4 A magnified schematic diagram of the structure at point D.

[0020] Reference numerals: 1. Main body; 2. Mounting plate; 3. Cylinder; 4. Slide plate; 5. Guide column; 6. First mounting frame; 7. Forming groove; 8. Heating pressure plate; 9. First rack; 10. Slide groove; 11. First reciprocating screw; 12. Slider; 13. First one-way gear; 14. Base; 15. Fixing plate; 16. Cooling chamber; 17. Nozzle; 18. Mounting chamber; 19. Sealing plate; 20. Connecting rod; 21. First one-way valve; 22. First connecting pipe; 23. Second one-way valve; 24. Second connecting pipe; 25. Filter chamber; 26. Second rack; 27. Second one-way gear; 28. Second reciprocating screw; 29. ​​Guide block; 30. Positioning plate; 31. Negative pressure chamber; 32. Dust suction groove; 33. Second mounting frame. Detailed Implementation

[0021] The technical solution of the present invention will now be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments.

[0022] The components of the embodiments of the invention described and shown in the accompanying drawings can typically be arranged and designed in a variety of different configurations. Therefore, the following detailed description of the embodiments of the invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention.

[0023] Example 1: like Figure 1-8 As shown, this invention proposes a high-pressure hot bending forming device for 3D curved PC mobile phone back covers, including a main body 1 and a mounting plate 2. The mounting plate 2 is fixedly mounted on the main body 1, and a cylinder 3 is fixedly mounted on the mounting plate 2. A sliding plate 4 is slidably arranged on the main body 1, and the piston rod of the cylinder 3 is fixedly connected to the sliding plate 4. A forming groove 7 is fixedly mounted on the main body 1, and the forming groove 7 has an arc-shaped design. A heating pressure plate 8 is fixedly mounted on the bottom of the sliding plate 4, and the heating pressure plate 8 is located directly above the forming groove 7. A first mounting frame 6 is fixedly mounted on the main body 1, and a first reciprocating screw 11 is rotatably mounted on the first mounting frame 6. A first one-way gear 13 is rotatably mounted on one end of the first mounting frame 6. A first rack 9 is fixedly mounted on the bottom of the sliding plate 4. One end of rack 9 passes through the main body 1. Only when rack 9 moves upward with slide plate 4 can the first one-way gear 13 drive the first reciprocating screw 11 to rotate. Rack 9 meshes with the first one-way gear 13. A slider 12 is slidably mounted on the first mounting frame 6. The slider 12 is threadedly connected to the first reciprocating screw 11. A fixing plate 15 is fixedly mounted on one side of slider 12. A cooling cavity 16 is fixedly mounted on the bottom of fixing plate 15. The cooling cavity 16 is hollow. Multiple nozzles 17 are fixedly mounted on the bottom of cooling cavity 16. An mounting cavity 18 is fixedly mounted on the bottom of mounting plate 2. The mounting cavity 18 is hollow. A sealing plate 19 is slidably mounted inside mounting cavity 18. Slide plate 4 is fixedly connected to sealing plate 19. A sealing plate 19 is fixedly mounted on sealing plate 19. Equipped with a first one-way valve 21, one end of which is connected to the cooling chamber 16, the first one-way valve 21 can only release air in one direction. The blank to be formed is placed in the forming groove 7. The cylinder 3 drives the slide plate 4 downward, and the heating plate 8 presses against the upper surface of the blank and heats the blank evenly, raising the blank temperature above the glass transition temperature and softening it sufficiently. Under the pressure output by the cylinder 3, the softened blank gradually conforms to the arc-shaped inner surface of the forming groove 7. The heating temperature is maintained at 130℃~160℃, the forming pressure is 0.4MPa~0.8MPa, and the pressure is held for 15s~30s, so that the blank is formed into the preset 3D curved surface shape. After the pressure holding and forming is completed, the cylinder 3 drives the slide plate 4 upward to reset. During the upward movement of the slide plate 4... The first rack 9 moves upward synchronously with the slide plate 4, meshes with the first one-way gear 13, and drives the first reciprocating screw 11 in the first mounting frame 6 to rotate. Through the slider 12 and the fixed plate 15, the cooling chamber 16 is driven to move laterally and reciprocally above the forming groove 7. At the same time, the slide plate 4 drives the sealing plate 19 to slide upward in the mounting cavity 18, compressing the air in the mounting cavity 18 to form a high-pressure airflow. The high-pressure airflow is introduced into the cooling chamber 16 through the first one-way valve 21 and the first connecting pipe 22. It is evenly sprayed onto the surface of the formed PC back cover by multiple nozzles 17 at the bottom of the cooling chamber 16, and the workpiece is cooled by air cooling until the workpiece temperature drops below 60°C to complete the shaping. The slide plate 4 is equipped with a dust collection device to clean the heating plate 8 before use.

[0024] Example 2: like Figure 1-8As shown, the vacuuming device includes a second mounting frame 33 fixedly installed at the bottom of the slide plate 4. A guide block 29 is slidably mounted on the second mounting frame 33. A second reciprocating screw 28 is rotatably mounted inside the second mounting frame 33 and threadedly connected to the guide block 29. A second one-way gear 27 is rotatably mounted at one end of the second mounting frame 33. A second rack 26 is fixedly mounted on the main body 1. One end of the second rack 26 passes through the slide plate 4 and meshes with the second one-way gear 27. Only when the slide plate 4 drives the second one-way gear 27 to move downwards can the second one-way gear 27 drive the second reciprocating screw 28 to rotate. The bottom of the guide block 29 is fixedly mounted... A positioning plate 30 is installed, on which a negative pressure chamber 31 is fixedly mounted. A dust suction groove 32 is provided on the negative pressure chamber 31. A second one-way valve 23 is fixedly mounted on one side of the mounting cavity 18. One end of the second one-way valve 23 is connected to the negative pressure chamber 31, and the second one-way valve 23 allows only one-way air intake. A first connecting pipe 22 is fixedly mounted on one end of the first one-way valve 21, and one end of the first connecting pipe 22 is connected to the cooling cavity 16. A second connecting pipe 24 is fixedly mounted on one end of the second one-way valve 23, and one end of the second connecting pipe 24 is connected to the negative pressure chamber 31. A connecting rod 20 is fixedly mounted on the slide plate 4, and one end of the connecting rod 20 is fixedly connected to the sealing plate 19. The second connecting pipe... A filter chamber 25 is fixedly installed on the main body 1. The second connecting pipe 24 is connected to the filter chamber 25. A filter bag is installed inside the filter chamber 25. A guide post 5 is fixedly installed on the main body 1. The slide plate 4 is slidably connected to the guide post 5. A groove 10 is opened on the first mounting frame 6. The slider 12 is slidably connected to the groove 10. A base 14 is fixedly installed on the main body 1. The base 14 is fixedly connected to the first mounting frame 6. During the downward movement of the slide plate 4, the second rack 26 fixed to the main body 1 meshes with the second one-way gear 27, which drives the second reciprocating screw 28 in the second mounting frame 33 to rotate. Through the guide block 29 and the positioning plate 30, the negative pressure chamber 31 is driven to move horizontally along the bottom surface of the heating plate 8. The slide plate 4 moves back and forth, while the connecting rod 20 drives the sealing plate 19 to slide in the mounting cavity 18 to generate negative pressure. The negative pressure is transmitted to the negative pressure chamber 31 through the second one-way valve 23, the second connecting pipe 24 and the filter chamber 25 in sequence, so that a continuous adsorption airflow is formed at the dust suction groove 32. Before the heated plate 8 contacts the blank, the dust and impurities on the entire working surface of the heated plate 8 are cleaned. The dust and impurities sucked in enter the filter chamber 25 for filtration and collection. The slide plate 4 is used to lift and lower to drive the sealing plate 19 to reciprocate to draw and compress air in the mounting cavity 18. When it goes down, the suction effect (negative pressure) is used to achieve dust suction. When it goes up, the compression effect (positive pressure) is used to achieve high-pressure jet cooling.By directly converting the mechanical motion of stamping into pneumatic energy, a self-sufficient air circulation system is achieved without the need for external high-pressure blowers or dust pumps. The entire process requires no additional servo motors, external high-pressure blowers, or dedicated dust pumps, significantly reducing the overall power consumption and electrical control costs of the equipment. The compact structure and stable and reliable operation effectively prevent pits, pinholes, and optical defects caused by impurities and dust being pressed into the softened PC surface, greatly improving the yield rate of 3D curved PC back covers. High-pressure airflow is evenly swept across the workpiece surface through multiple nozzles 27, achieving rapid and uniform cooling of the entire 3D curved back cover, eliminating internal stress concentration caused by local temperature differences, and effectively preventing warping, deformation, or surface annealing shrinkage of the PC back cover after demolding, ensuring high-precision curved surface contour dimensions.

[0025] Example 3: This invention proposes a high-pressure hot bending forming method for 3D curved PC mobile phone back covers, comprising the following steps; Step 1. Blank preparation: Select optical grade PC sheet and precisely cut it according to the outer dimensions of the target mobile phone back cover to obtain a flat blank. Perform electrostatic dust removal pretreatment on the front and back surfaces of the blank to remove surface dust and cutting burrs. Step 2. Pre-cleaning of the forming working surface: Position the pre-treated blank at the opening of the forming groove 7 on the main body 1. Start the cylinder 3 on the mounting plate 2 to drive the slide plate 4 to move down along the guide column 5. During the downward movement of the slide plate 4, the second rack 26 fixed to the main body 1 meshes with the second one-way gear 27 to drive the second reciprocating screw 28 in the second mounting frame 33 to rotate. Through the guide block 29 and the positioning plate 30, the negative pressure chamber 31 moves laterally and reciprocally along the bottom surface of the heating plate 8. At the same time, the slide plate 4 drives the sealing plate 19 to slide in the mounting cavity 18 through the connecting rod 20 to generate negative pressure. The negative pressure is transmitted to the negative pressure chamber 31 through the second one-way valve 23, the second connecting pipe 24 and the filter chamber 25 in sequence, so that a continuous adsorption airflow is formed at the dust suction groove 32. Before the heating plate 8 contacts the blank, the dust and impurities of the entire working surface of the heating plate 8 are cleaned. Step 3. High-pressure hot bending: The cylinder 3 continues to drive the slide plate 4 downward, and the heating plate 8 presses against the upper surface of the blank and heats the blank evenly, so that the temperature of the blank rises above the glass transition temperature and softens it fully; under the pressure output by the cylinder 3, the softened blank gradually conforms to the arc-shaped inner surface of the molding groove 7, maintaining the heating temperature at 130℃~160℃ and the forming pressure at 0.4MPa~0.8MPa, holding the pressure for 15s~30s, so that the blank is formed into the preset 3D curved surface shape; Step 4. Air Cooling and Shaping: After the pressure holding molding is completed, the cylinder 3 drives the slide plate 4 to move upward and reset. During the upward movement of the slide plate 4, the first rack 9 moves upward synchronously with the slide plate 4, meshes with the first one-way gear 13 and drives the first reciprocating screw 11 in the first mounting frame 6 to rotate. Through the slider 12 and the fixed plate 15, the cooling chamber 16 is driven to move laterally and reciprocally above the molding groove 7. At the same time, the slide plate 4 drives the sealing plate 19 to slide upward in the mounting cavity 18, compressing the air in the mounting cavity 18 to form a high-pressure airflow. The high-pressure airflow is introduced into the cooling chamber 16 through the first one-way valve 21 and the first connecting pipe 22. It is evenly sprayed onto the surface of the formed PC back cover by multiple nozzles 17 at the bottom of the cooling chamber 16 to perform full-area air cooling and cooling of the workpiece until the workpiece temperature drops below 60°C to complete the shaping. Step 5. Unloading and Removal: After the workpiece has cooled and solidified, remove the formed 3D curved PC mobile phone back cover from the forming groove 7 to complete the single-cycle high-pressure hot bending forming process.

[0026] Working principle: The blank to be formed is placed in the forming groove 7. The cylinder 3 drives the sliding plate 4 downward. The heating plate 8 presses against the upper surface of the blank and heats the blank evenly, raising the temperature of the blank above the glass transition temperature and softening it sufficiently. Under the pressure output by the cylinder 3, the softened blank gradually conforms to the arc-shaped inner surface of the forming groove 7. The heating temperature is maintained at 130℃~160℃, the forming pressure is 0.4MPa~0.8MPa, and the pressure is held for 15s~30s to form the blank. To achieve the preset 3D curved surface shape, after pressure holding and molding, cylinder 3 drives slide plate 4 to move upward and reset. During the upward movement of slide plate 4, the first rack 9 moves upward synchronously with slide plate 4, meshes with the first one-way gear 13, and drives the first reciprocating screw 11 in the first mounting frame 6 to rotate. Through slider 12 and fixed plate 15, it drives cooling cavity 16 to move laterally reciprocally above molding groove 7. At the same time, slide plate 4 drives sealing plate 19 to slide upward in mounting cavity 18, compressing the air in mounting cavity 18 to form high pressure gas. High-pressure airflow enters the cooling chamber 16 through the first one-way valve 21 and the first connecting pipe 22. Multiple nozzles 17 at the bottom of the cooling chamber 16 spray the air evenly onto the surface of the formed PC back cover, cooling the workpiece across the entire area until the workpiece temperature drops below 60°C to complete the shaping. During the downward movement of the slide plate 4, the second rack 26 fixed to the main body 1 meshes with the second one-way gear 27, driving the second reciprocating screw 28 in the second mounting frame 33 to rotate. Through the guide block 29 and the positioning plate 30, the negative pressure chamber 31 moves laterally back and forth along the bottom surface of the heating plate 8. At the same time, the slide plate 4 drives the sealing plate 19 to slide in the mounting chamber 18 through the connecting rod 20 to generate negative pressure. The negative pressure is transmitted to the negative pressure chamber 31 through the second one-way valve 23, the second connecting pipe 24 and the filter chamber 25, so that a continuous adsorption airflow is formed at the dust suction groove 32. Before the heating plate 8 contacts the blank, the dust and impurities on the entire working surface of the heating plate 8 are cleaned. The inhaled dust and impurities enter the filter chamber 25 for filtration and collection.

[0027] The above specific embodiments are merely several optional embodiments of the present invention. Based on the technical solutions of the present invention and the relevant teachings of the above embodiments, those skilled in the art can make various alternative improvements and combinations to the above specific embodiments.

Claims

1. A high-pressure hot bending forming device for 3D curved PC mobile phone back cover, comprising a main body (1), characterized in that, It also includes a mounting plate (2), which is fixedly mounted on the main body (1). A cylinder (3) is fixedly mounted on the mounting plate (2). A sliding plate (4) is slidably mounted on the main body (1). The piston rod of the cylinder (3) is fixedly connected to the sliding plate (4). A forming groove (7) is fixedly mounted on the main body (1). The forming groove (7) has an arc-shaped design. A heating pressure plate (8) is fixedly mounted on the bottom of the sliding plate (4). The heating pressure plate (8) is located directly above the forming groove (7). A first mounting frame (6) is fixedly mounted on the main body (1). A first reciprocating screw (11) is rotatably mounted on the first mounting frame (6). A first one-way gear (13) is rotatably mounted on one end of the first mounting frame (6). A first rack (9) is fixedly mounted on the bottom of the sliding plate (4). One end of the first rack (9) penetrates the main body (1). The first rack (9) meshes with the first one-way gear (13). A slider (12) is slidably mounted on the first mounting frame (6). The slider (12) is threadedly connected to the first reciprocating screw (11). A fixing plate (15) is fixedly mounted on one side of the slider (12). A cooling chamber (16) is fixedly mounted on the bottom of the fixing plate (15). The cooling chamber (16) is hollow. Multiple nozzles (17) are fixedly mounted on the bottom of the cooling chamber (16). An mounting cavity (18) is fixedly mounted on the bottom of the mounting plate (2). The mounting cavity (18) is hollow. A sealing plate (19) is slidably mounted inside the mounting cavity (18). The sliding plate (4) is fixedly connected to the sealing plate (19). A first one-way valve (21) is fixedly mounted on the sealing plate (19). One end of the first one-way valve (21) is connected to the cooling cavity (16). The first one-way valve (21) can only release air in one direction. A dust collection device for cleaning the heating pressure plate (8) before use is provided on the sliding plate (4).

2. The high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover according to claim 1, characterized in that, The dust collection device includes a second mounting frame (33) fixedly mounted on the bottom of the slide plate (4), a guide block (29) slidably mounted on the second mounting frame (33), a second reciprocating screw (28) rotatably mounted inside the second mounting frame (33), the second reciprocating screw (28) being threadedly connected to the guide block (29), a second one-way gear (27) rotatably mounted on one end of the second mounting frame (33), and a second rack (26) fixedly mounted on the main body (1). One end of the slide plate (4) is inserted through the second rack (26) and the second one-way gear (27) meshes. A positioning plate (30) is fixedly installed at the bottom of the guide block (29). A negative pressure chamber (31) is fixedly installed on the positioning plate (30). A dust suction groove (32) is opened on the negative pressure chamber (31). A second one-way valve (23) is fixedly installed on one side of the mounting cavity (18). One end of the second one-way valve (23) is connected to the negative pressure chamber (31). The second one-way valve (23) can only allow air to enter in one direction.

3. The high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover according to claim 1, characterized in that, One end of the first one-way valve (21) is fixedly installed with a first connecting pipe (22), and one end of the first connecting pipe (22) is connected to the cooling chamber (16).

4. The high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover according to claim 2, characterized in that, A second connecting pipe (24) is fixedly installed at one end of the second one-way valve (23), and one end of the second connecting pipe (24) is connected to the negative pressure chamber (31).

5. The high-pressure hot bending forming device for a 3D curved PC mobile phone back cover according to claim 1, characterized in that, A connecting rod (20) is fixedly installed on the slide plate (4), and one end of the connecting rod (20) is fixedly connected to the sealing plate (19).

6. The high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover according to claim 2, characterized in that, A filter chamber (25) is fixedly installed on the second connecting pipe (24), and the second connecting pipe (24) is connected to the filter chamber (25). A filter bag is provided inside the filter chamber (25).

7. The high-pressure hot bending forming device for a 3D curved PC mobile phone back cover according to claim 1, characterized in that, A guide post (5) is fixedly installed on the main body (1), and the slide plate (4) and the guide post (5) are slidably connected.

8. The high-pressure hot bending forming device for a 3D curved PC mobile phone back cover according to claim 1, characterized in that, The first mounting frame (6) has a sliding groove (10), and the slider (12) is slidably connected to the sliding groove (10).

9. The high-pressure hot bending forming device for a 3D curved surface PC mobile phone back cover according to claim 1, characterized in that, A base (14) is fixedly installed on the main body (1), and the base (14) is fixedly connected to the first mounting frame (6).

10. A method for high-pressure hot bending forming of a 3D curved PC mobile phone back cover, comprising a high-pressure hot bending forming apparatus for a 3D curved PC mobile phone back cover as described in claims 1-9, characterized in that, Includes the following steps; S1. Blank preparation: Select optical grade PC sheet and precisely cut it according to the outer dimensions of the target mobile phone back cover to obtain a flat blank. Perform electrostatic dust removal pretreatment on the front and back surfaces of the blank to remove surface dust and cutting burrs. S2. Pre-cleaning of the forming working surface: Position the pre-treated blank at the opening of the forming groove (7) on the main body (1), start the cylinder (3) on the mounting plate (2) to drive the slide plate (4) to descend along the guide column (5). During the descent of the slide plate (4), the second rack (26) fixed to the main body (1) meshes with the second one-way gear (27) to drive the second reciprocating screw (28) in the second mounting frame (33) to rotate, and drive the negative pressure through the guide block (29) and the positioning plate (30). The cavity (31) moves laterally back and forth along the bottom surface of the heating plate (8), while the slide plate (4) drives the sealing plate (19) to slide in the mounting cavity (18) through the connecting rod (20) to generate negative pressure. The negative pressure is transmitted to the negative pressure cavity (31) through the second one-way valve (23), the second connecting pipe (24) and the filter chamber (25) in sequence, so that a continuous adsorption airflow is formed at the dust suction groove (32), and the dust and impurities of the entire working surface of the heating plate (8) are cleaned before the heating plate (8) contacts the blank. S3. High-pressure hot bending forming: The cylinder (3) continues to drive the slide plate (4) downward, and the heating plate (8) presses against the upper surface of the blank and heats the blank evenly, so that the temperature of the blank rises above the glass transition temperature and softens it fully; under the pressure output by the cylinder (3), the softened blank gradually adheres to the arc-shaped inner surface of the forming groove (7), maintaining the heating temperature at 130℃~160℃ and the forming pressure at 0.4MPa~0.8MPa, holding the pressure for 15s~30s, so that the blank is formed into the preset 3D curved surface shape; S4. Air-cooled shaping: After the pressure molding is completed, the cylinder (3) drives the slide plate (4) to move upward and reset. During the upward movement of the slide plate (4), the first rack (9) moves upward synchronously with the slide plate (4), meshes with the first one-way gear (13) and drives the first reciprocating screw (11) in the first mounting frame (6) to rotate. Through the slider (12) and the fixing plate (15), the cooling chamber (16) is driven to move laterally and reciprocally above the molding groove (7). At the same time, the slide plate (4) drives the sealing plate (19) to slide upward in the mounting cavity (18), compressing the air in the mounting cavity (18) to form a high-pressure airflow. The high-pressure airflow is introduced into the cooling chamber (16) through the first one-way valve (21) and the first connecting pipe (22). It is evenly sprayed onto the surface of the PC back cover after molding by multiple nozzles (17) at the bottom of the cooling chamber (16) to cool the workpiece in the whole area until the workpiece temperature drops below 60°C to complete the shaping. S5. Unloading and Removal: After the workpiece has cooled and solidified, the formed 3D curved PC mobile phone back cover is removed from the forming groove (7) to complete the single-cycle high-pressure hot bending forming process.