A platinum complex phosphorescent doped material and an organic electroluminescent device

By utilizing the rigid closed-loop chelate structure of platinum complex phosphorescent doped materials, the problems of molecular aggregation effect and excited state stability of platinum-based blue phosphorescent materials were solved, thereby improving the luminous efficiency and lifespan of blue OLED devices and achieving high color purity blue light emission.

CN123106779APending Publication Date: 2026-11-17JILIN OPTICAL & ELECTRONICS MATERIALS CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611475275.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing platinum-based blue phosphorescent materials suffer from problems such as intermolecular π-π stacking and aggregation quenching effects, excited-state distortion of the metal center under excited state, poor matching degree between radiative and non-radiative transition rates, and insufficient solubility and film-forming properties. These problems lead to low color purity, severe efficiency roll-off, short working life, and poor stability in blue OLED devices.

Method used

By employing platinum complex phosphorescent doping materials, phenyl groups are linked through imidazole or benzimidazole type carbene structures and electron-withdrawing groups are introduced to form a rigid closed-loop chelate system. This restricts the rotation and vibration of ligands in the excited state, thereby improving the photoluminescence quantum yield, stabilizing the excited state, suppressing the excited state of the metal center, and improving luminescence efficiency and lifetime.

Benefits of technology

It achieves high-purity blue light emission, improves the luminous efficiency and lifespan of OLED devices, and enhances the thermal stability and film-forming properties of materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106779A_ABST
    Figure CN123106779A_ABST
Patent Text Reader

Abstract

This invention discloses a platinum complex phosphorescent doped material and an organic electroluminescent device, relating to the field of organic electroluminescence technology. The platinum-containing complex provided by this invention can be used as a blue phosphorescent doped material in the luminescent layer, and the fabricated device exhibits excellent luminous efficiency and lifespan. The compound structure consists of an imidazole or benzimidazole linked to a phenyl group, then a carbazole is linked to an oxygen atom via bridging, and the N atom of the carbazole is further linked to a pyridine group. A rigid closed-loop chelate system (with a tetradentate ligand) is then formed through the central divalent platinum ion. This tetradentate ligand locks the entire coordination framework, greatly restricting the rotation and bending vibrations of the ligand in the excited state; reducing non-radiative dissipation caused by vibrational coupling, thus improving the PLQY of the thin film; the rigid structure also stabilizes the excited state, suppressing ³MC, and the rigid framework raises the ³MC energy level, allowing T1 to mainly remain in the ³LC / ³MLCT luminescent state, reducing excited-state chemical decomposition, and improving device lifespan.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of organic electroluminescence technology, and more specifically, to a platinum complex phosphorescent doped material and an organic electroluminescent device. Background Technology

[0002] Organic light-emitting diodes (OLEDs), with their superior characteristics such as self-emission, high contrast, fast response speed, flexibility, and low power consumption, have become the core technology for next-generation displays and solid-state lighting, widely used in smartphones, tablet terminals, automotive displays, flexible wearable devices, and high-end lighting. In the OLED three-primary-color luminescent system, the technologies for red and green phosphorescent doping materials and corresponding devices have matured, achieving industrialization with high efficiency, long lifespan, and high color purity. However, blue phosphorescent materials remain a key bottleneck restricting the overall performance improvement of full-color OLED displays and high-end lighting devices, and are also a focus and challenge in this field's technological research and development. Compared to the red and green light bands, blue light photons have higher energy, and the corresponding excited-state energy level range is larger, placing more stringent requirements on the energy level structure, excited-state stability, and non-radiative transition suppression capabilities of luminescent molecules.

[0003] Platinum (Pt)-based complexes, as typical planar four-coordinate heavy metal phosphorescent materials, possess unique photoelectric performance advantages and represent a core research direction for next-generation high-performance blue phosphorescent doped materials. Platinum atoms exhibit stronger spin-orbit coupling effects, effectively accelerating triplet exciton radiative transitions, shortening exciton lifetime, and significantly suppressing exciton quenching and non-radiative energy loss. Simultaneously, platinum complexes can precisely control HOMO / LUMO and triplet energy levels through ligand structure, accurately matching deep blue and pure blue emission bands, while also possessing narrow half-width and high color purity emission characteristics, perfectly meeting the technical requirements of high-definition wide color gamut displays. Furthermore, the rigid molecular framework of platinum complexes effectively reduces energy loss caused by molecular vibration and rotation, further improving luminescence quantum efficiency, and possessing great potential to replace traditional iridium-based blue phosphors.

[0004] Existing technologies have developed some blue phosphorescent materials such as cyclic metallized platinum complexes and tetradentate chelated platinum complexes. By optimizing the luminescence performance through ligand modification and molecular rigidity regulation, the luminescence efficiency and color purity of blue OLEDs have been improved to a certain extent. However, existing platinum-based blue phosphorescent materials still have significant technical defects and have not yet achieved mature industrial application: First, the planar molecular structure of most platinum complexes is prone to intermolecular π-π stacking and aggregation quenching effects, resulting in a sharp decline in luminous efficiency at high doping concentrations and poor device concentration adaptability; Second, some small-molecule platinum blue phosphorescent materials have insufficient molecular rigidity, which easily leads to metal center excited state distortion in the excited state, causing chemical bond relaxation and breakage, resulting in poor thermal and optical stability and short device lifespan; Third, existing platinum complex blue phosphorescent materials generally suffer from poor matching between radiative and non-radiative transition rates, resulting in low luminous quantum efficiency in the deep blue light band, making it difficult to break through the external quantum efficiency of devices, and failing to meet the dual requirements of high efficiency and long lifespan; Fourth, most platinum-based blue phosphorescent materials have poor solubility and film-forming properties, resulting in insufficient uniformity of vacuum evaporation film formation, which easily leads to film defects, further reducing the optoelectronic performance and stability of devices.

[0005] In summary, there is an urgent need in this field to develop a novel platinum-based blue phosphorescent doped material with strong structural stability, weak molecular aggregation effect, high luminescence quantum efficiency, suitable exciton lifetime, and excellent film-forming performance. This material is intended to address the technical problems of low color purity, severe efficiency roll-off, short working life, and poor stability in existing blue OLED devices, break through the technical bottleneck of blue phosphorescent OLEDs, and promote the high-performance and industrialization of full-color OLED devices.

[0006] In view of this, the present invention is proposed. Summary of the Invention

[0007] The purpose of this invention is to provide a platinum complex phosphorescent doped material and an organic electroluminescent device, which aims to improve the luminous efficiency and lifespan of the device.

[0008] This invention is implemented as follows: In a first aspect, the present invention provides a platinum complex phosphorescent doped material having a structure as shown in Formula I: ; Wherein, ring H indicates the absence of a benzene ring; R1 is selected from fluorinated phenyl, trifluoromethyl substituted phenyl, or cyano substituted phenyl; R2 is selected from hydrogen, deuterium, unsubstituted or deuterated C1-24 alkyl, unsubstituted or alkyl-substituted phenyl; R3-R6 are each independently selected from any one of hydrogen, deuterium, fluorine, trifluoromethyl, trimethylsilyl, substituted or unsubstituted C1-C24 alkyl, substituted or unsubstituted C3-C24 alicyclic alkyl, substituted or unsubstituted amino, and substituted or unsubstituted C6-C24 aryl.

[0009] In a second aspect, the present invention also provides an organic electroluminescent device, comprising an anode, a cathode, and at least one organic layer disposed between the anode and the cathode, the organic layer comprising a light-emitting layer containing a platinum complex phosphorescent dopant.

[0010] The present invention has the following beneficial effects: The platinum-containing complex provided by the present invention can be used as a blue phosphorescent dopant material in the luminescent layer, and the device prepared by it has excellent luminous efficiency and lifespan. The structure of this compound is an imidazole or benzimidazole (imidazole carbene structure) linked to a phenyl group (the phenyl group has an electron-withdrawing group F, CF3, CN substituted benzene ring at a specific position), and then a carbazole is linked to a bridging oxygen atom. The N of the carbazole is then linked to a pyridine group, and then a rigid closed-loop chelate system (with a tetradentate ligand) is formed through the central divalent platinum ion. The tetradentate ligand locks the entire coordination framework, greatly restricting the rotation and bending vibration of the ligand in the excited state; reducing nonradiative dissipation caused by vibrational coupling, and improving the PLQY (photoluminescence quantum yield) of the thin film; the rigid structure can also stabilize the excited state, suppress ³MC (metal center excited state), and the rigid framework raises the ³MC energy level, so that T1 is mainly maintained in the ³LC / ³MLCT luminescent state, reducing the chemical decomposition of the excited state and improving the device lifespan. Attached Figure Description

[0011] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation on the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.

[0012] Figure 1 This is the hydrogen nuclear magnetic resonance spectrum of compound 1 provided in Example 1 of this invention. Detailed Implementation

[0013] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.

[0014] Additionally, it should be noted that the values ​​given in the following embodiments are as accurate as possible. However, those skilled in the art will understand that due to unavoidable measurement errors and experimental issues, each number should be understood as an approximation rather than an absolutely accurate value.

[0015] In the following sections, the synthetic methods of the above-described compounds will be described by representative examples. However, the synthetic methods of the compounds of the present invention are not limited to those illustrated below; the compounds of the present invention can be prepared by the illustrated methods and methods known in the art.

[0016] This invention provides a platinum complex phosphorescent doped material having the structure shown in Formula I: ; Here, ring H represents either the absence of a benzene ring or a benzene ring; it can be absent or a benzene ring.

[0017] R1 is selected from fluorinated phenyl, trifluoromethyl substituted phenyl, or cyano substituted phenyl, and the number of fluorine, trifluoromethyl, and cyano groups can be 1, 2, 3, 4, or 5.

[0018] R2 is selected from hydrogen, deuterium, unsubstituted or deuterated C1-24 alkyl groups, and unsubstituted or alkyl-substituted phenyl groups. The alkyl group substituted with the phenyl group is selected from C1-C8 alkyl groups that can be deuterated.

[0019] R3-R6 are each independently selected from any one of hydrogen, deuterium, fluorine, trifluoromethyl, trimethylsilyl, substituted or unsubstituted C1-C24 alkyl, substituted or unsubstituted C3-C24 alicyclic alkyl, substituted or unsubstituted amino, and substituted or unsubstituted C6-C24 aryl. R3-R6 can be any one or more of the above.

[0020] The substituents in Formula I can be the largest number of substitutions in the ring, and any H in Formula I can be deuterated.

[0021] In some embodiments, depending on the presence or absence of ring H, the platinum complex phosphorescent doped material has a structure as shown in formula IA or formula IB: .

[0022] In a preferred embodiment, R1 is selected from the following groups: .

[0023] Preferably, in R2, the alkyl group substituted with the phenyl group is selected from C1-C8 alkyl groups that can be substituted with deuterium. More preferably, R2 is selected from hydrogen, deuterium, unsubstituted or deuterated C1-10 alkyl groups, and unsubstituted or alkyl-substituted phenyl groups. The C1-C10 alkyl groups and the alkyl group substituted with the phenyl group are selected from the following groups that can be substituted with deuterium: methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, sec-butyl, 1-methylbutyl, 1-ethylbutyl, n-pentyl, isopentyl, neopentyl, tert-pentyl, n-hexyl, 1-methylpentyl, 2-methylpentyl, 4-methyl-2-pentyl, 3,3-dimethylbutyl, 2-ethylbutyl, 1-methylhexyl, cyclopropane, cyclobutane, cyclopentane, and cyclohexane, and can be any one or a combination of several of the above groups.

[0024] More preferably, R3-R6 are each independently selected from any one of hydrogen, deuterium, fluorine, trifluoromethyl, trimethylsilyl, substituted or unsubstituted C1-C10 alkyl, substituted or unsubstituted C3-C12 alicyclic alkyl, substituted or unsubstituted amino, and substituted or unsubstituted C6-C18 aryl. R3-R6 can be the same or different, and can be any one of the above independently.

[0025] More preferably, R3-R6 are each independently selected from hydrogen, deuterium, fluorine, trifluoromethyl, deuterated or unsubstituted methyl, deuterated or unsubstituted ethyl, deuterated or unsubstituted n-propyl, deuterated or unsubstituted isopropyl, deuterated or unsubstituted n-butyl, deuterated or unsubstituted isobutyl, deuterated or unsubstituted tert-butyl, deuterated or unsubstituted sec-butyl, deuterated or unsubstituted n-pentyl, deuterated or unsubstituted isopentyl, deuterated or unsubstituted... The following are all of the following: neopentyl, deuterated or unsubstituted tert-pentyl, deuterated or unsubstituted hexyl, deuterated or unsubstituted cyclopropane, deuterated or unsubstituted cyclobutane, deuterated or unsubstituted cyclopentane, deuterated or unsubstituted cyclohexane, substituted or unsubstituted dimethylamino, substituted or unsubstituted phenyl, substituted or unsubstituted biphenyl, substituted or unsubstituted terphenyl, substituted or unsubstituted naphthyl, substituted or unsubstituted phenanthryl, and substituted or unsubstituted anthracene.

[0026] Wherein, the "substituted" group in the substituted or unsubstituted form is selected from one or at least two of the following substituents or at least two connected substituents: hydrogen, deuterium, fluorine, cyano, trifluoromethyl, methyl, ethyl, -CD3, -CF3, -CH2F, -CHF2, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, sec-butyl, 1-methylbutyl, 1-ethylbutyl, n-pentyl, isopentyl, neopentyl, tert-pentyl, n-hexyl, 1-methylpentyl, 2-methylpentyl, 4-methyl-2-pentyl, 3,3-dimethylbutyl, 2-ethylbutyl, 1-methylhexyl, phenyl, biphenyl, naphthyl, anthracene, phenanthrene, cyclopropane, cyclobutane, cyclopentane, cyclohexane, and adamantyl.

[0027] In some embodiments, the platinum complex phosphorescent dopant is a blue phosphorescent dopant, and the platinum complex phosphorescent dopant is selected from any of the compounds shown in the following structural formulas, but is not limited thereto: .

[0028] The platinum-containing complex provided by this invention can be applied to organic electroluminescent devices as a blue phosphorescent dopant in the luminescent layer, resulting in devices with excellent luminous efficiency and lifespan. The compound structure consists of an imidazole or benzimidazole (imidazole-type carbene structure) linked to a phenyl group (with electron-withdrawing groups F, CF3, or CN substituted at specific positions on the phenyl ring), then a carbazole is linked via a bridging oxygen atom. The N atom of the carbazole is then linked to a pyridine group, forming a rigid closed-loop chelate system (with a tetradentate ligand) through a central divalent platinum ion. This tetradentate ligand locks the entire coordination framework, greatly limiting the rotation and bending vibrations of the ligand in the excited state; reducing non-radiative dissipation caused by vibrational coupling, and improving the PLQY (photoluminescence quantum yield) of the thin film; the rigid structure also stabilizes the excited state, suppressing the ³MC (metal-centered excited state), and the rigid framework raises the ³MC energy level, allowing T1 to mainly remain in the ³LC / ³MLCT luminescent state, reducing excited-state chemical decomposition and improving device lifespan.

[0029] Among them, the imidazole-type carbene structure NHC is a strong σ-donor ligand, which can regulate the HOMO / LUMO orbital distribution, distributing more HOMO in the NHC-carbazole segment and LUMO in the pyridine segment. The HOMO-LUMO band gap is large enough to push the emission wavelength into the blue / deep blue light range. The strong bonding between NHC and Pt increases the bond dissociation energy of the Pt-ligand bond, further resisting exciton-induced degradation under high brightness. Further attaching substituent groups to the N on the imidazole-type carbene structure allows for outward stereotactic extension, constructing a steric barrier around the molecule, separating adjacent luminescent molecules, and inhibiting intermolecular π-π stacking. Even at high doping concentrations, no excitoassociations are formed, resulting in a narrow spectrum and high color purity. Simultaneously, reduced concentration quenching allows for higher doping ratios, facilitating carrier recombination. It also improves molecular thermal stability, vacuum evaporation processability, and material solubility / film formation. Furthermore, devices fabricated with an imidazole-type carbene structure combined with a benzene structure (benzimidazole) exhibit superior performance. The pyridine-carbazole coordination structure also has a suitable triplet energy for blue light emission and a narrow spectral emission property. This gives these compounds a narrow blue phosphorescence emission spectrum, which can promote the emission color and improve the performance of blue phosphorescent devices.

[0030] Furthermore, electron-withdrawing groups (cyano, fluorine, trifluoromethyl) can lower the LUMO energy level, regulate the orbital distribution of HOMO-LUMO and triplet ³MLCT / ³LC (metal-to-ligand charge transfer + ligand local excitation), suppress excessive orbital delocalization, prevent redshift of emission, and more easily obtain high-purity deep blue emission. This invention places electron-withdrawing groups on the outer benzene ring, making only minor orbital adjustments without disrupting the conjugation and T1 energy levels of the coordination framework; simultaneously, it enhances π-feedback, raises the ³MC state energy level, suppresses non-radiative decay from T1 to ³MC, and improves photoluminescence quantum yield. It also maintains a higher ³MLCT / ³LC (ligand local excitation) ratio, resulting in better spin-orbit coupling, higher radiative transition rates, and shorter excited-state lifetimes; the shorter excited-state lifetime reduces triplet-triplet annihilation (TTA) and triplet-polaron annihilation (TPA), lowering efficiency roll-off. In addition, it forms a stereoscopic shield on the outside of the molecule, increasing intermolecular distance, suppressing planar molecular stacking, and weakening aggregation quenching.

[0031] The platinum complexes of the present invention can be prepared by synthetic methods known to those skilled in the art. Alternatively, the following reaction process is preferred for preparation:

[0032] In the above formula, R1-R6 and H are as defined in the above chemical formula I, where X represents or .

[0033] In contrast to the complex raw materials that are not publicly available, the synthesis will be carried out using classic Suzuki coupling reaction, Buchwald-Hartwig coupling reaction, metal coordination reaction, etc., and will be applied in this invention.

[0034] Specific preparation method: Step 1 specifically includes the following processes: Under nitrogen protection, raw material A (1.00-1.10 eq) and raw material B (1.00 eq) were added and dissolved in N,N-dimethylformamide (DMF), followed by potassium carbonate (K2CO3) (2.00-4.00 eq). The mixture was heated to 150 °C and reacted for 2-8 h. After the reaction was complete, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. After concentration, the product was separated by silica gel to obtain intermediate 1.

[0035] Step 2 specifically includes the following processes: Under nitrogen protection, intermediate 1 (1.00 eq) and starting material C (1.00-1.10 eq) were dissolved in DMF, and K2CO3 (2.00-4.00 eq) was added. The mixture was heated to 150 °C and reacted for 2-8 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. After concentration, the product was separated by silica gel to obtain intermediate 2.

[0036] Step 3 specifically includes the following processes: Under nitrogen protection, intermediate 2 (1.00 eq) and starting material D (1.00-1.10 eq) were added and dissolved in a mixed solvent of dioxane and water (Dioxane / H2O). K2CO3 (2.00-4.00 eq) and tetrakis(triphenylphosphine)palladium (Pd(pph3)4) (0.01-0.04 eq) were added, and the mixture was heated to 90-95 °C and reacted for 2-10 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. After concentration, the product was separated by silica gel to obtain intermediate 3.

[0037] Step 4 specifically includes the following processes: Under nitrogen protection, intermediate 3 (1.00 eq) and starting material E (2.00-3.00 eq) were added and dissolved in dioxane, followed by the addition of anhydrous copper acetate (Cu(OAc)2) (0.10-0.30 eq). The mixture was heated to 110-120 °C and reacted for 2-10 h. After the reaction was complete, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. The product was then concentrated and separated by silica gel to obtain intermediate 4.

[0038] Step 5 specifically includes the following processes: Under nitrogen protection, intermediate 4 (1.00 eq) and cyclooctadiene platinum chloride (Pt(COD)Cl2) (1.10-1.30 eq) were added and dissolved in DMF. Sodium acetate (NaOAc) (2.00-4.00 eq) was added, and the mixture was heated to 100-110 °C and reacted for 2-10 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with ethyl acetate / water. After concentration, the product was separated by silica gel to obtain chemical formula I.

[0039] Another objective of this application is to provide an organic electroluminescent device, comprising an anode, a cathode, and at least one organic layer disposed between the anode and the cathode, wherein the organic layer includes a light-emitting layer and the light-emitting layer contains the aforementioned platinum-containing complex; Preferably, the light-emitting layer comprises a host material and a dopant material, wherein the dopant material contains a platinum-containing complex; the mass ratio of the host material to the dopant material in the light-emitting layer is 90-99.5:0.5-10, for example 90:10, 92:8, 95:5, 97:3, 98:2, 99:1 or 99.5:0.5.

[0040] Furthermore, the main material is an aromatic fused-ring derivative or a heterocyclic compound; wherein the aromatic fused-ring derivative is anthracene derivative, pyrene derivative, naphthalene derivative, pentane derivative, phenanthrene compound, or fluoranthene compound; and the heterocyclic compound is carbazole derivative, dibenzofuran derivative, or pyrimidine derivative.

[0041] Furthermore, the organic layer also includes at least one of a hole injection layer, a hole transport layer, an electron blocking layer, a light-emitting auxiliary layer, a hole blocking layer, an electron transport layer, or an electron injection layer.

[0042] The organic material layer of the organic light-emitting device disclosed herein can be formed as a single-layer structure, but it can also be formed as a multilayer structure with one or more organic material layers. For example, the organic light-emitting device of this disclosure can have a structure that includes a hole injection layer, a hole transport layer, an electron blocking layer, a light-emitting auxiliary layer, a light-emitting layer, an electron transport layer, an electron injection layer, and a hole blocking layer as organic material layers. However, the structure of the organic light-emitting device is not limited to this, and it can include fewer or more organic material layers.

[0043] Furthermore, the organic layer is prepared using vacuum evaporation or solution coating methods, including spin coating, dip coating, blade coating, inkjet printing, screen printing, spray coating, and roll coating.

[0044] Furthermore, depending on the material used, the organic light-emitting element of the present invention is one of a top-emitting type, a bottom-emitting type, or a bidirectional-emitting type.

[0045] Finally, the devices described in this application can be used in organic light-emitting devices, including but not limited to flat panel displays, computer monitors, a medical monitor, a television set, billboards, a lamp for internal or external lighting and / or signaling, head-up displays, fully transparent or partially transparent displays, flexible displays, a laser printer, a telephone, a mobile phone, a photo album, a personal digital assistant (PDA), a wearable device, a laptop computer, a digital camera, a camcorder, a viewfinder, a microdisplay, a 3D display, a virtual reality or augmented reality display, vehicles, video walls including multiple displays tiled together, theater or stadium screens, phototherapy devices, and signs.

[0046] As an anode material, a material with a high work function is preferred in order to facilitate the injection of holes into the organic layer. Specific examples of anode materials that can be used in this invention include metals such as vanadium, chromium, copper, zinc, and gold, or their alloys; metal oxides such as zinc oxide, indium oxide, indium tin oxide (ITO), and indium zinc oxide (IZO); and combinations of metals and oxides such as ZnO:Al or SnO2:Sb.

[0047] The hole injection layer is preferably a p-doped hole injection layer, which means a hole injection layer doped with a p-doped agent. A p-doped agent is a material that can impart p-type semiconductor characteristics. P-type semiconductor characteristics refer to the characteristics of injecting or transporting holes at the HOMO energy level, that is, the characteristics of a material with high hole conductivity.

[0048] Hole transport materials are materials capable of receiving holes from the anode or hole injection layer and transporting them to the light-emitting layer; they are materials with high hole mobility. Hole transport materials can be selected from aryl amine derivatives, conductive polymers, and block copolymers containing both conjugated and non-conjugated parts.

[0049] An auxiliary light-emitting layer (multilayer hole transport layer) is added between the hole transport layer and the light-emitting layer. The auxiliary light-emitting layer primarily assists the hole transport layer and is therefore sometimes referred to as a second hole transport layer. This layer allows holes transferred from the anode to smoothly move to the light-emitting layer and blocks electrons transferred from the cathode, confining them within the light-emitting layer. This reduces the potential barrier between the hole transport layer and the light-emitting layer, lowers the driving voltage of the organic light-emitting device, and further increases hole utilization, thereby improving the device's luminous efficiency and lifetime.

[0050] An electron transport layer can facilitate electron transport. The electron transport material is one that advantageously receives electrons from the cathode and transports them to the light-emitting layer, preferably a material with high electron mobility. The electron transport layer may include at least one of an electron buffer layer, a hole blocking layer, an electron transport layer, and an electron injection layer, and preferably at least one of an electron transport layer and an electron injection layer.

[0051] The electron injection layer can promote electron injection and prevent excitons generated in the light-emitting layer from migrating to the hole injection layer. Materials for the electron injection layer include, but are not limited to, oxazoles, oxadiazoles, triazoles, imidazoles, perylenetetracarboxylic acids, fluorenemethane, anthrones and their derivatives, metals such as magnesium, calcium, sodium, potassium, titanium, indium, yttrium, lithium, gadolinium, aluminum, silver, tin, ytterbium, or their alloys, metal complexes, or nitrogen-containing 5-membered ring derivatives.

[0052] The cathode is typically made of a material with a low work function to facilitate electron injection into the organic material layer, the thickness of which is preferably between 0.5 and 5 nm. The cathode material is generally preferred to have a low work function in order to facilitate electron injection into the organic layer. Specific examples of cathode materials include metals such as magnesium, calcium, sodium, potassium, titanium, indium, yttrium, lithium, gadolinium, aluminum, silver, tin, and lead, or their alloys; among which, alloys are selected from multilayer structures such as LiF / Al or LiO2 / Al, Mg / Ag, etc.

[0053] Except for the doped material layer containing chemical formula I disclosed in this article, there are no special restrictions on other layer materials in OLED devices.

[0054] The features and performance of the present invention will be further described in detail below with reference to embodiments.

[0055] Example 1 The synthesis route in this embodiment is as follows:

[0056] Raw material E-1 is synthesized first, and the process is as follows: Under nitrogen protection, feedstock a-1 (3,5-di-tert-butyl-1-iodobenzene, CAS No.: 37055-53-1) (1.00 eq) and m-chloroperoxybenzoic acid (mCPBA) (1.20 eq) were added and dissolved in dichloromethane. The mixture was cooled to -5°C and reacted for 0.5 h. Then, the temperature was raised to room temperature and stirred for 1 h. Feedstock b-1 (1,3,5-trimethylbenzene, CAS No.: 108-67-8) (1.50 eq) was added. After cooling to -5°C, trifluoromethanesulfonic acid (TfOH) (2.00 eq) was added dropwise, and the mixture was reacted for 0.5 h. The temperature was then raised to room temperature and stirred for another 12 h. After the reaction was complete, sodium bicarbonate aqueous solution was added to neutralize the excess acid and adjust the pH to neutral. The organic phase was separated and collected using a separatory funnel, concentrated, and then separated by silica gel (polar DMC:PE = 1:10) to obtain the desired feedstock E-1 (yield 95.1%).

[0057] Step 1 specifically includes the following processes: Under nitrogen protection, starting materials A-1 (1.05 eq, CAS No.: 461-96-1) and B-1 (1.00 eq, CAS No.: 1636130-34-1) were added and dissolved in N,N-dimethylformamide (DMF), followed by potassium carbonate (K2CO3) (2.00 eq). The mixture was heated to 150 °C and reacted for 4 h. After the reaction was complete, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. The product was concentrated and separated by silica gel (polar DCM:PE = 1:3) to obtain intermediate 1-1 (yield 80.9%).

[0058] Step 2 specifically includes the following processes: Under nitrogen protection, intermediate 1-1 (1.00 eq) and starting material C-1 (1.05 eq, CAS No.: 288-32-4) were dissolved in DMF, and K2CO3 (2.00 eq) was added. The mixture was heated to 150 °C and reacted for 4 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. After concentration, the product was separated by silica gel (polar DCM:MeOH = 100:1) to obtain intermediate 2-1 (yield 81.2%).

[0059] Step 3 specifically includes the following processes: Under nitrogen protection, intermediate 2-1 (1.00 eq) and starting material D-1 (1.02 eq, CAS No.: 73852-19-4) were added and dissolved in a mixed solvent of dioxane and water (Dioxane / H2O). K2CO3 (2.00 eq) and tetrakis(triphenylphosphine)palladium (Pd(pph3)4) (0.02 eq) were added, and the mixture was heated to 90 °C and reacted for 4 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. After concentration, the product was separated by silica gel (polar DCM:MeOH = 100:1) to obtain intermediate 3-1 (yield 95.5%).

[0060] Step 4 specifically includes the following processes: Under nitrogen protection, intermediate 3-1 (1.00 eq) and starting material E-1 (2.00 eq) were added and dissolved in dioxane, followed by the addition of anhydrous copper acetate (Cu(OAc)2) (0.10 eq). The mixture was heated to 110 °C and reacted for 4 h. After the reaction was complete, the solvent was evaporated under reduced pressure, and the product was extracted with dichloromethane / water. The product was concentrated and separated by silica gel (polar DCM:MeOH = 1:30) to obtain intermediate 4-1 (yield 90.8%).

[0061] Step 5 specifically includes the following processes: Under nitrogen protection, intermediate 4-1 (1.00 eq) and cyclooctadiene platinum chloride (Pt(COD)Cl2) (1.10 eq) were added and dissolved in DMF. Sodium acetate (NaOAc) (3.00 eq) was added, and the mixture was heated to 100 °C and reacted for 4 h. After the reaction was completed, the solvent was evaporated under reduced pressure, and the product was extracted with ethyl acetate / water. The product was concentrated and separated by silica gel (polar DCM:PE = 1:3) to give compound 1 (yield 60.6%).

[0062] The obtained compound 1 was analyzed, and the results are as follows: HPLC purity: >99.5%.

[0063] Mass spectrometry test: Waters XEVO TQD mass spectrometer with ESI source.

[0064] Test value MS(ESI, m / Z): [M+H] + =1052.49 Elemental analysis: The test values ​​were: C, 58.96; H, 4.60; F, 10.90; N, 5.43; O, 1.61; Pt, 18.62.

[0065] In addition, it should be noted that other compounds of the present invention can be obtained by referring to the synthesis methods of the embodiments listed above, so they will not be listed one by one here.

[0066] Device Example 1: Fabrication of Blue Organic Light Emitting Device OLEDs are grown on glass substrates pre-coated with an indium tin oxide (ITO) layer. Before any organic layer deposition or coating, the glass substrate undergoes ultrasonic cleaning using DI-Water, followed by a baking process. All devices are grown in a high-vacuum environment (vacuum level below 10). -7 It is prepared by hot evaporation process under torr).

[0067] a. ITO anode: Using an ITO (indium tin oxide) glass substrate with a coating thickness of 1500 Å as the anode, other functional layers are sequentially deposited on it. b. HIL (hole injection layer): Hole injection layer material HI with a thickness of 100 Å is vacuum-deposited on the anode at a deposition rate of 1.0 Å / s as the hole injection layer. c. HTL (Hole Transport Layer): Hole transport material HT of 250 Å is vacuum-deposited on the hole injection layer at a deposition rate of 1.0 Å / s to serve as the hole transport layer. d. EBL (Electron Blocking Layer): An electron blocking material EB with a thickness of 50 Å is vacuum-deposited at a deposition rate of 0.5 Å / s as an electron blocking layer. e. EML (Light Emitting Layer): A host material with a total thickness of 300 Å and compound 1 are vacuum-deposited at a deposition rate of 1.0 Å / s as dopant materials for the light emitting layer. The deposition rate ratio of the host material to compound 1 is 90:10. f. HBL (hole blocking layer): A hole blocking material HB with a thickness of 50 Å is vacuum-deposited on the light-emitting layer at a deposition rate of 0.5 Å / s as a hole blocking layer. g. ETL (Electron Transport Layer): ET and Liq with a total thickness of 300 Å were vacuum-deposited on the hole blocking layer at a deposition rate of 1 Å / s as the electron transport layer; the deposition rate ratio of ET to EI (Liq) was 65:35. h. EIL (Electron Injection Layer): An EI (Liq) layer with a total thickness of 10 Å is deposited on the electron transport layer at a deposition rate of 0.5 Å / s as the electron injection layer; i. Cathode: At a deposition rate of 2 Å / s, metallic Al with a total thickness of 1000 Å is vacuum-deposited on the electron injection layer to form a cathode; The substrate after vapor deposition is packaged. First, the cleaned cover plate is coated with UV adhesive using an adhesive coating equipment. Then, the coated cover plate is moved to the lamination section, and the vapor-deposited substrate is placed on the top of the cover plate. Finally, the substrate and cover plate are laminated under the action of the lamination equipment, and the UV adhesive is cured by light.

[0068] The material structures involved in the device fabrication process are shown below:

[0069] Referring to the method provided in Device Example 1 above, the corresponding compounds in Table 1 below were selected to replace Compound 1, and the doped material layer was deposited by vapor deposition to prepare the corresponding organic electroluminescent devices, which are respectively referred to as Device Examples 2-94.

[0070] Device Comparison Examples 1-16: This comparative example provides an organic electroluminescent device. The only difference between this organic electroluminescent device and device example 1 is that the organic electroluminescent device uses the existing comparative compound ap instead of the dopant material (compound 1) in device example 1 for vapor deposition. The chemical structural formula of the comparative compound ap is as follows:

[0071] At a brightness of 1000 nits, the luminous efficiency and lifetime of the organic electroluminescent devices obtained in the above-mentioned device examples 1-94 and device comparative examples 1-16 were characterized, and the test results are shown in Table 1.

[0072] Table 1 Device Test Results

[0073] As can be seen from Table 1, the compound represented by chemical formula I in this invention has excellent luminescent properties, and the organic electroluminescent device prepared with it has excellent luminescent efficiency and lifespan. Compared with the organic electroluminescent device prepared with the comparative compound, the performance is significantly improved.

[0074] Comparative compounds ae, op, and compounds 81, 179, 554, 385, 337, 379, and 475 are parallel comparative examples. The difference lies in the structure: in the comparative compounds, the benzene ring on the lower left side has no substituents, only one phenyl group, or only a single cyano, fluorine, or trifluoromethyl group, while in the compounds of this invention, the phenyl group at the corresponding position has one phenyl group substituted by a cyano, fluorine, or trifluoromethyl group. The presence of electron-withdrawing groups (cyano, fluorine, trifluoromethyl) can lower the LUMO energy level, regulate the HOMO-LUMO and triplet state ³MLCT / ³LC (metal-to-ligand charge transfer + ligand local excitation) orbital distribution, suppress excessive orbital delocalization, prevent redshift of emission, and more easily obtain high-purity deep blue emission. Devices fabricated with structures containing electron-withdrawing groups exhibit superior performance compared to structures without electron-withdrawing groups. However, directly attaching electron-withdrawing groups to the conjugated ring near Pt can over-stabilize LUMO, lower the S1 / T1 energy level, cause a redshift in emission, and make it difficult to maintain deep blue light. Simultaneously, it increases the proportion of ³MC (metal-centric excited states), leading to non-radiative transitions and molecular structure distortion, resulting in rapid device lifetime decay. The structure of this invention places the electron-withdrawing group on the outer benzene ring, making only orbital fine-tuning without disrupting the conjugation and T1 energy levels of the coordination framework. It also enhances π-feedback, raising the ³MC state energy level, suppressing non-radiative decay from T1 to ³MC, and improving photoluminescence quantum yield. Furthermore, it maintains a higher ³MLCT / ³LC (ligand-localized excited states) ratio, resulting in better spin-orbit coupling, higher radiative transition rates, and shorter excited-state lifetimes. Short excited-state lifetimes reduce triplet-triplet annihilation (TTA) and triplet-polaron annihilation (TPA), reducing efficiency roll-off. In addition, a stereoscopic shield is formed on the outer side of the molecule, increasing intermolecular distance, suppressing planar molecular stacking, and weakening aggregation quenching.

[0075] Comparative examples f and 481 are parallel comparative examples. The difference lies in that the lower left benzene ring in compound 481 only has an electron-withdrawing group (cyano) substitution, while the corresponding benzene ring in comparative compound f also has two methyl groups. The steric repulsion of the methyl groups causes dihedral torsion between the cyanophenyl group and the parent benzene ring, disrupting the conjugated planarity and weakening the conjugated coupling. Simultaneously, the methyl group is a weak electron-donating group, which partially offsets the electron-withdrawing effect of -CN, leading to LUMO elevation, changes in the HOMO-LUMO gap, and a shift in the T1 energy level. This makes the emission more prone to redshift or spectral broadening, resulting in decreased color purity. It also weakens the electron transport capability of the material, easily causing carrier imbalance, exciton concentration at the interface, exacerbating exciton quenching, and affecting device performance.

[0076] Comparative compounds h and i and compounds 513 and 394 are parallel comparative examples. The difference is that in the structure of compounds 513 and 394 of the present invention, the substituents attached to the imidazole on the left side contain only substituted phenyl groups (containing at most one substituted or unsubstituted benzene ring), while in the structure of comparative compounds h and i, there is more than one benzene ring at the corresponding position, with larger polycyclic aromatic ring conjugated segments. The aromatic rings are more likely to stack π-stacking, and the large conjugated substituents will change the frontier orbital distribution, increase the ³MLCT component, and lengthen the excited state lifetime. Under high brightness, triplet-polaron annihilation is more likely to occur, causing efficiency roll-off, thereby leading to a decrease in device performance.

[0077] The above description of the disclosed embodiments enables those skilled in the art to make or use the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A platinum complex phosphorescent doped material, characterized in that, The platinum complex phosphorescent doped material has the structure shown in Formula I: ; Wherein, ring H indicates the absence of a benzene ring; R1 is selected from fluorinated phenyl, trifluoromethyl substituted phenyl, or cyano substituted phenyl; R2 is selected from hydrogen, deuterium, unsubstituted or deuterated C1-24 alkyl, unsubstituted or alkyl-substituted phenyl; R3-R6 are each independently selected from any one of hydrogen, deuterium, fluorine, trifluoromethyl, trimethylsilyl, substituted or unsubstituted C1-C24 alkyl, substituted or unsubstituted C3-C24 alicyclic alkyl, substituted or unsubstituted amino, and substituted or unsubstituted C6-C24 aryl.

2. The platinum complex phosphorescent doped material according to claim 1, characterized in that, The platinum complex phosphorescent doped material has a structure as shown in formula IA or formula IB: 。 3. The platinum complex phosphorescent doped material according to claim 1 or 2, characterized in that, R1 is selected from the following groups: 。 4. The platinum complex phosphorescent doped material according to claim 1 or 2, characterized in that, R2 is selected from hydrogen, deuterium, unsubstituted or deuterated C1-10 alkyl, unsubstituted or alkyl-substituted phenyl; Wherein, the C1-C10 alkyl and substituted phenyl alkyl groups are selected from at least one of the following groups: methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, sec-butyl, 1-methylbutyl, 1-ethylbutyl, n-pentyl, isopentyl, neopentyl, tert-pentyl, n-hexyl, 1-methylpentyl, 2-methylpentyl, 4-methyl-2-pentyl, 3,3-dimethylbutyl, 2-ethylbutyl, 1-methylhexyl, cyclopropane, cyclobutane, cyclopentane, and cyclohexane.

5. The platinum complex phosphorescent doped material according to claim 1 or 2, characterized in that, R3-R6 are each independently selected from any one of hydrogen, deuterium, fluorine, trifluoromethyl, trimethylsilyl, substituted or unsubstituted C1-C10 alkyl, substituted or unsubstituted C3-C12 alicyclic alkyl, substituted or unsubstituted amino, and substituted or unsubstituted C6-C18 aryl.

6. The platinum complex phosphorescent doped material according to claim 5, characterized in that, R3-R6 are each independently selected from hydrogen, deuterium, fluorine, trifluoromethyl, deuterated or unsubstituted methyl, deuterated or unsubstituted ethyl, deuterated or unsubstituted n-propyl, deuterated or unsubstituted isopropyl, deuterated or unsubstituted n-butyl, deuterated or unsubstituted isobutyl, deuterated or unsubstituted tert-butyl, deuterated or unsubstituted sec-butyl, deuterated or unsubstituted n-pentyl, deuterated or unsubstituted isopentyl, and deuterated or unsubstituted neopentyl. The following are all of the following: tert-amyl (deuterated or unsubstituted), hexyl (deuterated or unsubstituted), cyclopropane (deuterated or unsubstituted), cyclobutane (deuterated or unsubstituted), cyclopentane (deuterated or unsubstituted), cyclohexane (deuterated or unsubstituted), dimethylamino (substituted or unsubstituted), phenyl (substituted or unsubstituted), biphenyl (substituted or unsubstituted), terphenyl (substituted or unsubstituted), naphthyl (substituted or unsubstituted), phenanthryl (substituted or unsubstituted), and anthracene (substituted or unsubstituted).

7. The platinum complex phosphorescent doped material according to claim 6, characterized in that, The substituted or unsubstituted group is selected from at least one of the following: hydrogen, deuterium, fluorine, cyano, trifluoromethyl, methyl, ethyl, -CD3, -CF3, -CH2F, -CHF2, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, sec-butyl, 1-methylbutyl, 1-ethylbutyl, n-pentyl, isopentyl, neopentyl, tert-pentyl, n-hexyl, 1-methylpentyl, 2-methylpentyl, 4-methyl-2-pentyl, 3,3-dimethylbutyl, 2-ethylbutyl, 1-methylhexyl, phenyl, biphenyl, naphthyl, anthracene, phenanthrene, cyclopropane, cyclobutane, cyclopentane, cyclohexane, and adamantyl.

8. The platinum complex phosphorescent doped material according to any one of claims 1 to 7, characterized in that, The platinum complex phosphorescent doped material is selected from any one of the compounds shown in the following structural formulas: 。 9. An organic electroluminescent device, characterized in that, It includes an anode, a cathode, and at least one organic layer disposed between the anode and the cathode, the organic layer including a light-emitting layer containing the platinum complex phosphorescent dopant.

10. The organic electroluminescent device according to claim 9, characterized in that, The light-emitting layer further includes a host material and a doping material, wherein the doping material includes the platinum complex phosphorescent doping material; In the light-emitting layer, the mass ratio of the host material to the doped material is (90-99.5):(0.5-10).