A papermaking wastewater treatment agent and its preparation method

By controlling the isoelectric point and composition of the papermaking wastewater treatment agent, and utilizing the prepolymerization reaction of acrylamide, cationic monomers, and hydrophobic monomers, a highly efficient flocculant is formed, which solves the problem of reduced treatment efficiency caused by interference from soluble lignin and achieves a highly efficient flocculation effect with low dosage.

CN123106985APending Publication Date: 2026-11-17JIANGXI FUHONG PAPER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611563417.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-10
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing papermaking wastewater treatment agents suffer from reduced treatment efficiency when faced with soluble lignin interference, leading to increased flocculant dosage, higher sludge production, and higher operating costs. Existing technologies offer limited compensation.

Method used

Acrylamide, cationic monomers, and hydrophobic monomers were prepolymerized under an inert atmosphere. Anionic monomers were added and the temperature was raised for polymerization. The isoelectric point was controlled at 4.5-5.5 to form a cationic-rich prepolymer backbone. Soluble lignin was neutralized under pH matching to form micro-flocs.

Benefits of technology

It achieves efficient flocculation with low dosage, with fast floc settling speed, high turbidity and COD removal rate, and reduces flocculant dosage and operating costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention relates to the field of water treatment materials technology. More specifically, it relates to a papermaking wastewater treatment agent and its preparation method. The specific preparation steps of this invention include: prepolymer preparation: acrylamide, cationic monomer, and hydrophobic monomer are dispersed in water, and then an initiator is added under an inert atmosphere, and the reaction is carried out at a temperature of 40-50℃ for 1-3 hours to obtain a prepolymer; polymerization reaction: anionic monomer is added, and an initiator is added, then the temperature is raised to 55-60℃, and the reaction is continued for 2-3 hours. After naturally cooling to room temperature, acetone is added to precipitate, and the mixture is washed and dried to obtain the papermaking wastewater treatment agent; the molar ratio of the cationic monomer to the anionic monomer is 1.2-1.5:1, and the isoelectric point of the papermaking wastewater treatment agent is 4.5-5.5. The molar amounts of the following raw materials are: acrylamide 75-80 parts, cationic monomer 8-18 parts, anionic monomer 5-12 parts, and hydrophobic monomer 0.5-2 parts.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of water treatment materials technology. More specifically, it relates to a papermaking wastewater treatment agent and its preparation method. Background Technology

[0002] Currently, the treatment of papermaking wastewater commonly employs coagulation and sedimentation processes, involving the combined use of inorganic flocculants (such as polyaluminum chloride and aluminum sulfate) and organic polymeric flocculants (such as polyacrylamide). However, with the increasing closed-loop nature of papermaking systems, dissolved lignin and anionic waste accumulate in the process water, posing a serious challenge to existing treatment systems. Studies have shown that dissolved lignin is the component in papermaking process water that is most detrimental to the effectiveness of chemical additives. Its strong negative surface charge preferentially neutralizes cationic flocculants, preventing flocculant molecules from effectively bridging suspended particles, leading to a sharp decline in treatment efficiency and a significant increase in flocculant dosage.

[0003] To address this issue, existing technologies attempt to compensate for lignin interference by increasing the cationicity of the flocculant or increasing its dosage, but the effects are limited and lead to increased sludge production and operating costs. Another approach uses enzyme-catalyzed pretreatment (such as laccase) to promote lignin polymerization, followed by removal with cationic polymers; however, enzyme preparations are expensive and require stringent reaction conditions, making stable industrial-scale application difficult. Furthermore, some solutions combine flocculants with adsorbents such as activated calcium silicate, which can remove some pollutants through physical adsorption, but lacks sufficient targeted capture capability for dissolved lignin.

[0004] Therefore, there is an urgent need to develop a papermaking wastewater treatment agent that can effectively overcome the interference of dissolved lignin and achieve efficient flocculation at low dosage, in order to solve the key technical problems of the flocculant efficiency being inhibited by anionic waste and the high treatment cost in the existing technology. Summary of the Invention

[0005] The technical problem this invention aims to solve is to address the shortcomings of existing papermaking wastewater treatment agents mentioned above. Based on these challenges, this invention provides a papermaking wastewater treatment agent and its preparation method.

[0006] The purpose of this invention is to provide a method for preparing a papermaking wastewater treatment agent.

[0007] Another object of the present invention is to provide a papermaking wastewater treatment agent.

[0008] The above-mentioned objective of this invention is achieved through the following technical solution: A method for preparing a papermaking wastewater treatment agent, the specific preparation steps of which include: Prepolymer preparation: Acrylamide, cationic monomer, and hydrophobic monomer are dispersed in water, and then an initiator is added under an inert atmosphere. The mixture is reacted at a temperature of 40-50℃ for 1-3 hours to obtain a prepolymer. Polymerization reaction: An anionic monomer was added, and an initiator was added. The temperature was then raised to 55-60℃ and the reaction was continued for 2-3 hours. After naturally cooling to room temperature, acetone was added to precipitate the product. The product was then washed and dried to obtain a papermaking wastewater treatment agent. The molar ratio of the cationic monomer to the anionic monomer is 1.2-1.5:1, and the isoelectric point of the papermaking wastewater treatment agent is 4.5-5.5.

[0009] The beneficial effects of the above technical solution are as follows: The above technical solution uses acrylamide, cationic monomers, and hydrophobic monomers as raw materials in the prepolymerization stage. The cationic monomers fully participate in the polymerization, forming a cationic-rich prepolymer backbone. In the post-polymerization stage, anionic monomers are added, causing carboxyl groups to tend to be distributed in the terminal region of the polymer chain. Furthermore, by controlling the isoelectric point of the treatment agent product between 4.5 and 5.5, it matches the carboxyl dissociation characteristics of soluble lignin in papermaking wastewater. Thus, when the initial pH of the papermaking wastewater is approximately 5-7, which is higher than the isoelectric point of the treatment agent, the cationic groups in the treatment agent are fully dissociated and become positively charged, while the anionic carboxyl groups are essentially protonated and electrically neutral. The molecule as a whole exhibits a high cationic density polyelectrolyte, and its extended chain segments can efficiently neutralize the negative charge of soluble lignin. During this process, the negative charge of lignin is neutralized while releasing hydrogen ions, driving the pH of the system to decrease naturally. When the pH drops to near the isoelectric point, the carboxyl groups begin to deprotonate, the positive and negative charges of the molecule tend to be balanced, the chain segments change from an extended conformation to a contracted conformation, the hydrophobic chain segments are exposed and undergo intermolecular hydrophobic association, forming micro flocs with the ability to trap and sweep, which encapsulate and bridge the previously formed lignin-polyelectrolyte coagulation core, and finally form large flocs that can settle.

[0010] Furthermore, based on molar parts, the following raw materials are present in the following proportions: 75-80 parts acrylamide, 8-18 parts cationic monomer, 5-12 parts anionic monomer, and 0.5-2 parts hydrophobic monomer.

[0011] The beneficial effects of the above technical solution are as follows: Acrylamide, as the backbone monomer, constitutes the largest proportion, providing the polymer with sufficient molecular chain length to achieve bridging and flocculation. If the acrylamide dosage is too low, the molecular chain will be too short, resulting in insufficient flocculation and bridging capacity, small floc size, and slow settling velocity. The dosage of cationic monomers is limited to 8-18 parts to ensure sufficient positive charge density during the capture period to neutralize the negative charge of lignin. If the dosage is too low, the capture capacity will be insufficient, lignin cannot be effectively fixed, and subsequent flocculation will be interfered with by anions. If the dosage is too high, the polymer charge density will be too large, and the chain segments will extend excessively due to the repulsion of like charges, which is not conducive to hydrophobic association. The dosage of anionic monomers is limited to 5-12 parts to provide the carboxyl groups required for pH response. If the dosage is too low, the isoelectric point will be too high, and the response trigger pH will not match the lignin dissociation range. If the dosage is too high, the isoelectric point will be too low, and the carboxyl groups will have partially dissociated under the initial pH conditions of the wastewater, weakening the net cationic charge density during the capture period. The amount of hydrophobic monomer is limited to 0.5-2 parts to provide hydrophobic association driving force during the flocculation period; if the amount is too low, the hydrophobic association strength will be insufficient and the floc strength will be poor; if the amount is too high, the water solubility of the polymer will decrease, and it may even lead to phase separation in the prepolymerization stage.

[0012] Furthermore, the cationic monomer is selected from one or more of methacryloyloxyethyltrimethylammonium chloride, diallyldimethylammonium chloride, and acryloyloxyethyltrimethylammonium chloride.

[0013] Furthermore, the cationic monomer is a mixture of methacryloyloxyethyltrimethylammonium chloride and diallyldimethylammonium chloride, with a molar ratio of 3:1 to 1:1.

[0014] The beneficial effects of the above technical solution are as follows: Methacryloxyethyltrimethylammonium chloride provides a high density of positive charge, ensuring efficient neutralization of the negative charge of lignin, while the cyclic structure of diallyldimethylammonium chloride imparts rigidity to the polymer chain segments, allowing the molecular chains to maintain a more extended conformation under electrostatic repulsion during the capture period, increasing the probability of contact with lignin molecules; the two are compounded in a 3:1 to 1:1 ratio, which can achieve a balance between charge density and chain segment rigidity.

[0015] Furthermore, the hydrophobic monomer is selected from one or more of octyl acrylate, decyl acrylate, and dodecyl methacrylate.

[0016] Furthermore, the initiator is a redox initiation system; the initiator is composed of persulfate and sodium bisulfite in a molar ratio of 1:0.8 to 1:1.2.

[0017] Furthermore, the anionic monomer is selected from one or more of acrylic acid, methacrylic acid, and itaconic acid.

[0018] All of the above monomers contain carboxyl groups, and their dissociation constants (pKa) are in the range of 4-5, which matches the carboxyl dissociation characteristics of soluble lignin in papermaking wastewater. Acrylic acid has a pKa of approximately 4.25, methacrylic acid has a pKa of approximately 4.65, and itaconic acid contains two carboxyl groups, with pKas of 3.85 and 5.45, respectively. By selecting different types of anionic monomers, the isoelectric point of the treatment agent can be finely adjusted to fall within the target range of 4.5-5.5.

[0019] Furthermore, in the polymerization reaction step, the anionic monomer is added dropwise at a rate of 0.5-2 mL / min; and the anionic monomer is pre-neutralized with alkali to pH 6-7 before being added dropwise.

[0020] The dropping rate directly affects the sequence distribution of anionic units on the polymer chain. If the dropping rate is too fast, the local concentration of anionic monomers in the reaction system becomes excessively high, making it easy for acrylic monomers to homopolymerize or form block aggregates, resulting in uneven distribution of carboxyl groups within the chain segments and a steep, uncontrollable pH response. If the dropping rate is too slow, production efficiency is low, and anionic monomers may undergo side reactions due to prolonged exposure to high temperatures. A dropping rate of 0.5–2 mL / min allows anionic monomers to enter the reaction system at a controlled rate, ensuring sufficient contact with the active free radicals at the ends of the prepolymer chains and forming uniformly distributed carboxyl responsive units.

[0021] The pre-neutralization of anionic monomers to pH 6-7 with alkali before addition serves a dual purpose: firstly, unneutralized acrylic monomers possess a strong, pungent odor and are corrosive; neutralization improves operational safety. Secondly, partial neutralization causes the carboxyl groups to exist as sodium carboxylate, reducing the monomer's reactivity and preventing explosive polymerization due to exothermic reactions upon addition to the reaction system. The pH 6-7 neutralization deprotonates approximately 50-70% of the carboxyl groups, controlling reactivity while preserving sufficient polymerization capacity.

[0022] Furthermore, the amount of the supplementary initiator is 30-60% of the molar amount of the initiator used in the prepolymer preparation step; the supplementary initiator is added in two parts after the addition of the anionic monomer and before the temperature is raised to 55-60°C, the first addition being 50-70% of the total molar amount of the supplementary initiator, and the second addition being 30-50% of the total molar amount of the supplementary initiator.

[0023] The amount and timing of initiator addition determine the polymerization rate and molecular weight distribution in the post-polymerization stage. If all initiator is added at once, the free radical concentration increases sharply in the initial stage of the reaction, resulting in an excessively rapid polymerization rate. A large amount of anionic monomer is consumed in a short time, leading to block formation of carboxyl groups within the chain segments. Simultaneously, the molecular weight distribution widens, affecting the sensitivity of the pH response and the stability of the flocculation performance. Adding it in two stages allows for a relatively stable free radical concentration in the post-polymerization stage: the first addition of most of the initiator initiates the copolymerization reaction between the anionic monomer and the prepolymer chain ends; the second addition of a small amount of initiator maintains the free radical concentration in the later stages of the reaction, allowing for the full conversion of residual monomers and reducing the free monomer content in the product.

[0024] A papermaking wastewater treatment agent is prepared using the above-described preparation method. Detailed Implementation

[0025] The present invention will be further illustrated below with reference to specific embodiments, but the embodiments do not limit the present invention in any way. Unless otherwise specified, the reagents, methods, and equipment used in the present invention are conventional reagents, methods, and equipment in this technical field.

[0026] Unless otherwise specified, all reagents and materials used in the following examples are commercially available.

[0027] Example 1 This embodiment provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 78 parts acrylamide, 14 parts methacryloyloxyethyltrimethylammonium chloride (DMC), 1.0 part decyl acrylate, and 8 parts acrylic acid. Acrylamide, DMC, and decyl acrylate are used in the prepolymer preparation step, and acrylic acid is used in the polymerization reaction step.

[0028] (1) Preparation of prepolymer: Acrylamide, DMC, and decyl acrylate from the above proportions were added to a reaction flask, and deionized water was added to prepare a reaction solution with a total monomer mass fraction of 25%. Nitrogen gas was bubbled through the solution for 30 min to remove oxygen. Subsequently, a redox initiator composed of potassium persulfate and sodium bisulfite in a molar ratio of 1:1 (the total amount of initiator was 0.5% of the total molar amount of monomers) was added, and the reaction was carried out in a water bath at 45°C for 2 h with a stirring speed of 200 rpm to obtain a cationic prepolymer system. (2) Polymerization reaction: The acrylic acid in the above ratio was pre-neutralized to pH 6.5 with sodium hydroxide solution and added dropwise to the prepolymer system at a rate of 1.0 mL / min. After the addition was complete, the initiator (45% of the molar amount of the initiator in step (1)) was added in two parts: the first part was 60% of the total amount of initiator, and after stirring for 10 min, the remaining 40% was added. The temperature was then raised to 58°C and the reaction was continued for 2.5 h with a stirring rate of 150 rpm.

[0029] (3) Post-processing: After the reaction was completed, the mixture was allowed to cool naturally to room temperature. Excess acetone was added to precipitate the precipitate, which was then filtered, washed three times with acetone, and dried under vacuum at 55°C for 10 hours to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the agent obtained in this example was determined to be 5.0 by acid-base titration.

[0030] Example 2 This embodiment provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 80 parts acrylamide, 10 parts diallyl dimethyl ammonium chloride (DADMAC), 1.5 parts dodecyl methacrylate, and 10 parts methacrylic acid. Acrylamide, DADMAC, and dodecyl methacrylate are used in the prepolymer preparation step, and methacrylic acid is used in the polymerization reaction step.

[0031] (1) Preparation of prepolymer: Acrylamide, DADMAC, and dodecyl methacrylate from the above proportions were added to a reaction flask, and deionized water was added to prepare a reaction solution with a total monomer mass fraction of 20%. Nitrogen gas was bubbled through the solution for 30 min to remove oxygen. Subsequently, a redox initiator composed of ammonium persulfate and sodium bisulfite in a molar ratio of 1:1.2 (the total amount of initiator was 0.6% of the total molar amount of monomers) was added, and the reaction was carried out in a water bath at 50°C for 1.5 h with a stirring speed of 180 rpm to obtain the prepolymer system.

[0032] (2) Polymerization reaction: The methacrylic acid in the above ratio was pre-neutralized to pH 7.0 with sodium hydroxide solution and added dropwise to the prepolymer system at a rate of 0.8 mL / min. After the addition was complete, the initiator (50% of the molar amount of the initiator in step (1)) was added in two parts: the first part was 70% of the total amount of initiator, and after stirring for 10 min, the remaining 30% was added. Then the temperature was raised to 60°C and the reaction was continued for 2 h with a stirring rate of 120 rpm.

[0033] (3) Post-processing: After the reaction was completed, the mixture was allowed to cool naturally to room temperature. Excess acetone was added to precipitate the wastewater, which was then filtered, washed three times with acetone, and dried under vacuum at 60°C for 8 hours to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the agent obtained in this example was determined to be 4.8.

[0034] Example 3 This embodiment provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 76 parts acrylamide, 16 parts acryloyloxyethyltrimethylammonium chloride, 0.8 parts octyl acrylate, and 7 parts itaconic acid. Acrylamide, acryloyloxyethyltrimethylammonium chloride, and octyl acrylate are used in the prepolymer preparation step, while itaconic acid is used in the polymerization reaction step.

[0035] (1) Preparation of prepolymer: Acrylamide, acryloyloxyethyltrimethylammonium chloride, and octyl acrylate from the above proportions were added to a reaction flask, and deionized water was added to prepare a reaction solution with a total monomer mass fraction of 30%. Nitrogen gas was bubbled through the solution for 30 min to remove oxygen. Subsequently, a redox initiator composed of potassium persulfate and sodium bisulfite in a molar ratio of 1:0.9 (the total amount of initiator was 0.4% of the total molar amount of monomers) was added, and the reaction was carried out in a water bath at 42°C for 3 h with a stirring speed of 250 rpm to obtain the prepolymer system.

[0036] (2) Polymerization reaction: The itaconic acid in the above ratio was pre-neutralized to pH 6.0 with sodium hydroxide solution and added dropwise to the prepolymer system at a rate of 1.5 mL / min. After the addition was complete, the initiator (35% of the molar amount of the initiator in step (1)) was added in two parts: the first part was 55% of the total amount of initiator, and after stirring for 10 min, the remaining 45% was added. Then the temperature was raised to 55°C and the reaction was continued for 3 h with a stirring rate of 100 rpm.

[0037] (3) Post-processing: After the reaction was completed, the mixture was allowed to cool naturally to room temperature. Excess acetone was added to precipitate the wastewater, which was then filtered, washed three times with acetone, and dried under vacuum at 50°C for 12 hours to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the agent obtained in this example was determined to be 5.3.

[0038] Comparative Example 1 This comparative example provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 78 parts acrylamide, 14 parts methacryloyloxyethyltrimethylammonium chloride (DMC), and 8 parts acrylic acid. Acrylamide and DMC are used in the prepolymer preparation step, and acrylic acid is used in the polymerization reaction step. The difference from Example 1 is that the hydrophobic monomer decyl acrylate is not added.

[0039] (1) Preparation of prepolymer: Acrylamide and DMC from the above proportions were added to a reaction flask, and deionized water was added to prepare a reaction solution with a total monomer mass fraction of 25%. Nitrogen gas was bubbled through the solution for 30 minutes to remove oxygen. Subsequently, a redox initiator composed of potassium persulfate and sodium bisulfite in a molar ratio of 1:1 (the total amount of initiator was 0.5% of the total molar amount of monomers) was added, and the reaction was carried out in a water bath at 45°C for 2 hours with a stirring speed of 200 rpm to obtain the prepolymer system.

[0040] (2) Polymerization reaction: The acrylic acid in the above ratio was pre-neutralized to pH 6.5 with sodium hydroxide solution and added dropwise to the prepolymer system at a rate of 1.0 mL / min. After the addition was complete, the initiator (45% of the molar amount of the initiator in step (1)) was added in two parts: the first part was 60% of the total amount of initiator, and after stirring for 10 min, the remaining 40% was added. The temperature was then raised to 58°C and the reaction was continued for 2.5 h with a stirring rate of 150 rpm.

[0041] (3) Post-processing: After the reaction was completed, the mixture was allowed to cool naturally to room temperature. Excess acetone was added to precipitate the wastewater, which was then filtered, washed three times with acetone, and dried under vacuum at 55°C for 10 hours to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the agent obtained in this comparative example was determined to be 5.1.

[0042] Comparative Example 2 This comparative example provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 78 parts acrylamide, 14 parts methacryloyloxyethyltrimethylammonium chloride (DMC), 1.0 part decyl acrylate, and 8 parts acrylic acid. The difference from Example 1 is that a one-step polymerization method is used, meaning all monomers are added to the reaction system at once.

[0043] Acrylamide, DMC, decyl acrylate, and acrylic acid were added to a reaction flask in the above proportions. The acrylic acid was pre-neutralized to pH 6.5 with sodium hydroxide solution. Deionized water was added to prepare a reaction solution with a total monomer mass fraction of 25%, and nitrogen gas was bubbled through for 30 min to remove oxygen. Then, a redox initiator composed of potassium persulfate and sodium bisulfite in a molar ratio of 1:1 (the total amount of initiator was 0.5% of the total molar amount of monomers) was added, and the reaction was carried out in a water bath at 45°C for 2 h. The temperature was then raised to 58°C and the reaction was continued for 2.5 h with a stirring rate of 150 rpm. After the reaction was completed, the mixture was allowed to cool naturally to room temperature, and excess acetone was added to precipitate the wastewater. The precipitate was filtered, washed three times with acetone, and dried under vacuum at 55°C for 10 h to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the treatment agent obtained in this comparative example was determined to be 4.9.

[0044] Comparative Example 3 This comparative example provides a papermaking wastewater treatment agent. The amounts of each raw material, by molar parts, are as follows: 78 parts acrylamide, 8 parts methacryloyloxyethyltrimethylammonium chloride (DMC), 1.0 part decyl acrylate, and 10 parts acrylic acid. Acrylamide, DMC, and decyl acrylate are used in the prepolymer preparation step, and acrylic acid is used in the polymerization reaction step. The molar ratio of cationic monomer to anionic monomer is 8:10, or 0.8:1. The difference from Example 1 is that the amount of cationic monomer is lower than that of anionic monomer, and the molar ratio of cationic monomer to anionic monomer is not within the 1.2-1.5:1 range specified in this invention.

[0045] (1) Preparation of prepolymer: Acrylamide, DMC, and decyl acrylate from the above proportions were added to a reaction flask, and deionized water was added to prepare a reaction solution with a total monomer mass fraction of 25%. Nitrogen gas was bubbled through the solution for 30 minutes to remove oxygen. Subsequently, a redox initiator composed of potassium persulfate and sodium bisulfite in a molar ratio of 1:1 (the total amount of initiator was 0.5% of the total molar amount of monomers) was added, and the mixture was reacted in a water bath at 45°C for 2 hours with a stirring speed of 200 rpm to obtain the prepolymer system.

[0046] (2) Polymerization reaction: The acrylic acid in the above ratio was pre-neutralized to pH 6.5 with sodium hydroxide solution and added dropwise to the prepolymer system at a rate of 1.0 mL / min. After the addition was complete, the initiator (45% of the molar amount of the initiator in step (1)) was added in two parts: the first part was 60% of the total amount of initiator, and after stirring for 10 min, the remaining 40% was added. The temperature was then raised to 58°C and the reaction was continued for 2.5 h with a stirring rate of 150 rpm.

[0047] (3) Post-processing After the reaction was completed, the mixture was allowed to cool naturally to room temperature. Excess acetone was added to precipitate the wastewater, which was then filtered, washed three times with acetone, and dried under vacuum at 55°C for 10 hours to obtain a powdered papermaking wastewater treatment agent. The isoelectric point of the agent obtained in this comparative example was determined to be 3.8.

[0048] The performance of the products obtained in the examples and comparative examples was evaluated, and the specific evaluation methods and results are shown below; Flocculation performance test: Wastewater from the pulping workshop of a paper mill was collected. The initial pH was 6.5, the chemical oxygen demand (COD) was 2800 mg / L, the turbidity was 650 NTU, and the lignin content was 420 mg / L. The treatment agents obtained in Examples 1-3 and Comparative Examples 1-3 were added respectively, with a dosage of 80 mg / L for each. The mixture was first stirred rapidly at 250 rpm for 30 seconds, then stirred slowly at 60 rpm for 8 minutes. After standing for 10 minutes, the supernatant was collected to determine the turbidity removal rate and COD removal rate.

[0049] Zeta potential test: The change in zeta potential of the wastewater supernatant before and after treatment was measured using a zeta potential analyzer.

[0050] Floc settling velocity test: Record the time required for the floc to descend from the start of settling to the settling interface to 50% of the graduated cylinder, and calculate the settling velocity.

[0051] Table 1: Performance Evaluation Results As shown in the table, the treatment agents obtained in Examples 1-3 are significantly better than those in Comparative Examples 1-3 in terms of turbidity removal rate, COD removal rate, and floc settling speed. Comparative Example 1, due to the lack of hydrophobic monomers, lacks hydrophobic association driving force during the flocculation period, resulting in poor floc strength and slow settling speed. Comparative Example 2, due to the one-step polymerization, has randomly distributed cationic and anionic units on the polymer chain, failing to form an asymmetric structure of "cationic backbone - anionic end", and its functional switching between the capture and flocculation periods is insensitive. Comparative Example 3, due to insufficient cationic monomer dosage, has a low isoelectric point (3.8), and under the initial pH of 6.5 in the wastewater, the carboxyl groups have already dissociated in large quantities, resulting in insufficient net cationic charge density and a significant decrease in capture capacity.

[0052] The above embodiments are preferred embodiments of the present invention, but the embodiments of the present invention are not limited to the above embodiments. Any changes, modifications, substitutions, combinations, or simplifications made without departing from the spirit and principle of the present invention shall be considered equivalent substitutions and shall be included within the protection scope of the present invention.

Claims

1. A method for preparing a papermaking wastewater treatment agent, characterized by, The specific preparation steps include: Prepolymer preparation: Acrylamide, cationic monomer, and hydrophobic monomer are dispersed in water, and then an initiator is added under an inert atmosphere. The mixture is reacted at a temperature of 40-50℃ for 1-3 hours to obtain a prepolymer. Polymerization reaction: An anionic monomer was added, and an initiator was added. The temperature was then raised to 55-60℃ and the reaction was continued for 2-3 hours. After naturally cooling to room temperature, acetone was added to precipitate the product. The product was then washed and dried to obtain a papermaking wastewater treatment agent. The molar ratio of the cationic monomer to the anionic monomer is 1.2-1.5:1, and the isoelectric point of the papermaking wastewater treatment agent is 4.5-5.

5.

2. The method for preparing a papermaking wastewater treatment agent according to claim 1, characterized in that, The following raw materials are present in the following molar amounts: acrylamide 75-80 parts, cationic monomer 8-18 parts, anionic monomer 5-12 parts, and hydrophobic monomer 0.5-2 parts.

3. A method of preparing a papermaking effluent treatment agent according to any one of claims 1 or 2, characterized in that, The cationic monomer is selected from one or more of methacryloyloxyethyltrimethylammonium chloride, diallyldimethylammonium chloride, and acryloyloxyethyltrimethylammonium chloride.

4. The method of claim 3, wherein the papermaking wastewater treatment agent is prepared by adding the cationic polymer to the inorganic flocculant. The cationic monomer is a mixture of methacryloyloxyethyltrimethylammonium chloride and diallyldimethylammonium chloride in a molar ratio of 3:1 to 1:

1.

5. A method for preparing a papermaking wastewater treatment agent according to any one of claims 1 or 2, characterized in that, The hydrophobic monomer is selected from one or more of octyl acrylate, decyl acrylate, and dodecyl methacrylate.

6. A method for preparing a papermaking wastewater treatment agent according to any one of claims 1 or 2, characterized in that, The initiator is a redox initiation system; the initiator is composed of persulfate and sodium bisulfite in a molar ratio of 1:0.8 to 1:1.

2.

7. A method for preparing a papermaking wastewater treatment agent according to any one of claims 1 or 2, characterized in that, The anionic monomer is selected from one or more of acrylic acid, methacrylic acid, and itaconic acid.

8. The method for preparing a papermaking wastewater treatment agent according to claim 7, characterized in that, In the polymerization reaction step, the anionic monomer is added dropwise at a rate of 0.5-2 mL / min; and the anionic monomer is pre-neutralized with alkali to pH 6-7 before being added dropwise.

9. A method for preparing a papermaking wastewater treatment agent according to any one of claims 1 or 2, characterized in that, The amount of the supplementary initiator is 30-60% of the molar amount of the initiator used in the prepolymer preparation step; the supplementary initiator is added in two parts after the addition of the anionic monomer and before the temperature is raised to 55-60°C, the first addition being 50-70% of the total molar amount of the supplementary initiator, and the second addition being 30-50% of the total molar amount of the supplementary initiator.

10. A papermaking wastewater treatment agent, characterized in that, It is prepared by the preparation method according to any one of claims 1-9.