A precision tooling and method for preventing tinning of gold-plated Ω-wires.
By employing a multi-level blocking mechanism of micro-nano composite superhydrophobic tin barrier and flexible heat insulation block, the problem of solder crawling during the tinning process of gold-plated Ω wires is solved, achieving efficient anti-soldering effect and flexible adaptation, maintaining the flexibility of Ω wires, and improving assembly reliability.
Patent Information
- Application Number
- CN202611304634.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, during the tinning process of gold-plated Ω wires, the solder tends to climb vertically upwards along the lead wire, forming an arched solder climbing phenomenon. This causes the gold-plated Ω wire to lose its flexibility and elasticity, affecting the reliability of subsequent assembly. Furthermore, existing anti-solder climbing methods are either ineffective or have poor versatility.
A multi-level blocking mechanism combining micro-nano composite superhydrophobic tin barrier and flexible thermal insulation block is adopted. The molten solder is blocked from climbing by physical micro-groove structure and low surface energy coating, while the flexible contact body is used for thermal rapid cooling to form a chain blockage.
It effectively prevents solder bridging, adapts to different specifications of gold-plated Ω wires, maintains flexibility and elasticity, improves assembly reliability, and reduces processing costs.
Smart Images

Figure CN123108566A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of tinning technology for electronic component leads, and particularly to a precision tooling and method for preventing tinning creepage in gold-plated Ω-wires. Background Technology
[0002] In electronic assembly, gold-plated Ω leads typically require tinning before soldering to remove the embrittlement effect of the gold layer on the solder joint and improve solderability. However, due to capillary action and the excellent wetting properties of molten solder on the gold-plated leads, the solder tends to climb rapidly and vertically upwards along the leads during tinning, creating a visible "arched solder climb" phenomenon at the arched section of the lead. This solder climb causes the arched section of the gold-plated Ω lead to lose its flexibility and elasticity, severely affecting the reliability of subsequent assembly.
[0003] Existing anti-solder creep methods mainly include applying solder resist and setting physical baffles. However, solder resist is prone to decomposition and carbonization at the high temperatures of tinning, resulting in limited sustained solder resist effectiveness. Furthermore, manual application is time-consuming and inconsistent, leading to inconsistent solder resist results. Simple physical baffles rely on a single blocking principle, resulting in a low success rate. In addition, existing physical baffle fixtures are mostly designed with fixed dimensions, making it difficult to adapt to Ω-shaped wires with different arch heights and flat strip lengths, thus lacking versatility. For multi-sized workpieces with special geometries like gold-plated Ω-shaped wires, there is a lack of a systematic solution that provides a good, uniform, and sustained solder resist effect, and whose fixtures can be flexibly adjusted to meet various specifications.
[0004] The statements herein provide only background information in relation to this invention and do not necessarily constitute prior art. Summary of the Invention
[0005] The purpose of this invention is to provide a precision tooling and method for preventing tin-climbing of gold-plated Ω wires by tinning. This invention addresses the problems existing in the prior art by using a multi-level synergistic mechanism that combines physical morphology blocking, surface chemical tin repellency, and thermal rapid cooling to achieve efficient tin-climbing prevention and universal compatibility with gold-plated Ω wires of different specifications.
[0006] To achieve the above objectives, the present invention is implemented through the following technical solution: The first aspect of this invention provides a precision tooling for preventing tinning of gold-plated Ω wires, wherein the gold-plated Ω wire is a workpiece formed by arching gold-plated copper flat strips, having an arched section and lead-out sections located on both sides of the arched section, and the precision tooling includes: The base includes two opposing support blocks and a slide rail disposed between the two support blocks; The clamping mechanism comprises two clamping mechanisms slidably mounted to the slide rail and arranged opposite to each other; each clamping mechanism is provided with a clamping groove for clamping one side of the lead-out section, so that the arched section is located between the two clamping mechanisms; the clamping groove integrates a micro-nano composite superhydrophobic tin barrier on the side near the arched section, the micro-nano composite superhydrophobic tin barrier comprising a micro-trench structure and a low surface energy coating coated on the surface of the micro-trench structure; Two heat insulation blocks are slidably mounted to the slide rail and located between the two clamping mechanisms, each heat insulation block corresponding to one of the clamping mechanisms; each heat insulation block has a flexible contact body for fitting against the root position of the back side of the arched section when the clamping mechanism clamps the lead-out section.
[0007] Optionally, the microgroove structure is formed by laser etching.
[0008] Optionally, the low surface energy coating is a fluorosilane or fluorocarbon nano-coating, and after coating, the contact angle of the surface with molten solder is greater than 150° and the roll-off angle is less than 10°.
[0009] Optionally, the clamping groove is formed on the upper surface of the clamping mechanism, and its extending direction is parallel to the slide rail.
[0010] Optionally, the clamping mechanism further includes an elastic pressure plate that is elastically movable relative to one side wall of the clamping groove. The side of the elastic pressure plate opposite to the groove wall has an upwardly extending protrusion to hold the lead-out section between the protrusion and the groove wall.
[0011] Optionally, the precision tooling further includes a locking mechanism, with one locking mechanism provided for each clamping mechanism and each heat insulation block, the locking mechanism being used to lock the clamping mechanism and the heat insulation block to the slide rail.
[0012] Optionally, the heat insulation block includes a heat storage body and a flexible contact body disposed on the upper end of the heat storage body. The heat storage body is slidably mounted to the slide rail, and the bottom of the heat storage body is constructed with a heat dissipation fin structure.
[0013] Optionally, the flexible contact body is a flexible graphite thermal conductive film.
[0014] Optionally, the slide rail is constructed as two parallel cylindrical optical rods, and the clamping mechanism and the heat insulation block are provided with through holes for cooperating with the cylindrical optical rods.
[0015] A second aspect of the present invention provides a method for preventing tinning of gold-plated Ω-wires, used in a precision tooling as described in any of the first aspects above, comprising: The lead-out sections on both sides of the gold-plated Ω wire are fixed in the clamping groove, so that the arched section of the gold-plated Ω wire protrudes upward and is located between the two clamping mechanisms; the heat insulation block is moved so that the flexible contact body is pressed tightly against the root position of the back of the arched section. Tinning is applied to the ends of the lead-out sections on both sides of the gold-plated Ω wire; During the tinning process, the micro-nano composite superhydrophobic tin barrier forms a primary fluid barrier against the molten solder climbing upwards along the surface of the gold-plated Ω line; on both sides of the back of the arched section, the heat insulation block constructs a secondary passive thermal cutoff zone to physically block and force condense the molten solder that crosses the micro-nano composite superhydrophobic tin barrier.
[0016] This invention has at least the following technical effects: By using physical micro-grooves to block and chemically repel tin through micro-nano composite superhydrophobic tin barriers, combined with a heat-insulating block with flexible contacts to thermally cool and shut off the gold-plated Ω-wire at the root of the arched section, a chain of blocking-repelling-blocking-condensing tin is formed, effectively solving the problem of continuous tin climbing on a large surface of flat strip.
[0017] By using flexible materials to slide and adhere the insulation block to the root of the arched section, without a large rigid clamping force, deformation of the arched section can be effectively avoided.
[0018] By allowing both the clamping mechanism and the heat insulation block to slide independently along the slide rail, it can flexibly adapt to gold-plated Ω wires with different arch heights and flat strip lengths, and has the advantages of fewer parts, lower processing costs, and intuitive and efficient adjustment operation. Attached Figure Description
[0019] Figure 1 This is a schematic diagram of the structure of a precision tooling in an assembled state according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the structure at the contact point between the clamping mechanism and the gold-plated Ω wire according to an embodiment of the present invention; Figure 3 This is a schematic diagram of the structure at the contact point between the heat insulation block and the gold-plated Ω wire according to an embodiment of the present invention; Figure 4 This is a partial cross-sectional schematic diagram of the contact point between the clamping mechanism, the heat insulation block, and the gold-plated Ω line provided in an embodiment of the present invention.
[0020] Explanation of reference numerals in the attached figures: 10. Base; 11. Slide rail; 12. Support block; 20. Clamping mechanism; 21. Clamping groove; 22. Micro-nano composite superhydrophobic tin barrier; 221. Micro-groove structure; 222. Low surface energy coating; 23. Elastic pressure plate; 30. Gold-plated Ω wire; 31. Lead-out section; 32. Arched section; 40. Heat insulation block; 41. Flexible contact body; 42. Heat storage body; 50. Locking mechanism / locking screw. Detailed Implementation
[0021] The following detailed description, in conjunction with the accompanying drawings and specific embodiments, provides a more detailed explanation of the precision tooling and method for preventing solder creep in gold-plated Ω-wire tinning. The advantages and features of the present invention will become clearer from the following description. It should be noted that the drawings are in a very simplified form and use non-precise proportions, used only to facilitate and clearly illustrate the embodiments of the present invention. Please refer to the drawings to make the objectives, features, and advantages of the present invention more apparent and understandable. It should be understood that the structures, proportions, sizes, etc., depicted in the accompanying drawings are only for illustrative purposes to aid those skilled in the art and are not intended to limit the implementation conditions of the present invention. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in proportions, or adjustments to the size, without affecting the effects and objectives achieved by the present invention, should still fall within the scope of the technical content disclosed in the present invention.
[0022] like Figure 1-4 As shown, the first aspect of this embodiment provides a precision tooling for preventing tinning of gold-plated Ω-wires to prevent tinning. Referring to... Figure 4 The gold-plated Ω wire is a workpiece made of gold-plated copper flat strip after being arched, and it has an upwardly protruding arched section 32 and lead-out sections 31 located on both sides of the arched section 32.
[0023] refer to Figure 1 The precision tooling provided in this embodiment includes a base 10, clamping mechanisms 20, and heat insulation blocks 40. The base 10 includes two opposing support blocks 12 and a slide rail 11 positioned between the two support blocks 12. The two clamping mechanisms 20 are slidably mounted to the slide rail 11 and positioned opposite each other. Each clamping mechanism 20 has a clamping groove 21 for clamping the lead-out section 31 on one side of the gold-plated Ω wire 30, so that the arched section 32 of the gold-plated Ω wire 30 is located between the two clamping mechanisms 20. The two heat insulation blocks 40 are slidably mounted to the slide rail 11 and located between the two clamping mechanisms 20, with each heat insulation block 40 corresponding to one clamping mechanism 20.
[0024] Further, refer to Figure 2 and Figure 4 The clamping groove 21 has a micro / nano composite superhydrophobic tin barrier 22 integrated on its inner surface near the arched section 32. The micro / nano composite superhydrophobic tin barrier 22 includes a micro-trench structure 221 and a low surface energy coating 222 applied to the surface of the micro-trench structure 221. The micro / nano composite superhydrophobic tin barrier 22 is an independent block. Its working surface is formed, for example, by laser etching, periodic micro-trench structures 221.
[0025] In some embodiments, the low surface energy coating 222 on the surface of the micro-trench structure 221 is a fluorosilane or fluorocarbon nano-coating. After coating, the surface has a contact angle with molten solder greater than 150° and a roll-off angle less than 10°, exhibiting a super-solder-repellent state.
[0026] Specifically, refer to Figure 2 A clamping groove 21 is formed on the upper surface of the clamping mechanism 20, extending parallel to the slide rail 11. The clamping mechanism 20 also includes an elastic pressure plate 23, which is elastically movable relative to one side wall of the clamping groove 21, for example, by means of a spring connected to the inside of one side wall. The side of the elastic pressure plate 23 opposite to the wall has an upwardly extending protrusion to hold the lead-out section 31 between the protrusion and the wall. With this configuration, the area above the clamping groove 21 and the area above the end of the lead-out section 31 can be completely open, allowing the soldering iron to freely approach the lead-out section 31 from above for soldering operations. Furthermore, by using the elastic pressure plate 23 to gently clamp from the side without excessive rigid clamping force, damage to the plating can be avoided.
[0027] In this embodiment, the precision tooling also includes a locking mechanism 50. A locking mechanism 50 is provided for each clamping mechanism 20 and each heat insulation block 40, and the locking mechanism 50 is used to lock the clamping mechanism 20 and the heat insulation block 40 to the slide rail 11. Specifically, refer to... Figures 1 to 3 The locking mechanism 50 is, for example, a locking screw 50. Each clamping mechanism 20 and each heat insulation block 40 is provided with a locking screw 50 on both sides. The end of the locking screw 50 abuts against the surface of the slide rail 11. By tightening the locking screw 50, the position of the clamping mechanism 20 and the heat insulation block 40 can be locked.
[0028] In this embodiment, reference Figure 3 The heat insulation block 40 has a flexible composite structure, including a heat storage body 42 and a flexible contact body 41 disposed on the upper end of the heat storage body 42. The heat storage body 42 is slidably mounted to the slide rail 11. The bottom of the heat storage body 42 is constructed with a heat dissipation fin structure, and the heat storage body 42 has good thermal conductivity, for example, it is a copper block. The flexible contact body 41 is used to fit against the root position of the back side of the arched section 32 when the clamping mechanism 20 clamps the lead-out section 31.
[0029] In some embodiments, the flexible contact 41 is a flexible graphite thermal conductive film.
[0030] In some embodiments, the side of the flexible contact 41 facing the root of the arched segment 32 is constructed in an arc shape to better fit the arched segment 32.
[0031] In some embodiments, reference Figure 1The slide rail 11 is constructed as two parallel cylindrical guide rods, and the clamping mechanism 20 and the heat insulation block 40 have through holes for engaging with the cylindrical guide rods. Using a guide rod structure simplifies the structure and reduces costs. In an embodiment not shown in the figure, the slide rail 11 can also be constructed in other shapes.
[0032] Based on the aforementioned precision tooling, this embodiment also provides a method for preventing solder creep in gold-plated Ω-wire tinning, comprising: Based on the actual flat strip length and arch height of the gold-plated Ω wire 30, after sliding the two clamping mechanisms 20 along the slide rail 11 to a suitable distance, insert the lead-out sections 31 on both sides of the gold-plated Ω wire 30 into the clamping slots 21 respectively, and automatically press them together by the elastic pressure plate 23, so that the arched section 32 of the gold-plated Ω wire 30 protrudes upward and is located between the two clamping mechanisms 20. After clamping is completed, the locking screw 50 can be tightened to fix the position of the clamping mechanism 20.
[0033] Furthermore, the heat insulation block 40 can be moved along the slide rail 11 to the root area at both ends of the arched section 32, so that its flexible contact body 41 is tightly attached to the root position on the back of the arched section 32. It can naturally fit by relying on the flexibility of the flexible contact body 41 itself, and the locking screw 50 is tightened to fix the heat insulation block 40. After fixing is completed, the ends of the lead-out sections 31 on both sides of the gold-plated Ω wire 30 can be heated and tinned from above with a soldering iron.
[0034] During the tinning process, the molten solder will climb upward along the surface of the gold-plated Ω line 30. It will first encounter the micro-nano composite super-solder barrier 22, which will be effectively pinned and repelled by its micro-grooves and super-solder surface. The micro-nano composite super-solder barrier 22 can form a primary fluid barrier for the molten solder climbing upward along the surface of the gold-plated Ω line 30.
[0035] On both sides of the back of the arched section 32, a tiny amount of solder that might break through the primary fluid barrier will continue upwards and encounter a heat insulation block 40 with a flexible composite structure at the root of the arched section 32. The secondary passive thermal cutoff zone formed by the heat insulation block 40 physically blocks and forces the molten solder that has crossed the micro-nano composite super-solder barrier 22 to solidify. Specifically, this is physically blocked by the flexible contact body 41, while the highly thermally conductive heat storage body 42 rapidly absorbs the heat from the solder, causing it to instantly solidify and completely stop its ascent along the back of the arched section 32. After tinning and gold removal are complete, the locking screw 50 can be loosened, the clamping mechanism 20 and the heat insulation block 40 removed, and the workpiece taken off. The back of the arched section 32 is clean and free of solder residue.
[0036] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.
[0037] In the description of this invention, it should be understood that the terms "center," "height," "thickness," "upper," "lower," "vertical," "horizontal," "top," "bottom," "inner," "outer," "axial," "radial," and "circumferential," etc., indicating orientation or positional relationships, are based on the orientation or positional relationships shown in the accompanying drawings and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. In the description of this invention, unless otherwise stated, "a plurality of" means two or more.
[0038] In the description of this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0039] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0040] Although the present invention has been described in detail through the preferred embodiments above, it should be understood that the above description should not be considered as a limitation of the present invention. Various modifications and substitutions to the present invention will be apparent to those skilled in the art after reading the above description. Therefore, the scope of protection of the present invention should be defined by the appended claims.
Claims
1. A precision tooling for tinning and preventing tin creep of gold-plated Ω wire, wherein the gold-plated Ω wire is a workpiece formed by arching gold-plated copper flat strip, having an arched section and lead-out sections located on both sides of the arched section, characterized in that, The precision tooling includes: The base includes two opposing support blocks and a slide rail disposed between the two support blocks; The clamping mechanism comprises two clamping mechanisms slidably mounted to the slide rail and arranged opposite to each other; each clamping mechanism is provided with a clamping groove for clamping the lead-out section on one side, so that the arched section is located between the two clamping mechanisms; the clamping groove integrates a micro-nano composite superhydrophobic tin barrier on the side near the arched section, the micro-nano composite superhydrophobic tin barrier comprising a micro-trench structure and a low surface energy coating coated on the surface of the micro-trench structure; Two heat insulation blocks are slidably mounted to the slide rail and located between the two clamping mechanisms, each heat insulation block corresponding to one of the clamping mechanisms; each heat insulation block has a flexible contact body for fitting against the root position of the back side of the arched section when the clamping mechanism clamps the lead-out section.
2. The precision tooling according to claim 1, characterized in that, The micro-groove structure is formed by laser etching.
3. The precision tooling according to claim 1, characterized in that, The low surface energy coating is a fluorosilane or fluorocarbon nano-coating, and after coating, the contact angle of the surface with molten solder is greater than 150° and the roll-off angle is less than 10°.
4. The precision tooling according to claim 1, characterized in that, The clamping groove is formed on the upper surface of the clamping mechanism, and its extension direction is parallel to the slide rail.
5. The precision tooling according to claim 4, characterized in that, The clamping mechanism further includes an elastic pressure plate that is elastically movable relative to one side wall of the clamping groove. The side of the elastic pressure plate opposite to the groove wall has an upwardly extending protrusion to hold the lead-out section between the protrusion and the groove wall.
6. The precision tooling according to claim 1, characterized in that, It also includes a locking mechanism, with a locking mechanism provided for each of the clamping mechanisms and each of the heat insulation blocks, the locking mechanism being used to lock the clamping mechanism and the heat insulation block to the slide rail.
7. The precision tooling according to claim 1, characterized in that, The heat insulation block includes a heat storage body and a flexible contact body disposed on the upper end of the heat storage body. The heat storage body is slidably mounted to the slide rail, and the bottom of the heat storage body is constructed with a heat dissipation fin structure.
8. The precision tooling according to claim 1, characterized in that, The flexible contact body is a flexible graphite thermal conductive film.
9. The precision tooling according to claim 1, characterized in that, The slide rail is constructed as two parallel cylindrical optical rods, and the clamping mechanism and the heat insulation block are provided with through holes for cooperating with the cylindrical optical rods.
10. A method for tinning gold-plated Ω-wires to prevent tin creep, used in precision tooling as described in any one of claims 1-9, characterized in that, include: The lead-out sections on both sides of the gold-plated Ω wire are fixed in the clamping groove, so that the arched section of the gold-plated Ω wire protrudes upward and is located between the two clamping mechanisms; the heat insulation block is moved so that the flexible contact body is pressed tightly against the root position of the back of the arched section. Tinning is applied to the ends of the lead-out sections on both sides of the gold-plated Ω wire; During the tinning process, the micro-nano composite superhydrophobic tin barrier forms a primary fluid barrier against the molten solder climbing upwards along the surface of the gold-plated Ω line; on both sides of the back of the arched section, the heat insulation block constructs a secondary passive thermal cutoff zone to physically block and force condense the molten solder that crosses the micro-nano composite superhydrophobic tin barrier.