Fabrication process of a high-performance gallium nitride power device structure

By combining wet chemical cleaning and in-situ gas thermal annealing with conformal deposition of dielectric layers and multilayer passivation layers, the problems of chemical bond breakage and lattice defects in the recessed gate MIS-HEMT structure were solved, improving the current stability and reliability of gallium nitride power devices and extending their service life.

CN123124380APending Publication Date: 2026-11-17NANJING UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611401899.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing recessed gate MIS-HEMT structures are prone to introducing chemical bond breakage and lattice defects during dry etching of the barrier layer, leading to increased gate leakage current and higher interface state density. This severely affects the current collapse effect and reverse breakdown voltage of the device, reducing reliability and lifespan.

Method used

By combining wet chemical cleaning and in-situ gas thermal annealing, layer damage and lattice defects introduced by dry etching are repaired. Through conformal deposition of dielectric layers and multilayer passivation layers, an integrated gate field electrode and source field electrode are formed, optimizing the electric field distribution and realizing a high-performance gallium nitride power device structure.

Benefits of technology

This effectively reduces chemical bond breakage and lattice defects, lowers gate leakage current and interface state density, improves reverse breakdown voltage and reliability of the device, extends its lifespan, and enables the fabrication of high-performance gallium nitride power devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124380A_ABST
    Figure CN123124380A_ABST
Patent Text Reader

Abstract

This invention discloses a fabrication process for a high-performance gallium nitride power device structure, comprising the following steps: Step S1, providing an epitaxial substrate, and epitaxially growing a buffer layer, a channel layer, and a barrier layer sequentially from bottom to top on the epitaxial substrate; Step S2, depositing a first passivation layer on the upper surface of the barrier layer, defining a gate electrode opening region on the first passivation layer using patterning and etching processes, and etching the barrier layer downwards within the gate electrode opening region to form an inwardly recessed gate trench; Step S3, performing wet chemical cleaning on the epitaxial substrate exposing the gate trench to remove layer damage introduced by dry etching, followed by in-situ gas thermal annealing to repair lattice defects; Step S4, conformally depositing a dielectric layer on the upper surface of the first passivation layer and the inner wall of the gate trench as the gate dielectric layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor device manufacturing technology, and more specifically, to a fabrication process for a high-performance gallium nitride power device structure. Background Technology

[0002] Gallium nitride (GaN), as a third-generation wide-bandgap semiconductor material, has excellent physical properties such as high breakdown electric field, high saturated electron drift velocity, high thermal conductivity and low on-resistance, and has a very broad application prospect in the fields of high temperature, high frequency, high voltage and high power electronic devices.

[0003] In power electronics applications, to ensure safe system operation and simplify circuit design, power switching devices are typically required to be normally-off (enhancement-mode) devices. Traditional GaN HEMT devices, due to the ultra-high concentration of two-dimensional electron gas (2DEG) generated by the inherent polarization effect at the heterojunction interface, usually exhibit normally-on (depletion-mode) behavior. To achieve normally-off operation, current mainstream technologies include the use of recessed gate structures, p-type GaN gate structures, or fluorine ion implantation.

[0004] Among them, the recessed gate MIS-HEMT (metal-insulator-semiconductor high electron mobility transistor) structure blocks 2DEG by partially or completely etching away the barrier layer beneath the gate region, achieving forward blocking and increasing the threshold voltage. However, existing recessed gate processes, when dry etching the barrier layer, easily introduce a large number of chemical bond breaks and lattice defects on the channel surface, leading to increased gate leakage current and higher interface state density. This not only causes severe current collapse (increased dynamic on-resistance) but also limits the reverse breakdown voltage of the device, reducing its reliability and lifespan.

[0005] Therefore, providing a fabrication process for a high-performance gallium nitride power device structure is a problem that this invention urgently needs to solve. Summary of the Invention

[0006] To address the aforementioned technical problems, the purpose of this invention is to overcome the limitations of existing recessed gate MIS-HEMT (metal-insulator-semiconductor high electron mobility transistor) structures, which rely on partially or completely etching away the barrier layer beneath the gate region to block 2DEG, achieving forward blocking and increasing the threshold voltage. However, existing recessed gate processes, during dry etching of the barrier layer, easily introduce numerous chemical bond breaks and lattice defects onto the channel surface, leading to increased gate leakage current and interface state density. This not only causes severe current collapse (increased dynamic on-resistance) but also restricts the reverse breakdown voltage of the device, reducing its reliability and lifespan. Therefore, this invention provides a fabrication process for a high-performance gallium nitride power device structure.

[0007] To achieve the above objectives, the present invention provides a fabrication process for a high-performance gallium nitride power device structure, comprising the following steps: Step S1: Provide an epitaxial substrate, and epitaxially grow a buffer layer, a channel layer and a barrier layer sequentially from bottom to top on the epitaxial substrate; Step S2: Deposit a first passivation layer on the upper surface of the barrier layer, use patterning and etching processes to define the gate electrode opening region on the first passivation layer, and etch downwards within the gate electrode opening region to remove part of the barrier layer, forming an inwardly recessed gate trench. Step S3: Perform wet chemical cleaning on the exposed gate trenches to remove layer damage introduced by dry etching, followed by in-situ gas thermal annealing to repair lattice defects. Step S4: Conformally deposit a dielectric layer on the upper surface of the first passivation layer and the inner wall of the gate trench as the gate dielectric layer; Step S5: Deposit a first metal layer on the upper surface of the gate dielectric layer, and form a gate electrode on the first metal layer by patterned etching, wherein the gate electrode extends to opposite sides to form an integrated gate field electrode. Step S6: Deposit a second passivation layer on the upper surface of the first passivation layer; Step S7: In the second passivation layer, the gate dielectric layer and the first passivation layer, source contact holes and drain contact holes are respectively opened on both sides of the gate electrode by patterned etching, and the surface of the barrier layer is exposed. Step S8: Form source electrode and drain electrode in source contact hole and drain electrode contact hole respectively, and perform rapid thermal annealing to achieve alloyed ohmic contact with barrier layer. Step S9: Deposit a third passivation layer on the upper surface of the second passivation layer; Step S10: A source interconnect via is formed below the third passivation layer to expose the source electrode and the drain electrode, and a second metal layer is formed on the third passivation layer. The second metal layer is constructed as a source field electrode through a patterning process. The source field electrode is connected to the source electrode through the source interconnect via and extends towards the drain electrode, covering the gate electrode and the gate field electrode.

[0008] Preferably, the epitaxial substrate is a silicon substrate, a silicon carbide substrate, a sapphire substrate, or a gallium nitride single crystal substrate, and the buffer layer, channel layer, and barrier layer are all grown by metal-organic chemical vapor deposition or molecular beam epitaxy.

[0009] Preferably, in step S3, the reaction solution used in the wet chemical cleaning is an alkaline solution containing tetramethylammonium hydroxide, or an acidic mixed solution containing hydrochloric acid and hydrofluoric acid, used to remove the amorphous layer and oxide impurities remaining on the grid surface due to dry etching.

[0010] Preferably, in step S3, the in-situ gas thermal annealing treatment is carried out in an in-situ protective atmosphere by introducing high-purity ammonia, nitrogen, or a mixture thereof, and the defect repair of the exposed crystal surface inside the gate trench is achieved by thermally stimulating atomic migration.

[0011] Preferably, the first passivation layer, the second passivation layer, and the third passivation layer are all prepared by plasma-enhanced chemical vapor deposition or low-pressure chemical vapor deposition, and their materials independently include silicon nitride, silicon dioxide, or silicon oxynitride.

[0012] Preferably, in step S4, the gate dielectric layer is obtained by conformal growth through atomic layer deposition, and its material is one or more vertical composite layers selected from alumina, hafnium oxide, silicon dioxide, and yttrium oxide.

[0013] Preferably, in step S10, when the source field electrode extends toward the drain electrode, it is separated from the lower gate field electrode in the vertical direction by an insulating medium composed of the second passivation layer and the third passivation layer, so as to realize the two-dimensional electric field decoupling modulation of the electric field in the drift region inside the device.

[0014] According to the above technical solution, the beneficial effects of this invention compared to the prior art are as follows: This application overcomes the limitations of existing recessed gate MIS-HEMT (metal-insulator-semiconductor high electron mobility transistor) structures, which block 2DEG by partially or completely etching away the barrier layer beneath the gate region, thus achieving forward blocking and increasing the threshold voltage. However, existing recessed gate processes, during dry etching of the barrier layer, easily introduce a large number of chemical bond breaks and lattice defects on the channel surface, leading to increased gate leakage current and higher interface state density. This not only causes severe current collapse effects (increased dynamic on-resistance) but also restricts the reverse breakdown voltage of the device, reducing the reliability and lifespan of the device. Therefore, this invention provides a fabrication process for a high-performance gallium nitride power device structure.

[0015] Other features and advantages of the present invention will be described in detail in the following detailed description section; and all parts not covered in the present invention are the same as or can be implemented using the prior art. Attached Figure Description

[0016] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used together with the following detailed description to explain the invention, but do not constitute a limitation thereof. In the drawings: Figure 1 This is a cross-sectional view of a high-performance gallium nitride power device structure provided in a preferred embodiment of the present invention; Figure 2 This is a flowchart of the fabrication process of a high-performance gallium nitride power device structure provided in a preferred embodiment of the present invention.

[0017] Explanation of reference numerals in the attached figures: 1. Epitaxial substrate; 2. Buffer layer; 3. Channel layer; 4. Barrier layer; 5. First passivation layer; 6. Gate trench; 7. Gate dielectric layer; 8. First metal layer; 9. Gate electrode; 10. Gate field electrode; 11. Second passivation layer; 12. Source electrode; 13. Drain electrode; 14. Third passivation layer; 15. Source interconnect via; 16. Source field electrode. Detailed Implementation

[0018] The specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are for illustration and explanation only and are not intended to limit the present invention.

[0019] In the description of the embodiments of this invention, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," indicating orientation or positional relationships, are based on the orientation or positional relationships shown in the accompanying drawings, or the orientation or positional relationships commonly used when the product is in use. These are merely for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention. Furthermore, the terms "first," "second," and "third," etc., are only used for distinguishing descriptions and should not be construed as indicating or implying relative importance. Additionally, the terms "horizontal," "vertical," and "suspended," etc., do not indicate that the component is required to be absolutely horizontal or suspended, but can be slightly tilted. For example, "horizontal" simply means that its direction is more horizontal than "vertical," and does not mean that the structure must be completely horizontal, but can be slightly tilted.

[0020] In the description of the embodiments of the present invention, it should also be noted that, unless otherwise explicitly specified and limited, the terms "set," "install," "connect," and "link" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in the present invention according to the specific circumstances.

[0021] To further understand the features, technical means, and specific objectives and functions achieved by the present invention, the present invention will be described in further detail below with reference to the accompanying drawings and specific embodiments.

[0022] A fabrication process for a high-performance gallium nitride power device structure includes the following steps: Step S1: Provide an epitaxial substrate 1, and epitaxially grow a buffer layer 2, a channel layer 3 and a barrier layer 4 sequentially from bottom to top on the epitaxial substrate 1; Step S2: Deposit a first passivation layer 5 on the upper surface of the barrier layer 4, use patterning and etching processes to define the gate electrode 9 opening region on the first passivation layer 5, and etch down to remove part of the barrier layer 4 in the gate electrode 9 opening region to form an inwardly recessed gate trench 6. Step S3: Perform wet chemical cleaning on the exposed gate trench 6 to remove layer damage introduced by dry etching, and then perform in-situ gas thermal annealing to repair lattice defects. Step S4: Conformally deposit a dielectric layer on the upper surface of the first passivation layer 5 and the inner wall of the gate trench 6 as the gate dielectric layer 7; Step S5: Deposit a first metal layer 8 on the upper surface of the gate dielectric layer 7, and form a gate electrode 9 on the first metal layer 8 by patterned etching, wherein the gate electrode 9 extends to opposite sides to form an integrated gate field electrode 10. Step S6: Deposit a second passivation layer 11 on the upper surface of the first passivation layer 5; Step S7: In the second passivation layer 11, the gate dielectric layer 7 and the first passivation layer 5, source contact holes and drain contact holes are respectively opened on both sides of the gate electrode 9 by patterned etching, and the surface of the barrier layer 4 is exposed. Step S8: Form source electrode 12 and drain electrode 13 in source contact hole and drain electrode 13 contact hole respectively, and perform rapid thermal annealing to achieve alloyed ohmic contact with barrier layer 4. Step S9: Deposit a third passivation layer 14 on the upper surface of the second passivation layer 11; Step S10: A source interconnect via 15 is formed below the third passivation layer 14 to expose the source electrode 12 and the drain electrode 13, and a second metal layer is formed on the third passivation layer 14. The second metal layer is constructed as a source field electrode 16 through a patterning process. The source field electrode 16 is connected to the source electrode 12 through the source interconnect via 15, and the source field electrode 16 extends towards the drain electrode 13, covering the gate electrode 9 and the gate field electrode 10 above.

[0023] The epitaxial substrate 1 is a silicon substrate, a silicon carbide substrate, a sapphire substrate, or a gallium nitride single crystal substrate. The buffer layer 2, the channel layer 3, and the barrier layer 4 are all grown by metal-organic chemical vapor deposition or molecular beam epitaxy.

[0024] In step S3, the reaction solution used in the wet chemical cleaning is an alkaline solution containing tetramethylammonium hydroxide or an acidic mixed solution containing hydrochloric acid and hydrofluoric acid, used to remove the amorphous layer and oxide impurities remaining on the surface of the gate trench 6 due to dry etching.

[0025] In step S3, the in-situ gas thermal annealing process is carried out in an in-situ protective atmosphere by introducing high-purity ammonia, nitrogen, or a mixture thereof, and the defect repair of the exposed crystal surface inside the gate trench 6 is achieved by thermally stimulating atomic migration.

[0026] The first passivation layer 5, the second passivation layer 11, and the third passivation layer 14 are all prepared by plasma-enhanced chemical vapor deposition or low-pressure chemical vapor deposition processes, and their materials independently include silicon nitride, silicon dioxide, or silicon oxynitride.

[0027] In step S4, the gate dielectric layer 7 is obtained by conformal growth through atomic layer deposition, and its material is one or more vertical composite layers selected from alumina, hafnium oxide, silicon dioxide, and yttrium oxide.

[0028] In step S10, when the source field electrode 16 extends toward the drain electrode 13, it is separated from the lower gate field electrode 10 in the vertical direction by the insulating medium formed by the second passivation layer 11 and the third passivation layer 14, so as to realize the two-dimensional electric field decoupling modulation of the electric field in the drift region inside the device.

[0029] Step S1: The conductive core of the device is a heterojunction structure composed of an aluminum gallium nitride (AlGaN) barrier layer 4 and a gallium nitride (GaN) channel layer 3. Due to the spontaneous polarization and piezoelectric polarization effects of AlGaN and GaN materials, a layer of high-concentration, high-mobility two-dimensional electron gas (2DEG) is induced on the GaN side at the heterojunction interface, serving as a low-resistance conductive channel between the source and drain. The buffer layer 2 is used to alleviate the lattice mismatch and thermal mismatch between the substrate and GaN, and reduce the epitaxial defect density. The epitaxy adopts metal-organic chemical vapor deposition (MOCVD) or molecular beam epitaxy (MBE) processes, which can precisely control the film thickness and composition, ensuring the performance consistency of the 2DEG. The substrate supports a variety of choices, including silicon substrate, silicon carbide substrate, sapphire substrate, and gallium nitride single crystal substrate, which can flexibly adapt to different needs. Silicon substrate has low cost and large size, making it easy to mass-produce. Silicon carbide substrate has small GaN lattice mismatch and excellent thermal conductivity, making it suitable for high-frequency and high-power scenarios. Sapphire substrate has high process maturity.

[0030] Step S2: Traditional planar gallium nitride high electron mobility transistors are depletion-mode (normally on), with the channel naturally conducting at zero gate voltage, which does not meet the safety specifications of power systems. This process achieves normally-off characteristics through local trench etching. By dry etching, the AlGaN barrier layer 4 is thinned only in the gate electrode 9 region. The polarization effect in the under-gate region weakens as the barrier thickness decreases. At zero gate voltage, the 2DEG at the gate position is naturally depleted, and the device is in the off state by default, realizing the enhancement-mode operation. The non-gate region between the source and drain retains the complete thick barrier layer 4, maintaining high concentration of 2DEG and low on-resistance, achieving a balance between "normally-off safety" and "low conduction loss".

[0031] Step S3: During the dry etching process for fabricating gate trench 6, plasma bombardment introduces an amorphous damage layer, lattice defects, nitrogen vacancies, and surface oxide layer onto the surface of gate trench 6, significantly increasing the interface state density and causing threshold voltage drift and increased gate leakage current. This process precisely repairs these issues using a two-step method: Wet chemical cleaning: Alkaline tetramethylammonium hydroxide (TMAH) solution can selectively corrode the amorphous damage layer generated by dry etching (the corrosion rate of amorphous GaN is much higher than that of single crystal GaN), removing surface damage. The acidic mixture of hydrochloric acid and hydrofluoric acid can remove the surface oxide layer and metal residue impurities, cleaning the exposed crystal surface. In-situ gas thermal annealing: High-temperature annealing is carried out in a mixed atmosphere of high-purity ammonia and nitrogen. The thermal energy stimulates the migration of lattice atoms, repairing dislocations and point defects introduced by etching. The mixed atmosphere of ammonia and nitrogen can also replenish nitrogen vacancies on the surface of gate trench 6, further reducing the interface state density. The "in-situ" process can avoid secondary oxidation pollution during the transfer process after cleaning, ensuring interface cleanliness.

[0032] Step S4: The conformally deposited dielectric layer constitutes the MIS gate structure. Using atomic layer deposition (ALD) technology, through an atomic-level layer-by-layer growth mode of alternating precursor adsorption reactions, a thin film with uniform thickness can be grown at the bottom of the grooved gate, the vertical sidewalls, and the surface of the first passivation layer 5. This completely solves the problem of step coverage in the grooved structure, avoids local electric field concentration and premature breakdown caused by thin dielectric on the sidewalls or bottom, and ensures consistent insulation strength throughout the gate groove 6.

[0033] Step S5: The gate field electrode 10 (gate field plate) formed by extending the gate electrode 9 toward the drain electrode 13 is the first-stage electric field modulation structure. When the GaN device is turned off and subjected to high voltage, an extremely strong electric field concentration will appear at the edge of the gate electrode 9 near the drain electrode 13, which is a weak point for device breakdown. The gate field plate extends the equipotential surface of the gate electrode 9, disperses and flattens the peak electric field at the gate edge along the direction of the field plate, reduces the maximum electric field intensity, and directly improves the blocking voltage of the device. The gate field plate also covers part of the surface between the gate and drain, which can shield the influence of surface states on the channel and suppress the current collapse effect. Moreover, it is deposited in the same layer as the gate electrode 9 and patterned synchronously, without the need for additional photolithography steps, making the process simple.

[0034] Steps S6 and S9: The three passivation layers are fabricated using plasma-enhanced chemical vapor deposition (PECVD) or low-pressure chemical vapor deposition (LPCVD) processes. Each layer can be made of an independent material, such as silicon nitride, silicon dioxide, or silicon oxynitride, forming a complete protection and insulation system. First passivation layer 5: serves as a hard mask for etching the gate trench 6, while also protecting the surface of the barrier layer 4 in the non-gate region and reducing the surface state density. Second passivation layer 11: serves as an interlayer insulating medium between the gate plate metal and the source plate metal, ensuring electrical isolation between the two metal layers and also playing a surface passivation role. The third passivation layer 14 serves as the top passivation protection layer of the device, isolating it from external moisture, ions, and mechanical damage, thereby improving the long-term reliability of the device under complex environments such as high temperature and high humidity.

[0035] Steps S7 and S8: By etching contact holes to expose the surface of barrier layer 4, source and drain metals are deposited and then rapidly thermally annealed. The metals undergo an alloying reaction with AlGaN barrier layer 4 to form low-resistance ohmic contacts, reducing source and drain contact resistance and minimizing device conduction losses.

[0036] Step S10: The top-layer source field electrode 16 (source field plate) is at the same potential as the source electrode 12. It is electrically isolated from the lower gate field plate by a stacked insulating dielectric consisting of a second passivation layer 11 and a third passivation layer 14, forming a two-stage decoupled dual-field plate architecture. The gate field plate and the source field plate have independent potentials, independent dielectric thicknesses, and independent length dimensions, which can be optimized and designed separately without interfering with each other. Compared with a single-layer dielectric dual-field plate, it has a higher degree of design freedom and the electric field distribution can be optimized to be more uniform.

[0037] The preferred embodiments of the present invention have been described in detail above with reference to the accompanying drawings. However, the present invention is not limited to the specific details of the above embodiments. Within the scope of the technical concept of the present invention, various simple modifications can be made to the technical solution of the present invention, and these simple modifications all fall within the protection scope of the present invention.

[0038] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present invention will not describe the various possible combinations separately.

[0039] Furthermore, various different embodiments of the present invention can be combined in any way, as long as they do not violate the spirit of the present invention, they should also be regarded as the content disclosed by the present invention.

Claims

1. A fabrication process for a high-performance gallium nitride power device structure, characterized in that, Includes the following steps: Step S1: Provide an epitaxial substrate (1), and epitaxially grow a buffer layer (2), a channel layer (3) and a barrier layer (4) sequentially from bottom to top on the epitaxial substrate (1). Step S2: Deposit a first passivation layer (5) on the upper surface of the barrier layer (4), use patterning and etching processes to define the gate electrode (9) opening region on the first passivation layer (5), and etch down to remove part of the barrier layer (4) in the gate electrode (9) opening region to form an inwardly recessed gate trench (6). Step S3: Perform wet chemical cleaning on the exposed gate trench (6) to remove the layer damage introduced by dry etching, and then perform in-situ gas thermal annealing to repair lattice defects. Step S4: Conformally deposit a dielectric layer on the upper surface of the first passivation layer (5) and the inner wall of the gate trench (6) as the gate dielectric layer (7). Step S5: Deposit a first metal layer (8) on the upper surface of the gate dielectric layer (7), and form a gate electrode (9) above the first metal layer (8) by patterned etching, wherein the gate electrode (9) extends to opposite sides to form an integrated gate field electrode (10). Step S6: Deposit a second passivation layer (11) on the upper surface of the first passivation layer (5); Step S7: In the second passivation layer (11), the gate dielectric layer (7) and the first passivation layer (5), source contact holes and drain contact holes are respectively opened on both sides of the gate electrode (9) by patterned etching, and the surface of the barrier layer (4) is exposed. Step S8: Form source electrode (12) and drain electrode (13) in the source contact hole and drain electrode (13) contact hole respectively, and perform rapid thermal annealing to achieve alloyed ohmic contact with barrier layer (4); Step S9: Deposit a third passivation layer (14) on the upper surface of the second passivation layer (11). Step S10: A source interconnect via (15) is formed on and below the third passivation layer (14) to expose the source electrode (12) and the drain electrode (13). A second metal layer is formed on the third passivation layer (14). The second metal layer is constructed as a source field electrode (16) through a patterning process. The source field electrode (16) is connected to the source electrode (12) through the source interconnect via (15). The source field electrode (16) extends toward the drain electrode (13) and covers the gate electrode (9) and the gate field electrode (10).

2. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, The epitaxial substrate (1) is a silicon substrate, silicon carbide substrate, sapphire substrate or gallium nitride single crystal substrate, and the buffer layer (2), channel layer (3) and barrier layer (4) are all grown by metal-organic chemical vapor deposition or molecular beam epitaxy.

3. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, In step S3, the reaction solution used in wet chemical cleaning is an alkaline solution containing tetramethylammonium hydroxide or an acidic mixed solution containing hydrochloric acid and hydrofluoric acid, used to remove the amorphous layer and oxide impurities remaining on the surface of the gate trench (6) due to dry etching.

4. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, In step S3, the in-situ gas thermal annealing is carried out in an in-situ protective atmosphere by introducing high-purity ammonia, nitrogen or a mixture thereof, and the defect repair of the exposed crystal surface inside the gate trench (6) is achieved by thermally stimulating atomic migration.

5. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, The first passivation layer (5), the second passivation layer (11), and the third passivation layer (14) are all prepared by plasma-enhanced chemical vapor deposition or low-pressure chemical vapor deposition, and their materials independently include silicon nitride, silicon dioxide, or silicon oxynitride.

6. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, In step S4, the gate dielectric layer (7) is obtained by conformal growth through atomic layer deposition, and its material is one or more vertical composite stacks of alumina, hafnium oxide, silicon dioxide, and yttrium oxide.

7. The fabrication process of the high-performance gallium nitride power device structure according to claim 1, characterized in that, In step S10, when the source field electrode (16) extends toward the drain electrode (13), it is separated from the lower gate field electrode (10) in the vertical direction by an insulating medium composed of the second passivation layer (11) and the third passivation layer (14) to achieve two-dimensional electric field decoupling modulation of the electric field in the drift region inside the device.