Chips and their fabrication methods, packaging structures, and electronic devices
By using crystallized metal oxides as buffer and channel layers and controlling the uniformity of grain orientation, the short-channel effect and increased contact resistance of oxide semiconductor transistors are solved, thereby improving the stability and reliability of vertical transistors.
Patent Information
- Application Number
- CN202510637664.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-16
- Publication Date
- 2026-11-17
AI Technical Summary
The device performance and reliability of oxide semiconductor transistors are affected by the contact between the source/drain and the channel, leading to short-channel effect, increased contact resistance and poor thermal stability, especially when the problem is aggravated under high-temperature processes.
Crystallized metal oxides are used as the material for the first buffer layer and the channel layer. By controlling the grain orientation consistency, the contact resistance is reduced and the stability of the vertical transistor is improved.
It improves the switching characteristics and miniaturization potential of vertical transistors, reduces contact resistance, enhances thermal stability and reliability, and adapts to high-temperature process conditions.
Smart Images

Figure CN123124403A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the semiconductor field, and more particularly to a chip, its fabrication method, packaging structure, and electronic device. Background Technology
[0002] Oxide semiconductors (OS) are strong candidates for novel channel layer materials due to their advantages such as low leakage current (low power consumption), high mobility (large drive current), stable and adjustable threshold voltage, low-temperature deposition for easy integration, and low manufacturing cost.
[0003] Currently, the device performance and reliability of transistors using oxide semiconductors as the channel layer material are affected by the contact between the source / drain and the channel. Oxygen absorption from the source and drain introduces oxygen vacancies into the contact areas of the channel layer. These oxygen vacancies act as shallow donors in the oxide semiconductor, increasing the carrier concentration near the source and drain, thus shortening the effective length of the channel layer and exacerbating the short-channel effect, affecting the transistor's switching characteristics and miniaturization potential. Furthermore, oxygen absorption from the channel layer can form oxide layers between the source and channel layers, and between the drain and channel layers, increasing the contact resistance between the source and channel layers, and between the drain and channel layers, thereby affecting the transistor's thermal stability. High-temperature processes in subsequent manufacturing processes will further exacerbate these problems. Summary of the Invention
[0004] To address the aforementioned technical problems, this application provides a chip and its fabrication method, packaging structure, and electronic device, which can improve the switching characteristics and miniaturization potential of vertical transistors affected by the short-channel effect, and reduce the contact resistance between the first electrode and the channel layer, as well as the contact resistance between the second electrode and the channel layer.
[0005] In a first aspect, this application provides a chip including a substrate and a vertical transistor disposed on the substrate. The vertical transistor includes a first electrode, a first buffer layer, a channel layer, a second electrode, and a gate structure. The first electrode, the first buffer layer, the channel layer, and the second electrode are stacked along the direction from the substrate to the vertical transistor. The conductivity of the first buffer layer is greater than that of the channel layer. Both the first buffer layer and the channel layer are made of crystallized metal oxide. The gate structure is located on at least one side of the channel layer sidewall and includes a gate electrode and a gate dielectric for isolating the channel layer and the gate electrode.
[0006] In this application, due to the low conductivity of the channel layer and the limited number of oxygen vacancies, it is difficult to directly form a crystallized channel layer on the first electrode. However, the first buffer layer has higher conductivity and more oxygen vacancies. Within a certain range of oxygen vacancies, the abundance of oxygen vacancies can promote crystallization. Therefore, a crystallized first buffer layer can be directly formed on the first electrode, thereby achieving a first buffer layer material comprising a crystallized metal oxide. Those skilled in the art should understand that a crystallized channel layer can be grown on a crystallized material; therefore, a crystallized channel layer can be grown on the first buffer layer, achieving a channel layer material comprising a crystallized metal oxide.
[0007] Furthermore, crystallized metal oxides possess higher oxygen vacancy generation energy, meaning the energy required to form oxygen vacancies is relatively high, making it difficult to break the chemical bonds between the metal and oxygen in the metal oxide. As mentioned earlier, the channel layer in this application is a crystallized channel layer. Therefore, the chemical bonds between the metal and oxygen in the metal oxide within the channel layer are difficult to break, making it difficult for the first and second electrodes to absorb oxygen from the channel layer. This prevents the introduction of oxygen vacancies in the regions of the channel layer that contact the first and second electrodes, mitigating the problem of increased carrier concentration in the areas near the first and second electrodes in the channel layer. Consequently, this improves the short-channel effect and reduces its impact on the switching characteristics and miniaturization potential of vertical transistors. Based on this, the reduced short-channel effect can improve the variation in bond performance (e.g., threshold voltage) of vertical transistors, which is beneficial for the design of large-scale integrated circuits.
[0008] Furthermore, since the first and second electrodes are unlikely to absorb oxygen from the channel layer, and the crystallized first buffer layer is relatively stable, under certain conditions (such as high temperature conditions), the first electrode is unlikely to absorb oxygen from the first buffer layer and the channel layer, and the second electrode is unlikely to absorb oxygen from the channel layer. Consequently, oxide layers will not form between the first electrode and the channel layer, or between the second electrode and the channel layer. This avoids increasing the contact resistance between the first electrode and the channel layer, and between the second electrode and the channel layer due to the presence of oxide layers. At the same time, the thermal stability of the vertical transistor is improved, and even if the subsequent process involves high temperature processes, the aforementioned problems such as short-channel effect and increased contact resistance will be mitigated.
[0009] In some possible implementations, the vertical transistor further includes a second buffer layer disposed between the channel layer and the second electrode. The second buffer layer is made of a crystallized metal oxide and is a non-insulating material. The crystallized second buffer layer between the channel layer and the second electrode reduces the contact resistance between them, improves the high-temperature stability of the vertical transistor, and prevents oxygen from being extracted from the channel layer by the second electrode under high-temperature conditions.
[0010] In some other possible implementations, the second buffer layer disposed between the channel layer and the second electrode can also be an amorphous metal oxide, which can be used to reduce the contact resistance between the second buffer layer and the channel layer.
[0011] In some possible implementations, the dies in the first buffer layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis, and / or, the dies in the channel layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis; and / or, if the vertical transistor further includes a second buffer layer, the dies in the second buffer layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis.
[0012] Compared to crystallized channel layers where the grains are not oriented in a consistent manner on at least one of the a-axis, b-axis, or c-axis, using a metal oxide material with grains oriented in a consistent manner on at least one of the a-axis, b-axis, or c-axis as the channel layer material can further reduce the contact resistance between the channel layer and the first electrode, as well as between the channel layer and the second electrode. At the same time, it can further prevent the first and second electrodes from absorbing oxygen from the channel layer, improve the high-temperature stability and reliability of vertical transistors, and greatly enhance the miniaturization potential of vertical transistors and the design of large-scale integrated circuits.
[0013] Compared to a crystallized first buffer layer where the grains are not oriented in a consistent manner on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with grains oriented in a consistent manner on at least one of the a-axis, b-axis, or c-axis as the material of the first buffer layer can promote the growth of a crystallized channel layer on the first buffer layer. Moreover, the crystallized first buffer layer is relatively stable. Therefore, it is difficult for the first electrode to absorb oxygen from the first buffer layer and the channel layer, and thus an oxide layer will not form between the first electrode and the first buffer layer under certain conditions (e.g., under high temperature conditions), thereby further reducing the contact resistance between the first electrode and the channel layer.
[0014] Compared to crystallization, where the grains are not uniformly oriented on the a-axis, b-axis, or c-axis, a second buffer layer using a metal oxide with uniformly oriented grains on at least one of the a-axis, b-axis, or c-axis is used as the material for the second buffer layer. The second buffer layer is more stable, therefore, the second electrode is less likely to absorb oxygen from the second buffer layer and the channel layer, and thus will not form an oxide layer between the second electrode and the second buffer layer under certain conditions (e.g., high temperature conditions), thereby further reducing the contact resistance between the second electrode and the channel layer.
[0015] In some possible implementations, the material of the first buffer layer comprises a single-crystal metal oxide, and / or the material of the second buffer layer comprises a single-crystal metal oxide, and / or the material of the channel layer comprises a single-crystal metal oxide.
[0016] Compared to other crystallized metal oxides, using single-crystal metal oxides as the channel layer material can further reduce the contact resistance between the channel layer and the first electrode, as well as between the channel layer and the second electrode. At the same time, it can further prevent the first and second electrodes from absorbing oxygen from the channel layer, improve the high-temperature stability and reliability of vertical transistors, and greatly enhance the miniaturization potential of vertical transistors and the design of large-scale integrated circuits.
[0017] Compared to other crystallized metal oxides, using single-crystal metal oxides as the material for the first buffer layer can promote the growth of a crystallized channel layer on the first buffer layer. Moreover, the crystallized first buffer layer is relatively stable. Therefore, it is difficult for the first electrode to absorb oxygen from the first buffer layer and the channel layer, and thus an oxide layer will not form between the first electrode and the first buffer layer under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the first electrode and the channel layer.
[0018] Compared to other crystallized metal oxides, using single-crystal metal oxides as the material for the second buffer layer makes the second buffer layer more stable. Therefore, the second electrode is less likely to absorb oxygen from the second buffer layer and the channel layer, and thus will not form an oxide layer between the second electrode and the second buffer layer under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the second electrode and the channel layer.
[0019] In some possible implementations, the channel layer material also includes a polycrystalline metal oxide, and the channel layer comprises a single grain. There are multiple vertical transistors, and in these multiple vertical transistors, at least some of the grains in the channel layer have different orientations. The polycrystalline metal oxide containing a single grain is also a crystallized metal oxide; therefore, the beneficial effects of the channel layer 13 containing a single grain of polycrystalline metal oxide are the same as those of the channel layer containing a crystallized metal oxide, and will not be elaborated further here.
[0020] Furthermore, compared to using polycrystalline metal oxides as the channel layer material, using single-crystal metal oxides as the channel layer material can reduce grain boundary scattering, improve the carrier mobility of vertical transistors, and thus improve the reliability of vertical transistors, such as hot carrier injection effect and bias temperature instability.
[0021] In some possible implementations, the material of the first buffer layer includes at least one of indium and zinc; the total atomic percentage of indium and zinc in the material of the first buffer layer is greater than the total atomic percentage of indium and zinc in the material of the channel layer. The oxygen vacancies and conductivity of the first buffer layer can be improved by including a greater proportion of at least one of indium, zinc, or other elements in the metal oxide of the first buffer layer.
[0022] For example, the channel layer material includes at least one of indium gallium zinc oxide, indium gallium oxide, indium aluminum zinc oxide, and indium tin zinc oxide. And / or, the first buffer layer material includes at least one of indium tin oxide and indium gallium oxide. And / or, if the vertical transistor also includes a second buffer layer, the second buffer layer material includes at least one of indium gallium zinc oxide, indium gallium oxide, indium aluminum zinc oxide, indium tin zinc oxide, and indium tin oxide.
[0023] The material of the first buffer layer includes at least one of indium tin oxide and indium gallium oxide. The oxygen vacancies and conductivity of the first buffer layer can be improved by increasing the indium content in indium tin oxide and indium gallium oxide.
[0024] In some possible implementations, the chip further includes a first spacer layer and a second spacer layer. The first spacer layer is disposed between the gate structure and the first buffer layer, and the second spacer layer is disposed between the gate structure and the second electrode. The gate dielectric extends from between the gate and the channel layer, to between the gate and the first spacer layer, and to between the gate and the second spacer layer. The first spacer layer is used to electrically isolate the first electrode from the gate, and the second spacer layer is used to electrically isolate the second electrode from the gate.
[0025] In some possible implementations, the chip further includes a first spacer layer and a second spacer layer. The first spacer layer, the gate, and the second spacer layer are stacked along the direction from the substrate to the transistor, and the first spacer layer, the gate, and the second spacer layer are all disposed on the side of the gate dielectric away from the channel layer.
[0026] Based on this, the vertical transistor is either a ring-gate vertical transistor or a dual-gate vertical transistor. The gate dielectric is U-shaped and has an opening at the bottom. The channel layer includes a first channel layer and a second channel layer. The first channel layer fills the opening, and the second channel layer is located on the side of the first channel layer away from the first buffer layer. Specifically, along the direction from the gate to the channel layer, the size of the first channel layer is smaller than the size of the second channel layer, and the orthogonal projection of the first channel layer onto the second channel layer is centered.
[0027] Alternatively, the gate dielectric is plate-shaped and located on the sidewall of the second cutout, not extending along the surface parallel to the first buffer layer. The channel layer fills the area enclosed by the gate dielectric, or the channel layer fills the area enclosed by the gate dielectric, the first spacer layer, and the second spacer layer.
[0028] Compared to plate-shaped gate dielectrics, gate dielectrics with a concave shape and an opening at the bottom can save one mask during the fabrication process.
[0029] Secondly, this application provides a packaging structure, which includes a substrate and the chip described in the first aspect, with the chip disposed on the substrate.
[0030] The second aspect and any implementation thereof correspond to the first aspect and any implementation thereof, respectively. The technical effects of the second aspect and any implementation thereof are similar to those of the first aspect and any implementation thereof, and will not be repeated here.
[0031] Thirdly, this application provides an electronic device, which includes a circuit board and the packaging structure described in the second aspect. The packaging structure is disposed on the circuit board, and the substrate of the packaging structure is located between the chip and the circuit board.
[0032] The third aspect and any implementation thereof correspond to the first aspect and any implementation thereof, respectively. The technical effects of the third aspect and any implementation thereof are similar to those of the first aspect and any implementation thereof, and will not be repeated here.
[0033] Fourthly, this application provides a method for fabricating a chip, the chip including a vertical transistor. The method for fabricating the vertical transistor includes: forming a first electrode, a first buffer layer, a channel layer, and a gate structure on a substrate; stacking the first electrode, the first buffer layer, and the channel layer along the direction from the substrate to the vertical transistor, wherein the conductivity of the first buffer layer is greater than that of the channel layer; both the first buffer layer and the channel layer are made of crystallized metal oxide; the gate structure is located on at least one side of the sidewall of the channel layer, and the gate structure includes a gate electrode and a gate dielectric for isolating the channel layer and the gate electrode. A second electrode is formed on the side of the channel layer opposite to the substrate.
[0034] In some possible implementations, the chip further includes a first spacer layer and a second spacer layer. Forming a first electrode, a first buffer layer, a channel layer, and a gate structure on a substrate includes: sequentially forming a first electrode and a first buffer layer on the substrate; forming a first stacked structure on the side of the first buffer layer facing away from the substrate, the first stacked structure having a first cutout portion; along the direction from the substrate to the transistor, the first stacked structure includes a first spacer layer, a dummy gate, and a second spacer layer stacked together; filling the first cutout portion with a first sacrificial layer; the first sacrificial layer and the dummy gate have an etch selectivity ratio; removing the dummy gate, and forming a gate structure on the sidewall of the first sacrificial layer, the gate structure also being located between the first spacer layer and the second spacer layer; the gate dielectric extends from between the gate and the first sacrificial layer, to between the gate and the first spacer layer, and between the gate and the second spacer layer. Removing the first sacrificial layer, and filling the first cutout portion with a channel layer.
[0035] In some possible implementations, the chip further includes a first spacer layer and a second spacer layer. Forming a first electrode, a first buffer layer, a channel layer, and a gate structure on a substrate includes: sequentially forming the first electrode and the first buffer layer on the substrate; forming a second stacked structure on the side of the first buffer layer facing away from the substrate, the second stacked structure having a second cutout portion; along the direction from the substrate to the transistor, the second stacked structure includes a first spacer layer, a gate, and a second spacer layer stacked together. A gate dielectric and a channel layer are sequentially formed in the second cutout portion.
[0036] In some possible implementations, a gate dielectric and a channel layer are sequentially formed in the second cutout, including: sequentially forming an insulating layer and a second sacrificial layer in the second cutout; both the insulating layer and the second sacrificial layer extend from the side of the second spacer layer away from the substrate to the sidewall and bottom of the second cutout, with the portion of the second sacrificial layer in the second cutout forming a U-shape. The second sacrificial layer is partially removed to obtain a third sacrificial layer; the third sacrificial layer is located in the second cutout and is situated on the sidewall of the insulating layer. Under the protection of the third sacrificial layer, the insulating layer is partially removed to obtain the gate dielectric; the gate dielectric is U-shaped and has an opening at its bottom. The third sacrificial layer is removed. A channel layer is formed in the second cutout; the channel layer includes a first channel layer and a second channel layer, the first channel layer filling the opening, and the second channel layer located on the side of the first channel layer away from the first buffer layer. Wherein, along the direction from the gate to the channel layer, the size of the first channel layer is smaller than the size of the second channel layer, and the orthogonal projection of the first channel layer onto the second channel layer is centered.
[0037] The resulting gate dielectric is U-shaped with an opening at the bottom. The channel layer includes a first channel layer and a second channel layer, with the first channel layer filling the opening and the second channel layer located on the side of the first channel layer away from the first buffer layer. Specifically, along the direction from the gate to the channel layer, the size of the first channel layer is smaller than the size of the second channel layer, and the orthogonal projection of the first channel layer onto the second channel layer is centered.
[0038] In some possible implementations, a gate dielectric and a channel layer are sequentially formed in the second cutout, including: sequentially forming an insulating layer in the second cutout; the insulating layer extends from the side of the second spacer layer away from the substrate to the sidewall and bottom of the second cutout, and a portion of the insulating layer in the second cutout forms a U-shape. The insulating layer is partially removed to obtain the gate dielectric; the gate dielectric is located on the sidewall of the second cutout. The channel layer is then filled in the second cutout.
[0039] The resulting gate dielectric is plate-shaped and located on the sidewall of the second cutout, not extending along the surface parallel to the first buffer layer. The channel layer fills the area enclosed by the gate dielectric, or the channel layer fills the area enclosed by the gate dielectric, the first spacer layer, and the second spacer layer.
[0040] In some possible implementations, forming a first buffer layer includes: depositing the first buffer layer and subjecting the first buffer layer to high-temperature annealing; the high-temperature annealing temperature being greater than 300°C and less than 600°C; and / or forming a channel layer includes: depositing the channel layer and subjecting the channel layer to high-temperature annealing; the high-temperature annealing temperature being greater than 300°C and less than 600°C.
[0041] When removing excess material from the first buffer layer, the orientation of the first buffer layer may be disrupted. Therefore, after depositing the first buffer layer, it can be subjected to high-temperature annealing to promote crystallization of the first buffer layer and rearrange the disordered grains in the first buffer layer into ordered grains, thereby repairing defects.
[0042] After depositing the metal oxide layer of the channel layer, but before forming the pattern of the channel layer, the metal oxide layer of the channel layer can be subjected to high-temperature annealing; or, after forming the pattern of the channel layer, the metal oxide layer of the channel layer can be subjected to high-temperature annealing. This can promote the crystallization of the metal oxide layer of the channel layer, ensuring sufficient crystallization.
[0043] In related technologies, monocrystalline silicon is typically used as the channel layer material. However, the annealing temperature of monocrystalline silicon is usually high, for example, greater than or equal to 600°C. Therefore, even though the embodiments of this application perform high-temperature annealing on the first buffer layer and the channel layer, the high-temperature annealing temperature of this application is lower, which can mitigate the adverse effects of the high-temperature annealing process on the devices formed by the front-end processes.
[0044] In some possible implementations, after forming the first electrode, the first buffer layer, the channel layer, and the gate structure on the substrate, and before forming the second electrode on the side of the channel layer away from the substrate, the chip fabrication method further includes: forming a second buffer layer on the channel layer, wherein the material of the second buffer layer includes a crystallized metal oxide; wherein the material of the second buffer layer is a non-insulating material.
[0045] In some possible implementations, the dies in the first buffer layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis, and / or, the dies in the channel layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis; and / or, if the vertical transistor further includes a second buffer layer, the dies in the second buffer layer are oriented in a consistent manner on at least one of the a-axis, b-axis, and c-axis.
[0046] In some possible implementations, the material of the first buffer layer comprises a single-crystal metal oxide, and / or the material of the second buffer layer comprises a single-crystal metal oxide, and / or the material of the channel layer comprises a single-crystal metal oxide.
[0047] The fourth aspect and any implementation thereof correspond to the first aspect and any implementation thereof, respectively. The technical effects of the fourth aspect and any implementation thereof are similar to those of the first aspect and any implementation thereof, and will not be repeated here. Attached Figure Description
[0048] Figure 1 A schematic diagram of an electronic device provided in an embodiment of this application;
[0049] Figure 2a A schematic diagram of the structure of a vertical transistor provided for related technologies;
[0050] Figure 2b A schematic diagram of a vertical transistor forming an oxide layer, provided for related technologies;
[0051] Figures 3a-3c This is a schematic diagram of the chip structure provided in an embodiment of this application;
[0052] Figure 4a and Figure 4b This is a schematic diagram of the chip structure provided in an embodiment of this application;
[0053] Figure 5 This is a flowchart illustrating the fabrication process of the chip provided in an embodiment of this application.
[0054] Figures 6a-6h This is a diagram illustrating the chip fabrication process provided in an embodiment of this application.
[0055] Figure 7 This is a flowchart illustrating the fabrication process of the chip provided in an embodiment of this application.
[0056] Figure 8a and Figure 8b This is a diagram illustrating the chip fabrication process provided in an embodiment of this application.
[0057] Figures 9a-9d This is a diagram illustrating the chip fabrication process provided in an embodiment of this application.
[0058] Figures 10a-10c This is a diagram illustrating the fabrication process of the chip provided in an embodiment of this application. Detailed Implementation
[0059] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0060] In this article, the term "and / or" is merely a description of the relationship between related objects, indicating that there can be three relationships. For example, A and / or B can represent three situations: A exists alone, A and B exist simultaneously, and B exists alone.
[0061] The terms "first" and "second," etc., used in the specification and claims of this application are used to distinguish different objects, not to describe a specific order of objects. For example, "first target object" and "second target object," etc., are used to distinguish different target objects, not to describe a specific order of target objects.
[0062] In the embodiments of this application, the terms "exemplary" or "for example" are used to indicate that something is an example, illustration, or description. Any embodiment or design that is described as "exemplary" or "for example" in the embodiments of this application should not be construed as being more preferred or advantageous than other embodiments or design. Specifically, the use of the terms "exemplary" or "for example" is intended to present the relevant concepts in a specific manner.
[0063] In the description of the embodiments in this application, unless otherwise stated, "multiple" means two or more. For example, multiple processing units means two or more processing units; multiple systems means two or more systems.
[0064] This application provides an electronic device, which may be a consumer electronics product, a home electronics product, an automotive electronics product, a financial terminal product, a communication electronics product, or any other device containing a vertical transistor.
[0065] Consumer electronics include mobile phones, tablet computers, laptops, personal computers (PCs), personal digital assistants (PDAs), smart wearable products (e.g., smartwatches, smart bracelets), virtual reality (VR) terminal devices, augmented reality (AR) terminal devices, and drones. Home electronics include smart door locks, televisions, smart speakers, refrigerators, and robot vacuum cleaners. In-vehicle electronics include car navigation systems and in-vehicle displays. Financial terminal products include automated teller machines (ATMs) and self-service terminals. Communication electronics include servers, memory, radar, base stations, and other devices containing vertical transistors.
[0066] The electronic device includes a circuit board and a package structure disposed on the circuit board. The package structure includes a substrate and at least one chip. At least one chip is disposed on the substrate and electrically connected to the circuit board via traces in the substrate. This application does not limit the package structure; the package structure may include at least a portion of the functional modules in the electronic device to achieve at least some of the functions of each functional module.
[0067] Taking the memory module in an electronic device as an example, Figure 1 This application provides a schematic diagram of the structure of a memory in an electronic device. The memory may be, for example, a 3D dynamic random-access memory (3D DRAM), a resistive random-access memory (RRAM), a magnetic random-access memory (MRAM), a ferroelectric random-access memory (FeRAM), etc.
[0068] 3D DRAM is widely used in the memory of electronic devices. 3D DRAM increases storage density by effectively reducing the area of memory cells. 3D DRAM represents the next generation of DRAM technology. By replacing the planar transistors with oxide semiconductor vertical transistors (hereinafter referred to as vertical transistors), the chip area utilization can be improved, further increasing storage density. 3D DRAM also presents power consumption and heat dissipation issues. The ultra-low leakage current of vertical transistors can extend cell hold time and significantly reduce refresh power consumption.
[0069] like Figure 2a As shown, the vertical transistor includes a first electrode 11, a second electrode 12, a channel layer 13, a gate dielectric 14, and a gate electrode 15. The first electrode 11 is the source, and the second electrode 12 is the drain; or, the first electrode 11 is the drain, and the second electrode 12 is the source.
[0070] However, currently, the device performance and reliability of transistors (such as the aforementioned vertical transistors) are affected by the contact between the source / drain and the channel. The first electrode 11 and the second electrode 12 absorb oxygen from the channel layer 13, causing oxygen vacancies to be introduced into the region of the channel layer 13 that is in contact with the first electrode 11 and the second electrode 12. The oxygen vacancies formed in the oxide semiconductor will act as shallow donors, increasing the carrier concentration in the part of the oxide semiconductor located near the first electrode 11 and the second electrode 12, resulting in a shortening of the effective length of the channel layer 13, thereby exacerbating the short-channel effect and affecting the switching characteristics and miniaturization potential of the vertical transistor.
[0071] Specifically, the increased carrier concentration in the portion of the oxide semiconductor near the first electrode 11 and the second electrode 12 leads to a shortening of the effective length of the channel layer 13. This is because the increased carrier concentration in the portion of the oxide semiconductor (channel layer 13) near the first electrode 11 and the second electrode 12 improves the conductivity of this portion, thus shortening the effective semiconductor portion of the channel layer 13—a phenomenon known as the short-channel effect. The problems caused by the short-channel effect are: 1. Increased conductivity in the channel layer 13 makes it difficult to turn off the vertical transistor, affecting its switching characteristics; 2. Because the effective semiconductor portion of the channel layer 13 is shorter, the length of the channel layer 13 cannot be further shortened, affecting the miniaturization potential of the vertical transistor.
[0072] And, as Figure 2b As shown, after the first electrode 11 and the second electrode 12 absorb oxygen from the channel layer 13, an oxide layer 20 can be formed between the first electrode 11 and the channel layer 13, and between the second electrode 12 and the channel layer 13. This leads to an increase in the contact resistance between the first electrode 11 and the channel layer 13, and between the second electrode 12 and the channel layer 13, affecting the thermal stability of the vertical transistor. If the subsequent process involves high-temperature processes, the poor thermal stability of the vertical transistor will exacerbate the aforementioned short-channel effect and increased contact resistance problems.
[0073] Based on this, this application provides a chip, such as... Figures 3a-3c As shown, the chip includes a substrate 10 and a vertical transistor disposed on the substrate 10. The vertical transistor includes a first electrode, a first buffer layer, a channel layer, a second electrode, and a gate structure.
[0074] Along the direction perpendicular to the transistor from the substrate 10, a first electrode 11, a first buffer layer 31, a channel layer 13, and a second electrode 12 are stacked. The conductivity of the first buffer layer 31 is greater than that of the channel layer 13, and both the first buffer layer 31 and the channel layer 13 are made of crystallized metal oxide. A gate structure is located on at least one side of the sidewall of the channel layer 13, and the gate structure includes a gate 15 and a gate dielectric 14 for isolating the channel layer 13 and the gate 15.
[0075] It should be understood that, in order to fulfill the function of the vertical transistor, the channel layer 13 containing metal oxide is still a semiconductor. However, the embodiments of this application do not limit the first buffer layer 31, as long as its conductivity is greater than that of the channel layer 13. In this case, the first buffer layer 31 can be a semiconductor or a conductor.
[0076] In this application, because the channel layer 13 has low conductivity and few oxygen vacancies, it is difficult to directly form a crystallized channel layer 13 on the first electrode 11. However, the first buffer layer 31 has high conductivity and many oxygen vacancies. Within a certain range of oxygen vacancies, a large number of oxygen vacancies can promote crystallization. Therefore, a crystallized first buffer layer 31 can be directly formed on the first electrode 11, thereby achieving a material comprising a crystallized metal oxide. Those skilled in the art should understand that a crystallized channel layer 13 can be grown on a crystallized material; therefore, a crystallized channel layer 13 can be grown on the first buffer layer 31, achieving a material comprising a crystallized metal oxide.
[0077] Furthermore, crystallized metal oxides have a higher oxygen vacancy generation energy, meaning that the energy required to form oxygen vacancies is relatively high, making it difficult to break the chemical bonds between the metal and oxygen in the metal oxide. As mentioned earlier, the channel layer 13 in this application is a crystallized channel layer 13. Therefore, in the channel layer 13, the chemical bonds between the metal and oxygen in the metal oxide are difficult to break, and the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13. This prevents the introduction of oxygen vacancies in the regions of the channel layer 13 that are in contact with the first electrode 11 and the second electrode 12, thus mitigating the problem of increased carrier concentration in the portion of the channel layer 13 near the first electrode 11 and the second electrode 12. This improves the short-channel effect and reduces the impact of the short-channel effect on the switching characteristics and miniaturization potential of the vertical transistor. Based on this, since the short-channel effect is reduced, the variation in the bond performance (e.g., threshold voltage) of the vertical transistor can be improved, which is beneficial for the design of large-scale integrated circuits.
[0078] Furthermore, since the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13, and the crystallized first buffer layer 31 is relatively stable, under certain conditions (e.g., high temperature conditions), the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and the second electrode 12 is unlikely to absorb oxygen from the channel layer 13. Consequently, an oxide layer 20 will not form between the first electrode 11 and the channel layer 13, or between the second electrode 12 and the channel layer 13. This avoids increasing the contact resistance between the first electrode 11 and the channel layer 13, and between the second electrode 12 and the channel layer 13 due to the presence of the oxide layer 20. At the same time, the thermal stability of the vertical transistor is improved, and even if the subsequent process involves high temperature processes, the aforementioned problems such as short-channel effect and increased contact resistance will be improved.
[0079] In some possible implementations, the materials of the channel layer 13 and the first buffer layer 31 are not limited, as long as both the channel layer 13 and the first buffer layer 31 are metal oxides, and the conductivity of the channel layer 13 is less than that of the first buffer layer 31. Optionally, the metal oxide may include indium gallium zinc oxide (IGZO), indium gallium oxide (IGO), indium aluminum zinc oxide (IAZO), indium tin zinc oxide (ITZO), indium tin oxide (ITO), etc. The materials of the channel layer 13 and the first buffer layer 31 may be the same metal oxide, or they may be different metal oxides. For example, the material of the first buffer layer 31 may include at least one of ITO and IGO, and the material of the channel layer 13 may include at least one of IGZO, IGO, IAZO, and ITZO.
[0080] Optionally, the material of the channel layer 13 may include IGZO. Since IGZO has a relatively low deposition temperature, it is more compatible with the front end of line (FEOL) process, and vertical transistors are usually fabricated through the back end of line (BEOL) process. Therefore, using IGZO as the material of the channel layer 13 can improve the adverse effects on the performance of devices fabricated by the front end of the process due to the fabrication of vertical transistors.
[0081] In some possible implementations, the oxygen vacancies and conductivity of the first buffer layer 31 can be improved by including a greater proportion of at least one of elements such as indium (In) and zinc (Zn) in the metal oxide of the first buffer layer 31. Furthermore, the total atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the first buffer layer 31 is greater than the total atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the channel layer 13.
[0082] For example, if the metal oxides of the first buffer layer 31 and the channel layer 13 both contain indium (In) and zinc (Zn), then the total atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the first buffer layer 31 is greater than the total atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the channel layer 13.
[0083] For example, if the metal oxide of the first buffer layer 31 contains indium (In) and zinc (Zn), and the metal oxide of the channel layer 13 contains indium (In), then the total atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the first buffer layer 31 is greater than the atomic percentage of indium (In) in the metal oxide of the channel layer 13.
[0084] For example, if the metal oxide of the first buffer layer 31 contains indium (In), and the metal oxide of the channel layer 13 contains indium (In) and zinc (Zn), then the total atomic percentage of indium (In) in the metal oxide of the first buffer layer 31 is greater than the atomic percentage of indium (In) and zinc (Zn) in the metal oxide of the channel layer 13.
[0085] In some possible implementations, the gate structure is located on at least one side of the sidewall of the channel layer 13. For example, the gate structure is disposed on one side of the channel layer 13, and the vertical transistor is a single-gate vertical transistor; or, for another example, the gate structure is disposed on opposite sides of the channel layer 13, and the vertical transistor is a double-gate vertical transistor; or, for yet another example, the gate structure is disposed around the channel layer 13, and the vertical transistor is a ring-gate vertical transistor.
[0086] In some possible ways of implementation, such as Figure 3a and Figure 3b As shown, the chip also includes a first spacer layer 41 and a second spacer layer 42. Due to the different fabrication processes of vertical transistors, the positions of the first spacer layer 41 and the second spacer layer 42 relative to the gate structure are different.
[0087] like Figure 3a As shown, a first spacer layer 41 is disposed between the gate structure and the first buffer layer 31, and a second spacer layer 42 is disposed between the gate structure and the second electrode 12. The gate dielectric extends from between the gate electrode 15 and the channel layer 13, to between the gate electrode 15 and the first spacer layer 41, and to between the gate electrode 15 and the second spacer layer 42. The first spacer layer is used to electrically isolate the first electrode 11 from the gate electrode 15, and the second spacer layer is used to electrically isolate the second electrode 12 from the gate electrode 15.
[0088] Or, such as Figure 3b and Figure 3c As shown, along the direction of the substrate 10 pointing perpendicular to the transistor, the first spacer layer 41, the gate 15, and the second spacer layer 42 are stacked, and the first spacer layer 41, the gate 15, and the second spacer layer 42 are all disposed on the side of the gate dielectric 14 away from the channel layer 13.
[0089] Furthermore, the gate dielectric 14 and the channel layer 13 are fabricated using different processes, and their shapes are also different.
[0090] For example, such as Figure 3bAs shown, the vertical transistor is either a dual-gate vertical transistor or a ring-gate vertical transistor. The gate dielectric 14 is U-shaped and has an opening at its bottom. The channel layer 13 includes a first channel layer 131 and a second channel layer 132. The first channel layer 131 fills the opening, and the second channel layer 132 is located on the side of the first channel layer 131 opposite to the first buffer layer 21. Along the direction from the gate 15 to the channel layer 13, the size of the first channel layer 131 is smaller than the size of the second channel layer 132, and the orthogonal projection of the first channel layer 131 onto the second channel layer 132 is located at the center of the second channel layer 132.
[0091] For example, such as Figure 3c As shown, the gate dielectric 14 is plate-shaped and located on the sidewall of the second cutout portion, and does not extend along the surface parallel to the first buffer layer 31. The channel layer 13 fills the area enclosed by the gate dielectric 14, or the channel layer 13 fills the area enclosed by the gate dielectric 14, the first spacer layer 41, and the second spacer layer 42.
[0092] In some embodiments, such as Figure 4a and Figure 4b As shown, the vertical transistor also includes a second buffer layer 32, which is disposed between the channel layer 13 and the second electrode 12. The material of the second buffer layer 32 includes crystallized metal oxide, and the material of the second buffer layer 32 is a non-insulating material. The crystallized second buffer layer 32, disposed between the channel layer 13 and the second electrode 12, can reduce the contact resistance between the channel layer 13 and the second electrode 12, improve the high-temperature stability of the vertical transistor, and prevent the second electrode 12 from absorbing oxygen from the channel layer 13 under high-temperature conditions.
[0093] Optionally, the material of the second buffer layer 32 may include at least one of IGZO, IGO, IAZO, ITZO, and ITO.
[0094] In some other possible implementations, the second buffer layer 32 disposed between the channel layer 13 and the second electrode 12 can also be an amorphous metal oxide, which can be used to reduce the contact resistance between the second buffer layer 32 and the channel layer 13.
[0095] In some possible implementations, the crystallized first buffer layer 31 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, the crystallized channel layer 13 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, if the vertical transistor further includes a second buffer layer 32, the grains in the second buffer layer 32 have a consistent orientation along at least one of the a-axis, b-axis, and c-axis.
[0096] Crystal axes are straight lines that pass through the center of a crystal. These lines are used to determine the spatial position and orientation of crystal planes. The three crystal axes of a grain are the a-axis, b-axis, and c-axis. It should be understood that the a-axis, b-axis, and c-axis are not actual existing structures, but rather hypothetical straight lines.
[0097] For example, the material of the first buffer layer 31 is oriented in the same direction on the a-axis, the material of the first buffer layer 31 is also oriented in the same direction on the b-axis, the channel layer 13 is oriented in the same direction on the a-axis, and the material of the second buffer layer 32 is oriented in the same direction on the c-axis.
[0098] For example, the materials of the first buffer layer 31 are aligned on the b-axis, the channel layer 13 is aligned on the a-axis, and the materials of the second buffer layer 32 are aligned on the b-axis.
[0099] Compared to crystallization, where the grains are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with aligned grains on at least one of the a-axis, b-axis, or c-axis as the material of the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, and between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the miniaturization potential of the vertical transistor and the design of large-scale integrated circuits.
[0100] Compared to crystallization, where the grains of the first buffer layer 31 are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with grains aligned on at least one of the a-axis, b-axis, or c-axis as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (e.g., under high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0101] Compared to crystallization, but where the grains are not uniformly oriented on the a-axis, b-axis, or c-axis, the second buffer layer 32 is made of a metal oxide with uniformly oriented grains on at least one of the a-axis, b-axis, or c-axis. The second buffer layer 32 is more stable, so the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13. Consequently, under certain conditions (e.g., high temperature conditions), an oxide layer 20 will not form between the second electrode 12 and the second buffer layer 32, thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0102] Furthermore, the material of the first buffer layer 31 includes a single-crystal metal oxide, and / or the material of the second buffer layer 32 includes a single-crystal metal oxide, and / or the material of the channel layer 13 includes a single-crystal metal oxide. The single-crystal metal oxide has grains with consistent orientation along the a-axis, consistent orientation along the b-axis, and consistent orientation along the c-axis.
[0103] Compared to other crystallized metal oxides, using single-crystal metal oxides as the material for the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, as well as between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the potential for miniaturization of the vertical transistor and the design of large-scale integrated circuits.
[0104] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0105] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material for the second buffer layer 32 makes the second buffer layer 32 more stable. Therefore, the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13, and thus will not form an oxide layer 20 between the second electrode 12 and the second buffer layer 32 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0106] Furthermore, compared to using polycrystalline metal oxide as the material of the channel layer 13, using single-crystal metal oxide as the material of the channel layer 13 can reduce grain boundary scattering, improve the carrier mobility of the vertical transistor, and thus improve the reliability of the vertical transistor, such as hot carrier injection (HCI) and bias temperature instability (BTI).
[0107] In some embodiments, the channel layer 13 is further made of a polycrystalline metal oxide, and the channel layer 13 comprises a single grain. There can be multiple vertical transistors on the chip, and among the multiple vertical transistors, at least some of the grains in the channel layer 13 have different orientations. The polycrystalline metal oxide containing a single grain is also a crystallized metal oxide; therefore, the beneficial effects of the channel layer 13 containing a single grain of polycrystalline metal oxide are the same as those of the channel layer 13 containing a crystallized metal oxide, and will not be repeated here.
[0108] In another embodiment, this application also provides a method for fabricating a chip, the chip including vertical transistors, such as... Figure 5 As shown, the fabrication method of a vertical transistor includes:
[0109] S110, such as Figure 6a As shown, a first electrode 11 and a first buffer layer 31 are sequentially formed on the substrate 10, and the material of the first buffer layer 31 includes crystallized metal oxide.
[0110] In some possible implementations, removing the excess (dummy) portion of the first buffer layer 31 may disrupt its orientation. Therefore, after depositing the first buffer layer 31, it can be subjected to high-temperature annealing to promote crystallization and rearrange the disordered grains into ordered grains, thereby repairing defects. The high-temperature annealing temperature is greater than 300°C and less than 600°C.
[0111] In related technologies, monocrystalline silicon is typically used as the material for the channel layer 13. However, the annealing temperature of monocrystalline silicon is usually high, for example, greater than or equal to 600°C. Therefore, even though the first buffer layer 31 is subjected to high-temperature annealing in this application embodiment, the high-temperature annealing temperature in this application is lower, which can mitigate the adverse effects of the high-temperature annealing process on the devices formed by the previous process.
[0112] In some possible implementations, the substrate 10 may be routinely cleaned before the first electrode 11 and the first buffer layer 31 are sequentially formed on the substrate 10.
[0113] In some possible implementations, the material of the first electrode 11 is not limited in the embodiments of this application. Optionally, the material of the first electrode 11 may include metals such as tungsten.
[0114] S120, such as Figure 6b As shown, a first stacked structure is formed on the side of the first buffer layer 31 facing away from the substrate 10, and a first cutout is provided in the first stacked structure. Along the direction of the substrate 10 pointing to the vertical transistor, the first stacked structure includes a first spacer layer 41, a dummy gate 16, and a second spacer layer 42 stacked together.
[0115] In some possible implementations, the materials of the first spacer layer 41, the dummy gate 16, and the second spacer layer 42 are not limited, as long as the dummy gate 16 has an etch selectivity ratio with the first spacer layer 41 and with the second spacer layer 42.
[0116] Optionally, the first spacer layer 41 and the second spacer layer 42 are made of silicon oxide (SiOx), where x is a positive number. The dummy gate 16 is made of polysilicon (polySi).
[0117] In some possible ways of implementation, such as Figure 6b As shown, before creating the first cutout in the first stacked structure, a hard mask 51 can be formed on the first stacked structure to etch the first stacked structure under the protection of the hard mask 51, thereby creating the first cutout in the first stacked structure. Optionally, as... Figure 6b As shown, after forming the hard mask 51, silicon carbide (SiOC) 52 can be formed on the hard mask 51 to utilize the silicon carbide 52 as a buffer, preventing the hard mask 51 from generating stress on the vertical transistor and preventing damage to the hard mask 51 caused by the chemical mechanical polishing (CMP) process in step S130. Optionally, the material of the hard mask 51 may include silicon nitride (SiN).
[0118] In some possible implementations, fluorine can be used to etch the first stacked structure to create a first cutout in the first stacked structure. Compared to etching the first stacked structure with chlorine, etching the first stacked structure with fluorine can prevent the crystallized first buffer layer 31 from being damaged by the etching process.
[0119] If the crystallization of the first buffer layer 31 is affected by the process of opening the first hollow portion, the first buffer layer 31 can also be subjected to high-temperature annealing to promote the crystallization of the first buffer layer 31, rearrange the disordered grains in the first buffer layer 31 into ordered grains, thereby repairing the defects. The high-temperature annealing temperature is greater than 300℃ and less than 600℃.
[0120] S130, such as Figure 6c As shown, a first sacrificial layer 61 is filled in the first cutout portion, and the first sacrificial layer 61 has an etching selectivity ratio with the dummy gate 16. Filling the first cutout portion with the first sacrificial layer 61 first, instead of directly filling the channel layer 13 in the first cutout portion, can avoid damage to the channel layer 13 during the removal of the dummy gate 16 in step S140.
[0121] In some possible implementations, the material of the first sacrificial layer 61 is not limited in this application embodiment, as long as the first sacrificial layer 61 and the dummy gate 16 have an etch selectivity ratio. Optionally, the material of the first sacrificial layer 61 includes tungsten.
[0122] In some possible ways of implementation, such as Figure 6b and 6c As shown, during the process of forming the pattern of the first sacrificial layer 61, the first sacrificial layer 61 can be deposited first in the first cutout portion and on the side of the silicon carbide 52 facing away from the substrate 10. Then, the portion of the first sacrificial layer 61 located on the side of the silicon carbide 52 facing away from the substrate 10 is removed by CMP process. During this process, the surface of the silicon carbide 52 on the side facing away from the substrate 10 is also partially removed.
[0123] S140, such as Figures 6d-6f As shown, the dummy gate 16 is removed, and a gate structure is formed on the sidewall of the first sacrificial layer 61. The gate structure is also located between the first spacer layer 41 and the second spacer layer 42, and is located on at least one side of the sidewall of the first sacrificial layer 61. The gate structure includes a gate 15 and a gate dielectric 14, and the gate dielectric 14 extends from between the gate 15 and the first sacrificial layer 61, to between the gate 15 and the first spacer layer 41, and to between the gate 15 and the second spacer layer 42.
[0124] In some possible ways of implementation, such as Figure 6d As shown, after step S130 and before step S140, the method for fabricating a vertical transistor may further include: removing silicon dioxide 52.
[0125] In some possible implementations, a gate structure is formed on the sidewall of the first sacrificial layer 61, including: Figure 6e As shown, an insulating layer 141 and a conductive layer 151 are formed between adjacent first sacrificial layers 61, and the insulating layer 141 and the conductive layer 151 fill the region between adjacent first sacrificial layers 61. Next, as... Figure 6f As shown, the insulating layer 141 and the conductive layer 151 are partially removed. After the insulating layer 141 is partially removed, the gate dielectric 14 is obtained, and after the conductive layer 151 is partially removed, the gate 15 is obtained, so as to electrically isolate the gates 15 of adjacent vertical transistors.
[0126] Among some possible implementation methods, refer to Figure 6g After step S140 and before step S150, the method for fabricating vertical transistors further includes: removing the hard mask 51 and forming a dielectric layer 53 between adjacent vertical transistors.
[0127] S150, such as Figure 6g and Figure 6hAs shown, the first sacrificial layer 61 is removed, and the channel layer 13 is filled in the first hollow portion. The conductivity of the first buffer layer 31 is greater than that of the channel layer 13, and the material of the channel layer 13 includes crystallized metal oxide.
[0128] Thus, the first electrode 11, the first buffer layer 31, the channel layer 13, and the gate structure of the vertical transistor are formed on the substrate 10. The first electrode 11, the first buffer layer 31, and the channel layer 13 are stacked along the direction of the substrate 10 pointing to the vertical transistor.
[0129] Because the channel layer 13 has low conductivity and few oxygen vacancies, it is difficult to directly form a crystallized channel layer 13 on the first electrode 11. In contrast, the first buffer layer 31 has high conductivity and many oxygen vacancies. Within a certain range of oxygen vacancies, a large number of oxygen vacancies can promote crystallization. Therefore, a crystallized first buffer layer 31 can be directly formed on the first electrode 11, thereby achieving a material comprising a crystallized metal oxide. Those skilled in the art should understand that a crystallized channel layer 13 can be grown on a crystallized material; therefore, a crystallized channel layer 13 can be grown on the first buffer layer 31, achieving a material comprising a crystallized metal oxide.
[0130] In some possible implementations, to prevent the crystallization of the first buffer layer 31 from being affected by the process of removing the first sacrificial layer 61, the first buffer layer 31 may optionally be subjected to high-temperature annealing to promote the crystallization of the first buffer layer 31, rearranging the disordered grains in the first buffer layer 31 into ordered grains, thereby repairing defects. The high-temperature annealing temperature is greater than 300°C and less than 600°C.
[0131] In some possible implementations, after depositing the metal oxide of the channel layer 13 but before forming the pattern of the channel layer 13, the metal oxide of the channel layer 13 may be subjected to high-temperature annealing; or, after forming the pattern of the channel layer 13, the metal oxide of the channel layer 13 may be subjected to high-temperature annealing. This promotes the crystallization of the metal oxide of the channel layer 13, ensuring sufficient crystallization. The high-temperature annealing temperature is greater than 300°C and less than 600°C. The metal oxide of the channel layer 13 can be deposited using atomic layer deposition (ALD) technology.
[0132] In related technologies, monocrystalline silicon is typically used as the material for the channel layer 13. However, the annealing temperature of monocrystalline silicon is usually high, for example, greater than or equal to 600°C. Therefore, even though the channel layer 13 is subjected to high-temperature annealing in this application embodiment, the high-temperature annealing temperature in this application is lower, which can mitigate the adverse effects of the high-temperature annealing process on the devices formed by the previous process.
[0133] In some possible implementations, the materials of the channel layer 13 and the first buffer layer 31 are not limited, as long as both the channel layer 13 and the first buffer layer 31 are made of metal oxides, and the conductivity of the channel layer 13 is less than that of the first buffer layer 31. Optionally, the metal oxides may include IGZO, IGO, IAZO, ITZO, ITO, etc. The materials of the channel layer 13 and the first buffer layer 31 may be the same metal oxide, or they may be different metal oxides. For example, the material of the first buffer layer 31 may include at least one of ITO and IGO, and the material of the channel layer 13 may include at least one of IGZO, IGO, IAZO, and ITZO.
[0134] Optionally, the material of the channel layer 13 may include IGZO. Since IGZO has a relatively low deposition temperature, it is more compatible with the front-end process, and vertical transistors are usually fabricated through back-end processes. Therefore, using IGZO as the material of the channel layer 13 can improve the adverse effects on the performance of devices fabricated by the front-end process caused by the fabrication of vertical transistors.
[0135] S160, such as Figure 3a As shown, a second electrode 12 is formed on the side of the channel layer 13 away from the substrate 10.
[0136] In some possible ways of implementation, such as Figure 4a As shown, after step S150 and before step S160, the fabrication method of the vertical transistor further includes: forming a second buffer layer 32 on the side of the channel layer 13 facing away from the substrate 10. The material of the second buffer layer 32 includes crystallized metal oxide, and the material of the second buffer layer 32 is a non-insulating material. The crystallized second buffer layer 32 is disposed between the channel layer 13 and the second electrode 12, which can reduce the contact resistance between the channel layer 13 and the second electrode 12, improve the high-temperature stability of the vertical transistor, and prevent the second electrode 12 from absorbing oxygen from the channel layer 13 under high-temperature conditions.
[0137] In some other possible implementations, the second buffer layer 32 disposed between the channel layer 13 and the second electrode 12 can also be an amorphous metal oxide, which can be used to reduce the contact resistance between the second buffer layer 32 and the channel layer 13.
[0138] In some possible implementations, the crystallized first buffer layer 31 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, the crystallized channel layer 13 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, if the vertical transistor also includes a second buffer layer 32, the grains in the second buffer layer 32 have a consistent orientation along at least one of the a-axis, b-axis, and c-axis. For example, the material of the first buffer layer 31 has a consistent orientation along the a-axis, the material of the first buffer layer 31 also has a consistent orientation along the b-axis, the channel layer 13 has a consistent orientation along the a-axis, and the material of the second buffer layer 32 has a consistent orientation along the c-axis.
[0139] For example, the materials of the first buffer layer 31 are aligned on the b-axis, the channel layer 13 is aligned on the a-axis, and the materials of the second buffer layer 32 are aligned on the b-axis.
[0140] Compared to crystallization, where the grains are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with aligned grains on at least one of the a-axis, b-axis, or c-axis as the material of the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, and between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the miniaturization potential of the vertical transistor and the design of large-scale integrated circuits.
[0141] Compared to crystallization, where the grains of the first buffer layer 31 are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with grains aligned on at least one of the a-axis, b-axis, or c-axis as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (e.g., under high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0142] Compared to crystallization, but where the grains are not uniformly oriented on the a-axis, b-axis, or c-axis, the second buffer layer 32 is made of a metal oxide with uniformly oriented grains on at least one of the a-axis, b-axis, or c-axis. The second buffer layer 32 is more stable, so the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13. Consequently, under certain conditions (e.g., high temperature conditions), an oxide layer 20 will not form between the second electrode 12 and the second buffer layer 32, thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0143] Furthermore, the material of the first buffer layer 31 includes a single-crystal metal oxide, and / or the material of the second buffer layer 32 includes a single-crystal metal oxide, and / or the material of the channel layer 13 includes a single-crystal metal oxide. The single-crystal metal oxide has grains with consistent orientation along the a-axis, consistent orientation along the b-axis, and consistent orientation along the c-axis.
[0144] Compared to other crystallized metal oxides, using single-crystal metal oxides as the material for the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, as well as between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the potential for miniaturization of the vertical transistor and the design of large-scale integrated circuits.
[0145] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0146] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material for the second buffer layer 32 makes the second buffer layer 32 more stable. Therefore, the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13, and thus will not form an oxide layer 20 between the second electrode 12 and the second buffer layer 32 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0147] Furthermore, compared to using polycrystalline metal oxide as the material of the channel layer 13, using single-crystal metal oxide as the material of the channel layer 13 can reduce grain boundary scattering, improve the carrier mobility of the vertical transistor, and thus improve the reliability of the vertical transistor, such as the hot carrier injection effect and bias temperature instability.
[0148] In this application, since the channel layer 13 is made of crystallized metal oxide, and crystallized metal oxide has a higher oxygen vacancy generation energy (i.e., the energy required to form oxygen vacancies is relatively high), the chemical bonds between metal and oxygen in the metal oxide are difficult to break. As mentioned earlier, the channel layer 13 in this application is a crystallized channel layer. Therefore, the chemical bonds between metal and oxygen in the metal oxide in the channel layer 13 are difficult to break, and the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13. This prevents the introduction of oxygen vacancies in the region of the channel layer 13 that contacts the first electrode 11 and the second electrode 12, thus mitigating the problem of increased carrier concentration in the portion of the channel layer 13 near the first electrode 11 and the second electrode 12. This improves the short-channel effect and reduces the impact of the short-channel effect on the switching characteristics and miniaturization potential of the vertical transistor. Furthermore, because the short-channel effect is reduced, the variation in the bond performance (e.g., threshold voltage) of the vertical transistor can be improved, which is beneficial for the design of large-scale integrated circuits.
[0149] Furthermore, since the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13, and the crystallized first buffer layer 31 is relatively stable, under certain conditions (e.g., high temperature conditions), the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and the second electrode 12 is unlikely to absorb oxygen from the channel layer 13. Consequently, an oxide layer 20 will not form between the first electrode 11 and the channel layer 13, or between the second electrode 12 and the channel layer 13. This avoids increasing the contact resistance between the first electrode 11 and the channel layer 13, and between the second electrode 12 and the channel layer 13 due to the presence of the oxide layer 20. At the same time, it improves the thermal stability of the vertical transistor. Even if the subsequent process involves high temperature processes, the aforementioned problems such as short-channel effect and increased contact resistance will be improved.
[0150] Furthermore, the other explanations and beneficial effects of the embodiments of this application are the same as those of the previous embodiment, and will not be repeated here.
[0151] In another embodiment, this application also provides a method for fabricating a chip, the chip including vertical transistors, such as... Figure 7 As shown, the fabrication method of a vertical transistor includes:
[0152] S210, such as Figure 8a As shown, a first electrode 11 and a first buffer layer 31 are sequentially formed on the substrate 10, and the material of the first buffer layer 31 includes crystallized metal oxide.
[0153] In some possible implementations, removing excess portions of the first buffer layer 31 may disrupt its orientation. Therefore, after depositing the first buffer layer 31, it can be subjected to high-temperature annealing to promote crystallization and rearrange the disordered grains into ordered grains, thereby repairing defects. The high-temperature annealing temperature is greater than 300°C and less than 600°C.
[0154] In some possible implementations, the substrate 10 may be routinely cleaned before the first electrode 11 and the first buffer layer 31 are sequentially formed on the substrate 10.
[0155] In some possible implementations, the material of the first electrode 11 is not limited in the embodiments of this application. Optionally, the material of the first electrode 11 may include metals such as tungsten.
[0156] S220, such as Figure 8b As shown, a second stacked structure is formed on the side of the first buffer layer 31 away from the substrate 10, and a second cutout is provided in the second stacked structure. Along the direction of the substrate 10 pointing perpendicular to the transistor, the second stacked structure includes a first spacer layer 41, a gate 15, and a second spacer layer 42 stacked together.
[0157] In some possible implementations, the materials of the first spacer layer 41, the gate 15, and the second spacer layer 42 are not limited. Optionally, the materials of the first spacer layer 41 and the second spacer layer 42 include silicon oxide (SiOx), where x is a positive number. The material of the gate 15 includes metals such as tungsten.
[0158] In some possible implementations, fluorine can be used to etch the second stacked structure to create a second cutout within it. Compared to etching the second stacked structure with chlorine, etching with fluorine can prevent the crystallized first buffer layer 31 from being damaged by the etching process.
[0159] If the crystallization of the first buffer layer 31 is affected by the process of opening the second hollow portion, the first buffer layer 31 can also be subjected to high-temperature annealing to promote the crystallization of the first buffer layer 31, rearrange the disordered grains in the first buffer layer 31 into ordered grains, thereby repairing the defects. The high-temperature annealing temperature is greater than 300℃ and less than 600℃.
[0160] S230, a gate dielectric 14 and a channel layer 13 are sequentially formed in the second cutout. The conductivity of the first buffer layer 31 is greater than that of the channel layer 13, and the material of the channel layer 13 includes crystallized metal oxide.
[0161] Thus, the first electrode 11, the first buffer layer 31, the channel layer 13, and the gate structure of the vertical transistor are formed on the substrate 10. The first electrode 11, the first buffer layer 31, and the channel layer 13 are stacked along the direction of the substrate 10 pointing to the vertical transistor.
[0162] Specifically, different methods can be used to sequentially form the grid medium 14 and the channel layer 13 in the second hollow section.
[0163] The first method, such as Figure 9a As shown, an insulating layer 141 and a second sacrificial layer 62 are sequentially formed in the second hollow portion. Both the insulating layer 141 and the second sacrificial layer 62 extend from the side of the second spacer layer 42 away from the substrate 10 to the sidewall and bottom of the second hollow portion. The portion of the second sacrificial layer 62 in the second hollow portion forms a U-shape.
[0164] In some possible implementations, an insulating layer 141 and a second sacrificial layer 62 can be deposited using an ALD process. For example, the second sacrificial layer 62 is a 10 nm thick IGZO.
[0165] like Figure 9b As shown, the second sacrificial layer 62 is partially removed to obtain the third sacrificial layer 63. The third sacrificial layer 63 is located in the second hollow portion and is located on the side wall of the insulating layer 141.
[0166] like Figure 9b As shown, under the protection of the third sacrificial layer 63, the insulating layer 141 is partially removed to obtain the gate dielectric 14. The gate dielectric 14 is U-shaped and has an opening at the bottom.
[0167] In some possible implementations, to prevent the crystallization of the first buffer layer 31 from being affected by the fabrication process of the gate dielectric 14, the first buffer layer 31 may optionally be subjected to high-temperature annealing to promote crystallization and rearrange the disordered grains in the first buffer layer 31 into ordered grains, thereby repairing defects. The high-temperature annealing temperature is greater than 300°C and less than 600°C.
[0168] like Figure 9c As shown, the third sacrificial layer 63 is removed.
[0169] like Figure 9d As shown, a channel layer 13 is formed in the second cutout portion. The channel layer includes a first channel layer 131 and a second channel layer 132. The first channel layer 131 fills the opening, and the second channel layer 132 is located on the side of the first channel layer 131 away from the first buffer layer 31. Specifically, along the direction from the gate 15 to the channel layer 13, the size of the first channel layer 131 is smaller than the size of the second channel layer 132, and the orthogonal projection of the first channel layer 131 onto the second channel layer 132 is centered.
[0170] In some possible implementations, after depositing the metal oxide of the channel layer 13 but before forming the pattern of the channel layer 13, the metal oxide of the channel layer 13 may be subjected to high-temperature annealing; or, after forming the pattern of the channel layer 13, the metal oxide of the channel layer 13 may be subjected to high-temperature annealing. This promotes the crystallization of the metal oxide of the channel layer 13, ensuring sufficient crystallization. The high-temperature annealing temperature is greater than 300°C and less than 600°C. The metal oxide of the channel layer 13 can be deposited using an ALD process.
[0171] The second method, such as Figure 10a As shown, an insulating layer 141 is formed sequentially in the second cutout portion. The insulating layer 141 extends from the side of the second spacer layer 42 away from the substrate 10 to the sidewall and bottom of the second cutout portion. The portion of the insulating layer 141 in the second cutout portion forms a U-shape.
[0172] like Figure 10b As shown, the insulating layer 141 is partially removed to obtain the gate dielectric 14, which is located on the sidewall of the second cutout portion.
[0173] In some possible implementations, to prevent the crystallization of the first buffer layer 31 from being affected by the fabrication process of the gate dielectric 14, the first buffer layer 31 may optionally be subjected to high-temperature annealing to promote crystallization and rearrange the disordered grains in the first buffer layer 31 into ordered grains, thereby repairing defects. The high-temperature annealing temperature is greater than 300°C and less than 600°C.
[0174] like Figure 10c As shown, the second hollow section is filled with a channel layer 13.
[0175] Compared to Figures 10a-10b The proposed solution Figures 9a-9d The scheme shown can use the second sacrificial layer 62 and the third sacrificial layer 62 as protective layers to form the pattern of the gate medium 14, thereby saving one mask.
[0176] S240, such as Figure 3b and Figure 3c As shown, a second electrode 12 is formed on the side of the channel layer 13 away from the substrate 10.
[0177] In some possible ways of implementation, such as Figure 4bAs shown, after step S150 and before step S160, the fabrication method of the vertical transistor further includes: forming a second buffer layer 32 on the side of the channel layer 13 facing away from the substrate 10. The material of the second buffer layer 32 includes a crystalline metal oxide, and the material of the second buffer layer 32 is a non-insulating material. Compared with amorphous metal oxide, the second buffer layer 32 containing crystalline metal oxide has a smaller contact resistance. Therefore, by placing the second buffer layer 32 between the channel layer 13 and the second electrode 12, the contact resistance between the channel layer 13 and the second electrode 12 can be reduced, thereby improving the high-temperature stability of the vertical transistor.
[0178] In some possible implementations, the crystallized first buffer layer 31 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, the crystallized channel layer 13 may be characterized by the grains having a consistent orientation along at least one of the a-axis, b-axis, and c-axis. And / or, if the vertical transistor also includes a second buffer layer 32, the grains in the second buffer layer 32 have a consistent orientation along at least one of the a-axis, b-axis, and c-axis. For example, the material of the first buffer layer 31 has a consistent orientation along the a-axis, the material of the first buffer layer 31 also has a consistent orientation along the b-axis, the channel layer 13 has a consistent orientation along the a-axis, and the material of the second buffer layer 32 has a consistent orientation along the c-axis.
[0179] For example, the materials of the first buffer layer 31 are aligned on the b-axis, the channel layer 13 is aligned on the a-axis, and the materials of the second buffer layer 32 are aligned on the b-axis.
[0180] Compared to crystallization, where the grains are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with aligned grains on at least one of the a-axis, b-axis, or c-axis as the material of the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, and between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the miniaturization potential of the vertical transistor and the design of large-scale integrated circuits.
[0181] Compared to crystallization, where the grains of the first buffer layer 31 are not aligned on at least one of the a-axis, b-axis, or c-axis, using a metal oxide with grains aligned on at least one of the a-axis, b-axis, or c-axis as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (e.g., under high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0182] Compared to crystallization, but where the grains are not uniformly oriented on the a-axis, b-axis, or c-axis, the second buffer layer 32 is made of a metal oxide with uniformly oriented grains on at least one of the a-axis, b-axis, or c-axis. The second buffer layer 32 is more stable, so the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13. Consequently, under certain conditions (e.g., high temperature conditions), an oxide layer 20 will not form between the second electrode 12 and the second buffer layer 32, thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0183] Furthermore, the material of the first buffer layer 31 includes a single-crystal metal oxide, and / or the material of the second buffer layer 32 includes a single-crystal metal oxide, and / or the material of the channel layer 13 includes a single-crystal metal oxide. The single-crystal metal oxide has grains with consistent orientation along the a-axis, consistent orientation along the b-axis, and consistent orientation along the c-axis.
[0184] Compared to other crystallized metal oxides, using single-crystal metal oxides as the material for the channel layer 13 can further reduce the contact resistance between the channel layer 13 and the first electrode 11, as well as between the channel layer 13 and the second electrode 12. At the same time, it can further prevent the first electrode 11 and the second electrode 12 from absorbing oxygen from the channel layer 13, thereby improving the high-temperature stability and reliability of the vertical transistor and greatly enhancing the potential for miniaturization of the vertical transistor and the design of large-scale integrated circuits.
[0185] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material of the first buffer layer 31 can promote the growth of a crystallized channel layer 13 on the first buffer layer 31. Moreover, the crystallized first buffer layer 31 is relatively stable. Therefore, the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and thus will not form an oxide layer 20 between the first electrode 11 and the first buffer layer 31 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the first electrode 11 and the channel layer 13.
[0186] Compared to other crystallized metal oxides, using a single-crystal metal oxide as the material for the second buffer layer 32 makes the second buffer layer 32 more stable. Therefore, the second electrode 12 is less likely to absorb oxygen from the second buffer layer 32 and the channel layer 13, and thus will not form an oxide layer 20 between the second electrode 12 and the second buffer layer 32 under certain conditions (such as high temperature conditions), thereby further reducing the contact resistance between the second electrode 12 and the channel layer 13.
[0187] Furthermore, compared to using polycrystalline metal oxide as the material of the channel layer 13, using single-crystal metal oxide as the material of the channel layer 13 can reduce grain boundary scattering, improve the carrier mobility of the vertical transistor, and thus improve the reliability of the vertical transistor, such as the hot carrier injection effect and bias temperature instability.
[0188] In this application, since the channel layer 13 is made of crystallized metal oxide, and crystallized metal oxide has a higher oxygen vacancy generation energy (i.e., the energy required to form oxygen vacancies is relatively high), the chemical bonds between metal and oxygen in the metal oxide are difficult to break. As mentioned earlier, the channel layer 13 in this application is a crystallized channel layer. Therefore, the chemical bonds between metal and oxygen in the metal oxide in the channel layer 13 are difficult to break, and the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13. This prevents the introduction of oxygen vacancies in the region of the channel layer 13 that contacts the first electrode 11 and the second electrode 12, thus mitigating the problem of increased carrier concentration in the portion of the channel layer 13 near the first electrode 11 and the second electrode 12. This improves the short-channel effect and reduces the impact of the short-channel effect on the switching characteristics and miniaturization potential of the vertical transistor. Furthermore, because the short-channel effect is reduced, the variation in the bond performance (e.g., threshold voltage) of the vertical transistor can be improved, which is beneficial for the design of large-scale integrated circuits.
[0189] Furthermore, since the first electrode 11 and the second electrode 12 are unlikely to absorb oxygen from the channel layer 13, and the crystallized first buffer layer 31 is relatively stable, under certain conditions (e.g., high temperature conditions), the first electrode 11 is unlikely to absorb oxygen from the first buffer layer 31 and the channel layer 13, and the second electrode 12 is unlikely to absorb oxygen from the channel layer 13. Consequently, an oxide layer 20 will not form between the first electrode 11 and the channel layer 13, or between the second electrode 12 and the channel layer 13. This avoids increasing the contact resistance between the first electrode 11 and the channel layer 13, and between the second electrode 12 and the channel layer 13 due to the presence of the oxide layer 20. At the same time, it improves the thermal stability of the vertical transistor. Even if the subsequent process involves high temperature processes, the aforementioned problems such as short-channel effect and increased contact resistance will be improved.
[0190] Furthermore, the other explanations and beneficial effects of the embodiments of this application are the same as those of the first embodiment, and will not be repeated here.
[0191] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.
Claims
1. A chip, characterized by Includes a substrate and a vertical transistor disposed on the substrate; the vertical transistor includes: A first electrode, a first buffer layer, a channel layer, and a second electrode; the first electrode, the first buffer layer, the channel layer, and the second electrode are stacked along the direction from the substrate to the vertical transistor, and the conductivity of the first buffer layer is greater than that of the channel layer; the materials of the first buffer layer and the channel layer both include crystallized metal oxides; A gate structure; the gate structure is located on at least one side of the sidewall of the channel layer, the gate structure including a gate and a gate dielectric for isolating the channel layer from the gate.
2. The chip according to claim 1, characterized in that, The vertical transistor further includes a second buffer layer, which is disposed between the channel layer and the second electrode; The material of the second buffer layer includes crystallized metal oxide, and the material of the second buffer layer is a non-insulating material.
3. The chip according to claim 1 or 2, characterized in that, The grains in the first buffer layer are oriented uniformly on at least one of the a-axis, b-axis, and c-axis, and / or, the grains in the channel layer are oriented uniformly on at least one of the a-axis, b-axis, and c-axis; and / or, In the case where the vertical transistor further includes a second buffer layer, the grains in the second buffer layer are aligned on at least one of the a-axis, b-axis, and c-axis.
4. The chip of claim 3, wherein The material of the first buffer layer includes a single-crystal metal oxide, and / or the material of the second buffer layer includes a single-crystal metal oxide, and / or the material of the channel layer includes a single-crystal metal oxide.
5. The chip according to claim 1 or 2, characterized by The channel layer material also includes polycrystalline metal oxides, and the channel layer comprises a single grain; The number of vertical transistors is multiple, and among the multiple vertical transistors, at least some of the grains of the channel layer have different orientations.
6. The chip according to any one of claims 1 to 5, characterized in that The material of the first buffer layer includes at least one of indium and zinc; the total atomic percentage of indium and zinc in the material of the first buffer layer is greater than the total atomic percentage of indium and zinc in the material of the channel layer.
7. The chip of claim 6, wherein The channel layer material includes at least one of indium gallium zinc oxide, indium gallium oxide, indium aluminum zinc oxide, and indium tin zinc oxide; and / or, The material of the first buffer layer includes at least one of indium tin oxide and indium gallium oxide; and / or, If the vertical transistor further includes a second buffer layer, the material of the second buffer layer includes at least one of indium gallium zinc oxide, indium gallium oxide, indium aluminum zinc oxide, indium tin zinc oxide, and indium tin oxide.
8. The chip according to any one of claims 1 to 7, characterized in that The chip also includes a first spacer layer and a second spacer layer; The first spacer layer is disposed between the gate structure and the first buffer layer, and the second spacer layer is disposed between the gate structure and the second electrode; the gate dielectric extends from between the gate and the channel layer, to between the gate and the first spacer layer, and to between the gate and the second spacer layer.
9. The chip according to any one of claims 1-7, characterized in that, The chip also includes a first spacer layer and a second spacer layer; Along the direction from the substrate to the vertical transistor, the first spacer layer, the gate, and the second spacer layer are stacked, and the first spacer layer, the gate, and the second spacer layer are all disposed on the side of the gate dielectric away from the channel layer.
10. The chip according to claim 9, characterized in that, The vertical transistor is a ring-gate vertical transistor or a dual-gate vertical transistor; The gate dielectric is U-shaped and has an opening at the bottom; the channel layer includes a first channel layer and a second channel layer, the first channel layer fills the opening, and the second channel layer is located on the side of the first channel layer away from the first buffer layer. Wherein, along the direction from the gate to the channel layer, the size of the first channel layer is smaller than the size of the second channel layer, and the orthogonal projection of the first channel layer onto the second channel layer is located in the center.
11. A packaging structure, characterized in that, It includes a substrate and a chip as described in any one of claims 1-10, wherein the chip is disposed on the substrate.
12. An electronic device, characterized in that, The device includes a circuit board and the packaging structure of claim 11, wherein the packaging structure is disposed on the circuit board and the substrate of the packaging structure is located between the chip and the circuit board.
13. A method for fabricating a chip, characterized in that, The chip includes a vertical transistor, and the method for fabricating the vertical transistor includes: A first electrode, a first buffer layer, a channel layer, and a gate structure are formed on a substrate; the first electrode, the first buffer layer, and the channel layer are stacked along the direction from the substrate to the vertical transistor, and the conductivity of the first buffer layer is greater than that of the channel layer; the materials of the first buffer layer and the channel layer both include crystallized metal oxides; the gate structure is located on at least one side of the sidewall of the channel layer, and the gate structure includes a gate and a gate dielectric for isolating the channel layer and the gate; A second electrode is formed on the side of the channel layer opposite to the substrate.
14. The method for fabricating a chip according to claim 13, characterized in that, The chip also includes a first spacer layer and a second spacer layer; The formation of the first electrode, the first buffer layer, the channel layer, and the gate structure on the substrate includes: The first electrode and the first buffer layer are sequentially formed on the substrate; A first stacked structure is formed on the side of the first buffer layer away from the substrate, and a first cutout is provided in the first stacked structure; along the direction from the substrate to the vertical transistor, the first stacked structure includes a first spacer layer, a dummy gate, and a second spacer layer stacked together; A first sacrificial layer is filled in the first hollow portion; the first sacrificial layer has an etching selectivity ratio with the dummy gate; The dummy gate is removed, and the gate structure is formed on the sidewall of the first sacrificial layer. The gate structure is also located between the first spacer layer and the second spacer layer. The gate dielectric extends from between the gate and the first sacrificial layer, to between the gate and the first spacer layer, and to between the gate and the second spacer layer. Remove the first sacrificial layer and fill the channel layer into the first hollow portion.
15. The method for fabricating a chip according to claim 13, characterized in that, The chip also includes a first spacer layer and a second spacer layer; The formation of the first electrode, the first buffer layer, the channel layer, and the gate structure on the substrate includes: The first electrode and the first buffer layer are sequentially formed on the substrate; A second stacked structure is formed on the side of the first buffer layer away from the substrate, and a second cutout is provided in the second stacked structure; along the direction from the substrate to the vertical transistor, the second stacked structure includes a first spacer layer, the gate, and a second spacer layer stacked together; The gate medium and the channel layer are formed sequentially in the second hollow portion.
16. The method for fabricating a chip according to claim 15, characterized in that, The vertical transistor is a dual-gate vertical transistor or a ring-gate vertical transistor; the step of sequentially forming the gate dielectric and the channel layer in the second cutout includes: An insulating layer and a second sacrificial layer are sequentially formed in the second cutout portion; both the insulating layer and the second sacrificial layer extend from the side of the second spacer layer away from the substrate to the sidewall and bottom of the second cutout portion, and the portion of the second sacrificial layer in the second cutout portion forms a U-shape; The second sacrificial layer is partially removed to obtain a third sacrificial layer; the third sacrificial layer is located in the second hollow portion and is located on the side wall of the insulating layer; Under the protection of the third sacrificial layer, the insulating layer is partially removed to obtain the gate dielectric; the gate dielectric is U-shaped and has an opening at the bottom; Remove the third sacrificial layer; The channel layer is formed in the second cutout; the channel layer includes a first channel layer and a second channel layer, the first channel layer fills the opening, and the second channel layer is located on the side of the first channel layer away from the first buffer layer; wherein, along the direction from the gate to the channel layer, the size of the first channel layer is smaller than the size of the second channel layer, and the orthogonal projection of the first channel layer on the second channel layer is located in the center.
17. The method for fabricating a chip according to claim 15, characterized in that, The step of sequentially forming the gate dielectric and the channel layer in the second hollow portion includes: An insulating layer is formed sequentially in the second cutout portion; the insulating layer extends from the side of the second spacer layer away from the substrate to the sidewall and bottom of the second cutout portion, and the portion of the insulating layer in the second cutout portion forms a U-shape; The insulating layer is partially removed to obtain the gate dielectric; the gate dielectric is located on the sidewall of the second cutout portion. The channel layer is filled into the second hollowed-out portion.
18. The method for fabricating a chip according to any one of claims 13-17, characterized in that, Forming the first buffer layer includes: depositing the first buffer layer and subjecting the first buffer layer to high-temperature annealing; wherein the high-temperature annealing temperature is greater than 300°C and less than 600°C; and / or, Forming the trench layer includes: depositing the trench layer and subjecting the trench layer to high-temperature annealing; wherein the high-temperature annealing temperature is greater than 300°C and less than 600°C.
19. The method for fabricating a chip according to any one of claims 13-18, characterized in that, After forming the first electrode, the first buffer layer, the channel layer, and the gate structure on the substrate, and before forming the second electrode on the side of the channel layer opposite to the substrate, the chip fabrication method further includes: A second buffer layer is formed on the channel layer, the material of the second buffer layer comprising crystallized metal oxide; wherein the material of the second buffer layer is a non-insulating material.
20. The method for fabricating a chip according to any one of claims 13-19, characterized in that, The grains in the first buffer layer are oriented uniformly on at least one of the a-axis, b-axis, and c-axis, and / or, the grains in the channel layer are oriented uniformly on at least one of the a-axis, b-axis, and c-axis; and / or, In the case where the vertical transistor further includes a second buffer layer, the grains in the second buffer layer are aligned on at least one of the a-axis, b-axis, and c-axis.
21. The method for fabricating a chip according to claim 20, characterized in that, The material of the first buffer layer includes a single-crystal metal oxide, and / or the material of the second buffer layer includes a single-crystal metal oxide, and / or the material of the channel layer includes a single-crystal metal oxide.