A gallium oxide UMOSFET device and its fabrication method
By introducing a high-resistivity current blocking layer and etching a gate trench at a specific depth in the gallium oxide UMOSFET, a semi-enclosed gate oxide protection structure is constructed, which solves the problem of electric field concentration at the gate oxide corner and improves the device's breakdown voltage reliability and conduction performance.
Patent Information
- Application Number
- CN202611380324.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-07
- Publication Date
- 2026-11-17
AI Technical Summary
In existing gallium oxide UMOSFET technology, the deep trench through-hole structure removes the electric field shielding layer at the bottom of the gate oxide, resulting in electric field concentration at the gate oxide corner, which leads to a contradiction between decreased device reliability and limited conduction capability.
A high-resistance or semi-insulating current blocking layer is introduced on the upper part of the gallium oxide drift layer, and a semi-enclosed gate oxide protection structure is constructed through a gate trench etching process of a specific depth. The gate trench etching depth is less than the thickness of the current blocking layer, and the current blocking layers on both sides of the bottom of the gate trench are retained. A conductive recovery region is set in the center to connect the drift layer.
It effectively reduces the peak value of the gate oxide corner electric field, improves the withstand voltage reliability and conduction performance of the device, and balances high voltage reliability and low conduction loss.
Smart Images

Figure CN123124409A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor power device technology, and relates to a gallium oxide UMOSFET device and its fabrication method. Background Technology
[0002] Gallium oxide (β-Ga₂O₃) is considered an ideal material for manufacturing high-voltage, high-power power electronic devices due to its ultra-wide bandgap and extremely high theoretical critical breakdown electric field. To achieve high breakdown voltage, power devices typically require a thick, lightly doped drift layer to withstand reverse voltage. Vertically structured devices, where current flows vertically from the source to the drain, are more likely to achieve high current density and high breakdown voltage within the same chip area. However, unlike mature silicon carbide (SiC) or gallium nitride (GaN) technologies, β-Ga₂O₃ currently lacks a mature and reliable low-resistivity p-type doping technology. This limitation in material properties means that many traditional designs relying on p-body or p-shield regions in silicon-based or silicon carbide metal-oxide-semiconductor field-effect transistors (MOSFETs) cannot be directly applied to gallium oxide devices. To address this challenge and achieve enhanced turn-off while effectively suppressing leakage current, researchers commonly use high-resistivity or semi-insulating current blocking layers (CBLs) to replace the p-type region. CBLs are typically formed by implanting deep-level impurities such as N, Mg, C, and Fe, or by related defect engineering. Their core function is to prevent electrons from directly entering the drift layer from the source when the device is turned off.
[0003] In existing gallium oxide U-groove gate MOSFET (UMOSFET) designs, a common approach is to form a channel bottom layer (CBL) near the surface of the drift layer, and then etch out the U-shaped gate trench. To ensure effective control of the conductive channel by the gate, the gate trench is often etched quite deep, directly through the CBL and extending to the underlying n-type drift layer, such as... Figure 2 As shown. The advantage of this "through-hole" structure lies in its direct conduction path and strong gate control capability. Current can flow smoothly from the source region through the gate-controlled trench sidewalls or bottom path into the drift layer. This design concept solves the gate control problem to a certain extent and is an important advancement in existing technology.
[0004] However, this design, which sacrifices some shielding structure for conduction performance, also brings significant side effects and reliability issues. First, when the gate trench penetrates the CBL, the bottom of the gate oxide layer and its corners are closer to the drift layer subjected to high electric fields. Under high-voltage turn-off, due to the abrupt changes in geometric curvature and material interface, local peak electric fields are easily formed at the corners of the trench bottom. Second, once this peak electric field is concentrated at the corners of the thin gate dielectric layer, the device failure mode will preferentially manifest as gate oxide breakdown rather than semiconductor bulk breakdown. Since the thickness of the gate dielectric is much smaller than that of the semiconductor layer, it is more sensitive to defects and interface states, making reliability issues particularly prominent. Finally, this structure removes the high-resistivity CBL material at the bottom of the gate oxide for conduction, causing the gate oxide to lose a crucial electric field shielding layer. Conversely, if the CBL is fully retained for shielding, it will block the conduction current, causing the device to fail to turn on normally. Therefore, how to retain the electric field shielding advantage of the CBL while restoring an effective current conduction path has become the core contradiction that current gallium oxide UMOSFET technology urgently needs to solve. Summary of the Invention
[0005] To address the problems existing in the prior art, this invention provides a gallium oxide UMOSFET device and its fabrication method, thereby solving the core technical problem in the existing gallium oxide UMOSFET technology where the deep trench through-hole structure used to pursue conduction performance removes the electric field shielding layer at the bottom of the gate oxide, resulting in electric field concentration at the gate oxide corner, which leads to the core contradiction between decreased device reliability and limited conduction capability.
[0006] This invention is achieved through the following technical solution: A gallium oxide UMOSFET device includes a drain, a gallium oxide substrate, a gallium oxide drift layer, a current blocking layer, a conductivity recovery region, and an n-type UMOSFET. ++ Source region, source electrode, gate dielectric layer, and gate; The drain electrode is disposed on the lower surface of the gallium oxide substrate; The gallium oxide drift layer is disposed on the gallium oxide substrate; The current blocking layer is disposed on top of the gallium oxide drift layer; The device is provided with a gate trench, the etching depth of which is less than the thickness of the current blocking layer, the two sides of the bottom of the gate trench are retained with the current blocking layer, the conductive recovery region is provided in the center of the bottom of the gate trench, the conductive recovery region is connected downward to the gallium oxide drift layer, and the lateral width of the conductive recovery region is less than the lateral width of the gate trench. n is set above the current blocking layer ++ Source region, the n ++ A source electrode is formed on the source region; The inner wall of the gate trench is covered with a gate dielectric layer, and the gate dielectric layer fills the cavity of the trench. The current blocking layers on both sides are respectively arranged on the outside of the bottom corner of the gate dielectric layer to form an electric field shield for the bottom corner of the gate dielectric layer.
[0007] Optionally, the lateral width of the conductive recovery region is smaller than the lateral width of the gate slot.
[0008] Optionally, the lateral width of the gate groove is 2~8μm; the lateral width of the conductive recovery region is 0.5~5μm.
[0009] Optionally, the gate trench etching depth is 40% to 90% of the current blocking layer thickness.
[0010] Optionally, the thickness of the current blocking layer is 0.5~2.0μm, and the etching depth of the gate trench is 0.5~0.9μm.
[0011] Optionally, the current blocking layer is formed of at least one deep-level compensating impurity selected from N, Mg, C, and Fe; the conductivity recovery region is formed of at least one donor impurity selected from Si, Sn, Ge, Nb, and Ta.
[0012] Optionally, the gate dielectric layer includes Al2O3, SiO2, HfO2, and SiN. x One or more of AlN; the thickness of the gate dielectric layer is 30nm~80nm.
[0013] The above-mentioned method for fabricating a gallium oxide UMOSFET device includes the following steps: A gallium oxide substrate is provided, and a drain is formed on the lower surface of the gallium oxide substrate; A gallium oxide drift layer is formed on the upper surface of the gallium oxide substrate; A current blocking layer is formed on the gallium oxide drift layer; Etching forms a gate trench, wherein the etching depth of the gate trench is less than the thickness of the current blocking layer; A conductive recovery region is formed in the center of the bottom of the gate trench, and the conductive recovery region is connected downward to the gallium oxide drift layer; A gate dielectric layer is formed on the inner wall of the gate groove; A gate electrode is filled within the cavity enclosed by the gate dielectric layer; an n-type gate electrode is formed above the current blocking layer. ++ Source region and source pole.
[0014] Optionally, forming a conductive recovery region at the center of the bottom of the gate trench specifically involves: After forming a complete current blocking layer, the injection window is defined by photolithography; Donor impurities are injected into the center of the bottom of the gate trench through the injection window to locally offset the compensation effect of the current blocking layer, forming an n-type conductivity recovery region.
[0015] Optionally, forming a current blocking layer on the gallium oxide drift layer specifically involves: A patterned injection mask is formed by photolithography, and the mask has a window reserved in the central region at the bottom of the gate trench; Ion implantation is performed through the mask to form a current blocking layer in the regions on both sides of the window, while the window region remains a conductive gallium oxide drift layer as a subsequent conductive recovery region.
[0016] Compared with the prior art, the present invention has the following beneficial technical effects: This invention discloses a gallium oxide UMOSFET device. By introducing a high-resistance or semi-insulating current blocking layer on top of the gallium oxide drift layer and combining it with a gate trench etching process of a specific depth, a surrounding gate oxide protection structure is constructed, thereby solving the contradiction between electric field concentration at the gate oxide corner and limited conduction capability in existing deep trench through-hole structures. Specifically, this structure strictly controls the etching depth of the gate trench to be less than the thickness of the current blocking layer, so that after etching, undepleted current blocking layers are naturally retained on both sides of the bottom of the gate trench, while the gallium oxide drift layer is only connected downward through the conductivity recovery region in the central region of the bottom of the gate trench. This design ensures that the current blocking layers retained on both sides of the bottom of the gate trench are located precisely on the outer side of the bottom corner of the gate dielectric layer. The high-resistance characteristics of the current blocking layer effectively shield and buffer the electric field at the sharp corner of the bottom of the gate dielectric layer, avoiding excessive density and peak concentration of electric field lines at the gate oxide corner under high voltage, thereby significantly improving the withstand voltage reliability and gate oxide integrity of the device. Meanwhile, because a conductive recovery region connecting downwards to the drift layer is set in the central region at the bottom of the gate trench, this region is not completely blocked by the high-resistivity layer, but retains a low-resistivity conductive path in the vertical direction. This ensures that electrons can flow from the source region to the drift layer and drain in the conducting state, avoiding a sharp increase in on-resistance caused by the introduction of a blocking layer across the entire region. Therefore, this structure achieves electric field optimization at the weak point of the gate oxide without sacrificing the device's conduction performance, balancing high-voltage reliability and low conduction loss. Attached Figure Description
[0017] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation on the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1This is a schematic cross-sectional view of a gallium oxide UMOSFET device according to the present invention; Figure 2 This is a schematic cross-sectional view of a prior art punch-through gallium oxide UMOSFET device. Figure 3 The electric field distribution cloud map of gallium oxide UMOSFET devices in the off state under different gate trench etching depths; Figure 4 Comparison curves of electric field intensity at the corner of the gate oxide layer under different gate trench etching depths; Figure 5 This is a schematic cross-sectional view of the device fabrication process of the gate bottom donor recovery process after full-area current blocking layer (CBL) injection in Embodiment 4 of the present invention; Figure 6 This is a schematic cross-sectional view of the device fabrication process for forming a current blocking layer (CBL) by patterned injection in Embodiment 4 of the present invention.
[0019] Wherein: 1. Drain; 2. Gallium oxide substrate; 3. Gallium oxide drift layer; 4. Current blocking layer; 5. Conductivity recovery region; 6. n ++ 7. Source region; 8. Gate dielectric layer; 9. Gate. Detailed Implementation
[0020] To enable those skilled in the art to understand the features and effects of the present invention, the terms and expressions used in the specification and claims are explained and defined in general below. Unless otherwise specified, all technical and scientific terms used herein have the ordinary meaning understood by those skilled in the art regarding the present invention, and in case of conflict, the definitions in this specification shall prevail.
[0021] The theories or mechanisms described and disclosed herein, whether right or wrong, should not in any way limit the scope of the invention, that is, the contents of the invention can be implemented without being limited by any particular theory or mechanism.
[0022] In this document, all features defined by numerical ranges or percentage ranges, such as numerical values, quantities, contents, and concentrations, are for the sake of brevity and convenience only. Accordingly, descriptions of numerical ranges or percentage ranges should be considered as covering and specifically disclosing all possible sub-ranges and individual numerical values (including integers and fractions) within those ranges.
[0023] In this article, unless otherwise specified, “contains,” “includes,” “containing,” “has,” or similar terms cover the meanings of “composed of” and “mainly composed of,” for example, “A contains a” covers the meanings of “A contains a and others” and “A contains only a.”
[0024] For the sake of brevity, not all possible combinations of the technical features in each implementation scheme or embodiment are described herein. Therefore, as long as there is no contradiction in the combination of these technical features, the technical features in each implementation scheme or embodiment can be combined arbitrarily, and all possible combinations should be considered within the scope of this specification.
[0025] The present invention will be further illustrated below with reference to specific embodiments. It should be understood that these embodiments are for illustrative purposes only and are not intended to limit the scope of the invention. Furthermore, it should be understood that after reading the teachings of this invention, those skilled in the art can make various alterations or modifications to the invention, and these equivalent forms also fall within the scope defined by the appended claims.
[0026] The following examples use instruments and equipment conventional in the art. Experimental methods in the following examples, unless otherwise specified, are generally performed under conventional conditions or as recommended by the manufacturer. All raw materials used in the following examples are conventional commercially available products with specifications conventional in the art. In this specification and the following examples, unless otherwise specified, "%" refers to weight percentage, "parts" refers to parts by weight, and "ratio" refers to weight proportion.
[0027] Example 1 like Figure 1 As shown, this invention discloses a gallium oxide UMOSFET with a semi-enclosed gate oxide structure, including a drain 1, a gallium oxide substrate 2, a gallium oxide drift layer 3, a current blocking layer 4, a conductivity recovery region 5, and an n-type UMOSFET. ++ The device comprises a source region 6, a source electrode 7, a gate dielectric layer 8, and a gate electrode 9; a drain electrode 1 is disposed on the lower surface of a gallium oxide substrate 2; a gallium oxide drift layer 3 is disposed on the gallium oxide substrate 2; a current blocking layer 4 is disposed on the upper part of the gallium oxide drift layer 3; the device has a gate trench, the etching depth of which is less than the thickness of the current blocking layer 4; the bottom of the gate trench has current blocking layers 4 on both sides; a conductivity recovery region 5 is disposed in the center of the bottom of the gate trench; the conductivity recovery region 5 is connected downward to the gallium oxide drift layer 3; the lateral width of the conductivity recovery region 5 is less than the lateral width of the gate trench; an n is disposed above the current blocking layer 4. ++ Source region 6, the n ++ A source electrode 7 is formed on the source region 6; the inner wall of the gate trench is covered with a gate dielectric layer 8, and the gate 9 is filled in the cavity surrounded by the gate dielectric layer 8; the current blocking layers 4 on both sides are respectively arranged on the outside of the bottom corner of the gate dielectric layer 8 to form an electric field shield for the bottom corner of the gate dielectric layer 8.
[0028] Specifically, this invention discloses a gallium oxide UMOSFET with a semi-enclosed gate oxide structure. This device mainly includes a drain 1, a gallium oxide substrate 2, a gallium oxide drift layer 3, a current blocking layer 4, a conductivity recovery region 5, and an n... ++ The device consists of a source region (6), a source electrode (7), a gate dielectric layer (8), and a gate electrode (9). The overall structure is a vertical power device, allowing current to be transported vertically along the device's thickness.
[0029] The drain 1 is disposed on the lower surface of the gallium oxide substrate 2, serving as the bottom lead-out electrode of the device. The gallium oxide substrate 2 is a conductive gallium oxide substrate, providing mechanical support for the device while enabling current conduction. The gallium oxide drift layer 3 is formed on the upper surface of the gallium oxide substrate 2. The gallium oxide drift layer 3 undertakes the voltage withstand function of the device and is the main voltage withstand area when the device is operating at high voltage.
[0030] The current blocking layer 4 is disposed in the upper region of the gallium oxide drift layer 3. This device has a gate trench structure, and the gate trench is etched downwards. The etching depth of the gate trench is less than the thickness of the current blocking layer 4 itself. Therefore, after the gate trench etching is completed, a portion of the current blocking layer 4 is still retained on the left and right sides of the bottom of the gate trench, and the current blocking layer 4 is not completely etched through and removed.
[0031] A conductivity recovery region 5 is located at the center of the bottom of the gate trench, and the conductivity recovery region 5 is directly connected to the gallium oxide drift layer 3. The lateral width of the conductivity recovery region 5 is smaller than the lateral width of the gate trench, so that the current blocking layer 4 is retained on both sides of the bottom of the gate trench except for the conductivity recovery region 5. The conductivity recovery region 5 retains the vertical conduction path of the device, and avoids the current blocking layer 4 from completely blocking the carrier transport, which would cause the on-resistance of the device to deteriorate.
[0032] n is formed on the upper side of the current blocking layer 4. ++ Source region 6,n ++ Source region 6 is a heavily doped n-type gallium oxide region used to achieve a low-resistance contact at the source end; n ++ Source electrode 7 is formed above source region 6, and source electrode 7 serves as the metal lead-out electrode at the source end of the device.
[0033] The entire inner wall surface of the gate trench is covered by the gate dielectric layer 8, which also covers the sidewalls and bottom of the gate trench. The gate 9 is filled in the inner cavity formed by the gate dielectric layer 8 and serves as the gate conductive electrode of the device.
[0034] The remaining current blocking layers 4 on both sides are respectively arranged on the outer side of the bottom corner of the gate dielectric layer 8. By utilizing the charge compensation effect of the current blocking layers 4, an electric field shield is formed in the bottom corner area of the gate dielectric layer 8, which can effectively reduce the electric field peak at the gate oxide corner and the bottom position, alleviate the problem of local electric field concentration in the gate dielectric under high voltage conditions, reduce the risk of premature breakdown of the gate dielectric, and improve the high voltage reliability of the device.
[0035] Example 2 To further explain the solution of the present invention, this embodiment will be used as an example: like Figure 1 As shown, the present invention provides a gallium oxide UMOSFET device. Figure 2 This is a schematic cross-sectional view of a prior art punch-through gallium oxide UMOSFET device; that is... Figure 2 The device features a conventional through-hole structure with a gate trench etched through the current blocking layer 4. From bottom to top, the device is arranged with the drain (D), gallium oxide substrate (Ga2O3 substrate), gallium oxide drift layer (Ga2O3 drift layer), current blocking layer (CBL), and n... ++ The device consists of a source region and a source electrode (S). A gate trench is etched into the upper part of the device, and a gate electrode (G) is placed inside the trench. A gate dielectric layer is disposed between the gate electrode and the sidewall of the trench. This device is a conventional through-hole structure. During the downward etching process, the gate trench completely penetrates the current blocking layer (CBL), and the bottom of the trench is directly exposed to the gallium oxide drift layer (Ga2O3 drift layer). The current blocking layer (CBL) only remains on the left and right sides of the trench; there is no current blocking layer (CBL) material at the bottom of the trench. When the device is in the off-voltage state, the electric field is concentrated at the bottom corner of the gate dielectric layer. The peak electric field level at the gate oxide corner is high, which can easily cause premature breakdown of the gate dielectric, limiting the high-voltage operating reliability of the device. When the device is turned on, electrons are etched from n... ++ Starting from the source region, the current flows directly downwards through the conductive channel formed by the gate trench sidewalls into the gallium oxide drift layer, and then through the gallium oxide substrate to the drain (D). Although this punch-through structure ensures that the device has a complete conduction current path, it loses the electric field shielding capability of the current blocking layer (CBL) at the gate dielectric corner, resulting in significant gate dielectric reliability defects in high-voltage applications.
[0036] Unlike traditional through-hole structures, the etching depth of the gate trench in this invention is less than the thickness of the current blocking layer 4, so that the bottom of the gate trench does not completely penetrate the current blocking layer 4. The gate dielectric layer 8 covers the sidewalls and bottom of the gate trench, and the gate 9 is disposed inside the gate dielectric layer 8. Because the current blocking layer 4 is not completely etched through, it is retained on both sides of the bottom of the gate trench, in a local area below the bottom, or around the bottom, forming a semi-enclosed structure of the bottom and corners of the gate dielectric layer 8 when viewed in cross-section of the device.
[0037] Simultaneously, a conductivity recovery region 5 is provided at the corresponding central position at the bottom of the gate trench. The conductivity recovery region 5 can be an n-type recovery region formed by donor injection, or an original n-type region that has not been deeply compensated, or a region whose conductivity has been restored through local annealing, local epitaxy, or other process methods. The lateral width of the conductivity recovery region 5 is smaller than the lateral width of the gate trench, so that the current blocking layer 4 is still retained on both sides of the conductivity recovery region 5 as a shielding area.
[0038] Specifically, the gallium oxide vertical transistor of the present invention mainly includes a gate trench, a current blocking layer 4, a conductivity recovery region 5, and an n-type gate. ++ The specific positional relationships and functional descriptions of the components in source region 6 and gallium oxide drift layer 3 are as follows: Regarding the layout of the gate trench and current blocking layer 4: The gate trench extends downward from the device surface, and its etching depth is designed to be less than the thickness of the current blocking layer 4. The current blocking layer 4 is located in the upper region of the gallium oxide drift layer 3, and its distribution range covers at least to both sides of the bottom of the gate trench. The key to this layout is to ensure that the current blocking layer 4 is not completely etched through by the gate trench, thereby retaining shielding material at the bottom of the gate trench. When the device is in the off state, the retained current blocking layer 4 can effectively share and reshape the electric field distribution inside the device, significantly reducing the peak electric field at the corner of the gate dielectric layer 8 and preventing premature breakdown of the gate dielectric layer 8.
[0039] Regarding the construction of the conductive channel: A conductive recovery region 5 is provided at the center of the bottom of the gate trench, and the width of the conductive recovery region 5 is smaller than the width of the gate trench. The main function of the conductive recovery region 5 is to provide a current window, allowing electrons to bypass or pass through the current blocking layer 4 into the gallium oxide drift layer 3 when the device is in conduction mode. At the same time, the current blocking layer 4 material is still retained on both sides of the gate trench. This design can restore the conductivity of the device without destroying the electric field shielding effect on both sides.
[0040] In addition, the n ++ The source region 6 is located on the surface area above the current blocking layer 4 or on both sides of the gate trench, and is mainly used as an electron injection region; the gallium oxide drift layer 3 is arranged between the current blocking layer 4 and the gallium oxide substrate 2, and serves as the main functional part of the device. It can withstand the main blocking voltage in the off state and can complete the current transmission in the on state.
[0041] When the device is in the off state, the drain 1 experiences a high voltage, and a high electric field is formed inside the gallium oxide drift layer 3. Since the gate trench does not penetrate the current blocking layer 4, there are still high-resistivity or semi-insulating current blocking layers 4 on both sides of the bottom of the gate dielectric layer 8. This part of the current blocking layer 4 acts as an electric field buffer and shielding region, which can reduce the electric field concentration at the corner of the gate dielectric layer 8, so that the electric field peak is more distributed in the material body of the current blocking layer 4 and the gallium oxide drift layer 3, rather than concentrated at the corner of the thin gate dielectric layer 8.
[0042] When the device is in the ON state, a positive gate voltage is applied to the gate 9, forming a conductive channel for electron accumulation on or near the gate trench sidewall. Electrons flow from n... ++ Starting from source region 6, the current flows through the gate control region and into the conductivity recovery region 5 at the center of the bottom of the gate trench, then into the lower n-type gallium oxide drift layer 3, and finally to the drain 1. Therefore, it can be seen that the current blocking layer 4 does not completely block the current; it only serves as a shield on both sides of the bottom of the gate trench, while the conductivity recovery region 5 at the center of the bottom of the gate trench bears the conductivity function of the device.
[0043] Furthermore, in a specific embodiment of the present invention, in order to achieve a good balance between high breakdown voltage and low on-resistance, the key structural parameters of the gallium oxide vertical transistor were optimized. The thickness of the current blocking layer (CBL) can be set to 0.5~2.0 μm, with a preferred range of approximately 1.0 μm. If the CBL thickness is too thin, it will not provide effective electric field shielding, leading to a decrease in breakdown voltage performance; if it is too thick, it will significantly increase the difficulty of the subsequent formation of the conductive recovery region, affecting the device's conduction performance.
[0044] For the geometry of the gate trench, its depth is designed to be less than the thickness of the CBL, preferably 40%-90% of the CBL thickness, with specific examples ranging from 600 to 800 nm. This shallower-than-CBL design aims to retain the semi-enclosed shielding region at the bottom of the gate trench, thereby effectively protecting the gate oxide corners while ensuring sufficient gate control capability to regulate the channel current. The width of the gate trench can be set to 2-8 μm, preferably about 4 μm. This width range takes into account the gate control area, the resolution limitations of the photolithography process, and the layout requirements of the conductive window to ensure that the device maintains stable electrical characteristics under the trend of miniaturization. In addition, the conductive recovery region located in the center of the bottom of the gate trench can be set to a width of 0.5-5 μm and must be less than the width of the gate trench, preferably 2-3 μm. This size design ensures that the current mainly conducts through the central region, while retaining the CBL material on both sides to maintain the electric field shielding effect on the gate oxide corners.
[0045] Regarding material doping and dielectric selection, the CBL forms a high-resistivity or semi-insulating region by introducing deep-level impurities or compensating impurities. Optional dopants include N, Mg, C, Fe, or other deep-level impurities, with N or Mg being preferred as the dopant element to achieve effective compensation for background carriers. To form a conduction recovery region (i.e., a conduction window) in the CBL, donor impurities need to be introduced to counteract the deep-level compensation, restoring the n-type conductivity characteristics of the window region. Optional conduction recovery impurities include Si, Sn, Ge, Nb, Ta, or other donor elements; in this embodiment, Si is preferred as the dopant.
[0046] The choice of material for the gate insulating layer (gate dielectric) is crucial to the reliability of the device. Optional gate dielectric materials include Al₂O₃, SiO₂, HfO₂, and SiN₂. x AlN or a composite layer thereof. In a preferred embodiment of the present invention, Al2O3 is used as the gate dielectric. Compared with traditional SiO2, Al2O3 has a higher dielectric constant (high k value), which not only helps to improve gate control capability, but also further improves the insulation reliability of the gate oxide bottom through optimization of the equivalent oxide layer thickness or increase of the physical thickness, thereby withstanding higher electric field strength.
[0047] Example 3 To verify the effect of the structure of this invention on the regulation of the internal electric field of the device, two-dimensional device simulation was conducted. Three sets of comparative structures were set up for simulation. The current blocking layer (CBL) thickness of the three sets of devices was 1 μm, the gate trench width was set to 5 μm, and the width of the conductive channel reserved in the middle of the bottom of the gate trench was 3 μm. A reverse bias voltage of 2000V was applied to the simulation to obtain the two-dimensional electric field distribution results of the devices under the off state of different structures.
[0048] Figure 3 The electric field distribution cloud maps of gallium oxide UMOSFET devices in the off-state state are shown at different gate trench etching depths, corresponding from left to right to three simulation conditions: gate trench fully through the current blocking layer (CBL), gate trench depth 200 nm shallower than the current blocking layer (CBL), and gate trench depth 500 nm shallower than the current blocking layer (CBL). The electric field cloud maps show that, in the control group (gate trench fully through the current blocking layer (CBL) structure), significant electric field concentration occurs at the gate oxide corners and under the gate. As the gate trench etching depth decreases, the thickness of the current blocking layer (CBL) remaining on both sides of the bottom of the gate trench gradually increases, effectively suppressing the high electric field region at the gate oxide corners. The high electric field inside the device gradually shifts into the gallium oxide drift layer material, effectively alleviating the problem of local electric field concentration in the gate dielectric layer.
[0049] Figure 4 This is a comparison curve of the electric field intensity on the cross section at the bottom of the gate oxide layer at different gate trench etching depths. This curve is... Figure 3 The simulation results were plotted by extracting the electric field intensity data at each position on the bottom of the gate using a horizontal cross-section. The red curve represents the control group, corresponding to the conventional structure where the gate trench completely penetrates the current blocking layer (CBL). In this structure, the electric field peak is highest at the corner of the gate oxide layer, and the excessively high local electric field can easily cause gate dielectric breakdown failure. The blue curve corresponds to the structure designed in this invention, where a 100nm thick current blocking layer (CBL) is retained at the bottom of the gate trench without being etched through, and the electric field peak at the corner of the gate oxide layer is significantly reduced. The green curve also represents the structure designed in this invention, where a 500nm thick current blocking layer (CBL) is retained at the bottom of the gate trench without being etched through, and the electric field peak at the corner is further reduced.
[0050] The simulation results above confirm that by controlling the gate trench etching depth to not penetrate the current blocking layer (CBL), the electric field at the corner of the gate oxide layer can be suppressed by relying on the current blocking layer (CBL) left on both sides of the gate trench. The larger the thickness of the current blocking layer (CBL) left at the bottom of the gate trench, the more prominent the electric field suppression effect at the corner, which can significantly reduce the risk of breakdown failure of the gate dielectric layer and improve the high-voltage operation reliability of gallium oxide UMOSFET devices.
[0051] Example 4 like Figure 5 As shown, this embodiment discloses a method for fabricating a gallium oxide UMOSFET with a semi-enclosed gate oxide structure, which is a gate bottom donor recovery process after full-area current blocking layer (CBL) implantation. This process is suitable for first forming a uniform current blocking layer (CBL), and then restoring conductivity characteristics in the central region at the bottom of the gate trench through local donor implantation, fully embodying the design concept of "first forming the blocking layer, and then locally restoring the conductivity window" of this invention. Specifically, the above fabrication process is as follows: Step S1: Epitaxial layer growth First, an n+ type β-Ga2O3 substrate is provided as the starting material. The substrate thickness can be 300–700 μm, primarily serving as a low-resistivity layer on the drain side. An n- type β-Ga2O3 drift layer is formed on the first main surface of the substrate using an epitaxial growth process. The thickness of the drift layer is set to 4–15 μm, preferably 8–10 μm, to bear the main blocking voltage. The Si or Sn doping concentration in the drift layer is controlled at 5 × 10⁻⁶. 15 ~5×10 16 cm -3 Between, preferably about 2×10 16 cm -3 This is to ensure that the device has a suitable balance between withstand voltage and on-resistance.
[0052] Step S2: Surface cleaning and pretreatment The epitaxial wafer undergoes rigorous organic cleaning and surface pretreatment. It is ultrasonically cleaned sequentially with acetone, isopropanol or ethanol, and deionized water, each step lasting 3–10 minutes, followed by drying with N2. To further improve surface cleanliness, optional O2 plasma cleaning for 30–120 seconds can be performed. This step aims to thoroughly remove organic contaminants and particles, improving the uniformity of subsequent plasma-enhanced chemical vapor deposition (PECVD), photolithography, and ion implantation.
[0053] Step S3: Deposit and inject sacrificial layer A sacrificial implantation layer is deposited on the surface of the drift layer. SiO2 is deposited using PECVD, with a thickness ranging from 50 to 150 nm, preferably approximately 100 nm, and the deposition temperature is controlled between 250 and 350 °C. This sacrificial layer references existing UMOSFET patented technology and is primarily used to reduce surface damage and channel contamination caused by subsequent ion implantation.
[0054] Step S4: Forming the current blocking layer (CBL) Full-area ion implantation was performed to introduce deeply dominant or deep-level compensating impurities (such as N, Mg, C, Fe, etc., with N ions preferred) to form a continuous high-resistivity CBL. The target bulk concentration was set at 5 × 10⁻⁶. 18 ~5×10 19 cm -3 1×10 is preferred 19 ~4×10 19 cm -3 An approximate box-shaped distribution is formed through multi-energy injection (e.g., covering the range of 100–700 keV). The specific energy and dose are determined by simulation using Stopping and Range of Ions in Matter (SRIM) software / Transport of Ions in Matter (TRIM) software. In this embodiment, the target thickness of the CBL is approximately 1 μm (corresponding to a dose of approximately 5 × 10⁻⁶). 14 ~5×10 15 cm -2 This thickness design is to ensure that the subsequent 600~800 nm deep gate trench will not completely penetrate the CBL, thus preserving the shielding effect at the bottom.
[0055] Step S5: CBL injection followed by annealing The implanted samples are then subjected to high-temperature annealing to repair lattice damage and stabilize deep-level compensation. If N-ion implantation is used, annealing at 1100–1200 °C for 30–60 minutes (e.g., 1200 °C for 30 minutes) in an N2, O2, or inert atmosphere is preferred. The advantage of N-ions is their low diffusion at high temperatures, which helps maintain clear CBL boundaries. If Mg-ion implantation is used, the annealing temperature can be selected from 900–1100 °C, but special attention must be paid to the diffusion of Mg.
[0056] Step S6: Remove the sacrificial layer The SiO2 sacrificial layer on the surface is removed using a buffered oxide etchant (BOE) or dilute hydrofluoric acid (HF) solution, followed by rinsing with deionized water and drying with nitrogen. Alternatively, an HCl or organic cleaning step can be added. This step aims to prevent sacrificial layer residue from affecting subsequent source implantation and gate trench etching processes.
[0057] Step S7: Forming the source region To form an n++ source region or a highly doped source contact layer, two methods can be used: Method A involves selective Si ion implantation with a target depth of 50–150 nm and a concentration of 1 × 10⁻⁶. 19 ~5×10 19 cm -3 (Refer to 170 keV Si implantation to form a deep region of approximately 100 nm); Option B involves epitaxially growing a 100–300 nm highly doped β-Ga₂O₃ layer (doping concentration 1 × 10⁻⁶) via Metal-Organic Chemical Vapor Deposition (MOCVD). 19 ~5×10 19 cm -3 If Si implantation is used, subsequent annealing in a N2 atmosphere at 900~1000℃ for 1~30 minutes can activate impurities and provide low contact resistance.
[0058] Steps S8-S9: Gate trench definition and etching A thick resist or hard mask (such as SiO2, Ni, Cr, or Al2O3) is coated, and the gate trench region is defined by photolithography. The gate trench width is designed to be 2~8 μm, preferably about 4 μm, and the adjacent source regions are located on both sides of the gate trench. Subsequently, a shallow U-shaped gate trench is formed using an inductively coupled plasma (ICP) / reactive ion etching (RIE) process. The etching gas can be Cl2 / BCl3 / Ar (e.g., Cl2 35-60 sccm, BCl 35-10 sccm, Ar 5-10 sccm), the ICP power is 300~800 W (preferably 600 W), the radio frequency (RF) bias power is 50~150 W (preferably 50~100 W), and the chamber pressure is 5~20 mTorr (preferably 10~15 mTorr). The key is to control the etching depth to 600~800 nm by controlling the endpoint, ensuring that the trench depth is less than the CBL thickness of about 1 μm, so that the bottom of the trench is still within the CBL or only partially penetrated, without completely destroying the bottom shielding layer.
[0059] Step S10: Surface treatment of the grid groove After gate etching, surface damage repair and corner rounding are performed. This can be done by wet treatment in H3PO4 solution at 100-120℃ for 0.5-3 minutes (preferably 110℃, 1 minute), or by dilute acid cleaning, low-power O2 / Ar plasma treatment, or thermal annealing. This step references the phosphoric acid wet repair technology in existing UMOSFET processes, aiming to reduce dangling bonds and damage caused by ICP etching and lower gate leakage current.
[0060] Steps S11-S13: Formation of the conductivity recovery region This is a key feature of the invention. First, an implantation window is defined in the center of the bottom of the gate trench using photoresist, hard mask, or sidewall spacer technology. The window width is designed to be 0.5~5 μm, preferably 2~3 μm, and must be less than the gate trench width of 4 μm to ensure central conduction while retaining the semi-enclosed shielding of the CBL on both sides. Subsequently, donor impurities (preferably Si, but also Sn, Ge, Nb, and Ta) are implanted into the bottom of the gate trench through this window. The implantation depth should cover the remaining CBL thickness below the bottom of the gate trench (example target depth 200~500 nm), and the target donor concentration is 1×10⁻⁶. 18 ~5×10 19 cm -3 (Preferred 1×10) 19 ~2×10 19 cm -3 ), dosage approximately 1×10 13 -5×10 15 cm-2 Multiple energy injections can be used to penetrate the remaining CBL. Finally, the donor injection region is activated by annealing (e.g., annealing at 900-1000°C for 1-30 minutes in N2 or Ar; if there are concerns about disrupting the CBL distribution, rapid thermal annealing (RTA), such as at 950°C for 1-5 minutes, can be used) to locally offset the main compensation of N / Mg, forming an n-type conductivity recovery region, allowing current to enter the drift layer through the center of the gate trench bottom.
[0061] Step S14: Deposit gate dielectric layer The gate dielectric layer is deposited using atomic layer deposition (ALD), preferably Al2O3, with a thickness of 30–80 nm (preferably 40–70 nm), at a deposition temperature of approximately 200–300 °C. SiO2, HfO2, or an Al2O3 / SiO2 composite dielectric can also be used. The ALD process ensures the formation of a conformally sound MOS gate dielectric on the trench sidewalls and bottom. For issues with insufficient trench sidewall coverage, the number of ALD cycles can be appropriately increased.
[0062] Step S15: Metal electrode formation Form the source, drain, and gate metals. The source and drain metals can be Ti / Au (50 / 150 nm) or Ti / Al / Ni / Au systems, formed via electron beam evaporation or magnetron sputtering followed by a lift-off process; the drain is located on the back side of the substrate. Ohmic contact annealing of the source and drain can be performed at 400–500 °C in N2 for 1–2 minutes, or optimized according to the specific contact system. The gate metal can be Ni / Au (50 / 150 nm), or Pt / Au, Ti / Au, etc.
[0063] Step S16: Passivation and Windowing Finally, a passivation layer is formed and pad windows are created. SiN is deposited using plasma-enhanced chemical vapor deposition (PECVD). x A passivation layer of 100–500 nm is used, consisting of SiO2 or ALD Al2O3. Source, gate, and drain pad windows are then created using photolithography. This step aims to improve device surface stability and package compatibility.
[0064] Example 5 like Figure 6As shown, this embodiment discloses a method for fabricating a gallium oxide UMOSFET with a semi-surrounded gate oxide structure. The method involves shallow trench etching after reserving a window for patterned gate bottom implantation (CBL). This method is suitable for avoiding damage caused by secondary donor implantation at the bottom of the gate trench. The core principle is: a strong compensation CBL is not formed in the central window region initially; therefore, during subsequent shallow gate trench etching, the central region naturally becomes the conductivity recovery region. Specifically: Step S1: Epitaxial layer growth and cleaning First, an n+ type β-Ga2O3 substrate and an n- type β-Ga2O3 drift layer are provided, and standard cleaning is performed to establish the basic structure for vertical devices. The thickness of the drift layer is set to 4–15 μm, preferably 8–10 μm; the doping concentration is controlled at 5 × 10⁻⁶. 15 ~5×10 16 cm -3 The cleaning process can be carried out in accordance with the standard cleaning procedure described in subsequent step S2 to ensure surface cleanliness.
[0065] Step S2: Deposit sacrificial layer and patterned mask An implantation sacrificial layer is deposited on the surface of the drift layer, and a patterned implantation mask is formed by photolithography. Specifically, SiO2 is deposited as the sacrificial layer using PECVD, with a thickness ranging from 50 to 150 nm, preferably about 100 nm. Subsequently, a CBL (current blocking layer) implantation window is formed on the sacrificial layer using photoresist or a SiO2 / metal hard mask. The main function of this sacrificial layer is to reduce damage to the crystal surface caused by subsequent ion implantation, while the patterned mask precisely determines the formation area of the CBL and the position of the central reserved window.
[0066] Step S3: Ion implantation into the CBL region Ion implantation is performed in the predetermined CBL region to introduce deep-level compensating impurities such as N, Mg, C, or Fe. N ions are preferably used in this step, with an implantation depth of approximately 1 μm and a target bulk concentration set at 5 × 10⁻⁶. 18 ~5×10 19 cm -3 The total dose is approximately 5 × 10 14 ~5×10 15 cm -2 To achieve a uniform electric field shielding effect, a multi-energy injection process is employed to form an approximately box-shaped impurity distribution. The key to this step is to form a high-resistivity CBL only on both sides of the bottom of the gate trench and in the area requiring shielding, while the central window area is either not injected or only injected with a very low dose, reserving space for the formation of subsequent conductive channels.
[0067] Step S4: Reserve a central conductive window A central conductive window is reserved between adjacent CBL regions. The width of this window is set to 0.5~5 μm, preferably 2~3 μm. Simultaneously, the CBL regions on both sides can each extend outwards by 1~5 μm or more to ensure sufficient electric field shielding. This reserved area corresponds to the central current window at the bottom of the final device gate trench, and its presence can significantly reduce lattice damage during subsequent donor impurity re-implantation.
[0068] Step S5: CBL injection followed by annealing The implanted samples undergo high-temperature annealing to repair lattice damage and stabilize deep-level impurities in the CBL. For N-ion implantation, annealing at 1100–1200 °C for 30–60 minutes is preferred, with N2, O2, or Ar atmospheres being suitable. For Mg-ion implantation, the annealing temperature can be 900–1100 °C, but special attention must be paid to controlling impurity diffusion. Since the patterned window region is not implanted or only has a low-dose implantation, this region retains a relatively conductive state after annealing.
[0069] Step S6: Remove the sacrificial layer and form the source region Remove the implanted sacrificial layer from the surface and form an n++ source region or a highly doped source layer. The source region can be formed by Si ion implantation, with a depth controlled between 50 and 150 nm and a concentration range of 1 × 10⁻⁶. 19 ~5×10 19 cm -3 Alternatively, a highly doped β-Ga₂O₃ layer of 100–300 nm thickness can be grown epitaxially, with the concentration also controlled at 1 × 10⁻⁶. 19 ~5×10 19 cm -3 This step aims to create a low-resistance ohmic contact and provide sufficient electron injection regions on both sides of the gate trench.
[0070] Step S7: Photolithography defines the gate trench area The key to defining the gate trench region using photolithography is precisely aligning the center of the gate trench with the conductive window reserved in step S4. The gate trench width is set to a range of 2–8 μm, preferably about 4 μm; the window width is preferably 2–3 μm. To ensure alignment accuracy, it is recommended that the alignment deviation be less than half the difference between the window width and the gate trench width (e.g., less than 0.5 μm). This alignment strategy ensures that the conductive window is located at the center of the bottom of the gate trench, while the CBL semi-enclosed area is still retained on both sides to provide electric field shielding.
[0071] Step S8: Etching to form shallow U-shaped gate trenches Shallow U-shaped gate trenches are formed using an ICP / RIE dry etching process. The etching gas can be a Cl2 / BCl3 / Ar mixture, with an example flow ratio of Cl2: 35~60 sccm, BCl3: 5~10 sccm, and Ar: 5~10 sccm. Regarding process parameters, the ICP power is controlled at 300~800 W (preferably approximately 600 W), the RF bias power is controlled at 50~150 W (preferably 50~100 W), and the chamber pressure is 5~20 mTorr. The etching depth is set to 600~800 nm and must be less than the CBL thickness (approximately 1 μm). After etching, the trench bottom does not completely penetrate the CBL; the central position corresponds to a pre-reserved conductive window, and the two sides correspond to the CBL shielding area.
[0072] Step S9: Repair of gate trench damage Damage repair treatment is performed on the etched gate trenches to remove surface damage caused by ICP etching and improve the reliability of the subsequent gate dielectric interface. This can be achieved using a wet process with H3PO4, with the temperature controlled at 100~120℃ and the time at 0.5~3 min (preferably 110℃, 1 min); or a combination of low-damage wet processing and heat treatment can be used.
[0073] Step S10: Deposit gate dielectric layer A high-quality gate dielectric layer is deposited within the repaired gate trench. Al₂O₃ is deposited using the ALD process, with a thickness ranging from 30 to 80 nm, preferably 40 to 70 nm, and the deposition temperature is preferably 40 to 70 °C. Besides Al₂O₃, HfO₂, SiO₂, AlN, or composite dielectric materials can also be used. This dielectric layer covers the sidewalls and bottom of the gate trench, forming a reliable insulating layer.
[0074] Step S11: Metal electrode formation Form the source, drain, and gate metal electrodes. The source and drain metals can be Ti / Au (50 / 150 nm) or Ti / Al / Ni / Au systems, and undergo ohmic annealing at 400–500 °C for 1–2 minutes (or as optimized according to specific processes); the gate metal can be Ni / Au (50 / 150 nm). This step completes the construction of all electrodes for the device.
[0075] Step S12: Passivation and Pad Opening Finally, a passivation layer is deposited and photolithography is used to create the pad windows. The passivation layer can be SiN deposited by PECVD. x / SiO2 or ALD deposited Al2O3, with a thickness ranging from 100 to 500 nm. This step aims to improve the stability of the device surface and the reliability of the packaging, and to prevent environmental factors from affecting the device performance.
[0076] The semi-enclosed gate oxide structure gallium oxide UMOSFET proposed in this invention can effectively reduce the peak electric field at the bottom and corners of the gate oxide layer, alleviate the problem of local electric field concentration in the gate dielectric layer under high-voltage operating conditions, significantly reduce the risk of premature gate oxide breakdown failure, and improve the overall high-voltage operating reliability of the device. This invention fully utilizes the mature CBL current blocking layer technology in gallium oxide vertical power devices to achieve electric field shielding, eliminating the need for fabricating a highly difficult low-resistivity p-type gallium oxide bulk region, thus avoiding the device fabrication challenges caused by the bottleneck of gallium oxide p-type doping technology, and making the technology more feasible for practical application. This invention sets a conductivity recovery window in the center of the bottom of the gate trench to preserve the vertical conduction path of the device, avoiding complete blockage of carrier transport due to the intact retention of the CBL current blocking layer, effectively preventing a sharp increase in on-resistance, and balancing high-voltage shielding effect with device conduction performance. Within the device structure framework of this invention, designers can flexibly adjust the gate trench depth, CBL thickness, conductivity recovery window width, and doping dosage of donor impurities and deeply compensated impurities. Based on practical application requirements, trade-offs and optimizations are achieved among several key performance aspects, including device breakdown voltage, on-resistance, threshold voltage, and device reliability, adapting to diverse power application scenarios. This invention also provides two feasible device fabrication paths, adaptable to different semiconductor process platforms. The approach of first completing CBL implantation over the entire area and then fabricating the conductivity recovery window at the bottom of the gate trench is more suitable for verifying the device structure principle. The fabrication approach using patterned implantation to pre-reserve the conductivity recovery window eliminates the need for a secondary donor implantation process at the bottom of the gate trench, effectively reducing gate bottom process damage caused by secondary implantation and making it suitable for mass production process development.
[0077] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the essence and scope of the technical solutions of the present invention.
Claims
1. A gallium oxide UMOSFET device, characterized in that, Includes drain (1), gallium oxide substrate (2), gallium oxide drift layer (3), current blocking layer (4), conductivity recovery region (5), n ++ Source region (6), source electrode (7), gate dielectric layer (8) and gate (9); The drain (1) is disposed on the lower surface of the gallium oxide substrate (2); The gallium oxide drift layer (3) is disposed on the gallium oxide substrate (2); The current blocking layer (4) is disposed on the upper part of the gallium oxide drift layer (3); The device is provided with a gate trench, the etching depth of the gate trench is less than the thickness of the current blocking layer (4), the current blocking layer (4) is retained on both sides of the bottom of the gate trench, the conductive recovery region (5) is provided in the center of the bottom of the gate trench, the conductive recovery region (5) is connected downward to the gallium oxide drift layer (3), and the lateral width of the conductive recovery region (5) is less than the lateral width of the gate trench. n is provided above the current blocking layer (4). ++ Source region (6), the n ++ A source electrode (7) is formed on the source region (6); The inner wall of the gate trench is covered with a gate dielectric layer (8), and the cavity formed by the gate dielectric layer (8) is filled with a gate electrode (9). The current blocking layers (4) on both sides are respectively arranged on the outside of the bottom corner of the gate dielectric layer (8) to form an electric field shield for the bottom corner of the gate dielectric layer (8).
2. The gallium oxide UMOSFET device according to claim 1, characterized in that, The transverse width of the conductive recovery region (5) is smaller than the transverse width of the gate slot.
3. A gallium oxide UMOSFET device according to claim 1, characterized in that, The transverse width of the gate groove is 2~8μm; the transverse width of the conductive recovery region (5) is 0.5~5μm.
4. A gallium oxide UMOSFET device according to claim 1, characterized in that, The etching depth of the gate trench is 40% to 90% of the thickness of the current blocking layer (4).
5. A gallium oxide UMOSFET device according to claim 1, characterized in that, The thickness of the current blocking layer (4) is 0.5-2.0 μm, and the etching depth of the gate trench is 0.5-0.9 μm.
6. The gallium oxide UMOSFET device according to claim 1, characterized in that, The current blocking layer (4) is formed by at least one deep-level compensating impurity selected from N, Mg, C and Fe; the conductivity recovery region (5) is formed by at least one donor impurity selected from Si, Sn, Ge, Nb and Ta.
7. A gallium oxide UMOSFET device according to claim 1, characterized in that, The gate dielectric layer (8) includes Al2O3, SiO2, HfO2, and SiN. x One or more of AlN; the thickness of the gate dielectric layer (8) is 30nm~80nm.
8. A method for fabricating a gallium oxide UMOSFET device according to any one of claims 1 to 7, characterized in that, Includes the following steps: A gallium oxide substrate (2) is provided, and a drain (1) is formed on the lower surface of the gallium oxide substrate (2). A gallium oxide drift layer (3) is formed on the upper surface of the gallium oxide substrate (2); A current blocking layer (4) is formed on the gallium oxide drift layer (3); Etching forms a gate trench, wherein the etching depth of the gate trench is less than the thickness of the current blocking layer (4); A conductive recovery region (5) is formed in the center of the bottom of the gate trench, and the conductive recovery region (5) is connected downward to the gallium oxide drift layer (3); A gate dielectric layer (8) is formed on the inner wall of the gate groove; The gate electrode (9) is filled in the cavity enclosed by the gate dielectric layer (8); An n++ source region (6) and a source electrode (7) are formed above the current blocking layer (4).
9. The method for fabricating a gallium oxide UMOSFET device according to claim 8, characterized in that, The formation of a conductive recovery region (5) at the center of the bottom of the gate trench specifically involves: After forming a complete current blocking layer (4), the injection window is defined by photolithography; Donor impurities are injected into the center of the bottom of the gate trench through the injection window to locally offset the compensation effect of the current blocking layer (4) and form an n-type conductivity recovery region (5).
10. The method for fabricating a gallium oxide UMOSFET device according to claim 8, characterized in that, The formation of a current blocking layer (4) on the gallium oxide drift layer (3) specifically involves: A patterned injection mask is formed by photolithography, and the mask has a window reserved in the central region at the bottom of the gate trench; Ion implantation is performed through the mask to form a current blocking layer (4) in the region on both sides of the window, while the window region remains a conductive gallium oxide drift layer (3) as a subsequent conductive recovery region (5).