A ring hole detector based on indium pillar reverse solder interconnect and its fabrication method

By first connecting the via to the readout circuit using a flip-wire interconnect process and then etching the via, the problems of large etching aspect ratio and light loss in traditional via detectors are solved, enabling the fabrication of via detectors with smaller vias and higher quantum efficiency.

CN123124498APending Publication Date: 2026-11-17SHANGHAI INSTITUTE OF TECHNICAL PHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611630119.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the traditional fabrication process of ring aperture detectors, the etching aspect ratio is large, the selectivity is poor, and there are many residues, which leads to a reduction in the diameter of the ring aperture, severe light loss, and the p electrode cannot be placed below the absorption layer.

Method used

The process sequence of interconnecting first and then opening via is adopted. The conductive interconnect structure is connected to the readout circuit through the flip-flop interconnect process, and through-holes are formed in the mercury cadmium telluride material layer. The inner wall region is an n-type semiconductor region, avoiding the etching and filling adhesive layer step.

Benefits of technology

This improved pixel density and quantum efficiency, reduced light loss, and enabled the grid p-electrode to be placed below the absorption layer, thereby enhancing the light absorption rate and reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124498A_ABST
    Figure CN123124498A_ABST
Patent Text Reader

Abstract

This invention discloses a ring-hole detector based on indium pillar flip-chip interconnects and its fabrication method, belonging to the field of infrared detection technology. The fabrication method employs a process sequence of interconnecting first and then etching the hole; the method includes the following steps: S1: providing a mercury cadmium telluride (HCd) material layer and a readout circuit; S2: fabricating a conductive interconnect structure on the first surface of the HCd material layer; S3: interconnecting the conductive interconnect structure with the readout circuit using a flip-chip interconnect process; S4: fabricating a via extending to a thickened electrode at a corresponding position on the second surface of the HCd material layer, wherein the inner wall region of the via forms an n-type semiconductor region; S5: fabricating n-contact electrodes on the inner wall and bottom of the via. This invention, by employing a process sequence of flip-chip interconnecting first and then etching the hole, completely avoids the step of etching the filler layer, thereby reducing the effective etching depth to only the thickness of the HCd material layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of infrared detection technology, and particularly relates to a ring hole detector based on indium pillar reverse solder interconnect and its fabrication method. Background Technology

[0002] Mercury cadmium telluride ring aperture detectors are formed by etching, and the junction surface of the pn junction is perpendicular to the incident plane. This has the advantages of reducing the probability of dislocation crossing the junction region and reducing dark current. At the same time, the device has a large fill factor, which is beneficial to improving quantum efficiency.

[0003] The typical fabrication process for traditional via detectors involves first bonding a mercury cadmium telluride (HCDT) epitaxial material to the readout circuit using an adhesive (such as epoxy resin); then etching vias from the top surface of the material, penetrating the entire HCDT material layer and the intermediate filler layer; finally, depositing a conductive layer within the via to connect the inversion layer to the readout circuit. However, this process has a significant drawback: the etching depth of the via is the sum of the depth of the epitaxial material and the filler layer. Due to the inherent limitations of aspect ratio, this large etching depth directly restricts further reduction in the via diameter, becoming a key bottleneck for improving detector pixel density and quantum efficiency. Furthermore, the etching selectivity ratio of commonly used adhesives (such as epoxy resin) to photoresists is close to 1:1, requiring additional consideration of photoresist thickness when selecting the photoresist. In addition, adhesives are prone to polymer residue after etching, potentially causing sidewall contamination. These defects severely degrade the deposition quality and ohmic contact characteristics of subsequent electrode films.

[0004] In the typical fabrication process of traditional ring aperture detectors, the p electrode is a grid electrode deposited on the incident surface, i.e., the second surface of mercury cadmium telluride, which causes light loss. This is because it is difficult to align and bond the two sides using adhesives, so the p electrode cannot be placed under the absorption layer.

[0005] Therefore, overcoming the process challenges caused by etching the filler layer and providing a new method for fabricating ring-hole detectors is an urgent technical problem to be solved. Summary of the Invention

[0006] This invention provides a method for fabricating a ring hole detector based on indium pillar reverse solder interconnect, which solves the problems of large etching aspect ratio, poor selectivity and large amount of residue caused by the need to etch the filler layer in traditional processes.

[0007] A further technical problem to be solved by the present invention is to provide a ring hole detector based on indium pillar reverse solder interconnection prepared by the above method.

[0008] To achieve the above objectives, the present invention adopts the following technical solution:

[0009] A method for fabricating a ring-hole detector based on indium pillar flip-wire interconnection employs a process sequence of interconnection followed by hole opening; the fabrication method includes the following steps:

[0010] S1: Provides the mercury cadmium telluride material layer and readout circuitry;

[0011] S2: A conductive interconnect structure is prepared on the first surface of the mercury cadmium telluride material layer;

[0012] S3: The conductive interconnect structure is interconnected with the readout circuit using a flip-chip interconnect process (preferably flip-solder interconnect process);

[0013] S4: A via extending to the thickened electrode is prepared at a corresponding position on the second side of the mercury cadmium telluride material layer, wherein the inner wall region of the via forms an n-type semiconductor region;

[0014] S5: Prepare n-contact electrodes on the inner wall and bottom of the through hole;

[0015] The first surface and the second surface are two surfaces opposite to each other of the mercury cadmium telluride material layer.

[0016] A ring hole detector based on indium pillar flip-wire interconnect includes a mercury cadmium telluride material layer, a readout circuit, and a conductive interconnect structure; wherein the conductive interconnect structure is located between the mercury cadmium telluride material layer and the readout circuit and realizes electrical connection between the two;

[0017] The mercury cadmium telluride material layer has at least one through-hole, and the inner wall region of the through-hole is an n-type semiconductor region.

[0018] The beneficial effects of this invention are as follows:

[0019] (1) In traditional processes, the etching depth is equal to the sum of the thickness of the mercury cadmium telluride (MDT) material layer and the thickness of the filler layer. Since the etching depth-to-width ratio is usually limited to about 2:1, the maximum allowable etching depth limits the minimum machinable hole diameter. This invention completely avoids the step of etching the filler layer by first soldering the interconnects and then etching the openings, thus reducing the effective etching depth to only the thickness of the MDT material layer.

[0020] (2) Under the same aspect ratio constraint, the present invention can process smaller annular holes, thereby increasing the pixel density; or, while maintaining the same annular hole size, it allows the use of a thicker mercury cadmium telluride absorption layer, thereby improving the quantum efficiency of the device.

[0021] (3) The reverse soldering interconnection process of the present invention can transfer the grid p electrode on the incident surface to the other side, thereby improving the light absorption rate. Attached Figure Description

[0022] Figure 1 This is a cross-sectional schematic diagram of the annular hole detector based on indium pillar reverse solder interconnect of the present invention.

[0023] Figure 2This is a schematic diagram of step S2 in the fabrication method of the indium pillar flip-wire interconnect-based annular hole detector of the present invention.

[0024] Figure 3 for Figure 2 A cross-sectional diagram of the area marked with a red line.

[0025] Figure 4 This is a schematic diagram showing the location of the thickened electrode in this invention.

[0026] In the attached figures, the reference numerals are as follows: 1-mercury cadmium telluride material layer; 2-readout circuit; 31-first passivation layer; 32-second passivation layer; 4-n-type semiconductor region; 5-n-contact electrode; 6-thickened electrode; 7-conductive interconnect structure; 8-grid p-electrode; 9-filler layer; 10-substrate. Detailed Implementation

[0027] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention. Furthermore, the technical features involved in the various embodiments of this invention described below can be combined with each other as long as they do not conflict with each other.

[0028] See Figures 1 to 4 The present invention provides an indium pillar flip-wire interconnect-based ring hole detector, which includes a mercury cadmium telluride material layer 1, a readout circuit 2, a passivation layer, a thickened electrode 6, a conductive interconnect structure 7, a grid p electrode 8, an n-type semiconductor region 4, an n-contact electrode 5, and a filler adhesive layer 9.

[0029] Among them, the two opposite surfaces of the mercury cadmium telluride material layer 1 are the first surface and the second surface, respectively. A passivation layer exists on both the first surface and the second surface of the mercury cadmium telluride material layer 1, that is, the passivation layer includes the first surface passivation layer 31 and the second surface passivation layer 32.

[0030] The grid p-electrode 8 is located on the first surface of the mercury cadmium telluride material layer 1 (during fabrication, the passivation layer at the corresponding position needs to be etched before the grid p-electrode 8 is grown). Thickened electrodes 6 are provided on the outermost readout area of ​​the grid p-electrode 8 and the passivation layer area at the center of the grid. Conductive interconnection structure 7 is provided on the thickened electrodes 6, that is, the thickened electrodes 6 are in contact with the conductive interconnection structure 7.

[0031] In this embodiment, the conductive interconnect structure 7 is an indium pillar. The conductive interconnect structure 7 and the indium pillar of the readout circuit 2 are connected using a flip-chip interconnect process. That is, the conductive interconnect structure 7 is located between the mercury cadmium telluride material layer 1 and the readout circuit 2, achieving electrical connection between the two. After connection, an adhesive (preferably epoxy resin) is filled between the mercury cadmium telluride material layer 1 and the readout circuit 2 to form a filler layer 9. In this embodiment, the conductive interconnect structure 7 is connected to the indium pillar on the surface of the readout circuit 2.

[0032] See further Figure 1 and Figure 4 The outermost readout region of the grid p-electrode is Figure 4 Region two can be defined as the outermost convex point of the grid p-electrode, or as the first effective p-electrode region at the outermost edge; the convex points of the grid p-electrode 8 in region two contact the thickened electrode 6. The grid center region of the grid p-electrode is... Figure 4 In region one, there are no protrusions of the grid p electrode 8 in the center region of the grid. At this time, the thickened electrode 6 in region one is in direct contact with the n contact electrode 5.

[0033] See Figure 1 At least one through-hole is provided on the mercury cadmium telluride material layer 1, which penetrates the entire mercury cadmium telluride material layer 1 (including the passivation layer of the mercury cadmium telluride material layer 1). The termination position of the through-hole is the thickened electrode 6, that is, the bottom of the through-hole is the thickened electrode 6. The inner wall region of the through-hole is an n-type semiconductor region 4. An n-contact electrode 5 is provided on the inner wall and the bottom of the through-hole, and the n-contact electrode 5 is electrically connected to the thickened electrode 6 and the n-type semiconductor region 4.

[0034] Accordingly, this invention provides a method for fabricating a ring-hole detector based on indium pillar reverse solder interconnects, which adopts a process sequence of interconnection followed by hole opening; the fabrication method includes the following steps:

[0035] S1: Provide a mercury cadmium telluride material layer 1 with a substrate 10 and a readout circuit 2. In this embodiment, the substrate is preferably a cadmium zinc telluride substrate.

[0036] S2: A conductive interconnect structure 7 is prepared on the first surface of the mercury cadmium telluride material layer 1.

[0037] Specifically, step S2 includes the following steps:

[0038] S21: Fabricate a grid of p-electrodes 8 on the first passivation layer 31. See details below. Figure 2 and Figure 3First, a first passivation layer 31 is grown on the first surface of the mercury cadmium telluride material layer 1. In this embodiment, the first passivation layer 31 is a CdTe / ZnS double passivation layer, where CdTe serves as a contact layer that contacts the first surface of the mercury cadmium telluride material layer 1, and ZnS serves as an antireflection insulating layer. The total thickness of the first passivation layer 31 is 0.2–0.3 micrometers, which can be adjusted according to the process. Then, through photolithography and etching processes, holes are made in the first passivation layer 31, and a grid p-electrode 8 is fabricated by electron beam evaporation. In this embodiment, the grid p-electrode 8 is Au, with a thickness of 0.1–0.2 micrometers.

[0039] S22: A thickened electrode 6 is fabricated on the first passivation layer 31 of the outermost readout region and the center region of the grid p-electrode 8. Specifically, using photolithography and vacuum deposition processes, a thickened electrode 6 is fabricated on the first passivation layer 31 of the outermost readout region and the center region of the grid p-electrode. The thickened electrode 6 is Cr / Au, with the first Cr layer serving as a contact layer that contacts the first passivation layer 31 or the grid p-electrode 8. The total thickness of the thickened electrode 6 is 0.3–0.4 micrometers. See also... Figure 4 In this step, the thickened electrode 6 is fabricated on the protrusions of the outermost readout region of the grid p electrode, and at the same time, the thickened electrode 6 is fabricated on the first passivation layer 31 in the central region of the grid.

[0040] S23: The conductive interconnect structure 7 is fabricated on the thickened electrode; the thickened electrode 6 and the conductive interconnect structure 7 in the outermost readout region are used for signal readout. Specifically, an indium pillar is fabricated in the center of the thickened electrode 6 using photolithography and vacuum deposition processes. During fabrication, an Au layer is grown first, followed by the growth of the indium pillar, which has a height of 4–5 micrometers.

[0041] S3: The conductive interconnect structure is interconnected with the readout circuit using a flip-chip interconnect process. Specifically, the indium pillars of the mercury cadmium telluride material layer 1 are aligned and thermo-bonded with the indium pillars on the surface of the readout circuit 2 using a flip-chip interconnect process, and then fixed with epoxy resin after interconnection. At this time, the substrate 10 of the mercury cadmium telluride material layer 1 is on top.

[0042] S4: A via extending to the thickened electrode is fabricated at a corresponding position on the second side of the mercury cadmium telluride (HCDT) material layer, and an n-type semiconductor region is formed in the inner wall region of the via. Specifically, the substrate 10 is removed using a polishing process to expose the second side of the HCDT material layer 1; a second passivation layer 32 is grown on the second side of the HCDT material layer 1. In this embodiment, the second passivation layer 32 is a CdTe / ZnS double passivation layer; a ring hole pattern is defined on the second passivation layer 32 by photolithography; and an inductively coupled plasma etching process is used to etch downwards to remove the second passivation layer 32, the HCDT material layer 1, and the first passivation layer 31 in this region. By real-time monitoring of the etching endpoint, the etching is precisely controlled to stop when it reaches the surface of the thickened electrode 6 (i.e., the termination position of the via is the thickened electrode 6). This process forms a via penetrating the HCDT material layer 1, and simultaneously transforms the p-type HCDT material in the inner wall of the via into an n-type semiconductor region 4.

[0043] S5: An n-contact electrode 5 is fabricated on the inner wall and bottom of the through-hole. Specifically, the n-contact electrode 5 is fabricated on the inner wall and bottom of the through-hole using photolithography and vacuum deposition processes, followed by ion beam sputtering. In this embodiment, the n-contact electrode 5 is In / Au, where In is the contact layer and Au is the thickening layer. The total thickness of the n-contact electrode 5 is 0.7–0.8 micrometers.

[0044] This invention discloses a via detector based on indium pillar flip-chip interconnects and its fabrication method. The fabrication method includes: firstly, forming a conductive interconnect structure 7 on one surface of a mercury cadmium telluride (HCDT) material layer 1, and then interconnecting it with a readout circuit 2 using a flip-chip bonding process; then, etching a via from the other surface of the HCDT material layer 1, and forming an n-type semiconductor region on the wall of the via. In this embodiment, the via detector includes a HCDT material layer 1, a readout circuit 2, and a conductive interconnect structure 7 between them. The HCDT material layer 1 has a through-hole, and an n-contact electrode 5 is formed on the through-hole and connected to the readout circuit 2 through the conductive interconnect structure 7. This invention solves the alignment problem when the grid p-electrode is placed below by the "interconnect first, then open via" process sequence, avoids the problems of large etching aspect ratio, poor selectivity, and residue caused by etching the filler layer in traditional via processes, relaxes the restrictions on the thickness of the HCDT material layer and the width of the etched via, and is beneficial to improving the quantum efficiency and reliability of the device.

[0045] Those skilled in the art will readily understand that the above description is merely a preferred embodiment of the present invention. The above embodiments are provided only for the purpose of describing the present invention and are not intended to limit the present invention. Parts not described in detail in this specification are well-known in the art and are not intended to limit the scope of the present invention. The scope of the present invention is defined by the appended claims. All equivalent substitutions and modifications made without departing from the spirit and principle of the present invention should be covered within the scope of the present invention.

Claims

1. A method for fabricating a ring hole detector based on indium pillar flip-wire interconnection, characterized in that, The fabrication method employs a process sequence of interconnection followed by aperture opening; the fabrication method includes the following steps: S1: Provides the mercury cadmium telluride material layer and readout circuitry; S2: A conductive interconnect structure is prepared on the first surface of the mercury cadmium telluride material layer; S3: The conductive interconnect structure is interconnected with the readout circuit using a flip-chip interconnect process; S4: A via extending to the thickened electrode is prepared at a corresponding position on the second side of the mercury cadmium telluride material layer, wherein the inner wall region of the via forms an n-type semiconductor region; S5: Prepare n-contact electrodes on the inner wall and bottom of the through hole; The first and second surfaces are the two opposite surfaces of the mercury cadmium telluride material layer.

2. The method for fabricating a ring-hole detector based on indium pillar flip-wire interconnection according to claim 1, characterized in that, Step S2 specifically includes the following steps: S21: Fabricate a grid p-electrode on the passivation layer on the first surface; S22: Thickened electrodes are fabricated on the passivation layer of the outermost readout region and the central region of the grid p electrode; S23: The conductive interconnect structure is fabricated on the thickened electrode, and the thickened electrode and conductive interconnect structure in the outermost readout region are used for signal readout.

3. The method for fabricating a ring hole detector based on indium pillar reverse solder interconnect according to claim 2, characterized in that, The conductive interconnect structure is an indium pillar. In step S23, the conductive interconnect structure is prepared by first growing Au and then growing the indium pillar.

4. The method for fabricating a ring hole detector based on indium pillar reverse solder interconnect according to claim 3, characterized in that, In step S3, the conductive interconnect structure is interconnected with the readout circuit using a flip-chip interconnect process. Specifically, the conductive interconnect structure and the indium pillars of the readout circuit are aligned and hot-pressed together.

5. The method for fabricating a ring hole detector based on indium pillar reverse solder interconnect according to claim 4, characterized in that, Step S3, after hot-press bonding, also includes a step of filling with adhesive for fixation.

6. The method for fabricating a ring hole detector based on indium pillar reverse solder interconnect according to claim 1, characterized in that, Step S4 includes a step of removing the substrate of the mercury cadmium telluride material layer to expose the second surface before fabricating the via extending to the thickened electrode on the second surface of the mercury cadmium telluride material layer.

7. The method for fabricating a ring hole detector based on indium pillar reverse solder interconnect according to claim 2, characterized in that, In step S4, the through hole is prepared by etching, specifically by removing the passivation layer and mercury cadmium telluride material layer in the corresponding area by etching, and the process terminates when the surface of the thickened electrode is reached.

8. A ring hole detector based on indium pillar reverse solder interconnect, characterized in that, The ring-hole detector is fabricated using the fabrication method of indium pillar flip-bonded interconnect according to any one of claims 1 to 7; the ring-hole detector includes a mercury cadmium telluride material layer, a readout circuit, and a conductive interconnect structure; wherein the conductive interconnect structure is located between the mercury cadmium telluride material layer and the readout circuit and realizes electrical connection between the two; The mercury cadmium telluride material layer has at least one through-hole, and the inner wall region of the through-hole is an n-type semiconductor region.

9. The annular hole detector based on indium pillar reverse solder interconnect according to claim 8, characterized in that, Both the first and second sides of the mercury cadmium telluride material layer are covered with a passivation layer, wherein the first side is the side connected to the readout circuit through the conductive interconnect structure; The annular detector also includes a thickened electrode located on the first surface of the mercury cadmium telluride material layer, and the thickened electrode is in contact with the conductive interconnect structure.

10. The annular hole detector based on indium pillar reverse solder interconnect according to claim 9, characterized in that, The aperture detector further includes a grid p-electrode and an n-contact electrode. The grid p-electrode is located on the first surface of the mercury cadmium telluride material layer, and the n-contact electrode covers the inner wall and bottom of the aperture. The n-contact electrode is electrically connected to the thickened electrode and the n-type semiconductor region.