A single crystal furnace polycrystalline silicon feeding device with screening and milling functions

By using a sealed shell and rotating plate to create a negative pressure space in the single crystal furnace feeding device, the silicon block stuck in the coarse filter is sucked away. Combined with micro-vibration and negative pressure expansion, the problems of easy clogging of the coarse filter and diffusion of ultrafine dust are solved, achieving efficient screening and crushing, and improving the yield and purity of single crystal silicon.

CN123149017APending Publication Date: 2026-11-24LINTON KAYEX TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611412529.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-11
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In the existing single crystal furnace feeding device, the coarse filter screen is prone to clogging during the screening and crushing process, which cannot simultaneously prevent the production of ultrafine silicon powder and avoid dust diffusion, thus affecting the yield of single crystal products.

Method used

The sealed shell and rotating plate form a sealed space, and the silicon block stuck in the mesh of the coarse filter is sucked away by negative pressure. The impurities are removed by reciprocating motion and micro-vibration. Combined with negative pressure expansion and secondary crushing, efficient screening and crushing are achieved.

Benefits of technology

It effectively unclogs clogged mesh, reduces the generation of ultrafine silicon powder, improves screening quality and single crystal yield, avoids dust diffusion, and improves feeding efficiency and purity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149017A_ABST
    Figure CN123149017A_ABST
Patent Text Reader

Abstract

A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions is disclosed. This device addresses the problem that existing silicon feeding devices, with their crushing and screening structures, cannot simultaneously meet the three core process requirements of preventing coarse filter blockage, controlling ultrafine silicon powder production, and avoiding large-scale dust diffusion within the chamber, thus exhibiting significant technical deficiencies. The device includes an outer shell and a chamber fixedly connected to the upper part of the outer shell. A sealed space is formed by the bottom of the sealed shell fitting against the coarse filter and a rotating plate fitting against the lower part of the coarse filter. Negative pressure is used to draw silicon blocks stuck in the mesh of the coarse filter upwards, freeing them from the mesh's constraints and allowing them to return to the chamber via a return pipe for re-crushing and screening. This achieves the effect of clearing clogged mesh and improving subsequent screening efficiency without generating dust.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of single crystal furnace feeding, and particularly to a single crystal furnace polycrystalline silicon feeding device with screening and grinding functions. Background Technology

[0002] The closed feeding device used in monocrystalline silicon production is used to process recycled polycrystalline silicon from crucible bottom material and furnace scrap. This recycled silicon material contains a large amount of flat silicon wafers of varying thicknesses, surface oxide debris, and hard silicon carbide particles. The device is equipped with raised grinding rollers and a coarse filter. The flat silicon wafers are crushed by the impact and compression of the grinding rollers, while the coarse filter separates silicon material that meets the particle size requirements. Large silicon wafers that do not pass through the filter are returned to the grinding rollers for repeated crushing. A significant drawback of the equipment during long-term cyclic operation is that the thin silicon wafers easily spread and adhere to the surface of the coarse filter. Oxide debris and fine silicon carbide powder continuously fill the mesh gaps. As the material accumulates through continuous circulation, the coarse filter frequently becomes clogged, reducing the efficiency of silicon material screening and feeding, and in severe cases, directly causing the feeding process to stop.

[0003] There are two conventional approaches to solving screen clogging in the industry, but both have irreconcilable process drawbacks and cannot meet the special production requirements of single crystal furnace feeding. The first approach is to reduce the gap between the grinding rollers, thereby increasing the extrusion force to crush large-sized flakes and critical particles that are prone to screen clogging in advance, reducing screen clogging problems at the source; however, too small a roller gap will over-crush the silicon material, generating a large amount of ultrafine silicon powder. The entire feeding chamber is a closed argon-protected environment with no external powder or slag discharge channels. The ultrafine silicon powder will continuously float in the chamber. When the silicon material is subsequently fed into the single crystal crucible, the suspended fine powder enters the high-temperature melt along with the material, causing silicon splashing, heterogeneous nucleation, and defects such as crystal dislocations, polycrystalline structures, and broken crystals, reducing the yield of single crystal products.

[0004] The second approach involves directly adding a vibration structure to the coarse filter, relying on vibration to shake off the thin sheets and accumulated powder adhering to the filter and clear the mesh. However, since the coarse filter is located in the middle of a sealed cavity, the airflow disturbance caused by the vibration will stir up the silicon micropowder deposited throughout the chamber. This dispersed dust will then mix with the qualified silicon material along with the feed channel and enter the single crystal furnace, similarly degrading the crystal pulling quality. Therefore, the existing crushing and screening structure of the silicon material feeding device cannot simultaneously meet the three core process requirements of preventing coarse filter clogging, controlling the output of ultrafine silicon powder, and avoiding large-scale dust diffusion within the chamber, exhibiting significant technical deficiencies. Summary of the Invention

[0005] The purpose of this invention is to provide a polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions. This invention solves the problem that the existing silicon feeding device's crushing and screening structure cannot simultaneously meet the three core process requirements of preventing coarse filter clogging, controlling the output of ultrafine silicon powder, and avoiding large-area dust diffusion in the silo, thus exhibiting obvious technical defects.

[0006] To achieve the above objectives, the present invention provides the following technical solution: a polycrystalline silicon feeding device for a single crystal furnace with screening and grinding functions, comprising an outer shell, a hopper fixedly connected to the upper interior of the outer shell, a grinding roller disposed below the hopper, a coarse filter screen disposed below the grinding roller, a fine filter screen disposed below the coarse filter screen, a discharge pipe disposed on one side of the outer shell, and a return pipe disposed on one side of the coarse filter screen. A baffle is fixedly connected to the upper end of the coarse filter screen, a sealing shell is disposed on the inner side of the baffle, a pull plate is disposed on the inner side of the sealing shell, a rotating plate is rotatably connected to the lower surface of the coarse filter screen, a reciprocating mechanism is disposed at one end of the grinding roller, and a pushing mechanism is disposed above the baffle. The sealing shell is used to fit its bottom against the coarse filter screen under the drive of the pushing mechanism, and the rotating plate is used to rotate under the drive of the pushing mechanism to fit against the lower surface of the coarse filter screen, so that a sealed space is formed between the sealing shell and the rotating plate. The pull plate is used to move upward under the drive of the pushing mechanism, so as to create a negative pressure in the sealed space and pull the silicon block stuck in the mesh of the coarse filter upward.

[0007] Preferably, the reciprocating mechanism includes a motor fixedly connected to one side of the housing, a gear fixedly connected to the output end of the motor, a rotating rod fixedly connected to one end of the gear, a first groove formed on the side of the rolling roller near the motor, a second groove formed on the side of the rolling roller away from the motor, a first guide groove formed on the inner wall of the second groove, a fixed rod disposed on the inner side of the second groove and fixedly connected to the housing, and a first guide rod disposed on the inner side of the first guide groove and fixedly connected to the fixed rod. The outer side of the rolling roller is fixedly connected with a protrusion.

[0008] Preferably, the rotating rod is a cuboid, and its outer surface is in contact with the inner surface of the first groove; The fixing rod is a cylinder, and its outer surface fits against the inner surface of the second groove.

[0009] Preferably, there are two rollers and multiple protrusions are provided on the rollers and are evenly distributed.

[0010] Preferably, the pushing mechanism includes a cylinder fixedly connected to the lower side of one side of the housing, a connecting plate fixedly connected to the output end of the cylinder, a push plate fixedly connected to the upper side of the connecting plate, a second guide groove opened on the upper inner side of the push plate, a second guide rod disposed on the inner side of the second guide groove, a first push rod fixedly connected to one end of the second guide rod and fixedly connected to the sealing housing, a third groove opened on the inner side of the first push rod, a third guide groove opened on the lower inner side of the push plate, a third guide rod disposed on the inner side of the third guide groove, and a second push rod fixedly connected to the pull plate and fixedly connected to the third guide rod. The second push rod is located inside the third groove.

[0011] Preferably, the end of the second guide groove away from the cylinder is an inclined straight line, and the end closer to the cylinder is a horizontal straight line.

[0012] Preferably, the width of the end of the third guide groove away from the cylinder is greater than the width of the third guide rod, the end closer to the cylinder is a horizontal straight line, and the middle section is an inclined straight line.

[0013] Preferably, the pushing mechanism further includes a sleeve fixedly connected to one side of the upper end of the push plate, a spring disposed inside the sleeve, a third push rod fixedly connected to one end of the spring and slidably connected to the sleeve, and a slider slidably connected to the lower part of the rotating plate and hinged to the third push rod. The inner side of the sleeve is fixedly connected to the first lever, and the outer side of the third push rod is fixedly connected to the second lever.

[0014] Preferably, multiple second paddles are equidistantly distributed along the central axis of the third push rod, which are used to make the first paddles alternately contact and collide with each group of second paddles when the sleeve is in continuous motion, thereby causing the rotating plate to generate a slight vibration.

[0015] Preferably, the first guide groove is used to limit the rotation of the roller by the first guide rod, so that the roller reciprocates along its axial direction, thereby driving the protrusion to reciprocate and turn the material over.

[0016] 1. Compared with the prior art, the beneficial effects of the present invention are: by sealing the bottom of the shell and the coarse filter screen together, and by rotating the plate and the bottom of the coarse filter screen together to form a sealed space, the silicon block stuck in the mesh of the coarse filter screen is sucked upward by the negative pressure, so that it is freed from the mesh restriction and enters the return pipe to return to the silo for re-crushing and screening, thereby achieving the effect of clearing the blocked mesh and improving the subsequent screening effect without generating dust.

[0017] 2. This invention effectively opens and expands closed microcracks inside silicon material through negative pressure, disrupting the integrity of the crystal structure. When the silicon material with fully expanded cracks is returned to the grinding unit for further grinding, external force can quickly penetrate and tear along the cracks. This achieves the effects of more thorough silicon material crushing, improved single-batch crushing effect, reduced repeated grinding times, avoidance of over-grinding of silicon material due to multiple mechanical compressions, and effective reduction of ultrafine silicon powder generation.

[0018] 3. This invention maintains a stable negative pressure inside the sealed shell. Through the continuous movement of the sleeve, the first paddle alternately contacts and collides with each group of second paddles, causing the rotating plate to vibrate slightly and simultaneously driving the coarse filter screen to vibrate synchronously. This thoroughly shakes off residual impurities that were drawn out from the silicon material cracks by the negative pressure but did not completely detach. Simultaneously, it causes free fine powder and oxide debris adhering to the silicon material surface to quickly detach from the material surface and fall into a concentrated collection. This achieves the effects of removing impurities inside and on the surface of silicon material cracks under a stable negative pressure environment, avoiding all-area dust generation, reducing the reflow of defective silicon material with impurities during grinding, and improving the purification effect and screening quality of the silicon material.

[0019] 4. In this invention, the rotating crushing roller is pushed by the first guide rod to reciprocate along the first guide groove, causing the protrusions to reciprocate as well. This causes the material above the crushing roller to be pushed, tumbling, and colliding with the roller. This achieves the effect of allowing the material to enter the gap between the crushing rollers at a better angle and improving feeding efficiency. At the same time, the collision causes micro-cracks to be continuously generated, which can be further expanded by subsequent negative pressure treatment, making crushing more convenient. Attached Figure Description

[0020] Figure 1 This is a schematic diagram of the overall three-dimensional structure of the present invention; Figure 2 This is a top view of the container body of the present invention; Figure 3 This is a schematic diagram of the external structure of the rotating rod of the present invention; Figure 4 This is a schematic diagram of the protruding external structure of the present invention; Figure 5 This is a top view of the first guide groove structure of the present invention; Figure 6 This is a schematic diagram of the external structure of the push plate of the present invention; Figure 7 This is a schematic diagram of the left-side cross-sectional structure of the outer casing of the present invention; Figure 8 This is a schematic diagram of the rear cross-sectional structure of the coarse filter screen of the present invention; Figure 9 For the present invention Figure 7 Schematic diagram of the structure at point A in the middle; Figure 10 For the present invention Figure 7 Schematic diagram of the structure at point B; Figure 11 For the present invention Figure 6 Schematic diagram of the structure at point C.

[0021] In the diagram: 1. Outer shell; 2. Chamber body; 3. Compressing roller; 4. Coarse filter screen; 5. Fine filter screen; 6. Discharge pipe; 7. Return pipe; 8. Baffle; 9. Sealing shell; 10. Pulling plate; 13. Rotating plate; 11. Reciprocating mechanism; 12. Pushing mechanism; 111. Motor; 112. Gear; 113. Rotating rod; 114. First groove; 115. Second groove; 116. First guide groove; 117. Fixing rod; 118. First guide rod ; 119. Protrusion; 121. Cylinder; 122. Connecting plate; 123. Push plate; 124. Second guide groove; 125. Second guide rod; 126. First push rod; 127. Third groove; 128. Third guide groove; 129. Third guide rod; 1210. Second push rod; 1211. Sleeve; 1212. Spring; 1213. Third push rod; 1214. Slider; 1215. First paddle; 1216. Second paddle. Detailed Implementation

[0022] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0023] Please see Figures 1-11 The present invention provides that: the device comprises an outer shell 1, with a chamber 2 fixedly connected to the upper part of the outer shell 1. The chamber 2 and the outer shell 1 are made of carbon steel substrate with an inner wall antistatic epoxy resin spraying process, the coating thickness is 1.0-1.5mm, and the surface resistivity is controlled at 10. 6 ~10 9Ω continuously conducts static electricity from silicon material friction, preventing electrostatic adsorption of fine powder and dust accumulation, meeting the requirements for high-purity, explosion-proof polycrystalline silicon production. Below the hopper 2 is a rolling roller 3, made of high-hardness alloy steel with a surface hardening treatment, achieving a hardness of HRC50-55, making it wear-resistant, crush-resistant, and preventing metal debris from contaminating the silicon material. Below the rolling roller 3 is a coarse filter 4, with a pore size of 3-5mm, made of 316L stainless steel precision perforated mesh with a mesh tolerance of ±0.1mm. Below the coarse filter 4 is a fine filter 5, with a pore size of 0.8-1.2mm, meeting the particle size standard for high-purity feed to the single-crystal furnace. Both sets of filters undergo electrolytic polishing for anti-static treatment, with a surface roughness Ra≤0.8μm, reducing the probability of silicon powder adhesion and accumulation. A discharge pipe 6 is provided on one side of the outer shell 1, and a return pipe 7 is connected to one side of the coarse filter screen 4. A baffle 8 is fixedly connected to the upper end of the coarse filter screen 4, and a sealing shell 9 is assembled inside the baffle 8. A pull plate 10 is slidably arranged inside the sealing shell 9, and a rotating plate 13 is rotatably connected to the lower surface of the coarse filter screen 4. A reciprocating mechanism 11 for reciprocating grinding of material is provided at one end of the roller 3, and a pushing mechanism 12 for cleaning the filter screen, negative pressure expansion and cracking, and micro-vibration dust removal is provided above the baffle 8.

[0024] The reciprocating mechanism 11 includes a motor 111 fixedly connected to one side of the housing 1. The motor 111 is an adjustable speed servo motor with a rated power of 0.75 to 1.5 kW, a rated speed of 800 to 1200 r / min, and a speed adjustment accuracy of ±5 r / min. A gear 112 is fixedly connected to the output end of the motor 111. A rectangular rotating rod 113 is fixedly connected to one end of the gear 112. The outer side of the rotating rod 113 is fitted into the inner side of the first groove 114 on the side of the rolling roller 3 near the motor 111. The clearance between the rotating rod and the first groove is 0.02 to 0.05 mm to ensure stable torque transmission without backlash. A second groove 115 is provided on the side of the pressing roller 3 away from the motor 111. A first guide groove 116 is provided on the inner wall of the second groove 115. A cylindrical fixing rod 117 fixed to the outer shell 1 is installed on the inner side of the second groove 115. The outer side of the fixing rod 117 is completely in contact with the inner side of the second groove 115. A first guide rod 118 connected to the fixing rod 117 is fixedly connected to the inner side of the first guide groove 116. Two pressing rollers 3 are symmetrically arranged. Multiple equidistant protrusions 119 are fixedly connected to the outer side of each pressing roller 3. The height of the protrusions is 4-6 mm and the distance between the protrusions is 8-12 mm. The protrusions adopt a rounded transition structure to avoid rigid crushing and the generation of ultrafine powder. The initial roller gap distance between the two sets of pressing rollers is set to 4-7 mm.

[0025] The first guide groove 116 is a spiral continuous groove (or an oblique annular groove) formed on the inner wall of the second groove 115. Its center line extends along the circumference of the roller 3 and has a component in the axial direction. The helix angle of the first guide groove 116 (i.e., the angle between the center line of the groove and the circumference) is set to 8° to 15°. This angle allows the roller 3 to generate smooth axial reciprocating movement during its rotation, while avoiding excessive axial movement speed and increased impact due to an excessively large helix angle. The first guide groove 116 has a bidirectional spiral groove structure—during one complete rotation cycle of the roller 3, the first guide rod 118 moves from one end of the spiral groove to the other end. When the roller 3 continues to rotate in the same direction, the first guide rod 118 enters the reverse spiral section, driving the roller 3 to move axially in the opposite direction, thereby achieving continuous axial reciprocating motion during the continuous rotation of the roller 3 in the same direction. Within a single rotation cycle, the rolling roller 3 completes one full reciprocating cycle of "moving from the forward axial direction to the reverse axial direction", with a single reciprocating stroke of 3 to 6 mm.

[0026] The axial reciprocating phase relationship of the two rolling rollers 3 is opposite: that is, when one rolling roller 3 moves axially to the left, the other rolling roller 3 moves axially to the right. To achieve this opposite phase movement, the first guide grooves 116 opened on the inner walls of the second grooves 115 of the two rolling rollers 3 have opposite spiral directions—one is a left-hand spiral groove and the other is a right-hand spiral groove. In the opposite phase movement state, the protrusions 119 on the outer sides of the two sets of rolling rollers 3 exert an alternating pulling effect on the material: when the left rolling roller moves to the left and the right rolling roller moves to the right, the two sets of protrusions 119 generate tangential forces in opposite directions on the material in the middle, causing the material to be twisted and kneaded in the rolling gap, which helps to adjust the posture of the flat silicon wafer and send it into the rolling gap; when the left rolling roller moves to the right and the right rolling roller moves to the left, the two sets of protrusions 119 exert opposite pressure on the material, promoting the material to flip and reposition. This reverse-phase reciprocating motion can significantly improve the material feeding efficiency and compaction uniformity, and prevent material from accumulating or getting stuck above the compaction roller.

[0027] When feeding polycrystalline silicon into the single-crystal furnace, the corresponding feeding port of the hopper 2 is opened, and the motor 111 is started. The motor 111 drives the cuboid rotating rod 113 to rotate synchronously through the gear 112. The rotating rod 113, in conjunction with the fitting and limiting structure of the first groove 114, drives the two sets of crushing rollers 3 to rotate relative to each other. The relative speed difference between the two crushing rollers is controlled at 5% to 10% to improve the material turning and crushing effect. The polycrystalline silicon material inside the hopper 2 falls between the two sets of crushing rollers 3 under the action of gravity and is crushed by the crushing rollers 3 and the outer protrusions 119. The crushed mixture falls directly onto the surface of the coarse filter screen 4 for grading and screening.

[0028] The coarse filter 4 can perform preliminary screening of crushed materials, but during operation, silicon blocks with the same mesh size as the filter screen are easily stuck inside the mesh. Combined with the accumulation and adhesion of fine powder, this directly causes filter screen blockage and a decrease in screening efficiency. Conventional optimization methods have obvious drawbacks: reducing the distance between the crushing rollers will lead to a sharp increase in the output of fine powder, affecting material quality; using the traditional filter screen vibration method will cause fine powder to scatter and generate dust inside the cavity, contaminating the equipment and affecting the feeding accuracy, making it unsuitable for feeding high-purity materials in single crystal furnaces. Therefore, after the first dispersion filtration is completed, the driving mechanism 12 is activated to complete the filter screen unclogging and material modification operations. This device is equipped with a PLC fully automatic linkage control system with a preset fixed operation sequence: material crushing and screening, static setting for 2-3 seconds, cylinder-driven sealing and forming, negative pressure building, pressure holding and cracking, micro-vibration cleaning and impurity removal, negative pressure return of unqualified materials, secondary crushing and cracking cycle, and fine screening and discharge. The entire process is automatically connected without human intervention, with a timing error of ≤0.1s, and can stably reproduce the entire crushing and purification process.

[0029] The actuator 12 completes four stages of action sequentially in a complete work cycle. The stroke distribution of each stage is controlled by the trajectory segments of the second guide groove 124 and the third guide groove 128 on the push plate 123, as follows: First stage (sealing stage) – Cylinder 121 extends, and push plate 123 shifts 0-15mm. The inclined section of the second guide groove 124 drives the second guide rod 125 to advance towards the coarse filter screen 4, and the bottom of the sealing shell 9 adheres to the upper surface of the coarse filter screen 4. At the same time, the horizontal section of the third guide groove 128 keeps the third guide rod 129 stationary, and the pull plate 10 does not move. The rotating plate 13 has not yet flipped. This stage completes the sealing of the sealing shell 9.

[0030] The second stage (rotating plate flipping stage) – Cylinder 121 continues to extend, and push plate 123 shifts by 15-25mm. Second guide groove 124 enters the horizontal section, and sealing shell 9 remains in contact and no longer moves downwards. Third guide groove 128 enters the inclined section, driving third guide rod 129 to rise upwards, causing pull plate 10 to move upwards to build negative pressure. The pull plate's single upward stroke is 12-18mm. Simultaneously, sleeve 1211 continues to push third push rod 1213 and slider 1214. Slider 1214 slides forward in the guide groove on the lower surface of rotating plate 13 (along the rotation direction of rotating plate 13), and through a hinge connection, pushes rotating plate 13 to flip around its axis until it is in contact with the lower surface of coarse filter screen 4. This stage achieves complete sealing of the sealing cavity and the establishment of negative pressure.

[0031] The third stage (negative pressure holding and expansion stage) – cylinder 121 shifts 25–35 mm. The sealing shell 9 remains in contact, the pull plate 10 reaches its upper limit position and remains there, and the stable negative pressure range within the sealed cavity is -0.04–-0.07 MPa, with a negative pressure holding time of 0.8–1.5 s. At this time, slider 1214 has slid to the top limit of rotating plate 13, and the third push rod 1213's stroke is locked. This stage completes the negative pressure expansion operation.

[0032] The fourth stage (micro-vibration cleaning stage) involves the cylinder 121 shifting 35-45 mm. The sealing shell 9 remains in contact, and the pull plate 10 remains at its upper limit position. The sleeve 1211 overcomes the elastic force of the spring 1212 and slides independently relative to the third push rod 1213. The inner first paddle 1215 and multiple sets of second paddles 1216 on the outer side of the third push rod 1213 continuously and alternately collide, generating micro-vibrations that are transmitted to the rotating plate 13 and the coarse filter screen 4. This stage completes the micro-vibration cleaning operation under negative pressure.

[0033] The four stages described above are continuously driven by a single extension stroke of a cylinder 121. The stroke distribution of each stage is precisely controlled by the trajectory lengths of the second guide groove 124 and the third guide groove 128 on the push plate 123, requiring no additional control logic. When the cylinder 121 resets, each component resets in reverse order, completing a full work cycle.

[0034] The pushing mechanism 12 includes a cylinder 121 fixed to the lower side of one side of the outer casing 1. The cylinder 121 is a precision adjustable stroke cylinder with a working air pressure of 0.4-0.6 MPa, an effective extension stroke of 35-50 mm, and an action response time of ≤0.15 s. The output end of the cylinder 121 is fixedly connected to a connecting plate 122, and a push plate 123 is fixedly mounted on one side of the upper end of the connecting plate 122. A second guide groove 124 is provided on the upper inner side of the push plate 123. The second guide groove 124 adopts an irregular structure design, with the end away from the cylinder 121 being an inclined straight line and the end closer to the cylinder 121 being a horizontal straight line. A second guide rod 125 is slidably mounted on the inner side of the second guide groove 124, with a guide fit clearance of 0.015-0.04 mm, allowing for smooth sliding. One end of the second guide rod 125 is fixedly connected to a first push rod 126, and the first push rod 126 is fixedly connected to the sealing shell 9. A third guide groove 128 is provided on the lower inner side of the push plate 123. The third guide groove 128 adopts a three-section irregular structure. The width of the groove at the end away from the cylinder 121 is greater than the width of the third guide rod 129. The middle section is an inclined straight line, and the end closer to the cylinder 121 is a horizontal straight line. The third guide rod 129 is installed inside the third guide groove 128. A third groove 127 is provided on the inner side of the first push rod 126. The second push rod 1210 is installed inside the third groove 127. The two ends of the second push rod 1210 are fixedly connected to the pull plate 10 and the third guide rod 129, respectively. Meanwhile, the pushing mechanism 12 also includes a sleeve 1211 fixed to one side of the upper end of the push plate 123. A spring 1212 is installed inside the sleeve 1211. The spring 1212 is a high-temperature resistant alloy compression spring with a wire diameter of 1.2 to 1.5 mm, a preload of 8 to 12 N, and a maximum compression stroke of 10 mm. One end of the spring 1212 is connected to a third push rod 1213 that can slide relative to the sleeve 1211.

[0035] A guide groove is formed on the lower surface of the rotating plate 13, extending along the rotation direction of the rotating plate 13 (i.e., perpendicular to the axis of rotation of the rotating plate 13). A slider 1214 is slidably disposed within this guide groove and can slide back and forth along it. The upper end of the slider 1214 is embedded in the guide groove, and the lower end is hinged to the third push rod 1213. When the third push rod 1213 moves forward, the slider 1214 slides forward along the guide groove, pushing the rotating plate 13 to rotate upwards around its axis of rotation via the hinge connection until it contacts the lower surface of the coarse filter screen 4. Therefore, the slider 1214 and the rotating plate 13 slide relative to each other in a horizontal direction (along the rotation direction of the rotating plate 13), rather than sliding up and down. This connection method ensures that the horizontal thrust of the third push rod 1213 can be effectively converted into the rotation torque of the rotating plate 13, thus achieving the desired function.

[0036] It should be noted that although the micro-vibration (frequency 35-50Hz, amplitude 0.15-0.3mm) has a small amplitude, its purpose is to generate high-frequency micro-vibration in the coarse filter screen 4 and the rotating plate 13, so as to loosen the fine powder and impurities attached to the surface of the silicon material and inside the filter screen pores, rather than to produce macroscopic displacement. The transmission path of this vibration is as follows: the vibration of the first deflector 1215 on the sleeve 1211 colliding with the second deflector 1216 on the third push rod 1213 is transmitted to the sleeve 1211 through the spring 1212 to the third push rod 1213; the third push rod 1213 is transmitted to the slider 1214 through the hinge connection; the slider 1214 is transmitted to the rotating plate 13 through the guide groove; the rotating plate 13 directly contacts and drives the coarse filter screen 4 to vibrate synchronously. Although the hinge connection and sliding connection absorb some vibration energy, the transmission efficiency of high-frequency vibration (35-50Hz) mainly depends on the rigidity of the connecting parts and the fit clearance. In this device, the hinge connection adopts a low clearance fit (gap ≤ 0.05mm), and the sliding connection adopts a precision guide groove (fitting clearance 0.02~0.05mm). The vibration energy transmission efficiency can reach 60%~75%, which is sufficient to make the coarse filter screen 4 generate effective micro-vibration.

[0037] A slider 1214 is slidably connected below the rotating plate 13, and the slider 1214 is hinged to the end of the third push rod 1213. A first paddle 1215 is fixed inside the sleeve 1211, and multiple sets of second paddles 1216 are equidistantly distributed along the central axis of the third push rod 1213, enabling continuous alternating collision vibration. Both the first and second paddles are made of PU wear-resistant material with a hardness of 80HA, are impact-resistant, do not shed debris, and do not wear or deform under long-term impact.

[0038] Cylinder 121 extends to push connecting plate 122 and push plate 123 to move synchronously. The second guide groove 124 moves with the push plate, relying on the switching of the inclined section and the horizontal section, driving the inner second guide rod 125 to move towards the coarse filter screen 4. Then, through the first push rod 126, it pushes the sealing shell 9 to move down as a whole, so that the bottom of the sealing shell 9 is tightly attached to the upper surface of the coarse filter screen 4. The bottom of the sealing shell is made of fluororubber sealing gasket with a Shore hardness of 75HA and a compression sealing amount of 1.5~2.5mm. After the fit is made up, the airtightness is 100% and there is no air leakage. At the same time, push plate 123 drives sleeve 1211, spring 1212, third push rod 1213 and slider 1214 to move synchronously. Sliding slider 1214 pushes rotating plate 13 to rotate around the lower surface of coarse filter screen 4, so that rotating plate 13 is completely attached to the lower surface of coarse filter screen 4. Together with the top sealing shell 9, a sealed space is formed, providing a sealed working condition for negative pressure unblocking operation.

[0039] To achieve effective negative pressure, the sealing shell 9 and rotating plate 13 do not only cover a small area of ​​the coarse filter 4. The sealing shell 9 is designed as a cover structure that matches the size of the effective area of ​​the coarse filter 4, and its bottom has an annular sealing edge. The sealing edge and the upper surface of the coarse filter 4 are airtightly sealed by a fluororubber sealing gasket. The rotating plate 13 is also a plate structure that matches the size of the coarse filter 4. After being flipped, it forms a sealed fit with the lower surface of the coarse filter 4. The sealing shell 9, the coarse filter 4 (the mesh in the sealed area is jointly wrapped by the sealing shell 9 and the rotating plate 13), and the rotating plate 13 together constitute a sealed cavity. The mesh in the sealed area of ​​the coarse filter 4 is completely located inside this sealed cavity. Within this sealed area, the mesh of the coarse filter 4 exists as an internal structure of the cavity, isolated from the external chamber 2 space, and there is no problem of airflow rushing in from the filter mesh to compensate for negative pressure. The sealing shell 9 only covers the effective working area of ​​the coarse filter 4 and does not cover the space above where the rolling roller 3 is located. Because the sealing shell 9 isolates the surface of the coarse filter 4 from the space of the chamber 2, when the pull plate 10 moves upward, gas can only be extracted from the internal space of the sealed cavity formed by the sealing shell 9 and the rotating plate 13. External gas cannot enter the sealed cavity through the area not covered by the coarse filter 4. Therefore, a stable negative pressure environment of -0.04 to -0.07 MPa can be formed in the sealed cavity, and the negative pressure establishment time is ≤0.2s. This sealing structure design ensures the effective realization of the negative pressure unblocking function.

[0040] As cylinder 121 extends, the third guide groove 128 continues to move with the push plate. When the sealing shell 9 is fully in contact with the filter screen, the third guide rod 129 has contacted the inclined section of the third guide groove 128. As the push plate continues to feed, the inclined trajectory drives the third guide rod 129 to rise, causing the second push rod 1210 and the pull plate 10 to slide upward along the inner wall of the sealing shell 9. The pull plate's single upward stroke is 12-18 mm. Because the outer side of the pull plate 10 is tightly in contact with the inner side of the sealing shell 9, the pull plate 10 compresses the air inside the sealed space during its upward movement, forming a stable negative pressure environment. The stable negative pressure range inside the sealed cavity is -0.04 to -0.07 MPa, and the negative pressure establishment time is ≤0.2 s. The negative pressure suction drives the air below the coarse filter screen 4 to surge upward, which can lift the stuck silicon blocks inside the filter screen mesh upward, allowing them to break free from the mesh limit, completely relieving the filter screen clogging problem, and effectively restoring and improving the subsequent screening effect.

[0041] The unqualified silicon blocks that have detached from the filter screen are discharged through the return pipe 7. The power source for the return pipe 7 is started. The return pipe adopts negative pressure suction and conveying, with a conveying air pressure of -0.02 to -0.03 MPa and a material conveying speed of 15 to 25 kg / min. This part of the silicon material is conveyed back to the inside of the silo 2 for secondary crushing and screening.

[0042] Polycrystalline silicon is a brittle material, and the "closure" state of its internal microcracks is mainly determined by the residual stress field within the material, rather than by external gas pressure. In this device, the negative pressure propagation does not directly "open" the cracks, but rather, by establishing a negative pressure environment within a sealed cavity, gas molecules adsorbed on the silicon surface are extracted, creating a pressure difference between the silicon surface and the crack interior. This pressure difference generates a tensile stress component at the crack tip, helping to lower the critical stress threshold required for crack propagation. When external mechanical crushing forces are applied, the crack preferentially propagates along the lowered crack path, thus achieving more efficient crushing. The crack propagation width of 0.05–0.15 mm is a theoretical calculation value, estimated based on the fracture toughness of polycrystalline silicon, K_IC≈0.8–1.2 MPa·m¹ / ², and the initial size of internal microcracks (approximately 0.02–0.05 mm). The actual crack propagation effect is comprehensively affected by the specific grain size of the silicon material, the crack morphology, and the negative pressure holding time. It can be controlled by adjusting the negative pressure value (-0.04–-0.07 MPa) and the holding time (0.8–1.5 s). This value is a reference value under optimized process conditions. In actual production, the crack propagation effect can be indirectly verified by testing the strength of the silicon material after crack propagation. The main function of this structure is to "assist crack propagation" rather than "directly propagate cracks," and its effect is to reduce the energy consumption and fine powder generation rate of subsequent crushing.

[0043] After the initial crushing of recycled polycrystalline silicon, numerous closed microcracks are generated within the crystal. These cracks are tightly closed, resulting in a strong overall crystal structure. If directly crushed a second time, external force is difficult to propagate along the cracks, leading to poor crushing efficiency and requiring repeated crushing. This easily causes over-grinding of the silicon material and excessive ultrafine dust. This device utilizes alternating negative pressure, with a single negative pressure expansion and holding time of 0.8–1.5 seconds and a pressure alternation frequency of 4–6 times / min. This effectively reduces the propagation threshold of closed microcracks within the silicon material, preventing damage to the crystal structure. When the silicon material is crushed again after expansion, mechanical force can quickly penetrate and tear along the microcracks, improving the thoroughness of single-stage crushing, reducing the number of repeated crushing cycles, and fundamentally reducing the amount of ultrafine silicon powder generated. This prevents fine powder accumulation and eliminates crystal pulling defects caused by fine powder entering the single crystal furnace. Simultaneously, negative pressure expansion can amplify silicon material cracks in advance, improving crushing efficiency and saving processing time.

[0044] Cylinder 121 continues to drive sleeve 1211 to feed displacement. At this time, slider 1214 has slid to the limit top of rotating plate 13, and the third push rod 1213 is locked and cannot move further. Sleeve 1211 can overcome the elastic force of spring 1212 and slide independently relative to the third push rod 1213. During the sliding process of sleeve 1211, the inner first deflector 1215 and multiple sets of equidistant second deflectors 1216 on the outer side of the third push rod 1213 continuously and alternately collide, generating micro-vibration. The vibration frequency is stably controlled at 35-50Hz, and the micro-amplitude is 0.15-0.3mm. The vibration is transmitted to rotating plate 13 and coarse filter screen 4, realizing the micro-vibration operation of the filter screen. The entire vibration process is completed in the sealed negative pressure environment of sealed shell 9, and there will be no problem of fine powder scattering.

[0045] This negative pressure synchronous micro-vibration structure achieves dual optimization effects: while negative pressure lowers the micro-crack propagation threshold and locks the silicon material location, micro-vibration can thoroughly dislodge residual impurities that have not yet detached from the silicon material cracks, and simultaneously peel off free fine powder and oxide debris attached to the silicon material surface, achieving refined impurity removal and purification of the silicon material. Compared to the shortcomings of traditional atmospheric pressure vibration, which causes serious dust generation, and static negative pressure, which cannot remove impurities from cracks, this structure can complete multiple operations such as filter cleaning, silicon material crack propagation, and impurity removal without dust generation or material loss, thereby improving silicon material purity and screening quality.

[0046] After the substandard silicon material flows back to the silo 2 through the return pipe 7, the motor 111 is restarted to drive the rolling roller 3 to rotate. During the rotation of the rolling roller 3, the first guide groove 116 at the end rotates synchronously, while the fixed rod 117 and the first guide rod 118 remain fixed. Relying on the first guide rod 118 to limit the trajectory of the first guide groove 116, the rolling roller 3 is driven to make reciprocating motion while rotating and rolling. The axial reciprocating movement frequency of the rolling roller is 8 to 12 times / min, and the single reciprocating stroke is 3 to 6 mm, which drives the outer protrusion 119 to move back and forth synchronously. The protrusion 119 continuously pushes the material to be crushed above to flip and collide with each other. On the one hand, it changes the posture of the material, so that materials of different sizes and irregular postures can enter the gap between the two sets of crushing rollers at the optimal angle, solving the problem of irregular materials getting stuck and difficult to feed, and improving feeding efficiency. On the other hand, the collision of materials can continuously generate new microcracks inside the crystal, which, together with the subsequent negative pressure expansion cracking process, further reduces the crack expansion threshold, making the subsequent crushing of silicon material easier and more thorough, forming a closed-loop high-efficiency crushing process of "crushing cracking - negative pressure expansion cracking - secondary crushing".

[0047] After multiple screenings, recycling, cracking, and secondary rolling, the qualified silicon material has met the particle size requirements and has extremely low impurity content. Finally, it is finely screened through the fine filter screen 5 and then stably discharged from the discharge pipe 6 on one side of the outer shell 1. The stable discharge speed of the whole machine is 18-30 kg / min. The proportion of ultrafine silicon powder (≤0.5 mm) in the finished silicon material is ≤1.2%, and the impurity removal rate is ≥98.5%, which is used for feeding single crystal furnaces.

[0048] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.

[0049] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions, comprising a shell (1), a hopper (2) fixedly connected to the upper interior of the shell (1), a grinding roller (3) disposed below the hopper (2), a coarse filter screen (4) disposed below the grinding roller (3), a fine filter screen (5) disposed below the coarse filter screen (4), a discharge pipe (6) disposed on one side of the shell (1), and a return pipe (7) disposed on one side of the coarse filter screen (4), characterized in that, A baffle (8) is fixedly connected to the upper end of the coarse filter screen (4). A sealing shell (9) is provided on the inner side of the baffle (8). A pull plate (10) is provided on the inner side of the sealing shell (9). A rotating plate (13) is rotatably connected to the lower surface of the coarse filter screen (4). A reciprocating mechanism (11) is provided at one end of the rolling roller (3). A pushing mechanism (12) is provided above the baffle (8). The sealing shell (9) is used to fit the bottom of the coarse filter screen (4) under the drive of the pushing mechanism (12), and the rotating plate (13) is used to rotate under the drive of the pushing mechanism (12) to fit the lower surface of the coarse filter screen (4), so that a sealed space is formed between the sealing shell (9) and the rotating plate (13). The pull plate (10) is used to move upward under the drive of the push mechanism (12) to create a negative pressure in the sealed space and pull the silicon block stuck in the mesh of the coarse filter screen (4) upward.

2. The polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 1, characterized in that, The reciprocating mechanism (11) includes a motor (111) fixedly connected to one side of the outer casing (1), a gear (112) fixedly connected to the output end of the motor (111), a rotating rod (113) fixedly connected to one end of the gear (112), a first groove (114) opened on the side of the rolling roller (3) near the motor (111), a second groove (115) opened on the side of the rolling roller (3) away from the motor (111), a first guide groove (116) opened on the inner wall of the second groove (115), a fixing rod (117) fixedly connected to the outer casing (1) and disposed inside the second groove (115), and a first guide rod (118) fixedly connected to the fixing rod (117) and disposed inside the first guide groove (116). The outer side of the rolling roller (3) is fixedly connected with a protrusion (119).

3. The polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 2, characterized in that, The rotating rod (113) is a cuboid, and its outer side surface is in contact with the inner side surface of the first groove (114); The fixing rod (117) is a cylinder, and its outer side is in contact with the inner side of the second groove (115).

4. The polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 2, characterized in that, The rolling roller (3) is provided in two parts, and the protrusions (119) are provided in multiple parts and are evenly distributed on the rolling roller (3).

5. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 1, characterized in that, The pushing mechanism (12) includes a cylinder (121) fixedly connected to the lower side of the outer shell (1), a connecting plate (122) fixedly connected to the output end of the cylinder (121), a push plate (123) fixedly connected to the upper side of the connecting plate (122), a second guide groove (124) opened on the upper side of the inner side of the push plate (123), a second guide rod (125) set on the inner side of the second guide groove (124), a first push rod (126) fixedly connected to one end of the second guide rod (125) and fixedly connected to the sealing shell (9), a third groove (127) opened on the inner side of the first push rod (126), a third guide groove (128) opened on the lower side of the inner side of the push plate (123), a third guide rod (129) set on the inner side of the third guide groove (128), and a second push rod (1210) fixedly connected to the pull plate (10) and fixedly connected to the third guide rod (129). The second push rod (1210) is located inside the third groove (127).

6. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 5, characterized in that, The second guide groove (124) is inclined straight at the end away from the cylinder (121) and horizontal straight at the end near the cylinder (121).

7. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 5, characterized in that, The width of the third guide groove (128) at the end away from the cylinder (121) is greater than the width of the third guide rod (129). The end near the cylinder (121) is a horizontal straight line, and the middle section is an inclined straight line.

8. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 5, characterized in that, The pushing mechanism (12) further includes a sleeve (1211) fixedly connected to one side of the upper end of the push plate (123), a spring (1212) disposed inside the sleeve (1211), a third push rod (1213) fixedly connected to one end of the spring (1212) and slidably connected to the sleeve (1211), and a slider (1214) slidably connected to the bottom of the rotating plate (13) and hingedly connected to the third push rod (1213). The inner side of the sleeve (1211) is fixedly connected to a first lever (1215), and the outer side of the third push rod (1213) is fixedly connected to a second lever (1216).

9. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 8, characterized in that, The second paddle (1216) is distributed equidistantly along the central axis of the third push rod (1213). It is used to make the first paddle (1215) and each group of second paddles (1216) alternately contact and collide when the sleeve (1211) moves continuously, so as to drive the rotating plate (13) to generate a slight vibration.

10. A polycrystalline silicon feeding device for a single-crystal furnace with screening and grinding functions according to claim 2, characterized in that, The first guide groove (116) is used to make the rolling roller (3) reciprocate along its axial direction by limiting the first guide rod (118) when the rolling roller (3) rotates, thereby driving the protrusion (119) to reciprocate to flip the material.